Mold for preparing co-curing typical grid reinforced laminated plate with embedded damping layer

By designing the preparation mold for co-curing typical mesh reinforced laminated plates with embedded damping layer, the problem of easy aging and reduction of traditional damping structural materials during co-curing is solved, and good interface curing and high bearing capacity of the reinforced reinforcement layer is achieved, improving The vibration and noise reduction performance of the structure is achieved.

CN221968643UActive Publication Date: 2024-11-08HARBIN FRP INST
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420607227.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-27
Publication Date
2024-11-08
Estimated Expiration
2034-03-27

AI Technical Summary

Technical Problem

Traditional damping structural materials are prone to aging and reducing during co-curing, resulting in loss of interlayer mechanical properties and poor interfaces, which affect the bearing capacity of the structure and vibration and noise reduction effect.

Method used

Design a preparation mold for co-curing typical grid reinforced laminated plates with embedded damping layer, including base plate, cover plate, flap structure, limit structure and connection structure, and fix the flap blocks through predetermined gaps and limit structures to ensure composite Good interface contact and curing between material and damping material.

Benefits of technology

The bearing capacity and interface performance of the structure are improved, the problem of damping material shedding in traditional methods is avoided, and the vibration and noise reduction ability of the reinforced laminate is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221968643U_ABST
    Figure CN221968643U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of manufacturing dies for reinforcing ribs, in particular to a manufacturing die for a co-curing typical grid reinforced laminated plate embedded with a damping layer, which comprises a bottom plate, a first positioning structure and a second positioning structure. The cover plate is arranged above the bottom plate, and a second positioning structure is arranged on the outer edge of the cover plate; the sectioning structure is arranged between the bottom plate and the cover plate, the sectioning structure comprises a plurality of sectioning blocks arranged in an array mode, and a preset gap is formed between every two adjacent sectioning blocks; the limiting structure is arranged on the bottom plate and the sectioning block and is connected with the sectioning structure and the bottom plate; and the connecting structure penetrates through the first positioning structure and the second positioning structure. And then the connecting structure is used for connecting the first positioning structure and the second positioning structure on the cover plate on the bottom plate, so that the composite material and the damping material can be subsequently processed and treated, the reinforcing rib plate is smoothly manufactured, the interface performance is improved, and the bearing capacity of the structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of a preparation mold for reinforcing ribs, in particular to a preparation mold for a typical grid-reinforced laminated plate embedded with a damping layer and co-cured. Background Art

[0002] With the development of modern industry and the growth of lightweight structure applications, higher and newer requirements are put forward for the performance of constrained damping structures. Traditional damping structural materials include free damping structures and general constrained damping structures.

[0003] Among them, the free damping structure is to directly bond high-viscoelastic damping material on the surface of the composite material. This method has a poor interface and the damping layer is easy to fall off. The general constrained damping structure is to first vulcanize the damping material and then connect it to the composite structure through an adhesive. During the co-curing process, the damping material is prone to aging and reduction, and is easy to fall off, resulting in the loss of interlayer mechanical properties. It is restricted by factors such as space, structural quality and size, and also affects the interlayer mechanical properties of the structure. Utility Model Content

[0004] Therefore, the technical problem to be solved by the utility model is to overcome the problem in the prior art that after the damping material is vulcanized, the connection between the damping material and the composite material structure is achieved by adhesive, and during the co-curing process, the damping material is prone to aging and reduction, and is easy to fall off, thereby providing a preparation mold for a typical grid-reinforced laminate with an embedded damping layer for co-curing.

[0005] In order to solve the above technical problems, the utility model provides a preparation mold for a typical grid-reinforced laminate with an embedded damping layer co-cured, comprising: a base plate, the outer edge of which is provided with a first positioning structure; a cover plate, arranged above the base plate, and the outer edge of the cover plate is provided with a second positioning structure; a petal structure, arranged between the base plate and the cover plate, the petal structure comprising a plurality of petal blocks arranged in an array, and a predetermined gap is provided between two adjacent petals; a limiting structure, arranged on the base plate and the petal blocks, and connecting the petal structure and the base plate; a connecting structure, which runs through the first positioning structure and the second positioning structure.

[0006] Furthermore, the sizes of the plurality of petal blocks are the same.

[0007] Furthermore, the petal blocks have three groups, the petal blocks of the first group are arranged in the middle of the bottom plate, the petal blocks of the second group are arranged on the peripheral wall of the bottom plate, and the petal blocks of the third group are arranged at the top corners of the bottom plate.

[0008] Further, the first group of petal blocks has nine central petals, the second group of petal blocks has twelve side petals, and the third group of petal blocks has four corner petals.

[0009] Furthermore, the first positioning structure and the second positioning structure are positioning holes formed on the bottom plate and the cover plate.

[0010] Furthermore, a plurality of the positioning holes are arranged at intervals.

[0011] Furthermore, the connection structure is a locking member.

[0012] Furthermore, the limiting structure includes a bolt hole and a pin hole, and the bolt hole and the pin hole are both arranged on the petal block and the bottom plate.

[0013] Furthermore, the limiting structure further includes a first limiting member and a second limiting member, wherein the first limiting member passes through the bolt hole, and the second limiting member passes through the pin hole and connects the petal block and the base plate.

[0014] Furthermore, the bottom plate and the cover plate have the same size.

[0015] The technical solution of the utility model has the following advantages:

[0016] 1. The preparation mold used in the manufacturing process of the typical grid-reinforced laminate with embedded damping layer co-cured provided by the utility model includes: a base plate, the outer edge of which is provided with a first positioning structure; a cover plate, which is arranged above the base plate and the outer edge of which is provided with a second positioning structure; a petal structure, which is arranged between the base plate and the cover plate, and the petal structure includes a plurality of petal blocks arranged in an array, and a predetermined gap is provided between two adjacent petals; a limiting structure, which is arranged on the base plate and the petal blocks and connects the petal structure and the base plate; a connecting structure, which runs through the first positioning structure and the second positioning structure.

[0017] By setting the base plate and the cover plate, it is convenient to set multiple petal blocks between the base plate and the cover plate, and a predetermined gap is left between the multiple petal blocks. The setting of the predetermined gap is convenient for placing composite materials and damping materials in the predetermined gap, as well as the composite materials and damping materials on the multiple petal blocks, and finally forming a reinforced laminate; at the same time, the petal blocks and the base plate are limited by a limiting structure to ensure that the petal blocks are fixed on the base plate, and then the first positioning structure and the second positioning structure on the cover plate are connected by a connecting structure, so that the composite materials and damping materials can be subsequently processed, thereby ensuring the smooth production of the reinforced rib plate, increasing the interface performance, and improving the bearing capacity of the structure.

[0018] The preparation mold of the typical grid-reinforced laminate with embedded damping layer co-curing avoids the shortcomings of traditional free constraint and direct constraint free structure, ensures a good interface between the resin-based composite material structural layer and the damping layer, and at the same time has the advantages of high bearing capacity, vibration reduction and noise reduction.

[0019] 2. The manufacturing process of the typical grid reinforced laminated plate with embedded damping layer and co-cured by the utility model uses a preparation mold, and the bottom plate and the cover plate have the same size. That is, in actual use, the bottom plate and the cover plate can be used interchangeably, which increases the versatility of the bottom plate and the cover plate.

[0020] The utility model summary is provided to introduce a selection of concepts in a simplified form, which will be further described in the following detailed description. The utility model summary is not intended to identify key features or essential features of the present disclosure, nor is it intended to limit the scope of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 This is a schematic diagram of the structure of the utility model in which the petal blocks are placed on the bottom plate;

[0023] Figure 2 It is the distribution diagram of the petal blocks on the base plate;

[0024] Figure 3 This is a schematic diagram of the structure of laying out the center-split reinforcement ribs;

[0025] Figure 4 Schematic diagram of the structure for laying longitudinal fibers in the middle split petal;

[0026] Figure 5 It is a schematic diagram of the structure of the connection between the middle petal and the bottom plate;

[0027] Figure 6 It is a schematic diagram of the structure of the fiber direction of two adjacent middle petals;

[0028] Figure 7 It is a cross-sectional view of the fiber direction of two adjacent middle petals;

[0029] Figure 8 This is a schematic diagram of the structure for laying out the edge-split reinforcement ribs;

[0030] Fig. 9 Schematic diagram of the structure for laying longitudinal fibers in edge petals;

[0031] Fig.10 This is a schematic diagram of the structure for laying out the corner petal reinforcement;

[0032] Fig.11Schematic diagram of the structure for laying longitudinal fibers in corner petals;

[0033] Fig.12 is a schematic diagram of the structure of the base plate;

[0034] Fig.13 The figure is a schematic diagram of the connection structure between the petal block and the base plate;

[0035] Fig.14 A schematic diagram of the structure for applying adhesive;

[0036] Fig.15 This is a schematic diagram of the structure for polishing the damping layer;

[0037] Fig.16 A schematic structural diagram of a mold for preparing a typical grid-reinforced laminate with an embedded damping layer and co-cured according to the utility model;

[0038] Fig.17 It is a schematic diagram of the structure of the resin-based composite material structural layer and the damping layer;

[0039] Fig.18 A schematic structural diagram of a reinforced laminate of a mold for preparing a typical grid reinforced laminate with an embedded damping layer and co-cured provided by the utility model.

[0040] Description of reference numerals:

[0041] 1. Bottom plate; 2. First positioning structure; 3. Cover plate; 4. Second positioning structure; 5. Limiting structure; 6. Connection structure; 7. Center petal; 8. Side petal; 9. Corner petal; 10. Bolt hole; 11. Pin hole; 12. Resin-based composite material structural layer; 13. Damping layer; 14. Reinforced laminate. DETAILED DESCRIPTION

[0042] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present disclosure. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.

[0043] In the description of the present disclosure, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present disclosure. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present disclosure, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.

[0044] In the description of the present disclosure, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or can communicate with each other; it can be directly connected, or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to specific circumstances.

[0045] In the present disclosure, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply means that the first feature is lower in level than the second feature.

[0046] The disclosure below provides many different embodiments or examples to realize different structures of the present disclosure. In order to simplify the disclosure of the present disclosure, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present disclosure. In addition, the present disclosure can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplicity and clarity, and does not itself indicate the relationship between the various embodiments and / or settings discussed. In addition, the present disclosure provides various specific examples of processes and materials, but those of ordinary skill in the art can be aware of the application of other processes and / or the use of other materials.

[0047] The preferred embodiments of the present disclosure are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present disclosure, and are not used to limit the present disclosure.

[0048] See also Figures 1 to 18 As shown, the utility model provides a preparation mold used in the manufacturing process of a typical grid-reinforced laminate with an embedded damping layer co-cured, comprising: a base plate 1, wherein a first positioning structure 2 is provided at the outer edge of the base plate 1; a cover plate 3, which is arranged above the base plate 1, and a second positioning structure 4 is provided at the outer edge of the cover plate 3; a petal structure, which is arranged between the base plate 1 and the cover plate 3, and the petal structure includes a plurality of petal blocks arranged in an array, and a predetermined gap is provided between two adjacent petals; a limiting structure 5, which is arranged on the base plate 1 and the petal blocks, and connects the petal structure and the base plate 1; a connecting structure 6, which passes through the first positioning structure 2 and the second positioning structure 4.

[0049] By setting the base plate 1 and the cover plate 3, it is convenient to set a plurality of petal blocks between the base plate 1 and the cover plate 3, and a predetermined gap is left between the plurality of petal blocks. The setting of the predetermined gap facilitates the placement of composite materials and damping materials in the predetermined gap, as well as the composite materials and damping materials on the plurality of petal blocks, and finally forms a reinforced laminate 14; at the same time, the limiting structure 5 is used to limit the petal blocks and the base plate 1 to ensure that the petal blocks are fixed on the base plate 1, and then the connecting structure 6 is used to connect the first positioning structure 2 and the second positioning structure 4 on the cover plate 3 on the base plate 1, so that the composite materials and damping materials can be subsequently processed, thereby ensuring the smooth production of the reinforcing rib plate, increasing the interface performance, and improving the bearing capacity of the structure.

[0050] The preparation mold of the typical grid reinforced laminate with embedded damping layer 13 co-cured avoids the shortcomings of traditional free constraint and direct constraint free structure, ensures a good interface between the resin-based composite material structure layer 12 and the damping layer 13, and at the same time has the advantages of high bearing capacity, vibration reduction and noise reduction.

[0051] In some optional embodiments, the sizes of the plurality of petal blocks are the same, thereby ensuring the consistency of molding.

[0052] The petal blocks have three groups, the first group of petal blocks are arranged in the middle of the bottom plate 1, the second group of petal blocks are arranged on the peripheral wall of the bottom plate 1, and the third group of petal blocks are arranged at the top corners of the bottom plate 1. Specifically, the first group of petal blocks has nine middle petals 7, the second group of petal blocks has twelve side petals 8, and the third group of petal blocks has four corner petals 9.

[0053] In some optional embodiments, the first positioning structure 2 and the second positioning structure 4 are positioning holes formed on the bottom plate 1 and the cover plate 3. In addition, a plurality of the positioning holes are arranged at intervals.

[0054] The connection structure 6 is a locking member, which can be inserted into the positioning hole for positioning; of course, a positioning block can also be inserted into the positioning hole for positioning.

[0055] In some optional embodiments, the limiting structure 5 includes a bolt hole 10 and a pin hole 11, and the bolt hole 10 and the pin hole 11 are both provided on the petal block and the bottom plate 1. At the same time, the limiting structure 5 also includes a first limiting member and a second limiting member, the first limiting member passes through the bolt hole 10, and the second limiting member passes through the pin hole 11, and connects the petal block and the bottom plate 1.

[0056] In this embodiment, the bottom plate 1 and the cover plate 3 have the same size, that is, in actual use, the bottom plate 1 and the cover plate 3 can be used interchangeably, which increases the versatility of the bottom plate 1 and the cover plate 3.

[0057] The utility model provides a manufacturing process of a typical grid reinforced laminate with an embedded damping layer and co-cured, comprising: S1, laying petal blocks: first laying a middle petal 7, fixing it to a bottom plate 1, then laying an edge petal 8, fixing it to the bottom plate 1, and finally laying an angle petal 9, fixing it to the bottom plate 1; S2, laying reinforcing ribs and longitudinal limiters, as well as a resin-based composite material structural layer 12 for the middle petal 7, the edge petal 8, and the angle petal 9 respectively; S3, fixing the middle petal 7, the edge petal 8, and the angle petal 9 on the bottom plate 1, first installing the middle middle petal 7. Install the side petals 8 on all sides, and finally install the corner petals 9 at the four corners, and fix them; S4. Lay the composite skin and damping layer 13 materials on the resin-based composite material structural layer 12 of each petal; S5. Install the cover plate 3 on multiple petal blocks and fix them, cold-close the mold, and apply a pre-tightening force at room temperature; then push the mold to the curing furnace, heat it to the mold heat-sealing temperature, and heat-seal the mold; S6. After the product is cured, cool it down to room temperature, start demoulding, and trim the reinforced laminate 14 after demoulding.

[0058] Among them, the reinforcement ribs are composed of 25 petals (5×5). The formed reinforcement ribs are 4×4, and the reinforcement plate has no reinforcement ribs on the four sides. The 25 petals are divided into 4 corner petals 9, 12 side petals 8 and 9 center petals 7. The laying order is to lay the center petal 7 first and fix it to the bottom plate 1, then lay the side petal 8 and fix it to the bottom plate 1, and finally lay the corner petal 9 and fix it to the bottom plate 1.

[0059] In step S2, circumferential reinforcement ribs are laid on the center flap 7, and longitudinal fibers excluding the bottom surface and the resin-based composite material structure layer 12 are laid on the center flap 7. Then, the longitudinal fibers on the other side are laid in an orthogonal direction. In this way, the reinforcement ribs of the center flap 7 and the resin-based composite material structure layer 12 of the center flap 7 are laid orthogonally, ensuring that there are continuous fibers between the reinforcement ribs and the resin-based composite material structure layer 12, which helps the load-bearing capacity of the structure.

[0060] This method of laying the reinforcing ribs ensures that the reinforcing ribs and the resin-based composite material structure layer 12 are transitioned through continuous fibers, rather than relying solely on interface bonding between the reinforcing ribs and the resin-based composite material structure layer 12. After laying the middle petal 7, it is first positioned with the bottom plate 1 through the second stopper and the pin hole 11, and then connected and fixed with the bottom plate 1 through the first stopper and the bolt hole 10.

[0061] Furthermore, when positioning the two center petals 7, the fiber directions of the center petals 7 remain consistent.

[0062] At the same time, in step S2, circumferential reinforcement ribs are laid on the side petals 8, reinforcement ribs are not laid on the borders, and longitudinal fibers and resin-based composite material structural layers 12 are laid on the side petals 8 except for the bottom surface and the borders. The second stopper and the pin hole 11 are first used to position the bottom plate 1, and then the first stopper and the bolt hole 10 are used to connect and fix the bottom plate 1, and the connection method is the same as that of the middle petal 7.

[0063] In step S2, circumferential reinforcement ribs are laid on the diagonal petals 9, reinforcement ribs are not laid at the boundaries, and longitudinal fibers excluding the bottom surface and the boundaries and the resin-based composite material structure layer 12 are laid on the diagonal petals 9. After laying the diagonal petals 9, they are first positioned with the bottom plate 1 through the second stopper and the pin hole 11, and then connected and fixed with the bottom plate 1 through the first stopper and the bolt hole 10, and the connection method is the same as that of the diagonal petals 9.

[0064] Then, install each petal on the base plate 1. During installation, first locate the pin hole 11, then screw on the second limiter, but do not tighten it into place first. After all petal blocks are installed, tighten each petal block.

[0065] The installation sequence is to first install the middle petal 7, then the side petals 8 on the four sides, and finally the corner petals 9 on the four corners. After each petal is installed in place, the second stopper is tightened, and the reinforcement rib is formed.

[0066] In some optional embodiments, composite skin and damping layer 13 materials are laid on the resin-based composite material structure layer 12 of each petal.

[0067] First, lay the composite skin. According to the designed layering, lay n layers of composite skin, and then prepare to lay the damping layer 13. In step S4, S41, first apply adhesive to the upper surface of the nth layer of composite material, apply it evenly, and use a scraper to scrape off the excess adhesive on the surface after applying; prevent excessive adhesive from forming a resin-rich layer on the surface, which affects the interface performance. S42, treat the surface of the damping layer 13 with fine sandpaper, gently polish both sides of the damping layer 13, and wipe off burrs, powder, etc. with a surface treatment agent such as ethyl acetate; S43, apply adhesive on the surface of the damping layer 13, lay it on the surface of the nth layer of composite skin, and then continue to apply adhesive on the back of the damping layer 13, and use a scraper to remove excess adhesive; S44, apply adhesive to the surface of the n+1th layer of composite skin, lay it on the back of the damping layer 13, and continue to lay the composite material according to the design until the next layer of damping layer 13, repeat the above steps until the composite skin is laid.

[0068] Place the locking piece between the positioning holes of the bottom plate 1, which are used to ensure the surface quality and dimensional accuracy of the product. Cover the cover plate 3, tighten the bottom plate 1 and the cover plate 3 with the locking piece, cold-close the bottom plate 1 and the cover plate 3, and apply pre-tightening force at room temperature.

[0069] The mold is then pushed into a curing furnace, heated to the mold heat-sealing temperature, and heat-sealed to allow the resin to flow fully. The incompressible properties of the damping layer 13 are utilized to form an interpenetrating grid structure between the resin-based composite material structural layer 12 and the damping layer 13, thereby increasing the interface performance and improving the bearing capacity of the structure.

[0070] After the product solidifies, it is cooled to room temperature and demoulding begins. The demoulding sequence is to first remove the locking piece between the bottom plate 1 and the cover plate 3, remove the locking piece, then lift the bottom plate 1, and successively remove the positioning pins and the first limiting piece of the corner petal 9, the side petal 8 and the middle petal 7, so that the petal block and the bottom plate 1 are separated.

[0071] Then use a pin puller to remove each petal from the product one by one. And trim the demoulding product, such as removing burrs and polishing the surface resin-rich layer.

[0072] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention of the utility model.

Claims

1. A mold for preparing a typical grid-reinforced laminate with an embedded damping layer and co-cured, characterized in that: include: A bottom plate (1), wherein the outer edge of the bottom plate (1) is provided with a first positioning structure (2); A cover plate (3) is arranged above the base plate (1), and a second positioning structure (4) is provided on the outer edge of the cover plate (3); A petal structure is arranged between the base plate (1) and the cover plate (3), the petal structure comprising a plurality of petal blocks arranged in an array, and a predetermined gap is provided between two adjacent petals; A limiting structure (5) is provided on the base plate (1) and the petal block, and connects the petal structure and the base plate (1); A connecting structure (6) passes through the first positioning structure (2) and the second positioning structure (4).

2. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 1, characterized in that: The sizes of the plurality of petal blocks are the same.

3. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 2, characterized in that: The petal blocks have three groups, the first group of petal blocks are arranged in the middle of the base plate (1), the second group of petal blocks are arranged on the peripheral wall of the base plate (1), and the third group of petal blocks are arranged at the top corners of the base plate (1).

4. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 3, characterized in that: The first group of petals has nine central petals (7), the second group of petals has twelve side petals (8), and the third group of petals has four corner petals (9).

5. The mold for preparing a typical grid-reinforced laminate with embedded damping layer co-cured according to any one of claims 1 to 4, characterized in that: The first positioning structure (2) and the second positioning structure (4) are positioning holes formed on the bottom plate (1) and the cover plate (3).

6. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 5, characterized in that: A plurality of the positioning holes are arranged at intervals.

7. The mold for preparing a typical grid-reinforced laminate with embedded damping layer co-cured according to claim 5, characterized in that: The connecting structure (6) is a locking piece.

8. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 5, characterized in that: The limiting structure (5) comprises a bolt hole (10) and a pin hole (11), and the bolt hole (10) and the pin hole (11) are both arranged on the petal block and the base plate (1).

9. The mold for preparing the typical grid-reinforced laminate with embedded damping layer co-cured according to claim 8, characterized in that: The limiting structure (5) further comprises a first limiting member and a second limiting member, wherein the first limiting member passes through the bolt hole (10), and the second limiting member passes through the pin hole (11) and connects the petal block and the base plate (1).

10. The mold for preparing a typical grid-reinforced laminate with embedded damping layer co-cured according to claim 1, characterized in that: The bottom plate (1) and the cover plate (3) have the same size.

Citation Information

Cited By

  • Manufacturing process and mold for co-curing typical grid reinforced laminated plate embedded with damping layer

    CN118181808A