Device for improving adhesive force of tinplate coating

The surface of tinplate is cleaned and activated by excimer lamps and plasma devices, combined with conveyor belts and heating devices, and the problem of poor adhesion of water-based coatings and photocured coatings is solved, achieving efficient and environmentally friendly adhesion improvement.

CN221983010UActive Publication Date: 2024-11-12HUAAO NEW CONTAINERS (HANGZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420459056.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-11
Publication Date
2024-11-12
Estimated Expiration
2034-03-11

AI Technical Summary

Technical Problem

Water-based coatings and photocuring coatings have poor adhesion on the surface of tinplate. The prior art such as water washing cleaning and flame spraying treatment poses waste of resources and safety risks, and adding solvents to the coatings is not environmentally friendly.

Method used

The surface of tinplate is treated twice using excimer lamp equipment and plasma devices, and the stains are cleaned and the surface is activated respectively. Adhesion is improved through the conveyor belt and heating device, and secondary pollution is prevented using protective covers and inert gases.

Benefits of technology

It effectively enhances the adhesion of tinplate surface coating, avoids the problems of high energy consumption and low accuracy of a single treatment method, and ensures environmental protection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221983010U_ABST
    Figure CN221983010U_ABST
Patent Text Reader

Abstract

The utility model provides a device for improving the adhesive force of a tinplate coating. The device for improving the adhesive force of the tinplate coating comprises excimer lamp equipment, a plasma device and a conveying belt, tinplate is arranged on the conveying belt, the conveying belt conveys the tinplate to sequentially pass through the excimer lamp equipment and the plasma device, an electromagnetic heating ring is arranged below the conveying belt, and the electromagnetic heating ring is arranged on the conveying belt in the moving direction of the conveying belt. A plurality of heating devices arranged at intervals and a plurality of temperature detection devices arranged at intervals are arranged beside the conveying belt. Two times of surface treatment are carried out on the tinplate through the excimer lamp device and the plasma device, stains on the surface of the tinplate are cleaned respectively, the surface of the tinplate is activated, and then the surface adhesive force of the tinplate is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of metal processing equipment, in particular to a device for improving the adhesion of tinplate coating. Background Art

[0002] With the increasing requirements for environmental protection, the traditional oily paint used on the surface of tinplate is gradually replaced by water-based paint and light-curing paint. However, water-based paint and light-curing paint have high requirements on the surface of the substrate. Water-based paint and light-curing paint have low internal solvent content and cannot dissolve oil on the metal surface, resulting in poor adhesion on the tinplate surface and cannot be firmly attached to the tinplate surface.

[0003] In the prior art, tinplate is generally washed with water, or flame-sprayed on the surface of tinplate, or solvents are added to the coating to improve the adhesion of the coating on the tinplate surface. However, water washing and cleaning consumes a large amount of water, which easily causes waste of water resources and pollutes the site; flame treatment has great safety hazards; adding solvents to the coating requires high requirements for the treatment of printing and coating waste gas, which is not environmentally friendly. Utility Model Content

[0004] The purpose of the utility model is to propose a device for improving the adhesion of tinplate coatings in view of the above-mentioned deficiencies in the prior art, and to perform two surface treatments on tinplate by using an excimer lamp device and a plasma device, respectively cleaning the stains on the tinplate surface and activating the tinplate surface, thereby increasing the adhesion of the tinplate surface.

[0005] The utility model provides a device for improving the adhesion of tinplate coating, comprising an excimer lamp device, a plasma device and a conveyor belt, wherein the tinplate is arranged on the conveyor belt, and the conveyor belt transports the tinplate to pass through the excimer lamp device and the plasma device in sequence, an electromagnetic heating ring is arranged under the conveyor belt, and a plurality of heating devices and a plurality of temperature detection devices arranged at intervals are arranged on the side of the conveyor belt along the moving direction of the conveyor belt.

[0006] The better technical solution of the utility model is as follows: the irradiation wavelength of the excimer lamp device is 172nm, and the irradiation intensity of the excimer lamp device is 100mw / cm2.

[0007] A better technical solution of the utility model is as follows: a plurality of suction ports are arranged below the excimer lamp device, the suction ports are arranged beside the conveyor belt, and the suction ports are arranged toward the tinplate processing surface.

[0008] A better technical solution of the utility model is as follows: a protective cover is provided on the conveyor belt, the protective cover is connected to the plasma device, and extends to the moving end of the conveyor belt.

[0009] A better technical solution of the utility model is that the protective cover is filled with inert gas, and the inert gas flows in the protective cover.

[0010] A better technical solution of the utility model is as follows: the temperature detection device is arranged at the moving head end, the moving end end of the conveyor belt, and inside the protective cover.

[0011] A better technical solution of the utility model is as follows: a contact angle measuring instrument is arranged at the moving end of the conveyor belt, and the contact angle measuring instrument is arranged in the protective cover.

[0012] The better technical solution of the utility model is that the conveyor belt is connected to the coating link.

[0013] A better technical solution of the utility model: the heating device is an infrared heater.

[0014] A better technical solution of the utility model: the conveyor belt is a non-metallic belt.

[0015] The utility model provides a device for improving the adhesion of tinplate coatings, which has the following beneficial effects:

[0016] 1. Set up the excimer lamp equipment and plasma device in sequence, use the excimer lamp equipment to clean the stains on the tinplate surface, and use the plasma device to activate the tinplate surface, so as to increase the adhesion of the tinplate surface, and avoid the problems of too long time, too much energy consumption, low processing accuracy, and deposition of by-products on the tinplate surface after treatment when a single excimer lamp equipment or a single plasma device is used to treat the tinplate surface;

[0017] 2. Set up a protective cover on the conveyor belt and fill the protective cover with inert gas to avoid degradation of the tinplate surface after plasma treatment, forming new oxides and causing secondary pollution. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The accompanying drawings, which are incorporated into the specification and constitute a part of the specification, illustrate embodiments of the utility model and are used together with the description to explain the principles of the utility model. In these drawings, similar reference numerals are used to represent similar elements. The drawings described below are some embodiments of the utility model, rather than all embodiments. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without paying creative work.

[0019] Figure 1 It is a schematic diagram of an embodiment of the utility model.

[0020] Figure 2 It is a side view schematic diagram of an embodiment of the utility model.

[0021] In the figure: 10, excimer lamp equipment; 11, ultraviolet lamp tube; 20, plasma device; 30, conveyor belt; 41, electromagnetic heating coil; 42, heating device; 43, suction port; 44, temperature detection device; 45, air inlet; 50, protective cover; 51, contact angle measuring instrument; 60, tinplate. DETAILED DESCRIPTION

[0022] In order to make the purpose, technical scheme and advantages of the embodiment of the utility model clearer, the technical scheme in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model. It should be noted that the embodiments in this application and the features in the embodiments can be combined with each other arbitrarily without conflict.

[0023] See also Figure 1 to Figure 2 A device for improving the adhesion of tinplate coating comprises an excimer lamp device 10, a plasma device 20 and a conveyor belt 30. Tinplate 60 is placed on the conveyor belt 30. The conveyor belt 30 drives the tinplate 60 to pass through the excimer lamp device 10 and the plasma device 20 in sequence for surface treatment. An electromagnetic heating ring 41 is arranged under the conveyor belt 30. Along the moving direction of the conveyor belt 30, a plurality of heating devices 42 and temperature detection devices 44 are arranged at intervals on the side of the conveyor belt 30, which are used to heat the tinplate 60 and detect the temperature of the tinplate 60 respectively.

[0024] A plurality of ultraviolet lamp tubes 11 are arranged inside the excimer lamp device 10, and the ultraviolet lamp tubes 11 are arranged in parallel above the conveyor belt 30, and the plurality of ultraviolet lamp tubes 11 are arranged in parallel and spaced apart to irradiate the surface of the tinplate 60 to be coated on the conveyor belt 30. In order to effectively remove pollutants on the surface of the tinplate 60, such as organic matter such as grease, when the excimer lamp device 10 irradiates the tinplate 60, in the present application, the irradiation wavelength of the ultraviolet lamp tube 11 is set to 172nm, and the irradiation intensity is 100mw / cm2. After the excimer lamp device 10 irradiates the tinplate 60, the pollutants on the surface of the tinplate 60 can be decomposed and oxidized to form gas. In order to smoothly discharge such decomposition products, a plurality of suction ports 43 are further provided below the excimer lamp device 10. The plurality of suction ports 43 are arranged at intervals along the moving direction of the conveyor belt 30. The suction ports 43 face the upper surface of the tinplate 60, so as to timely discharge the gas generated after the excimer lamp device 10 irradiates the tinplate 60, thereby preventing products such as ozone, carbon dioxide, and water from remaining on the surface of the tinplate 60.

[0025] Along the moving direction of the conveyor belt 30, an electromagnetic heating coil 41 is arranged below the conveyor belt 30, and the electromagnetic heating coil 41 is connected to a power source, and uses electromagnetic induction to directly heat the tinplate 60, so as to accelerate the speed at which the excimer lamp device 10 and the plasma device 20 clean the pollutants on the surface of the tinplate 60. In the present application, when the excimer lamp device 10 and the plasma device 20 perform surface treatment on the tinplate 60, the temperature thereof should be limited to below 200°C, so as to avoid the surface of the tinplate 60 after the surface treatment from reacting again; considering comprehensive reasons such as production safety and heating power, in the present embodiment, the heating temperature of the tinplate 60 within the treatment range of the excimer lamp device 10 is set to below 60°C.

[0026] Furthermore, in order to avoid the influence of the electromagnetic heating coil 41 on the molecular lamp equipment 10 and the plasma device 20, the electromagnetic heating coil 41 is arranged below the conveyor belt 30 and is far away from the upper belt surface of the conveyor belt 30; accordingly, in order to compensate for the defects that the electromagnetic heating coil 41 is far away from the tinplate 60 and the heating effect is poor, a heating device 42 is also arranged above the conveyor belt 30. In this embodiment, the heating device 42 is an infrared heater, and a plurality of heating devices 42 are arranged at intervals along the moving direction of the conveyor belt 30. The heating device 42 and the electromagnetic heating coil 41 work together to heat the tinplate 60.

[0027] Furthermore, in order to avoid the influence of the electromagnetic heating ring 41, the conveyor belt 30 is a non-metallic belt. In this embodiment, the conveyor belt 30 is a rubber belt; further, the conveyor belt 30 transports the tinplate 60 to the bottom of the excimer lamp device 10. In order to reduce the problem of accelerated aging of the conveyor belt 30 caused by ultraviolet radiation, in this embodiment, the conveyor belt 30 is silicone rubber.

[0028] The tinplate 60 treated by the excimer lamp device 10 is moved by the conveyor belt 30 into the plasma device 20. The plasma device 20 bombards the surface of the tinplate 60 to form a large number of active groups, thereby increasing the surface energy of the tinplate 60 to increase the surface adhesion of the tinplate 60, so that the water-based paint and the light-curing paint can stably adhere to the surface of the tinplate 60. Considering that the surface activity of the tinplate 60 treated by the plasma device 20 is relatively high, in order to avoid degradation effects on the surface of the treated tinplate 60, to avoid oxidation of the tinplate 60, and to generate pollutants again, in the present application, a protective cover 50 is provided above the conveyor belt 30. Along the moving direction of the conveyor belt 30, the protective cover 50 extends from the plasma device 20 to the moving end of the conveyor belt 30. An air inlet 45 is provided above the protective cover 50. The air inlet 45 is used to fill the protective cover 50 with an inert gas such as nitrogen, helium, etc.; the tinplate 60 treated by the plasma device 20 directly enters the protective cover 50 to avoid contact between the tinplate 60 and the air. Preferably, the inert gas circulates in the protective cover 50, and the inert gas circulation takes away the residual products on the surface of the tinplate 60 after the plasma device 20 is treated.

[0029] Since the surface of the activated tinplate 60 has a certain time-effect, in order to avoid the reduction of the surface activity of the tinplate 60, in this application, the conveyor belt 30 is connected to the coating link, and the tinplate 60 treated by the excimer lamp device 10 and the plasma device 20 in sequence is directly sent to the coating link through the conveyor belt 30 for coating. Preferably, the heating range of the tinplate 60 by the electromagnetic heating coil 41 should cover from the end of the conveyor belt 30 to the tail of the conveyor belt 30. Along the moving direction of the conveyor belt 30, a plurality of heating devices 42 are arranged at intervals in front of the plasma device 20. The electromagnetic coil and the heating device 42 work together to heat the tinplate 60 so that the tinplate 60 enters the coating link in a hot state. Under high temperature conditions, the capillaries on the surface of the tinplate 60 expand, which helps the tinplate 60 to bond with water-based paint or photocuring paint. In this embodiment, the temperature inside the protective cover 50 is controlled to be 100°C-120°C. Along the moving direction of the conveyor belt 30, a plurality of temperature detection devices 44 are arranged at intervals inside the protective cover 50. Furthermore, the measuring head of the temperature detection device 44 is arranged obliquely close to the surface of the tinplate 60.

[0030] A contact angle measuring instrument 51 is provided at the moving end of the conveyor belt 30. The contact angle measuring instrument 51 is provided in the protective cover 50 to detect the contact angle of the surface of the treated tinplate 60. In this embodiment, if the contact angle after detection is less than 50 degrees, the surface treatment of the tinplate 60 is qualified.

[0031] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the utility model, rather than to limit it. Although the utility model is described in detail with reference to the above embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the above embodiments, or replace some of the technical features therein by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the utility model.

Claims

1. A device for improving the adhesion of tinplate coatings, It is characterized in that The invention comprises an excimer lamp device (10), a plasma device (20) and a conveyor belt (30), wherein tinplate (60) is arranged on the conveyor belt (30), and the conveyor belt (30) transports the tinplate (60) to pass through the excimer lamp device (10) and the plasma device (20) in sequence, an electromagnetic heating coil (41) is arranged below the conveyor belt (30), and a plurality of heating devices (42) and a plurality of temperature detection devices (44) arranged at intervals are arranged on the side of the conveyor belt (30) along the moving direction of the conveyor belt (30).

2. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that The irradiation wavelength of the excimer lamp device (10) is 172 nm, and the irradiation intensity of the excimer lamp device (10) is 100 mw / cm2.

3. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that A plurality of suction ports (43) are arranged below the excimer lamp device (10); the suction ports (43) are arranged beside the conveyor belt (30); and the suction ports (43) are arranged toward the processed surface of the tinplate (60).

4. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that A protective cover (50) is provided on the conveyor belt (30); the protective cover (50) is connected to the plasma device (20) and extends to the moving end of the conveyor belt (30).

5. A device for improving the adhesion of tinplate coating according to claim 4, It is characterized in that The protective cover (50) is filled with an inert gas, and the inert gas flows in the protective cover (50).

6. A device for improving the adhesion of tinplate coating according to claim 4, It is characterized in that The temperature detection device (44) is arranged at the moving head end and the moving end of the conveyor belt (30), and inside the protective cover (50).

7. A device for improving the adhesion of tinplate coating according to claim 4, It is characterized in that A contact angle measuring instrument (51) is provided at the moving end of the conveyor belt (30), and the contact angle measuring instrument (51) is arranged in the protective cover (50).

8. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that The conveyor belt (30) is connected to the coating link.

9. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that The heating device (42) is an infrared heater.

10. A device for improving the adhesion of tinplate coating according to claim 1, It is characterized in that The conveyor belt (30) is a non-metallic belt.