Cross-shaped steel reinforced column and processing technology thereof
By introducing a quick disassembly reinforcement mechanism and a positioning block/slot system in the processing technology of the cross steel bone column, the problems of cumbersome and misalignment in the prior art are solved, and the processing efficiency and quality of the cross steel bone column are improved.
Patent Information
- Application Number
- CN202411227264.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-03
AI Technical Summary
The processing technology of existing cross steel bone columns is cumbersome and inefficient, and misalignment is prone to occur during welding, resulting in poor processing quality.
The quick-removal reinforcement mechanism and positioning block/slot system are adopted to achieve stable welding of T-shaped steel and H-shaped steel and reliable assembly of adjacent columns through automatic welding and mechanical correction.
The processing time of the cross steel bone column is greatly shortened, the processing efficiency and quality is improved, and the misalignment phenomenon during welding is avoided.
Smart Images

Figure CN119077296A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cross steel column, in particular to a cross steel column and a processing technology thereof. Background Art
[0002] Cross steel column is a common building structural member, which is usually used to support and reinforce the columns of buildings. It is mainly used for structural support and reinforcement of industrial plants, commercial buildings and large public buildings. Cross steel column can bear vertical loads and provide good bending and torsion resistance through its cross structure.
[0003] The current cross steel column is mainly composed of an H-shaped steel and a T-shaped steel welded on the two side walls of the H-shaped steel, and the end of the cross steel column is smooth. The processing process of the cross steel skeleton of this structure is: cutting and blanking, groove processing, H-shaped steel assembly, T-shaped steel assembly, H-shaped steel and T-shaped steel correction, cross main assembly, cross steel column welding and assembly. Although the welding processing of the cross steel column can be realized under the above processing technology, on the one hand, during the assembly process of the cross column, the above process is mainly to weld a reinforcing rib every 0.5m at the edge of the T-shaped steel and the H-shaped steel. In order to ensure the connection strength of the T-steel and the H-steel during welding, and avoid bending deformation of the T-steel and the H-steel during welding, the above-mentioned reinforcement ribs need to be removed by cutting after welding. Since the welding and removal of the reinforcement ribs are relatively cumbersome, the entire processing of the cross column is time-consuming and the processing efficiency is relatively low. On the other hand, when assembling two adjacent cross columns into a cross steel column, there is no reliable structure at the ends of the two adjacent cross columns, which makes it easy for the adjacent cross columns to be misaligned when they are aligned and welded, resulting in poor final processing quality of the cross steel column. Summary of the invention
[0004] The purpose of the present invention is to provide a cross steel column and a processing technology thereof in order to solve the above problems.
[0005] The present invention achieves the above-mentioned purpose through the following technical solutions: A cross steel column and a processing technology thereof, the cross steel column is composed of an H-shaped steel and T-shaped steels welded on the upper and lower sides of the H-shaped steel, wherein one end of the H-shaped steel and the two T-shaped steels are welded and fixed with a positioning plug, and the other ends of the H-shaped steel and the two T-shaped steels are provided with a positioning groove matching the positioning plug, and a quick-release reinforcement mechanism for reinforcing and supporting the T-shaped steel during welding is also installed on the outer side of the H-shaped steel; the processing steps of the cross steel column are as follows: Step 1: Cutting and blanking, select appropriate steel materials, and cut the steel materials into webs and wing plates of corresponding sizes according to the drawing requirements; Step 2: Bevel processing: a V-shaped welding groove is opened in the middle of the wing plate welding surface, and a V-shaped platform corresponding to the V-shaped groove on the wing plate is opened on both sides of the web; Step 3: Assemble the H-beam, place the web and wing plates on the welding machine, and use gate-type submerged arc welding for automatic welding; Step 4: T-shaped assembly, divide the assembled H-shaped steel into two parts from the middle of the web to obtain a T-shaped steel; Step 5: Correction processing: correct the assembled H-shaped steel and T-shaped steel to ensure that the overall structure of the H-shaped steel and T-shaped steel is flat and vertical without any bending; Step 6: Assemble the cross column. First, lay the assembled H-shaped steel flat, and open a welding groove in the middle of the web of the H-shaped steel. Then align the edge of the web on the T-shaped steel with the welding groove on the H-shaped steel. At the same time, use a quick-release reinforcement mechanism to clamp and support the T-shaped steel. Then weld the T-shaped steel to the H-shaped steel. After a piece of T-shaped steel is welded, remove the quick-release reinforcement mechanism. At the same time, turn the H-shaped steel over. Then, just repeat the above welding operation to complete the assembly of the cross column. Step 7: Welding and assembly of the cross steel frame columns. After the cross column is welded and formed, the two adjacent cross columns are reliably assembled with the help of the positioning plug and the positioning slot. Then the connecting parts of the two adjacent cross columns are completely welded to complete the assembly and fixation of the cross steel frame columns.
[0006] Furthermore, the quick-release reinforcement mechanism includes a guide rail with a groove at the bottom, a two-way threaded rod installed in the guide rail, clamps symmetrically installed at two sections of threaded parts with opposite rotation directions on the two-way threaded rod, connecting rods symmetrically installed on both sides of the bottom end of the guide rail, an L-shaped plate installed at the bottom end of each connecting rod, a hook plate slidably installed on one side of the bottom end of the L-shaped rod, a linkage block welded on one side wall of the hook plate, and a T-shaped adjustment bolt installed on the L-shaped plate and passing through the linkage block. When the T-steel and the annular steel are welded and assembled, the T-steel is first placed on the H-steel, and then the two sides of the wing plate of the T-steel are clamped under the action of the hook plate, and then the hook plate is fixed to the bottom end of the web of the H-steel, thereby realizing the reinforcement support of the T-steel during the welding and assembly of the H-steel.
[0007] Furthermore, both ends of the bidirectional threaded rod are rotatably connected to the guide rail, and one end of the bidirectional threaded rod is provided with a cross swivel. Such a design can realize convenient rotation adjustment of the bidirectional threaded rod.
[0008] Furthermore, the top end of the connecting rod is hinged to the guide rail, and the bottom end of the connecting rod is hinged to the L-shaped plate. Under the action of the connecting rod, the guide rail and the L-shaped plate can be connected into one.
[0009] Furthermore, the T-shaped adjusting bolt is rotatably connected to the L-shaped plate, and the T-shaped adjusting bolt is threadably connected to the linkage block. Rotating the T-shaped adjusting bolt can adjust the height of the hook plate to achieve reliable tightening of the hook plate against the bottom end of the upper wing plate of the H-shaped steel.
[0010] Furthermore, in step 1, before cutting the steel, it is necessary to remove the debris on the surface of the steel by wiping and cleaning. This design can effectively avoid the adverse effects of debris on the surface of the steel on the welding quality during welding.
[0011] Furthermore, in the step 3, when assembling the H-beam, the groove weld should first be primed with CO2 gas shielded welding and then covered with submerged arc welding. This design can effectively avoid damage defects in the welds on the H-beam in the welding transfer layer.
[0012] Furthermore, when assembling the T-steel in step 4, an appropriate welding allowance should be reserved in the height direction of the H-steel for cutting. Such a design can effectively avoid excessive deformation of the T-steel after welding on the H-steel.
[0013] Furthermore, in the step 2, a flame cutting machine should be used to cut the groove, and the oxides on the groove surface and the groove edge should be cleaned in time after cutting. Such a design can effectively ensure that the weld width and thickness at the groove after welding are uniform.
[0014] Furthermore, in step 5, the correction method of combining mechanical roller correction with flame correction is mainly adopted for the correction processing of H-shaped steel and T-shaped steel, which can effectively ensure the stability of the overall structure of H-shaped steel and T-shaped steel and avoid complete deformation.
[0015] The beneficial effects of the present invention are: On the one hand, the present invention uses a quick-release reinforcement mechanism to achieve support and fixation of T-shaped steel and H-shaped steel during welding, which not only avoids excessive deformation of T-shaped steel and H-shaped steel during welding, but also facilitates rapid disassembly of the quick-release reinforcement mechanism, avoids tedious operations of repeated welding and cutting, and greatly shortens the entire processing time of the cross steel column, improves processing efficiency, and simultaneously cooperates with the positioning plug and the positioning slot to achieve reliable limiting of two adjacent cross columns during welding and assembly, avoids mutual misalignment of two adjacent cross columns during welding, and improves the final processing quality of the cross steel column. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a structural schematic diagram of a cross steel frame column and a cross steel frame column in a processing technology thereof according to the present invention; Figure 2It is a rear view of a cross steel column and a processing technology thereof according to the present invention; Figure 3 It is a cross-sectional view of a cross steel column and a quick-release reinforcement mechanism used in its processing technology according to the present invention; Figure 4 The present invention is a process flow chart of a cross steel column and its processing technology.
[0017] The accompanying drawings are described as follows: 1. H-shaped steel; 2. Positioning plug; 3. T-shaped steel; 4. Quick-release reinforcement mechanism; 401. Guide rail; 402. Clamp; 403. L-shaped plate; 404. T-shaped adjustment bolt; 405. Linkage block; 406. Hook plate; 407. Connecting rod; 408. Bidirectional threaded rod; 5. Positioning slot. DETAILED DESCRIPTION
[0018] A cross steel column and its processing technology, the cross steel column is composed of an H-shaped steel 1 and T-shaped steels 3 welded on the upper and lower sides of the H-shaped steel 1, wherein one end of the H-shaped steel 1 and the two T-shaped steels 3 are welded and fixed with a positioning plug 2, and the other ends of the H-shaped steel 1 and the two T-shaped steels 3 are provided with a positioning groove matching the positioning plug 2, and the outer side of the H-shaped steel 1 is also installed with a quick-release reinforcement mechanism 4 for reinforcing and supporting the T-shaped steel 3 during welding; the processing steps of the cross steel column are as follows: Step 1: Cutting and blanking, select appropriate steel materials, and cut the steel materials into webs and wing plates of corresponding sizes according to the drawing requirements; Step 2: Bevel processing: a V-shaped welding groove is opened in the middle of the wing plate welding surface, and a V-shaped platform corresponding to the V-shaped groove on the wing plate is opened on both sides of the web; Step 3: Assemble the H-shaped steel 1, place the web and the wing plate on the welding machine, and use gate-type submerged arc welding for automatic welding; Step 4: T-shaped assembly, the assembled H-shaped steel 1 is divided into two parts from the middle of the web to obtain the T-shaped steel 3; Step 5: Correction processing: correct the assembled H-shaped steel 1 and T-shaped steel 3 to ensure that the overall structure of the H-shaped steel 1 and T-shaped steel 3 is flat and vertical without any bending; Step 6: Assembling the cross column, first lay the assembled H-beam 1 flat, and open a welding groove in the middle of the web of the H-beam 1, then align the web edge of the T-beam 3 with the welding groove on the H-beam 1, and use the quick-release reinforcement mechanism 4 to clamp and support the T-beam 3, and then weld the T-beam 3 to the H-beam 1. After a piece of T-beam 3 is welded, remove the quick-release reinforcement mechanism 4, and at the same time turn the H-beam 1 over. Then just repeat the above welding operation to complete the assembly of the cross column; Step 7: Welding and assembling of the cross steel column. After the cross column is welded and formed, the positioning insert and the positioning slot 5 are used to realize the reliable assembly of two adjacent cross columns, and then the connecting parts of the two adjacent cross columns are completely welded to complete the assembly and fixation of the cross steel columns.
[0019] In this embodiment, the quick-release reinforcement mechanism 4 includes a guide rail 401 with a groove at the bottom, a bidirectional threaded rod 408 installed in the guide rail 401, a clamping plate 402 symmetrically installed at two sections of the bidirectional threaded rod 408 with opposite threaded parts, a connecting rod 407 symmetrically installed on both sides of the bottom end of the guide rail 401, an L-shaped plate 403 installed at the bottom end of each connecting rod 407, a hook plate 406 slidably installed on one side of the bottom end of the L-shaped rod, a linkage block 405 welded on one side wall of the hook plate 406, and a T-shaped adjustment bolt 404 installed on the L-shaped plate 403 and passing through the linkage block 405. When the T-shaped steel 3 is welded and assembled with the annular steel, the T-shaped steel 3 is first placed on the H-shaped steel 1, and then the two sides of the wing plate of the T-shaped steel 3 are clamped under the action of the hook plate 406, and then the hook plate 406 is fixed to the bottom end of the web of the H-shaped steel 1, so as to realize the reinforcement support of the T-shaped steel 3 when the H-shaped steel 1 is welded and assembled.
[0020] In this embodiment, both ends of the bidirectional threaded rod 408 are rotatably connected to the guide rail 401 , and one end of the bidirectional threaded rod 408 is provided with a cross swivel, so that the bidirectional threaded rod 408 can be easily rotated and adjusted.
[0021] In this embodiment, the top end of the connecting rod 407 is hinged to the guide rail 401 , and the bottom end of the connecting rod 407 is hinged to the L-shaped plate 403 . Under the action of the connecting rod 407 , the guide rail 401 and the L-shaped plate 403 can be connected into one.
[0022] In this embodiment, the T-shaped adjustment bolt 404 is rotatably connected to the L-shaped plate 403, and the T-shaped adjustment bolt 404 is threadedly connected to the linkage block 405. Rotating the T-shaped adjustment bolt 404 can adjust the height of the hook plate 406 to achieve reliable tightening of the hook plate 406 on the bottom end of the upper wing plate of the H-shaped steel 1.
[0023] In this embodiment, in step 1, before cutting the steel, it is necessary to remove debris on the surface of the steel by wiping and cleaning. This design can effectively avoid the adverse effects of debris on the surface of the steel on the welding quality during welding.
[0024] In this embodiment, when assembling the H-beam 1 in step 3, the groove weld should first be primed with CO2 gas shielded welding and then covered with submerged arc welding. This design can effectively avoid damage defects in the weld on the H-beam 1 in the welding transfer layer.
[0025] In this embodiment, when assembling the T-steel 3 in step 4, an appropriate welding allowance should be reserved in the height direction of the H-steel 1 for cutting. This design can effectively avoid excessive deformation of the T-steel 3 after welding on the H-steel 1.
[0026] In this embodiment, in step 2, a flame cutting machine should be used to cut the groove, and the oxides on the groove surface and the groove edge should be cleaned in time after cutting. This design can effectively ensure that the weld width and thickness at the groove after welding are uniform.
[0027] In this embodiment, in step 5, a correction method combining mechanical roller correction and flame correction is mainly adopted for the correction processing of the H-shaped steel 1 and the T-shaped steel 3, which can effectively ensure the stability of the overall structure of the H-shaped steel 1 and the T-shaped steel 3 and avoid complete deformation.
[0028] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A cross steel column and its processing technology, characterized by: The cross steel column is composed of an H-shaped steel (1) and T-shaped steels (3) welded to the upper and lower sides of the H-shaped steel (1), wherein one end of the H-shaped steel (1) and the two T-shaped steels (3) are welded and fixed with a positioning plug (2), and the other ends of the H-shaped steel (1) and the two T-shaped steels (3) are provided with a positioning groove matching the positioning plug (2), and a quick-release reinforcement mechanism (4) for reinforcing and supporting the T-shaped steel (3) during welding is also installed on the outer side of the H-shaped steel (1); the processing steps of the cross steel column are specifically as follows: Step 1: Cutting and blanking, select appropriate steel materials, and cut the steel materials into webs and wing plates of corresponding sizes according to the drawing requirements; Step 2: Bevel processing: a V-shaped welding groove is opened in the middle of the wing plate welding surface, and a V-shaped platform corresponding to the V-shaped groove on the wing plate is opened on both sides of the web; Step 3: Assemble the H-shaped steel (1), place the web and wing plates on a welding machine, and perform automatic welding using gate-type submerged arc welding; Step 4: T-shaped assembly, the assembled H-shaped steel (1) is divided into two parts along the middle of the web to obtain a T-shaped steel (3); Step 5: Correction processing, correcting the assembled H-shaped steel (1) and T-shaped steel (3) to ensure that the overall structure of the H-shaped steel (1) and T-shaped steel (3) is flat and vertical without any bending; Step 6: Assembling the cross column, first lay the assembled H-shaped steel (1) flat, and open a welding groove in the middle of the web of the H-shaped steel (1), then align the web edge of the T-shaped steel (3) with the welding groove on the H-shaped steel (1), and use the quick-release reinforcement mechanism (4) to clamp and support the T-shaped steel (3), and then weld the T-shaped steel (3) to the H-shaped steel (1). After a piece of T-shaped steel (3) is welded, remove the quick-release reinforcement mechanism (4), and at the same time turn over the H-shaped steel (1), and then repeat the above welding operation to complete the assembly of the cross column; Step 7: Welding and assembling of the cross steel column. After the cross column is welded and formed, the positioning insert and the positioning slot (5) are used to realize the reliable assembly of two adjacent cross columns. Then, the connecting parts of the two adjacent cross columns are completely welded to complete the assembly and fixation of the cross steel columns.
2. The cross steel column and its processing technology according to claim 1 are characterized in that: The quick-release reinforcement mechanism (4) comprises a guide rail (401) with a groove at the bottom, a bidirectional threaded rod (408) installed in the guide rail (401), a clamping plate (402) symmetrically installed at two sections of the bidirectional threaded rod (408) with opposite threaded parts, connecting rods (407) symmetrically installed at both sides of the bottom end of the guide rail (401), an L-shaped plate (403) installed at the bottom end of each connecting rod (407), a hook plate (406) slidably installed on one side of the bottom end of the L-shaped rod, a linkage block (405) welded to a side wall of the hook plate (406), and a T-shaped adjustment bolt (404) installed on the L-shaped plate (403) and passing through the linkage block (405).
3. The cross steel column and its processing technology according to claim 2 are characterized in that: Both ends of the bidirectional threaded rod (408) are rotatably connected to the guide rail (401), and one end of the bidirectional threaded rod (408) is provided with a cross swivel.
4. The cross steel column and its processing technology according to claim 2, characterized in that: The top end of the connecting rod (407) is hinged to the guide rail (401), and the bottom end of the connecting rod (407) is hinged to the L-shaped plate (403).
5. The cross steel column and its processing technology according to claim 2, characterized in that: The T-shaped adjusting bolt (404) is rotatably connected to the L-shaped plate (403), and the T-shaped adjusting bolt (404) is threadedly connected to the linkage block (405).
6. The cross steel column and the processing technology thereof according to claim 1 are characterized in that: In step 1, before cutting the steel, it is necessary to remove the debris on the surface of the steel by wiping and cleaning.
7. The cross steel column and the processing technology thereof according to claim 1 are characterized in that: In step 3, when assembling the H-beam (1), the groove weld should first be primed with CO2 gas shielded welding and then covered with submerged arc welding.
8. The cross steel column and the processing technology thereof according to claim 1 are characterized in that: When assembling the T-shaped steel (3) in step 4, an appropriate welding margin should be reserved in the height direction of the H-shaped steel (1) for cutting.
9. The cross steel column and the processing technology thereof according to claim 1 are characterized in that: In the step 2, a flame cutting machine should be used to cut the groove when processing the groove, and the oxides on the groove surface and the groove edge should be cleaned in time after cutting.
10. The cross steel column and the processing technology thereof according to claim 1, characterized in that: In the step 5, when correcting the H-shaped steel (1) and the T-shaped steel (3), a correction method combining mechanical roller correction and flame correction is mainly adopted.
Citation Information
Patent Citations
Quick positioning device and method for cross columns
CN105014282A
Processing and manufacturing method of wall-mounted cross crane beam
CN115383407A
Cross-shaped steel structure and machining process thereof
CN116393889A
Cross column welding jacking tool
CN212330195U
Clamping and positioning tool based on polishing machining technology
CN218364054U
Cited By
Steel structure cross column welding method
CN121447306A
A steel structure cross column welding method
CN121447306B
Cross steel column welding device
CN121733101A