Formation method of air gap isolation structure

By etching the prefilled layer and the low-temperature oxide layer in the semiconductor structure to form through holes, and then using the CVD process to seal it, the problem of high trench etching requirements in traditional processes is solved, and the uniformity and isolation effect of the air gap are improved.

CN119069424APending Publication Date: 2024-12-03SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411146959.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The traditional air gap isolation formation process has high requirements for the trench etching process, resulting in the inclination of the side wall of the trench, resulting in the accumulation of reactants, filling the dielectric material, and reducing the uniformity of the air gap morphology and isolation effect.

Method used

In the semiconductor structure, a gap trench is first formed, the prefilled layer is not higher than the surface of the dielectric layer, a low-temperature oxide layer is formed and the through holes is etched to form through holes, the photoresist layer is removed, and the through holes are sealed using the CVD deposition process to form an air gap. Isolation structure.

Benefits of technology

The requirements for trench etching process are reduced, the spatial size, uniformity and controllability of the air gap are improved, and the isolation effect is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069424A_ABST
    Figure CN119069424A_ABST
Patent Text Reader

Abstract

The invention provides a method for forming an air gap isolation structure, and the method comprises the steps: providing a semiconductor structure which comprises a dielectric layer and metal interconnection wires which are formed in the dielectric layer and are distributed at intervals; etching the dielectric layer between the metal interconnection wires to form gap grooves; forming a pre-filling layer in the gap groove, wherein the surface of the pre-filling layer is not higher than the surface of the dielectric layer; forming a low-temperature oxide layer on the surface of the semiconductor structure filled with the pre-filling layer; etching the low-temperature oxide layer formed on the surface of the pre-filling layer to form a through hole; removing the photoresist layer; and forming a film layer in the through hole by using a CVD deposition process, and enabling the film layer to block the bottom end of the through hole so that the gap groove is not filled to form an air gap isolation structure. According to the invention, the problem that the existing air gap forming process has high requirements on the groove etching process is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a method for forming an air gap isolation structure. Background Art

[0002] In an integrated circuit, thousands of transistors are connected by wires. With the development of integrated circuit technology, the size of devices continues to shrink, and the integration of device units per unit area becomes higher and higher, which leads to smaller and smaller spacing between wires and more significant coupling capacitance between wires. All these increase the RC delay between interconnection layers, that is, the useless power consumption in the circuit increases, which hinders the further improvement of the performance of integrated circuit devices.

[0003] Since the size of the equivalent capacitance C in the RC delay is proportional to the dielectric constant k of the medium between the wires, the use of an interconnect medium with a low dielectric constant can reduce the equivalent capacitance and reduce the RC delay effect, thereby improving the performance of integrated circuit devices. This technology is particularly critical for semiconductor devices with high operating efficiency and low power consumption requirements.

[0004] There are many ways to reduce the dielectric k value. The most common method is to make it a porous material with tiny bubbles by doping. More voids mean a lower k value. Since the lowest limit of the k value is 1 (i.e. vacuum), the ultimate way to reduce the k value is to seal an air bubble between two wires to replace the original solid dielectric material, so that the corresponding k value is as close to 1 as possible. This technology is called air-gap technology.

[0005] To form an air-gap structure, a CVD process with poor step coverage and fast lateral growth rate is usually used to quickly pinch off and seal the gaps between the wires, so that the air is retained. The traditional air gap isolation formation process relies on a dry etching process to form a groove with smooth sidewalls and perpendicular to the substrate, and then a CVD process with poor step coverage and fast lateral growth rate is used to quickly pinch off and seal the groove. However, in actual applications, such traditional processes still have the following problems:

[0006] The step coverage of the CVD process is highly dependent on the groove morphology. When the groove sidewalls are completely perpendicular to the substrate, the reactants are more likely to accumulate at the groove mouth due to the different arrival angles of the reactants, and at the same time, subsequent reactants are prevented from continuing to enter the groove, thereby achieving the purpose of quickly forming a pinch-off seal for the groove. However, the actual situation is that the sidewalls of the grooves after the etching process, especially near the groove mouth, often have a certain inclination angle. The through hole at the top of the inclined groove is larger than the bottom. Compared with the groove with completely vertical sidewalls, the reactants have a higher probability of entering the groove and reacting to form a film. Even if the step coverage of the CVD process is adjusted to an extremely poor level, the bottom of the groove will still be partially filled with dielectric material (i.e., thin film) (such as Figure 1 As shown in FIG. 1 , the cross-sectional area of ​​the air gap is reduced, the uniformity of the gap morphology is difficult to control, and the isolation effect is correspondingly reduced. At the same time, the inclined sidewalls also make it difficult to quickly pinch off the trench through hole. Summary of the invention

[0007] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a method for forming an air gap isolation structure, so as to solve the problem that the existing air gap formation process has high requirements on the trench etching process.

[0008] To achieve the above objectives and other related objectives, the present invention provides a method for forming an air gap isolation structure, the method comprising:

[0009] A semiconductor structure is provided, comprising a dielectric layer and metal interconnect wires formed in the dielectric layer and arranged at intervals;

[0010] Etching the dielectric layer between the metal interconnect wires to form gap trenches;

[0011] forming a pre-filling layer in the gap trench, wherein the surface of the pre-filling layer is not higher than the surface of the dielectric layer;

[0012] forming a low temperature oxide layer on the surface of the semiconductor structure filled with the pre-filled layer;

[0013] Etching the low temperature oxide layer formed on the surface of the pre-fill layer until the pre-fill layer is exposed to form a through hole, wherein the bottom opening of the through hole is smaller than the surface width of the pre-fill layer;

[0014] removing the photoresist layer;

[0015] A film layer is formed in the through hole by using a CVD deposition process, wherein the film layer blocks the bottom end of the through hole so that the gap trench is not filled to form an air gap isolation structure.

[0016] Optionally, the material of the pre-filled layer includes photoresist.

[0017] Optionally, when the material of the pre-filled layer is photoresist, the temperature used when forming the low-temperature oxide layer is less than 80°.

[0018] Optionally, the material of the low temperature oxidation layer includes silicon oxide.

[0019] Optionally, the low temperature oxide layer is etched by a dry etching process to form the through hole.

[0020] Optionally, the CVD deposition process includes a plasma-assisted CVD process.

[0021] Optionally, the film layer formed by the CVD deposition process includes a silicon dioxide layer or a silicon nitride layer.

[0022] Optionally, when the film layer is filled in the through hole, the film layer is also formed on the surface of the low-temperature oxide layer that has not been etched.

[0023] Optionally, the applicable technology node is less than or equal to 28 nm.

[0024] As described above, the method for forming the air gap isolation structure of the present invention pre-fills the gap grooves where the air gap isolation structure is to be formed by using photoresist, then grows a low-temperature oxide layer thereon, etches the low-temperature oxide layer to form a pinch-off structure, and finally removes the photoresist by a stripping process to form the air gap isolation structure. The above method can reduce the requirements for the trench etching process and improve the spatial size, uniformity, integrity and controllability of the air gap. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 The diagram shows a conventional semiconductor structure with an air gap.

[0026] Figure 2 to Figure 7 It is a cross-sectional structural schematic diagram of the process of forming an air gap isolation structure according to the present invention.

[0027] Figure 8 A flow chart of a method for forming an air gap isolation structure according to the present invention is shown.

[0028] Description of Figure Numbers

[0029] 10: semiconductor structure; 11: dielectric layer; 12: metal interconnect wire; 20: gap trench; 30: pre-fill layer; 40: low temperature oxide layer; 50: through hole; 60: film layer DETAILED DESCRIPTION

[0030] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0031] See also Figures 1 to 8 It should be noted that the illustrations provided in this embodiment are only schematic illustrations of the basic concept of the present invention. Although the illustrations only show components related to the present invention and are not drawn according to the number, shape and size of components in actual implementation, the form, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.

[0032] like Figure 8 As shown, this embodiment provides a method for forming an air gap isolation structure, the method comprising:

[0033] Step 1) providing a semiconductor structure 10, which includes a dielectric layer 11 and metal interconnect wires 12 formed in the dielectric layer 11 and arranged at intervals;

[0034] Step 2) etching the dielectric layer 11 between the metal interconnect wires 12 to form gap trenches 20;

[0035] Step 3) forming a pre-filling layer 30 in the gap trench 20, wherein the surface of the pre-filling layer 30 is not higher than the surface of the dielectric layer 11;

[0036] Step 4) forming a low temperature oxide layer 40 on the surface of the semiconductor structure 10 filled with the pre-filled layer 30;

[0037] Step 5) etching the low temperature oxide layer 40 formed on the surface of the pre-fill layer 30 until the pre-fill layer 30 is exposed to form a through hole 50, wherein the bottom opening of the through hole 50 is smaller than the surface width of the pre-fill layer 30;

[0038] Step 6) removing the photoresist layer;

[0039] Step 7) forming a film layer 60 in the through hole 50 by using a CVD deposition process, wherein the film layer 60 blocks the bottom end of the through hole 50 so that the gap trench 20 is not filled to form an air gap isolation structure.

[0040] Specifically, the applicable technology node is less than or equal to 28nm.

[0041] The following is combined with Figures 2 to 8The method for forming the air gap isolation structure provided in this embodiment is described in detail.

[0042] In step 1), a semiconductor structure 10 is provided, which includes a dielectric layer 11 and metal interconnection wires 12 formed in the dielectric layer 11 and arranged at intervals.

[0043] In this embodiment, the metal interconnection wire 12 is formed by etching the dielectric layer 11 to form a groove and then filling the groove with metal. In addition, the semiconductor structure 10 is also formed with a source, a drain and a gate (not shown in the figure), and the dielectric layer 11 is formed between and above the three.

[0044] like Figure 2 As shown, in step 2), the dielectric layer 11 between the metal interconnection wires 12 is etched to form gap trenches 20 .

[0045] In this embodiment, the dielectric layer 11 may be etched by dry etching to form the gap groove 20. Moreover, in this embodiment, the gap groove 20 formed by etching may be an inverted trapezoidal structure that is wide at the top and narrow at the bottom.

[0046] like Figure 3 As shown, in step 3), a pre-filling layer 30 is formed in the gap trench 20 , and the surface of the pre-filling layer 30 is not higher than the surface of the dielectric layer 11 .

[0047] In this embodiment, since the surface of the pre-filling layer 30 is lower than the surface of the dielectric layer 11 , a portion of the sidewall of the gap trench 20 is exposed above the gap trench 20 .

[0048] Specifically, the material of the pre-filling layer 30 includes photoresist.

[0049] like Figure 4 As shown, in step 4), a low temperature oxide layer 40 is formed on the surface of the semiconductor structure 10 filled with the pre-filled layer 30 .

[0050] In this embodiment, the surface of the pre-filled layer 30 is lower than the surface of the dielectric layer 11. Therefore, the low-temperature oxide layer 40 covers the surface of the metal interconnection wire 12, the surface of the unetched dielectric layer 11, the surface of the side wall of the gap groove 20 at the exposed partial depth, and the surface of the pre-filled layer 30.

[0051] Specifically, when the material of the pre-filling layer 30 is photoresist, the temperature used to form the low-temperature oxidation layer 40 is less than 80°.

[0052] In this embodiment, the temperature used when forming the low temperature oxide layer 40 is less than 80°, which is lower than the fission temperature of the photoresist material, thereby preventing the photoresist from fissioning.

[0053] Specifically, the material of the low temperature oxidation layer 40 includes silicon oxide.

[0054] like Figure 5 As shown, in step 5), the low temperature oxide layer 40 formed on the surface of the pre-fill layer 30 is etched until the pre-fill layer 30 is exposed to form a through hole 50, wherein the bottom opening of the through hole 50 is smaller than the surface width of the pre-fill layer 30.

[0055] In this embodiment, when forming the through hole 50, the structure formed by the low temperature oxide layer 40 retained on the sidewall of the gap groove 20 and the part of the low temperature oxide layer 40 retained on the surface of the pre-filled layer is a pinch-off structure. Moreover, the through hole 50 serves as a channel for the volatilization of the byproducts of the degumming.

[0056] Specifically, the low temperature oxide layer 40 is etched by a dry etching process to form the through hole 50 .

[0057] like Figure 6 As shown, in step 6), the photoresist layer is removed. In this embodiment, a stripping process is used to remove the photoresist layer.

[0058] like Figure 7 As shown, in step 7), a film layer 60 is formed in the through hole 50 by using a CVD deposition process, wherein the film layer 60 blocks the bottom end of the through hole 50 so that the gap trench 20 is not filled to form an air gap isolation structure.

[0059] In this embodiment, the CVD deposition process has poor step coverage and fast lateral growth rate.

[0060] Specifically, the CVD deposition process includes a plasma-assisted CVD process.

[0061] More specifically, the film layer 60 formed by the CVD deposition process includes a silicon dioxide layer or a silicon nitride layer. In this embodiment, silane and ammonia are used to form the silicon nitride layer, or silane and N 2 O to form the silicon dioxide layer.

[0062] Specifically, when the film layer 60 is filled in the through hole 50 , the film layer 60 is also formed on the surfaces of the metal interconnection wire 12 and the dielectric layer 11 .

[0063] Furthermore, in this embodiment, the thickness of the film layer 60 formed after the bottom of the through hole 50 is sealed may be 10 μm to 20 μm.

[0064] In summary, the method for forming an air gap isolation structure of the present invention is to pre-fill the gap grooves where the air gap isolation structure is to be formed by using photoresist, then grow a low-temperature oxide layer thereon, and etch the low-temperature oxide layer to form a pinch-off structure, and finally remove the photoresist by a stripping process to form the air gap isolation structure. The above method can reduce the requirements for the groove etching process and improve the spatial size, uniformity, integrity and controllability of the air gap. Therefore, the present invention effectively overcomes the various shortcomings of the prior art and has a high industrial utilization value.

[0065] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for forming an air gap isolation structure, characterized in that: The method comprises: A semiconductor structure is provided, comprising a dielectric layer and metal interconnect wires formed in the dielectric layer and arranged at intervals; Etching the dielectric layer between the metal interconnect wires to form gap trenches; forming a pre-filling layer in the gap trench, wherein the surface of the pre-filling layer is not higher than the surface of the dielectric layer; forming a low temperature oxide layer on the surface of the semiconductor structure filled with the pre-filled layer; Etching the low temperature oxide layer formed on the surface of the pre-fill layer until the pre-fill layer is exposed to form a through hole, wherein the bottom opening of the through hole is smaller than the surface width of the pre-fill layer; removing the photoresist layer; A film layer is formed in the through hole by using a CVD deposition process, wherein the film layer blocks the bottom end of the through hole so that the gap trench is not filled to form an air gap isolation structure.

2. The method for forming an air gap isolation structure according to claim 1, characterized in that: The material of the pre-filled layer includes photoresist.

3. The method for forming an air gap isolation structure according to claim 2, characterized in that: When the material of the pre-filled layer is photoresist, the temperature used when forming the low-temperature oxide layer is less than 80°.

4. The method for forming an air gap isolation structure according to claim 3, characterized in that: The material of the low temperature oxidation layer includes silicon oxide.

5. The method for forming an air gap isolation structure according to claim 1, characterized in that: The low temperature oxide layer is etched by a dry etching process to form the through hole.

6. The method for forming an air gap isolation structure according to claim 1, characterized in that: The CVD deposition process includes a plasma assisted CVD process.

7. The method for forming an air gap isolation structure according to claim 6, characterized in that: The film layer formed by the CVD deposition process includes a silicon dioxide layer or a silicon nitride layer.

8. The method for forming an air gap isolation structure according to claim 1, characterized in that: When the film layer is filled in the through hole, the film layer is also formed on the surface of the low temperature oxide layer that has not been etched.

9. The method for forming an air gap isolation structure according to claim 1, characterized in that: Applicable technology nodes are less than or equal to 28nm.