Metal ceramic composite structure

By using a composite structure of ceramic layer and metal layer in the metal cermet composite structure and setting materials with high wear resistance at the connection parts, the problem of ceramic impeller collapse when large-particle materials are impacted is solved, and the resistance of the overall structure is improved Abrasiveness and stability.

CN222080285UActive Publication Date: 2024-11-29HANJIANG HONGYUAN XIANGYANG SILICON CARBIDE SPECIAL CERAMICS
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323335915.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-06
Publication Date
2024-11-29
Estimated Expiration
2033-12-06

AI Technical Summary

Technical Problem

When the existing metal cermet composite structure encounters impact of large-particle materials, the ceramic impeller is prone to large pieces of porcelain collapse, resulting in insufficient wear resistance.

Method used

Using a composite structure of ceramic layer and metal layer, the ceramic layer is connected to the metal layer through the connecting components, and materials with wear resistance better than the ceramic layer are provided at the connection parts, such as silicon carbide ceramic, silicon nitride ceramic and boron carbide ceramic. A concave and convex mating structure is formed to enhance the connection strength, and an wear-resistant layer is provided on the side of the metal layer away from the ceramic layer to provide additional protection.

Benefits of technology

Through the use of connecting components, the ceramic melting area of ​​the ceramic layer is reduced, the corrosion resistance and wear resistance of the ceramic layer are improved, and the strength and toughness of the metal layer are improved, which avoids the fall of the ceramic layer and enhances the stability of the overall structure and Wear resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222080285U_ABST
    Figure CN222080285U_ABST
Patent Text Reader

Abstract

The utility model discloses a metal ceramic composite structure, which comprises a ceramic layer, a metal layer and at least one connecting assembly, the metal layer is connected with the ceramic layer, the connecting assembly comprises a connecting part and a first bonding layer, the connecting part is inserted into the ceramic layer and the metal layer, and the first bonding layer is connected with the connecting part, the ceramic layer and the metal layer. According to the connecting assembly, the composite strength of the ceramic and the metal is improved, the composite structure is more stable and reliable, the ceramic is divided into a plurality of areas through the connecting parts, large ceramic cracking of the ceramic layer is avoided, the ceramic cracking area is reduced, and ceramic cracking of the ceramic layer can be effectively avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of metal-ceramic composites, in particular to a metal-ceramic composite structure. Background Art

[0002] Metals have high strength and toughness, while ceramics have high hardness and wear resistance. When the two are combined, their respective advantages can be fully utilized, making the composite material stronger.

[0003] Announcement No. CN212479680U discloses a structure for conveying fluid, including an all-metal skeleton and a silicon carbide ceramic coating; the all-metal skeleton includes a front cover plate support part, a rear cover plate support part, a blade support part connecting the front cover plate support part and the rear cover plate support part, and a hub support part arranged in the middle of the rear cover plate support part; the inner and outer surfaces of the front cover plate support part, the rear cover plate support part and the blade support part are all coated with a silicon carbide ceramic coating; the inner side of the hub support part is a connecting hole matching the shape of the pump shaft, and the outer side of the hub support part is coated with a silicon carbide ceramic coating; the front cover plate support part, the rear cover plate support part and the blade support part are provided with coating adsorption holes.

[0004] Although silicon carbide ceramics have good hardness, they are relatively brittle. When the above-mentioned impeller is in use, if larger particles of material hit the silicon carbide ceramics, large pieces of ceramic may break off at the edge of the ceramic impeller. Utility Model Content

[0005] In view of this, it is necessary to provide a metal-ceramic composite structure to solve the technical problem of large-scale ceramic chipping on the edge of the ceramic impeller in the prior art.

[0006] In order to achieve the above-mentioned technical objectives, the technical solution of the utility model provides a metal-ceramic composite structure, characterized in that it includes a ceramic layer, a metal layer and at least one connecting component, the metal layer is connected to the ceramic layer, the connecting component includes a connecting part and a first adhesive layer, the connecting part is inserted in the ceramic layer and the metal layer, and the first adhesive layer connects the connecting part, the ceramic layer and the metal layer.

[0007] In one embodiment, the ceramic layer forms a first matching portion, the metal layer forms a second matching portion, and the first matching portion and the second matching portion are matched in a concave-convex structure.

[0008] In one embodiment, the ceramic layer includes a first ceramic layer and a second ceramic layer, and the metal layer is at least partially disposed between the first ceramic layer and the second ceramic layer.

[0009] In one of the embodiments, it further includes a wear-resistant layer, and the wear-resistant layer is arranged on a side of the metal layer away from the ceramic layer.

[0010] In one embodiment, a second adhesive layer is further included, and the second adhesive layer is disposed between the metal layer and the ceramic layer and connects the metal layer and the ceramic layer.

[0011] In one embodiment, the connecting portion is integrally formed with one of the first ceramic layer and the second ceramic layer and plugged into the other one.

[0012] In one embodiment, the wear resistance of the connection portion is better than that of the ceramic layer, and the connection portion is made of one or more of silicon carbide ceramics, silicon nitride ceramics and boron carbide ceramics.

[0013] In one embodiment, any one of the first ceramic layer, the second ceramic layer and the metal layer forms a first clamping structure, and the connecting part forms a second clamping structure. The connecting part can drive the second clamping structure to rotate by rotating, so that the second clamping structure is clamped with the first clamping structure, which is used to limit the movement of the connecting part along the insertion direction.

[0014] In one embodiment, the metal layer is provided with at least one first fixing hole, the first ceramic layer is provided with at least one second fixing hole relative to the first fixing hole, the second ceramic layer is provided with at least one third fixing hole relative to the first fixing hole, and the connecting portion is inserted into the first fixing hole, the second fixing hole and the third fixing hole.

[0015] In one embodiment, the second fixing hole passes through the first ceramic layer.

[0016] In one embodiment, there are multiple connection components, and the multiple connection components are distributed at intervals along the circumference of the metal layer.

[0017] In one embodiment, at least some of the connection components are arranged in a triangle.

[0018] In one embodiment, an end of the connecting portion is flush with outer walls of the first ceramic layer and the second ceramic layer.

[0019] In one embodiment, the second fixing hole is larger than the first fixing hole, one end of the connecting portion is inserted into the first fixing hole, and the other end of the connecting portion is inserted into the second fixing hole, and the outer diameter of the other end of the connecting portion is larger than the outer diameter of one end of the connecting portion.

[0020] Compared with the prior art, the utility model has the following beneficial effects: by setting the ceramic layer, the ceramic layer can provide high hardness and wear resistance, the ceramic layer can provide better corrosion resistance, and can protect the metal layer from wear; by setting the metal layer, the metal layer can provide high strength and toughness;

[0021] By setting a connecting component, the connecting part of the connecting component passes through the metal layer, and the first adhesive layer in the connecting component connects the metal layer, the connecting part, and the ceramic layer, thereby realizing the connection between the connecting part and the metal layer, and realizing the connection between the connecting part and the ceramic layer; the connecting part strengthens the connection strength between the ceramic layer and the metal layer through the first adhesive layer, and the structure is more stable and reliable. When large particles of material hit the ceramic layer, due to the existence of the connecting part, the force of the ceramic layer can be transferred to the metal layer, thereby strengthening the strength of the metal-ceramic structure. Multiple connecting parts divide the ceramic into multiple areas, thereby avoiding large-scale collapse of the ceramic layer and reducing the area of ​​collapsed ceramic. The connecting part can be made of a material that is more wear-resistant than the ceramic layer, thereby increasing the wear resistance of the weak positions of the ceramic layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0023] Figure 2 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0024] Figure 3 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0025] Figure 4 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0026] Figure 5 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0027] Figure 6 It is a structural schematic diagram of a first clamping structure in a metal-ceramic composite structure according to an embodiment of the utility model;

[0028] Figure 7 It is a structural schematic diagram of a connecting portion and a first clamping structure in a metal-ceramic composite structure according to an embodiment of the utility model;

[0029] Figure 8 It is a structural schematic diagram of a metal-ceramic composite structure according to an embodiment of the utility model;

[0030] Fig. 9It is a structural schematic diagram of a ceramic layer, a first matching portion, a metal layer, a second matching portion and a first adhesive layer in a metal-ceramic composite structure according to an embodiment of the utility model;

[0031] Fig.10 It is a structural schematic diagram of a metal-ceramic composite structure described in an embodiment of the utility model.

[0032] Description of reference numerals:

[0033] Ceramic layer 1;

[0034] A first matching portion 1a;

[0035] A first ceramic layer 11;

[0036] A second ceramic layer 12;

[0037] Metal layer 2;

[0038] The second matching portion 2a;

[0039] Connect component 3;

[0040] Connecting portion 31;

[0041] A first adhesive layer 32;

[0042] A third adhesive layer 321;

[0043] a fourth adhesive layer 322;

[0044] Wear-resistant layer 4;

[0045] Second adhesive layer 5;

[0046] Leak-proof layer 6;

[0047] A first clamping structure a;

[0048] The second clamping structure b. DETAILED DESCRIPTION

[0049] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings, wherein the accompanying drawings constitute a part of the present application and are used together with the embodiments of the present invention to illustrate the principles of the present invention, but are not used to limit the scope of the present invention.

[0050] Embodiment 1

[0051] like Figure 1 and Fig. 9As shown, the utility model provides a metal-ceramic composite structure, including a ceramic layer 1, a metal layer 2 and at least one connecting component 3, the connecting component 3 includes a connecting portion 31 and a first adhesive layer 32, the connecting portion 31 is inserted between the ceramic layer 1 and the metal layer 2, and the first adhesive layer 32 connects the connecting portion 31, the metal layer 2 and the ceramic layer 1. It should be understood that the ceramic layer 1, the metal layer 2 and the connecting portion 31 can all be produced by 3D printing.

[0052] By providing the ceramic layer 1, the ceramic layer 1 can provide high hardness and wear resistance, and the ceramic layer 1 can provide better corrosion resistance and protect the metal layer 2 from wear; by providing the metal layer 2, the metal layer 2 can provide high strength and toughness;

[0053] By setting the connection component 3, the connection part 31 of the connection component 3 penetrates the metal layer 2, and the first adhesive layer 32 in the connection component 3 connects the metal layer 2, the connection part 31 and the ceramic layer 1, so as to realize the connection between the connection part 31 and the metal layer 2, and realize the connection between the connection part 31 and the ceramic layer 1; the connection part 31 strengthens the connection strength with the ceramic layer 1 through the first adhesive layer 32, and when large particles of material hit the ceramic layer 1, due to the existence of the connection part 31, it can avoid large pieces of ceramic layer 1 from breaking, and reduce the area of ​​ceramic breaking. Moreover, compared with the prior art, the wear-resistant blocks are embedded in the ceramic by bonding, so that the wear-resistant blocks are distributed in an array. The wear-resistant blocks fixed in this way are easy to fall off, and in the present application, the ceramic layer 1 and the metal layer 2 are connected as a whole through the connection component 3, which greatly enhances the connection strength between the ceramic layer 1 and the metal layer 2, and avoids the ceramic layer 1 from falling off relative to the metal layer 2.

[0054] In one embodiment, the ceramic layer 1 is formed with a first matching portion 1a, and the metal layer 2 is formed with a second matching portion 2a, and the first matching portion 1a and the second matching portion 2a are matched in a concave-convex structure. It should be understood that the first matching portion 1a can be a groove, and the second matching portion 2a is a protrusion that matches the groove of the first matching portion 1a, or the second matching portion 2a is a groove, and the first matching portion 1a is a protrusion that matches the groove of the second matching portion 2a.

[0055] Through the coordination of the concave-convex structure, the ceramic layer 1 can be prevented from moving relative to the metal layer 2 , and the connection strength between the ceramic layer 1 and the metal layer 2 can be enhanced.

[0056] In one embodiment, the ceramic layer 1 includes a first ceramic layer 11 and a second ceramic layer 12, and the metal layer 2 is at least partially disposed between the first ceramic layer 11 and the second ceramic layer 12. It should be understood that the ceramic layer 1 can also be a single layered structure disposed on one side of the metal layer 2; it should be understood that the first ceramic layer 11 and the second ceramic layer 12 can be integrally formed, or can be separately formed and then bonded by an adhesive.

[0057] By arranging the metal layer 2 between the first ceramic layer 11 and the second ceramic layer 12 , the first ceramic layer 11 and the second ceramic layer 12 can protect both ends of the metal layer 2 , thereby preventing materials from directly contacting and wearing the metal layer 2 .

[0058] In one embodiment, the metal-ceramic composite structure further includes a wear-resistant layer 4, which is disposed on a side of the metal layer 2 away from the ceramic layer 1. It should be understood that the wear-resistant layer 4 can be a wear-resistant branch, a wear-resistant coating, a wear-resistant metal, and the like.

[0059] For application scenarios where the side of the metal layer 2 away from the ceramic layer 1 has relatively less wear, the wear-resistant layer 4 is provided to protect the metal layer 2 .

[0060] In one embodiment, the metal-ceramic composite structure further includes a second bonding layer 5, which is disposed between the metal layer 2 and the ceramic layer 1 and connects the metal layer 2 and the ceramic layer 1. It should be understood that the second bonding layer 5 is disposed between the first ceramic layer 11 and the metal layer 2 and / or between the second ceramic layer 12 and the metal layer 2.

[0061] By providing the second adhesive layer 5 , which is used to bond the metal layer 2 and the ceramic layer 1 , a stable connection between the metal layer 2 and the ceramic layer 1 can be achieved.

[0062] It should be understood that the connection portion 31 may be inserted in the first ceramic layer 11 and the metal layer 2 , may be inserted in the second ceramic layer 12 and the metal layer 2 , or may be inserted in the first ceramic layer 11 , the metal layer 2 and the second ceramic layer 12 .

[0063] In one embodiment, the connection portion 31 is integrally formed with one of the first ceramic layer 11 and the second ceramic layer 12 and plugged into the other one.

[0064] Through the above-mentioned arrangement, the one-piece molding method can strengthen the connection strength between the connecting part 31 and the ceramic layer, and the connecting part 31 can also play a role of positioning and guiding, which is convenient for the first ceramic layer 11 to be combined with the second ceramic layer 12. Moreover, after the connecting part 31 is integrally molded with any one of the first ceramic layer 11 and the second ceramic layer 12, the one-time connection between the connecting part 31 and the first ceramic layer 11 and the second ceramic layer 12 is reduced, thereby reducing the number of connections.

[0065] In one embodiment, the wear resistance of the connection portion 31 is better than that of the ceramic layer 1 , and the connection portion 31 is made of one or more of silicon carbide ceramics, silicon nitride ceramics and boron carbide ceramics.

[0066] Through the above arrangement, the connection portion 31 is more wear-resistant than the ceramic layer 1 , and the structural strength of the weak position of the ceramic layer 1 can be enhanced.

[0067] In one of the embodiments, any one of the first ceramic layer 11, the second ceramic layer 12 and the metal layer 2 forms a first clamping structure a, and the connecting part 31 forms a second clamping structure b. The connecting part 31 can drive the second clamping structure b to rotate by rotating, so that the second clamping structure b is clamped with the first clamping structure a, which is used to limit the movement of the connecting part 31 along the insertion direction.

[0068] By providing the first clamping structure a and the second clamping structure b, the second clamping structure b can restrict the connection portion 31 from moving along the insertion direction when clamped with the first clamping structure a.

[0069] In one embodiment, the metal layer 2 is provided with at least one first fixing hole, the first ceramic layer 11 is provided with at least one second fixing hole relative to the first fixing hole, the second ceramic layer 12 is provided with at least one third fixing hole relative to the first fixing hole, and the connecting portion 31 is inserted into the first fixing hole, the second fixing hole and the third fixing hole. It should be understood that the second fixing hole and the third fixing hole can be through holes or blind holes; it should be understood that the first fixing hole, the second fixing hole and the third fixing hole can be formed when the component is formed or formed by subsequent processing.

[0070] By providing the first fixing hole, the second fixing hole and the third fixing hole, the connecting portion 31 can pass through the metal layer 2 through the first fixing hole, can be inserted into the first ceramic layer 11 through the second fixing hole, and can be inserted into the second ceramic layer 12 through the third fixing hole.

[0071] In one embodiment, the first clamping structure a is a clamping slot opened in the first ceramic layer 11, the second ceramic layer 12 and the metal layer 2, and the clamping slot is connected to any one of the first fixing hole, the second fixing hole and the third fixing hole. The second clamping structure b is a spring pin fixed to the connecting part 31 and arranged along the radial direction of the connecting part 31. The spring pin cooperates with the clamping slot to limit the movement of the connecting part 31 along the insertion direction.

[0072] In one embodiment, the first clamping structure a is an annular groove opened in the first ceramic layer 11, the second ceramic layer 12 and the metal layer 2, and the annular groove is connected to any one of the first fixing hole, the second fixing hole and the third fixing hole. The second clamping structure b is a block protruding from the connecting part 31. When the connecting part 31 is inserted into the first fixing hole, the second fixing hole, the third fixing hole and the annular groove, the connecting part 31 is rotated so that the connecting part 31 is clamped in the annular groove, thereby limiting the movement of the connecting part 31 along the insertion direction.

[0073] In one embodiment, the third fixing hole passes through the second ceramic layer 12, and the metal-ceramic composite structure further includes a leakproof layer 6, which is detachably connected to a side of the second ceramic layer 12 away from the metal layer 2, and the leakproof layer 6 blocks the third fixing hole.

[0074] By penetrating the third fixing hole through the second ceramic layer 12, the connecting part 31 can penetrate into the second ceramic layer 12 through the penetrated third fixing hole, and be inserted into the metal layer 2 and the first ceramic layer 11, so that the first adhesive layer 32 can be injected into the third fixing hole, the first fixing hole and the second fixing hole through the penetrated third fixing hole; by setting the leak-proof layer 6, when the first adhesive layer 32 is injected into the third fixing hole, the first fixing hole and the second fixing hole, since the first adhesive layer 32 has a certain fluidity, in order to prevent the first adhesive layer 32 from flowing out through the penetrated third fixing hole, in this embodiment, a leak-proof layer 6 is set, and the leak-proof layer 6 can block the third fixing hole to prevent the first adhesive layer 32 from flowing out of the third fixing hole.

[0075] In one embodiment, the second fixing hole passes through the first ceramic layer 11 .

[0076] By penetrating the second fixing hole through the first ceramic layer 11, the connecting part 31 can penetrate into the first ceramic layer 11 through the penetrating third fixing hole and be inserted into the metal layer 2 and the second ceramic layer 12, so that the first adhesive layer 32 can be injected into the second fixing hole, the first fixing hole and the third fixing hole through the penetrating second fixing hole.

[0077] In one embodiment, there are multiple connection components 3 , and the multiple connection components 3 are distributed at intervals along the circumference of the metal layer 2 .

[0078] By setting up multiple connecting components 3, the multiple connecting components 3 can strengthen the structural strength of multiple parts of the first ceramic layer 11 and the second ceramic layer 12, and can strengthen the structural strength of the first ceramic layer 11 and the second ceramic layer 12 from multiple areas to avoid large-area ceramic collapse of the first ceramic layer 11 and the second ceramic layer 12.

[0079] In one embodiment, at least part of the connecting components 3 are arranged in a triangle.

[0080] The connecting components 3 arranged in a triangle can bear forces from multiple angles, thereby increasing the stability of the structure and the impact resistance of the structure.

[0081] In one embodiment, an end of the connecting portion 31 is flush with the outer walls of the first ceramic layer 11 and the second ceramic layer 12 .

[0082] By making the end of the connecting part 31 flush with the outer walls of the first ceramic layer 11 and the second ceramic layer 12, it is possible to prevent the connecting part 31 from protruding from the first ceramic layer 11 and the second ceramic layer 12. Avoiding the protrusion of the connecting part 31 increases the flow damping of the liquid, so that the liquid can pass through the first ceramic layer 11 and the second ceramic layer 12 more smoothly.

[0083] In one embodiment, the first adhesive layer 32 includes two third adhesive layers 321 located at two ends of the connecting portion 31 and a fourth adhesive layer 322 located between the two third adhesive layers 321 ;

[0084] The third adhesive layer 321 includes the following components in parts by mass:

[0085] 60-80 parts of silicon carbide powder with a mesh size of 200 or above;

[0086] 60-80 parts of vinyl ester resin;

[0087] Accelerator 0.1-0.5 parts;

[0088] Curing agent 0.5-1 part;

[0089] Defoaming agent 0.2-0.5 parts;

[0090] 1-2 parts of leveling agent;

[0091] 1-2 parts of coupling agent;

[0092] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0093] The fourth adhesive layer 322 includes the following components in parts by mass:

[0094] 30-40 parts of silicon carbide powder above 80 mesh;

[0095] 60-80 parts of vinyl ester resin;

[0096] Accelerator 0.1-0.5 parts;

[0097] Curing agent 0.5-1 part;

[0098] Defoaming agent 0.2-0.5 parts;

[0099] 1-2 parts of leveling agent;

[0100] 1-2 parts of coupling agent;

[0101] Among them, the ratio of silicon carbide powder to vinyl ester resin is 1:2. It should be understood that the accelerator can be cobalt naphthenate, cobalt isooctanoate, etc., the curing agent can be methyl ethyl ketone peroxide, benzoyl peroxide, tert-butyl perbenzoate, cumene hydroperoxide, etc.; the defoamer can be polyoxyethylene polyoxypropylene pentaerythritol ether, polyamide and polyether amine, etc., the leveling agent can also be acrylic resin, polyvinyl alcohol and polyester resin, etc.; the coupling agent can be KH570, KBM-555 and A-187, etc.

[0102] By setting two third bonding layers 321 and a fourth bonding layer 322, the third bonding layer 321 is located at both ends of the connecting part 31, and is located in the gap between the connecting part 31 and the first ceramic layer 11 and in the gap between the connecting part 31 and the second ceramic layer 12. Since the granular material may flow through the outer walls of the first ceramic layer 11 and the second ceramic layer 12, the gap between the connecting part 31 and the first ceramic layer 11 and the gap between the connecting part 31 and the second ceramic layer 12 need to have higher wear resistance requirements. For this reason, in the present embodiment, two third bonding layers 321 are set, and the proportion of silicon carbide powder in the two third bonding layers 321 is relatively high, and silicon carbide powder has high wear resistance, and reduces the amount of resin used, thereby preventing the granular material from wearing the resin and entering the ceramic layer 1 through the gap after wear. The silicon carbide powder has a small particle size and can enter In the gap between the connecting part 31 and the first ceramic layer 11 and the second ceramic layer 12, the particle size of the silicon carbide powder is small, the hydration reaction is fast and complete, the early strength and the later strength are relatively high, and it has relatively high activity; and the fourth bonding layer 322 located between the two third bonding layers 321, the fourth bonding layer 322 will not contact the granular material, therefore, the fourth bonding layer 322 does not have high requirements for wear resistance, for this reason, the proportion of resin in the fourth bonding layer 322 is increased, the resin can provide excellent bonding properties, can effectively and firmly bond the metal layer 2, the first ceramic layer 11, the second ceramic layer 12 and the connecting part 31 together to form a high-strength bond, and the vinyl ester resin has good durability, can maintain the bonding strength during long-term use, and avoid the relative movement of the metal layer 2, the first ceramic layer 11, the second ceramic layer 12 and the connecting part 31.

[0103] In one embodiment, the silicon carbide powder in the third bonding layer 321 is a graded silicon carbide powder, which includes the following particle sizes in parts by weight:

[0104] 20-25 parts of silicon carbide powder with a particle size of 80 mesh;

[0105] 30-35 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0106] 40-45 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0107] In this embodiment, the particle size of the silicon carbide powder is 80 mesh, which can smoothly enter the gap between the connecting portion 31 and the ceramic layer 1 and can fill the gap well. In addition, the silicon carbide powder of 80 mesh has high activity, fast and complete hydration reaction, and high early strength and late strength.

[0108] By setting 80 mesh silicon carbide powder, the particle size of silicon carbide in this particle size range is relatively large and can act as aggregate. The gaps between the 80 mesh silicon carbide powders are filled in stages by silicon carbide powder with a particle size of 50-80 mesh and silicon carbide powder with a particle size of 20-50 mesh, so that more silicon carbide powder is filled in the gaps, thereby enhancing the wear resistance of the third bonding layer 321.

[0109] like Fig.10 As shown, in one embodiment, the second fixing hole is larger than the first fixing hole, one end of the connecting portion 31 is inserted in the first fixing hole, and the other end of the connecting portion 31 is inserted in the second fixing hole and the third fixing hole, and the outer diameter of the other end of the connecting portion 31 is larger than the outer diameter of one end of the connecting portion 31.

[0110] Through the above-mentioned arrangement, the connecting portion 31 is stepped. When the connecting portion 31 connects the metal layer 2 and the first ceramic layer 11, the end of the connecting portion 31 with a relatively larger diameter can cover the first fixing hole. Moreover, when the connecting portion 31 is set as a reinforced ceramic block, the connecting portion 31 can not only play a connecting role, but also strengthen the local performance of the first ceramic layer 11. The reinforced ceramic block can be a ceramic material with better wear resistance, impact resistance and corrosion resistance. Moreover, since the connecting portion 31 is embedded in the first fixing hole and is also inserted in the second fixing hole and the third fixing hole, the connection strength between the connecting portion 31 and the metal layer 2, the first ceramic layer 11 and the second ceramic layer 12 can be strengthened, so that the connecting portion 31 is not easy to fall off from the first ceramic layer 11.

[0111] Embodiment 2

[0112] The similarities between the second embodiment and the first embodiment are not discussed here. The differences between the second embodiment and the first embodiment are as follows:

[0113] In this embodiment, the third adhesive layer 321 includes the following components in parts by mass:

[0114] 60 parts of silicon carbide powder with a mesh size of 200 or above;

[0115] 60 parts of vinyl ester resin;

[0116] 0.5 part of accelerator;

[0117] 0.5 parts of curing agent;

[0118] 0.2 parts of defoaming agent;

[0119] 1 part of leveling agent;

[0120] 2 parts of coupling agent;

[0121] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0122] The fourth adhesive layer 322 includes the following components in parts by mass:

[0123] 30 parts of silicon carbide powder with mesh size of 80 or above;

[0124] 60 parts of vinyl ester resin;

[0125] 0.5 part of accelerator;

[0126] 0.5 parts of curing agent;

[0127] 0.2 parts of defoaming agent;

[0128] 1 part of leveling agent;

[0129] 2 parts of coupling agent;

[0130] The ratio of silicon carbide powder to vinyl ester resin is 1:2.

[0131] The silicon carbide powder in the third bonding layer 321 is graded silicon carbide powder, and includes the following particle sizes by weight:

[0132] 25 parts of silicon carbide powder with a particle size of 80 mesh;

[0133] 30 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0134] 45 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0135] Embodiment 3

[0136] The similarities between the third embodiment and the first embodiment are not discussed here. The differences between the third embodiment and the first embodiment are as follows:

[0137] In this embodiment, the third adhesive layer 321 includes the following components in parts by mass:

[0138] 80 parts of silicon carbide powder with a mesh size of 200 or above;

[0139] 80 parts of vinyl ester resin;

[0140] Accelerator 0.1 part;

[0141] 1 part of curing agent;

[0142] 0.5 parts of defoaming agent;

[0143] 2 parts of leveling agent;

[0144] 1 part of coupling agent;

[0145] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0146] The fourth adhesive layer 322 includes the following components in parts by mass:

[0147] 30-40 parts of silicon carbide powder above 80 mesh;

[0148] 60-80 parts of vinyl ester resin;

[0149] Accelerator 0.1 part;

[0150] 1 part of curing agent;

[0151] 0.5 parts of defoaming agent;

[0152] 2 parts of leveling agent;

[0153] 1 part of coupling agent;

[0154] The ratio of silicon carbide powder to vinyl ester resin is 1:2.

[0155] The silicon carbide powder in the third bonding layer 321 is graded silicon carbide powder, and includes the following particle sizes by weight:

[0156] 20 parts of silicon carbide powder with a particle size of 80 mesh;

[0157] 35 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0158] 40 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0159] Embodiment 4

[0160] The similarities between the fourth embodiment and the first embodiment are not discussed here. The differences between the fourth embodiment and the first embodiment are as follows:

[0161] In this embodiment, the third adhesive layer 321 includes the following components in parts by mass:

[0162] 70 parts of silicon carbide powder with a mesh size of 200 or above;

[0163] 70 parts of vinyl ester resin;

[0164] 0.3 parts of accelerator;

[0165] 0.75 parts of curing agent;

[0166] 0.35 parts of defoaming agent;

[0167] 1.5 parts of leveling agent;

[0168] 1.5 parts of coupling agent;

[0169] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0170] The fourth adhesive layer 322 includes the following components in parts by mass:

[0171] 35 parts of silicon carbide powder with mesh size of 80 or above;

[0172] 70 parts of vinyl ester resin;

[0173] 0.3 parts of accelerator;

[0174] 0.75 parts of curing agent;

[0175] 0.35 parts of defoaming agent;

[0176] 1.5 parts of leveling agent;

[0177] 1.5 parts of coupling agent;

[0178] The ratio of silicon carbide powder to vinyl ester resin is 1:2.

[0179] The silicon carbide powder in the third bonding layer 321 is graded silicon carbide powder, and includes the following particle sizes by weight:

[0180] 22.5 parts of silicon carbide powder with a particle size of 80 mesh;

[0181] 32.5 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0182] 42.5 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0183] Embodiment 5

[0184] The similarities between the fifth embodiment and the first embodiment are not discussed here. The differences between the fifth embodiment and the first embodiment are as follows:

[0185] In this embodiment, the third adhesive layer 321 includes the following components in parts by mass:

[0186] 70 parts of silicon carbide powder with a mesh size of 200 or above;

[0187] 70 parts of vinyl ester resin;

[0188] 0.5 part of accelerator;

[0189] 0.5 parts of curing agent;

[0190] 0.2 parts of defoaming agent;

[0191] 1 part of leveling agent;

[0192] 2 parts of coupling agent;

[0193] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0194] The fourth adhesive layer 322 includes the following components in parts by mass:

[0195] 35 parts of silicon carbide powder with mesh size of 80 or above;

[0196] 70 parts of vinyl ester resin;

[0197] 0.5 part of accelerator;

[0198] 0.5 parts of curing agent;

[0199] 0.2 parts of defoaming agent;

[0200] 1 part of leveling agent;

[0201] 2 parts of coupling agent;

[0202] The ratio of silicon carbide powder to vinyl ester resin is 1:2.

[0203] The silicon carbide powder in the third bonding layer 321 is graded silicon carbide powder, and includes the following particle sizes by weight:

[0204] 25 parts of silicon carbide powder with a particle size of 80 mesh;

[0205] 30 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0206] 45 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0207] Embodiment 6

[0208] The similarities between the sixth embodiment and the first embodiment are not discussed here. The differences between the sixth embodiment and the first embodiment are as follows:

[0209] In this embodiment, the third adhesive layer 321 includes the following components in parts by mass:

[0210] 70 parts of silicon carbide powder with a mesh size of 200 or above;

[0211] 70 parts of vinyl ester resin;

[0212] Accelerator 0.1 part;

[0213] 1 part of curing agent;

[0214] 0.5 parts of defoaming agent;

[0215] 2 parts of leveling agent;

[0216] 1 part of coupling agent;

[0217] Wherein, the ratio of silicon carbide powder to vinyl ester resin is 1:1;

[0218] The fourth adhesive layer 322 includes the following components in parts by mass:

[0219] 35 parts of silicon carbide powder with mesh size of 80 or above;

[0220] 70 parts of vinyl ester resin;

[0221] Accelerator 0.1 part;

[0222] 1 part of curing agent;

[0223] 0.5 parts of defoaming agent;

[0224] 2 parts of leveling agent;

[0225] 1 part of coupling agent;

[0226] The ratio of silicon carbide powder to vinyl ester resin is 1:2.

[0227] The silicon carbide powder in the third bonding layer 321 is graded silicon carbide powder, and includes the following particle sizes by weight:

[0228] 20 parts of silicon carbide powder with a particle size of 80 mesh;

[0229] 35 parts of silicon carbide powder with a particle size of 50-80 mesh;

[0230] 40 parts of silicon carbide powder with a particle size of 20-50 mesh.

[0231] Comparative Example 1

[0232] Except for not containing the accelerator, the other slurry proportions are the same as those in Example 5.

[0233] Comparative Example 2

[0234] Except for not containing curing agent, the rest of the slurry ratio is the same as that of Example 5.

[0235] Comparative Example 3

[0236] Except for not containing the leveling agent, the other slurry proportions are the same as those in Example 5.

[0237] Comparative Example 4

[0238] Except for not containing coupling agent, the other slurry proportions are the same as those in Example 5.

[0239] The corrosion and wear performance of the third bonding layer 321 is tested by a corrosion and wear machine. The corrosion and wear machine uses quartz sand as abrasive, and uses a dilute sulfuric acid solution to adjust the pH value of the corrosion solution to 3. The test speed is 50r / min, the load is 6N, and the abrasion and wear rate = average weight loss of the abrasion and wear specimen / abrasion and wear test time; when testing the separation force, the ceramic layer and the metal layer are first clamped and fixed, and then the hydraulic pushing device is used to push the connecting part to move relative to the ceramic layer. When the connecting part moves relative to the ceramic layer or the metal layer, the pushing force applied to the connecting part by the hydraulic pushing device is recorded. The pushing force is the separation force between the connecting part and the ceramic layer or the metal layer.

[0240] The test data is shown in Table 1 below:

[0241]

[0242] It can be seen from Table 1 that in the metal-ceramic composite structure provided by the utility model, the abrasive wear rate and the separation force can meet the working conditions required by the metal-ceramic composite structure. Compared with other adhesives, the corrosion wear rate is low, and the third adhesive layer 321 and the fourth adhesive layer 322 can effectively achieve the bonding between the connecting part 31 and the ceramic layer 1 and the metal layer 2, thereby avoiding separation of the connecting part 31 from the ceramic layer 1 and the metal layer 2.

[0243] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by any technician familiar with the technical field within the technical scope disclosed in the present invention should be included in the protection scope of the present invention.

Claims

1. A metal-ceramic composite structure, characterized in that: It includes a ceramic layer, a metal layer and at least one connecting component, the metal layer is connected to the ceramic layer, the connecting component includes a connecting part and a first adhesive layer, the connecting part is inserted in the ceramic layer and the metal layer, and the first adhesive layer connects the connecting part, the ceramic layer and the metal layer.

2. The metal-ceramic composite structure according to claim 1, characterized in that: The ceramic layer forms a first matching portion, the metal layer forms a second matching portion, and the first matching portion and the second matching portion match in a concave-convex structure.

3. The metal-ceramic composite structure according to claim 1, characterized in that: The ceramic layer includes a first ceramic layer and a second ceramic layer, and the metal layer is at least partially disposed between the first ceramic layer and the second ceramic layer.

4. The metal-ceramic composite structure according to claim 1, characterized in that: It also includes a wear-resistant layer, which is arranged on a side of the metal layer away from the ceramic layer.

5. The metal-ceramic composite structure according to claim 1, characterized in that: The invention also includes a second adhesive layer, which is arranged between the metal layer and the ceramic layer and connects the metal layer and the ceramic layer.

6. The metal-ceramic composite structure according to claim 3, characterized in that: The connecting portion is integrally formed with one of the first ceramic layer and the second ceramic layer and plugged with the other one thereof.

7. The metal-ceramic composite structure according to claim 1, characterized in that: The wear resistance of the connecting portion is better than that of the ceramic layer, and the connecting portion is made of one or more of silicon carbide ceramics, silicon nitride ceramics and boron carbide ceramics.

8. The metal-ceramic composite structure according to claim 3, characterized in that: Any one of the first ceramic layer, the second ceramic layer and the metal layer forms a first clamping structure, and the connecting part forms a second clamping structure. The connecting part can drive the second clamping structure to rotate by rotating, so that the second clamping structure is clamped with the first clamping structure, which is used to limit the movement of the connecting part along the insertion direction.

9. The metal-ceramic composite structure according to claim 3, characterized in that: The metal layer is provided with at least one first fixing hole, the first ceramic layer is provided with at least one second fixing hole relative to the first fixing hole, the second ceramic layer is provided with at least one third fixing hole relative to the first fixing hole, and the connecting portion is inserted into the first fixing hole, the second fixing hole and the third fixing hole.

10. The metal-ceramic composite structure according to claim 9, characterized in that: The third fixing hole penetrates the second ceramic layer. The metal-ceramic composite structure further includes a leakproof layer. The leakproof layer is detachably connected to a side of the second ceramic layer away from the metal layer. The leakproof layer blocks the third fixing hole.

11. The metal-ceramic composite structure according to claim 9, characterized in that: The second fixing hole penetrates the first ceramic layer.

12. The metal-ceramic composite structure according to claim 1, characterized in that: There are multiple connection components, and the multiple connection components are distributed at intervals along the circumference of the metal layer.

13. The metal-ceramic composite structure according to claim 12, characterized in that: At least some of the connection components are arranged in a triangle.

14. The metal-ceramic composite structure according to claim 3, characterized in that: An end of the connection portion is flush with outer walls of the first ceramic layer and the second ceramic layer.

15. The metal-ceramic composite structure according to claim 9, characterized in that: The second fixing hole is larger than the first fixing hole, one end of the connecting portion is inserted in the first fixing hole, the other end of the connecting portion is inserted in the second fixing hole, and the outer diameter of the other end of the connecting portion is larger than the outer diameter of one end of the connecting portion.

Citation Information

Cited By

  • Metal ceramic composite structure and preparation method thereof

    CN117484973A