Internal decoration helmet and processing method
By spraying transparent varnish and gold oil layers on the inner wall of the helmet shell and applying decorative materials to form a solid protective layer, the problem of insufficient adhesion of decorative materials in the prior art is solved, and the aesthetics and durability of the helmet are significantly improved.
Patent Information
- Application Number
- CN202411466559.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-18
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing helmet decorative materials are directly attached to the outer wall of the shell, which has poor adhesion and is prone to fall off or wear, affecting aesthetics and durability.
Using the processing method of interior decorative helmets, by spraying transparent varnish and gold oil layers on the inner wall of the transparent helmet shell, and applying decorative materials such as glitter powder and water stickers on the varnish layer, it is formed after being left to stand and dried and baked. Strong protective layer.
It improves the adhesion and wear resistance of the decorative materials, extends the service life of the helmet inner wall coating, enhances the aesthetics and durability of the helmet, and prevents fraying or falling off.
Smart Images

Figure CN119055003A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of helmet manufacturing, and in particular to an internally decorated helmet and a processing method thereof. Background Art
[0002] In the existing helmet manufacturing technology, the decoration of the helmet is usually processed on the outer wall of the shell. However, this traditional decoration method has several significant shortcomings. First, since the decorative material is directly attached to the outer wall of the helmet shell, its adhesion is often not strong, and it is easy to fall off or wear during use, which not only affects the aesthetics of the helmet, but also reduces its durability. Secondly, the decorative material on the outer wall of the helmet shell is easy to contact with external objects, so it is more prone to wear and scratching, which further shortens the durability of the helmet decorative material.
[0003] Therefore, while pursuing individuality and aesthetics, how to ensure the firmness and durability of decorative materials has become a technical problem that needs to be solved urgently. Summary of the invention
[0004] The purpose of the present invention is to provide a method for processing an internally decorated helmet in view of the problems existing in the prior art. The method not only improves the adhesion of the decorative material, but also, by virtue of the protective effect of the helmet shell, enables the internal coating to be used for a long time without being easily scratched or falling off, thereby significantly improving the aesthetics and durability of the helmet.
[0005] To achieve the above object, the technical solution adopted by the present invention is:
[0006] A method for processing an internally decorated helmet comprises the following steps:
[0007] S1. Choose a transparent helmet as the basic product;
[0008] S2. Clean the inner wall of the helmet shell to remove dust and impurities;
[0009] S3, spraying a transparent varnish layer on the inner wall of the helmet shell;
[0010] S4, applying decorative materials on the varnish layer;
[0011] S5, spraying a transparent varnish layer again to fix the decorative material;
[0012] S6. Allow the helmet to stand and dry and bake to allow the varnish to fully penetrate and solidify;
[0013] S7. Grinding the inner wall of the helmet shell to obtain a flat and smooth surface;
[0014] S8, clean the inner wall of the helmet shell again and spray the gold oil layer;
[0015] S9, the helmet is allowed to stand and dry and bake again until the required hardness is reached;
[0016] S10. Conduct quality inspection on the finished helmet shells and rework unqualified ones.
[0017] In step S4, applying the decorative material on the varnish layer includes:
[0018] Sprinkle glitter powder evenly on the inner wall of the helmet shell coated with a transparent varnish layer to form dense glittering spots.
[0019] In step S4, before applying the flashing decorative material on the varnish layer, the process includes:
[0020] Stick the water-based sticker with the designed pattern on the predetermined position of the inner wall of the helmet shell to absorb excess moisture.
[0021] In step S6, the step of placing the helmet in a static state and performing a drying and baking process comprises:
[0022] The helmet shell is placed at room temperature for a predetermined time, and then placed in an oven for a first drying and baking process, and the helmet shell is baked at a predetermined temperature for a predetermined time.
[0023] In step S7, the grinding process of the inner wall of the helmet shell includes:
[0024] Use sandpaper to manually smooth out any bumps or uneven areas on the inner wall of the helmet shell to make the surface smooth.
[0025] In step S8, the step of cleaning the inner wall of the helmet shell again and spraying the gold oil layer comprises:
[0026] Use an air gun and a brush to clean the inner wall of the helmet shell to ensure that no dust and impurities remain on the inner wall of the helmet shell;
[0027] Use a spray gun to spray PU gold oil, making sure that the PU gold oil evenly covers the inner wall of the helmet shell.
[0028] In step S9, the helmet is placed in a static state and dried and baked again, including:
[0029] The helmet shell is placed at room temperature for a predetermined time, and then placed in the oven again for drying and baking. The helmet shell is baked at a predetermined temperature for a predetermined time or until the hardness of the varnish layer reaches Grade F.
[0030] The processing method also includes the following steps:
[0031] S11. Process the outer wall surface of the helmet shell that has passed the inspection to remove residual processing materials accidentally attached to the outer wall.
[0032] In step S11, the outer wall surface of the helmet shell that has passed the inspection is processed, including:
[0033] S11.1. Use a pneumatic sander with pneumatic sandpaper to remove the gloss from the outer wall of the helmet shell and remove the residues initially;
[0034] S11.2. Use an air gun to blow away dust and grinding debris from the outer wall of the helmet shell;
[0035] S11.3. Place the shell in water containing detergent and use water-abrasive sandpaper to carefully polish it to remove the sandpaper marks on the outer wall of the helmet shell.
[0036] S11.4. After the helmet shell is dried, use a lint-free cotton towel dipped in water containing detergent to wipe the outer wall of the helmet shell again;
[0037] S11.5. Use a dust-removing cloth to wipe the outer wall of the helmet shell to remove any remaining dust and impurities.
[0038] S11.6. Spray a layer of varnish evenly on the outer wall of the helmet shell;
[0039] S11.7. Place the sprayed helmet shell in an oven and let it stand for a predetermined time, then bake the helmet shell at a predetermined temperature for a predetermined time, or until the hardness of the outer wall varnish layer reaches the F grade standard and then take it out;
[0040] S11.8. Conduct secondary quality inspection on the processed helmet shells, and rework the unqualified ones.
[0041] An internally decorated helmet, comprising:
[0042] Helmet shell;
[0043] A first transparent varnish layer, attached to the inner wall of the helmet shell;
[0044] A decorative material layer attached to the inner side of the first transparent varnish layer;
[0045] a second transparent varnish layer, attached to the inner side of the decorative material layer;
[0046] The gold oil layer is attached to the inner side of the second transparent varnish layer.
[0047] Compared with the prior art, the present invention has the following beneficial effects:
[0048] 1. By applying decorative materials such as glitter powder, sequins and water stickers with unique designs on the inner wall of the transparent helmet shell, the helmet can present colorful patterns and flashing effects under the irradiation of light, which greatly improves the aesthetics and personalized decorative effect of the helmet;
[0049] 2. The protective effect of the helmet shell ensures that the internal coating will not be scratched or fall off even after long-term use, further enhancing the durability and protection of the helmet;
[0050] 3. Spray transparent varnish layer and gold oil layer multiple times, and then let it stand and dry and bake to allow the coating to fully penetrate and solidify, forming a strong, beautiful and wear-resistant protective layer, which not only improves the adhesion and wear resistance of the inner wall coating of the helmet, but also ensures the gloss and beauty of the coating. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0052] Figure 1 This is a flow chart of a method for processing an internally decorated helmet according to an embodiment of the present application;
[0053] Figure 2 This is a flow chart of the method for processing the outer wall of the helmet shell in an embodiment of the present application;
[0054] Figure 3 This is a schematic cross-sectional view of a helmet shell in an embodiment of the present application;
[0055] In the figure: 1. Helmet shell; 2. First transparent varnish layer; 3. Decorative material layer; 4. Second transparent varnish layer; 5. Gold varnish layer. DETAILED DESCRIPTION
[0056] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0057] In view of the problems in the background technology, the present application provides a method for processing an internally decorated helmet, comprising the following steps:
[0058] S1. Choose a transparent helmet as the basic product to ensure the transparency and structural strength of the helmet;
[0059] S2. Use professional cleaning agents and tools to clean the inner wall of the helmet shell to remove dust and impurities, ensuring that the inner wall surface is clean and free of pollution;
[0060] S3. Spray a 0.2mm thick transparent varnish layer evenly on the inner wall of the helmet shell to form a smooth and uniform bottom layer, providing a base for subsequent decorative materials to adhere to;
[0061] S4. Apply decorative materials on the varnish layer, such as glitter powder, sequins, and water stickers. Decorative materials of different colors and shapes can be applied according to design requirements;
[0062] S5. Spray a layer of transparent varnish again to fix the glittering decorative material, ensure that the decorative material will not fall off or shift, and enhance the glossiness and aesthetics of the inner wall of the helmet;
[0063] S6. Place the helmet at room temperature for a period of time to allow the varnish to initially penetrate and level. Then, place the helmet in an oven for drying and baking to allow the varnish to fully penetrate and solidify to form a solid coating.
[0064] S7. Use sandpaper or grinding tools to grind the inner wall of the helmet shell to remove protrusions, unevenness and burrs to obtain a flat and smooth surface;
[0065] S8. After cleaning the inner wall of the helmet shell, use a spray gun to spray a layer of gold oil to enhance the golden luster of the inner wall of the helmet;
[0066] S9. Place the helmet at room temperature for a period of time to allow the gold oil to initially penetrate and level. Then, place the helmet in an oven for drying and baking again until the required hardness is reached to ensure that the gold oil layer is fully solidified to form a strong and beautiful coating.
[0067] S10. Carry out quality inspection on the finished helmet shell, such as appearance inspection, coating adhesion test, and hardness test, to ensure that the helmet meets the design requirements and quality standards, and rework unqualified products.
[0068] Through the above steps, the present embodiment directly processes the inner wall of the transparent helmet shell to form a pattern and a flashing effect. Due to the protective effect of the helmet shell, the inner coating will not be worn or fall off after long-term use. At the same time, by spraying the varnish layer and the gold oil layer multiple times, and then standing and drying and baking, the coating is fully penetrated and solidified to form a strong and beautiful coating. This not only improves the wearing comfort and aesthetics of the helmet, but also prolongs the service life of the helmet.
[0069] In some embodiments, in step S4, applying a decorative material on the varnish layer includes:
[0070] Glitter powder is used as a flashing decorative material and is evenly and finely spread on the inner wall of the helmet shell that has been coated with a transparent varnish layer through a special powder spreading tool, forming dense and uniform flashing points.
[0071] Through the above steps, the helmet can present a flashing effect under the irradiation of light, and because the glitter powder is firmly fixed on the inner wall of the helmet, it is not easy to fall off or wear during use, thereby ensuring the long-term beauty and durability of the helmet.
[0072] In some embodiments, in step S4, before applying the decorative material on the varnish layer, the process includes:
[0073] Select a water-based sticker with a unique design pattern, and accurately fit it to the predetermined position on the inner wall of the helmet shell. Press gently to ensure that the sticker is in close contact with the varnish layer. Then, use a professional water-absorbing tool to absorb excess water to avoid residual water affecting subsequent processes and ensure that the water-based sticker is firmly bonded to the inner wall of the helmet.
[0074] Through the above steps, the helmet can present a specific pattern, enrich the personalized decoration of the helmet, and enhance the overall beauty of the helmet.
[0075] In some embodiments, in step S6, the step of placing the helmet in a static state and performing a drying and baking process includes:
[0076] Place the helmet shell at room temperature for 1 hour to allow the varnish layer to initially level out naturally. Then, place the helmet shell in an oven for the first drying and baking. The oven temperature is set to 70°C. The choice of oven temperature is based on the characteristics of the varnish material. It can effectively accelerate the curing reaction of the varnish without causing material denaturation or helmet deformation due to excessive temperature. The baking time is 2 hours to ensure that the varnish layer can fully penetrate and solidify to form a hard, wear-resistant protective layer.
[0077] Allow the varnish layer to level slowly at room temperature to reduce defects. The 70°C baking temperature promotes the cross-linking reaction between varnish molecules and accelerates the curing process. The 2-hour baking time ensures that the varnish layer can be completely cured to achieve the ideal hardness and durability. Through the above steps, the adhesion and wear resistance of the inner wall coating of the helmet are improved, the gloss and aesthetics of the coating are guaranteed, and the service life of the helmet is extended.
[0078] In some embodiments, in step S7, the grinding process on the inner wall of the helmet shell includes:
[0079] Use 240-grit sandpaper to manually polish the bumps or unevenness on the inner wall of the helmet shell to make the surface smooth. Using 240-grit sandpaper can effectively remove the bumps or unevenness that may be caused by the previous process on the inner wall of the helmet without excessively wearing the varnish layer or base material.
[0080] In some embodiments, in step S8, the step of cleaning the inner wall of the helmet shell again and spraying the gold oil layer comprises:
[0081] Use an air gun and a brush to clean the inner wall of the helmet shell to ensure that no dust and impurities remain on the inner wall of the helmet shell; use a spray gun to spray PU gold oil to ensure that the PU gold oil is evenly covered on the inner wall of the helmet shell.
[0082] Through the above steps, the PU gold oil not only gives the helmet a golden luster, improving the overall aesthetics of the helmet, but also enhances the wear resistance and protective performance of the inner wall of the helmet, extending the service life of the helmet.
[0083] In some embodiments, in step S9, the step of placing the helmet in a static state and drying and baking the helmet again includes:
[0084] Place the helmet shell at room temperature for 1 hour to achieve initial leveling and reduce uneven surface tension. Then, place the shell back into the oven for drying and baking. For the second drying and baking, set the oven temperature to 70°C. This will not cause material denaturation due to excessive temperature and can effectively accelerate the curing reaction of the gold oil layer. Set the baking time to 2 hours or until the hardness of the varnish layer reaches grade F, then take out the helmet.
[0085] Through the above steps, the adhesion and wear resistance of the gold oil layer on the inner wall of the helmet are significantly improved, and the gloss and aesthetics of the coating are guaranteed, thereby further extending the service life of the helmet.
[0086] In some embodiments, the processing method further comprises the following steps:
[0087] S11. Treat the outer wall surface of the helmet shell that has passed the inspection to remove the residual processing materials accidentally attached to the outer wall, and keep the appearance of the helmet clean and beautiful.
[0088] In some embodiments, in step S11, the processing of the outer wall surface of the helmet shell that has passed the inspection includes:
[0089] S11.1. Use a pneumatic sander with 320-grit air-grit sandpaper to remove the gloss from the outer wall of the helmet shell and the initial removal of residues;
[0090] S11.2. Use an air gun to blow away dust and grinding debris from the outer wall of the helmet shell;
[0091] S11.3. Place the shell in water containing detergent and use 1000-grit water-abrasive sandpaper to carefully polish it to remove the sandpaper marks on the outer wall of the helmet shell;
[0092] S11.4. After the helmet shell is dried, use a lint-free cotton towel dipped in water containing detergent to wipe the outer wall of the helmet shell again;
[0093] S11.5. Use a dust-removing cloth to wipe the outer wall of the helmet shell to remove any remaining dust and impurities.
[0094] S11.6. Spray a layer of varnish evenly on the outer wall of the helmet shell;
[0095] S11.7. Place the sprayed helmet shell in an oven and let it stand for 1 hour. Then bake the helmet shell at 70 degrees for 3 hours, or until the hardness of the outer wall varnish layer reaches the F grade standard.
[0096] S11.8. Conduct secondary quality inspection on the processed helmet shells, and rework the unqualified ones.
[0097] Through a series of fine grinding, cleaning and spraying processes in the above steps, the residue on the outer wall of the helmet shell is completely removed, and the aesthetics and protection are improved.
[0098] A second aspect of the present application provides an internally decorated helmet, which is manufactured using the above processing method, comprising:
[0099] Helmet shell 1;
[0100] A first transparent varnish layer 2, attached to the inner wall of the helmet shell 1;
[0101] A decorative material layer 3, attached to the inner side of the first transparent varnish layer 2;
[0102] a second transparent varnish layer 4, attached to the inner side of the decorative material layer 3;
[0103] The gold oil layer 5 is attached to the inner side of the second transparent varnish layer 4 .
[0104] It should be understood that the size of the serial numbers of the steps in the above embodiments does not mean the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.
[0105] In the description of the present specification and the appended claims, the terms "first", "second", "third", etc. are only used to distinguish descriptions and cannot be understood as indicating or suggesting relative importance. It should also be understood that although the terms "first", "second", etc. are used to describe various elements in some embodiments of the present application in the text, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. For example, the first table can be named as the second table, and similarly, the second table can be named as the first table without departing from the scope of the various described embodiments. The first table and the second table are both tables, but they are not the same table.
[0106] References to "one embodiment" or "some embodiments" etc. described in the specification of this application mean that one or more embodiments of the present application include specific features, structures or characteristics described in conjunction with the embodiment. Therefore, the statements "in one embodiment", "in some embodiments", "in some other embodiments", "in some other embodiments", etc. that appear in different places in this specification do not necessarily refer to the same embodiment, but mean "one or more but not all embodiments", unless otherwise specifically emphasized in other ways. The terms "including", "comprising", "having" and their variations all mean "including but not limited to", unless otherwise specifically emphasized in other ways.
[0107] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for processing an internally decorated helmet, It is characterized in that The following steps are involved: S1. Choose a transparent helmet as the basic product; S2. Clean the inner wall of the helmet shell to remove dust and impurities; S3, spraying a transparent varnish layer on the inner wall of the helmet shell; S4, applying decorative materials on the varnish layer; S5, spraying a transparent varnish layer again to fix the decorative material; S6. Allow the helmet to stand and dry and bake to allow the varnish to fully penetrate and solidify; S7. Grinding the inner wall of the helmet shell to obtain a flat and smooth surface; S8, clean the inner wall of the helmet shell again and spray the gold oil layer; S9, the helmet is allowed to stand and dry and bake again until the required hardness is reached; S10. Conduct quality inspection on the finished helmet shells and rework unqualified ones.
2. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S4, applying the decorative material on the varnish layer includes: Sprinkle glitter powder evenly on the inner wall of the helmet shell coated with a transparent varnish layer to form dense glittering spots.
3. A method for processing an inner helmet according to claim 2, It is characterized in that In step S4, before applying the flashing decorative material on the varnish layer, the process includes: Stick the water-based sticker with the designed pattern on the predetermined position of the inner wall of the helmet shell to absorb excess moisture.
4. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S6, the step of placing the helmet in a static state and performing a drying and baking process comprises: The helmet shell is placed at room temperature for a predetermined time, and then placed in an oven for a first drying and baking process, and the helmet shell is baked at a predetermined temperature for a predetermined time.
5. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S7, the grinding process of the inner wall of the helmet shell includes: Use sandpaper to manually smooth out any bumps or uneven areas on the inner wall of the helmet shell to make the surface smooth.
6. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S8, the step of cleaning the inner wall of the helmet shell again and spraying the gold oil layer comprises: Use an air gun and a brush to clean the inner wall of the helmet shell to ensure that no dust and impurities remain on the inner wall of the helmet shell; Use a spray gun to spray PU gold oil, making sure that the PU gold oil evenly covers the inner wall of the helmet shell.
7. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S9, the helmet is placed in a static state and dried and baked again, including: The helmet shell is placed at room temperature for a predetermined time, and then placed in the oven again for drying and baking. The helmet shell is baked at a predetermined temperature for a predetermined time or until the hardness of the varnish layer reaches Grade F.
8. The method for processing an internal flash helmet according to claim 1, It is characterized in that The following steps are also included: S11. Process the outer wall surface of the helmet shell that has passed the inspection to remove residual processing materials accidentally attached to the outer wall.
9. A method for processing an internal flash helmet according to claim 1, It is characterized in that In step S11, the outer wall surface of the helmet shell that has passed the inspection is processed, including: S11.
1. Use a pneumatic sander with pneumatic sandpaper to remove the gloss from the outer wall of the helmet shell and remove the residues initially; S11.
2. Use an air gun to blow away dust and grinding debris from the outer wall of the helmet shell; S11.
3. Place the shell in water containing detergent and use water-abrasive sandpaper to carefully polish it to remove the sandpaper marks on the outer wall of the helmet shell. S11.
4. After the helmet shell is dried, use a lint-free cotton towel dipped in water containing detergent to wipe the outer wall of the helmet shell again; S11.
5. Use a dust-removing cloth to wipe the outer wall of the helmet shell to remove any remaining dust and impurities. S11.
6. Spray a layer of varnish evenly on the outer wall of the helmet shell; S11.
7. Place the sprayed helmet shell in an oven and let it stand for a predetermined time, then bake the helmet shell at a predetermined temperature for a predetermined time, or until the hardness of the outer wall varnish layer reaches the F grade standard and then take it out; S11.
8. Conduct secondary quality inspection on the processed helmet shells, and rework the unqualified ones.
10. A helmet manufactured by the processing method according to any one of claims 1 to 9, It is characterized in that include: Helmet shell (1); A first transparent varnish layer (2) is attached to the inner wall of the helmet shell (1); A decorative material layer (3) attached to the inner side of the first transparent varnish layer (2); A second transparent varnish layer (4) attached to the inner side of the decorative material layer (3); The gold oil layer (5) is attached to the inner side of the second transparent varnish layer (4).