Plasma chemical vapor deposition (PCVD) process uniform deposition system and method
Patent Information
- Application Number
- CN202411210380.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-12-06
AI Technical Summary
The axial unevenness caused by uneven temperature of the reaction gas in the existing PCVD process affects the quality of the quartz glass deposition layer and the refractive index distribution of the optical fiber preform rod.
By setting a rotary sealing chuck and microwave resonant cavity in the PCVD deposition system, the microwave output power and frequency are dynamically adjusted using a solid microwave source to control the gas phase reaction deposition to achieve the axial uniformity of liner deposition.
It improves the refractive index distribution accuracy of optical fiber preform rods, reduces equipment energy consumption and losses, extends the life of the microwave system, reduces defects such as bubbles and cracks, and improves deposition quality and stability.
Smart Images

Figure CN119082712A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a PCVD process uniform deposition system and method, belonging to the technical field of optical fiber preform preparation. Background Art
[0002] The PCVD (plasma chemical vapor deposition) process is a plasma chemical vapor deposition method. It performs high-temperature oxidation reaction and vapor deposition in a pure quartz glass tube. The raw material gas for the reaction can be SiCl4, O2, GeCl4, C2F6 and a small amount of dopant. The heat source used for the reaction is microwave. The reaction mechanism is that microwaves activate the gas to generate plasma to ionize the reaction gas. After ionization, the charged ions recombine to release heat energy to generate gaseous reactants, and transparent quartz glass is formed in an environment with a temperature of about 1000°C and deposited on the inner wall of the pure quartz glass tube to form a silicon dioxide doped layer with different refractive indices, which is then melted and corroded to finally form a solid preform.
[0003] In the existing PCVD process, the reaction raw material gas enters the glass liner through a conduit, and the microwave resonant cavity moves along the axial direction of the liner to vitrify the raw material reaction, and the tailings after the reaction are pumped out from the other end of the liner by a vacuum pump. Usually, the preform obtained by PCVD deposition has the problem of axial non-uniformity, because the temperature of the reaction gas is low when it enters the liner, generally below 100°C. The low inlet temperature of the reaction gas is not conducive to the formation of a transparent and defect-free quartz glass deposition layer during the deposition process. For example, the low temperature of the reaction gas will cause bubbles in the core rod or cracks in the deposition layer. If the reaction gas is higher than 100°C, it will not only cause damage to the gas flow controller, but also accelerate the aging of the rubber sealing ring of the pneumatic valve and cause uncontrolled leakage. In order to avoid this phenomenon, the temperature of the inlet end will be artificially increased inside the insulation furnace so that the temperature of the reaction gas is increased before entering the microwave reaction cavity. Increasing the temperature of the inlet end in the insulation furnace can prevent cracks from appearing on the inner wall of the deposition area of the inlet end of the liner, but the disadvantage is that increasing the temperature of the gas end in the insulation furnace will reduce the deposition efficiency of Ge in this area, increase the deposition efficiency of F, and cause uneven deposition. The temperature at the pump end of the holding furnace is generally higher because, on the one hand, the gas raw material in the liner flows to the pump end, bringing part of the heat to the pump end, and on the other hand, artificially increasing the furnace temperature at the pump end can prevent the reaction tail from forming cracks in the deposition layer at the end of the liner. However, a high temperature at the pump end will also reduce the deposition efficiency of Ge, causing the refractive index of the preform to decrease in this area.
[0004] At present, the common solution to the problem of non-uniformity caused by low Ge doping efficiency due to high PCVD deposition temperature is to control the temperature so that the temperature field of the entire insulation furnace tends to be uniform. Patent CN108046583A discloses welding extension tubes at both ends of the glass liner tube, adding a preheating pipeline heating device to the gas end extension tube, and preheating the reaction gas in advance through the heating device to avoid the generation of cracks. This method does not fully preheat the gas raw material and also increases the material cost of the extension tube. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a PCVD process uniform deposition system and method to address the deficiencies in the prior art, which can dynamically and real-time adjust the microwave output power, control the gas phase reaction deposition, and achieve axial uniformity of liner deposition.
[0006] The deposition system technical solution adopted by the present invention to solve the above-mentioned problems is:
[0007] It includes rotary sealing chucks coaxially arranged on both sides of the bed, the rotary sealing chucks on both sides are connected to a synchronous rotation driving device, a microwave resonance cavity is arranged between the two rotary sealing chucks, the microwave resonance cavity is arranged in a heat preservation furnace, the microwave resonance cavity extends out of the heating furnace through a waveguide and is connected to a microwave generating device and an axial reciprocating device, the two rotary sealing chucks include an air intake rotary sealing chuck and an exhaust rotary sealing chuck, the air intake rotary sealing chuck is connected to a raw material gas source through an air intake pipe, and the exhaust rotary sealing chuck is connected to a vacuum pump exhaust system through an exhaust pipe, and is characterized in that the microwave generating device includes a solid-state microwave source power supply and a solid-state microwave source, and the output end of the solid-state microwave source is connected to the waveguide through a circulator.
[0008] According to the above scheme, the solid-state microwave source is a frequency-adjustable solid-state microwave source; the frequency adjustment range of the frequency-adjustable solid-state microwave source is 2380-2520MHz.
[0009] According to the above scheme, the power of the solid-state microwave source is adjustable when the frequency is fixed, and the power adjustment range is 1000W-15000W.
[0010] According to the above scheme, a three-pin automatic distributor is connected in series between the circulator and the waveguide, and the three-pin automatic distributor is used to detect the output power of the solid-state microwave source and the reflected power returned by the resonant cavity.
[0011] According to the above scheme, the resonant frequency of the microwave resonant cavity is 2450±30MHz.
[0012] According to the above scheme, the waveguide includes a straight waveguide and a curved waveguide, and the waveguide is connected to the resonant cavity.
[0013] According to the above scheme, the insulation furnace is provided with three temperature zones, namely, the gas end, the middle, and the pump end, and each temperature zone is provided with a temperature sensor.
[0014] According to the above scheme, the solid-state microwave source power supply is provided with a PLC control unit to automatically adjust the output microwave frequency according to the position of the microwave resonant cavity.
[0015] The technical solution of the PCVD process deposition method adopted by the present invention to solve the above problems is:
[0016] A pure glass liner is used as a base tube and clamped on the rotary sealing chucks on both sides of the PCVD deposition system. The insulation furnace is heated to 920°C to 1150°C. The raw gas enters the liner from the gas end (inlet rotary sealing chuck). The microwave resonant cavity moves back and forth from the gas end to the pump end (exhaust rotary sealing chuck) along the axial direction of the liner to perform PCVD deposition processing. The solid-state microwave source of the microwave generating device has the same preset output power. The frequency of the output microwave is adjusted and changed according to the position of the microwave resonant cavity. The period of frequency change is consistent with the period of the microwave resonant cavity moving from the gas end to the pump end. When the microwave resonant cavity is in the gas end area, the starting frequency of the output microwave is consistent with the resonant frequency of the microwave resonant cavity. The microwave resonant cavity moves from the gas end area through the middle area to the pump end area. The frequency of the output microwave gradually changes. When it reaches the pump end area, the frequency returns to the starting frequency. When the microwave resonant cavity returns from the pump end area through the middle area to the gas end area, the frequency of the output microwave gradually changes. When it reaches the gas end, the frequency returns to the starting frequency. This cycle is repeated until the deposition is completed.
[0017] According to the above scheme, the frequency of the output microwave gradually changes so that the frequency of the output microwave gradually increases or decreases relative to the starting frequency. The starting frequency is the output microwave frequency that is consistent with the resonant frequency of the microwave resonant cavity and at which the reflected power reaches the minimum value.
[0018] According to the above scheme, when the output microwave frequency gradually increases or decreases relative to the initial frequency, the power used for deposition in the microwave resonance cavity decreases, the reflected power increases, and the reflected power is absorbed by the circulator.
[0019] According to the above scheme, the insulation furnace is provided with three temperature zones: gas end, middle and pump end. The temperature of the gas end zone is 1000℃~1100℃, the temperature of the middle zone is 950℃~1000℃, and the temperature of the pump end zone is 970℃~1060℃.
[0020] The beneficial effects of the present invention are as follows: 1. During the deposition process, the deposition power of the resonant cavity is dynamically and real-time adjusted by adjusting the frequency of the output microwave, so that the microwave frequency can be adjusted along the axial direction of the liner tube. By adjusting the matching degree between the frequency of the solid-state microwave source and the resonant frequency of the resonant cavity, the axial region reaction absorption power is controlled, the gas phase reaction deposition is controlled, the deposition rate of each region is balanced, and the temperature difference of each region in the holding furnace is reduced, thereby improving the axial uniformity of the liner tube deposition. In particular, the uniformity of the doping deposition can be improved, thereby improving the accuracy of the refractive index distribution of the optical fiber preform. 2. Using a solid-state microwave source microwave generator, on the one hand, the microwave frequency can be directly adjusted to match the frequency of the resonant cavity, so that the output frequency and the use frequency are more matched, and the reflected power of the entire high-frequency system is lower, generally lower than 20W. This not only reduces energy consumption and equipment loss, but also greatly reduces the difficulty of debugging the microwave source high-frequency system. 3. The solid-state microwave source has a long service life and no power attenuation problem, which improves the use stability of the high-frequency microwave device, reduces defects such as bubbles and cracks in the optical fiber preform, and thus improves the deposition quality of the optical fiber preform. The present invention has a high degree of automation, a longer microwave system life, simple operation, and is easy to implement. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic structural diagram of an embodiment of a deposition system of the present invention.
[0022] Figure 2 Schematic diagram of the structure of a microwave system in one embodiment of the deposition system of the present invention.
[0023] Figure 3 1 is a temperature distribution diagram of the holding furnace of the embodiment of the present invention and the comparative example.
[0024] Figure 4 1 is a distribution diagram of the resonant cavity position and microwave frequency according to an embodiment of the present invention.
[0025] Figure 5 The relative refractive index full map of the core layer of the optical fiber preform core rod of the embodiment of the present invention and the comparative example.
[0026] Figure 6 It is a full-scale measurement diagram of the core diameter of the optical fiber preform core rod according to the embodiment of the present invention and the comparative example. DETAILED DESCRIPTION
[0027] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0028] The embodiment of the deposition system of the present invention is as follows Figure 1 , Figure 2As shown, it includes coaxially corresponding rotary sealing chucks arranged on both sides of the bed, the rotary sealing chucks on both sides are connected to the synchronous rotation driving device, a microwave resonant cavity 6 is arranged between the two rotary sealing chucks, and the microwave resonant cavity is arranged in the heat preservation furnace 9, and the heat preservation furnace is provided with three temperature zones of gas end, middle and pump end, and each temperature zone is provided with a temperature sensor. The microwave resonant cavity extends out of the heating furnace through a waveguide and is connected to the microwave generating device and the axial reciprocating device, the two rotary sealing chucks include an intake rotary sealing chuck 1 and an exhaust rotary sealing chuck 2, the intake rotary sealing chuck is connected to the raw material gas source through an intake pipe, and the exhaust rotary sealing chuck is connected to the vacuum pump exhaust system through an exhaust pipe, and the microwave generating device includes a solid-state microwave source power supply 10 and a solid-state microwave source 11, and the solid-state microwave source power supply is provided with a PLC control unit to automatically adjust the output microwave frequency according to the position of the microwave resonant cavity. The output end of the solid-state microwave source is connected to a waveguide 14 through a circulator 12 and a three-pin automatic distributor 13. The waveguide includes a straight waveguide and a curved waveguide. The waveguide is connected to a microwave resonant cavity 15. The resonant frequency of the microwave resonant cavity is 2450 MHz.
[0029] Two comparative examples are used to compare the PCVD deposition method with the present invention.
[0030] Comparative Example 1: The reaction gas at a relatively low temperature enters the insulation furnace 9 and the liner 4 area through the gas end rotary chuck 1 and the extension tube 3. The gas is heated and reacts in the reciprocating microwave resonant cavity 6 to produce glass deposited on the inner wall of the liner. The exhaust gas and dust particles are pumped away by the vacuum pump through the pump end extension tube 5 and the pump end rotary chuck 2. The insulation furnace is divided into a gas end area, a middle area and a pump end area. The microwave generator 8 generates microwaves that enter the microwave resonant cavity through the waveguide column 7. The frequency of the microwave resonant cavity is 2450MHz. In order to ensure that there are no cracks in the core rod deposition area, the furnace temperature is set higher in the gas end area and the pump end area, with the gas end area having the highest temperature. Figure 3 Scheme 1 is the temperature setting used during deposition, with the gas end area set at 1090°C, the middle area set at 980°C, and the pump end area set at 1040°C. The microwave power is set to 7000W, and the microwave frequency emitted by the magnetron is 2450MHz, so that the raw gas enters the liner from the gas end rotating chuck, and the resonant cavity reciprocates along the liner. The relative refractive index and core diameter test results of the core rod produced with this parameter are shown in Figure 5 and Figure 6 Solution 1.
[0031] Comparative Example 2: In order to increase the relative refractive index of the core rod in the gas end and pump end regions, Scheme 2 reduced the furnace temperature at both ends, the gas end setting value was reduced from 1090°C to 1050°C, and the pump end setting value was reduced from 1040°C to 1020°C. The actual furnace temperature is shown in Figure 3Solution 2. The microwave power is set to 7000W, and the microwave frequency emitted by the magnetron is 2450MHz. The relative refractive index and core diameter test results of the core rod produced with this parameter are shown in Figure 5 and Figure 6 In Scheme 2, the uniformity of core rod parameters is improved, but the improvement is not significant. In addition, when using this parameter in production, it is found that the liner is prone to cracking and explosion during the melting and shrinking process and is scrapped, and the core rod yield is significantly reduced.
[0032] The embodiment of the present invention adopts the above deposition system. Since the resonant cavity is designed according to a frequency of 2450MHz, when the input microwave frequency is 2450MHz, the matching degree of the entire system is the highest and the reflected power is the lowest. By adjusting the frequency of the microwave output by the solid-state microwave source, the magnitude of the reflected power can be adjusted. The following table shows the reflected power at different microwave frequencies when the microwave power is 7500W and 7000W.
[0033]
[0034]
[0035] The solid-state microwave source control system is linked to the movement of the resonant cavity. The solid-state microwave source can output microwaves of different frequencies at different positions of the resonant cavity. Set the gas end area of the holding furnace to 1010℃, the middle area to 980℃, and the pump end area to 990℃. The actual furnace temperature is shown in Figure 3 Solution 3. When the resonant cavity is in the gas end area of the insulation furnace, the microwave frequency output is 2450MHz, the reflected power is the lowest, and the microwave power is set to 7500W. On the one hand, the plasma temperature generated by the high microwave power is used to compensate for the furnace temperature in the gas end area of the insulation furnace, and on the other hand, the doping efficiency of Ge is improved. When the resonant cavity gradually moves to the middle area of the furnace, the solid-state microwave source reduces or increases the output microwave frequency, and consumes the excess microwave energy through reflected power, thereby ensuring the stability of the core rod parameters. When the resonant cavity moves to the pump end area, the solid-state microwave source outputs 2450MHz microwaves again, thereby compensating for the low furnace temperature in the pump end area and preventing the core rod from bursting during the melting and shrinking process. Figure 4 The relationship between the resonant cavity at different positions in the holding furnace and the microwave frequency output by the solid microwave source is shown in FIG. Figure 5 and Figure 6 Scheme 3. It can be seen from the figure that the uniformity of the core rod has been greatly improved.
[0036] It can be seen from the above embodiments that the present invention replaces the traditional magnetron microwave system with a solid-state microwave source system, thereby realizing the controllability of the microwave frequency along the axial direction of the liner tube, and controlling the reaction absorption power by adjusting the matching degree between the frequency of the solid-state microwave source and the resonant frequency of the resonant cavity, thereby controlling the uniformity of the deposition.
Claims
1. A PCVD process uniform deposition system, comprising coaxially arranged rotary sealing chucks on both sides of a bed, the rotary sealing chucks on both sides are connected to a synchronous rotation driving device, a microwave resonance cavity is arranged between the two rotary sealing chucks, the microwave resonance cavity is arranged in a heat preservation furnace, the microwave resonance cavity extends out of the heating furnace through a waveguide and is connected to a microwave generating device and an axial reciprocating device, the two rotary sealing chucks include an intake rotary sealing chuck and an exhaust rotary sealing chuck, the intake rotary sealing chuck is connected to a raw material gas source through an intake pipe, and the exhaust rotary sealing chuck is connected to a vacuum pump exhaust system through an exhaust pipe, characterized in that The microwave generating device comprises a solid-state microwave source power supply and a solid-state microwave source, and the output end of the solid-state microwave source is connected to the waveguide through a circulator.
2. The PCVD process uniform deposition system according to claim 1, characterized in that The solid-state microwave source is a frequency-adjustable solid-state microwave source; the frequency adjustment range of the frequency-adjustable solid-state microwave source is 2380-2520 MHz.
3. The PCVD uniform deposition system according to claim 1 or 2, characterized in that The solid-state microwave source has adjustable power when the frequency is fixed, and the power adjustment range is 1000W-15000W.
4. The PCVD uniform deposition system according to claim 1 or 2, characterized in that A three-pin automatic distributor is connected in series between the circulator and the waveguide, and the three-pin automatic distributor is used to detect the output power of the solid-state microwave source and the reflected power returned by the resonant cavity.
5. The PCVD process uniform deposition system according to claim 1 or 2, characterized in that The resonant frequency of the microwave resonant cavity is 2450±30 MHz.
6. The PCVD process uniform deposition system according to claim 1 or 2, characterized in that The waveguide comprises a straight waveguide and a curved waveguide, and the waveguide is connected to the resonant cavity.
7. The PCVD process uniform deposition system according to claim 1 or 2, characterized in that The insulation furnace is provided with three temperature zones, namely, a gas end, a middle end and a pump end, and each temperature zone is provided with a temperature sensor.
8. The PCVD process uniform deposition system according to claim 1 or 2, characterized in that The solid-state microwave source power supply is provided with a PLC control unit to automatically adjust the output microwave frequency according to the position of the microwave resonant cavity.
9. A PCVD process uniform deposition method, characterized in that Using any deposition system according to claim 1-8, A pure glass liner is used as a base tube and clamped on the rotating sealing chucks on both sides of the PCVD deposition system. The insulation furnace is heated to 920°C to 1150°C, and the raw gas enters the liner from the gas end. The microwave resonant cavity moves back and forth from the gas end to the pump end along the axial direction of the liner to perform PCVD deposition processing. The solid-state microwave source of the microwave generating device has the same preset output power, and the frequency of the output microwave is adjusted and changed according to the position of the microwave resonant cavity. The period of frequency change is consistent with the period of the microwave resonant cavity moving from the gas end to the pump end. When the microwave resonant cavity is in the gas end area, the starting frequency of the output microwave is consistent with the resonant frequency of the microwave resonant cavity. The microwave resonant cavity moves from the gas end area through the middle area to the pump end area, and the frequency of the output microwave gradually changes. When it reaches the pump end area, the frequency returns to the starting frequency. When the microwave resonant cavity returns from the pump end area through the middle area to the gas end area, the frequency of the output microwave gradually changes. When it reaches the gas end, the frequency returns to the starting frequency, and this cycle is repeated until the deposition is completed.
10. The PCVD uniform deposition method according to claim 9, characterized in that The frequency of the output microwave changes gradually, that is, the frequency of the output microwave increases or decreases gradually relative to the starting frequency, and the starting frequency is the output microwave frequency that is consistent with the resonant frequency of the microwave resonant cavity and at which the reflected power reaches the minimum value.
11. The PCVD uniform deposition method according to claim 9 or 10, characterized in that When the output microwave frequency gradually increases or decreases relative to the initial frequency, the power used for deposition in the microwave resonance cavity decreases, the reflected power increases, and the reflected power is absorbed by the circulator.
12. The PCVD uniform deposition method according to claim 9 or 10, characterized in that The insulation furnace is provided with three temperature zones, namely, the gas end, the middle zone and the pump end. The temperature of the gas end zone is 1000°C to 1100°C, the temperature of the middle zone is 950°C to 1000°C, and the temperature of the pump end zone is 970°C to 1060°C.