Composite neutron target film and neutron tube

By using a composite structure of a deuterium storage coating and an Al protective layer in the neutron target film, the problem of easy oxidation and pollution of the neutron target film is solved, the yield and life of the neutron tube are improved, and the anti-oxidation and anti-oxidation properties are achieved. The pollution effect has broken the foreign technology monopoly.

CN221807266UActive Publication Date: 2024-10-01ZHONGKE SHIJIN (GUANGDONG) NEUTRON TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323379384.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-12
Publication Date
2024-10-01
Estimated Expiration
2033-12-12

AI Technical Summary

Technical Problem

The existing neutron target film is easily oxidized and polluted by air, resulting in a decrease in the yield and life of the neutron tube, and there is a lack of sputter-resistant materials that resist oxidation and pollution.

Method used

A composite neutron target film structure is used, including a deuterium storage coating and a protective layer. The protective layer is evenly coated on one side of the deuterium storage coating to reduce damage and contamination of the neutron target by ion beam impurity ions. Choose Al film It serves as a protective layer to block the sputtering of impurity ions, and ensures the amount of deuterium absorption by reasonably setting the thickness of the titanium film and the incident depth of deuterium ions.

Benefits of technology

It effectively protects the high-purity titanium membrane from contamination and oxidation, increases the yield and life of the neutron target membrane, breaks the foreign technology monopoly, and ensures the performance stability and output of the neutron tube.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221807266U_ABST
    Figure CN221807266U_ABST
Patent Text Reader

Abstract

The utility model relates to a composite neutron target film and a neutron tube, the neutron target film comprises a deuterium storage coating and a protective layer, and the protective layer is uniformly coated on one side surface of the deuterium storage coating and is used for reducing damage of foreign ions released by ion beams to a neutron target and resisting pollution and oxidation. The composite neutron target film structure has the beneficial effects that the structure is simple, the design is reasonable, the damage of impurity ions released by ion beams to the high-purity titanium film is reduced, the total deuterium absorption amount of the titanium film is ensured, the effect of protecting the high-purity titanium film from being polluted and oxidized is achieved, the yield of the neutron target film is greatly improved, the service life of the neutron target film is greatly prolonged, and the service life of the neutron target film is prolonged. And the technical monopoly of foreign neutron target films is broken.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of neutron tubes, in particular to a composite neutron target film and a neutron tube. Background Art

[0002] Neutron tube is a sealed micro neutron generator that integrates the ion source system, acceleration system, target system, and gas pressure regulation system in a ceramic tube to form a high-voltage, high-vacuum compact electric vacuum device. Its working principle is: deuterium ions are accelerated to bombard the neutron target to produce neutrons through nuclear fusion reaction. Neutron tubes are widely used in neutron logging, explosive and drug detection, irradiation breeding, neutron photography, online neutron activation analysis and other fields.

[0003] The performance of neutron target determines the neutron yield, stability and life. Neutron target is composed of target substrate and target film. The target substrate material is usually made of metal materials such as Mo and Cu with high melting point and good thermal diffusion effect. The target film material is usually made of Ti, Zr and Sc. However, Ti is the single metal with the highest hydrogen absorption density discovered so far and is also the most common target film material. Its main function is to store deuterium / tritium gas. It is also an important carrier for nuclear fusion reaction. Its preparation material and process directly determine the performance of neutron tube.

[0004] During the storage or transportation of neutron targets, high-purity Ti films are easily oxidized by air to form titanium oxide layers, and are also easily oxidized by C + 、N + On the one hand, there are many impurity ions in the ion beam of the neutron tube, which displace deuterium / tritium gas and damage the target after bombarding the target, which eventually leads to a decrease in the yield and life of the neutron tube. Therefore, it is urgent to develop anti-oxidation, anti-pollution and sputtering resistant neutron target films to improve the level of domestic neutron tubes. Utility Model Content

[0005] The utility model provides a composite neutron target film and a neutron tube, aiming to solve the problems in the prior art.

[0006] The technical solution of the utility model to solve the above technical problems is as follows:

[0007] A composite neutron target film comprises a deuterium storage coating and a protective layer. The protective layer is uniformly coated on one side surface of the deuterium storage coating and is used to reduce the damage of impurity ions released by an ion beam to the neutron target and resist contamination and oxidation.

[0008] The beneficial effects of the utility model are as follows: the utility model has a simple structure and a reasonable design. The composite neutron target membrane structure reduces the damage of the impurity ions released by the ion beam to the high-purity titanium membrane, while ensuring the total amount of deuterium absorbed by the titanium membrane, thereby protecting the high-purity titanium membrane from pollution and oxidation, greatly improving the yield and life of the neutron target membrane, and thus breaking the foreign technical monopoly on neutron target membranes.

[0009] On the basis of the above technical solution, the present invention can also be improved as follows.

[0010] Furthermore, the protective layer is an Al film.

[0011] The beneficial effect of adopting the above further scheme is that the surface structure of the pure Al film is dense, without obvious defects and holes, and can effectively block the sputtering of impurity ions in the ion beam; if the Al is too thick, the incident energy of the deuterium ion beam will be reduced, thereby reducing the neutron yield.

[0012] Furthermore, the thickness of the sputtered Al film is 50-100 nm.

[0013] The beneficial effect of adopting the above further solution is that the design is reasonable and the sputtering of impurity ions in the ion beam can be well blocked.

[0014] Furthermore, the deuterium storage coating is a titanium film.

[0015] The beneficial effect of adopting the above further scheme is that it is reasonable to choose and convenient to store deuterium.

[0016] Furthermore, the thickness of the titanium film is 2-5 μm.

[0017] The beneficial effect of adopting the above further solution is that the thickness of the titanium film is set reasonably, which plays a protective role and ensures the neutron yield of the deuterium-deuterium fusion reaction.

[0018] Furthermore, the deuterium ions are incident on the titanium film to a depth ranging from 800 to 850 nm.

[0019] The beneficial effect of adopting the above further solution is that the depth range of deuterium ions incident on the titanium film is reasonably set to ensure the total amount of deuterium absorbed by the titanium film.

[0020] Furthermore, a target substrate is included, and the other side of the deuterium storage coating is combined with the target substrate.

[0021] The beneficial effect of adopting the above further scheme is that the target substrate is reasonably arranged, and the deuterium storage coating and the protective layer are conveniently assembled.

[0022] The utility model also relates to a neutron tube, comprising a shell and an ion source, an accelerating electrode and a neutron target coaxially distributed in the shell in sequence, and also comprising the composite neutron target film as described above, wherein a protective layer is fixed on one end of the neutron target close to the accelerating electrode.

[0023] The beneficial effect of adopting the above further scheme is that during the operation, the ion source ionizes the gas and generates an ion beam, and the accelerating electrode applies voltage to form an electric field, which accelerates the ion beam to bombard the neutron target film on the neutron target to generate neutrons by fusion.

[0024] Furthermore, it also includes a storage device, which is fixedly installed in the shell and is used for releasing and absorbing gas.

[0025] The beneficial effect of adopting the above further solution is that during operation, the gas can be released and absorbed through the storage, thereby adjusting the gas in the shell to ensure that the ion source can smoothly ionize the gas and generate an ion beam. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a schematic diagram of the structure of the composite neutron target film of the utility model;

[0027] Figure 2 This is a schematic diagram of the structure of the neutron tube of the utility model;

[0028] Figure 3 This is a comparison chart of the bonding performance between the neutron target film of the utility model and the traditional neutron target film;

[0029] Figure 4 This is a schematic diagram of the composite neutron target film Mapping test structure of the utility model;

[0030] Figure 5 Schematic diagram of the traditional composite neutron target film Mapping test structure.

[0031] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0032] 1. Deuterium storage coating; 2. Protective layer; 3. Target substrate; 4. Housing; 5. Ion source; 6. Accelerating electrode; 7. Neutron target; 8. Storage device; 9. Neutron target membrane. DETAILED DESCRIPTION

[0033] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments can be combined with each other.

[0034] In the description of the present utility model, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present utility model and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, the terms "first", "second", etc. are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, features defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the present utility model, unless otherwise specified, "multiple" means two or more.

[0035] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.

[0036] The present invention will be described in detail below with reference to the accompanying drawings and in combination with embodiments.

[0037] Example 1

[0038] like Figure 1 As shown, this embodiment provides a composite neutron target film, including a deuterium storage coating 1 and a protective layer 2. The protective layer 2 is uniformly coated on one side surface of the deuterium storage coating 1 to reduce the damage of impurity ions released by the ion beam to the neutron target and to resist contamination and oxidation.

[0039] This embodiment has a simple structure and a reasonable design. The composite neutron target film structure reduces the damage to the high-purity titanium film caused by impurity ions released by the ion beam, while ensuring the total amount of deuterium absorbed by the titanium film, thereby protecting the high-purity titanium film from contamination and oxidation, greatly improving the yield and life of the neutron target film, and thus breaking the foreign technical monopoly on neutron target films.

[0040] Example 2

[0041] On the basis of Example 1, in this example, the protective layer 2 is an Al film.

[0042] Preferably, in this embodiment, the Al film is preferably a pure Al film.

[0043] The surface structure of pure Al film is dense, without obvious defects and holes, which can effectively block the sputtering of impurity ions in the ion beam; if Al is too thick, the incident energy of the deuterium ion beam will be reduced, thereby reducing the neutron yield.

[0044] The protective layer 2 has two functions. First, it is sputtering resistant, minimizing the damage to the neutron target caused by impurity ions released by the ion beam. Second, it is anti-pollution and oxidation resistant, minimizing the contamination of the high-purity titanium film and maintaining the maximum deuterium storage capacity of the high-purity titanium layer. When plating the protective layer, the thickness parameter should be considered as the key consideration, which is to protect the deuterium storage coating from oxidation and contamination, and not to lose the incident energy of the deuterium ions in the ion beam.

[0045] Example 3

[0046] On the basis of Example 2, in this example, the thickness of the sputtered Al film is 50-100 nm.

[0047] The scheme is reasonably designed and can effectively block the sputtering of impurity ions in the ion beam.

[0048] Preferably, in this embodiment, the thickness of the sputtered Al film is 70 nm.

[0049] An Al film with a thickness of 50-100nm is sputtered on the high-purity titanium deuterium storage film. The surface structure of the pure Al film is dense, without obvious defects and holes, and can effectively block the sputtering of impurity ions in the ion beam. If the Al film is too thick, the incident energy of the deuterium ion beam will be reduced, thereby reducing the neutron yield.

[0050] In addition, the pure Al film does not form a deuterated phase after absorbing deuterium because AlDx is thermodynamically unstable and easily decomposes Al+D. The D ions exist in the Al in a free state and do not affect the amount of deuterium absorbed by the titanium film.

[0051] Example 4

[0052] On the basis of the above embodiments, in this embodiment, the deuterium storage coating 1 is a titanium film.

[0053] This scheme is a reasonable choice and convenient for storing deuterium.

[0054] Example 5

[0055] On the basis of Example 4, in this example, the thickness of the titanium film is 2-5 μm.

[0056] The thickness of the titanium film is set reasonably to play a protective role and ensure the neutron yield of the deuterium-deuterium fusion reaction.

[0057] Example 6

[0058] On the basis of any one of Examples 4 to 5, in this embodiment, the deuterium ions are incident on the titanium film at a depth ranging from 800 to 850 nm.

[0059] The depth range of deuterium ions incident on the titanium film is set reasonably to ensure the total amount of deuterium absorbed by the titanium film.

[0060] Taking advantage of the easy oxidation characteristic of high-purity titanium itself, the titanium film is anodized under different oxidation conditions to prepare a surface oxide layer. The depth of deuterium ions entering the pure titanium film is about 800-850nm, and the depth of the incident titanium oxide layer is about 500-580nm. If the oxide layer is too thin, it cannot play a protective role. If the oxide layer is too thick, it will reduce the neutron yield of the deuterium-deuterium fusion reaction.

[0061] Example 7

[0062] On the basis of the above embodiments, this embodiment further includes a target substrate 3 , and the other side of the deuterium storage coating 1 is combined with the target substrate 3 .

[0063] The target substrate 3 is reasonably arranged to facilitate the assembly of the deuterium storage coating 1 and the protective layer 2 .

[0064] Preferably, in this embodiment, the material of the target substrate 3 is usually selected from metal materials such as Mo and Cu with high melting point and good thermal diffusion effect.

[0065] Example 8

[0066] Based on the above embodiments, Figure 2 As shown, this embodiment also provides a neutron tube, including a shell 4 and an ion source 5, an accelerating electrode 6 and a neutron target 7 coaxially distributed in the shell 4, and also includes the composite neutron target film as described above, and the protective layer 2 is fixed on one end of the neutron target 7 close to the accelerating electrode 6.

[0067] During operation, the ion source 5 ionizes the gas and generates an ion beam. The accelerating electrode 6 applies voltage and forms an electric field. The electric field accelerates the ion beam to bombard the neutron target film 9 on the neutron target 7 to generate fusion and generate neutrons.

[0068] According to the different neutron generating reactions, it can be divided into DT neutron tube and DD neutron tube, etc. However, many factors will affect the neutron yield and life of neutron tube, among which the neutron target film is one of the key factors.

[0069] The deuterium ion beam produced by the ion source is a mixture of various ion components, including deuterium diatomic ions, deuterium triatomic ions, and C + 、N + , O +Isoheavy impurity ions will reduce the probability of deuterium monatomic ions being adsorbed on the membrane surface and affect their distribution in the film, resulting in a decrease in neutron yield. After the ion beam bombards the titanium target, the surface of the target film changes from silvery white to light yellow and yellow, indicating that titanium oxide is formed on its surface. As the beam intensity increases, the titanium oxide layer becomes denser and the neutron yield decreases. During the transportation and storage of neutron tube targets, an oxide layer and a contamination layer are easily formed on the surface of the target film. It can be found that the oxide layer generated on the surface of the target film is mainly composed of TiO, Ti2O3, and TiO2. The oxide layer causes a decrease in the amount of deuterium absorbed. The deuterium ions in the ion beam can only react with deuterium in the target film after passing through the oxide layer, that is, the oxide layer affects the fusion reaction, thereby reducing the neutron yield.

[0070] It should be noted that the above-mentioned ion source 5 and acceleration electrode 6 both adopt the existing technology, and their specific structures and principles are not described in detail here.

[0071] In addition, the deuterium storage coating 1 , the protective layer 2 and the target substrate 3 constitute a neutron target film 9 .

[0072] Example 9

[0073] On the basis of Embodiment 8, this embodiment further includes a storage 8, which is fixedly installed in the housing 4 and is used for releasing and absorbing gas.

[0074] During operation, the gas can be released and absorbed through the storage 8, thereby adjusting the gas in the housing 4 to ensure that the ion source 5 can smoothly ionize the gas and generate an ion beam.

[0075] It should be noted that the above-mentioned memory 8 adopts the existing technology, and its specific structure and principle are not described in detail here.

[0076] The working principle of the utility model is as follows:

[0077] During the operation, the ion source 5 ionizes the gas and generates an ion beam. The accelerating electrode 6 applies voltage and forms an electric field. The electric field accelerates the ion beam to bombard the neutron target film 9 on the neutron target 7 to generate neutrons: D+T→He+n+17.590MeV or D+D→He+n+3.270MeV;

[0078] During this process, the gas can be released and absorbed through the storage 8, thereby adjusting the gas in the housing 4 to ensure that the ion source 5 can smoothly ionize the gas and generate an ion beam.

[0079] The material composition, structure and protective layer thickness of the neutron target film provided by the utility model improve the sputtering resistance, oxidation resistance and pollution resistance of the target film without reducing the total amount of deuterium absorption, thereby increasing the neutron yield and service life.

[0080] It should be noted that all electronic components involved in the present invention adopt the existing technology, and the above components are electrically connected, and the control circuits between the components are the existing technology.

[0081] Attached Figure 3 The figure shows a comparison of the bonding performance of the neutron target film of the present invention and the conventional neutron target film. Taking the bonding performance between the Al film and the target substrate 3 as an example, the bonding performance before optimization in the figure refers to the bonding performance between the Al film and the target substrate 3 in the conventional neutron target film, and the bonding performance after optimization refers to the bonding performance between the Al film and the target substrate 3 in the neutron target film of the present invention. As can be seen from the figure, the bonding performance between the Al film and the target substrate 3 in the neutron target film provided by the present invention is significantly greater than that between the Al film and the target substrate 3 in the conventional neutron target film.

[0082] Attached Figure 4 The following is a schematic diagram of the composite neutron target film mapping test structure of the utility model. Figure 5 It shows a schematic diagram of a conventional composite neutron target film Mapping test structure. By comparison, it can be seen that the oxidation degree of the neutron target film provided by the present invention with an Al film is significantly lower than the oxidation degree of the neutron target film without an Al film in the conventional technology.

[0083] Among them, Mapping is a technology that scans the surface of a sample with an electron beam to display the distribution and content of elements.

[0084] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.

[0085] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

[0086] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A composite neutron target film, characterized in that: The invention comprises a deuterium storage coating (1) and a protective layer (2); the protective layer (2) is evenly coated on a surface of one side of the deuterium storage coating (1) and is used to reduce the damage of impurity ions released by an ion beam to a neutron target and resist contamination and oxidation; the protective layer (2) is an Al film.

2. The composite neutron target film according to claim 1, characterized in that: The thickness of the Al film sputtered is 50-100 nm.

3. The composite neutron target film according to any one of claims 1 to 2, characterized in that: The deuterium storage coating (1) is a titanium thin film.

4. The composite neutron target film according to claim 3, characterized in that: The thickness of the titanium film is 2-5 μm.

5. The composite neutron target film according to claim 3, characterized in that: The deuterium ions are incident on the titanium film at a depth ranging from 800 to 850 nm.

6. The composite neutron target film according to any one of claims 1 to 2, characterized in that: It also comprises a target substrate (3), and the other side of the deuterium storage coating (1) is combined with the target substrate (3).

7. A neutron tube, comprising a housing (4) and an ion source (5), an accelerating electrode (6) and a neutron target (7) coaxially distributed in the housing (4), characterized in that: It also comprises the composite neutron target film according to any one of claims 1 to 6, wherein the protective layer (2) is fixed on one end of the neutron target (7) close to the accelerating electrode (6).

8. The neutron tube according to claim 7, characterized in that: It also comprises a storage (8), which is fixedly installed in the housing (4) and is used for releasing and absorbing gas.