Steel rail medium-frequency induction welding heat treatment equipment based on carbon dioxide protection and working method of steel rail medium-frequency induction welding heat treatment equipment
Through the medium frequency induction welding heat treatment equipment for rail welding based on carbon dioxide protection, the problems of gray spot defects, long process cycles and poor joint quality of rail welding in the prior art are solved, efficient and automated welding and heat treatment are achieved, and joint performance is improved and appearance quality.
Patent Information
- Application Number
- CN202411422099.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-12
- Publication Date
- 2024-11-29
AI Technical Summary
The existing railway rail welding technology has problems such as difficult to eliminate gray spot defects, long process debugging cycle, environmental pollution, use of flammable gases, large influence on the gas source factors, difficulty in accurately measuring the flame heating temperature, and lack of automation.
Using medium-frequency induction welding heat treatment equipment for rails based on carbon dioxide protection, including induction heating mechanism, rail clamping mechanism, lifting mechanism, electronic control system, intermediate frequency power supply, hydraulic pump station, chiller unit, carbon dioxide gas supply system and air cooling system, through carbon dioxide The atmosphere protective cover prevents weld oxidation, uses an intermediate frequency power supply to provide heating power, and the air-cooled system quickly cools down, achieving efficient welding and heat treatment.
It improves welding quality and efficiency, avoids weld oxidation defects, reduces internal welding defects, improves joint performance and appearance quality, and realizes automation of the welding process and precise temperature control.
Smart Images

Figure CN119035831A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of railway rail welding and heat treatment, and in particular relates to a rail medium frequency induction welding heat treatment device based on carbon dioxide protection and a working method thereof. Background Art
[0002] The three main technologies used for welding rails on my country's seamless railway lines are flash welding, gas pressure welding and thermite welding.
[0003] Flash welding is a process in which electricity is passed through both ends of the rails to generate resistance heat and then pressure is applied to forge the welded joint. It is currently the most widely used rail welding technology, but it also has problems such as gray spot defects that are difficult to eliminate, long process debugging cycle, and easy environmental pollution.
[0004] Gas pressure welding is a welding method that uses gas flame heating to heat the joint and then pressurizes it for upsetting. The main disadvantage is that it requires a large amount of flammable and explosive gas, the quality of the joint is greatly affected by the gas source factors, and it is easy to have defects that are difficult to detect. In addition, the flame heating temperature cannot be accurately measured, making it difficult to achieve full automation and placing high requirements on the operators.
[0005] Thermite welding is a welding method that uses thermite flux to produce an oxidation-reduction reaction, releasing heat to generate liquid metal to fill the weld gap. Its essence is a metal casting process, and the joint quality and performance are not as good as the above two welding methods.
[0006] The basic principle of medium frequency induction heating is to place a metal workpiece in a copper coil and apply an oscillating current of a certain frequency in the coil to form an alternating magnetic field, thereby generating induced eddy currents inside the metal for heating. In the field of rail welding, medium frequency induction technology has been widely used in joint post-weld heat treatment operations, but has not yet been directly used for rail welding. The medium frequency induction heat treatment welding and working method for rails based on carbon dioxide protection proposed in the present invention can make up for the shortcomings of the existing technology and effectively improve welding quality and efficiency. Summary of the invention
[0007] In order to overcome the above-mentioned defects of the prior art, the present invention proposes a rail medium frequency induction welding heat treatment equipment based on carbon dioxide protection and a working method thereof.
[0008] A medium-frequency induction welding heat treatment equipment for rails based on carbon dioxide protection and a working method thereof, the medium-frequency induction welding heat treatment equipment for rails comprises a rail clamping mechanism, an induction heating mechanism, a lifting mechanism, an electric control system, a medium-frequency power supply, a hydraulic pump station, a chiller, a carbon dioxide gas supply system and an air cooling system, wherein the induction heating mechanism is installed in the middle of the rail clamping mechanism, and the induction heating mechanism is connected to the central axis of the rail clamping mechanism through the lifting mechanism.
[0009] The induction heating mechanism includes an induction coil, a coil seat, a carbon dioxide atmosphere protection cover, a transformer, a frame, and an opening and closing cylinder. The induction coil consists of two parts, which are welded with a hollow copper tube and processed into a shape similar to the cross-section of a rail. The left and right parts of the induction coil are respectively fixed on the left and right parts of the coil seat and separated by an insulating plate. The carbon dioxide atmosphere protection cover consists of two parts, which are respectively fixed on the left and right parts of the coil seat and wrap the entire induction coil and the rail joint. The left and right parts of the left and right coil seats are respectively hinged to the frame through an opening and closing cylinder. The cylinder can be extended and retracted to realize the opening and closing of the coil seat, thereby realizing the opening and closing of the left and right induction coils. The transformer is fixed on the frame, and the secondary of the transformer is connected to the induction coil through two bus bars to form a single-turn induction loop.
[0010] The lifting mechanism includes a motor, a screw, a screw nut, a guide rail, a slider and a fixed plate, wherein the motor is fixed on the fixed plate, the motor and the screw are connected by a coupling, the screw and the fixed plate are connected by a bearing, the guide rail is fixed on the fixed plate, the screw nut and the slider are fixed on the frame, and the screw is driven to rotate by the rotation of the motor, so that the screw nut drives the induction heating mechanism to realize linear motion in the vertical direction.
[0011] The rail clamping mechanism includes a left clamp, a right clamp, two upsetting shafts, and two guide shafts. The left clamp and the right clamp are connected by two upsetting shafts and two guide shafts, which can ensure the straightness of rail welding and meet the space for installation in the middle of the induction heating mechanism. One end of the upsetting shaft passes through the right clamp to connect the upsetting cylinder, and the other end of the upsetting shaft is fixed on the left clamp. One end of the guide shaft is fixed on the right clamp by a nut, and the other end of the guide shaft passes through the left clamp. The extension and retraction of the upsetting cylinder can drive the left clamp to move linearly along the guide shaft through the upsetting shaft, thereby realizing the upsetting of the rail joint.
[0012] Among them, the rail clamping mechanism also includes a tumor pushing cylinder, a tool holder and a tumor pushing knife. The tumor pushing cylinder is fixed at the end of the left clamp and is connected to the tool holder through the cylinder shaft. The tumor pushing knife is hung on the rail and fits with the tool holder. After the rail top forging is completed, the force of the tumor pushing cylinder pushes the tumor pushing knife through the tool holder to cut off the weld tumor flash squeezed out of the joint.
[0013] The equipment also includes an electronic control system, a medium frequency power supply, a hydraulic pump station, a chiller, a carbon dioxide gas supply system and an air cooling system, wherein the rail clamping mechanism and the induction heating mechanism constitute the head part of the rail induction welding machine, the rail clamping mechanism realizes the functions of rail waist clamping, upsetting and pushing the nodule, and the induction heating mechanism forms a closed magnetic field to provide a heating heat source; the electronic control system controls the actions of various parts of the mechanism by a PLC programmable controller, and monitors various sensors in the system at the same time; the medium frequency power supply provides heating power for the induction coil through IGBT inverter and series resonance; the hydraulic pump station connects the head cylinder to provide kinetic energy for clamping, upsetting and other actions; the chiller provides cooling for the induction coil and other heating components; the carbon dioxide gas supply system provides carbon dioxide atmosphere protection for the welding process; the air cooling system provides a gas source for the heat treatment process, which is used to quickly reduce the joint temperature, achieve under-speed quenching, and improve the surface hardness of the joint.
[0014] Among them, 15 small nozzles are set on each of the two coil seats. The small nozzles are connected to the air pipe joint through the internal aperture, and then connected to the carbon dioxide gas supply system and the air cooling system through the air pipe. During the welding process, the coil seat and the carbon dioxide protective cover form a relatively closed cavity around the rail joint. Carbon dioxide is injected into the cavity through the small nozzle to form an inert gas protection, which can prevent the weld joint surface from being oxidized and forming defects during the heating process. During the heat treatment process, the air pipe is switched to connect to the air cooling system. After heating to temperature, the small nozzle is used to spray air to quickly cool the joint.
[0015] Among them, the carbon dioxide atmosphere protection cover is made of high-temperature resistant materials, including but not limited to graphite plates, mica plates, asbestos cloth, etc.; the carbon dioxide atmosphere protection cover also plays a role of heat preservation and insulation during the heating process, thereby improving the heating efficiency.
[0016] A medium frequency induction welding heat treatment device for rails based on carbon dioxide protection and a working method thereof, the method comprising:
[0017] Step 1: Grind and remove rust from the end face of the rail joint to be welded, and make the butt joint surface smooth by end grinding or end milling;
[0018] Step 2: Use the rail clamping device to clamp the rail to be welded and center it, and use the upsetting cylinder to apply force to make the butt joint surfaces close together;
[0019] Step 3: The induction coil adopts an open-and-close structure and is installed in the middle of the rail clamping device. It is lowered to the butt joint of the rail to be welded, and then the coil is closed by the open-and-close cylinder to form a closed loop around the rail.
[0020] Step 4: Control the valve to open the carbon dioxide gas supply system and inject gas into the carbon dioxide atmosphere protective cover through a small nozzle; it is required to start injecting gas 30 seconds before welding, the purity of carbon dioxide should not be less than 99.5%, and the flow rate should be 5-15L / min;
[0021] Step 5: Start the medium frequency power supply to perform induction heating on the rail joint, and the temperature meter monitors the heating temperature throughout the process;
[0022] Step 6: During the heating process, the upsetting cylinder always applies force, and the carbon dioxide injection flow rate is gradually reduced. When the temperature reaches 800-900℃, the carbon dioxide supply is stopped.
[0023] Step 7: When the set welding temperature (1200℃~1300℃) is reached, the medium frequency power supply is turned off, and the upsetting cylinder accelerates and pressurizes the rail to be welded to close the butt joint and squeeze out the weld nodule, while the induction coil opens and rises;
[0024] Step 8: The rail nodule pushing mechanism removes the weld nodule;
[0025] Step 9: The induction heating mechanism descends and closes again, and the control valve opens the air cooling system. Compressed air is sprayed toward the weld rail head and rail waist through a small nozzle, and the spraying is stopped when the temperature drops below 400℃.
[0026] Step 10: Start the medium frequency power supply again to heat the weld joint to about 900°C and complete the post-weld heat treatment to refine the grain structure and improve the toughness and strength of the joint;
[0027] Step 11: The air cooling system is turned on again, and compressed air is used to perform under-speed quenching treatment on the joint surface to increase the joint surface hardness;
[0028] Step 12: Finally, open the induction coil, release the rail by the rail clamping device, and then perform post-weld tumor removal, grinding and other treatments.
[0029] The present invention adopts carbon dioxide atmosphere protection, which can effectively avoid oxidation of the weld joint surface during the induction heating process, which is beneficial to improving the joint performance and reducing the internal defects of the welding. The atmosphere protection cover is made of high temperature resistant material, which can play a role in heat insulation during the heating process, and improve the heating and welding efficiency. The rail clamp mechanism is connected by four axes, which can not only ensure the straightness of the rail welding, but also meet the space for installation in the middle of the induction heating mechanism, which is helpful to improve the appearance quality of the joint. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is an overall schematic diagram of a rail medium-frequency induction welding heat treatment equipment based on carbon dioxide protection.
[0031] Figure 2 This is a schematic diagram of the structure of the medium frequency induction welding heat treatment equipment for rails.
[0032] Figure 3 It is a schematic diagram of the induction heating mechanism structure.
[0033] Figure 4 This is a schematic diagram of the induction heating mechanism coil opening structure.
[0034] Figure 5 It is a schematic diagram of the structure of the rail clamping mechanism.
[0035] Figure 6 Schematic diagram of the internal structure of carbon dioxide injection and air jet.
[0036] Figure 7 Schematic diagram of the distribution of small nozzles on the coil seat. DETAILED DESCRIPTION
[0037] The heat treatment of a rail medium frequency induction welding heat treatment equipment based on carbon dioxide protection and its working method provided by the present invention are described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0038] Attached Figure 1-7 As shown, a medium-frequency induction welding heat treatment equipment for rails based on carbon dioxide protection and a working method thereof, the medium-frequency induction welding heat treatment equipment for rails comprises a rail clamping mechanism 1, an induction heating mechanism 2, a lifting mechanism 5, an electric control system, a medium-frequency power supply, a hydraulic pump station, a chiller, a carbon dioxide gas supply system and an air cooling system, wherein the induction heating mechanism 2 is installed in the middle part 1 of the rail clamping mechanism, and the induction heating mechanism 2 is connected to the central axis of the rail clamping mechanism 1 through the lifting mechanism 5.
[0039] The induction heating mechanism 2 includes an induction coil 6, a coil seat 7, a carbon dioxide atmosphere protection cover 8, a transformer 9, a frame 10, and an opening and closing cylinder 11. The induction coil 6 consists of two left and right parts, which are welded with a hollow copper tube and processed into a shape similar to the cross-section of the rail; wherein the left and right parts of the induction coil 6 are respectively fixed on the left and right parts of the coil seat 7 and separated by an insulating plate 14, the carbon dioxide atmosphere protection cover 8 consists of two parts, which are respectively fixed on the left and right parts of the coil seat 7, and wrap the entire induction coil 6 and the rail joint, and the left and right parts of the left and right coil seats 7 are respectively hinged to the frame 10 through the opening and closing cylinder 11, and the cylinder can be extended and retracted to realize the opening and closing of the coil seat, thereby realizing the opening and closing of the left and right induction coils; the transformer 9 is fixed on the frame 10, and the secondary of the transformer 9 is connected to the induction coil through two bus bars 13 to form a single-turn induction loop.
[0040] The lifting mechanism 5 includes a motor 15, a screw 16, a screw nut 17, a guide rail 18, a slider 19 and a fixed plate 20, wherein the motor 15 is fixed on the fixed plate 20, the motor 15 and the screw 16 are connected by a coupling, the screw 16 and the fixed plate 20 are connected by a bearing, the guide rail 18 is fixed on the fixed plate 20, the screw nut 17 and the slider 19 are fixed on the frame 10, and the screw 16 is driven to rotate by the rotation of the motor 15, so that the screw nut 17 drives the induction heating mechanism 2 to realize linear motion in the vertical direction.
[0041] The rail clamping mechanism 1 includes a left clamp 21, a right clamp 22, two upsetting shafts 23, and two guide shafts 24, wherein the left clamp 21 and the right clamp 22 are connected by two upsetting shafts 23 and two guide shafts 24, which can ensure the straightness of rail welding and meet the space for installation in the middle of the induction heating mechanism; one end of the upsetting shaft 23 passes through the right clamp 22 to connect the upsetting cylinder 25, and the other end of the upsetting shaft 23 is fixed on the left clamp 21; one end of the guide shaft 24 is fixed on the right clamp 22 by a nut 26, and the other end of the guide shaft 24 passes through the left clamp 21. The extension and retraction of the upsetting cylinder can drive the left clamp to move linearly along the guide shaft through the upsetting shaft, thereby realizing the upsetting of the rail joint.
[0042] The rail clamping mechanism clamps the ends of the first rail 3 and the second rail 4, and brings the butt joint surfaces together directly below the induction heating mechanism 2; the induction heating mechanism 2 opens and descends to heat the butt joint surfaces of the rails.
[0043] The rail clamping mechanism 1 also includes a tumor pushing cylinder 27, a tool holder 28 and a tumor pushing knife 29. The tumor pushing cylinder 27 is fixed to the end of the left clamp 21 and is connected to the tool holder 28 through a cylinder shaft. The tumor pushing knife 29 is hung on the rail and fits with the tool holder 28. After the rail top forging is completed, the force of the tumor pushing cylinder 27 pushes the tumor pushing knife 29 through the tool holder 28 to cut off the weld tumor flash squeezed out of the joint.
[0044] The equipment also includes an electric control system, a medium frequency power supply, a hydraulic pump station, a chiller, a carbon dioxide gas supply system and an air cooling system, wherein the rail clamping mechanism 1 and the induction heating mechanism 2 constitute the head part of the rail induction welding machine, the rail clamping mechanism 1 realizes the functions of rail waist clamping, upsetting and pushing the nodule, and the induction heating mechanism 2 forms a closed magnetic field to provide a heating heat source; the electric control system controls the actions of various parts of the mechanism by a PLC programmable controller, and monitors various sensors in the system at the same time; the medium frequency power supply provides heating power for the induction coil through IGBT inversion and series resonance; the hydraulic pump station is connected to the head cylinder to provide kinetic energy for actions such as clamping and upsetting; the chiller provides cooling for the induction coil and other heating components; the carbon dioxide gas supply system provides carbon dioxide atmosphere protection for the welding process; the air cooling system provides a gas source for the heat treatment process, which is used to quickly reduce the joint temperature, realize under-speed quenching, and improve the surface hardness of the joint.
[0045] The two coil seats 7 are each provided with 15 small nozzles 30, which are connected to the air pipe joint 31 through the internal aperture, and then connected to the carbon dioxide gas supply system and the air cooling system through the air pipe 32; the coil seat 7 and the carbon dioxide protective cover (8) form a relatively closed cavity 33 around the rail joint, and carbon dioxide is injected into the cavity through the small nozzles 30 to form an inert gas protection, which can prevent the weld joint surface from being oxidized and forming defects during the heating process. During the heat treatment process, the air pipe is switched to be connected to the air cooling system, and after heating to the temperature, the small nozzle is used to spray air to quickly cool the joint.
[0046] The carbon dioxide atmosphere protection cover is made of high temperature resistant materials, including but not limited to graphite plates, mica plates, asbestos cloth, etc. The carbon dioxide atmosphere protection cover also plays a role of heat preservation and insulation during the heating process, thereby improving the heating efficiency.
[0047] A medium frequency induction welding heat treatment device for rails based on carbon dioxide protection and a working method thereof, the method comprising:
[0048] Step 1: Grind and remove rust from the end face of the rail joint to be welded, and make the butt joint surface smooth by end grinding or end milling;
[0049] Step 2: Use the rail clamping device to clamp the rail to be welded and center it, and use the upsetting cylinder to apply force to make the butt joint surfaces close together;
[0050] Step 3: The induction coil adopts an open-and-close structure and is installed in the middle of the rail clamping device. It is lowered to the butt joint of the rail to be welded, and then the coil is closed by the open-and-close cylinder to form a closed loop around the rail.
[0051] Step 4: Control the valve to open the carbon dioxide gas supply system and inject gas into the carbon dioxide atmosphere protective cover through a small nozzle; it is required to start injecting gas 30 seconds before welding, the purity of carbon dioxide should not be less than 99.5%, and the flow rate should be 5-15L / min;
[0052] Step 5: Start the medium frequency power supply to perform induction heating on the rail joint, and the temperature meter monitors the heating temperature throughout the process;
[0053] Step 6: During the heating process, the upsetting cylinder always applies force, and the carbon dioxide injection flow rate is gradually reduced. When the temperature reaches 800-900℃, the carbon dioxide supply is stopped.
[0054] Step 7: When the set welding temperature (1200℃~1300℃) is reached, the medium frequency power supply is turned off, and the upsetting cylinder accelerates and pressurizes the rail to be welded to close the butt joint and squeeze out the weld nodule, while the induction coil opens and rises;
[0055] Step 8: The rail nodule pushing mechanism removes the weld nodule;
[0056] Step 9: The induction heating mechanism descends and closes again, the control valve opens the air cooling system, and compressed air is sprayed toward the weld rail head and rail waist through a small nozzle, and the temperature drops to 400
[0057] Stop spraying air after the temperature drops below ℃.
[0058] Step 10: Start the medium frequency power supply again to heat the weld joint to about 900°C and complete the post-weld heat treatment to refine the grain structure and improve the toughness and strength of the joint;
[0059] Step 11: The air cooling system is turned on again, and compressed air is used to perform under-speed quenching treatment on the joint surface to increase the joint surface hardness;
[0060] Step 12: Finally, open the induction coil, release the rail by the rail clamping device, and then perform post-weld tumor removal, grinding and other treatments.
[0061] Finally, it should be noted that the above embodiments are only used to describe the technical solution of the present invention rather than to limit the technical method. The present invention can be extended to other modifications, changes, applications and embodiments in application, and therefore it is believed that all such modifications, changes, applications and embodiments are within the spirit and teaching scope of the present invention.
Claims
1. A medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection and a working method thereof, characterized in that: The rail medium frequency induction welding heat treatment equipment comprises a rail clamping mechanism (1), an induction heating mechanism (2), a lifting mechanism (5), an electric control system, a medium frequency power supply, a hydraulic pump station, a chiller, a carbon dioxide gas supply system and an air cooling system, wherein the induction heating mechanism (2) is installed in the middle part (1) of the rail clamping mechanism, and the induction heating mechanism (2) is connected to the central axis of the rail clamping mechanism (1) through the lifting mechanism (5).
2. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 1 is characterized in that: The induction heating mechanism (2) comprises an induction coil (6), a coil seat (7), a carbon dioxide atmosphere protection cover (8), a transformer (9), a frame (10), and an opening and closing oil cylinder (11). The induction coil (6) consists of two left and right parts, which are welded with a hollow copper tube and processed into a shape similar to the cross section of a rail. The left and right parts of the induction coil (6) are respectively fixed on the left and right parts of the coil seat (7) and separated by an insulating plate (14). The carbon dioxide atmosphere protection cover (8) consists of two parts, which are respectively fixed on the left and right parts of the coil seat (7) and wrap the entire induction coil (6) and the rail joint. The left and right parts of the left and right coil seats (7) are respectively hinged to the frame (10) through an opening and closing oil cylinder (11). The cylinder can be extended and retracted to realize the opening and closing of the coil seat, thereby realizing the opening and closing of the left and right induction coils. The transformer (9) is fixed on the frame (10). The secondary of the transformer (9) is connected to the induction coil through two bus bars (13) to form a single-turn induction loop.
3. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 1 is characterized in that: The lifting mechanism (5) comprises a motor (15), a screw rod (16), a screw rod nut (17), a guide rail (18), a slider (19) and a fixed plate (20), wherein the motor (15) is fixed on the fixed plate (20), the motor (15) and the screw rod (16) are connected via a coupling, the screw rod (16) and the fixed plate (20) are connected via a bearing, the guide rail (18) is fixed on the fixed plate (20), the screw rod nut (17) and the slider (19) are fixed on the frame (10), and the screw rod (16) is driven to rotate by the rotation of the motor (15), so that the screw rod nut (17) drives the induction heating mechanism (2) to realize vertical linear motion.
4. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 1 is characterized in that: The rail clamping mechanism (1) comprises a left clamp (21), a right clamp (22), two upsetting shafts (23), and two guide shafts (24), wherein the left clamp (21) and the right clamp (22) are connected via the two upsetting shafts (23) and the two guide shafts (24); one end of the upsetting shaft (23) passes through the right clamp (22) to connect to the upsetting cylinder (25), and the other end of the upsetting shaft (23) is fixed to the left clamp (21); one end of the guide shaft (24) is fixed to the right clamp (22) via a nut (26), and the other end of the guide shaft (24) passes through the left clamp (21).
5. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 1 is characterized in that: The rail clamping mechanism (1) further comprises a tumor-pushing cylinder (27), a tool holder (28) and a tumor-pushing knife (29); the tumor-pushing cylinder (27) is fixed to the end of the left clamp (21) and connected to the tool holder (28) via a cylinder shaft; the tumor-pushing knife (29) is hung on the rail and fits with the tool holder (28); after the top forging of the rail is completed, the force of the tumor-pushing cylinder (27) pushes the tumor-pushing knife (29) through the tool holder (28) to remove the flash of the weld tumor squeezed out of the joint.
6. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 1 is characterized in that: The rail clamping mechanism (1) and the induction heating mechanism (2) constitute the head part of the rail induction welding machine. The rail clamping mechanism (1) realizes the functions of clamping the rail waist, upsetting and pushing the nodule, and the induction heating mechanism (2) forms a closed magnetic field to provide a heating source. The electric control system controls the actions of various parts of the mechanism by a PLC programmable controller, and monitors various sensors in the system at the same time. The medium frequency power supply provides heating power for the induction coil through IGBT inverter and series resonance; the hydraulic pump station connects to the machine head cylinder to provide kinetic energy for clamping and upsetting actions; the chiller provides cooling for the induction coil and other heating components; the carbon dioxide gas supply system provides carbon dioxide atmosphere protection for the welding process; the air cooling system provides gas source for the heat treatment process, which is used to quickly reduce the joint temperature, achieve under-speed quenching, and improve the surface hardness of the joint.
7. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 2 is characterized in that: Fifteen small nozzles (30) are respectively arranged on the two coil seats (7), and the small nozzles are connected to the air pipe joint (31) through the internal aperture, and then connected to the carbon dioxide gas supply system and the air cooling system through the air pipe (32); the coil seat (7) and the carbon dioxide protection cover (8) form a relatively closed cavity (33) around the rail joint, and carbon dioxide is injected into the cavity through the small nozzles (30) to form an inert gas protection.
8. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection according to claim 2 is characterized in that: The carbon dioxide atmosphere protection cover (8) is made of high temperature resistant materials, including but not limited to graphite plates, mica plates, asbestos cloth, etc. The carbon dioxide atmosphere protection cover (8) also plays a role of heat preservation and insulation during the heating process, thereby improving the heating efficiency.
9. The medium frequency induction welding heat treatment equipment for rails based on carbon dioxide protection and the working method thereof according to claim 1, characterized in that: The method comprises Step 1: Grind and remove rust from the end face of the rail joint to be welded, and make the butt joint surface smooth by end grinding or end milling; Step 2: Use the rail clamping device to clamp the rail to be welded and center it, and use the upsetting cylinder to apply force to make the butt joint surfaces close together; Step 3: The induction coil adopts an open-and-close structure and is installed in the middle of the rail clamping device. It is lowered to the butt joint of the rail to be welded, and then the coil is closed by the opening and closing cylinder to form a closed loop around the rail. Step 4: Control the valve to open the carbon dioxide gas supply system and inject gas into the carbon dioxide atmosphere protective cover through a small nozzle; it is required to start injecting gas 30 seconds before welding, the purity of carbon dioxide should not be less than 99.5%, and the flow rate should be 5-15L / min; Step 5: Start the medium frequency power supply to perform induction heating on the rail joint, and the temperature meter monitors the heating temperature throughout the process; Step 6: During the heating process, the upsetting cylinder always applies force, and the carbon dioxide injection flow rate is gradually reduced. When the temperature reaches 800-900°C, the carbon dioxide supply is stopped; Step 7: When the set welding temperature (1200℃~1300℃) is reached, the medium frequency power supply is turned off, and the upsetting cylinder accelerates and pressurizes the rail to be welded to close the butt joint and squeeze out the weld nodule, while the induction coil opens and rises; Step 8: The rail nodule pushing mechanism removes the weld nodule; Step 9: The induction heating mechanism descends and closes again, the control valve opens the air cooling system, and compressed air is sprayed toward the weld rail head and rail waist through a small nozzle. The spraying stops when the temperature drops below 400℃; Step 10: Start the medium frequency power supply again to heat the weld joint to about 900°C and complete the post-weld heat treatment to refine the grain structure and improve the toughness and strength of the joint; Step 11: The air cooling system is turned on again, and compressed air is used to perform under-speed quenching treatment on the joint surface to increase the joint surface hardness; Step 12: Finally, open the induction coil, release the rail by the rail clamping device, and then perform post-weld tumor removal, grinding and other treatments.
Citation Information
Cited By
Turnout welding machine with postweld heat treatment function
CN119658375A