Automobile A column decorative plate assembly

By using decorative panels made of PC+ABS plastic alloy, combined with welding tooling, solder joints, puncture welding bosses and copper sheets, as well as elastic plastic buffer layers, the problem of "sink marks" during the welding process is solved and the vehicle A The stability and beauty of column decorative panels.

CN221794547UActive Publication Date: 2024-10-01SHANGHAI REAL INDAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420306088.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-19
Publication Date
2024-10-01
Estimated Expiration
2034-02-19

AI Technical Summary

Technical Problem

During the welding process of automobile A-pillar decorative panels, puncture welding "sink marks" are prone to occur, resulting in surface material dents and reduced aesthetics.

Method used

A decorative plate made of PC+ABS plastic alloy is used, and a welding tooling, a number of solder points and a puncture welding boss are set on it, combined with a copper sheet and an elastic plastic buffer layer, to accurately control the heat input and positioning during the welding process, reducing Thermal deformation and impact effects.

Benefits of technology

It effectively reduces the occurrence of "sink marks" during the welding process, ensures the flatness and aesthetics of the decorative panels, and improves the welding stability and appearance quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221794547U_ABST
    Figure CN221794547U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of decorating parts of automobile parts, in particular to an automobile A column decorating plate assembly which comprises a decorating plate and a decorating base plate, the decorating plate is formed by compounding PC and ABS (plastic alloy), and a welding tool is arranged on the decorating plate. And a welding tool is additionally arranged on the decorative plate, so that the position accuracy and stability of the decorative plate in the welding process are ensured, and thermal deformation and sink marks of materials are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of decorative parts of automobile parts, and in particular to an automobile A-pillar decorative panel assembly. Background Art

[0002] The A-pillar of a car is a pillar located between the front door and the front windshield. It is an important part of the car structure. The traditional A-pillar of a car is made of metal, but with the development of the automobile industry and the demand of consumers for automobile appearance and light weight, more and more cars are beginning to use A-pillars made of plastic or composite materials. This material can provide better impact resistance and light weight, and can also better meet consumers' demand for automobile appearance aesthetics.

[0003] In order to make the A-pillar look more beautiful, some automobile manufacturers will also install decorative panels on the A-pillar. These decorative panels are usually made of plastic or composite materials and can be combined with the A-pillar through injection molding, spraying, film pasting, etc. to provide better visual effects.

[0004] The A-pillar decorative panel assembly used in the related art is composed of a decorative panel, a decorative substrate, a sealing strip, foam and buckles, and the assembly is manufactured by injection molding, painting, welding, assembly and other process methods, among which the decorative panel and the decorative substrate are welded by ultrasonic puncture.

[0005] However, due to the raw materials of the decorative panels and the design of key dimensions, the problem of "sink marks" in puncture welding is prone to occur during the welding process. The "sink marks" are caused by the softening and melting of the plastic layer of the product under the action of welding heat. When the welding is completed and the product gradually cools down, the plastic shrinks, causing the surface material to shrink and collapse toward the middle layer under the action of internal stress, thus forming a surface depression, which is felt from the perspective as a "sink mark".

[0006] Therefore, in order to solve this problem, an automobile A-pillar decorative panel assembly is provided. Utility Model Content

[0007] In order to solve the problem of puncture welding "sink marks" that are easily generated during the welding process, the present application provides an automobile A-pillar decorative panel assembly.

[0008] The present application provides an automobile A-pillar decorative panel assembly adopting the following technical solution:

[0009] An automobile A-pillar decorative panel assembly comprises a decorative panel and a decorative base plate, wherein the decorative panel is composited with PC+ABS (plastic alloy) and a welding tool is arranged on the decorative panel.

[0010] By adopting the above technical solution: the decorative panel made of plastic alloy combines the advantages of PC and ABS, so that it maintains better stability during the welding process. At the same time, the setting of the welding tooling can provide better positioning and fixation, ensuring the position accuracy of the decorative panel during the welding process and reducing thermal deformation and "shrinkage marks".

[0011] Preferably, a plurality of welding points are provided on the decorative plate.

[0012] By adopting the above technical solution: the setting of several welding points on the decorative panel makes it possible to more accurately control the heat input during the welding process. The welding points can provide local high-temperature areas, making the material easier to melt and flow, and can also reduce the overall heated area, thereby reducing the impact of thermal deformation. The shrinkage and deformation of the material around the welding points are limited, which helps to maintain the flatness of the decorative panel and thereby reduce the generation of "sink marks".

[0013] Preferably, puncture welding bosses are provided on some of the welding points.

[0014] By adopting the above technical solution: the puncture welding boss can increase the wall thickness of the product, the heat transfer gradient to the surface of the decorative panel is small during ultrasonic puncture welding, and heat and softening are not allowed near the surface, thereby avoiding the "shrinkage mark" formed by the collapse of the product after softening to a certain extent.

[0015] Preferably, the puncture welding boss has a length of 26.5 mm, a width of 16.2 mm, and a thickness of 3.8 mm.

[0016] By adopting the above technical solution: precise size design enables each puncture welding boss to provide consistent welding effect, which helps to ensure the consistent performance and quality of each A-pillar decorative panel assembly, reduce the occurrence of "sink marks", and also make the puncture welding boss more coordinated with the decorative panel, improve the overall aesthetics, and make the surface of the decorative panel flatter and smoother.

[0017] Preferably, the welding tool is provided with a copper sheet corresponding to the puncture welding boss.

[0018] By adopting the above technical solution: the copper sheet and the piercing welding boss can correspond one to one, covering the range of the piercing welding, so that part of the heat conducted during the piercing welding head welding is absorbed and taken away by the copper sheet, so that the surface of the product is first cooled and solidified to form a hard surface layer that can withstand greater tensile stress, and "sink marks" are not easy to form.

[0019] Preferably, the copper sheet has a length of 23 mm, a width of 18 mm, and a thickness of 0.5 mm.

[0020] By adopting the above technical solution: the heat conduction and positioning during the welding process can be accurately controlled, which helps to improve the appearance quality and overall performance of the A-pillar decorative panel assembly. The appropriate size design (such as length, width and thickness) enables the copper sheet to adapt to different decorative panel shapes and sizes, improving its applicability under different production conditions.

[0021] Preferably, a buffer layer is provided between the decorative plate and the decorative substrate.

[0022] By adopting the above technical solution: a layer of buffer material is added between the traditional decorative panel and the decorative substrate. This layer of buffer material can play a buffering role and absorb part of the thermal deformation caused by welding. When the welding is completed, the plastic may shrink and deform due to the effect of heat. However, due to the existence of the buffer layer, it can absorb this part of the deformation, effectively disperse the shrinkage stress, and reduce the phenomenon of local stress concentration. In this way, even if some thermal deformation occurs during the welding process, the buffer layer can also play a role of regulation and compensation, so that the surface material remains relatively flat and the appearance of "shrinkage marks" is reduced.

[0023] Preferably, the buffer layer is composed of elastic plastic.

[0024] By adopting the above technical solution: elastic plastic can be customized according to actual needs to adapt to different decorative panel shapes, sizes and material requirements, which helps to improve the flexibility and adaptability of the product. At the same time, it has good elasticity and cushioning properties, and can effectively absorb and disperse the impact and vibration generated during the welding process, effectively reducing the "shrinkage marks" caused by impact and vibration.

[0025] In summary, the present application includes at least one of the following beneficial technical effects:

[0026] 1. This application changes the material of the decorative panel to a plastic alloy composed of PC and ABS, and sets a welding tool on the decorative panel to ensure the position accuracy and stability of the decorative panel during the welding process, thereby reducing thermal deformation and "sink marks";

[0027] 2. The present application sets welding points on the decorative panel, so that the heat input and distribution during the welding process can be precisely controlled. The design of the welding points can provide a local high-temperature area, promote the melting and flow of the material, and help reduce the generation of "sink marks". At the same time, the copper sheet can be used as part of the welding tooling to provide stable positioning and protection for the decorative panel, further reducing the "sink marks" caused by thermal deformation and stress;

[0028] 3. This application can further reduce the impact of the impact and vibration generated during the welding process on the decorative panel by setting a buffer layer between the decorative panel and the decorative substrate. The elastic plastic used as the buffer layer material can absorb and disperse these forces and reduce the "shrinkage marks" caused by the impact. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a schematic diagram of the overall structure of the A-pillar decorative panel assembly of an automobile according to an embodiment of the present application;

[0030] Figure 2 It is a schematic diagram of the exploded structure of the A-pillar decorative panel assembly of an automobile according to an embodiment of the present application;

[0031] Figure 3 It is a schematic diagram of the overall structure of the decorative panel of the A-pillar decorative panel assembly of an automobile according to an embodiment of the present application;

[0032] Figure 4 yes Figure 3 A schematic diagram of the enlarged structure at point A;

[0033] Figure 5 It is a schematic diagram of the overall structure of the welding tooling of the automobile A-pillar decorative panel assembly according to the embodiment of the present application;

[0034] Figure 6 yes Figure 5 Schematic diagram of the enlarged structure at point B.

[0035] Figure numerals: 1. decorative plate; 11. welding point; 111. piercing welding boss; 2. decorative plate substrate; 3. welding tool; 31. copper sheet; 4. buffer layer. DETAILED DESCRIPTION

[0036] The following is combined with Figure 1-5 This application is described in further detail. Example

[0037] The present application embodiment discloses an automobile A-pillar decorative panel 1 assembly, referring to Figure 1 , Figure 2 and Figure 3 , including a decorative panel substrate 2, a decorative panel 1 and a welding tool 3 arranged in sequence from top to bottom, so that good stability can be maintained during the welding process. At the same time, the setting of the welding tool 3 can provide better positioning and fixation. The decorative panel 1 is made of a plastic alloy composite, and welding points 11 are evenly distributed on the inner side of the decorative panel 1, which ensures the position accuracy of the decorative panel 1 during welding, accurately controls the heat input during welding, and is conducive to reducing thermal deformation.

[0038] To reduce sink marks, refer to Figure 3 and Figure 4A piercing welding boss 111 with a length of 26.5 mm, a width of 16.2 mm, and a thickness of 3.8 mm is installed at the center of the welding point 11. The piercing welding boss 111 can increase the wall thickness of the product, and the heat transfer gradient to the surface of the decorative plate 1 is small during ultrasonic piercing welding, and the area close to the surface is not allowed to heat up and soften. In addition, the precise size design enables each piercing welding boss 111 to provide a consistent welding effect, which helps to maintain consistency in performance and quality, thereby avoiding the "sink mark" formed by the collapse of the product after softening to a certain extent;

[0039] In addition, refer to Figure 5 and Figure 6 A copper sheet 31 with a length of 23 mm, a width of 18 mm and a thickness of 0.5 mm is installed on the outer surface of the welding tool 3, which corresponds to the piercing welding boss 111. It can ensure that the copper sheet 31 and the piercing welding boss 111 correspond one to one and cover the range of the piercing welding. In this way, part of the heat conducted during welding by the piercing welding head is absorbed and taken away by the copper sheet 31, so that the surface of the product is first cooled and solidified to form a hard surface layer that can withstand greater tensile stress, and "sink marks" are not easy to form. In addition, through precise size design, the heat conduction and positioning during the welding process can be controlled, which helps to improve the appearance quality and overall performance.

[0040] To further reduce the formation of sink marks, refer to Figure 1 and Figure 2 A buffer layer 4 is further provided between the decorative plate 1 and the decorative substrate 2. In this embodiment, the buffer layer 4 is made of elastic plastic. The elastic plastic can be customized according to actual needs to adapt to different shapes, sizes and material requirements of the decorative plate 1, which helps to improve the flexibility and adaptability of the product.

[0041] After welding is completed, shrinkage and deformation may occur due to the effect of heat. However, due to the existence of the buffer layer 4, it can absorb this part of the deformation, effectively disperse the shrinkage stress, and reduce the phenomenon of local stress concentration. In this way, even if some thermal deformation occurs during the welding process, the buffer layer 4 can also play a role of regulation and compensation, so that the surface material remains relatively flat and the appearance of "sink marks" is reduced.

[0042] The working process and implementation principle of Example 1 are as follows: the decorative plate 1 and the decorative plate substrate 2 are sequentially installed on the welding tool 3 from top to bottom, and then the space between the decorative plate 1 and the decorative plate substrate 2 is filled with elastic plastic, and then ultrasonic puncture welding can be performed. The elastic plastic as a buffer layer 4 can play a supporting and regulating role, which is conducive to reducing thermal deformation;

[0043] At the same time, thanks to the piercing welding boss 111 added to the decorative panel 1 and the copper sheet 31 installed correspondingly thereto on the welding tool 3, the piercing welding boss 111 and the copper sheet 31 are respectively precisely dimensioned, and the welding head is aligned with the piercing welding boss 111 on the welding point 11. Heat is conducted to the copper sheet 31 through the piercing welding boss 111, so that the heat conduction can be precisely controlled, which is beneficial to reducing the risk of local stress concentration and the occurrence of "sink marks" due to uneven heat distribution.

[0044] The above are preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.

Claims

1. An automobile A-pillar decorative panel assembly, comprising a decorative panel (1) and a decorative substrate (2), wherein the decorative panel (1) is made of PC+ABS, i.e., a composite of plastic alloys, and characterized in that: A welding tool (3) is provided on the decorative plate (1).

2. The automobile A-pillar decorative panel assembly according to claim 1, characterized in that: A plurality of welding points (11) are arranged on the decorative plate (1).

3. The automobile A-pillar decorative panel assembly according to claim 2, characterized in that: A plurality of the welding points (11) are provided with puncture welding bosses (111).

4. The automobile A-pillar decorative panel assembly according to claim 3, characterized in that: The piercing welding boss (111) has a length of 26.5 mm, a width of 16.2 mm, and a thickness of 3.8 mm.

5. The automobile A-pillar decorative panel assembly according to claim 1, characterized in that: The welding tool (3) is provided with a copper sheet (31) corresponding to the piercing welding boss (111).

6. The automobile A-pillar decorative panel assembly according to claim 5, characterized in that: The copper sheet (31) has a length of 23 mm, a width of 18 mm and a thickness of 0.5 mm.

7. The automobile A-pillar decorative panel assembly according to claim 1, characterized in that: A buffer layer (4) is provided between the decorative plate (1) and the decorative substrate (2).

8. The automobile A-pillar decorative panel assembly according to claim 7, characterized in that: The buffer layer (4) is composed of elastic plastic.