Low-warpage fan-out wafer level packaging structure and preparation method thereof

By preparing an efficient heat dissipation structure on the back of the fan-out wafer, the problems of warping and poor heat dissipation of the reconstructed wafer are solved, and higher reliability and quality consistency are achieved, and production costs are reduced.

CN119050064AInactive Publication Date: 2024-11-29GUIZHOU ZHENHUA FENGGUANG SEMICON

Patent Information

Application Number
CN202410964568.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the existing fan-out wafer-level packaging technology, the reconstruction wafer has large warpage and poor heat dissipation, resulting in high production costs, complex processes and short device service life.

Method used

The heat dissipation structure is prepared on the back of the fan-out wafer, including metal seed layer, interconnect structure and fill layer, to form an efficient heat dissipation structure and manufactured through physical vapor deposition and electroless plating technology to ensure that the structure is rigid and warped.

Benefits of technology

It effectively reduces the warpage after wafer reconstruction, improves heat dissipation ability, improves the reliability and quality consistency of wafers, reduces production costs, and simplifies process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050064A_ABST
    Figure CN119050064A_ABST
Patent Text Reader

Abstract

The invention discloses a low-warpage fan-out wafer level packaging structure and a preparation method thereof, and belongs to the field of semiconductor chip packaging. The packaging structure comprises a core particle, a molding layer, a back heat dissipation metal seed layer, a back heat dissipation interconnection structure passivation layer, a metal filling layer, an RDL layer, an RDL passivation layer and salient points. The core particles are embedded in the molding layer, the back surface of each core particle and the lower surface of the molding layer are sequentially provided with a back surface heat dissipation metal seed layer and a back surface heat dissipation interconnection structure passivation layer, patterns of the back surface passivation layer are filled with a metal filling layer, and the front surface of each core particle and the upper surface of the molding layer are sequentially provided with an RDL layer, an RDL passivation layer and salient points. The heat dissipation structure of the reconstructed wafer is prepared on the back surface of the fan-out wafer, and the heat dissipation structure and the reconstructed wafer are integrally packaged, so that the warping of the reconstructed wafer is reduced and the heat dissipation capability is improved in the wafer reconstruction process. The problems that in an existing wafer-level packaging technology, a reconstructed wafer is large in warping and poor in heat dissipation are solved. The method is widely applied to the technical field of fan-out wafer level packaging products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductor chip packaging, and further relates to the field of semiconductor wafer-level packaging, and specifically, to a low-warpage fan-out wafer-level packaging structure and a preparation method thereof. Background Art

[0002] It is a very common phenomenon that the mismatch of thermal expansion coefficients of materials at high temperatures causes the wafer to warp during the reconstruction process of fan-out wafer-level packaging, which is also one of the key factors affecting product yield in the fan-out wafer-level packaging process. Fan-out wafer-level packaging wafer reconstruction is the process of recombining the cut core particles into heterogeneous wafers by molding. This process is usually completed on a carrier (glass, steel plate, etc.). The last step of wafer reconstruction is to remove the carrier. After removal, the reconstructed wafer warps due to stress. Warping makes it more difficult for the robot to clamp the wafer during the wafer transfer process, or even makes it impossible to clamp it. Warped wafers also affect process processing, such as lithography, PVD, etc., making it impossible for many processes to achieve higher precision and uniformity.

[0003] like Figure 1 As shown, the existing fan-out wafer-level packaging (RDL Last-Face Down process) includes the following steps: like Figure 1 As shown in A, first, a temporary adhesive film 2 for bonding the core particles is coated on the temporary adhesive carrier 1 provided, and then the core particles 3 are mounted on the carrier according to the design drawing with the electrode 301 facing downward; like Figure 1 As shown in B, the mounted core particles are then molded to reconstruct the wafer; like Figure 1 As shown in C, after removing the temporary adhesive carrier and the temporary adhesive film, a reconstructed wafer is obtained; like Figure 1 As shown in D, the electrode surface of the core particle is used as the front surface to manufacture the rewiring layer 9 and the bump 11; like Figure 1 As shown in E, the reconstructed wafer is cut into independent fan-out wafer-level packaging structure chips.

[0004] In the above steps, the warping of the reconstructed wafer makes the subsequent rewiring and bump processing difficult. The warping is often reduced by increasing the thickness of the back of the mold and post-processing (mechanical and thermal treatment) of the reconstructed wafer. The increase in molding thickness makes it difficult to dissipate heat from the chip after packaging, and the number of rewiring layers after reconstruction increases. The number of high-temperature curing processes also increases, resulting in frequent mechanical and thermal treatments, low yields, and complex processes.

[0005] In the existing fan-out wafer-level packaging process, warped wafers are often leveled by mechanical leveling, annealing to reduce stress, or a combination of the two. On the one hand, the warping is reduced by designing a reconstructed structure with lower stress. On the other hand, the difficulty of the warped wafer process is solved or reduced by two ideas: post-warping leveling. The core reason for the warping of the reconstructed wafer is the mismatch of the thermal expansion coefficients between different materials of the reconstructed wafer, the anti-yield performance of the material itself, and the difference in materials in different dimensions. At present, some technologies are dedicated to reducing wafer warping. For example, Chinese patent application number 2013076369.X discloses a device and method for wafer warpage treatment, Chinese patent application number 20220715887.2 discloses a wafer warpage adjustment device and anti-warpage method, Chinese patent application number 20222255873.2 discloses a wafer warpage adjustment jig, and US patent application number US 87288301 B2 discloses a reconstructed wafer warpage correction method. All of them reduce warpage through post-warpage processing, but still fail to solve the core problem of warpage.

[0006] In addition, reconstructed wafers often have poor heat dissipation due to the properties of the molding material. Especially in ultra-high-density fan-out wafer-level packaging products, poor heat dissipation can easily lead to device failure. The current technology usually increases the power of the heat dissipation device outside the chip to achieve heat dissipation. Therefore, in the fan-out wafer-level packaging process, how to solve the problem of reconstructed wafer warping and heat dissipation of packaged devices has always been a concern for people in this field.

[0007] In view of this, the present invention is proposed. Summary of the invention

[0008] The technical problem to be solved by the present invention is to solve the problems of large warping and poor heat dissipation of the reconstructed wafer in the existing fan-out wafer-level packaging technology.

[0009] The inventive concept of the present invention is to prepare the heat dissipation structure of the reconstructed wafer on the back of the fan-out wafer and integrate it with the reconstructed wafer for packaging, thereby reducing the warping of the reconstructed wafer and improving the heat dissipation capacity during the wafer reconstruction process. This avoids the difficulty of handling the warping afterwards, improves the reliability and quality consistency of the reconstructed wafer, and reduces the overall production cost.

[0010] To this end, the present invention provides a low-warpage fan-out wafer-level packaging structure, such as Figure 2-3 The packaging structure includes: Core particle 3, molding layer 4, back heat dissipation metal seed layer 5, back heat dissipation interconnection structure passivation layer 6, metal filling layer 7, RDL layer 9, RDL passivation layer 10, bump 11.

[0011] The front, back, left and right peripheries of the core particle 3 are all embedded in the molding layer 4, the front surface of the core particle 3 (the surface containing the core particle electrode 301) is on the same plane as the upper surface of the molding layer 4, and the back surface of the core particle 3 (the chip substrate surface) is on the same plane as the lower surface of the molding layer 4.

[0012] The back heat dissipation metal seed layer 5 is located on the back side of the core particle 3 and the lower surface of the molding layer 4 .

[0013] The back heat dissipation interconnection structure passivation layer 6 is located on the lower surface of the back heat dissipation metal seed layer 5 and presents a set pattern (the passivation layer outside the pattern is completely removed).

[0014] The metal filling layer 7 is filled in the pattern of the back heat dissipation interconnection structure passivation layer 6 and is on the same plane as the back heat dissipation interconnection structure passivation layer 6 .

[0015] The RDL layer 9 is located on the front surface of the core particle 3 and the upper surface of the molding layer 4 .

[0016] The RDL passivation layer 10 is located on the upper surface of the RDL layer 9 and has electrode lead-out holes.

[0017] The bumps 11 are located on the upper surface of the RDL passivation layer 10 and are connected to the electrodes of the RDL layer 9 below the electrode lead-out holes of the RDL passivation layer 10 .

[0018] The backside heat dissipation metal seed layer 5 , the backside heat dissipation interconnection structure passivation layer 6 and the metal filling layer 7 form a heat dissipation structure.

[0019] Preferably, the lower surfaces of the metal filling layer 7 and the back heat dissipation interconnection structure passivation layer 6 are metal filling overflow connection layers 8 to further enhance the heat dissipation capability of the heat dissipation structure.

[0020] Preferably, the number of the core particles 3 is 2 or more.

[0021] Preferably, the backside heat dissipation interconnection structure passivation layer 6 is in a strip, belt or grid shape.

[0022] The present invention provides a method for preparing a low-warpage fan-out wafer-level packaging structure. Figure 4-5 As shown. The following steps are included: Step S1: providing a temporary carrier 1 for wafer reconstruction, coating or pasting an adhesive film (adhesive film 2) for temporary bonding on the carrier 1, and fixing the core particles 3 on the adhesive film of the carrier 1 with the front side (the side with the electrode 301 is defined as the front side) facing downward and arranged in a certain pattern according to the designed position; Step S2: Molding and curing the core particles mounted on the carrier 1, and then leveling the molded surface by chemical mechanical grinding until the back material of the core particles is exposed to form a molding layer 4. Depositing a heat dissipation metal seed layer 5 on the flattened surface by physical vapor deposition (PVD) technology, and performing a photolithography process (including photoresist coating, exposure, development and residual adhesive removal) on the surface of the heat dissipation metal seed layer 5 to prepare a back heat dissipation interconnection structure passivation layer 6 pattern (strip or grid shape), and then chemically depositing a metal filling layer 7 to complete the heat dissipation structure manufacturing; Step S3: removing the carrier plate 1 of the reconstructed wafer on which the heat dissipation structure is fabricated, and removing the temporary adhesive remaining on the surface of the reconstructed wafer, and defining this surface as the front side of the reconstructed wafer; Step S4: manufacturing the RDL layer 9 and the bumps 11 on the front side of the reconstructed wafer to realize the arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan.

[0023] Optionally, step S2 includes: The heat dissipation metal seed layer 5 is a single-layer or multi-layer metal structure. The single-layer metal includes gold, aluminum, etc., with a thickness of 50nm to 500nm; the multi-layer metal structure includes: titanium / copper, with a thickness of 50nm to 200nm / 100nm to 500nm, titanium / tungsten / copper, with a thickness of 50nm to 200nm / 500nm to 200nm / 100nm to 500nm, titanium / beryllium / copper, with a thickness of 50nm to 200nm / 500nm to 200nm / 100nm to 500nm, etc.

[0024] Optionally, step S2 includes: The heat dissipation interconnection structure is strip-shaped or grid-shaped. The material of the metal filling layer 7 includes gold, copper, tin / silver alloy, etc. The deposition methods include chemical plating, electrochemical plating, etc. The line width of the heat dissipation structure is 1μm~300μm, and the spacing is 1.5~5 times the line width. The heat dissipation interconnection structure includes the internal structure of the passivation layer and the surface overflow structure. The overflow structure can be removed according to design requirements.

[0025] Optionally, step S2 includes: The heat dissipation interconnection structure will penetrate the back of the reconstructed wafer according to a certain rule, and the rigidity of the interconnection structure will support the back of the reconstructed wafer, reducing the warping after the carrier 1 is removed and during the subsequent photoresist curing process.

[0026] The technical principle of the packaging structure of the present invention: Before the temporary bonding carrier is removed during the wafer reconstruction process, an interconnect structure is manufactured on the back of the reconstructed wafer. The interconnect structure is composed of metal and has a greater yield strength. After the temporary bonding carrier is removed, the rigidity of the interconnect structure is used to offset the warping effect of the reconstructed wafer stress on the wafer, thereby achieving low warpage. The interconnect structure is interconnected from the core substrate to the surface of the package body, which is conducive to the heat dissipation of high-density fan-out wafer-level packaging devices during operation and improves the service life of the device.

[0027] Technical effect: The traditional post-warping correction method is changed to optimize the reconstructed wafer structure to reduce the warping of the wafer after reconstruction. At the same time, the structure also has heat dissipation capabilities, solving the heat dissipation problem of high-density plastic-encapsulated chips.

[0028] A low warpage fan-out wafer-level packaging structure is formed.

[0029] Reduce fan-out wafer reconstruction warpage while taking into account heat dissipation function.

[0030] The heat dissipation structure density can be changed to increase the heat dissipation effect according to the packaging requirements of chips with different densities. The heat dissipation structure can also be used to reduce the warpage of the reconstructed wafer to achieve single-chip or multi-chip reconstruction.

[0031] The heat dissipation structure can be manufactured and reconstructed on the back of the wafer in fan-out wafer-level packaging through the existing mature advanced packaging technology, solving the problem of heat dissipation difficulties of plastic-encapsulated chips. At the same time, the rigidity of the heat dissipation structure can reduce the warping of the wafer after the temporary bonding carrier is removed. It has low manufacturing difficulty and strong practicality. It can be widely used in the field of fan-out wafer-level packaging product technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 It is a schematic diagram of the existing fan-out wafer-level packaging structure process.

[0033] Figure 2 It is a schematic diagram of the cross-sectional structure of the low-warpage fan-out wafer-level package of the present invention.

[0034] Figure 3 It is a schematic diagram of the three-dimensional structure of the low-warpage fan-out wafer-level package of the present invention.

[0035] Figure 4 It is a schematic diagram of the process structure of the low-warpage fan-out wafer-level packaging structure of the present invention.

[0036] Figure 5 It is a schematic diagram of the process flow of the low-warpage fan-out wafer-level packaging structure of the present invention.

[0037] In the figure: 1 is a carrier board, 2 is an adhesive film, 3 is a core particle, 301 is a core particle electrode, 4 is a molding layer, 5 is a back heat dissipation metal seed layer, 6 is a back heat dissipation interconnection structure passivation layer, 7 is a metal filling layer, 8 is a metal filling overflow layer, 9 is a front rewiring metal layer (RDL layer), 10 is a front rewiring passivation layer (RDL passivation layer), and 11 is a bump. DETAILED DESCRIPTION

[0038] like Figure 2-5 As shown, the low-warpage fan-out wafer-level packaging structure and its preparation method, the specific implementation case is as follows: Implementation Example 1: Step S1: Coating a temporary bonding adhesive film on the carrier plate 1 (made of stainless steel) with a diameter of 300 mm and a thickness of 700 μm, with a thickness of 30 μm, and placing the front side of the core particles (the electrode side is defined as the front side) facing downward, with a size of 12 mm*12 mm*0.2 mm, and fixing them on the adhesive film of the carrier plate 1 in a certain arrangement according to the designed position; Step S2: Molding and curing the core particles mounted on the carrier 1. After curing, the molding thickness is 0.25 mm. Then, the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed. The heat dissipation metal seed layer titanium / copper is deposited on the flattened surface by physical vapor deposition (PVD) technology with a thickness of 0.1μm and 0.5μm respectively. The metal seed layer titanium / copper surface is subjected to photoresist coating, exposure, development, curing and residual adhesive removal to obtain a strip-shaped (blade-shaped, such as Figure 3 A heat dissipation structure pattern, the line width / line spacing of the pattern is 10μm / 100μm, the thickness is 50μm, and then the heat dissipation metal copper is deposited and filled by electrochemical method. The metal copper filling thickness is higher than the photoresist and overflows on the surface of the photoresist to form a heat dissipation structure; Step S3: removing the carrier plate 1 of the reconstructed wafer with the heat dissipation structure by heating and debonding, and removing the temporary adhesive remaining on the surface of the reconstructed wafer by plasma, and defining this surface as the front side of the reconstructed wafer. The diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are copper pillar bumps, the diameter is 60μm, and the pitch is 130μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

[0039] Implementation Example 2: Step S1: Coat a 30 μm thick adhesive film on the carrier 1 (made of silicon) with a diameter of 300 mm and a thickness of 750 μm for temporary bonding, and place the front side of the core particles (the electrode side is defined as the front side) downward, with a size of 12 mm*12 mm*0.2 mm, and arrange and fix on the adhesive film of the carrier 1 in a certain pattern according to the designed position; Step S2: Molding and curing the core particles mounted on the carrier 1. After curing, the molding thickness is 0.25mm. Then, the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed. The heat dissipation metal seed layer titanium / copper is deposited on the flattened surface by physical vapor deposition (PVD) technology with a thickness of 0.1μm and 0.5μm respectively. The metal seed layer titanium / copper surface is subjected to photoresist coating, exposure, development, curing and residual adhesive removal to obtain a grid-like heat dissipation structure pattern (such as Figure 3 As shown in B), the line width / line spacing of the pattern is 10μm / 80μm, the thickness is 50μm, and then the heat dissipation metal copper is filled by chemical plating. The metal copper filling thickness is higher than the photoresist and overflows on the surface of the photoresist to form a heat dissipation structure; Step S3: removing the carrier plate 1 of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the temporary adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent, and defining this surface as the front side of the reconstructed wafer, and the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are solder ball bumps, the diameter is 100μm, and the pitch is 220μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

[0040] Implementation Example 3: Step S1: Coat a 30 μm thick adhesive film on the carrier 1 (made of silicon) with a diameter of 300 mm and a thickness of 750 μm for temporary bonding, and place the front sides (the electrode side is defined as the front side) of the two core particles A and B facing downward, with the size of the A core particle being 12 mm*5 mm*0.2 mm and the size of the B core particle being 4 mm*4 mm*0.2 mm, and arrange and fix them on the adhesive film of the carrier 1 in a certain pattern according to the designed position; Step S2: Molding and curing the core particles mounted on the carrier 1. After curing, the molding thickness is 0.25 mm. Then, the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed. The heat dissipation metal seed layer gold is deposited on the flattened surface by physical vapor deposition (PVD) technology with a thickness of 0.1 μm. The surface of the metal seed layer is subjected to photoresist coating, exposure, development, curing and residual adhesive removal to obtain a strip-shaped (blade-shaped, such as Figure 3 C) heat dissipation structure pattern, the line width / line spacing of the pattern is 1μm / 6μm, the thickness is 1.15μm, and then the heat dissipation metal gold-cobalt alloy is deposited and filled by electrochemical method. The thickness of the gold-cobalt alloy filling is slightly lower than the photoresist. The photoresist and the gold-cobalt alloy are placed in the same plane by chemical mechanical grinding to form a heat dissipation structure; Step S3: removing the carrier plate 1 of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the temporary adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent, and defining this surface as the front side of the reconstructed wafer, and the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are solder ball bumps, the diameter is 100μm, and the pitch is 220μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.5mm.

[0041] Implementation Example 4: Step S1: Coat a 30 μm thick adhesive film on the carrier 1 (made of silicon) with a diameter of 300 mm and a thickness of 750 μm for temporary bonding, and place the front sides (the electrode side is defined as the front side) of the two core particles A and B facing downward, with the size of the A core particle being 12 mm*5 mm*0.2 mm and the size of the B core particle being 4 mm*4 mm*0.2 mm, and arrange and fix them on the adhesive film of the carrier 1 in a certain pattern according to the designed position; Step S2: Molding and curing the core particles mounted on the carrier 1. After curing, the molding thickness is 0.25mm. Then, the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed. The heat dissipation metal seed layer titanium / copper is deposited on the flattened surface by physical vapor deposition (PVD) technology with a thickness of 0.1μm and 0.5μm respectively. The metal seed layer titanium / copper surface is subjected to photoresist coating, exposure, development, curing and residual adhesive removal to obtain a grid-like heat dissipation structure pattern (such as Figure 3D), the line width / line spacing of the pattern is 10μm / 40μm, the thickness is 50μm, and then the heat dissipation metal copper is filled by chemical plating. The metal copper filling thickness is higher than the photoresist and overflows on the surface of the photoresist to form a heat dissipation structure; Step S3: removing the carrier plate 1 of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the temporary adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent, and defining this surface as the front side of the reconstructed wafer, and the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are copper pillar bumps, the diameter is 60μm, and the pitch is 130μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

[0042] Finally, it should be noted that the above embodiments are merely examples for the purpose of clear explanation. The present invention includes but is not limited to the above embodiments. It is not necessary and impossible to list all implementation methods exhaustively. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. All implementation methods that meet the requirements of the present invention belong to the protection scope of the present invention.

Claims

1. A low-warpage fan-out wafer-level packaging structure, characterized in that: The packaging structure comprises: Core particle (3), molding layer (4), back side heat dissipation metal seed layer (5), back side heat dissipation interconnection structure passivation layer (6), metal filling layer (7), RDL layer (9), RDL passivation layer (10), bump (11); The core particle (3) is one or more than one particle, and the front, back, left, and right peripheries of the core particle (3) are all embedded in the molding layer (4), the front surface of the core particle (3) and the upper surface of the molding layer (4) are on the same plane, and the back surface of the core particle (3) and the lower surface of the molding layer (4) are on the same plane; The back heat dissipation metal seed layer (5) is located on the back side of the core particle (3) and the lower surface of the molding layer (4); The backside heat dissipation interconnection structure passivation layer (6) is located on the lower surface of the backside heat dissipation metal seed layer (5) and is in a set pattern shape; The metal filling layer (7) is filled in the pattern of the back heat dissipation interconnection structure passivation layer (6) and is on the same plane as the back heat dissipation interconnection structure passivation layer (6); The RDL layer (9) is located on the front surface of the core particle (3) and the upper surface of the molding layer (4); The RDL passivation layer (10) is located on the upper surface of the RDL layer (9) and is provided with electrode lead-out holes; The bump (11) is located on the upper surface of the RDL passivation layer (10) and is connected to the electrode of the RDL layer (9) below the electrode lead-out hole of the RDL passivation layer (10); The backside heat dissipation metal seed layer (5), the backside heat dissipation interconnection structure passivation layer (6) and the metal filling layer (7) form an interconnection heat dissipation structure.

2. A low warpage fan-out wafer-level packaging structure according to claim 1, characterized in that: The lower surfaces of the metal filling layer (7) and the backside heat dissipation interconnection structure passivation layer (6) are metal filling overflow layers (8).

3. The low warpage fan-out wafer-level packaging structure according to claim 1, characterized in that: The back-side heat dissipation interconnection structure passivation layer (6) is in the shape of a strip, a belt or a grid.

4. The low warpage fan-out wafer-level packaging structure according to claim 1, characterized in that: The heat dissipation metal seed layer (5) is a single-layer or multi-layer metal structure. The single-layer metal structure is gold or aluminum with a thickness of 50nm to 500nm; the multi-layer metal structure is a titanium-copper composite layer, a titanium-tungsten-copper composite layer or a titanium-beryllium-copper composite layer; The thickness of the titanium-copper composite layer is 50nm-200nm and 100nm-500nm respectively; The thickness of titanium tungsten copper in the titanium tungsten copper composite layer is 50nm-200nm, 500nm-200nm, and 100nm-500nm respectively; The thickness of titanium beryllium copper in the titanium beryllium copper composite layer is 50nm-200nm, 500nm-200nm, and 100nm-500nm, respectively.

5. The low warpage fan-out wafer-level packaging structure according to claim 1, characterized in that: The metal filling material of the metal filling layer (7) is gold, copper or tin / silver alloy, and the deposition method is chemical plating or electrochemical plating. The line width of the interconnected heat dissipation structure is 1 μm to 300 μm, and the spacing is 1.5 to 5 times the line width.

6. The method for preparing a low-warpage fan-out wafer-level packaging structure according to claim 1, characterized in that: The following steps are involved: Step S1: coating or pasting an adhesive film (2) on the carrier (1), and arranging and fixing the core particles (3) on the adhesive film (2) with the front side facing downward according to design requirements; Step S2: molding and curing the mounted core particles, and then leveling the molded surface by chemical mechanical grinding until the back material of the core particles is exposed to form a molding layer (4); depositing a heat dissipation metal seed layer (5) on the ground and leveled surface by physical vapor deposition technology; and coating a photoresist layer on the surface of the heat dissipation metal seed layer (5), etching and debonding the photoresist layer by photolithography technology to prepare a back heat dissipation interconnection structure passivation layer (6) with a strip or grid structure; and then chemically depositing a metal filling layer (7) to complete the heat dissipation structure manufacturing; Step S3: removing the reconstructed wafer with the heat dissipation structure from the carrier (1), and removing the adhesive film (2) remaining on the surface of the reconstructed wafer to form the front side of the reconstructed wafer; Step S4: manufacturing an RDL layer (9), an RDL passivation layer (10) and bumps (11) on the front side of the reconstructed wafer to achieve a core particle electrode array arrangement; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independently packaged wafer-level packaging structure chips according to design requirements.

7. The method for preparing a low-warpage fan-out wafer-level packaging structure according to claim 6, characterized in that: The specific implementation process is: Step S1: coating an adhesive film with a thickness of 30 μm on a stainless steel carrier plate (1) with a diameter of 300 mm and a thickness of 700 μm, and placing the core particles with the front side facing downwards and the core particles with a size of 12 mm*12 mm*0.2 mm, and arranging and fixing them on the adhesive film of the carrier plate (1) in a certain pattern according to the designed position; Step S2: the core particles mounted on the carrier (1) are molded and cured, and the molding thickness after curing is 0.25 mm, and then the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed; a heat dissipation metal seed layer titanium / copper layer is deposited on the flattened surface by physical vapor deposition technology, with a thickness of 0.1 μm and 0.5 μm respectively, and photoresist coating, exposure, development, curing and residual adhesive removal are performed on the surface of the metal seed layer titanium / copper layer to obtain a strip-type heat dissipation structure pattern, with a pattern line width / line spacing of 10 μm / 100 μm and a thickness of 50 μm, and then heat dissipation metal copper is deposited by electrochemical means, and the metal copper filling thickness is higher than the photoresist layer thickness, and overflows on the photoresist surface to form a heat dissipation structure; Step S3: removing the carrier plate (1) of the reconstructed wafer with the heat dissipation structure by heating and debonding, and removing the adhesive remaining on the surface of the reconstructed wafer by plasma to form the front side of the reconstructed wafer. The diameter of the reconstructed wafer is 300 mm. Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are copper pillar bumps, the diameter is 60μm, and the pitch is 130μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

8. The method for preparing a low-warpage fan-out wafer-level packaging structure according to claim 6, characterized in that: The specific implementation process is: Step S1: coating an adhesive film with a thickness of 30 μm on a silicon carrier (1) with a diameter of 300 mm and a thickness of 700 μm, and placing the core particles with the front side facing downwards and the core particles with a size of 12 mm*12 mm*0.2 mm, and arranging and fixing them on the film of the carrier (1) in a certain pattern according to the designed position; Step S2: the core particles mounted on the carrier (1) are molded and cured, and the molding thickness after curing is 0.25 mm, and then the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed; a heat dissipation metal seed layer titanium / copper layer is deposited on the flattened surface by physical vapor deposition technology, with a thickness of 0.1 μm and 0.5 μm respectively, and photoresist coating, exposure, development, curing and residual adhesive removal are performed on the surface of the metal seed layer titanium / copper layer to obtain a grid-like heat dissipation structure pattern with a line width / line spacing of 10 μm / 80 μm and a thickness of 50 μm, and then heat dissipation metal copper is deposited by electrochemical means, and the metal copper filling thickness is higher than the photoresist layer thickness, and overflows on the photoresist surface to form a heat dissipation structure; Step S3: removing the carrier plate (1) of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent to form the front side of the reconstructed wafer, wherein the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are solder ball bumps, the diameter is 100μm, and the pitch is 220μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

9. The method for preparing a low-warpage fan-out wafer-level packaging structure according to claim 6, characterized in that: The specific implementation process is: Step S1: coating an adhesive film with a thickness of 30 μm on a silicon carrier (1) with a diameter of 300 mm and a thickness of 700 μm, and placing two types of core particles A and B facing downward, with the size of the A core particle being 12 mm*5 mm*0.2 mm and the size of the B core particle being 4 mm*4 mm*0.2 mm, and arranging them in a certain pattern according to the designed positions and fixing them on the adhesive film of the carrier (1); Step S2: the core particles mounted on the carrier (1) are molded and cured, and the molding thickness after curing is 0.25 mm, and then the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed; a heat dissipation metal seed layer and a gold layer are deposited on the flattened surface by physical vapor deposition technology, and the thickness is 0.1 μm, and photoresist coating, exposure, development, curing and residual adhesive removal are performed on the surface of the heat dissipation metal seed layer and the gold layer to obtain a strip-type heat dissipation structure pattern, and the pattern line width / line spacing is 1 μm / 6 μm and the thickness is 1.15 μm, and then the heat dissipation metal gold-cobalt alloy is deposited and filled by electrochemical means, and the filling thickness of the gold-cobalt alloy is slightly lower than the photoresist, and the photoresist and the gold-cobalt alloy are placed in the same plane by chemical mechanical grinding to form a heat dissipation structure; Step S3: removing the carrier plate (1) of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent to form the front side of the reconstructed wafer, wherein the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are solder ball bumps, the diameter is 100μm, and the pitch is 220μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.5mm.

10. The method for preparing a low-warpage fan-out wafer-level packaging structure according to claim 6, characterized in that: The specific implementation process is: Step S1: coating an adhesive film with a thickness of 30 μm on a silicon carrier (1) with a diameter of 300 mm and a thickness of 700 μm, and placing two types of core particles A and B facing downward, with the size of the A core particle being 12 mm*5 mm*0.2 mm and the size of the B core particle being 4 mm*4 mm*0.2 mm, and arranging them in a certain pattern according to the designed positions and fixing them on the adhesive film of the carrier (1); Step S2: the core particles mounted on the carrier (1) are molded and cured, and the molding thickness after curing is 0.25 mm, and then the molding surface is flattened by chemical mechanical grinding until the back material of the core particles is exposed; a heat dissipation metal seed layer titanium / copper layer is deposited on the flattened surface by physical vapor deposition technology, with thicknesses of 0.1 μm and 0.5 μm respectively, and photoresist coating, exposure, development, curing and residual adhesive removal are performed on the surface of the heat dissipation metal seed layer titanium / copper layer to obtain a grid-like heat dissipation structure pattern with a line width / line spacing of 10 μm / 40 μm and a thickness of 50 μm, and then heat dissipation metal copper is filled by chemical plating, and the metal copper filling thickness is higher than the photoresist and overflows on the surface of the photoresist to form a heat dissipation structure; Step S3: removing the carrier plate (1) of the reconstructed wafer with the heat dissipation structure fabricated thereon by laser debonding, and removing the adhesive remaining on the surface of the reconstructed wafer by wet chemical solvent to form the front side of the reconstructed wafer, wherein the diameter of the reconstructed wafer is 300 mm; Step S4: rewiring and bump manufacturing are performed on the front side of the reconstructed wafer, the number of rewiring layers is 2, the line width / line spacing is 5μm / 5μm, the bumps are copper pillar bumps, the diameter is 60μm, and the pitch is 130μm, so as to realize the fan-out arrangement of the core particle electrode array; Step S5: Cut the reconstructed wafer that has completed front-side rewiring and bump manufacturing from the front side, and divide the core particles into independent packaged chips according to the design plan, with a size of 14mm*14mm*0.55mm.

Citation Information

Patent Citations

  • Fan-out type packaging structure and packaging method

    CN114334672A

  • Fan-out wafer level packaging process applying wafer with distortion prevention and radiation function

    KR101393701B1

  • Semiconductor package and manufacturing method thereof

    US20200365486A1

Cited By

  • Chip three-dimensional packaging method

    CN120072659A

  • Method for avoiding layering in embedded wafer level ball grid array bonding process

    CN120072668A

  • A method for avoiding delamination in an embedded wafer-level ball grid array bonding process

    CN120072668B

  • Packaging method of photoelectric sealing structure and photoelectric sealing structure

    CN120882147A