Aluminum material surface oxidation treatment preparation device

By using stirring members and vibrating members in the aluminum surface oxidation treatment device, the problem of insufficient flow of the electrolyte is solved, and more uniform ion transport and more efficient oxidation treatment are achieved, avoiding waste of electrolyte and improving overall preparation efficiency.

CN221971707UActive Publication Date: 2024-11-08JIANGSU FENGHUA METAL PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420097054.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-16
Publication Date
2024-11-08
Estimated Expiration
2034-01-16

AI Technical Summary

Technical Problem

During the oxidation process of aluminum surface, the flow and mixing of the electrolyte is insufficient, resulting in low oxidation treatment efficiency and low preparation efficiency.

Method used

A preparation device for surface oxidation treatment of aluminum materials is designed, including a stirring member and a vibration member. The stirring member realizes uniform stirring of the electrolyte through the motor driving gear and the stirring rod to speed up ion transmission; the vibration member realizes the electrolyte through the motor driving cam and roller. reflux and shaking of residual liquid.

Benefits of technology

The uniformity and efficiency of oxidation treatment are improved, the waste of electrolyte is reduced, and the preparation efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221971707U_ABST
    Figure CN221971707U_ABST
Patent Text Reader

Abstract

The utility model discloses an aluminum material surface oxidation treatment preparation device, and relates to the technical field of aluminum material processing. The device comprises a bottom plate, a mounting frame is arranged at the top end of the bottom plate, an oxidation treatment electrolysis barrel is arranged at the top end of the mounting frame, a stirring component is arranged in the oxidation treatment electrolysis barrel, and an anode reaction rod and a cathode reaction rod are arranged at the bottom end in the oxidation treatment electrolysis barrel; and a mounting frame for mounting the aluminum material is movably arranged above the oxidation treatment electrolysis barrel. According to the utility model, through the arranged stirring component, electrolyzed water can be uniformly stirred when an aluminum plate is subjected to oxidation treatment processing, so that the transmission of ions in a solvent can be accelerated, the reaction is more uniform, the reaction efficiency can be accelerated, and the oxidation preparation efficiency is improved; after the aluminum profile is subjected to oxidation treatment, the aluminum profile can be vibrated up and down in a reciprocating mode, and residual electrolyte on the surface of the aluminum profile is shaken off and collected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of aluminum material processing, in particular to a device for preparing aluminum material surface oxidation treatment. Background Art

[0002] With the development of the profile processing industry, in order to optimize the decorative effect of aluminum profiles, enhance their corrosion resistance and extend their service life, aluminum alloy profiles generally undergo surface oxidation treatment. The commonly used method is anodizing. Anodizing is carried out under high voltage and is an electrochemical reaction process.

[0003] When aluminum is subjected to surface oxidation treatment, it needs to be immersed in an electrolyte. The aluminum can react with the electrolyte, thereby causing an oxidation reaction on its surface. However, during the immersion process, its oxidation reaction can only be achieved after ion exchange is completed. During use, simply immersing it makes it difficult for the electrolyte to flow and mix sufficiently, thereby reducing its oxidation treatment efficiency and resulting in low preparation efficiency.

[0004] For this purpose, a preparation device for surface oxidation treatment of aluminum material is proposed. Utility Model Content

[0005] In order to solve the problems existing in the prior art, the utility model provides a device for preparing an aluminum material surface oxidation treatment.

[0006] In order to achieve the above-mentioned purpose, the utility model specifically adopts the following technical solutions:

[0007] A surface oxidation treatment preparation device for aluminum materials comprises a bottom plate, a mounting frame is arranged at the top of the bottom plate, an oxidation treatment electrolytic barrel is arranged at the top of the mounting frame, a stirring member is arranged in the oxidation treatment electrolytic barrel, an anode reaction rod and a cathode reaction rod are arranged at the bottom of the oxidation treatment electrolytic barrel, a mounting frame for mounting the aluminum material is movably arranged above the oxidation treatment electrolytic barrel, the stirring member comprises a first motor arranged at the top of the mounting frame and a connecting rod rotatably arranged inside the oxidation treatment electrolytic barrel, the connecting rod is connected to the main shaft end of the first motor, a rotating rod is rotatably arranged at the top of the connecting rod, a gear is arranged at the top of the rotating rod, an inner gear ring meshing with the gear is arranged on the inner side of the oxidation treatment electrolytic barrel, a connecting rotating rod is connected to the top of the gear, and a stirring rod is arranged on the connecting rotating rod.

[0008] Furthermore, two mounting plates are arranged at the top of the bottom plate, an electric slide rail is arranged at the top of the mounting plate, and a sliding plate is slidably arranged on the electric slide rail.

[0009] Furthermore, an electric telescopic rod is provided at the bottom end of the sliding plate, the bottom end of the electric telescopic rod is connected to a first connecting plate, the bottom end of the first connecting plate is connected to the telescopic rod, a spring is sleeved on the telescopic rod, the telescopic end of the telescopic rod is connected to a second connecting plate, and the mounting frame is arranged at the bottom end of the second connecting plate.

[0010] Furthermore, a vibration component for accelerating the outflow of electrolyte is arranged on the first connecting plate, and the vibration component includes a fixed plate arranged at the bottom end of the first connecting plate and a roller arranged at the top end of the second connecting plate. A second motor is arranged on one side of the fixed plate, and a cam is connected to the output end of the second motor.

[0011] Furthermore, the heights of the anode reaction rod and the cathode reaction rod are lower than the height of the connecting rod.

[0012] The beneficial effects of the utility model are as follows:

[0013] 1. The utility model provides a stirring component, which can evenly stir the electrolyzed water when the aluminum plate is oxidized, thereby accelerating the transmission of ions in the solvent, making the reaction more uniform, accelerating the reaction efficiency, and improving its oxidation preparation efficiency.

[0014] 2. The utility model provides a vibration component, which can take the aluminum profile out of the electrolyte after oxidation treatment, and then vibrate it up and down to shake off the electrolyte remaining on the surface for collection, thereby avoiding the waste of electrolyte and increasing the reflux speed of the electrolyte, thereby ensuring its preparation efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a three-dimensional structural schematic diagram of the utility model;

[0016] Figure 2 It is the first cross-sectional view of the utility model;

[0017] Figure 3 It is the second cross-sectional view of the utility model;

[0018] Figure 4 This is a schematic diagram of the structure of the vibration component of the utility model;

[0019] Figure 5 It is an enlarged view of part A of the utility model.

[0020] Figure numerals: 1. bottom plate; 2. mounting plate; 3. electric slide rail; 301. sliding plate; 4. mounting frame; 5. oxidation treatment electrolytic barrel; 6. stirring member; 601. first motor; 602. connecting rod; 603. rotating rod; 604. gear; 605. inner ring gear; 606. connecting rotating rod; 607. stirring rod; 7. anode reaction rod; 701. cathode reaction rod; 8. electric telescopic rod; 801. first connecting plate; 802. telescopic rod; 803. spring; 804. second connecting plate; 9. vibration member; 901. fixing plate; 902. second motor; 903. cam; 904. roller; 10. mounting frame. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical scheme and advantages of the embodiments of the utility model clearer, the technical scheme in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Generally, the components of the embodiments of the utility model described and shown in the drawings here can be arranged and designed in various different configurations.

[0022] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the present invention to be protected, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0023] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings. In addition, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.

[0024] In the description of the embodiments of the present invention, it should be noted that the terms "inside", "outside", "upper", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or are the orientations or positional relationships in which the utility model product is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0025] like Figure 1-3As shown, a surface oxidation treatment preparation device for aluminum material comprises a bottom plate 1, a mounting frame 4 is arranged at the top of the bottom plate 1, an oxidation treatment electrolytic barrel 5 is arranged at the top of the mounting frame 4, a stirring member 6 is arranged in the oxidation treatment electrolytic barrel 5, an anode reaction rod 7 and a cathode reaction rod 701 are arranged at the bottom of the oxidation treatment electrolytic barrel 5, a mounting frame 10 for mounting aluminum material is movably arranged above the oxidation treatment electrolytic barrel 5, and the stirring member 6 comprises a first motor 601 arranged at the top of the mounting frame 4 and a connecting rod 602 rotatably arranged inside the oxidation treatment electrolytic barrel 5 , the connecting rod 602 is connected to the main shaft end of the first motor 601, the top of the connecting rod 602 is rotatably provided with a rotating rod 603, the top of the rotating rod 603 is provided with a gear 604, the inner side of the oxidation treatment electrolytic barrel 5 is provided with an inner gear ring 605 meshing with the gear 604, the top of the gear 604 is connected with a connecting rotating rod 606, and a stirring rod 607 is provided on the connecting rotating rod 606; specifically, there is electrolyte in the oxidation treatment electrolytic barrel 5, after the aluminum plate is installed on the mounting frame 10, it is immersed in the electrolyte, so that the oxidation treatment of its surface can be achieved, During the reaction, the stirring member 6 can stir the electrolyte, thereby accelerating the transmission of ions in the solvent, making the reaction more uniform and accelerating the reaction efficiency. The first motor 601 can drive the connecting rod 602 to rotate, thereby stirring the electrolyte from the bottom. When the connecting rod 602 rotates, it can drive the gear 604 to rotate around the main axis of the first motor 601. During the rotation, the gear 604 meshes with the inner gear ring 605, which can drive the gear 604 to rotate on its own, thereby During the process, the stirring rod 607 can be driven to rotate around the connecting rotating rod 606, and can also be driven to rotate on the outside around the center of the oxidation treatment electrolytic barrel 5, so that the electrolyte can be evenly stirred, so that during the reaction, the flow of the solvent is accelerated, and at the same time, its reaction efficiency is accelerated. When the aluminum plate is oxidized, it and the mounting frame 10 will be immersed in the center position of the oxidation treatment electrolytic barrel 5 at the same time. When stirring, the stirring rod 607 can rotate around its side, so it will not affect the immersion oxidation process of the aluminum plate.

[0026] like Figure 3 As shown, two mounting plates 2 are arranged at the top of the base plate 1, an electric slide rail 3 is arranged at the top of the mounting plate 2, and a sliding plate 301 is slidingly arranged on the electric slide rail 3; specifically, the electric slide rail 3 can drive the sliding plate 301 to slide, thereby driving the transportation of the aluminum plate. The electric slide rail 3 is a prior art, so its principle, structure and model are not described in detail here.

[0027] like Figure 3 and 4As shown, an electric telescopic rod 8 is provided at the bottom end of the sliding plate 301, and the bottom end of the electric telescopic rod 8 is connected to a first connecting plate 801, and the bottom end of the first connecting plate 801 is connected to a telescopic rod 802, and a spring 803 is sleeved on the telescopic rod 802, and the telescopic end of the telescopic rod 802 is connected to a second connecting plate 804, and the mounting frame 10 is arranged at the bottom end of the second connecting plate 804; specifically, the extension and retraction of the electric telescopic rod 8 can drive the mounting frame 10 to rise and fall, so that the aluminum plate can be immersed in the electrolyte, and after the preparation is completed, it can be taken out.

[0028] like Figure 4 and 5 As shown, a vibration component 9 for accelerating the outflow of electrolyte is arranged on the first connecting plate 801, and the vibration component 9 includes a fixed plate 901 arranged at the bottom end of the first connecting plate 801 and a roller 904 arranged at the top end of the second connecting plate 804. A second motor 902 is arranged on one side of the fixed plate 901, and a cam 903 is connected to the output end of the second motor 902; specifically, under the action of the spring 803 and the telescopic rod 802, the mounting frame 10 can be lifted and lowered. After the electrolytic preparation is completed, the mounting frame 10 is lifted upward to take out the oxidized aluminum plate, and then the second motor 902 can drive the cam 903 to rotate, and the rotation of the cam 903 squeezes the roller 904, thereby driving the mounting frame 10 to rise and fall back and forth, thereby realizing a vibration effect, thereby accelerating the outflow of electrolyte on the oxidized aluminum plate.

[0029] like Figure 3 As shown, the heights of the anode reaction rod 7 and the cathode reaction rod 701 are lower than the height of the connecting rod 602 .

[0030] In summary: there is electrolyte in the oxidation treatment electrolytic barrel 5. After the aluminum plate is installed on the mounting frame 10, it is immersed in the electrolyte to achieve oxidation treatment on its surface. During the reaction, the stirring member 6 can stir the electrolyte, thereby accelerating the transmission of ions in the solvent, making the reaction more uniform and accelerating the reaction efficiency. After the oxidation preparation is successful, the oxidized aluminum plate and the mounting frame 10 can be taken out by the electric telescopic rod 8, and then under the action of the vibration member 9, the reflux of the residual electrolyte thereon can be accelerated.

[0031] The above shows and describes the basic principle, main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and the specification only describe the principles of the utility model. The utility model may be subject to various changes and improvements without departing from the spirit and scope of the utility model. These changes and improvements fall within the scope of the utility model to be protected. The scope of protection claimed by the utility model is defined by the attached claims and their equivalents.

Claims

1. A device for preparing aluminum surface oxidation treatment, characterized in that: The invention comprises a bottom plate (1), a mounting frame (4) is arranged at the top of the bottom plate (1), an oxidation treatment electrolysis barrel (5) is arranged at the top of the mounting frame (4), a stirring member (6) is arranged inside the oxidation treatment electrolysis barrel (5), an anode reaction rod (7) and a cathode reaction rod (701) are arranged at the bottom of the oxidation treatment electrolysis barrel (5), a mounting frame (10) for mounting the aluminum material is movably arranged above the oxidation treatment electrolysis barrel (5), and the stirring member (6) comprises a first motor (601) and a rotating device (601) arranged at the top of the mounting frame (4). A connecting rod (602) is arranged inside the oxidation treatment electrolytic barrel (5), the connecting rod (602) is connected to the main shaft end of the first motor (601), a rotating rod (603) is rotatably arranged at the top end of the connecting rod (602), a gear (604) is arranged at the top end of the rotating rod (603), an inner gear ring (605) meshing with the gear (604) is arranged on the inner side of the oxidation treatment electrolytic barrel (5), a connecting rotating rod (606) is connected to the top end of the gear (604), and a stirring rod (607) is arranged on the connecting rotating rod (606).

2. The aluminum surface oxidation treatment preparation device according to claim 1 is characterized in that: Two mounting plates (2) are arranged at the top of the bottom plate (1), an electric slide rail (3) is arranged at the top of the mounting plate (2), and a sliding plate (301) is slidably arranged on the electric slide rail (3).

3. The aluminum surface oxidation treatment preparation device according to claim 2 is characterized in that: An electric telescopic rod (8) is arranged at the bottom end of the sliding plate (301), the bottom end of the electric telescopic rod (8) is connected to a first connecting plate (801), the bottom end of the first connecting plate (801) is connected to a telescopic rod (802), a spring (803) is sleeved on the telescopic rod (802), the telescopic end of the telescopic rod (802) is connected to a second connecting plate (804), and the mounting frame (10) is arranged at the bottom end of the second connecting plate (804).

4. The aluminum material surface oxidation treatment preparation device according to claim 3, characterized in that: A vibration component (9) for accelerating the outflow of electrolyte is arranged on the first connecting plate (801), and the vibration component (9) comprises a fixed plate (901) arranged at the bottom end of the first connecting plate (801) and a roller (904) arranged at the top end of the second connecting plate (804); a second motor (902) is arranged on one side of the fixed plate (901), and a cam (903) is connected to the output end of the second motor (902).

5. The aluminum material surface oxidation treatment preparation device according to claim 1, characterized in that: The heights of the anode reaction rod (7) and the cathode reaction rod (701) are lower than the height of the connecting rod (602).