Stretch-proof blended fabric and preparation method thereof
Through multi-layer structural design and process optimization, the problem of the reduced tensile performance of blended fabrics after long-term use is solved, extending the service life and improving the breathability, antibacterial effect and comfort of the fabric.
Patent Information
- Application Number
- CN202411529442.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-30
- Publication Date
- 2024-12-06
AI Technical Summary
After a long time of use, the tensile performance of the blended fabric will decrease, affecting the use feeling.
Using multi-layer structural designs such as wear-resistant layer, breathable layer, ultraviolet layer, anti-static layer, bacteriostatic layer, tensile layer, braided layer and chemical fiber layer, the overall performance of the fabric is improved through the sewing and extrusion process, including There are equally spaced breathable holes on the breathable layer, and the antibacterial beads are filled with antibacterial beads. The stretching layer and braided layer improve the stretchability, and the skin-friendly layer made of pure cotton improves comfort.
It extends the service life of the fabric, improves breathability, antibacterial effect and comfort, and enhances the overall performance of the fabric, especially the stretchability and heat dissipation effect.
Smart Images

Figure CN119078303A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of blended fabrics, in particular to a stretch-resistant blended fabric and a preparation method thereof. Background Art
[0002] Blended fabrics combine the advantages of polyester and cotton fabrics. They have the advantages of good elasticity and good wear resistance. At the same time, they are not easily shrunk. Blended fabrics are widely used in the production of T-shirts, shirts, and skirts. For example, a blended fabric and its production method with publication number CN111778612A is made of yarns of two materials, cotton fiber and viscose fiber. In the finished fabric, cotton fiber accounts for 53% and viscose fiber accounts for 47%. This blended fabric solves the problem of excessive shrinkage of single viscose fiber, and the color fastness to friction and alkali sweat exceeds the national standard. At the same time, the production method of the blended fabric of the present invention, through the technique of dyeing first and then jacquard, more prominently expresses the flower type and pattern, and the fabric produced by jacquard organization can meet the international shrinkage index; When blended fabrics are used, they will be stretched due to various situations. After the blended fabrics are used for a long time, the tensile properties of the blended fabrics will decrease, which will affect the usage experience of subsequent users. Therefore, we propose a stretch-resistant blended fabric and a preparation method thereof to solve the above-mentioned problems. Summary of the invention
[0003] The purpose of the present invention is to provide a stretch-resistant blended fabric and a preparation method thereof, so as to solve the problem that the blended fabric proposed in the above background technology will be stretched due to various situations when in use, and after the blended fabric is used for a long time, the tensile performance of the blended fabric will be reduced, which will affect the use experience of subsequent users.
[0004] To achieve the above object, the present invention provides the following technical solutions: a stretch-resistant blended fabric and a preparation method thereof, comprising a wear-resistant layer, the wear-resistant layer is made of bamboo charcoal fiber, and a breathable layer is sewn and connected to the lower surface of the wear-resistant layer, and the breathable layer is made of silk; A stretch-resistant blended fabric and a preparation method thereof, further comprising: An anti-ultraviolet layer, wherein the anti-ultraviolet layer is sewn and connected to the lower surface of the breathable layer, and the anti-ultraviolet layer is polyester pongee; The antistatic layer is sewn and connected to the lower surface of the anti-ultraviolet layer, and the material of the antistatic layer is mixed fabric.
[0005] Preferably, the surface of the breathable layer is provided with air holes, and the air holes are "Y"-shaped when viewed from the front, and the air holes are evenly spaced inside the breathable layer. By setting evenly spaced "Y"-shaped air holes, the overall air permeability of the fabric is optimized.
[0006] Preferably, the lower surface of the antistatic layer is sewn and connected with an antibacterial layer, and the material of the antibacterial layer is silver ion antibacterial fabric, and antibacterial beads are arranged inside the antibacterial layer. The multiple antibacterial beads effectively improve the overall antibacterial effect of the fabric and also have the effect of removing mites.
[0007] Preferably, the lower surface of the antibacterial layer is sewn and connected with a stretch layer, and the material of the stretch layer is cotton and linen, and the lower surface of the stretch layer is sewn and connected with a woven layer, and a heat dissipation channel is opened inside the woven layer, and the stretch layer and the woven layer both improve the overall stretchability of the fabric and extend the overall service life of the fabric.
[0008] Preferably, the heat dissipation channels are distributed in a criss-cross manner inside the woven layer, and the material of the woven layer is Lycra fabric, and the lower surface of the woven layer is sewn and connected with a chemical fiber layer. The criss-cross distribution of the heat dissipation channels further optimizes the overall heat dissipation effect of the fabric and optimizes the user experience.
[0009] Preferably, the lower surface of the chemical fiber layer is sewn and connected with a skin-friendly layer, and the skin-friendly layer is made of pure cotton, and heat dissipation holes are opened at equal intervals on the lower surface of the skin-friendly layer. The skin-friendly layer made of pure cotton makes the fabric more comfortable as a whole and further optimizes the use experience.
[0010] A method for preparing a stretch-resistant blended fabric comprises the following steps: S1: Raw material processing steps: S11: Place raw materials such as cotton and fiber into the opener, release the pressure, and restore the raw materials to a soft state; S12: Combing the raw materials with a carding machine that drives a vibration structure to clean the impurities inside the raw materials, while fully mixing the fibers and increasing the uniformity of the fabric; S2: Drawing process: S21: Connect the combed raw materials to the drawing frame to mix the raw materials of different types and qualities evenly and finally reach the mixing ratio according to the regulations; S3: Combing process: S31: Arrange the raw materials after drawing on the combing machine to discharge the shorter fibers and make the fibers further straighten and parallel, improve the overall quality, and finally generate the chemical fiber layer; S4: Textile process: S41: using a hole-opening device, opening air holes on the upper surface of the air-permeable layer, opening a heat dissipation channel inside the woven layer, and then opening a heat dissipation port on the lower surface of the skin-friendly layer; S41: using a textile machine to sew the wear-resistant layer and the breathable layer together, then sew the lower surface of the breathable layer to the anti-ultraviolet layer, and then sew the lower surface of the anti-ultraviolet layer to the antistatic layer; S43: sewing the lower surface of the antistatic layer to the antibacterial layer, filling the antibacterial bead particles into the antibacterial layer, and then sewing the antibacterial layer to the upper surface of the stretch layer; S44: sewing the lower surface of the stretch layer to the woven layer, then sewing the lower surface of the woven layer to the upper surface of the chemical fiber layer, and finally sewing the chemical fiber layer to the upper surface of the skin-friendly layer; S45: using a fabric extrusion device to extrude the stitched fabric, and finally completing the fabric production; S5: Post-processing process: S51: Use the testing equipment to test the tensile properties of the fabric, and then use the cutting machine and packaging machine to pack the fabric.
[0011] Preferably, the operating speed of the licker-in roller inside the opener is 1660r / min, the working diameter of the licker-in roller of the carding machine is Ф225mm, the working speed of the licker-in roller of the carding machine is 625r / min, the working diameter of the cylinder is Ф425mm, and the working speed of the cylinder is 562r / min.
[0012] Preferably, when the chemical fiber layer is drawn, it needs to go through the first drawing process, the second drawing process and the third drawing process.
[0013] Preferably, during the tensile performance test, the testing device can quickly adjust the tensile strength and record the performance of the fabric under different strengths.
[0014] Compared with the prior art, the beneficial effects of the present invention are as follows: the stretch-resistant blended fabric and the preparation method thereof adopt a new structural design, and the specific contents are as follows: (1) The stretch-resistant blended fabric and its preparation method, during the preparation process, the raw materials are decompressed by an opener, and then the raw materials are combed to reduce the impurities inside the raw materials. Then, the raw materials are combed by a carding machine with a vibrating structure to clean the impurities inside the raw materials, and at the same time, the fibers are fully mixed and the uniformity of the fabric is increased, which is convenient for subsequent processing steps; (2) The stretch-resistant blended fabric and its preparation method optimize the overall air permeability of the fabric by setting "Y"-shaped air holes with equal spacing. The multiple antibacterial beads effectively improve the overall antibacterial effect of the fabric and also have the function of removing mites. The stretch layer, the woven layer and the chemical fiber layer all improve the overall stretchability of the fabric and extend the service life of the fabric. The skin-friendly layer of pure cotton material at the bottom makes the fabric more comfortable as a whole, further optimizing the use experience. (3) The stretch-resistant blended fabric and its preparation method, after the chemical fiber layer is made, the wear-resistant layer, the breathable layer, the UV protection layer, the antistatic layer, the antibacterial layer, the stretch layer, the woven layer, the chemical fiber layer and the skin-friendly layer are sewn together by sewing, and then the sewn fabric is extruded by a fabric extrusion device to finally complete the fabric production. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the front cross-sectional structure of the present invention; Figure 2 For the present invention Figure 1 The enlarged structural diagram at A in the middle; Figure 3 This is a schematic diagram of the structure of the skin-friendly layer of the present invention when viewed from above; Figure 4 It is a partial side view of the structure of the present invention.
[0016] In the figure: 1. Wear-resistant layer; 2. Breathable layer; 3. Breathable holes; 4. UV protection layer; 5. Antistatic layer; 6. Antibacterial layer; 7. Antibacterial beads; 8. Stretch layer; 9. Woven layer; 10. Chemical fiber layer; 11. Skin-friendly layer; 12. Heat dissipation port; 13. Heat dissipation channel. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0018] See also Figure 1-Figure 4 The present invention provides a technical solution: a stretch-resistant blended fabric and a preparation method thereof, comprising a wear-resistant layer 1, the material of the wear-resistant layer 1 is bamboo charcoal fiber, and the lower surface of the wear-resistant layer 1 is sutured and connected with a breathable layer 2, and the material of the breathable layer 2 is silk; A stretch-resistant blended fabric and a preparation method thereof, further comprising: The anti-ultraviolet layer 4 is sewn and connected to the lower surface of the breathable layer 2, and the anti-ultraviolet layer 4 is polyester pongee; The antistatic layer 5 is sewn and connected to the lower surface of the anti-ultraviolet layer 4, and the material of the antistatic layer 5 is mixed woven fabric.
[0019] The surface of the breathable layer 2 is provided with breathable holes 3 , and the front cross-section of the breathable holes 3 is a “Y” shape, and the breathable holes 3 are evenly spaced and distributed inside the breathable layer 2 .
[0020] The antibacterial layer 6 is sewn and connected to the lower surface of the antistatic layer 5 . The antibacterial layer 6 is made of silver ion antibacterial fabric, and antibacterial beads 7 are arranged inside the antibacterial layer 6 .
[0021] The lower surface of the antibacterial layer 6 is sutured and connected with a stretch layer 8 made of cotton and linen. The lower surface of the stretch layer 8 is sutured and connected with a braided layer 9 , and a heat dissipation channel 13 is opened inside the braided layer 9 .
[0022] The heat dissipation channels 13 are distributed in a crisscross pattern inside the braided layer 9 , and the braided layer 9 is made of Lycra fabric, and the lower surface of the braided layer 9 is sewn and connected with a chemical fiber layer 10 .
[0023] The lower surface of the chemical fiber layer 10 is sutured and connected with a skin-friendly layer 11 , and the skin-friendly layer 11 is made of pure cotton, and heat dissipation openings 12 are opened at equal intervals on the lower surface of the skin-friendly layer 11 .
[0024] A method for preparing a stretch-resistant blended fabric comprises the following steps: S1: Raw material processing steps: S11: Place raw materials such as cotton and fiber into the opener, release the pressure, and restore the raw materials to a soft state; S12: Combing the raw materials with a carding machine that drives a vibration structure to clean the impurities inside the raw materials, while fully mixing the fibers and increasing the uniformity of the fabric; S2: Drawing process: S21: Connect the combed raw materials to the drawing frame to mix the raw materials of different types and qualities evenly and finally reach the mixing ratio according to the regulations; S3: Combing process: S31: Arranging the raw materials after drawing on a combing machine to discharge shorter fibers and further straighten and parallelize the fibers to improve the overall quality, and finally generate a chemical fiber layer 10; S4: Textile process: S41: using a hole-opening device, opening a ventilation hole 3 on the upper surface of the breathable layer 2, opening a heat dissipation channel 13 inside the woven layer 9, and then opening a heat dissipation port 12 on the lower surface of the skin-friendly layer 11; S41: using a textile machine to sew the wear-resistant layer 1 and the breathable layer 2 together, then sew the lower surface of the breathable layer 2 to the anti-ultraviolet layer 4, and then sew the lower surface of the anti-ultraviolet layer 4 to the antistatic layer 5; S43: sew the lower surface of the antistatic layer 5 and the antibacterial layer 6, and fill the antibacterial beads 7 into the antibacterial layer 6, and then sew the antibacterial layer 6 and the upper surface of the stretching layer 8; S44: sewing the lower surface of the stretch layer 8 to the woven layer 9, then sewing the lower surface of the woven layer 9 to the upper surface of the chemical fiber layer 10, and finally sewing the chemical fiber layer 10 to the upper surface of the skin-friendly layer 11; S45: using a fabric extrusion device to extrude the stitched fabric, and finally completing the fabric production; S5: Post-processing process: S51: Use the testing equipment to test the tensile properties of the fabric, and then use the cutting machine and packaging machine to pack the fabric.
[0025] The working speed of the licker-in roller inside the opener is 1660r / min, the working diameter of the licker-in roller of the carding machine is: Ф225mm, the working speed of the licker-in roller of the carding machine is: 625r / min, the working diameter of the cylinder is: Ф425mm, the working speed of the cylinder is: 562r / min.
[0026] When the chemical fiber layer 10 is drawn, it needs to go through the first drawing process, the second drawing process and the third drawing process. Embodiment 2:
[0027] In order to better demonstrate the preparation method of the blended fabric, the preparation method of a stretch-resistant blended fabric in this embodiment includes the following steps: S1: Raw material processing steps: S11: Place raw materials such as cotton and fiber into the opener, release the pressure, and restore the raw materials to a soft state; S12: Combing the raw materials with a carding machine that drives a vibration structure to clean the impurities inside the raw materials, while fully mixing the fibers and increasing the uniformity of the fabric; S2: Drawing process: S21: Connect the combed raw materials to the drawing frame to mix the raw materials of different types and qualities evenly and finally reach the mixing ratio according to the regulations; S3: Combing process: S31: Arranging the raw materials after drawing on a combing machine to discharge shorter fibers and further straighten and parallelize the fibers to improve the overall quality, and finally generate a chemical fiber layer 10; S4: Textile process: S41: using a hole-opening device, opening a ventilation hole 3 on the upper surface of the breathable layer 2, opening a heat dissipation channel 13 inside the woven layer 9, and then opening a heat dissipation port 12 on the lower surface of the skin-friendly layer 11; S41: using a textile machine to sew the wear-resistant layer 1 and the breathable layer 2 together, then sew the lower surface of the breathable layer 2 to the anti-ultraviolet layer 4, and then sew the lower surface of the anti-ultraviolet layer 4 to the antistatic layer 5; S43: sew the lower surface of the antistatic layer 5 and the antibacterial layer 6, and fill the antibacterial beads 7 into the antibacterial layer 6, and then sew the antibacterial layer 6 and the upper surface of the stretching layer 8; S44: sewing the lower surface of the stretch layer 8 to the woven layer 9, then sewing the lower surface of the woven layer 9 to the upper surface of the chemical fiber layer 10, and finally sewing the chemical fiber layer 10 to the upper surface of the skin-friendly layer 11; S45: using a fabric extrusion device to extrude the stitched fabric, and finally completing the fabric production; S5: Post-processing process: S51: Use the testing equipment to test the tensile properties of the fabric, and then use the cutting machine and packaging machine to pack the fabric.
[0028] The working speed of the licker-in roller inside the opener is 1700r / min, the working diameter of the licker-in roller of the carding machine is: Ф230mm, the working speed of the licker-in roller of the carding machine is: 630r / min, the working diameter of the cylinder is: Ф430mm, the working speed of the cylinder is: 565r / min.
[0029] When the chemical fiber layer 10 is drawn, it needs to go through the first drawing process, the second drawing process and the third drawing process.
[0030] When testing tensile properties, the testing device can quickly adjust the tensile strength and record the performance of the fabric under different intensities.
[0031] The above is the working process of the entire device, and the contents not described in detail in this specification belong to the existing technology known to professional and technical personnel in this field.
[0032] In the description of the present invention, unless otherwise specified, "plurality" means two or more than two; the orientations or positional relationships indicated by the terms "upper", "lower", "left", "right", "inner", "outer", "front end", "rear end", "head", "tail", etc. are based on the orientations or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0033] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0034] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A stretch-resistant blended fabric, comprising a wear-resistant layer (1), wherein the wear-resistant layer (1) is made of bamboo charcoal fiber, and a breathable layer (2) is sewn and connected to the lower surface of the wear-resistant layer (1), and the breathable layer (2) is made of silk; It is characterized in that Also includes: an anti-ultraviolet layer (4), the anti-ultraviolet layer (4) being sewn and connected to the lower surface of the breathable layer (2), and the anti-ultraviolet layer (4) is polyester pongee; An antistatic layer (5), the antistatic layer (5) being sewn and connected to the lower surface of the anti-ultraviolet layer (4), and the material of the antistatic layer (5) is a mixed woven fabric.
2. The stretch-resistant blended fabric according to claim 1, characterized in that: The surface of the air permeable layer (2) is provided with air permeable holes (3), and the air permeable holes (3) are "Y"-shaped when viewed in a front cross-section. The air permeable holes (3) are evenly spaced and distributed inside the air permeable layer (2).
3. The stretch-resistant blended fabric according to claim 1, characterized in that: The antibacterial layer (6) is sewn and connected to the lower surface of the antistatic layer (5), and the antibacterial layer (6) is made of silver ion antibacterial fabric, and antibacterial beads (7) are arranged inside the antibacterial layer (6).
4. The stretch-resistant blended fabric according to claim 3, characterized in that: The lower surface of the antibacterial layer (6) is sutured and connected to a stretch layer (8), and the material of the stretch layer (8) is cotton and linen. The lower surface of the stretch layer (8) is sutured and connected to a braided layer (9), and a heat dissipation channel (13) is provided inside the braided layer (9).
5. The stretch-resistant blended fabric according to claim 4, characterized in that: The heat dissipation channels (13) are distributed in a crisscross pattern inside the braided layer (9), the braided layer (9) is made of Lycra fabric, and the lower surface of the braided layer (9) is sutured and connected to a chemical fiber layer (10).
6. The stretch-resistant blended fabric according to claim 5, characterized in that: The lower surface of the chemical fiber layer (10) is sutured and connected to a skin-friendly layer (11), the skin-friendly layer (11) is made of pure cotton, and heat dissipation openings (12) are provided at equal intervals on the lower surface of the skin-friendly layer (11).
7. A method for preparing a stretch-resistant blended fabric as claimed in claim 1, characterized in that: The following steps are involved: S1: Raw material processing steps: S11: Place raw materials such as cotton and fiber into the opener, release the pressure, and restore the raw materials to a soft state; S12: Combing the raw materials with a carding machine that drives a vibration structure to clean the impurities inside the raw materials, while fully mixing the fibers and increasing the uniformity of the fabric; S2: Drawing process: S21: Connect the combed raw materials to the drawing frame to mix the raw materials of different types and qualities evenly and finally reach the mixing ratio according to the regulations; S3: Combing process: S31: Arranging the raw materials after drawing on a combing machine to discharge shorter fibers and further straighten and parallelize the fibers to improve the overall quality, and finally generate a chemical fiber layer (10); S4: Textile process: S41: using a hole-opening device, opening a ventilation hole (3) on the upper surface of the breathable layer (2), opening a heat dissipation channel (13) inside the woven layer (9), and then opening a heat dissipation port (12) on the lower surface of the skin-friendly layer (11); S41: using a textile machine to sew the wear-resistant layer (1) and the breathable layer (2) together, then sew the lower surface of the breathable layer (2) to the anti-ultraviolet layer (4), and then sew the lower surface of the anti-ultraviolet layer (4) to the antistatic layer (5); S43: sewing the lower surface of the antistatic layer (5) and the antibacterial layer (6), filling the interior of the antibacterial layer (6) with antibacterial beads (7), and then sewing the antibacterial layer (6) and the upper surface of the stretch layer (8); S44: sewing the lower surface of the stretch layer (8) and the woven layer (9), then sewing the lower surface of the woven layer (9) and the upper surface of the chemical fiber layer (10), and finally sewing the chemical fiber layer (10) and the upper surface of the skin-friendly layer (11); S45: using a fabric extrusion device to extrude the stitched fabric, and finally completing the fabric production; S5: Post-processing process: S51: Use the testing equipment to test the tensile properties of the fabric, and then use the cutting machine and packaging machine to pack the fabric.
8. The stretch-resistant blended fabric and preparation method thereof according to claim 7, characterized in that: The working speed of the licker-in roller inside the opener is 1660r / min, the working diameter of the licker-in roller of the carding machine is Ф225mm, the working speed of the licker-in roller of the carding machine is 625r / min, the working diameter of the cylinder is Ф425mm, and the working speed of the cylinder is 562r / min.
9. The stretch-resistant blended fabric and the preparation method thereof according to claim 8, characterized in that: When the chemical fiber layer (10) is drawn, it needs to go through the first drawing process, the second drawing process and the third drawing process.
10. The stretch-resistant blended fabric and preparation method thereof according to claim 9, characterized in that: During the tensile performance test, the testing device can quickly adjust the tensile strength and record the performance of the fabric under different strengths.
Citation Information
Patent Citations
Blended fabric and manufacturing method thereof
CN111778612A