SONOS memory device and preparation method thereof

Through self-alignment process and oxide layer isolation technology, the problem of large area occupancy of memory cells is solved, the storage density and uniformity are improved, and a two-tube two-bit SONOS memory device for two-bit data storage is realized.

CN119095382APending Publication Date: 2024-12-06SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411204849.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing two-tube and two-bit SONOS memory devices occupy a large area of ​​storage cells under smaller process nodes, and the common source ends and side walls between storage tubes occupy a large amount of space, affecting storage density and uniformity.

Method used

The self-alignment process is used to form the discrete first oxide layer and the second oxide layer, eliminating the source end and side walls between the storage tubes, and directly using the second oxide layer to isolate the storage tubes, reducing the area of ​​the storage unit, and heavy doping Miscellaneous and lightly doped regions optimize the storage well structure.

Benefits of technology

It effectively improves the storage density and uniformity of storage units, facilitates control of operation interference, and realizes two-bit data storage per storage unit.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119095382A_ABST
    Figure CN119095382A_ABST
Patent Text Reader

Abstract

The invention provides an SONOS memory device and a preparation method thereof, and the preparation method comprises the steps: providing a substrate, and forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the substrate; forming two discrete first oxide layers in the opening of the hard mask layer by using a self-alignment etching process; etching the polysilicon gate material layer exposed out of a gap between the two first oxide layers; a gap between the polysilicon gate material layers and a gap between the two first oxide layers are filled with the second oxide layers; performing etching to form two discrete polycrystalline silicon grids; forming a side wall; and performing source-drain heavily doped ion implantation in the substrate. According to the invention, the storage density can be increased, a source end shared between the two storage tubes and side walls, close to one sides of the source end, of the two storage tubes are omitted, the two storage tubes are directly isolated by the second oxide layer, and the area of the storage unit can be effectively reduced. And the two storage tubes are formed by using a self-alignment process, so that the consistency is high, and the uniformity of the storage unit is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of integrated circuit manufacturing, and in particular relates to a SONOS memory device and a preparation method thereof. Background Art

[0002] As an essential storage device in computers, non-volatile memory plays an important role in storing the information being processed. Among non-volatile memories, Silicon-Oxide-Nitride-Oxide-Silicon (SONOS) memory has the characteristics of small cell size, good storage retention, low operating voltage, and compatibility with complementary metal oxide semiconductor (CMOS) manufacturing process.

[0003] like Figure 1 As shown, there is a two-tube two-bit SONOS memory, in which one storage unit is composed of two storage tubes (storage tube 1 and storage tube 2). In this two-tube two-bit SONOS memory, the two storage tubes share a source terminal S, and the source terminal S does not need to be connected with a contact hole (CT). At a smaller process node, the sidewalls (Spacer) of the two storage tubes close to the source terminal S and the source terminal S that does not need to be connected with a contact hole occupy a larger area. Summary of the invention

[0004] The object of the present invention is to provide a SONOS memory device and a method for preparing the same, which can increase the storage density and store two bits of data in each storage unit. The source end shared by two storage tubes and the manufacturing process of heavily doping the source end are omitted, and the side walls of the two storage tubes close to the source end are omitted. The two storage tubes are directly isolated by the second oxide layer, which can effectively reduce the area of ​​the storage unit. The two storage tubes are formed by a self-alignment process, and the consistency is higher than that of the existing process, which is conducive to improving the uniformity of the storage unit and facilitating the control of the interference of the operation.

[0005] The present invention provides a method for preparing a SONOS memory device, comprising:

[0006] Providing a substrate, and sequentially forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the surface of the substrate;

[0007] Etching the hard mask layer to form an opening to define a total channel length of two storage tubes;

[0008] forming two separate first oxide layers in the opening using a self-aligned etching process;

[0009] Etching the polysilicon gate material layer exposed in the gap between the two first oxide layers until the charge storage layer is exposed;

[0010] forming a second oxide layer, wherein the second oxide layer fills the gap between the polysilicon gate material layers and the gap between the two first oxide layers from bottom to top;

[0011] Etching and removing the hard mask layer; and etching and removing the polysilicon gate material layers exposed by the two first oxide layers, and etching the remaining polysilicon gate material layers to form two separate polysilicon gates;

[0012] Forming sidewalls, the sidewalls covering the sidewalls of the stacked polysilicon gate and the first oxide layer on both sides of the second oxide layer, each of which is away from the second oxide layer;

[0013] Source and drain heavy doping ions are implanted into the substrate at a side of the sidewalls on both sides of the second oxide layer away from the second oxide layer to form a first heavily doped region and a second heavily doped region.

[0014] Further, forming the two first oxide layers by using a self-aligned etching process specifically includes:

[0015] Growing a first oxide material layer, wherein the first oxide material layer covers the surface of the hard mask layer and the surface of the polysilicon gate material layer exposed by the opening, and the first oxide material layer forms a recess in a middle region of the opening;

[0016] The first oxide material layer is self-aligned etched to remove the first oxide material layer above the upper surface of the hard mask layer and the first oxide material layer below the recess to expose the polysilicon gate material layer of a preset width. The first oxide material layer after the self-aligned etching is defined as the first oxide layer.

[0017] Furthermore, after etching the polysilicon gate material layer exposed through the gap between the two first oxide layers and before forming the second oxide layer, the preparation method further includes:

[0018] Lightly doped implantation is performed into the substrate below the gap of the polysilicon gate material layer, that is, lightly doped implantation is performed between the two storage tubes, so as to form a first lightly doped region in the substrate.

[0019] Furthermore, after providing the substrate and before forming the charge storage layer, the preparation method further includes:

[0020] Forming a pad oxide layer on the surface of the substrate, and performing ion implantation on the substrate to form a storage well;

[0021] The pad oxide layer formed on the entire surface of the substrate is removed by an etching process.

[0022] Furthermore, after forming the two separate polysilicon gates and before forming the sidewalls, the preparation method further includes:

[0023] Light doping is implanted into the substrate at a side of the polysilicon gates on both sides of the second oxide layer away from the second oxide layer to form a second lightly doped region.

[0024] The present invention further provides a SONOS storage device, the SONOS storage device comprising a plurality of storage units, the storage units comprising:

[0025] A substrate, on which a first storage tube and a second storage tube are formed; the first storage tube comprises a charge storage layer 1, a polysilicon gate 1 and a first oxide layer 1 from bottom to top on the substrate; the second storage tube comprises a charge storage layer 2, a polysilicon gate 2 and a first oxide layer 2 from bottom to top on the substrate;

[0026] A second oxide layer, wherein the second oxide layer fills a gap between the first polysilicon gate and the second polysilicon gate; the second oxide layer also fills a gap between the first oxide layer and the second first oxide layer;

[0027] Sidewalls, the sidewalls comprising sidewall 1 and sidewall 2; the sidewall 1 covers the sidewalls of the stacked polysilicon gate 1 and the first oxide layer 1 away from the second oxide layer; the sidewall 2 covers the sidewalls of the stacked polysilicon gate 2 and the first oxide layer 2 away from the second oxide layer;

[0028] A first heavily doped region and a second heavily doped region, wherein the first heavily doped region is located in the substrate on a side of the first sidewall away from the second oxide layer, and the second heavily doped region is located in the substrate on a side of the second sidewall away from the second oxide layer.

[0029] Furthermore, the storage unit also includes:

[0030] A first lightly doped region, wherein the first lightly doped region is located in the substrate below the gap between the first polysilicon gate and the second polysilicon gate;

[0031] A second lightly doped region, wherein the second lightly doped region is located in a storage well in the substrate on a side of the polysilicon gate 1 and the polysilicon gate 2 respectively away from the second oxide layer.

[0032] Furthermore, the first heavily doped region serves as the source region of the first storage tube, and the first lightly doped region serves as the drain region of the first storage tube; moreover, the first lightly doped region also serves as the source region of the second storage tube, and the second heavily doped region serves as the drain region of the second storage tube.

[0033] Furthermore, one of the storage units is composed of two storage tubes, namely the first storage tube and the second storage tube, wherein when one storage tube is read, the other storage tube is forced to be turned on or off to act as a selection tube.

[0034] Furthermore, the storage unit further includes: an interlayer dielectric layer, the interlayer dielectric layer covers the substrate, the sidewall, the first oxide layer 1, the first oxide layer 2 and the second oxide layer; a plurality of contact holes are formed in the interlayer dielectric layer, the contact holes are filled with metal to lead out the electrical signals corresponding to each electrode;

[0035] The first contact hole penetrates the interlayer dielectric layer to expose the first heavily doped region; in the first storage tube, the second contact hole penetrates the interlayer dielectric layer and the first oxide layer 1 to expose the polysilicon gate 1; in the second storage tube, the third contact hole penetrates the interlayer dielectric layer and the first oxide layer 2 to expose the polysilicon gate 2; and the fourth contact hole penetrates the interlayer dielectric layer to expose the second heavily doped region.

[0036] Compared with the prior art, the present invention has the following beneficial effects:

[0037] The invention provides a SONOS memory device and a preparation method thereof. The preparation method comprises: providing a substrate, sequentially forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the surface of the substrate; etching the hard mask layer to form an opening to define the total channel length of two storage tubes; forming two separate first oxide layers in the opening by using a self-aligned etching process; etching the polysilicon gate material layer exposed in the gap between the two first oxide layers until the charge storage layer is exposed; forming a second oxide layer, the second oxide layer filling the gap between the polysilicon gate material layers and the gap between the two first oxide layers from bottom to top; etching and removing the hard mask layer; and etching and removing the polysilicon gate material layer exposed by the two first oxide layers, etching the remaining polysilicon gate material layer to form two separate polysilicon gates; forming sidewalls, the sidewalls covering the stacked polysilicon gates on both sides of the second oxide layer and the sidewalls of the first oxide layer on the side away from the second oxide layer; and performing source and drain heavy doping ion implantation into the substrate on the side of the sidewalls on both sides of the second oxide layer on the side away from the second oxide layer to form a first heavily doped region and a second heavily doped region.

[0038] The present invention provides a novel two-tube two-bit SONOS memory device and a preparation method thereof, which can increase the storage density, and each storage unit can store two bits of data. The source end shared by the two storage tubes and the manufacturing process of the heavily doped source end are omitted, and the side walls of the two storage tubes close to the source end are omitted. The two storage tubes are directly isolated by the second oxide layer, which can effectively reduce the area of ​​the storage unit. The two storage tubes are formed by a self-alignment process, and the consistency is higher than the existing process, which is conducive to improving the uniformity of the storage unit and facilitating the control of the interference of the operation. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Figure 1 A schematic diagram of a SONOS storage device.

[0040] Figure 2 The present invention is a schematic flow chart of a method for preparing a SONOS memory device according to an embodiment of the present invention.

[0041] Figure 3 It is a schematic diagram of a method for preparing a SONOS memory device according to an embodiment of the present invention after a liner oxide layer is formed.

[0042] Figure 4 It is a schematic diagram after forming a charge storage layer, a polysilicon gate material layer and a hard mask layer in the method for preparing a SONOS memory device according to an embodiment of the present invention.

[0043] Figure 5 It is a schematic diagram of a method for manufacturing a SONOS memory device according to an embodiment of the present invention after an opening is formed in a hard mask layer.

[0044] Figure 6 It is a schematic diagram of a method for preparing a SONOS memory device according to an embodiment of the present invention after forming a first oxide material layer.

[0045] Figure 7 It is a schematic diagram of a method for manufacturing a SONOS memory device according to an embodiment of the present invention after forming a first oxide layer.

[0046] Figure 8 It is a schematic diagram after forming a first lightly doped region in the method for preparing a SONOS memory device according to an embodiment of the present invention.

[0047] Fig. 9 It is a schematic diagram of the method for preparing a SONOS memory device according to an embodiment of the present invention after forming a second oxide material layer.

[0048] Fig.10 It is a schematic diagram of a method for manufacturing a SONOS memory device according to an embodiment of the present invention after forming a second oxide layer.

[0049] Fig.11It is a schematic diagram of the method for preparing a SONOS memory device according to an embodiment of the present invention after etching away the hard mask layer.

[0050] Fig.12 It is a schematic diagram of a method for manufacturing a SONOS memory device according to an embodiment of the present invention after a polysilicon gate is formed.

[0051] Fig.13 It is a schematic diagram of a method for manufacturing a SONOS memory device according to an embodiment of the present invention after forming a sidewall spacer.

[0052] Fig.14 It is a schematic diagram after forming heavily doped regions and contact holes in the method for preparing a SONOS memory device according to an embodiment of the present invention.

[0053] The reference numerals are as follows:

[0054] 01-substrate; 02-storage well; 03-liner oxide layer; 04-charge storage layer; 05-polysilicon gate material layer; 05'-polysilicon gate; 06-hard mask layer; 07-first oxide material layer; 07'-first oxide layer; 08-second oxide material layer; 08'-second oxide layer; 09-side wall; a-first lightly doped region; LDD-second lightly doped region; P1-first heavily doped region; P2-second heavily doped region; 10-first contact hole; 11-second contact hole; 12-third contact hole; 13-fourth contact hole; 41-charge storage layer one; 42-charge storage layer two; 51-polysilicon gate one; 52-polysilicon gate two; 71-first oxide layer one; 72-first oxide layer two; 91-side wall one; 92-side wall two. DETAILED DESCRIPTION

[0055] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become more apparent from the following description. It should be noted that the accompanying drawings are in a very simplified form and use an inaccurate scale, which is only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0056] In the drawings, the sizes of layers, regions, elements and their relative sizes may be exaggerated for clarity. Like reference numerals denote like elements throughout.

[0057] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present application, the first element, component, region, layer or part discussed below can be represented as the second element, component, region, layer or part. And when the second element, component, region, layer or part is discussed, it does not indicate that the present application necessarily has the first element, component, region, layer or part.

[0058] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.

[0059] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present application. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0060] The embodiment of the present invention provides a method for preparing a SONOS memory device, such as Figure 2 As shown, including:

[0061] Step S1, providing a substrate, and sequentially forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the surface of the substrate;

[0062] Step S2, etching the hard mask layer to form an opening to define the total channel length of the two storage tubes;

[0063] Step S3, forming two separate first oxide layers in the opening by using a self-aligned etching process;

[0064] Step S4, etching the polysilicon gate material layer exposed in the gap between the two first oxide layers until the charge storage layer is exposed;

[0065] Step S5, forming a second oxide layer, the second oxide layer filling the gap between the polysilicon gate material layers and the gap between the two first oxide layers from bottom to top;

[0066] Step S6, etching to remove the hard mask layer; and etching to remove the polysilicon gate material layer exposed by the two first oxide layers, and etching the remaining polysilicon gate material layer to form two separate polysilicon gates;

[0067] Step S7, forming sidewalls, the sidewalls covering the stacked polysilicon gates on both sides of the second oxide layer and the sidewalls of the first oxide layer away from the second oxide layer;

[0068] Step S8, performing source and drain heavy doping ion implantation into the substrate on the side of the sidewalls on both sides of the second oxide layer away from the second oxide layer, to form a first heavily doped region and a second heavily doped region.

[0069] The following will introduce the SONOS memory device and the manufacturing method thereof provided in the embodiments of the present invention in detail in combination with the accompanying drawings. It should be noted that, in order to simplify the difficulty of drawing, the following embodiments and the accompanying drawings of the present invention are introduced by taking a memory cell forming a SONOS memory device as an example, and the actual situation may include a plurality of memory cells provided in the embodiments of the present invention in which the memory area includes two memory cells, but is not limited thereto.

[0070] The method for manufacturing any memory cell in a SONOS memory device will be described in detail below by combining the structural schematic diagram corresponding to each manufacturing step of the method for manufacturing any memory cell in a SONOS memory device provided in an embodiment of the present invention.

[0071] See also Figure 3 , Figure 3 Schematic diagram of the structure after providing a substrate 01 and forming a liner oxide layer 03 and a storage well 02 in the storage area in an embodiment of the present invention. Figure 3As shown, the above step S01 is performed to provide a substrate 01, which provides a platform for various components included in a storage unit of a SONOS storage device to be formed subsequently. The substrate 01 can be any suitable substrate material known in the art, for example, it can be at least one of the following materials: silicon (Si), germanium (Ge), silicon germanium (SiGe), carbon silicon (SiC), carbon germanium silicon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP) or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or it can also be double-sided polished silicon wafers (Double Side Polished Wafers, DSP), or it can also be a ceramic substrate of aluminum oxide, quartz or glass substrate, etc. Exemplarily, in this embodiment, the substrate 01 is, for example, a silicon wafer, and it is a doped silicon wafer, and its doping type can be determined according to the type of storage tube actually formed. In this embodiment, it is exemplarily set to a P-type doped substrate.

[0072] Next, an etching process, such as a dry etching process or a wet etching process, is used to form a plurality of grooves in the substrate 01, and a deposition process, such as a chemical vapor deposition process, a physical vapor deposition process, and an atomic layer deposition process, is used to fill each groove with an insulating material, such as silicon dioxide, to form a plurality of device isolation structures, such as a shallow trench isolation structure (STI), for isolating and defining active areas.

[0073] Afterwards, a deposition process, such as at least one of a chemical vapor deposition process, a physical vapor deposition process, and an atomic layer deposition process, is used to form a pad oxide layer 03 on the entire surface of the substrate 01, and ions are implanted into the substrate 01 region of the storage area to form a storage well 02 in the region. Whether to form an N-well or a P-well can be determined according to the type of storage tubes in the SONOS storage device. In the embodiment of the present invention, a P-well is exemplarily formed in the region to prepare for the subsequent formation of an N-channel storage tube in the region.

[0074] Then, if Figure 3 and Figure 4As shown, the liner oxide layer 03 formed on the entire surface of the substrate 01 can be removed by an etching process, and a charge storage layer 04, a polysilicon gate material layer 05 and a hard mask layer 06 stacked in sequence are formed on the exposed surface of the substrate 01 by a deposition process, wherein the charge storage layer 04 can be a multi-layer film structure, such as an ONO stacking structure, but is not limited thereto; the hard mask layer 06 is, for example, a silicon nitride layer. The thickness of the charge storage layer 04 is, for example, 80 angstroms to 150 angstroms, the thickness of the polysilicon gate material layer 05 is, for example, 800 angstroms to 2000 angstroms, and the thickness of the hard mask layer 06 is, for example, 800 angstroms to 2000 angstroms.

[0075] Then, if Figure 5 As shown, the hard mask layer 06 is etched to form an opening to define the total channel length of the two storage tubes, and the hard mask layer 06 is etched using a photomask to expose the polysilicon gate material layer 05 .

[0076] Then, if Figure 6 As shown, a first oxide material layer 07 is grown, and the first oxide material layer 07 covers the surface of the hard mask layer 06 and the surface of the polysilicon gate material layer 05 exposed by the opening, and the first oxide material layer 07 forms a recess in the middle area of ​​the opening. The thickness of the first oxide material layer 07 defines the channel length of the SONOS tube. The thickness of the first oxide material layer 07 is, for example, 50 angstroms to 100 angstroms.

[0077] Then, if Figure 7 As shown, the first oxide material layer 07 is self-alignedly etched to remove the first oxide material layer 07 above the upper surface of the hard mask layer 06 and the first oxide material layer 07 below the recess to expose the polysilicon gate material layer 05 of a preset width. The first oxide material layer 07 after self-aligned etching is defined as a first oxide layer 07'.

[0078] Then, if Figure 8 As shown, the first oxide layer 07' is used as a mask to etch the polysilicon gate material layer 05 of a preset width to expose the charge storage layer 04. A light doping injection is performed into the substrate 01 of a preset width, that is, a light doping injection is performed between the two storage tubes to form a first light doping region a in the substrate 01.

[0079] Then, if Fig. 9 As shown, a second oxide material layer 08 is grown, and the second oxide material layer 08 fills the gap between the two storage tubes above the first lightly doped region a. The thickness of the second oxide material layer 08 is, for example, 100 angstroms to 300 angstroms. Specifically, the second oxide material layer 08 fills the gap between the polysilicon gate material layer 05 above the first lightly doped region a and the gap between the first oxide layers 07' and covers the upper surface of the hard mask layer 06 and the upper surface of the first oxide layer 07'. Fig.10As shown, the second oxide material layer 08 is chemically mechanically polished to make the hard mask layer 06, the first oxide layer 07' and the upper surface of the second oxide material layer 08 flush, and the polished second oxide material layer 08 is defined as a second oxide layer 08'.

[0080] Then, if Fig.11 As shown, the hard mask layer 06 is removed by etching to expose the polysilicon gate material layer 05 .

[0081] Then, if Fig.12 As shown, the polysilicon gate material layer 05 exposed by the first oxide layer 07' on both sides of the second oxide layer 08' is removed by etching, and the remaining polysilicon gate material layer 05 is etched to form a polysilicon gate 05'.

[0082] Then, if Fig.13 As shown, light doping is injected into the substrate 01 on the side of the polysilicon gate 05' on both sides of the second oxide layer 08' away from the second oxide layer 08' to form a second lightly doped region LDD. A sidewall 09 is formed, and the sidewall 09 covers the side surfaces of the stacked polysilicon gate 05' and the first oxide layer 07' on both sides of the second oxide layer 08' away from the second oxide layer 08'. The sidewall 09 also covers the surface of the charge storage layer 04 of a portion of the width of the two polysilicon gates 05' away from the second oxide layer 08'. The sidewalls 09 on both sides of the second oxide layer 08' away from the charge storage layer 04 on the side of the second oxide layer 08' are etched and removed to expose the surface of the substrate 01. Source and drain heavy doping ions are injected into the substrate 01 on the side of the sidewalls 09 on both sides of the second oxide layer 08' away from the second oxide layer 08' to form a first heavily doped region P1 and a second heavily doped region P2.

[0083] Then, if Fig.13 and Fig.14As shown, an interlayer dielectric layer (not shown) is formed, and the interlayer dielectric layer covers the substrate 01, the sidewall 09, the first oxide layer 07' and the second oxide layer 08'. A contact hole is formed in the interlayer dielectric layer, and a metal (plug) is filled in the contact hole to lead out the electrical signals of each pole. Exemplarily, the SONOS memory is composed of a plurality of memory cells, and the memory cell includes a first memory tube and a second memory tube. The first heavily doped region P1 serves as the source region of the first memory tube, and the first lightly doped region a serves as the drain region of the first memory tube; moreover, the first lightly doped region a also serves as the source region of the second memory tube, and the second heavily doped region P2 serves as the drain region of the second memory tube. The first contact hole 10 penetrates the interlayer dielectric layer to expose the first heavily doped region P1 and leads out the first heavily doped region P1 through the metal in the contact hole. In the first memory tube, the second contact hole 11 penetrates the interlayer dielectric layer and the first oxide layer 07' to expose the polysilicon gate 05' and leads out the polysilicon gate 05' through the metal in the contact hole. In the second storage tube, the third contact hole 12 penetrates the interlayer dielectric layer and the first oxide layer 07' to expose the polysilicon gate 05' and leads the polysilicon gate 05' out through the metal in the contact hole. The fourth contact hole 13 penetrates the interlayer dielectric layer to expose the second heavily doped region P2 and leads the second heavily doped region P2 out through the metal in the contact hole.

[0084] The present invention provides a novel method for preparing a two-tube two-bit SONOS memory device, wherein each memory cell can store two bits of data, thereby increasing the storage density. The source end shared by the two memory cells and the manufacturing process of heavily doping the source end are omitted, and the sidewalls (Spacer) on the side of the two memory cells close to the source end S are omitted. The second oxide layer 08' is directly used to isolate the two memory cells, thereby effectively reducing the area of ​​the memory cell. The two memory cells are formed using a self-alignment process, and the consistency is higher than that of the existing process, which is conducive to improving the uniformity of the memory cell and facilitating the control of the interference of the operation.

[0085] The present invention also provides a SONOS storage device, such as Fig.13 and Fig.14 As shown, the SONOS memory device includes a plurality of memory cells, and the memory cells include:

[0086] A substrate 01, on which a first storage tube and a second storage tube are formed; the first storage tube includes a charge storage layer 41, a polysilicon gate 51 and a first oxide layer 71 from bottom to top on the substrate; the second storage tube includes a charge storage layer 42, a polysilicon gate 52 and a first oxide layer 72 from bottom to top on the substrate; the charge storage layer 41 and the charge storage layer 42 are connected to form a charge storage layer 04; the polysilicon gate 05' includes a polysilicon gate 51 and a polysilicon gate 52; the first oxide layer 07' includes a first oxide layer 71 and a first oxide layer 72; the second oxide layer 08', the second oxide layer 08' fills the gap between the polysilicon gate 51 and the polysilicon gate 52; the second oxide layer 08' also fills the gap between the first oxide layer 71 and the first oxide layer 72;

[0087] The sidewall 09 includes a sidewall 1 91 and a sidewall 2 92. The sidewall 1 91 covers the side surface of the stacked polysilicon gate 1 51 and the first oxide layer 1 71 away from the second oxide layer 08'. The sidewall 1 91 also covers a portion of the width of the charge storage layer 04 surface on the side of the polysilicon gate 1 51 away from the second oxide layer 08'.

[0088] The second sidewall 92 covers the side surface of the stacked polysilicon gate 2 52 and the first oxide layer 2 72 away from the second oxide layer 08 ′, and the second sidewall 92 also covers a portion of the width of the charge storage layer 04 surface on the side of the polysilicon gate 2 52 away from the second oxide layer 08 ′;

[0089] The first heavily doped region P1 and the second heavily doped region P2 are located in the substrate 01 on the side of the first sidewall 91 away from the second oxide layer 08 ′, and the second heavily doped region P2 is located in the substrate 01 on the side of the second sidewall 92 away from the second oxide layer 08 ′.

[0090] Specifically, the first heavily doped region P1 serves as the source region of the first storage tube, and the first lightly doped region a serves as the drain region of the first storage tube; moreover, the first lightly doped region a also serves as the source region of the second storage tube, and the second heavily doped region P2 serves as the drain region of the second storage tube. In the present invention, a storage unit is composed of two storage tubes (a first storage tube and a second storage tube), and when one storage tube is read, the other storage tube is forced to be turned on or off to act as a selection tube. The present invention provides a novel two-tube two-bit SONOS storage unit structure, and each storage unit stores two bits of data, which can increase the storage density. The source end shared between the two storage tubes and the manufacturing process of heavily doping the source end are omitted, and the sidewalls (Spacer) on the side of the two storage tubes close to the source end S are omitted. The second oxide layer 08' is directly used to isolate the two storage tubes, which can effectively reduce the area of ​​the storage unit. The two storage tubes are formed using a self-alignment process, and the consistency is higher than that of the existing process, which is conducive to improving the uniformity of the storage unit and facilitating the control of operation interference.

[0091] The memory cell may further include: a first lightly doped region a and a second lightly doped region LDD, wherein the first lightly doped region a is located in the substrate 01 below the gap between the first polysilicon gate 51 and the second polysilicon gate 52. The second lightly doped region LDD is located in the memory well 02 on the side of the first polysilicon gate 51 and the second polysilicon gate 52 away from the second oxide layer 08'.

[0092] The storage unit further includes: an interlayer dielectric layer (not shown), the interlayer dielectric layer covers the substrate 01, the sidewall 09, the first oxide layer 07' and the second oxide layer 08'. A contact hole is formed in the interlayer dielectric layer, and the contact hole is filled with metal (plug) to lead out the electrical signals of each pole. The first contact hole 10 penetrates the interlayer dielectric layer to expose the first heavily doped region P1 and leads out the first heavily doped region P1 through the metal in the contact hole. In the first storage tube, the second contact hole 11 penetrates the interlayer dielectric layer and the first oxide layer 71 to expose the polysilicon gate 51 and leads out the polysilicon gate 51 through the metal in the contact hole. In the second storage tube, the third contact hole 12 penetrates the interlayer dielectric layer and the first oxide layer 72 to expose the polysilicon gate 2 52 and leads out the polysilicon gate 2 52 through the metal in the contact hole. The fourth contact hole 13 penetrates the interlayer dielectric layer to expose the second heavily doped region P2 and leads out the second heavily doped region P2 through the metal in the contact hole.

[0093] In summary, the present invention provides a SONOS memory device and a preparation method thereof, the preparation method comprising: providing a substrate, sequentially forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the surface of the substrate; etching the hard mask layer to form an opening to define the total channel length of two storage tubes; forming two separate first oxide layers in the opening by a self-aligned etching process; etching the polysilicon gate material layer exposed in the gap between the two first oxide layers until the charge storage layer is exposed; forming a second oxide layer, the second oxide layer filling the gap between the polysilicon gate material layers and the gap between the two first oxide layers from bottom to top; etching and removing the hard mask layer; and etching and removing the polysilicon gate material layer exposed by the two first oxide layers, etching the remaining polysilicon gate material layer to form two separate polysilicon gates; forming sidewalls, the sidewalls covering the stacked polysilicon gates on both sides of the second oxide layer and the sidewalls of the first oxide layer on the side away from the second oxide layer; performing source and drain heavy doping ion implantation into the substrate on the side of the sidewalls on both sides of the second oxide layer away from the second oxide layer to form a first heavily doped region and a second heavily doped region.

[0094] The present invention provides a novel two-tube two-bit SONOS memory device and a preparation method thereof, which can increase the storage density, and each storage unit can store two bits of data. The source end shared by the two storage tubes and the manufacturing process of the heavily doped source end are omitted, and the side walls of the two storage tubes close to the source end are omitted. The two storage tubes are directly isolated by the second oxide layer, which can effectively reduce the area of ​​the storage unit. The two storage tubes are formed by a self-alignment process, and the consistency is higher than the existing process, which is conducive to improving the uniformity of the storage unit and facilitating the control of the interference of the operation.

[0095] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the method disclosed in the embodiment, since it corresponds to the device disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part description.

[0096] The above description is only a description of the preferred embodiment of the present invention, and is not any limitation on the scope of rights of the present invention. Any technical personnel in this field can make possible changes and modifications to the technical solution of the present invention by using the methods and technical contents disclosed above without departing from the spirit and scope of the present invention. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.

Claims

1. A method for preparing a SONOS memory device, characterized in that: include: Providing a substrate, and sequentially forming a charge storage layer, a polysilicon gate material layer and a hard mask layer on the surface of the substrate; Etching the hard mask layer to form an opening to define a total channel length of two storage tubes; forming two separate first oxide layers in the opening using a self-aligned etching process; Etching the polysilicon gate material layer exposed in the gap between the two first oxide layers until the charge storage layer is exposed; forming a second oxide layer, wherein the second oxide layer fills the gap between the polysilicon gate material layers and the gap between the two first oxide layers from bottom to top; Etching and removing the hard mask layer; and etching away the polysilicon gate material layers exposed by the two first oxide layers, and etching the remaining polysilicon gate material layers to form two separate polysilicon gates; Forming sidewalls, the sidewalls covering the sidewalls of the stacked polysilicon gate and the first oxide layer on both sides of the second oxide layer, each of which is away from the second oxide layer; Source and drain heavy doping ions are implanted into the substrate at a side of the sidewalls on both sides of the second oxide layer away from the second oxide layer to form a first heavily doped region and a second heavily doped region.

2. The method for preparing a SONOS memory device according to claim 1, wherein: Forming the two first oxide layers by a self-aligned etching process specifically includes: Growing a first oxide material layer, wherein the first oxide material layer covers the surface of the hard mask layer and the surface of the polysilicon gate material layer exposed by the opening, and the first oxide material layer forms a recess in a middle region of the opening; The first oxide material layer is self-aligned etched to remove the first oxide material layer above the upper surface of the hard mask layer and the first oxide material layer below the recess to expose the polysilicon gate material layer of a preset width. The first oxide material layer after the self-aligned etching is defined as the first oxide layer.

3. The method for preparing a SONOS memory device according to claim 1, wherein: After etching the polysilicon gate material layer exposed through the gap between the two first oxide layers and before forming the second oxide layer, the preparation method further includes: Lightly doped implantation is performed into the substrate below the gap of the polysilicon gate material layer, that is, lightly doped implantation is performed between the two storage tubes, so as to form a first lightly doped region in the substrate.

4. The method for preparing a SONOS memory device according to claim 1, wherein: After providing the substrate and before forming the charge storage layer, the preparation method further includes: Forming a pad oxide layer on the surface of the substrate, and performing ion implantation on the substrate to form a storage well; The pad oxide layer formed on the entire surface of the substrate is removed by an etching process.

5. The method for preparing a SONOS memory device according to claim 1, wherein: After forming the two separate polysilicon gates and before forming the sidewalls, the preparation method further includes: Light doping is implanted into the substrate at a side of the polysilicon gates on both sides of the second oxide layer away from the second oxide layer to form a second lightly doped region.

6. A SONOS memory device, comprising a plurality of memory cells, characterized in that: The storage unit comprises: A substrate, on which a first storage tube and a second storage tube are formed; the first storage tube comprises a charge storage layer 1, a polysilicon gate 1 and a first oxide layer 1 from bottom to top on the substrate; the second storage tube comprises a charge storage layer 2, a polysilicon gate 2 and a first oxide layer 2 from bottom to top on the substrate; A second oxide layer, wherein the second oxide layer fills a gap between the first polysilicon gate and the second polysilicon gate; the second oxide layer also fills a gap between the first oxide layer and the second first oxide layer; Sidewalls, the sidewalls comprising sidewall 1 and sidewall 2; the sidewall 1 covers the sidewalls of the stacked polysilicon gate 1 and the first oxide layer 1 away from the second oxide layer; the sidewall 2 covers the sidewalls of the stacked polysilicon gate 2 and the first oxide layer 2 away from the second oxide layer; A first heavily doped region and a second heavily doped region, wherein the first heavily doped region is located in the substrate on a side of the first sidewall away from the second oxide layer, and the second heavily doped region is located in the substrate on a side of the second sidewall away from the second oxide layer.

7. The SONOS memory device according to claim 6, wherein: The storage unit also includes: A first lightly doped region, wherein the first lightly doped region is located in the substrate below the gap between the first polysilicon gate and the second polysilicon gate; A second lightly doped region, wherein the second lightly doped region is located in a storage well in the substrate on a side of the polysilicon gate 1 and the polysilicon gate 2 respectively away from the second oxide layer.

8. The SONOS memory device according to claim 7, wherein: The first heavily doped region serves as the source region of the first storage tube, and the first lightly doped region serves as the drain region of the first storage tube; moreover, the first lightly doped region also serves as the source region of the second storage tube, and the second heavily doped region serves as the drain region of the second storage tube.

9. The SONOS memory device according to claim 6, wherein: One of the storage units is composed of two storage tubes, namely the first storage tube and the second storage tube; wherein when one storage tube is read, the other storage tube is forced to be turned on or off to act as a selection tube.

10. The SONOS memory device according to claim 6, wherein: The storage unit further includes: an interlayer dielectric layer, the interlayer dielectric layer covers the substrate, the sidewall, the first oxide layer 1, the first oxide layer 2 and the second oxide layer; a plurality of contact holes are formed in the interlayer dielectric layer, the contact holes are filled with metal to lead out the electrical signals corresponding to each electrode; The first contact hole penetrates the interlayer dielectric layer to expose the first heavily doped region; in the first storage tube, the second contact hole penetrates the interlayer dielectric layer and the first oxide layer 1 to expose the polysilicon gate 1; in the second storage tube, the third contact hole penetrates the interlayer dielectric layer and the first oxide layer 2 to expose the polysilicon gate 2; and the fourth contact hole penetrates the interlayer dielectric layer to expose the second heavily doped region.