High-temperature-resistant defoaming agent and preparation method thereof
By using raw materials such as polyethylene glycol and polypropylene glycol in high-temperature defoamers for esterification and condensation reactions, an antifoaming agent with high-temperature resistance and rapid defoaming characteristics is formed, and the failure of existing defoamers in high-temperature environments is solved. The problem of efficient foam removal and long-term stability is achieved.
Patent Information
- Application Number
- CN202411401579.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-29
AI Technical Summary
In high-temperature environments, existing defoamers are prone to failure in the paper industry and power plant flue gas treatment, which makes it difficult to effectively solve the foam problem, and the defoaming efficiency is low and the amount of injection is large.
It is composed of polyethylene glycol, polypropylene glycol, oxalic acid, stearic acid, p-methylbenzenesulfonic acid, sodium hydroxide, polysiloxane silicate, emulsifier, advanced alcohol, ultrafine white carbon black and tackifier The high-temperature defoamer is used to form a hydrophilic and hydrophobic polyetherester defoamer through esterification and condensation technology. Combined with the characteristics of polysiloxane defoamer, it can achieve rapid defoaming and long-term Suppress bubbles.
The prepared defoamer is characterized by high temperature resistance, rapid defoaming, long-term foam suppression, non-toxic, corrosion-free and low dosage, which significantly improves the defoaming effect in high-temperature systems and solves the problem of foam hazards.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of defoamers, and in particular to a high temperature resistant defoamer and a preparation method thereof. Background Art
[0002] In the papermaking industry, a variety of surfactants are often used. For example, in the wet end of papermaking, various surfactants such as sizing agents, retention aids, filter aids, enhancers, deinking agents, dyes, etc. are used according to different paper types. They are also easy to foam during the operation of the paper machine; the raw material residue oil of delayed coking contains natural surfactants, which causes a large amount of foam to be generated in the coking reaction tower during the delayed coking process, forming a very high foam layer; the high-temperature agent mainly used in the high-temperature treatment of power plants is limestone slurry. During the high-temperature process, the slurry in the flue gas absorption tower will cause foam due to factors such as flue gas dust, oil content in the flue gas, incomplete combustion, metal ions in the slurry, and water quality. The generation of foam affects the measurement of the liquid level and the efficiency of the pump, which will have a great impact on production; this situation is currently solved by adding defoaming agents, but because the above environments are characterized by high temperature, it is easy to decompose and fail the effective cost of the defoaming agent, resulting in the problem that most of the existing defoaming agents have large dosage and low defoaming efficiency, so it is very important to develop a high-temperature resistant defoaming agent.
[0003] In view of this, the present invention is proposed. Summary of the invention
[0004] The first purpose of the present invention is to provide a high temperature resistant defoamer, which has the characteristics of high temperature resistance, fast defoaming, long foam suppression time and small dosage, and can well solve the problem of harmful foam in high temperature system.
[0005] The second object of the present invention is to provide a method for preparing the above-mentioned high temperature resistant defoaming agent, which can effectively improve the performance of the defoaming agent and increase the stability of the product.
[0006] In order to achieve the above-mentioned purpose of the present invention, the following technical solutions are particularly adopted: The invention provides a high temperature resistant defoaming agent, which is mainly composed of the following raw materials, measured by weight: 7-11 parts of polyethylene glycol, 5-9 parts of polypropylene glycol, 5-9 parts of oxalic acid, 9-15 parts of stearic acid, 0.3-1.5 parts of p-toluenesulfonic acid, 4-11 parts of sodium hydroxide, 4-8 parts of polysiloxane silicone grease, 4-7 parts of emulsifier, 2-6 parts of higher alcohol, 1-5 parts of ultrafine white carbon black, 0.05-0.5 parts of tackifier and 9-22 parts of deionized water.
[0007] Preferably, as a further specific embodiment, it is mainly composed of the following raw materials: 8-10 parts of polyethylene glycol, 6-8 parts of polypropylene glycol, 6-8 parts of oxalic acid, 10-14 parts of stearic acid, 0.5-1 parts of p-toluenesulfonic acid, 5-10 parts of sodium hydroxide, 5-7 parts of polysiloxane grease, 3-6 parts of emulsifier, 3-5 parts of higher alcohol, 2-4 parts of ultrafine white carbon black, 0.1-0.3 parts of tackifier and 10-20 parts of deionized water.
[0008] Preferably, as a further specific embodiment, it is mainly composed of the following raw materials: 9 parts of polyethylene glycol, 7 parts of polypropylene glycol, 7 parts of oxalic acid, 12 parts of stearic acid, 0.8 parts of p-toluenesulfonic acid, 7 parts of sodium hydroxide, 6 parts of polysiloxane grease, 4 parts of emulsifier, 4 parts of higher alcohol, 3 parts of ultrafine white carbon black, 0.2 parts of thickener and 15 parts of deionized water.
[0009] Polyethylene glycol itself has good compatibility and can be miscible with components of various organic substances. In the present invention, polyethylene glycol is selected to participate in the esterification reaction to form the molecular structure of polyether ester and increase the hydrophilicity of polyether ester; and its content is limited to 7-11 parts, at which it can be ensured that other organic components can be well dissolved in polyethylene glycol to form a liquid phase reaction system; at the same time, polyethylene glycol can act as a reactant to cause the reaction to occur. When its content is too little, it is easy to cause insufficient reaction, which ultimately affects the performance of the defoamer, and too much content is easy to cause unnecessary waste.
[0010] Polypropylene glycol has hydroxyl groups at both ends, which can be esterified to form monoesters or diesters. During the reaction, polypropylene glycol can be esterified to form hydrophobic ester groups, which can make the foam liquid film thinner, thereby reducing the stability of the foam and achieving the effect of suppressing foam. Its actual dosage is slightly less than that of polyethylene glycol. At this dosage, the performance of the prepared defoamer is more superior. Oxalic acid itself can undergo esterification, acyl halide, and amidation reactions, and the defoaming ability of the defoamer can be improved through chemical reactions.
[0011] Stearic acid, as an acid in the esterification reaction, has the chemical properties of general organic carboxylic acids and is non-toxic, thus ensuring the safety of the preparation process. p-Toluenesulfonic acid, as a catalyst, catalyzes the reaction.
[0012] In the present invention, the ultrafine white carbon black is preferably 1500-3500 mesh. The fine white carbon black itself has a small particle size, a large specific surface area, and a high surface activity. Adding it to the defoamer can effectively improve the hydrophobicity of the defoamer. The tackifier is preferably a mixture of polyacrylate and CMC in a mass ratio of 1:1. The defoamer prepared under this ratio can effectively avoid defoamer stratification, making the performance of the defoamer more uniform and stable.
[0013] Polyethylene glycol, polypropylene glycol, oxalic acid, stearic acid, and p-toluenesulfonic acid can form polyether ester defoamers with hydrophilic hydroxyl groups and lipophilic fatty chain groups through esterification reaction; polysiloxane silicone grease, higher alcohol, and ultrafine white carbon black can form high temperature resistant polysiloxane defoamers. Polysiloxane defoamers have the characteristics of rapid defoaming, long antifoaming time, safety and non-toxicity, but they are difficult to dissolve in water, high temperature resistant, and poor in strong alkali resistance; polyether defoamers have good water solubility, high temperature resistance, and strong alkali resistance, but their defoaming speed and antifoaming time are not ideal. The polyether chain is introduced into the polysiloxane chain through condensation technology, so that it has the advantages of the second type of defoamer. The addition of emulsifiers can adjust the mutual solubility between the components, and the addition of thickeners can increase the stability of the agent, so that the finished product will not be stratified due to long-term placement. Sodium hydroxide is added to adjust the pH value, and in the present invention, sodium hydroxide with a mass fraction of 30% is preferred. Sodium hydroxide can adjust the reaction conditions, and water can increase the dissolution, homogenization and emulsification properties of the solution. The synthetic defoamer, emulsifier and tackifier of the present invention are all high temperature resistant substances. Therefore, the high temperature resistant defoamer prepared by the present invention has the characteristics of high temperature resistance, good solubility, rapid defoaming, long foam suppression time and small dosage, which well solves the problem of foam hazards in high temperature foaming systems.
[0014] In the system of the present invention, since it is an organic reaction, the ratio and selection of the various substances of the reactants are subject to relatively strict restrictions. When one component is excessive, the content of another component will inevitably decrease relatively, thereby increasing side reactions, reducing the purity of the defoamer, and thus reducing its performance.
[0015] Preferably, as a further specific embodiment, the emulsifier is a mixture of 50 wt % of Span and 50 wt % of Tween 80.
[0016] Preferably, the tackifier is a mixture of polyacrylate and CMC in a mass ratio of 1:1.
[0017] In the present invention, both Span and Tween are substances with relatively high viscosity. When the two are mixed at 50wt%, they can form a stable emulsion with relatively high viscosity, which can be adsorbed on the surface of droplets and more effectively reduce surface tension, and are more suitable for the present invention.
[0018] Preferably, as a further specific embodiment, the weight average molecular weight of the polypropylene glycol is 600-1000; Preferably, the weight average molecular weight of the polypropylene glycol is 300-600; Preferably, the weight average molecular weight of the polypropylene glycol is 300.
[0019] The present invention limits the molecular weight of the selected polypropylene glycol, and the molecular weight of the selected polypropylene glycol is relatively small to ensure its solubility. At the same time, the polypropylene glycol under this molecular weight also has good affinity and is more suitable for the reaction system of the present invention. When the molecular weight is too large, the polypropylene glycol is difficult to dissolve and difficult to participate in the reaction.
[0020] Preferably, as a further specific embodiment, the higher alcohol is a fatty alcohol having a carbon number in the range of 16-28.
[0021] Preferably, a fatty alcohol having 16 carbon atoms is selected.
[0022] In the present invention, a part of the higher alcohol participates in the phosphoric acid group reaction to generate phosphate, and a part performs pH adjustment. The higher alcohol within the carbon number range has good surface activity properties and can better help the internal adhesion of the defoamer, thereby making the prepared defoamer have better defoaming performance.
[0023] The present invention also provides a method for preparing the above-mentioned high temperature resistant defoaming agent, comprising the following steps: Stirring polyethylene glycol, polypropylene glycol, oxalic acid and stearic acid, and adding p-toluenesulfonic acid during the stirring process to mix well, to obtain a mixed solution A; Introducing an inert gas into the mixed solution A, heating and cooling in stages, and adjusting the pH to 6.5-7.5 to obtain a mixed solution B; The polysiloxane silicone grease and the emulsifier are mixed and heated, and then the higher alcohol and ultrafine white carbon black are added, heated and stirred, and then cooled to obtain a mixed solution C; Stir deionized water and thickener evenly to obtain a mixed solution D; The mixed solution B, the mixed solution C and the mixed solution D are stirred and heated in sequence, and then cooled to obtain the mixture.
[0024] In the present invention, a polyether ester defoamer is first prepared, and then a polyether chain is grafted onto a polysiloxane chain by a condensation technique to make it have the characteristics of a polysiloxane defoamer. The defoamer prepared in this way has the advantages of both polyether ester defoamers and polysiloxane defoamers, namely, rapid defoaming, high temperature resistance and stronger stability.
[0025] During the reaction, inert gas is introduced to protect the mixed liquid obtained by the reaction to prevent it from contacting with oxygen and thus undergoing an oxidation reaction. During the reaction, it is necessary to add materials in stages, heat in stages and control the stirring rate to ensure that the reaction proceeds normally.
[0026] Preferably, as a further specific implementation, the specific steps of the segmented heating are: The mixed solution A is heated to 140°C-160°C and kept warm for 8h-10h; Then heat to 200°C and keep warm for 1h-2h.
[0027] Preferably, as a further specific embodiment, in the step of mixing and heating the polysiloxane grease and the emulsifier, the heating temperature is 40°C-60°C; the heat preservation time is 0.5h-1h; In the step of adding higher alcohol and ultrafine white carbon black and heating and stirring, the heating temperature is 80° C.-90° C., the heat preservation time is 1 h-2 h, and the stirring rate is 150 r / min-200 r / min.
[0028] When the reaction temperature is too high, the insulation time is too long or the stirring rate is too fast, impurities are easily produced due to side reactions; when the reaction temperature is too low, the insulation time is short or the stirring rate is too slow, it is easy to cause incomplete reaction and ultimately affect the quality of the defoamer.
[0029] Preferably, as a further specific embodiment, the specific steps of stirring and heating the mixed solution B, the mixed solution C and the mixed solution D in sequence are: The heating temperature is controlled at 60℃-80℃, and each mixed liquid is stirred for 0.5h-1h at a stirring speed of 120r / min-180r / min, and the temperature is lowered to 15℃-30℃.
[0030] Compared with the prior art, the present invention has the following beneficial effects: (1) The present invention adjusts the components of the defoaming agent so that the defoaming agent finally prepared has the characteristics of high temperature resistance, fast defoaming speed, long foam suppression time, non-toxicity, non-corrosiveness and low dosage, which effectively solves the problem of foam hazards in high-temperature foaming systems.
[0031] (2) The present invention improves the preparation method of the defoamer, which can effectively stabilize the prepared defoamer. At the same time, through the condensation technology, the prepared defoamer has the advantages of the second type of defoamer. DETAILED DESCRIPTION
[0032] The technical scheme of the present invention will be clearly and completely described below in conjunction with specific embodiments, but it will be appreciated by those skilled in the art that the following described embodiments are part of embodiments of the present invention, rather than all embodiments, and are only used to illustrate the present invention, and should not be considered as limiting the scope of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by those of ordinary skill in the art without making creative work, all belong to the scope of protection of the present invention. If specific conditions are not indicated in the embodiments, they are carried out according to normal conditions or conditions recommended by the manufacturer. If the manufacturer is not indicated in the reagents or instruments used, they are all conventional products that can be purchased commercially.
[0033] Example 1 7 g of polyethylene glycol, 5 g of polypropylene glycol with a weight average molecular weight of 1000, 5 g of oxalic acid and 9 g of stearic acid were added to a reaction kettle 1 in sequence, and 0.3 g of p-toluenesulfonic acid was added thereto while stirring to obtain a mixed solution A; The mixed solution A was stirred and nitrogen was introduced, heated to 140-160°C, kept warm for 8-10 hours, then heated to 200°C, kept warm for 1-2 hours, cooled to 25-35°C, and 4 g of sodium hydroxide with a mass concentration of 30% was added to adjust the pH to 6.5 to obtain a mixed solution B; 4 g of polysiloxane silicone grease, 2 g of Span and 2 g of Tween 80 were mixed into the reaction kettle 2 and added in sequence, heated to 40°C-60°C and maintained for 0.5 h-1 h, then 2 g of octacosanol was added, and 1 g of ultrafine white carbon black having passed through a 1500 mesh sieve was added into the reaction kettle, stirred at a rate of 150 r / min-200 r / min, heated to 80°C-90°C, maintained for 1 h-2 h, and then cooled to 20°C-30°C to obtain a mixed solution C; 9 g of deionized water was added to the reaction kettle 3, and 0.025 g of polyethylene ether and 0.025 g of CMC were mixed to prepare a tackifier, and then the tackifier was added to the reaction system, and stirred at a stirring rate of 120 r / min-180 r / min for 1.5 h to obtain a mixed solution D; Add mixed liquid C to mixed liquid D, heat it to 60℃-80℃, and stir it at a rate of 120r / min-180r / min for 0.5h-1h. Then add mixed liquid B to the reaction system, stir it at the same rate for the same time, and finally cool it to 15℃-30℃ to obtain a defoaming agent.
[0034] Example 2 11 g of polyethylene glycol, 9 g of polypropylene glycol with a weight average molecular weight of 600, 9 g of oxalic acid and 15 g of stearic acid were added to a reaction kettle 1 in sequence, and 1.5 g of p-toluenesulfonic acid was added thereto while stirring to obtain a mixed solution A; The mixed solution A was stirred and nitrogen was introduced, heated to 140-160°C, kept warm for 8-10 hours, then heated to 200°C, kept warm for 1-2 hours, cooled to 25-35°C, and 11 g of sodium hydroxide with a mass concentration of 30% was added to adjust the pH to 7.5 to obtain a mixed solution B; 8 g of polysiloxane silicone grease, 3.5 g of Span and 3.5 g of Tween 80 were mixed into the reactor 2 and added in sequence, heated to 40°C-60°C and maintained for 0.5 h-1 h, then 6 g of hexadecanol was added, and 5 g of ultrafine white carbon black having a 3000 mesh sieve was added to the reactor, stirred at a rate of 150 r / min-200 r / min, heated to 80°C-90°C, maintained for 1 h-2 h, and then cooled to 20°C-30°C to obtain a mixed solution C; 22 g of deionized water was added to the reaction kettle 3, and 0.25 g of polyethylene ether and 0.25 g of CMC were mixed to prepare a tackifier, and then the tackifier was added to the reaction system, and stirred at a stirring rate of 120 r / min-180 r / min for 1.5 h to obtain a mixed solution D; Add mixed liquid C to mixed liquid D, heat it to 60℃-80℃, and stir it at a rate of 120r / min-180r / min for 0.5h-1h. Then add mixed liquid B to the reaction system, stir it at the same rate for the same time, and finally cool it to 15℃-30℃ to obtain a defoaming agent.
[0035] Example 3 8 g of polyethylene glycol, 6 g of polypropylene glycol with a weight average molecular weight of 600, 6 g of oxalic acid and 10 g of stearic acid were added to a reaction kettle 1 in sequence, and 0.5 g of p-toluenesulfonic acid was added thereto while stirring to obtain a mixed solution A; The mixed solution A was stirred and nitrogen was introduced, heated to 140-160°C, kept warm for 8-10 hours, then heated to 200°C, kept warm for 1-2 hours, cooled to 25-35°C, and 5 g of sodium hydroxide with a mass concentration of 30% was added to adjust the pH to 6.5 to obtain a mixed solution B; 5 g of polysiloxane silicone grease, 1.5 g of Span and 1.5 g of Tween 80 were mixed into the reactor 2 and added in sequence, heated to 40°C-60°C and maintained for 0.5 h-1 h, then 3 g of hexadecanol was added, and 2 g of ultrafine white carbon black having a 2000 mesh sieve was added to the reactor, stirred at a rate of 150 r / min-200 r / min, heated to 80°C-90°C, maintained for 1 h-2 h, and then cooled to 20°C-30°C to obtain a mixed solution C; 10 g of deionized water was added to the reaction kettle 3, and 0.05 g of polyethylene ether and 0.05 g of CMC were mixed to prepare a tackifier, and then the tackifier was added to the reaction system, and stirred at a stirring rate of 120 r / min-180 r / min for 1.5 h to obtain a mixed solution D; Add mixed liquid C to mixed liquid D, heat it to 60℃-80℃, and stir it at a rate of 120r / min-180r / min for 0.5h-1h. Then add mixed liquid B to the reaction system, stir it at the same rate for the same time, and finally cool it to 15℃-30℃ to obtain a defoaming agent.
[0036] Example 4 10 g of polyethylene glycol, 8 g of polypropylene glycol with a weight average molecular weight of 300, 8 g of oxalic acid and 14 g of stearic acid were added to a reaction kettle 1 in sequence, and 1 g of p-toluenesulfonic acid was added thereto while stirring to obtain a mixed solution A; The mixed solution A was stirred and nitrogen was introduced, heated to 140-160°C, kept warm for 8-10 hours, then heated to 200°C, kept warm for 1-2 hours, cooled to 25-35°C, and 10 g of sodium hydroxide with a mass concentration of 30% was added to adjust the pH to 7.5 to obtain a mixed solution B; 7g of polysiloxane silicone grease, 3g of Span and 3g of Tween 80 were mixed into the reactor 2 and added in sequence, heated to 40-60°C and maintained for 0.5-1h, then 5g of hexadecanol was added, and 4g of ultrafine white carbon black having a 2000 mesh sieve was added to the reactor, stirred at a rate of 150-200r / min, heated to 80-90°C, maintained for 1-2h, and then cooled to 20-30°C to obtain a mixed solution C; 20 g of deionized water was added to the reaction kettle 3, and 0.15 g of polyethylene ether and 0.15 g of CMC were mixed to prepare a tackifier, and then the tackifier was added to the reaction system, and stirred at a stirring rate of 120 r / min-180 r / min for 1.5 h to obtain a mixed solution D; Add mixed liquid C to mixed liquid D, heat it to 60℃-80℃, and stir it at a rate of 120r / min-180r / min for 0.5h-1h. Then add mixed liquid B to the reaction system, stir it at the same rate for the same time, and finally cool it to 15℃-30℃ to obtain a defoaming agent.
[0037] Example 5 9 g of polyethylene glycol, 7 g of polypropylene glycol with a weight average molecular weight of 400, 7 g of oxalic acid and 12 g of stearic acid were added to a reaction kettle 1 in sequence, and 0.8 g of p-toluenesulfonic acid was added thereto while stirring to obtain a mixed solution A; Mixed solution A was stirred and nitrogen was introduced, heated to 140-160°C, kept warm for 8-10 hours, then heated to 200°C, kept warm for 1-2 hours, cooled to 25-35°C, and 7 g of sodium hydroxide with a mass concentration of 30% was added to adjust the pH to 7.0 to obtain mixed solution B; 6 g of polysiloxane silicone grease, 2 g of Span and 2 g of Tween 80 were mixed into the reactor 2 and added in sequence, heated to 40°C-60°C and maintained for 0.5 h-1 h, then 4 g of hexadecanol was added, and 3 g of ultrafine white carbon black having passed through a 2000 mesh sieve was added to the reactor, stirred at a rate of 150 r / min-200 r / min, heated to 80°C-90°C, maintained for 1 h-2 h, and then cooled to 20°C-30°C to obtain a mixed solution C; 15 g of deionized water was added to the reaction kettle 3, and 0.1 g of polyethylene ether and 0.1 g of CMC were mixed to prepare a tackifier, and then the tackifier was added to the reaction system, and stirred at a stirring rate of 120 r / min-180 r / min for 1.5 h to obtain a mixed solution D; Add mixed liquid C to mixed liquid D, heat it to 60℃-80℃, and stir it at a rate of 120r / min-180r / min for 0.5h-1h. Then add mixed liquid B to the reaction system, stir it at the same rate for the same time, and finally cool it to 15℃-30℃ to obtain a defoaming agent.
[0038] Example 6 The specific implementation method is consistent with Example 5, except that the emulsifier is changed to Tween 80 of the same mass.
[0039] Example 7 The specific implementation method is consistent with Example 5, except that the tackifier is changed to CMC of the same mass.
[0040] Example 8 The specific implementation method is consistent with Example 5, except that hexadecanol is replaced by a fatty alcohol having 10 carbon atoms.
[0041] Example 9 The specific implementation method is consistent with Example 5, except that hexadecanol is replaced by a fatty alcohol having 19 carbon atoms.
[0042] Comparative Example 1 The specific implementation method is consistent with Example 5, and the component contents of the main raw materials involved in the reaction are adjusted, as shown in Table 1.
[0043] Table 1: Changes in the components of the raw materials involved in the reaction
[0044] Comparative Example 2 The specific implementation method is consistent with Example 5, and the component contents of other raw materials participating in the reaction are adjusted, as shown in Table 2.
[0045] Table 2: Changes in the components of other raw materials involved in the reaction
[0046] In this comparative example, the emulsifier is still a mixture of 50 wt % of Span and 50 wt % of Tween 80.
[0047] The tackifier is still polyacrylate mixed with CMC in a mass ratio of 1:1.
[0048] The selected higher alcohol is an aliphatic alcohol having 16 carbon atoms.
[0049] Comparative Example 3 Choose a common defoaming agent available on the market, whose main components are emulsifier, carrier, emulsifying aid and active ingredient.
[0050] Experimental Example 1 Sodium lauryl sulfate, Tween 80 and lecithin were mixed in a ratio of 1:1:1, and then prepared into a 1% aqueous solution as a foaming solution; an air pump was used to ventilate 100 mL of the foaming solution in a 500 mL measuring cylinder in a constant temperature water bath at 50°C, with an air flow rate of 1000 mL / min. When the foam volume reached 500 mL, aeration was stopped, and 0.1 g of defoaming agent was added for defoaming. The time from the addition of the agent to the disappearance of the foam was recorded, which was the defoaming time. Continue to blow air, and record the time when the foam reaches 500 mL again. At the same time, the defoaming agent was used at different temperatures, and the highest temperature that could be tolerated was recorded.
[0051] The experimental results are shown in Table 3, Table 4 and Table 5.
[0052] Table 3: Defoaming time, foam suppression time and high temperature resistance performance test results of the examples
[0053] Table 4: Defoaming time, foam suppression time and high temperature resistance test results of Comparative Example 1
[0054] Table 5: Defoaming time, foam suppression time and high temperature resistance test results of Comparative Examples 2 and 3
[0055] Based on the above data, we can draw the following conclusions: Comparing the experimental data of Example 5 with Scheme 1 to Scheme 10 of Comparative Example 1, it can be seen that when the components of the reactants mainly involved in the reaction change, the performance of the defoamer will be affected. When polyethylene glycol, polypropylene glycol, oxalic acid and stearic acid can form a polyetherester defoamer through an esterification reaction, polyethylene glycol in the present invention not only participates in the reaction, but also plays a role in dissolving other organic matter; when the content of polyethylene glycol is too low, it is easy to make other organic matter insoluble, thereby making the reaction incomplete; and when its content is too high, in addition to easily causing unnecessary waste, it is also easy to produce side reactions that are difficult to separate during the reaction, thereby affecting the performance of the defoamer.
[0056] The contents of polypropylene glycol, oxalic acid and stearic acid are relative. When the content of one component is too high, it will inevitably lead to a decrease in the content of another component. Oxalic acid and stearic acid are both acidic substances. When they are excessive, they will affect the occurrence of esterification reaction. Excessive polypropylene glycol is prone to other organic reactions, and the above situations will make the performance of the defoaming agent unstable. It can also be seen from the experimental results that the defoaming time and anti-foaming time are unstable, and changes in different components will lead to large differences in the experimental results.
[0057] Comparing the experimental data of Example 5 with the schemes 1 to 10 of Examples 6 to 9 and Comparative Example 2, it can be seen that changes in other adjuvants will also affect the performance of the defoamer. Since the present invention is to condense a polyether ester defoamer and a polysiloxane defoamer to finally obtain a defoamer having the properties of both, the selection of adjuvants is also very important. When the content of various adjuvants is low, it is difficult to play its own role, and when the content is high, it will also have a negative impact. Taking emulsifiers as an example, when the content of emulsifiers is high, the defoamer will produce too much foam and too much viscosity during the preparation process, resulting in the performance of the defoamer being not stable enough; when the content of tackifiers is high, it will affect the stability of the defoamer; when the higher alcohol is excessive or the number of carbon atoms therein is too much, it will cause the reaction system to solidify, thereby reducing the defoaming performance of the defoamer; and excessive super white carbon black will affect the quality of the defoamer and also cause unnecessary waste.
[0058] The specific formula of the emulsifier and the thickener is also limited in the present invention, the purpose of which is to better adapt to the reaction system of the present invention, to better exert their effectiveness while also saving materials, and to avoid other adverse effects that may occur during the reaction process.
[0059] At the same time, the present invention also optimizes the reaction conditions and reaction methods, and achieves a smooth reaction by heating in stages, and controls the reaction temperature and stirring rate to prevent the reaction from being too violent and having adverse effects on the equipment; and the reaction is carried out more fully by heat preservation. The staged feeding can also prevent cross-reactions between different components and the production of unwanted substances. It can be seen that when the reaction temperature is too high, the stirring rate is too fast, or the heat preservation time is too long, it will have an adverse effect on the reaction system, thereby affecting the quality of the prepared defoamer.
[0060] Finally, by comparing the defoamer of the present invention with the commercial defoamer, it can be seen that the defoaming time of the defoamer prepared by the present invention is 1 / 3-1 / 2 of the same amount of commercial high-temperature defoamer, and the foam suppression time is 2-3 times that of the commercial high-temperature defoamer. The experiment shows that the high-temperature resistant defoamer prepared by the present invention has excellent defoaming and foam suppression performance, and has obvious technical progress.
[0061] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A high temperature resistant defoaming agent, characterized in that: The invention is mainly composed of the following raw materials in parts by mass: 7-11 parts of polyethylene glycol, 5-9 parts of polypropylene glycol, 5-9 parts of oxalic acid, 9-15 parts of stearic acid, 0.3-1.5 parts of p-toluenesulfonic acid, 4-11 parts of sodium hydroxide, 4-8 parts of polysiloxane grease, 4-7 parts of emulsifier, 2-6 parts of higher alcohol, 1-5 parts of ultrafine white carbon black, 0.05-0.5 parts of tackifier and 9-22 parts of deionized water.
2. The high temperature resistant defoamer according to claim 1, characterized in that The invention is mainly composed of the following raw materials: 8-10 parts of polyethylene glycol, 6-8 parts of polypropylene glycol, 6-8 parts of oxalic acid, 10-14 parts of stearic acid, 0.5-1 parts of p-toluenesulfonic acid, 5-10 parts of sodium hydroxide, 5-7 parts of polysiloxane grease, 3-6 parts of emulsifier, 3-5 parts of higher alcohol, 2-4 parts of ultrafine white carbon black, 0.1-0.3 parts of tackifier and 10-20 parts of deionized water.
3. The high temperature resistant defoamer according to claim 1, characterized in that It is mainly composed of the following raw materials: 9 parts of polyethylene glycol, 7 parts of polypropylene glycol, 7 parts of oxalic acid, 12 parts of stearic acid, 0.8 parts of p-toluenesulfonic acid, 7 parts of sodium hydroxide, 6 parts of polysiloxane grease, 4 parts of emulsifier, 4 parts of higher alcohol, 3 parts of ultrafine white carbon black, 0.2 parts of tackifier and 15 parts of deionized water.
4. The high temperature resistant defoaming agent according to claim 1, characterized in that The emulsifier is a mixture of 50 wt% Span and 50 wt% Tween 80; Preferably, the tackifier is a mixture of polyacrylate and CMC in a mass ratio of 1:
1.
5. The high temperature resistant defoaming agent according to claim 1, characterized in that: The weight average molecular weight of the polypropylene glycol is 600-1000; Preferably, the weight average molecular weight of the polypropylene glycol is 300-600; Preferably, the weight average molecular weight of the polypropylene glycol is 300.
6. The high temperature resistant defoaming agent according to claim 1, characterized in that: The higher alcohol is a fatty alcohol having a carbon number in the range of 16-28; Preferably, the higher alcohol is a fatty alcohol having 16 carbon atoms.
7. A method for preparing a high temperature resistant defoaming agent according to any one of claims 1 to 6, characterized in that: The steps include: Stirring polyethylene glycol, polypropylene glycol, oxalic acid and stearic acid, and adding p-toluenesulfonic acid during the stirring process to mix well, to obtain a mixed solution A; Inert gas is introduced into the mixed solution A, and the mixture is heated and cooled in stages, and sodium hydroxide is added to adjust the pH to 6.5-7.5 to obtain a mixed solution B; The polysiloxane silicone grease and the emulsifier are mixed and heated, and then the higher alcohol and ultrafine white carbon black are added, heated and stirred, and then cooled to obtain a mixed solution C; Stir deionized water and thickener evenly to obtain a mixed solution D; The mixed solution B, the mixed solution C and the mixed solution D are stirred and heated in sequence, and then cooled to obtain the mixture.
8. The method for preparing a high temperature resistant defoaming agent according to claim 7, characterized in that: The specific steps of the segmented heating are: The mixed solution A is heated to 140°C-160°C and kept warm for 8h-10h; Then heat to 200°C and keep warm for 1h-2h.
9. The method for preparing a high temperature resistant defoaming agent according to claim 7, characterized in that: In the step of mixing and heating the polysiloxane silicone grease and the emulsifier, the heating temperature is 40°C-60°C and the insulation time is 0.5h-1h; In the step of adding higher alcohol and ultrafine white carbon black and heating and stirring, the heating temperature is 80° C.-90° C., the heat preservation time is 1 h-2 h, and the stirring rate is 150 r / min-200 r / min.
10. The method for preparing a high temperature resistant defoaming agent according to claim 7, characterized in that: The specific steps of stirring and heating the mixed solution B, the mixed solution C and the mixed solution D in sequence are: The heating temperature is controlled at 60℃-80℃, and each mixed liquid is stirred for 0.5h-1h at a stirring speed of 120r / min-180r / min, and the temperature is lowered to 15℃-30℃.
Citation Information
Patent Citations
Polyether defoaming agent and preparation method thereof
CN112774260A
Defoaming agent special for coal chemical desulfurization system and preparation method thereof
CN115193104A