Double-layer oil-edge-free belt and press fitting process thereof
Through the double-layer oil-free belt design and pressing process, the cladding bending and sewing technology is used to solve the problems of easy wear and harmful oil-edge agent of traditional belts, improving the durability and aesthetics of the belt, ensuring the belt's Structural firmness and environmental protection.
Patent Information
- Application Number
- CN202411257455.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-09
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional oil-edged belts are prone to wear and fall off during use, and oil-edged belts may cause harm to human health and the environment. The structure is single, making it difficult to meet the strength and durability needs of modern consumers for high-quality belts.
It adopts a double-layer oil-free belt design, press-fitting through two-layer pressing parts, cladding is bent and stitched, combining glue and sewing technology to avoid the use of oil-edge agent and enhance the wear resistance and service life of the belt.
It effectively avoids the problem of belt cracking and layering, improves the durability and service life of the belt, and avoids the potential harm of oil-edged agent to the human body and the environment, ensuring the firm structure and aesthetics of the belt.
Smart Images

Figure CN119058215A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of belts, and in particular to a double-layer oil-free edge belt and a press-fitting process thereof. Background Art
[0002] At present, in the field of belt manufacturing, oil-coated belts occupy a large market share. Oil-coated belts are usually made of a single material or a simple multi-layer combination structure, and their manufacturing process is relatively traditional.
[0003] Traditional belts with oil edges are usually coated with oil edge agents to achieve the purpose of aesthetics and edge protection. However, this design with oil edges has some obvious defects. On the one hand, the oil edge agent is easy to wear and fall off during use, affecting the appearance and service life of the belt. On the other hand, the oil edge agent may cause certain harm to human health and the environment, especially under special conditions such as long-term contact or high temperature, and may release harmful substances.
[0004] In addition, the structure of traditional oil-side belts is relatively simple, and their strength and durability are often unable to meet the needs of modern consumers for high-quality belts. In terms of material combination, simpler gluing or stitching is usually used. The firmness of this combination is limited, and it is easy to have problems such as delamination and cracking during use. Therefore, it is necessary to design a double-layer oil-free edge belt and its pressing process to solve the above problems. Summary of the invention
[0005] The purpose of the present invention is to solve the shortcomings existing in the prior art, and proposes a double-layer oil-free edge belt and its pressing process. The belt is pressed by two layers of pressing parts, so that two coating layers are formed on the belt. There is no need to apply oil on the edge of the belt, thereby effectively avoiding the cracking of the belt and improving the wear resistance of the belt. At the same time, through the combination of gluing and sewing, it can further avoid the delamination and cracking of the belt during use, further improving the service life of the belt.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] A double-layer oil-free edge belt comprises two belt bodies, the two belt bodies are adhered to each other through a first adhesive layer, the two belt bodies are wrapped with a covering layer, both ends of the two covering layers are bent between the two belt bodies, the two covering layers are sewn to the corresponding belt bodies through a first needle and thread, and the adjacent sides of the two covering layers are adhered to each other through a second adhesive layer.
[0008] Preferably, the covering layer and the corresponding belt body form a press-fitted part, and the two press-fitted parts are sewn together by a second needle and thread.
[0009] The invention also includes a press-fitting process of a double-layer oil-free edge belt, the processing process comprising the following steps:
[0010] Prepare two belt bodies and two covering layers, wrap the two covering layers on the two belt bodies so that the covering layers are tightly attached to the three surfaces of the two belt bodies, then overlap the two unwrapped surfaces of the two belt bodies, bend the two sides of the covering layers into the space between the two belt bodies, sew the two belt bodies and the corresponding covering layers together with a first needle and thread, after sew- ing is completed, use glue to adhere the adjacent sides of the two belt bodies and the adjacent sides of the two covering layers together, and finally use a second needle and thread to sew the two pressed parts together.
[0011] Preferably, in the step of preparing materials, the selected coating layer needs to have flexibility, wear resistance and aesthetics, and the belt body needs to have strength and stability.
[0012] Preferably, when bonding two belts, the bonding surfaces of the two belts need to be cleaned to remove surface dust, oil and other impurities, and the adhesive is selected and evenly applied to the bonding surface of one of the belts. The other belt is covered on it and ensured to be aligned without bubbles. The bonded belts are pressurized using a pressure device for two minutes with a pressure of 100N. The coating layer and the belt are adhered together using the same magnification. The adhesive is an environmentally friendly polyurethane adhesive.
[0013] Preferably, both sides of the coating layer are pre-treated to make it easy to bend, and the two sides of the coating layer are bent between the corresponding belt bodies to ensure that the bending angle is accurate and the coating layer fits tightly with the belt body; a clamp or other fixing device is used to fix the bent coating layer on the belt body.
[0014] Preferably, a suitable needle and thread are selected, and sewing is performed from the junction of the covering layer and the belt body using a needle method, and the sewing stitch length and thread tension are uniform and consistent.
[0015] Preferably, the adjacent surfaces of the two coating layers are cleaned to remove surface impurities; a suitable adhesive is selected and evenly applied to the adjacent surfaces of the two coating layers; the adjacent surfaces of the two coating layers are bonded together to ensure alignment without bubble generation; and pressure equipment is used to pressurize the bonded coating layers.
[0016] Preferably, suture thread and needle method are selected to sew the two pressed parts at the edges. During the sew process, the stitch length and thread tension need to be uniform. The stitched belt is inspected to ensure that the suture quality meets the requirements. If necessary, repair or reinforcement is performed.
[0017] Preferably, the stitching method can be a lock stitch, a back stitch or a cross stitch. The lock stitch can make the stitching line fit closely to the edge of the material. In the back stitch process, a stitch is first sewed forward, then a stitch is sewed backward, and so on. The distance between each two stitches is kept at one millimeter. When sewed with a cross stitch, the stitches are cross-stitched at a certain angle, and the distance between the intersections is controlled at 0.5 millimeters. The color of the thread matches the color of the material to ensure the aesthetics of the belt.
[0018] The present invention has the following beneficial effects:
[0019] Compared with the prior art, the present invention designs the belt into two layers, and there is no need to apply oil edges on both sides of the belt, thereby avoiding the release of harmful substances by the oil edge agent, which may cause potential harm to human health and the environment. The belt is designed into two layers, and the two sides of the wrapping layer are bent between the two belt bodies for sewing. At the same time, the two layers of the belt are sewn together, so that the layers of the belt are tightly combined and the structure is firm, which greatly improves the durability of the belt and is not prone to problems such as delamination and cracking. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 A schematic diagram of the structure of a double-layer oil-free belt proposed by the present invention;
[0021] Figure 2 for Figure 1 Schematic diagram of the front structure;
[0022] In the figure: 1 belt body, 2 covering layer, 3 first adhesive layer. DETAILED DESCRIPTION
[0023] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0024] Reference Figure 1-2 A double-layer oil-free edge belt comprises two belt bodies 1, the two belt bodies 1 are adhered to each other through a first adhesive layer 3, the two belt bodies 1 are wrapped with a covering layer 2, the covering layer 2 is made of wear-resistant material, both ends of the two covering layers 2 are bent between the two belt bodies 1, the two covering layers 2 are sewn on the corresponding belt bodies 1 through a first needle and thread, the adjacent sides of the two covering layers 2 are adhered to each other through a second adhesive layer, the covering layer 2 and the corresponding belt body 1 constitute a press-fit part, and the two press-fit parts are sewn together through a second needle and thread. The process of the belt can be used for a punched pin buckle belt, a limit tooth belt with a strip groove, and a flat belt with a groove print.
[0025] The invention also includes a press-fitting process of a double-layer oil-free edge belt, the processing process comprising the following steps:
[0026] Prepare two belt bodies 1 and two covering layers 2, wrap the two covering layers 2 on the two belt bodies 1 so that the covering layers 2 are tightly attached to the three surfaces of the two belt bodies 1, then overlap the two unwrapped surfaces of the two belt bodies 1, bend the two sides of the covering layers 2 into the space between the two belt bodies 1, sew the two belt bodies 1 and the corresponding covering layers 2 together with a first needle and thread, after sew- ing, use glue to adhere the adjacent sides of the two belt bodies 1 and the adjacent sides of the two covering layers 2 together, and finally sew the two pressed parts together with a second needle and thread.
[0027] Among them, in the material preparation step, the selected coating layer 2 needs to be flexible, wear-resistant and beautiful, and the belt body 1 needs to have strength and stability. When bonding the two belt bodies 1, the bonding surfaces of the two belt bodies 1 need to be cleaned to remove surface dust, oil and other impurities, and the adhesive is selected to be evenly applied on the bonding surface of one of the belt bodies 1, and the other belt body 1 is covered on it and ensured to be aligned without bubbles. The bonded belt body 1 is pressurized using a pressure device for two minutes and a pressure of 100N. The coating layer 2 and the belt body 1 are adhered together using the same magnification, and the adhesive is an environmentally friendly polyurethane adhesive.
[0028] Among them, the bending step of the coating layer 2 includes pre-treating both sides of the coating layer 2 to make it easy to bend, and the plasticity of the coating layer 2 can be improved by heating, softening, etc.; bending both sides of the coating layer 2 to the corresponding belt body 1 to ensure that the bending angle is accurate and the coating layer 2 fits tightly with the belt body 1; using a clamp or other fixing device to fix the bent coating layer 2 on the belt body 1, selecting a suitable needle and thread, and starting from the junction of the coating layer 2 and the belt body 1, using a needle method to sew, and the sew stitch length and thread tension are uniform and consistent.
[0029] Among them, the adjacent surfaces of the two coating layers 2 are cleaned to remove surface impurities to improve the adhesion effect; a suitable adhesive is selected and evenly applied to the adjacent surfaces of the two coating layers 2; the adjacent surfaces of the two coating layers 2 are bonded together to ensure alignment and no bubbles are generated; a pressure device is used to pressurize the bonded coating layers 2, and suture threads and needles are selected to sew the two pressed parts at the edges. During the sew process, it is necessary to ensure that the stitch length and thread tension are uniform and consistent, avoid stitches that are too large or too small and threads that are loose or too tight, and check the stitched belt to ensure that the suture quality meets the requirements, and repair or reinforce it if necessary.
[0030] Among them, the suture stitch method can adopt the lock stitch method, back stitch method or cross stitch method. The lock stitch method can make the suture line fit closely to the edge of the material, effectively prevent the edge of the material from being untied, and enhance the firmness and durability of the belt. The spacing between each stitch is maintained at 0.2 mm, and the tension of the thread is controlled to cause slight deformation of the material but not affect the overall structure. In the suture process of the back stitch method, one stitch is first sewed forward, and then one stitch is returned, and this is repeated. The distance between each two stitches is maintained at one millimeter to ensure that the suture lines are evenly distributed and the tensile strength of the belt is improved. When sewed with the cross stitch method, the stitches are cross-stitched at a certain angle, and the distance between the intersections is controlled at 0.5 mm, which enhances the tensile and tear resistance of the belt. The color of the thread matches the color of the material to ensure the aesthetics of the belt.
[0031] The above are only preferred specific implementation modes of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solutions and inventive concepts of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A double-layer oil-free belt, comprising two belt bodies (1), characterized in that: The two belt bodies (1) are adhered to each other through a first adhesive layer (3), the two belt bodies (1) are each wrapped with a covering layer (2), both ends of the two covering layers (2) are bent between the two belt bodies (1), the two covering layers (2) are sewn to the corresponding belt bodies (1) through a first needle and thread, the adjacent sides of the two covering layers (2) are adhered to each other through a second adhesive layer, and the covering layer (2) is located on the upper side.
2. The press-fitting process of a double-layer oil-free edge belt according to claim 1 is characterized in that: The covering layer (2) and the corresponding belt body (1) form a pressed part, and the two pressed parts are sewn together by a second needle and thread.
3. A double-layer oil-free edge belt press-fitting process, characterized in that: The processing technology includes the following steps: Two belt bodies (1) and two covering layers (2) are prepared, and the two covering layers (2) are wrapped on the two belt bodies (1) so that the covering layers (2) are tightly attached to the three surfaces of the two belt bodies (1), and then the two unwrapped surfaces of the two belt bodies (1) are superimposed together, and the two sides of the covering layers (2) are bent into the space between the two belt bodies (1), and the two belt bodies (1) and the corresponding covering layers (2) are sewn together by a first needle and thread. After the sewing is completed, the adjacent sides of the two belt bodies (1) and the adjacent sides of the two covering layers (2) are adhered together by glue, and finally the two pressed parts are sewn together by a second needle and thread.
4. A double-layer oil-free edge belt press-fitting process according to claim 3, characterized in that: In the step of preparing materials, the selected coating layer (2) needs to have flexibility, wear resistance and aesthetics, and the belt body (1) needs to have strength and stability.
5. The double-layer oil-free edge belt press-fitting process according to claim 3 is characterized in that: When bonding two belt bodies (1), the bonding surfaces of the two belt bodies (1) need to be cleaned to remove surface dust, oil stains and other impurities, and adhesive is selected and evenly applied to the bonding surface of one of the belt bodies (1). The other belt body (1) is covered thereon and ensured to be aligned without bubbles. The bonded belt bodies (1) are pressurized using a pressure device for two minutes at a pressure of (100)N. The coating layer (2) and the belt body (1) are adhered together using the same magnification. The adhesive is an environmentally friendly polyurethane adhesive.
6. A double-layer oil-free edge belt press-fitting process according to claim 3, characterized in that: Pre-treat both sides of the coating layer (2) to make it easy to bend, and bend both sides of the coating layer (2) to the corresponding belt body (1), ensuring that the bending angle is accurate and the coating layer (2) and the belt body (1) are tightly fitted; and use a clamp or other fixing device to fix the bent coating layer (2) on the belt body (1).
7. A double-layer oil-free edge belt press-fitting process according to claim 3, characterized in that: Select appropriate needle and thread, and start sewing from the junction of the coating layer (2) and the belt body (1) with needle method, and the sewing stitch length and thread tension are uniform and consistent.
8. The double-layer oil-free edge belt press-fitting process according to claim 3 is characterized in that: The adjacent surfaces of the two coating layers (2) are cleaned to remove surface impurities; a suitable adhesive is selected and evenly applied to the adjacent surfaces of the two coating layers (2); the adjacent surfaces of the two coating layers (2) are bonded together to ensure alignment without the generation of bubbles; and a pressure device is used to pressurize the bonded coating layers (2).
9. A double-layer oil-free edge belt press-fitting process according to claim 7, characterized in that: Select the stitching thread and needle method to sew the two pressed parts at the edges. During the sew process, the stitch length and thread tension must be uniform. Check the stitched belt to ensure that the stitching quality meets the requirements. If necessary, repair or reinforce it.
10. A double-layer oil-free edge belt press-fitting process according to claim 9, characterized in that: The stitching method can be lock stitch, back stitch or cross stitch. The lock stitch can make the stitching line fit closely to the edge of the material. In the back stitch process, first sew one stitch forward, then one stitch backward, and repeat this process. The distance between each two stitches is kept at one millimeter. When cross stitching, the stitches are cross-stitched at a certain angle, and the distance between the intersections is controlled at (0). (5) mm. The color of the thread matches the color of the material to ensure the aesthetics of the belt.