Preparation method of semiconductor device and semiconductor device prepared by same
By irradiating protons in the FRD frontal structure of RC-IGBT devices to absorb precious metal doping, the aggregation defects are solved at the PN junction, and the reverse recovery performance and leakage current problems of RC-IGBT devices are solved, achieving faster reverse Recovery and lower leakage current improves device stability and reliability.
Patent Information
- Application Number
- CN202310643746.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-31
- Publication Date
- 2024-12-03
AI Technical Summary
The reverse recovery performance of existing RC-IGBT devices is different from that of FRD, and there is a disadvantage of large leakage.
By irradiating protons in the frontal structure of FRD, local life control of precious metal doping is absorbed, precious metal defects are induced to aggregate at the PN junction, and carrier concentration distribution of FRD and IGBT structures is optimized, and reverse recovery time and leakage current are reduced. , and proton irradiation is performed in the terminal main junction region to absorb precious metal doping to avoid latching effect.
Accelerated reverse recovery is achieved, reverse recovery current and leakage current are reduced, device stability and reliability are improved, and carrier distribution conflicts of FRD and IGBT structures are optimized.
Smart Images

Figure CN119069508A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor device, and a semiconductor device prepared by the method. Background Art
[0002] Reverse Conducting IGBT (RC-IGBT) is a new type of IGBT device with high integration, which integrates the Fast Recovery Diode (FRD) and IGBT on the same chip. Compared with traditional IGBT devices, RC-IGBT improves device power density, reduces chip area, manufacturing cost and packaging cost, and improves IGBT reliability.
[0003] Due to the limitation of manufacturing process, the reverse recovery performance of existing RC-IGBT still lags behind that of FRD, and it also has the disadvantage of large leakage. Summary of the invention
[0004] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the first object of the present invention is to provide a method for preparing a semiconductor device, which can shorten the reverse recovery time of the FRD device, reduce the device leakage current, and will not affect the performance of the semiconductor device.
[0005] A second object of the present invention is to provide a semiconductor device.
[0006] In order to achieve the above-mentioned purpose, the preparation method of the semiconductor device of the embodiment of the first aspect of the present invention obtains a drift layer; prepares a device front structure on the front side of the drift layer, including preparing an IGBT front structure and an FRD front structure; and performs proton irradiation on the FRD front structure to extract the local lifetime control of the precious metal doping, so as to induce the defects generated by the precious metal in the FRD front structure to gather near the PN junction of the FRD front structure.
[0007] In some embodiments, the local lifetime control of precious metal doping by proton irradiation is performed on the FRD front structure, including: local lifetime control of platinum doping by proton irradiation is performed on the FRD front structure, or local lifetime control of gold doping by proton irradiation is performed on the FRD front structure.
[0008] In some embodiments, the FRD front structure is subjected to proton irradiation to extract local lifetime control of precious metal doping, including: preparing a precious metal layer on the front side of the FRD front structure; removing the precious metal layer; proton irradiating the FRD front structure; and annealing the FRD front structure after completing the proton irradiation.
[0009] In some embodiments, proton irradiating the FRD front structure includes at least one of the following: proton irradiating the front side of the FRD front structure; or proton irradiating the back side of the FRD front structure.
[0010] In some embodiments, before performing proton irradiation to extract the local lifetime control of the noble metal doping on the FRD front structure, the preparation method further includes: preparing an insulating dielectric layer on the IGBT front structure.
[0011] In some embodiments, the IGBT front side structure and the FRD front side structure are alternately arranged along the lateral direction of the device.
[0012] In some embodiments, the preparation method also includes: preparing a terminal structure around the front structure of the device, the terminal structure surrounds the front structure of the device, the terminal structure includes a terminal main junction region, and the terminal main junction region is adjacent to the front structure of the device; and performing proton irradiation on the terminal main junction region to absorb local lifetime control of precious metal doping.
[0013] In some embodiments, the terminal main junction region is subjected to local lifetime control by proton irradiation to absorb precious metal doping, including: preparing an insulating dielectric layer on the terminal structure except the terminal main junction region; performing local lifetime control by proton irradiation to absorb platinum doping on the terminal main junction region, or performing local lifetime control by proton irradiation to absorb gold doping on the terminal main junction region.
[0014] In some embodiments, the terminal main junction region is subjected to proton irradiation to extract local lifetime control of precious metal doping, including: preparing a precious metal layer on the front side of the terminal main junction region; removing the precious metal layer; proton irradiating the terminal main junction region; and after completing the proton irradiation, annealing the terminal main junction region.
[0015] In some embodiments, proton irradiating the terminal main junction region includes at least one of the following: proton irradiating the front side of the terminal main junction region; or proton irradiating the back side of the terminal main junction region.
[0016] In some embodiments, a front structure of the device is prepared on the front side of the drift layer, including: preparing a carrier storage layer on the drift layer; preparing an IGBT well region on the carrier storage layer corresponding to the IGBT region and preparing an FRD well region on the carrier storage layer corresponding to the FRD region; preparing gate trenches, emitter trenches and dummy trenches spaced apart along the lateral direction of the device on the drift layer in the IGBT region, the gate trenches, emitter trenches and dummy trenches all passing through the IGBT well region and the carrier storage layer and extending into the drift layer; preparing an emitter trench on the drift layer in the FRD region, the emitter trench passing through the FRD well region and the carrier storage layer and extending into the drift layer.
[0017] In some embodiments, the preparation method further includes: preparing an emitter metal layer on the insulating dielectric layer of the IGBT front structure and on the FRD front structure, wherein the emitter metal layer is connected to the emitter trench.
[0018] In some embodiments, the preparation method further includes: preparing a field stop layer on the back side of the drift layer; preparing a collector region and a short circuit region arranged laterally along the device on the field stop layer; and preparing a collector metal layer on the collector region and the short circuit region.
[0019] The semiconductor device of the embodiment of the second aspect of the present invention is manufactured by using the semiconductor device manufacturing method.
[0020] The preparation method of the semiconductor device and the semiconductor device of the embodiment of the present invention perform proton irradiation in the FRD region of the device to extract the local lifetime control of the precious metal doping, and induce the defects generated by the precious metal in the FRD front structure to gather near the PN junction of the FRD front structure, which can accelerate the recombination speed of minority carriers near the PN junction near the anode of the drift region during reverse recovery. The electron concentration will drop to the level of equilibrium carrier concentration in a shorter time, and the shutdown will be accelerated, thereby reducing the reverse recovery current, increasing the softness factor, reducing the leakage current of the device, and optimizing the conflict of carrier concentration distribution between the FRD structure and the IGBT structure.
[0021] In addition, the proton irradiation extraction of precious metal doping lifetime control in the terminal main junction region avoids the latch-up effect caused by excessive carrier concentration when the device is turned off, making the device have good stability and reliability.
[0022] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:
[0024] Figure 1 is a flow chart of a method for preparing a semiconductor device according to an embodiment of the present invention;
[0025] Figure 2 is a schematic diagram of a cross section of a semiconductor device according to an embodiment of the present invention;
[0026] Figure 3 is a schematic diagram of a semiconductor device structure according to an embodiment of the present invention;
[0027] Figure 4 is a schematic diagram of a cross-section of an IGBT structure according to an embodiment of the present invention;
[0028] Figure 5 is a schematic diagram of a cross-section of an FRD structure according to an embodiment of the present invention;
[0029] Figure 6 is a flow chart of a method for preparing a semiconductor device according to an embodiment of the present invention;
[0030] Figure 7 is a schematic diagram of a process for depositing a precious metal according to an embodiment of the present invention;
[0031] Figure 8 is a schematic diagram of a proton irradiation process according to an embodiment of the present invention.
[0032] Reference numerals:
[0033] 1 collector metal; 2 collector region; 3 short circuit region; 4 field stop layer; 100 drift layer; 5 carrier storage layer; 6 gate oxide layer; 7 polysilicon gate electrode; 8 ohmic contact region; 9 first conductivity type highly doped emitter region; 10 insulating dielectric layer; 12 IGBT region second conductivity type doped well region; 22 FRD region second conductivity type doped well region; 11 gate trench; 21 emitter trench; 31 dummy trench; 13 contact hole; 14 emitter metal; 23 metal platinum; 24 photoresist; 110 active region; 1101 IGBT region; 1102 FRD region; 120 terminal region; 1201 terminal main junction region. DETAILED DESCRIPTION
[0034] Embodiments of the present invention are described in detail below. The embodiments described with reference to the accompanying drawings are exemplary. Embodiments of the present invention are described in detail below.
[0035] A method for manufacturing a semiconductor device according to an embodiment of the first aspect of the present invention will be described below with reference to the accompanying drawings.
[0036] Figure 1 is a flow chart of a method for preparing a semiconductor device according to an embodiment of the present invention, such as Figure 1 As shown, the preparation method includes the following steps S1-S3.
[0037] S1, obtain the drift layer.
[0038] Specifically, a substrate may be obtained, pre-processed such as cleaning and decontamination, and the desired substrate material, i.e., the drift layer, may be obtained by doping, or the prepared substrate material, i.e., the drift layer may be obtained directly, or the drift layer may be obtained by epitaxial treatment on the original substrate.
[0039] S2, preparing a device front structure on the front side of the drift layer, including preparing an IGBT front structure and an FRD front structure.
[0040] In some embodiments, the semiconductor device of the embodiment of the present invention includes a reverse conducting IGBT device, the reverse conducting IGBT device includes an FRD structure and an IGBT structure, wherein the front structure of the device is as follows: Figure 2 The FRD front structure includes an active region 110 of the device, and may include a well region, an emitter trench, and other structures. The IGBT front structure includes a gate structure, an emitter structure, a well region, and other device structures.
[0041] In the embodiment, in terms of electrical connection, the IGBT structure is connected in reverse parallel with the FRD structure, and in terms of device structure, as shown in FIG. Figure 2 As shown, the IGBT structure 1101 and the FRD structure 1102 may be alternately arranged along the lateral direction of the device or distributed in other suitable forms.
[0042] S3, performing proton irradiation on the FRD front structure to extract the local lifetime control of the noble metal doping, so as to induce the defects generated by the noble metal in the FRD front structure to gather near the PN junction of the FRD front structure.
[0043] In the embodiments, noble metal diffusion such as platinum diffusion process or gold diffusion process is used as a global lifetime control method, which will cause the FRD front structure to be doped with noble metals such as platinum or gold, which will have a greater impact on the forward conduction voltage drop of the FRD, and it is difficult to accurately control the concentration distribution of the recombination center by diffusing noble metals such as platinum or gold. However, platinum diffusion or gold diffusion can make the leakage current of the device relatively small, because the energy level of the recombination center formed by the noble metal such as platinum is located 0.23eV below the conduction band of the substrate such as the silicon substrate, away from the center of the forbidden band, and the leakage current of the prepared device is small.
[0044] In the embodiments, light ion irradiation is a local lifetime control method, and the location where the defect occurs can be determined by changing the irradiation energy. However, light ion irradiation technology increases the leakage current of the device. The most effective defect energy level induced by light ion irradiation (including proton irradiation) is generally located about 0.42 eV below the conduction band of the silicon substrate, which is relatively close to the center of the bandgap. Although this defect energy level can effectively reduce the carrier lifetime and increase the switching speed, the device leakage current is large.
[0045] However, in the embodiment of the present application, proton irradiation is used to extract precious metal doping to perform local lifetime control on the front structure of the FRD. By controlling the irradiation energy during proton irradiation and changing the proton injection depth, the defect position can be controlled near the pn junction of the FRD region to achieve local control. That is, proton irradiation extraction of platinum doping can induce defects generated by precious metals such as platinum to gather near the PN junction of the FRD region, reducing the impact on the forward conduction voltage drop of the FRD region, reducing the reverse recovery time of the device, and reducing the leakage current of the device.
[0046] Among them, through precious metal doping and proton irradiation, a higher concentration of defect distribution can be formed at the end of the range of the precious metal, thereby generating a stable recombination center at a set local position, such as near the PN junction of the FRD region, while no or very few recombination centers are introduced at other positions, thereby achieving the effect of local lifetime control.
[0047] In addition, considering the energy level distribution characteristics of precious metals such as platinum and gold, which are far away from the center of the substrate band gap, the device leakage current is small. Combined with proton irradiation, that is, using proton irradiation to extract the local lifetime control of precious metal doping, local control of the recombination center can be achieved, so that precious metal impurities can be accumulated in the local area of the PN junction in the FRD region, thereby reducing the device leakage current without affecting the reverse recovery characteristics of the device.
[0048] The preparation method of the embodiment of the present invention, when performing a proton irradiation treatment on the FRD front structure to extract the local lifetime control of the precious metal doping, introduces a recombination center locally in the FRD front structure, that is, inducing the defects generated by the precious metal in the FRD front structure to gather near the PN junction of the FRD front structure, which can accelerate the recombination speed of minority carriers near the PN junction near the anode of the drift region during reverse recovery, and the electron concentration will drop to the level of equilibrium carrier concentration in a shorter time, and the shutdown will be accelerated, thereby reducing the reverse recovery current, increasing the softness factor, reducing the device leakage current, and optimizing the conflict of carrier concentration distribution between the FRD structure and the IGBT structure.
[0049] Furthermore, when the local lifetime control of the noble metal doping is performed on the FRD front structure by proton irradiation, for example, the local lifetime control of the platinum doping is performed on the FRD front structure by proton irradiation, or the local lifetime control of the gold doping is performed on the FRD front structure by proton irradiation. In the embodiment of the present invention, the noble metal is selected as platinum or gold or other applicable metals, which can achieve the effect of locally introducing stable recombination centers, and combined with proton irradiation, the generated recombination centers can be gathered close to the PN junction of the FRD front structure, thereby reducing the reverse recovery current and the device leakage current.
[0050] In some embodiments, the local lifetime control of the FRD front structure by proton irradiation to extract the noble metal doping includes: preparing a noble metal layer on the front of the FRD front structure, at which time there is already a situation where the noble metal layer is introduced into the FRD front structure, then removing the noble metal layer, and proton irradiating the FRD front structure to form a higher concentration of defect distribution at the end of the range of the noble metal. After the proton irradiation is completed, the FRD front structure is annealed to allow the noble metal ions to diffuse and be absorbed by the proton irradiation-induced defects to form localized noble metal doping.
[0051] In the embodiment, when the FRD front structure is subjected to proton irradiation, the front and / or back of the FRD front structure may be subjected to proton irradiation, such as H+ irradiation. For example, the front of the FRD front structure is subjected to proton irradiation, or the back of the FRD front structure is subjected to proton irradiation, or both the front and back of the FRD front structure are subjected to proton irradiation, so as to more efficiently modulate the defect, i.e., the recombination center, to the vicinity of the PN junction of the FRD region, thereby achieving the purpose of reducing the leakage current.
[0052] For example, platinum doping is used to achieve local noble metal doping lifetime control on the front structure of FRD. As a kind of overall lifetime control technology, platinum diffusion achieves lifetime control by forming a recombination center that is approximately evenly distributed in the device body. However, the introduction of the same recombination center in the device space charge region does not contribute much to the reduction of the turn-off time, and will also increase the forward voltage drop and reverse leakage to a certain extent, and even lead to a decrease in the softness factor. The proton irradiation method is a kind of longitudinal local lifetime control. Although this method can achieve local lifetime control, it causes the leakage current generated by the IGBT device to be larger.
[0053] However, the preparation method of the embodiment of the present invention introduces a new method for local precious metal doping lifetime control to prepare RC-IGBT devices. In the embodiment of the present invention, proton irradiation is used to introduce a recombination center with a high platinum doping concentration at an appropriate local position of the FRD front structure, while no or very few recombination centers are introduced at other longitudinal positions to achieve a better lifetime control effect. Proton irradiation can achieve local platinum doping because the injected light ions will form a defect distribution with a very high concentration at the end of its range, which is called a defect peak, and the defect density between the irradiated surface and the defect peak is only 10%-20% of the peak. The RC-IGBT device is made by the local platinum doping lifetime control method, which realizes the lifetime control of the FRD region in the RC-IGBT device at an appropriate local position without affecting the carrier lifetime of the IGBT region, not only reducing the reverse recovery time of the FRD device, but also reducing the device leakage current, optimizing the voltage drop Vf of the FRD structure, and at the same time, it will not affect the performance of the IGBT device, and optimizes the conflict between the FRD and IGBT regarding the carrier concentration distribution.
[0054] Furthermore, in order not to affect device performance, an insulating dielectric layer is prepared on the IGBT front structure before the local lifetime control of the FRD front structure by proton irradiation to extract precious metal doping, which can reduce the impact on the carrier lifetime of the IGBT front structure.
[0055] Among them, the insulating dielectric layer can prevent the noble metal from diffusing to the IGBT front structure, reducing the impact on the carrier lifetime of the IGBT front structure. That is, by introducing a recombination center with a high noble metal doping concentration at an appropriate local position of the FRD front structure, while not introducing or introducing very few recombination centers at other positions in the lateral direction of the device, a better lifetime control effect can be achieved.
[0056] Due to the different polarities of the back electrodes, the RC-IGBT device extracts electrons faster when it is turned off, and accordingly, the hole extraction is also faster, which is beneficial to reduce the turn-off loss. However, the current spike is large when it is turned off, which is easy to form latch and burn the device. In order to solve this problem, the preparation method process is also improved in the embodiment of the present invention.
[0057] like Figure 2 As shown, the semiconductor device further includes a terminal structure 120 , which surrounds the device front side structure 110 . The terminal structure 120 includes a terminal main junction region 1201 , and the terminal main junction region 1201 is adjacent to the device front side structure.
[0058] In an embodiment, the preparation method of the embodiment of the present invention further includes: preparing a terminal structure around the front structure of the device, and performing proton irradiation on the terminal main junction area to extract precious metals such as platinum or gold or other applicable metal doping to control the local lifetime.
[0059] For example, in some embodiments, an insulating dielectric layer is prepared on the terminal structure except for the terminal main junction region, and the terminal main junction region is subjected to proton irradiation to extract local lifetime control of platinum doping, or the terminal main junction region is subjected to proton irradiation to extract local lifetime control of gold doping.
[0060] Among them, the insulating dielectric layer can block the diffusion of noble metal ions to other locations, reducing the impact on the carrier lifetime in other locations. By introducing a recombination center with a high noble metal doping concentration in the terminal main junction area, a better lifetime control effect can be achieved.
[0061] By preparing an insulating dielectric layer on the terminal structure except for the terminal main junction area, and performing proton irradiation on the terminal main junction area to extract the local lifetime control of platinum doping, the hole current at the main junction during shutdown can be effectively reduced, avoiding the latch effect caused by excessive hole current when the device is turned off, and making the device have better stability and reliability.
[0062] Specifically, a noble metal layer is prepared on the front side of the terminal main junction region, where the noble metal layer is already introduced into the terminal main junction region, and then the noble metal layer is removed, and the terminal main junction region is subjected to proton irradiation to form a defect distribution with a higher concentration at the end of the range of the noble metal. After the proton irradiation is completed, the terminal main junction region is annealed to allow the noble metal ions to diffuse and be absorbed by the proton irradiation-induced defects to form localized noble metal doping.
[0063] In some embodiments, when proton irradiation is performed on the terminal main junction region, proton irradiation may be performed on the front side of the terminal main junction region, and / or proton irradiation may be performed on the back side of the terminal main junction region. For example, proton irradiation may be performed on the front side of the terminal main junction region; or, proton irradiation may be performed on the back side of the terminal main junction region. Alternatively, proton irradiation may be performed on both the front side and the back side of the terminal main junction region, which is more efficient and faster.
[0064] Similarly, local control of proton irradiation extraction of precious metal doping in the terminal main junction region can make the recombination centers produced by the precious metals gather near the terminal main junction region. When the device is turned off, the hole current here can recombine with the recombination center, thereby increasing the hole recombination rate, thereby reducing the hole current caused by excessive hole current at the terminal main junction, avoiding the latch effect when the device is turned off, and improving the device stability and reliability.
[0065] As described above, the preparation method of the embodiment of the present invention uses an insulating oxide layer as a barrier layer in the IGBT region, performs local precious metal doping lifetime control in the FRD region, and introduces a stable recombination center to greatly reduce the reverse recovery time of the RC-IGBT device, improve the device softness, and reduce the leakage current of the device. The proton irradiation extraction precious metal doping lifetime control performed in the terminal main junction region avoids the latch-up effect caused by excessive carrier concentration when the RC-IGBT is turned off, so that the device has good stability and reliability.
[0066] Figure 3 is a schematic diagram of a semiconductor device structure according to an embodiment of the present invention, Figure 4 is a schematic diagram of an IGBT structure cross section according to an embodiment of the present invention, Figure 5 FIG. 1 is a schematic diagram of a cross-section of an FRD structure according to an embodiment of the present invention. Figure 3-5 As shown, the semiconductor device structure includes: 1 collector metal; 2 back side second conductivity type highly doped collector region; 3 back side first conductivity type highly doped short circuit region; 4 first conductivity type doped field stop layer; 100 first conductivity type low doped drift region; 5 first conductivity type highly doped carrier storage layer; 6 gate oxide layer; 7 polysilicon gate electrode; 8 second conductivity type doped ohmic contact region; 9 first conductivity type highly doped emitter region; 10 insulating dielectric layer; 12 IGBT region second conductivity type doped well region; 22 FRD region second conductivity type doped well region; 11 gate trench; 21 emitter trench; 31 dummy trench; 13 contact hole; 14 emitter metal; 23 metal platinum.
[0067] In an embodiment of the present invention, a front structure of the device is prepared on the front side of the drift layer, including: preparing a carrier storage layer on the drift layer; preparing an IGBT well region on the carrier storage layer corresponding to the IGBT region and preparing an FRD well region on the carrier storage layer corresponding to the FRD region; preparing gate trenches, emitter trenches and dummy trenches spaced apart along the lateral direction of the device on the drift layer in the IGBT region, the gate trenches, emitter trenches and dummy trenches all passing through the IGBT well region and the carrier storage layer and extending into the drift layer; preparing an emitter trench on the drift layer in the FRD region, the emitter trench passing through the FRD well region and the carrier storage layer and extending into the drift layer.
[0068] The preparation method further comprises: preparing an emitter metal layer on the barrier layer of the IGBT front structure and on the FRD front structure, wherein the emitter metal layer is connected to the emitter trench.
[0069] As shown in the figure, the preparation method also includes preparing a back structure on the back side of the drift layer, for example, preparing a field stop layer on the back side of the drift layer; preparing a collector area and a short circuit area arranged laterally along the device on the field stop layer; and preparing a collector metal layer on the collector area and the short circuit area.
[0070] For example, Figure 6 is a flow chart of a method for preparing a semiconductor device according to an embodiment of the present invention, such as Figure 6 As shown, the preparation method comprises:
[0071] S11, providing a silicon substrate.
[0072] S12, ion implantation forms a field limiting ring (terminal structure), a carrier storage layer, and a cutoff ring (terminal structure).
[0073] S13, etching a groove on the silicon substrate, growing gate oxide in the groove and then depositing polysilicon.
[0074] S14, forming a second conductivity type doped well region and a first conductivity type highly doped channel emitter region by ion implantation.
[0075] S15, in the FRD region and the terminal main junction region, proton irradiation is used to induce defects to absorb platinum or gold to form a localized platinum or gold doping region.
[0076] S16, etching the IGBT region contact hole, and forming a second conductivity type doped ohmic contact region at the bottom of the contact hole by ion implantation.
[0077] S17, depositing front emitter metal.
[0078] S18, ion implantation is performed to form a second conductivity type highly doped collector region and a first conductivity type highly doped short circuit region.
[0079] S19, implanting first conductive type ions into the back surface to form a field stop layer.
[0080] S20, depositing a back collector metal.
[0081] The following takes the preparation process of the RC-IGBT device with local platinum doping lifetime control as an example. Figure 3-5 The semiconductor device structure shown is an example to describe the manufacturing method of the embodiment of the present invention.
[0082] Specifically, in an embodiment, the preparation process of a local platinum doped lifetime controlled RC-IGBT device includes:
[0083] (1) A field limiting ring of the terminal region 120 is formed in the semiconductor substrate 100 by ion implantation and high temperature well driving.
[0084] (2) A first conductivity type doped carrier storage layer 5 is formed in the device of the semiconductor substrate 100 by ion implantation and high temperature well driving.
[0085] (3) The gate trench 11, the dummy trench 31 and the emission trench 21 are formed in the surface of the semiconductor substrate 100 by photolithography and reactive ion etching. The trenches can be arranged at equal intervals or at unequal intervals.
[0086] (4) A high-density insulating oxide layer 6 is grown on the inner wall of each groove.
[0087] Specifically, in order to reduce crystal defects and impurities and grow an insulating oxide layer with good density, a sacrificial oxide layer is first grown on the inner wall of each groove area by high temperature oxidation, and then the sacrificial oxide layer is etched away by wet method to ensure the smoothness of the insulating oxide layer, and an insulating oxide layer is grown on the inner wall of each groove area by high temperature oxidation. The thickness of the insulating oxide layer is
[0088] (5) Depositing a polysilicon gate electrode 7 doped with the first conductivity type on the oxide layer in the trench.
[0089] Specifically, polysilicon is deposited on the surface of the semiconductor substrate 100 through a high-temperature furnace tube and in-situ doped to form polysilicon doped with a first conductivity type.
[0090] (6) Form the second conductivity type doped well region 12 in the IGBT region and the second conductivity type doped well region 22 in the FRD region by ion implantation.
[0091] Specifically, ion implantation is performed in the IGBT and FRD regions together, and then ion implantation is performed again in the IGBT region through a photolithography mask, thereby forming the second conductivity type doped well region 12 in the IGBT region and the second conductivity type doped well region 22 in the FRD region. The second conductivity type ion dose implanted in the IGBT region and the FRD region for the first time is 5E13-6E13 cm -2 , the second IGBT region second conductivity type ion implantation dose 1E12-1E14 cm -2 .
[0092] (7) A first conductivity type highly doped emitter region 9 is formed at the gate trench 11 of the IGBT region by ion implantation and high temperature well driving.
[0093] Specifically, a photolithography mask is used to form an injection window of the first conductive type emitter region in the gate trench region 11, and high-energy first conductive type ions are injected into the injection window of the first conductive type highly doped emitter region and pushed into the trap at high temperature, thereby forming a first conductive type highly doped emitter region 9 in the gate trench region 11 of the IGBT region. The first conductive type ion implantation dose is 1E15-5E15 cm -2 .
[0094] (8) Figure 7As shown, an insulating dielectric layer 10 is deposited on the surface of the semiconductor substrate as a barrier layer for the IGBT region and the terminal region except the main junction, metal platinum 23 is deposited, and the metal platinum 23 is removed.
[0095] (9) Deposit photoresist 24 on the surface or back of the semiconductor substrate to remove the terminal main junction area and Figure 8 After the photoresist of the FRD region is shown, H+ irradiation is performed on the front or back side of the FRD front structure. The H+ implantation dose range is 1E11-5E14 cm -2 , remove the photoresist 24, and then perform annealing, the purpose of which is to allow platinum to diffuse and be absorbed by proton irradiation-induced defects to form localized platinum doping.
[0096] (10) Etch the insulating dielectric layer 10 of the IGBT region to obtain Figure 3 The contact hole 13 is shown. By implanting the second conductivity type ions into the contact hole 13, the second conductivity type doped ohmic contact region 8 is formed.
[0097] (11) Deposit emitter metal 14 on the device surface.
[0098] Specifically, a layer of metal with a thickness of 1um-5um is deposited on the surface of the device. The metal is an aluminum / silicon alloy or an aluminum / silicon / copper alloy or other materials, and is alloyed by thermal annealing to form an ohmic contact between the highly doped silicon and the metal, thereby reducing the contact resistance.
[0099] (12) Thinning, forming a second conductive type highly doped collector region 2 on the back side of the semiconductor substrate by second conductive type ion implantation and high temperature well driving process; wherein the ion doping concentration of the second conductive type highly doped collector region 2 is 1E18-5E19 cm -3 The junction depth is 0.5um-1um, which can achieve the effect of controlling the emission injection efficiency. The second conductive type high concentration doped collector region 2 is only formed in the IGBT region.
[0100] (13) Forming a first conductive type high-concentration doped short-circuit region 3 on the back side of the semiconductor substrate by first conductive type ion implantation and high-temperature well-driving process; wherein the doping concentration of the first conductive type high-concentration doped short-circuit region 3 is 1E18-5E19 cm -3 , the first conductivity type high-concentration doped short-circuit region 3 is only formed in the FRD region.
[0101] (14) Forming a first conductive type doped field stop region 4 on the back side of the semiconductor substrate by ion implantation; the ion implantation dose is 5E12-8E13 cm -2 .
[0102] (15) Deposit the back collector metal 1 of the RC-IGBT device.
[0103] In the above, in the embodiment of the present invention, the first conductivity type may be N-type, the first conductivity type may also be P-type, when the first conductivity type is N-type, the second conductivity type is P-type, when the first conductivity type is P-type, the second conductivity type is N-type. At the same time, the doped element type of the P-type doping region may be boron (B) and boron fluoride (BF2), etc., and the doped element type of the N-type doping region may be phosphorus (P), arsenic (As) and hydrogen (H) and other elements, both of which are not specifically limited.
[0104] In an embodiment, the trench regions of the IGBT region and the FRD region of the present invention may be arranged at equal intervals or at unequal intervals.
[0105] In an embodiment, the front structure of the IGBT may also be a cellular structure of other IGBTs (for example, a cellular structure including one gate trench and three dummy trenches), and the front structure of the FRD may also be a cellular structure of other FRDs.
[0106] In an embodiment, both the IGBT structure on the front side of the device and the drift layer in the FRD region include a carrier storage layer, and it is also possible that no carrier storage layer is prepared in the drift layer in the FRD region.
[0107] In the embodiment, the area ratio of the IGBT region to the FRD region is 1:1-10:1. The area ratio of the IGBT region to the FRD region can be adjusted according to actual conditions, and the specific implementation case shall be based on actual needs.
[0108] In the embodiment, the second conductivity type ion doping concentrations in the well regions of the IGBT region and the FRD region are inconsistent. The second conductivity type ion doping dose in the well region of the IGBT region is 5E13-1.6E14 cm-2, and the second conductivity type ion doping dose in the well region of the FRD region is 1E12-1E14 cm-2. The well region ion doping doses in the IGBT region and the FRD region can be adjusted according to actual conditions, and the specific implementation case shall be based on actual needs.
[0109] As an example, the shape of the back first conductivity type doped short-circuit region of the FRD region of the present invention can be circular, triangular, rectangular, trapezoidal, ring-shaped, star-shaped or polygonal.
[0110] As an example, the contact hole may be a rectangular groove, a trapezoidal groove, a tapered groove, or a special-shaped groove.
[0111] In the embodiment, the preparation method of the embodiment of the present invention reduces the reverse recovery time of the RC-IGBT device by adopting a local platinum doping lifetime control method in the second conductive type doped well region of the FRD region. The H+ injection dose can be adjusted according to actual conditions, and the specific implementation case shall be based on actual needs.
[0112] In general, the method for preparing a semiconductor device in an embodiment of the present invention uses an insulating oxide layer and a photoresist as a barrier layer in the IGBT region, performs local platinum doping lifetime control in the FRD region, and introduces a stable recombination center to greatly reduce the reverse recovery time of the RC-IGBT device, improve the device softness, and reduce the leakage current of the device. The proton irradiation-absorbed platinum doping lifetime control performed in the terminal main junction region avoids the latch-up effect caused by excessive carrier concentration when the RC-IGBT is turned off, so that the device has good stability and reliability.
[0113] Based on the method for preparing the semiconductor device in the above embodiment, the second embodiment of the present invention further provides a semiconductor device. The semiconductor device is prepared by the method for preparing the semiconductor device in the above embodiment, such as Figure 3 shown.
[0114] The semiconductor device according to the embodiment of the present invention is prepared by adopting the preparation method of the above embodiment, and local precious metal doping lifetime control is performed in the FRD region of the device. By introducing a stable recombination center, the reverse recovery time of the RC-IGBT device is greatly reduced, the device softness is improved, and the leakage current of the device is reduced.
[0115] In addition, the proton irradiation-absorbed platinum doping lifetime control in the terminal main junction region avoids the latch-up effect caused by excessive carrier concentration when the RC-IGBT is turned off, making the device have good stability and reliability.
[0116] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example.
[0117] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A method for preparing a semiconductor device, characterized in that: include: Obtaining a drift layer; Preparing a device front structure on the front side of the drift layer, including preparing an IGBT front structure and an FRD front structure; The FRD front structure is subjected to proton irradiation to extract the local lifetime control of the noble metal doping, so as to induce the defects generated by the noble metal in the FRD front structure to gather near the PN junction of the FRD front structure.
2. The method for preparing a semiconductor device according to claim 1, wherein: The local lifetime control of the noble metal doping by proton irradiation on the front structure of the FRD includes: The FRD front structure is subjected to proton irradiation to extract the local lifetime control of platinum doping, or the FRD front structure is subjected to proton irradiation to extract the local lifetime control of gold doping.
3. The method for preparing a semiconductor device according to claim 1 or 2, characterized in that: The local lifetime control of the noble metal doping by proton irradiation on the front structure of the FRD includes: preparing a noble metal layer on the front side of the FRD front structure; removing the noble metal layer; performing proton irradiation on the FRD front structure; After the proton irradiation is completed, the FRD front structure is annealed.
4. The method for preparing a semiconductor device according to claim 3, characterized in that: The FRD front structure is subjected to proton irradiation, comprising at least one of the following: performing proton irradiation on the front side of the FRD front side structure; The back side of the FRD front side structure is subjected to proton irradiation.
5. The method for preparing a semiconductor device according to claim 1, characterized in that: Before the FRD front structure is subjected to proton irradiation to extract the local lifetime control of the noble metal doping, the preparation method further comprises: An insulating dielectric layer is prepared on the IGBT front structure.
6. The method for preparing a semiconductor device according to claim 1, wherein: The IGBT front structure and the FRD front structure are alternately arranged along the lateral direction of the device.
7. The method for preparing a semiconductor device according to claim 1, characterized in that: The preparation method further comprises: Preparing a terminal structure around the device front structure, the terminal structure surrounds the device front structure, the terminal structure includes a terminal main junction region, and the terminal main junction region is adjacent to the device front structure; The terminal main junction region is subjected to proton irradiation to extract the local lifetime control of the noble metal doping.
8. The method for preparing a semiconductor device according to claim 7, characterized in that: The local lifetime control of the terminal main junction region by proton irradiation to extract the noble metal doping includes: preparing an insulating dielectric layer on the terminal structure except the terminal main junction region; The terminal main junction region is subjected to proton irradiation to extract the local lifetime control of platinum doping, or the terminal main junction region is subjected to proton irradiation to extract the local lifetime control of gold doping.
9. The method for preparing a semiconductor device according to claim 8, characterized in that: The local lifetime control of the terminal main junction region by proton irradiation to extract the noble metal doping includes: Preparing a noble metal layer on the front side of the terminal main junction region; removing the noble metal layer; Performing proton irradiation on the terminal main junction region; After the proton irradiation is completed, an annealing process is performed on the terminal main junction region.
10. The method for preparing a semiconductor device according to claim 9, characterized in that: The terminal main junction region is subjected to proton irradiation, comprising at least one of the following: Performing proton irradiation on the front side of the terminal main junction region; The back side of the terminal main junction region is subjected to proton irradiation.
11. The method for preparing a semiconductor device according to claim 5, characterized in that: A device front structure is prepared on the front side of the drift layer, comprising: preparing a carrier storage layer on the drift layer; Prepare an IGBT well region on the carrier storage layer corresponding to the IGBT region and prepare an FRD well region on the carrier storage layer corresponding to the FRD region; On the drift layer of the IGBT region, a gate trench, an emitter trench and a dummy trench are prepared, which are arranged in a lateral direction of the device and are spaced apart from each other, wherein the gate trench, the emitter trench and the dummy trench all penetrate the IGBT well region and the carrier storage layer and extend into the drift layer; An emitter trench is formed on the drift layer of the FRD region, wherein the emitter trench penetrates the FRD well region and the carrier storage layer and extends into the drift layer.
12. The method for preparing a semiconductor device according to claim 11, characterized in that: The preparation method further comprises: An emitter metal layer is prepared on the insulating dielectric layer of the IGBT front structure and on the FRD front structure, and the emitter metal layer is connected to the emitter trench.
13. The method for preparing a semiconductor device according to claim 1, characterized in that: The preparation method further comprises: preparing a field stop layer on the back side of the drift layer; Preparing a collector region and a short-circuit region on the field stop layer and arranged laterally along the device; A collector metal layer is prepared on the collector region and the short-circuit region.
14. A semiconductor device, characterized in that: The semiconductor device is manufactured by the method for manufacturing a semiconductor device according to any one of claims 1 to 13.