T-shaped groove anode GaN MIS temperature sensor and preparation method thereof

By introducing an extremely thin insulating layer under the anode groove of the GaN MIS temperature sensor and designing a circular P-type GaN layer, the reliability problem of GaN HEMT devices under high temperature and high electrical stress is solved, the reverse leakage current is reduced, and the improvement of the improvement of The temperature sensitivity and reliability are achieved, and good compatibility integration with HEMT devices is achieved.

CN119063857AActive Publication Date: 2024-12-03XIDIAN UNIV

Patent Information

Application Number
CN202411160335.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-12-03
Estimated Expiration
2044-08-22

AI Technical Summary

Technical Problem

The existing GaN HEMT devices are ineffective under high temperature and high electrical stress conditions, and the existing temperature sensors lack effective reinforcement measures, resulting in excessive reverse leakage current, affecting the temperature measurement accuracy and device reliability.

Method used

A T-shaped groove anode GaN MIS temperature sensor is designed. By introducing an extremely thin first insulating layer under the anode groove, the interface state defects are passivated and the longitudinal dislocation of the epitaxial structure is reduced, and the thermal electron emission and direct tunneling are realized. The linear conduction mechanism reduces the reverse leakage current and depletes the two-dimensional electron gas as an equivalent resistance through the circular P-type GaN layer, further reducing the reverse leakage current.

Benefits of technology

It effectively reduces the reverse leakage current of GaN MIS temperature sensor, improves temperature sensitivity and reliability, makes it more stable to work in high temperature and high electrical stress environments, and is consistent with the structure of HEMT devices, suitable for high density integration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119063857A_ABST
    Figure CN119063857A_ABST
Patent Text Reader

Abstract

The invention discloses a T-shaped groove anode GaN MIS temperature sensor and a preparation method thereof. The sensor comprises a substrate layer; the nucleating layer, the buffer layer, the channel layer and the barrier layer are sequentially arranged on the substrate layer; the annular P-type GaN layer is located on the middle area of the barrier layer; the anode groove is located in a circular ring of the circular-ring-shaped P-type GaN layer and penetrates through the barrier layer to the interior of the channel layer; the ring-shaped cathode groove surrounds the ring-shaped P-type GaN layer, is spaced from the ring-shaped P-type GaN layer by a certain distance, and penetrates through the barrier layer to the interior of the channel layer; the first insulating layer is located on the barrier layer, the annular P-type GaN layer and the bottom and the side wall of the anode groove; the T-shaped groove anode in contact with the MIS is positioned in the anode groove and on the first insulating layer above the annular P-type GaN layer; the annular cathode is located in the annular cathode groove and on the first insulating layer around the annular cathode groove. The temperature sensor has high temperature sensitivity and reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of temperature sensors, and in particular relates to a T-shaped groove anode GaN MIS temperature sensor and a preparation method thereof. Background Art

[0002] In recent years, GaN HEMT devices are core devices for high-frequency power conversion applications. In recent years, they have been widely used in electric vehicles and new energy fields, but new applications have higher reliability requirements for GaN-based HEMT devices. With the widespread use of GaN HEMT devices in high-power and high-frequency applications, the demand for monitoring and controlling their operating environment has gradually increased. Temperature is one of the key factors affecting the performance and reliability of GaN HEMT power devices. Therefore, integrated GaN temperature sensors came into being.

[0003] By using GaN temperature sensors on the same GaN HEMT chip, not only can the complexity and cost of the system be reduced, but the response speed and measurement accuracy of the system can also be improved, thereby effectively monitoring and controlling the operating status of the GaN HEMT device and preventing the GaN HEMT device from failing due to operation at too high a temperature. Since the reverse current changes dramatically with temperature, this may cause problems in any sensing circuit that may be in use. Excessive leakage current in the temperature sensor diode will reduce the reliability of the circuit, and leakage paths entering high-impedance circuits will cause erroneous readings, so this must be considered in the device or circuit design.

[0004] However, due to the late start of the development of all-gallium nitride integrated circuits, there is little research on integrated temperature sensors, and there is still much room for improvement in temperature measurement performance. In addition, existing temperature sensing devices lack reinforcement measures to cope with high temperature and high electrical stress conditions. The reliability issue of GaN HEMT devices has not been well resolved. Summary of the invention

[0005] In order to solve the above problems existing in the prior art, the present invention provides a T-shaped groove anode GaN MIS temperature sensor and a preparation method. The technical problem to be solved by the present invention is achieved by the following technical solutions:

[0006] In a first aspect, an embodiment of the present invention provides a T-groove anode GaN MIS temperature sensor, the GaN MIS temperature sensor comprising:

[0007] A substrate layer; an AlN nucleation layer, an AlGaN buffer layer, a GaN channel layer and an AlGaN barrier layer sequentially arranged on the substrate layer;

[0008] A circular P-type GaN layer, located on the middle region of the AlGaN barrier layer;

[0009] an anode groove, located in the annular ring of the annular P-type GaN layer, and penetrating the AlGaN barrier layer to the GaN channel layer; wherein the depth of the anode groove is the thickness of the annular P-type GaN layer, the AlGaN barrier layer and a portion of the GaN channel layer;

[0010] An annular cathode groove surrounds the annular P-type GaN layer and is spaced a certain distance from the annular P-type GaN layer, and penetrates the AlGaN barrier layer to the GaN channel layer;

[0011] A first insulating layer is located on the AlGaN barrier layer, the annular P-type GaN layer, and the bottom and sidewall of the anode groove; wherein the first insulating layer is an insulating layer with a thickness of less than 10 nm;

[0012] A T-shaped groove anode in MIS contact is located on the first insulating layer in the anode groove and on the first insulating layer above the annular P-type GaN layer;

[0013] A circular annular cathode is located in the circular annular cathode groove and on the first insulating layer around the circular annular cathode groove;

[0014] Among them, the first insulating layer is introduced under the T-groove anode of the MIS contact, and the first insulating layer passivates the interface state defects of the anode groove, reduces the forward leakage related to the interface state, and at the same time, the anode groove reduces the forward leakage of the longitudinal dislocation of the epitaxial structure, so that the forward conduction of the GaN MIS temperature sensor has two mechanisms: thermal electron emission and direct tunneling. Since the conduction voltage drop of the thermal electron emission and direct tunneling models changes linearly with temperature under the temperature measurement current, and the linearity is close to the ideal value, it is ensured that the GaN MIS temperature sensor reduces the reverse leakage current under the forward conduction condition, the temperature sensitivity increases with the reduction of the reverse leakage current, and the reliability increases with the reduction of the reverse leakage current.

[0015] In one embodiment of the present invention, the thickness of the first insulating layer is 1 nm to 4 nm.

[0016] In one embodiment of the present invention, the material of the first insulating layer is AlN or Al2O3.

[0017] In one embodiment of the present invention, the GaN MIS temperature sensor further includes:

[0018] An isolation mesa, located at both ends of the device and penetrating the AlGaN barrier layer to the lower surface of the GaN channel layer;

[0019] a second insulating layer, located on the isolation table, the annular cathode, the T-groove anode of the MIS contact and the first insulating layer;

[0020] The first insulating layer is also located on the isolation table.

[0021] In one embodiment of the present invention, the thickness of the second insulating layer is 200 nm to 250 nm.

[0022] In one embodiment of the present invention, the material of the second insulating layer is SiN or SiO2.

[0023] In a second aspect, an embodiment of the present invention provides a method for preparing a T-groove anode GaN MIS temperature sensor, the method comprising:

[0024] Prepare an epitaxial wafer; the epitaxial wafer comprises, from bottom to top, a substrate layer, an AlN nucleation layer, an AlGaN buffer layer, a GaN channel layer, an AlGaN barrier layer and a P-type GaN layer;

[0025] Etching the P-type GaN layer at both ends of the device until the lower surface of the GaN channel layer is reached to form an isolation mesa;

[0026] A circular ring region is defined on the surface of the P-type GaN layer, and an area outside the circular ring region is etched downward, and the etching depth extends to the upper surface of the AlGaN barrier layer to form a circular ring P-type GaN layer;

[0027] The area in the annular ring of the annular P-type GaN layer is defined as an anode area, and the anode area is etched downwards to a depth extending into the GaN channel layer to form an anode groove;

[0028] Depositing a first insulating layer on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and the inside and sidewall of the anode groove; wherein the first insulating layer is an insulating layer with a thickness of less than 10 nm;

[0029] A cathode region is defined on the surface of the first insulating layer around the annular P-type GaN layer, and the cathode region is etched downwards to a depth extending into the GaN channel layer to form an annular cathode groove; wherein the cathode region is spaced a certain distance from the annular P-type GaN layer;

[0030] Depositing an ohmic metal on the first insulating layer in and around the annular cathode groove and performing annealing to form an ohmic contact annular cathode;

[0031] MIS metal is deposited on the first insulating layer in the anode groove and on the first insulating layer above the annular P-type GaN layer to form a T-shaped groove anode with MIS contact.

[0032] In one embodiment of the present invention, depositing a first insulating layer on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and inside and on the sidewall of the anode groove comprises:

[0033] A first insulating layer with a thickness of 1 nm to 4 nm is deposited on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and the inside and sidewall of the anode groove by using the ALD technology.

[0034] In one embodiment of the present invention, the preparation method further comprises:

[0035] A second insulating layer is deposited on the annular cathode, the MIS-contacted T-groove anode and the first insulating layer, and the anode region and the cathode region are photolithographically led out to form the MIS-contacted T-groove anode and the annular cathode.

[0036] In one embodiment of the present invention, depositing a second insulating layer on the annular cathode, the T-groove anode of the MIS contact and the first insulating layer comprises:

[0037] A second insulating layer with a thickness of 200 nm to 250 nm is deposited on the annular cathode, the T-groove anode of the MIS contact and the first insulating layer by using PECVD technology.

[0038] Beneficial effects of the present invention:

[0039] The T-groove anode GaN MIS temperature sensor proposed in the present invention innovatively introduces a first insulating layer under the T-groove anode of the MIS contact. The first insulating layer passivates the interface state defects of the anode groove, reduces the forward leakage related to the interface state, and at the same time, the anode groove reduces the forward leakage of the longitudinal dislocation of the epitaxial structure, so that the forward conduction of the GaN MIS temperature sensor has two mechanisms: thermal electron emission and direct tunneling. Since the conduction voltage drop of the thermal electron emission and direct tunneling models varies linearly with temperature under the temperature measurement current, and the linearity is close to the ideal value, it is ensured that the GaN MIS temperature sensor reduces the reverse leakage current under the forward conduction condition, the temperature sensitivity is improved as the reverse leakage current is reduced, and the reliability is improved as the reverse leakage current is reduced, thereby making the GaN The MIS temperature sensor works more stably in a high temperature and high electrical stress environment; the annular P-type GaN layer in the structure proposed by the present invention depletes the two-dimensional electron gas and can act as an equivalent resistor, further reducing the reverse leakage current and improving the temperature sensitivity and reliability; at the same time, the MIS barrier diode with a lateral structure of a 2DEG channel in the structure proposed by the present invention can be prepared on the same epitaxial wafer as a HEMT device based on the same structure. The temperature sensor has a simple structure and is consistent with the structure of the HEMT device. During integration, the temperature sensor can be well compatible and integrated with the HEMT device without additional processes, making the T-groove anode GaN MIS temperature sensor feasible for high-density integration.

[0040] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 It is a schematic diagram of the structure of an existing GaN Schottky temperature sensor;

[0042] Figure 2 It is a schematic diagram of the experimental results of the forward conduction IV curve of the existing structure;

[0043] Figure 3 It is a structural schematic diagram of a T-groove anode GaN MIS temperature sensor provided by an embodiment of the present invention;

[0044] Figure 4 Schematic diagram of the forward conduction IV curve experimental results of the structure proposed by the present invention;

[0045] Figure 5 It is a schematic flow chart of a method for preparing a T-groove anode GaN MIS temperature sensor provided by an embodiment of the present invention;

[0046] Figure 6(a) to Figure 6(i) It is a schematic diagram of the structure corresponding to the preparation process of the T-groove anode GaN MIS temperature sensor provided in an embodiment of the present invention.

[0047] Description of reference numerals:

[0048] 1-substrate layer; 2-AlN nucleation layer; 3-AlGaN buffer layer; 4-GaN channel layer; 5-AlGaN barrier layer; 6-P-type GaN layer; 7-first insulating layer; 8-annular cathode; 9-MIS contacted T-groove anode; 10-second insulating layer. DETAILED DESCRIPTION

[0049] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.

[0050] Figure 1 The present invention illustrates an existing GaN Schottky temperature sensor. Although the measurement accuracy of GaN heterojunction temperature is improved and the sensor has certain advantages of high linearity, low on-state voltage and low reverse leakage current, the inventors found in the experiment that the forward conduction IV curve of the existing structure has a turning point such as Figure 2 In the area marked by the blue dotted circle in the middle, a platform will appear in the test, which will seriously affect the range of the temperature measurement current. If there is no such platform, a lower reverse leakage current can be used to obtain a greater temperature sensitivity; at the same time, there is the problem of the inherent large reverse leakage current of the Schottky diode, such as the area marked by the red dotted circle in 2. The final test results are: Figure 1 The temperature sensitivity of the structure shown is 5.32mV / K and the linearity is 0.98293. Figure 2 Where Ra is the radius of the annular cathode, Lac is the distance between the cathode and the anode, 25 to 200 is the temperature, and J is the magnitude of the measured current. Figure 2 The horizontal axis represents the reverse leakage current Current, in amperes A, and the horizontal axis represents the forward conduction voltage Voltage, in V.

[0051] Based on the above research, the inventor innovatively proposed a T-groove anode GaN MIS temperature sensor and a preparation method, specifically:

[0052] First, see Figure 3 , an embodiment of the present invention provides a T-shaped groove anode GaN MIS temperature sensor, the GaN MIS temperature sensor comprising:

[0053] A substrate layer 1; an AlN nucleation layer 2, an AlGaN buffer layer 3, a GaN channel layer 4 and an AlGaN barrier layer 5 sequentially arranged on the substrate layer 1;

[0054] A circular P-type GaN layer 6 is located on the middle region of the AlGaN barrier layer 5;

[0055] The anode groove is located in the annular P-type GaN layer 6 and penetrates the AlGaN barrier layer 5 to the GaN channel layer 4; wherein the depth of the anode groove is the thickness of the annular P-type GaN layer 6, the AlGaN barrier layer 5 and a part of the GaN channel layer 4;

[0056] The annular cathode groove surrounds the annular P-type GaN layer 6 and is spaced a certain distance from the annular P-type GaN layer 6, and penetrates the AlGaN barrier layer 5 to the GaN channel layer 4;

[0057] A first insulating layer 7 is located on the AlGaN barrier layer 5, the annular P-type GaN layer 6, and the bottom and sidewall of the anode groove; wherein the first insulating layer 7 is an insulating layer with a thickness of less than 10 nm;

[0058] The MIS-contacted T-shaped groove anode 9 is located on the first insulating layer 7 in the anode groove and on the first insulating layer 7 above the annular P-type GaN layer 6;

[0059] The annular cathode 8 is located in the groove of the annular cathode 8 and on the first insulating layer 7 around the groove of the annular cathode 8 .

[0060] In an embodiment of the present invention, the GaN MIS temperature sensor further includes:

[0061] Isolation mesas, located at both ends of the device and penetrating the AlGaN barrier layer 5 to the lower surface of the GaN channel layer 4;

[0062] A second insulating layer 10 is located on the isolation table, the annular cathode 8, the MIS-contacted T-groove anode 9 and the first insulating layer 7;

[0063] The first insulating layer 7 is also located on the isolation table.

[0064] In the embodiment of the present invention, the substrate layer 1 may be a P-type silicon material with a (1, 1, 1) crystal orientation.

[0065] In an embodiment of the present invention, the AlN nucleation layer 2 includes a low-temperature AlN nucleation layer 2 and a high-temperature AlN nucleation layer 2, the thickness of the low-temperature AlN nucleation layer 2 may be 30 nm, and the thickness of the high-temperature AlN nucleation layer 2 may be 170 nm; the thickness of the AlGaN buffer layer 3 may be 5 μm; the thickness of the GaN channel layer 4 may be 200 nm; the thickness of the AlGaN barrier layer 5 may be 15 nm; the thickness of the annular P-type GaN layer 6 may be 70 nm and the width of the annular ring may be 10 μm.

[0066] In the embodiment of the present invention, the thickness of the first insulating layer 7 is 1 nm to 4 nm; the material of the first insulating layer 7 is AlN or Al2O3.

[0067] In the embodiment of the present invention, the thickness of the second insulating layer 10 is 200 nm to 250 nm; the material of the second insulating layer 10 is SiN or SiO2.

[0068] In the embodiment of the present invention, the MIS-contacted T-groove anode 9 is an anode MIS contact metal, which may include Ti, Al and Au. The radius of the anode MIS contact metal in the anode groove is 35 μm.

[0069] In the embodiment of the present invention, the annular cathode 8 is an ohmic cathode metal, which may include Ti, Al, Ni and Au. The interval between the annular cathode 8 and the annular P-type GaN layer 6 is 25 μm to 35 μm; the width of the annular cathode 8 is 10 μm.

[0070] The first insulating layer 7 in the embodiment of the present invention is the insulating layer in the metal-insulating layer-semiconductor MIS structure. This insulating layer is different from the insulating layer in the MOS structure. The role of the insulating layer in the MOS structure is electrical isolation, preventing leakage current and improving reliability. The gate voltage can be used to control the channel opening and closing. Usually, the MIS structure is not used in the diode, because the insulating layer in the normal MIS structure needs to be tens to hundreds of nanometers for isolation, and the diode needs to be forward-conducted, and generally no insulating layer is added in the anode groove. In the embodiment of the present invention, the leakage of the anode groove side is the main leakage path. An extremely thin insulating layer is introduced into the T-shaped groove anode of the MIS contact, and the thickness is required to be less than 10nm. Its role is completely different from the existing insulating layer in the anode area. In the structure of the present invention, the first insulating layer 7 can be regarded as a Schottky contact in the metal-semiconductor contact type, which is equivalent to increasing the height of the Schottky barrier, while increasing the on-resistance, and passivating a large number of interface state defects generated when etching the anode groove, reducing the reverse leakage current while ensuring forward conduction, and improving the reliability of the MIS structure diode under high temperature and high electrical stress.

[0071] The forward conduction mechanism of the embodiment of the present invention mainly includes thermionic emission generated by crossing the Schottky barrier, and direct tunneling generated by the Schottky barrier. The groove and passivation reduce the conduction mechanism related to dislocation and interface state defects. Since the conduction voltage drop of the thermal electron emission and direct tunneling models changes linearly with temperature under the temperature measurement current, the linearity of the temperature measurement of the general Schottky diode has not degraded, and the linearity is close to the ideal value, and the ideal linearity is 1.0. This structure will affect the forward characteristics of diodes outside the field of temperature sensors, bringing very low reverse leakage current, but this point not only improves the forward temperature sensitivity of the temperature sensor, but also greatly reduces the reverse leakage current and improves reliability. In general, the structure proposed by the present invention utilizes the MIS structure that is not commonly used for diodes, because such a structure brings very low reverse leakage current and loses forward characteristics, so the diode of the MIS structure is a compromise choice in specific cases, and the sensitivity in the field of temperature sensors decreases with the forward current, and the sensitivity increases, so the MIS structure is no longer a compromise but a two-way optimization, which has great advantages.

[0072] In order to verify the effectiveness of the T-shaped groove anode GaN MIS temperature sensor provided by the embodiment of the present invention, the following Figure 1 The same structural parameters were used for the experiment. The experimental results are shown in Figure 4 As shown, from Figure 4 It can be seen that the forward conduction IV curve of the structure proposed in the present invention does not exist as Figure 2 Platform issues are outlined in blue dashed circles and have Figure 1 The reverse leakage current of the existing structure is lower, even lower by at least three orders of magnitude. In general, the structure proposed by the present invention solves the problem well. Figure 1 The problems of the existing structure shown. The final test results are: Figure 3 The temperature sensitivity of the structure proposed by the present invention is 3.33mV / K, and the linearity is 0.99724. The lower the temperature sensitivity value, the better, and the closer the linearity value is to 1, the better. Both indicators of the present invention are greatly improved.

[0073] In summary, the T-groove anode GaN MIS temperature sensor proposed in the embodiment of the present invention innovatively introduces a first insulating layer 7 under the T-groove anode 9 of the MIS contact. The first insulating layer 7 passivates the interface state defects of the anode groove, reduces the forward leakage related to the interface state, and at the same time, the anode groove reduces the forward leakage of the longitudinal dislocation of the epitaxial structure, so that the forward conduction of the GaN MIS temperature sensor has two mechanisms: thermal electron emission and direct tunneling. Since the conduction voltage drop of the thermal electron emission and direct tunneling models varies linearly with temperature under the temperature measurement current, and the linearity is close to the ideal value, it is ensured that the GaN MIS temperature sensor reduces the reverse leakage current under the forward conduction condition, the temperature sensitivity is improved as the reverse leakage current is reduced, and the reliability is improved as the reverse leakage current is reduced, thereby making the GaN The MIS temperature sensor works more stably in a high temperature and high electrical stress environment; the annular P-type GaN layer 6 in the structure proposed by the present invention depletes the two-dimensional electron gas and can act as an equivalent resistor, further reducing the reverse leakage current and improving the temperature sensitivity and reliability; at the same time, the MIS barrier diode with a lateral structure of a 2DEG channel in the structure proposed by the present invention can be prepared on the same epitaxial wafer as a HEMT device based on the same structure. The temperature sensor has a simple structure and is consistent with the structure of the HEMT device. During integration, the temperature sensor can be well compatible and integrated with the HEMT device without additional processes, making the T-groove anode GaN MIS temperature sensor feasible for high-density integration.

[0074] Second, see Figure 5 The embodiment of the present invention provides a method for preparing a T-shaped groove anode GaN MIS temperature sensor, the preparation method comprising:

[0075] S10, preparing an epitaxial wafer; the epitaxial wafer includes, from bottom to top, a substrate layer 1, an AlN nucleation layer 2, an AlGaN buffer layer 3, a GaN channel layer 4, an AlGaN barrier layer 5 and a P-type GaN layer.

[0076] In the embodiment of the present invention, a low-temperature AlN nucleation layer 2 is first epitaxially grown on the upper surface of a Si material substrate layer 1 using a MOCVD (Metal-organic Chemical Vapor Deposition) technique, and then a high-temperature AlN nucleation layer 2 is epitaxially grown on the upper surface of the low-temperature AlN nucleation layer 2. The low-temperature AlN nucleation layer 2 and the high-temperature AlN nucleation layer 2 together constitute an AlN nucleation layer 2; the thickness of the low-temperature AlN nucleation layer 2 may be 30 nm, and the thickness of the high-temperature AlN nucleation layer 2 may be 170 nm.

[0077] After the AlN nucleation layer 2 is prepared, an AlGaN buffer layer 3 with a thickness of 5 μm is deposited on the AlN nucleation layer 2 by MOCVD. For example, undoped Al is deposited on the upper surface of the nucleation layer by using trimethylaluminum as an aluminum source, trimethylgallium as a gallium source, and ammonia as an ammonia source. 0.3 Ga 0.7 N buffer layer, the thickness of the buffer layer may be 5 μm.

[0078] After the AlGaN buffer layer 3 is prepared, a GaN channel layer 4 with a thickness of 200 nm is deposited on the AlGaN buffer layer 3 using MOCVD. For example, trimethylgallium is used as a gallium source and ammonia is used as an ammonia source. An undoped GaN channel layer 4 is deposited on the upper surface of the buffer layer using MOCVD technology. The thickness of the GaN channel layer 4 can be 200 nm.

[0079] After the GaN channel layer 4 is prepared, an AlGaN barrier layer 5 with a thickness of 15 nm is deposited on the GaN channel layer 4 using MOCVD. For example, trimethylgallium is used as a gallium source, trimethylaluminum is used as an aluminum source, and ammonia is used as an ammonia source. Undoped Al is deposited on the upper surface of the GaN channel layer 4 using MOCVD technology. 0.2 Ga 0.8 The thickness of the N barrier layer, the AlGaN barrier layer 5 is 15 nm.

[0080] After the AlGaN barrier layer 5 is prepared, a P-type GaN layer with a thickness of 70 nm is epitaxially grown on the AlGaN barrier layer 5 using the MOCVD technology. For example, a P-type GaN layer with a thickness of 70 nm and a doping concentration of 10 Mg+ ions is epitaxially grown on the AlGaN barrier layer 5 using the MOCVD technology. 19 cm -3 The GaN layer is formed by high temperature annealing to form a P-type GaN layer. Finally, the structure shown in Figure 6(a) is formed.

[0081] S20, etching the P-type GaN layer at both ends of the device until the lower surface of the GaN channel layer 4 is reached to form an isolation mesa.

[0082] The embodiment of the present invention utilizes an ICP (Inductively Coupled Plasma) etching process to etch the P-type GaN layer at both ends of the device in FIG. 6( a ) until the lower surface of the GaN channel layer 4 , forming an isolation mesa as shown in FIG. 6( b ).

[0083] S30 , defining a circular ring-shaped region on the surface of the P-type GaN layer, and etching downwards the region outside the circular ring-shaped region, with the etching depth extending to the upper surface of the AlGaN barrier layer 5 , to form a circular ring-shaped P-type GaN layer 6 .

[0084] In the embodiment of the present invention, Si3N4 is deposited on the surface of the prepared device shown in 6(b) for passivation to form a Si3N4 passivation layer, and the Si3N4 layer deposited on the surface of the P-type GaN layer is removed by a hydrogen ion wet method to introduce hydrogen ions into the P-type GaN layer; a photoresist is spin-coated on the Si3N4 passivation layer to define a first annular area and exposed and developed, the Si3N4 passivation layer is wet-removed by a BHF (Buffered Hydrofluoric Acid) solution, and the P-type GaN layer outside the annular area is etched downward, and the etching depth extends to the upper surface of the AlGaN barrier layer 5, to form an annular P-type GaN layer 6 as shown in FIG6(c), and the annular width of the annular P-type GaN layer 6 is 10 μm. Among them, the BHF solution is prepared by mixing 6 volumes of ammonium fluoride (NH4F, 40% solution) and 1 volume of hydrofluoric acid (HF). Diluting it in water at a ratio of 7:1 before use can better control the etching rate. By removing the Si3N4 passivation layer by wet method, the defect states in the P-type GaN layer can be passivated.

[0085] S40 , defining the area inside the annular P-type GaN layer 6 as an anode area, etching the anode area downwards, and extending the etching depth into the GaN channel layer 4 to form an anode groove.

[0086] In the embodiment of the present invention, the area within the circular ring of the annular P-type GaN layer 6 is defined as the anode area, that is, the diameter of the circular ring-shaped P-type GaN layer 6 is used as the width of the anode groove. The anode area is etched downward using the ICP etching process, and the etching depth extends to the GaN channel layer 4 to form an anode groove as shown in Figure 6(d). The radius of the anode groove is 35μm.

[0087] S50, depositing a first insulating layer 7 on the isolation mesa, the AlGaN barrier layer 5, the annular P-type GaN layer 6, and the inside and side walls of the anode groove; wherein the first insulating layer 7 is an insulating layer with a thickness of less than 10 nm.

[0088] The embodiment of the present invention utilizes ALD (Atomic Layer Deposition) technology to deposit a first insulating layer 7 on the isolation table, the AlGaN barrier layer 5, the annular P-type GaN layer 6, and the inside and side walls of the anode groove as shown in Figure 6(e). For example, using trimethylaluminum as the aluminum source and ozone as the oxygen source, the ALD technology is utilized to deposit a first insulating layer 7 of AlN or Al2O3 with a thickness of 1nm to 4nm on the isolation table, the AlGaN barrier layer 5, the annular P-type GaN layer 6, and the inside and side walls of the anode groove.

[0089] S60, defining a cathode region on the surface of the first insulating layer 7 surrounding the annular P-type GaN layer 6, etching the cathode region downwards, with the etching depth extending into the GaN channel layer 4, to form an annular cathode 8 groove; wherein the cathode region is spaced a certain distance from the annular P-type GaN layer 6.

[0090] In the embodiment of the present invention, a photoresist is spin-coated on the first insulating layer 7 to define the cathode region, and then exposed and developed. The cathode region is etched downward using an ICP etching process, and the etching depth extends into the GaN channel layer 4 to form a circular cathode 8 groove as shown in FIG6(f). The cathode region is spaced a certain distance from the circular P-type GaN layer 6, for example, the cathode region is spaced 25 μm to 35 μm from the circular P-type GaN layer 6; the radius of the cathode region is 10 μm.

[0091] S70, depositing an ohmic metal on the first insulating layer 7 in the groove of the annular cathode 8 and around the groove of the annular cathode 8 and performing high temperature annealing to form an ohmic contact annular cathode 8.

[0092] In the embodiment of the present invention, the PVD (Physical Vapor Deposition) technology is used to sputter Ti, Al, Ni and Au metals from bottom to top in the groove of the annular cathode 8 to prepare the annular cathode 8 with ohmic contact, and the thickness of each metal layer is 20nm, 140nm, 50nm and 30nm respectively; the metal of the annular cathode 8 formed by sputtering is subjected to rapid thermal annealing for 35s in a N2 atmosphere at a temperature of 865°C to complete the preparation of the annular cathode 8 with ohmic contact as shown in Figure 6(g).

[0093] S80 , depositing MIS metal on the first insulating layer 7 in the anode groove and on the first insulating layer 7 above the annular P-type GaN layer 6 to form a T-shaped groove anode 9 with MIS contact.

[0094] In the embodiment of the present invention, the PVD technology is used to sputter Ti, Al and Au metals from bottom to top in the anode groove to prepare a MIS contact T-groove anode, and the thickness of each metal layer is 20nm, 250nm and 30nm respectively. The T-groove anode metal with MIS contact formed by sputtering is annealed in N2 atmosphere at 450°C for 300s to complete the preparation of the T-groove anode with MIS contact as shown in Figure 6(h).

[0095] Furthermore, the preparation method of the embodiment of the present invention also includes:

[0096] A second insulating layer 10 is deposited on the annular cathode 8, the MIS-contacted T-groove anode 9 and the first insulating layer 7, and the anode region and the cathode region are photolithographically led out to the MIS-contacted T-groove anode 9 and the annular cathode 8. Specifically: using PECVD (Plasma Enhanced Chemical Vapor Deposition, plasma enhanced chemical vapor deposition) technology, a second insulating layer 10 of SiN or SiO2 with a thickness of 200nm to 250nm is deposited on the annular cathode 8, the MIS-contacted T-groove anode 9 and the first insulating layer 7 as shown in Figure 6(i). Contact holes are opened by photolithography in the cathode region and the anode region, and electrodes are led out to finally complete the preparation of the entire T-groove anode GaN MIS temperature sensor.

[0097] As for the method embodiment of the second aspect, since it is basically similar to the structural embodiment of the first aspect, the description is relatively simple, and the relevant parts may refer to the partial description of the structural embodiment of the first aspect.

[0098] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0099] Although the present invention is described herein in conjunction with various embodiments, in the process of implementing the claimed invention, those skilled in the art may understand and implement other variations of the disclosed embodiments by viewing the specification and its drawings. In the specification, the word "comprising" does not exclude other components or steps, and "a" or "one" does not exclude multiple situations. Certain measures are recorded in different embodiments, but this does not mean that these measures cannot be combined to produce good results.

[0100] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.

Claims

1. A T-groove anode GaN MIS temperature sensor, It is characterized in that The GaN MIS temperature sensor comprises: A substrate layer; an AlN nucleation layer, an AlGaN buffer layer, a GaN channel layer and an AlGaN barrier layer sequentially arranged on the substrate layer; A circular P-type GaN layer, located on the middle region of the AlGaN barrier layer; an anode groove, located in the annular ring of the annular P-type GaN layer, and penetrating the AlGaN barrier layer to the GaN channel layer; wherein the depth of the anode groove is the thickness of the annular P-type GaN layer, the AlGaN barrier layer and a portion of the GaN channel layer; An annular cathode groove surrounds the annular P-type GaN layer and is spaced a certain distance from the annular P-type GaN layer, and penetrates the AlGaN barrier layer to the GaN channel layer; A first insulating layer is located on the AlGaN barrier layer, the annular P-type GaN layer, and the bottom and sidewall of the anode groove; wherein the first insulating layer is an insulating layer with a thickness of less than 10 nm; A T-shaped groove anode in MIS contact is located on the first insulating layer in the anode groove and on the first insulating layer above the annular P-type GaN layer; A circular annular cathode is located in the circular annular cathode groove and on the first insulating layer around the circular annular cathode groove; Among them, the first insulating layer is introduced under the T-groove anode of the MIS contact, and the first insulating layer passivates the interface state defects of the anode groove, reduces the forward leakage related to the interface state, and at the same time, the anode groove reduces the forward leakage of the longitudinal dislocation of the epitaxial structure, so that the forward conduction of the GaN MIS temperature sensor has two mechanisms: thermal electron emission and direct tunneling. Since the conduction voltage drop of the thermal electron emission and direct tunneling models changes linearly with temperature under the temperature measurement current, and the linearity is close to the ideal value, it is ensured that the GaN MIS temperature sensor reduces the reverse leakage current under the forward conduction condition, the temperature sensitivity increases with the reduction of the reverse leakage current, and the reliability increases with the reduction of the reverse leakage current.

2. The T-groove anode GaN MIS temperature sensor according to claim 1, It is characterized in that The thickness of the first insulating layer is 1 nm to 4 nm.

3. The T-groove anode GaN MIS temperature sensor according to claim 1, It is characterized in that The material of the first insulating layer is AlN or Al 2 O 3 .

4. The T-groove anode GaN MIS temperature sensor according to claim 1, It is characterized in that The GaN MIS temperature sensor further comprises: An isolation mesa, located at both ends of the device and penetrating the AlGaN barrier layer to the lower surface of the GaN channel layer; a second insulating layer, located on the isolation table, the annular cathode, the T-groove anode of the MIS contact and the first insulating layer; The first insulating layer is also located on the isolation table.

5. The T-groove anode GaN MIS temperature sensor according to claim 4, It is characterized in that The thickness of the second insulating layer is 200 nm to 250 nm.

6. The T-groove anode GaN MIS temperature sensor according to claim 4, It is characterized in that The material of the second insulating layer is SiN or SiO 2 .

7. A method for preparing a T-groove anode GaN MIS temperature sensor, It is characterized in that The preparation method comprises: Prepare an epitaxial wafer; the epitaxial wafer comprises, from bottom to top, a substrate layer, an AlN nucleation layer, an AlGaN buffer layer, a GaN channel layer, an AlGaN barrier layer and a P-type GaN layer; Etching the P-type GaN layer at both ends of the device until the lower surface of the GaN channel layer is reached to form an isolation mesa; A circular ring region is defined on the surface of the P-type GaN layer, and an area outside the circular ring region is etched downward, and the etching depth extends to the upper surface of the AlGaN barrier layer to form a circular ring P-type GaN layer; The area in the annular ring of the annular P-type GaN layer is defined as an anode area, and the anode area is etched downwards to a depth extending into the GaN channel layer to form an anode groove; Depositing a first insulating layer on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and the inside and sidewall of the anode groove; wherein the first insulating layer is an insulating layer with a thickness of less than 10 nm; A cathode region is defined on the surface of the first insulating layer around the annular P-type GaN layer, and the cathode region is etched downwards to a depth extending into the GaN channel layer to form an annular cathode groove; wherein the cathode region is spaced a certain distance from the annular P-type GaN layer; Depositing an ohmic metal on the first insulating layer in and around the annular cathode groove and performing annealing to form an ohmic contact annular cathode; MIS metal is deposited on the first insulating layer in the anode groove and on the first insulating layer above the annular P-type GaN layer to form a T-shaped groove anode with MIS contact.

8. The method for preparing the T-groove anode GaN MIS temperature sensor according to claim 7, It is characterized in that Depositing a first insulating layer on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and inside and on the sidewall of the anode groove, comprising: A first insulating layer with a thickness of 1 nm to 4 nm is deposited on the isolation mesa, the AlGaN barrier layer, the annular P-type GaN layer, and the inside and sidewall of the anode groove by using the ALD technology.

9. The method for preparing the T-groove anode GaN MIS temperature sensor according to claim 7, It is characterized in that The preparation method further comprises: A second insulating layer is deposited on the annular cathode, the MIS-contacted T-groove anode and the first insulating layer, and the anode region and the cathode region are photolithographically led out to form the MIS-contacted T-groove anode and the annular cathode.

10. The method for preparing the T-groove anode GaN MIS temperature sensor according to claim 9, It is characterized in that Depositing a second insulating layer on the annular cathode, the T-groove anode of the MIS contact and the first insulating layer comprises: A second insulating layer with a thickness of 200 nm to 250 nm is deposited on the annular cathode, the T-groove anode of the MIS contact and the first insulating layer by using PECVD technology.

Citation Information

Patent Citations

  • Enhanced fin-type insulated gate high-electronic mobility transistor

    CN105810728A

  • GaN-based double-layer passivation groove gate enhanced MIS-HEMT device and preparation method thereof

    CN114823891A

  • Double-layer passivation depletion type MIS-HEMT device and preparation method thereof

    CN114937597A

  • T-type anode GaN Schottky temperature sensor and preparation method thereof

    CN117367611A

  • GaN intelligent power chip with junction temperature monitoring capability and preparation method thereof

    CN118156302A

Cited By

  • CZT detection device and detection method based on gradient annular cathode

    CN122430887A

  • CzT detection device based on gradient ring cathode and detection method

    CN122430887B