Blanking method for U-shaped metal part
Through the three-folding method and mold design optimization, the problem that the proportion of bright belts in the U-shaped metal parts slicing cutting edge is difficult to meet customer needs, and a higher proportion of bright belts and product performance improvement is achieved.
Patent Information
- Application Number
- CN202411383091.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-11-29
AI Technical Summary
The proportion of slitting blades of existing U-shaped metal parts is difficult to meet customer needs and is unstable.
Three-brushing method is adopted, combining specific slitting margin and mold design, including the design of the module and the lower module on the punching equipment, and the slitting mould and concave mold made of SKH-51 cold work mold steel , and the surface treatment of nitrogen-titanium carbide was coated by physical meteorological deposition method, and the knife and extrusion angle were arranged to improve the stability of the slitting mould.
By increasing the number of punching times and adjusting the slitting margin, optimizing the proportion of the blade edge bright band, improving product performance, and improving punching stability by improving mold material and design.
Smart Images

Figure CN119035376A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal processing, in particular to a U-shaped metal part punching method. Background Art
[0002] The cutting edges of some high-precision parts on the market need to be used in conjunction with other parts. The larger the contact area between them, the better the performance of the end product. Increasing the proportion of the bright band of the cutting edge on the cut surface is a way to increase the contact area.
[0003] When forming the blade of existing U-shaped metal parts, they are generally formed by direct one-time punching, and a small number of them are formed by two-time punching. The proportion of the blade bright band formed by this process is difficult to meet customer needs and is extremely unstable. Summary of the invention
[0004] The present invention provides a U-shaped metal part punching method to solve the problem in the related art that the proportion of the bright band of the slitting blade of the U-shaped metal part is difficult to meet customer requirements and is extremely unstable.
[0005] The present invention provides a U-shaped metal part punching method, comprising the following steps: S1, performing a first punching of a metal strip that is intermittently fed, wherein the punching positions are positions opposite to each other on both sides of the metal strip;
[0006] S2, performing a second punching of the metal strip;
[0007] S3, performing a third punching of the metal strip;
[0008] S4, performing notch cutting on the metal strip after three punchings by the knife edge, wherein the first cutting is to cut the area between two adjacent punching positions on the metal strip to form a notch, and at this time the metal strip is not completely cut;
[0009] S5, bending the metal strip into a U-shape, the bending times being two times;
[0010] S6, cutting the continuous U-shaped metal strip into separate U-shaped metal pieces in sequence, cutting the continuous portion between two opposite notches of the metal strip, and cutting the U-shaped metal strip into U-shaped metal pieces one by one;
[0011] Among them, steps S1-S3 are completed by using a punching equipment, which includes an upper die group and a lower die group, and the upper die group includes an upper die base, an upper pad, a fixed plate, a height limiting plate, a stripping plate and a slitting punch. The lower surface of the upper die base is fixed with an upper pad, the lower surface of the upper pad is fixed with a fixed plate, the lower surface of the fixed plate is fixed with a slitting punch through a fixed plate insert, the lower surface of the fixed plate is connected to the stripping plate through a height limiting plate, a stripping plate insert is fixed on the stripping plate, and the lower end of the slitting punch slides through the height limiting plate and the stripping plate insert on the stripping plate.
[0012] In one possible implementation, the cutting allowances of the three knife-edge punching are different. The cutting allowance A of the first punching is 15% of the thickness of the metal strip, the cutting allowance B of the second punching is 8% of the thickness of the metal strip, and the cutting allowance of the third punching is 0, that is, the third punching cuts the metal strip into the required size.
[0013] In one possible implementation, a supporting knife is provided at the bottom of the slitting punch, one end of the supporting knife is flush with the slitting punch, and an extrusion bevel is provided at the end of the bottom of the slitting punch away from the supporting knife. The extrusion bevel is extended 0.3 mm in the vertical direction of the slitting punch and deflected 65°. The supporting knife strengthens the slitting punch and improves the stability of the slitting punch during punching.
[0014] In one possible implementation, the lower die assembly includes a lower die base, a lower pad, a concave mold plate and a slitting die. The lower die base is fixedly mounted with the lower pad, the upper surface of the lower pad is fixedly mounted with the concave mold plate, the slitting die is fixed on the concave mold plate and corresponds to the slitting punch.
[0015] In a possible implementation, the slitting punch and the slitting die are both made of cold working die steel, and the material is SKH-51.
[0016] In one possible implementation, the surfaces of the slitting punch and the slitting die are treated with a surface coating using a physical vapor deposition method to coat titanium nitride carbide. The single-sided thickness of the coating is 0.002-0.003 mm, and the roughness after coating is ≤ Ra0.2. The coating must not have pits, scratches, peeling, bubbles, or wrinkles.
[0017] The above one or more technical schemes in the embodiments of the present invention have at least one of the following technical effects: under the same slitting allowance, the proportion of the bright band at the blade edge is increased by increasing the number of punching times at the blade edge of the metal strip; under three punching times, the proportion of the bright band at the blade edge is optimized by adjusting the slitting allowance each time, and in addition, the proportion of the bright band at the blade edge when the slitting punch slitting the metal strip is increased by changing the materials of the slitting punch and the slitting die, and the stability of the slitting punch during punching is increased by arranging a knife at the bottom of the slitting punch, and the above methods are combined to increase the proportion of the bright band at the blade edge of the metal strip, thereby improving the performance of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a process flow chart of the present invention.
[0019] Figure 2 It is a schematic diagram of the cutting allowance when the punching equipment punches the metal strip.
[0020] Figure 3 yes Figure 2 Schematic diagram of the enlarged M region.
[0021] Figure 4 It is a schematic diagram of the three-time punching and cutting allowance ratio.
[0022] Figure 5 It is a structural diagram of the punching equipment.
[0023] Figure 6 It is a schematic diagram of the structure of the optimized slitting punch.
[0024] In the figure: 1. upper die seat; 2. upper pad; 3. fixed plate; 31. fixed plate insert; 4. height limit plate; 5. unloading plate; 51. unloading plate insert; 6. slitting punch; 61. backing knife; 7. lower die seat; 8. lower pad; 9. concave die plate; 10. slitting concave die; 11. metal strip. DETAILED DESCRIPTION
[0025] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described below, and those skilled in the art can make similar improvements without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.
[0026] See also Figure 1 , a U-shaped metal part punching method, comprising the following steps:
[0027] S1, performing the first punching of the metal strip 11 with a knife edge. Specifically, a suitable metal sheet is selected, and the metal sheet is cut into the metal strip 11. Then, the metal strip 11 is placed on the concave mold plate 9, and the metal strip 11 is intermittently moved from the avoidance notch below the unloading plate 5 to the first punching position. When the metal strip 11 stops moving, the first punching is performed on the edges of both sides of the metal strip 11 using the slitting punch 6;
[0028] S2, performing a second punching of the metal strip 11. Specifically, after the first punching of the metal strip 11 is completed, it continues to move in the direction of the next punching. When the metal strip 11 stops moving again, the slitting punch 6 performs a second punching of the first punching position on the two side edges of the metal strip 11.
[0029] S3, the metal strip 11 is punched for the third time, and the third punching is performed similarly. The three slitting punches 6 used in the three punchings have different slitting allowances for punching the metal strip 11. The slitting allowance A of the first punching is 15% of the thickness of the metal strip 11, and the slitting allowance B of the second punching is 8% of the thickness of the metal strip 11. The third punching cuts the metal strip 11 into the required size. After the three punchings, the bright band at the edge of the metal strip 11 increases compared with the two punchings.
[0030] S4, performing notch cutting on the metal strip 11 after three punchings by the knife edge. Specifically, when the metal strip 11 continues to move to the next stop, the area between two adjacent punching positions is cut, so that a notch is formed between the two adjacent punching positions of the metal strip 11, so as to facilitate the subsequent bending of the metal strip 11;
[0031] S5, bending the metal strip 11 to make it U-shaped. Specifically, when the metal strip 11 continues to move to the next stop, the metal strip 11 is bent at the punching position. The bending is performed twice to ensure that the U-shaped metal strip 11 will not be reset after being bent.
[0032] S6. Cut the continuous U-shaped metal strip 11 into separate U-shaped metal pieces in sequence. Specifically, when the bent U-shaped metal strip 11 continues to move until the next stop, the continuous portion between two opposite notches of the U-shaped metal strip 11 is cut to form separate U-shaped metal pieces.
[0033] Steps S1-S3 are completed by using a punching device, such as Figure 2 and Figure 5As shown, the punching equipment includes an upper die group and a lower die group, and the upper die group includes an upper die base 1, an upper pad 2, a fixed plate 3, a height limiting plate 4, a stripping plate 5 and a slitting punch 6. The upper pad 2 is fixed to the lower surface of the upper die base 1, the fixed plate 3 is fixed to the lower surface of the upper pad 2, the slitting punch 6 is fixed to the lower surface of the fixed plate 3 through a fixed plate insert 31, the lower surface of the fixed plate 3 is connected to the stripping plate 5 through the height limiting plate 4, the stripping plate insert 51 is fixed to the stripping plate 5, and the lower end of the slitting punch 6 slides through the height limiting plate 4 and the stripping plate insert 51 on the stripping plate 5.
[0034] like Figure 5 As shown, the lower die assembly includes a lower die base 7, a lower pad 8, a concave mold plate 9 and a slitting die 10. The lower die base 7 is fixedly mounted with the lower pad 8 on its upper surface, the lower pad 8 is fixedly mounted with the concave mold plate 9 on its upper surface, the slitting die 10 is fixed on the concave mold plate 9 and corresponds to the slitting punch 6. When the upper die assembly and the lower die assembly are closed, the slitting punch 6 is plugged into the slitting die 10, and the height limiting plate 4 can ensure that the upper die assembly and the lower die assembly will not be over-extruded when they are closed.
[0035] It should be noted that, when the number of punching is determined three times, the control variable method is used to determine the cutting allowance for each punching, such as Figure 3 and Figure 4 As shown, Figure 3 The overlapping portion of the metal strip 11 and the slitting punch 6 is the slitting allowance. The slitting allowances of the three knife-edge punchings are different. The slitting allowance A of the first punching is 15% of the thickness of the metal strip 11, the slitting allowance B of the second punching is 8% of the thickness of the metal strip 11, and the slitting allowance of the third punching is 0, that is, the third punching cuts the metal strip 11 to the required size.
[0036] In addition, in order to increase the stability of the slitting punch 6 when the metal strip 11 is punched by a knife, a support knife 61 is provided at the bottom of the slitting punch 6, one end of the support knife 61 is flush with the slitting punch 6, and an extrusion bevel is provided at the end of the bottom of the slitting punch 6 away from the support knife 61, and the extrusion bevel is extended by 0.3 mm in the vertical direction of the slitting punch 6 and deflected by 65°.
[0037] It should be noted that in order to enhance the strength of the slitting punch 6 and the slitting die 10, the slitting punch 6 and the slitting die 10 are made of cold working die steel of SKH-51, and the outer surfaces of the slitting punch 6 and the slitting die 10 are coated. The surface coating treatment method and parameter requirements are as follows: Use the physical vapor deposition (PVD) method to apply the coating titanium nitride carbide (Ti CN)-gray black, and the single-sided thickness of the coating is 0.002-0.003mm; the roughness after coating is ≤Ra0.2; the coating must not have defects such as pits, scratches, peeling, bubbles, and wrinkles.
[0038] In the embodiments of the present invention, unless otherwise clearly specified and limited, the first feature being "above" or "below" the second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, the first feature being "above", "above" and "above" the second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. The first feature being "below", "below" and "below" the second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0039] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "connect", "install", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, an integral connection, or a sliding connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0040] The embodiments of this specific implementation method are all preferred embodiments of the present invention, and are not intended to limit the protection scope of the present invention. Therefore, all equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A U-shaped metal part punching method, characterized in that: The following steps are involved: S1, performing a first punching of the metal strip (11); S2, performing a second punching of the metal strip (11); S3, performing a third punching of the metal strip (11); S4, cutting the metal strip (11) after the three-time punching by the knife edge; S5, bending the metal strip (11) to form a U-shape; S6, cutting the continuous U-shaped metal strip (11) into individual U-shaped metal pieces in sequence; Steps S1-S3 are completed by using a punching device, the punching device comprising an upper die group and a lower die group, the upper die group comprising an upper die base (1), an upper pad (2), a fixed plate (3), a height limiting plate (4), a stripping plate (5) and a slitting punch (6), the lower surface of the upper die base (1) is fixed with an upper pad (2), the lower surface of the upper pad (2) is fixed with a fixed plate (3), the lower surface of the fixed plate (3) is fixed with a slitting punch (6) via a fixed plate insert (31), the lower surface of the fixed plate (3) is connected to the stripping plate (5) via a height limiting plate (4), a stripping plate insert (51) is fixed on the stripping plate (5), and the lower end of the slitting punch (6) slides through the height limiting plate (4) and the stripping plate insert (51) on the stripping plate (5).
2. A U-shaped metal part punching method according to claim 1, characterized in that: The cutting allowances of the three times of punching are different. The first time the cutting allowance A is 15% of the thickness of the metal strip (11), the second time the cutting allowance B is 8% of the thickness of the metal strip (11), and the third time the cutting allowance is 0.
3. A U-shaped metal part punching method according to claim 1, characterized in that: A support knife (61) is arranged at the bottom of the slitting punch (6), one end of the support knife (61) is flush with the slitting punch (6), and an extrusion bevel is arranged at the end of the bottom of the slitting punch (6) away from the support knife (61), wherein the extrusion bevel is extended by 0.3 mm in the vertical direction of the slitting punch (6) and then deflected by 65°.
4. A U-shaped metal part punching method according to claim 1, characterized in that: The lower die assembly comprises a lower die base (7), a lower pad (8), a concave die plate (9) and a slitting die (10); the lower pad (8) is fixedly mounted on the upper surface of the lower die base (7); the concave die plate (9) is fixedly mounted on the upper surface of the lower pad (8); the slitting die (10) is fixed on the concave die plate (9) and corresponds to the slitting punch (6).
5. A U-shaped metal part punching method according to claim 4, characterized in that: The slitting punch (6) and the slitting die (10) are both made of cold working die steel, and the material is SKH-51.
6. A U-shaped metal part punching method according to claim 4, characterized in that: The surfaces of the slitting convex die (6) and the slitting concave die (10) are subjected to surface coating treatment by using a physical vapor deposition method to coat titanium nitride carbide. The single-side thickness of the coating is 0.002-0.003 mm. The roughness after coating is ≤Ra0.
2. The coating must not have pits, scratches, peeling, bubbles or wrinkles.
Citation Information
Patent Citations
Stamping forming method for improving bright band of thick-material product
CN107597947A
Thin material stamping die with limiting structure
CN111515294A
Thin material sharp corner blanking structure and process
CN118106415A
Metal plate punching process
CN1672830A
Thin material closed angle blanking mould
CN205463836U