Gas gun flash evaporation device based on powder surface quenching control

By using a filter in the gas cannon flash device to destroy the gaseous protective layer and introduce the buckling failure fracture mechanism of the diaphragm, combined with liquid nitrogen cooling and electromagnetic coil heating, the preservation of lithium iron phosphate powder forming metastable phase under high temperature and high pressure is solved. The problem is that efficient quenching of materials and improved durability of the device are achieved.

CN222111738UActive Publication Date: 2024-12-06SOUTHWEAT UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322778769.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-17
Publication Date
2024-12-06
Estimated Expiration
2033-10-17

AI Technical Summary

Technical Problem

The existing lithium iron phosphate powders are damaged due to local stress during charging and discharging, and the metastable phase formed under high temperature and high pressure conditions is difficult to preserve. The traditional device design has unreasonable diaphragm crushing and gaseous protective layer hinders heat transfer. question.

Method used

A gas cannon flash evaporation device based on powder surface quenching control was designed, and a buckling failure rupture mechanism is used to destroy the gaseous protective layer and introduce the diaphragm. The metastable phase is quickly formed through low-temperature filter and liquid nitrogen cooling, and the Electromagnetic coil heating increases the phase transition temperature of the material under high pressure.

Benefits of technology

It significantly improves the supercooling degree of the powder material, ensures that the metastable phase can be effectively preserved under normal conditions, extends the service life of the device, and achieves the efficient quenching effect of the material by controlling the diaphragm crushing time point and optimizing the filter structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222111738U_ABST
    Figure CN222111738U_ABST
Patent Text Reader

Abstract

The utility model belongs to the field of dynamic high-pressure impact experiments, and particularly relates to a gas gun flash evaporation device based on powder surface quenching control. Comprising a light-gas gun, bullets, a flash tube, a material collecting bin, a liquid nitrogen storage device, a low-pressure chamber and a vacuum pump. According to the utility model, through high-speed loading of the projectile on a sample, the temperature of a powder material is rapidly raised by utilizing the adiabatic compression effect of shock waves; then, the gas applies limit loads capable of enabling the diaphragm to generate buckling failure at the two ends of the diaphragm, so that the diaphragm is rapidly broken along a preset path, and the powder material is rapidly released to enter the quenching outside; in the flying process of the high-temperature powder material, a gas protection layer generated by surface quenching prevents the material from conducting energy transfer with the environment, by arranging fiber net lines and damaging a steam layer wrapping the powder material, the powder surface and liquid nitrogen are made to make full contact for heat transfer, and therefore the powder surface obtains the enough supercooling degree within a short time; and the metastable phase state shell of the powder material can be more easily kept in a normal state.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the field of dynamic high-pressure impact experiments, and in particular relates to a gas gun flash evaporation device based on powder surface quenching control. Background Art

[0002] Under some extreme conditions, alloy materials may form a new phase rarely seen in the equilibrium phase diagram, namely the metastable phase, in the microstructure. This metastable phase has a different substructure from the stable phase. The metastable phase usually has some properties that are not common in the stable phase, especially the metastable phase formed under high temperature and high pressure, which is difficult to maintain stably under normal conditions. From a thermodynamic point of view, the metastable phase is an intermediate form in the solid-solid phase transition. Under extreme conditions, there is a competitive growth process between the metastable phase and the stable phase during the multiphase transition. Over time, the metastable phase will transform into a stable phase with lower energy. However, giving the metastable phase a higher supercooling when it is formed can reduce the system energy, making it difficult for the atoms of the metastable phase material to cross the energy barrier, thereby allowing the metastable phase material to be retained under normal conditions. Therefore, high supercooling is a key factor in obtaining metastable materials.

[0003] Lithium iron phosphate has been widely used in the field of battery energy due to its excellent performance. However, due to the repeated deintercalation of lithium iron phosphate particles during the charging and discharging process, local stress will cause structural damage, thus affecting the safety performance of the battery. Therefore, improving the strength of lithium iron phosphate particles is a potential way to effectively delay particle damage. Zhu Luhang proposed in the article "Research on shock flash evaporation technology for lithium iron phosphate powder" that the surface of lithium iron phosphate powder particles can be transformed by high-temperature flash evaporation, so that a metastable phase is generated on the surface of the powder to achieve a self-coating effect, thereby enhancing the strength of lithium iron phosphate particles. In this article, high-energy gas is used to impact the material at high speed. Under the adiabatic compression of the shock wave, the temperature and pressure of the sample increase sharply in a very short time, prompting the material to quickly overcome the energy barrier and reach a metastable phase. Before the material undergoes a stable phase transition, the diaphragm is compressed and ruptured, and the material quickly leaves the high-temperature and high-pressure environment. It should be noted that the device in the article has design defects: after breaking the diaphragm, high-pressure and high-temperature gas entrains the powder material into the material collection device. Due to the Leidenfrost phenomenon, there is a high-temperature gaseous protective layer on the surface of the powder material. This gas layer has insulating and heat-insulating characteristics, which will hinder the heat energy transfer between the powder material and the environment, resulting in a slow drop in the temperature of the powder material, making it difficult to obtain a high degree of supercooling, and unable to effectively preserve the metastable phase of the powder material. In addition, the design of diaphragm breaking is unreasonable. The projectile must contact and puncture the diaphragm before it can break the diaphragm. At this time, the projectile still has a large kinetic energy and will hit the target mouth loaded with the diaphragm. The contact surface between the projectile and the target mouth will form an explosive welding effect, making it difficult to separate the projectile and the nozzle, causing the device to be damaged and unable to continue the experiment, and ultimately leading to the failure of obtaining the metastable phase material. Utility Model Content

[0004] In view of this, the utility model innovatively proposes to add a filter screen to the collection device. When the powder after high pressure loading passes through the low temperature filter screen, the powder contacts the serrations on the mesh line, and the serrations will pierce the gaseous protective layer wrapped around the outer layer of the powder material, so that the powder contacts the cold air environment, and the heat transfer channel between the powder and the environment is unobstructed. The powder surface can obtain an ultra-high degree of supercooling, so that the metastable phase can be effectively maintained under normal conditions; at the same time, the buckling failure rupture mechanism of the diaphragm is introduced, and radial pressure is applied to the diaphragm, which greatly reduces the axial crushing stress threshold of the diaphragm. The diaphragm can quickly collapse in stability after reaching the stress threshold on its surface. At the moment of collapse, there is a compressed gas layer between the projectile and the diaphragm, which prevents the projectile from impacting and welding the diaphragm together. The device can be used repeatedly and its durability is improved. Through the above design, a real quenching effect can be produced on the powder surface, and the high-pressure metastable phase of the powder material can be effectively maintained.

[0005] The utility model adopts the following technical solutions:

[0006] A gas gun flash evaporation device based on powder surface quenching control is characterized by comprising a light gas gun, a projectile, a flash evaporation tube, a material collection bin, a liquid nitrogen storage device, a low-pressure chamber, and a vacuum pump.

[0007] Preferably, a vortex groove is formed on the surface of the projectile facing the muzzle, the groove is spiral in direction, the vortex head is wide and deep, and the groove is shallow and narrow and extends forward.

[0008] Preferably, the inner diameter of the flash tube, the inner diameter of the light gas gun nozzle and the outer diameter of the projectile are the same, the projectile can smoothly enter the flash tube body from the light gas gun nozzle and has good air tightness, the gases on the front and rear sides of the projectile will not communicate with each other, and the powder material is placed in the front pipeline. The projectile compresses the front gas to quickly increase the internal energy of the gas, and the thermal motion of the powder material in the gas is intensified, which can quickly reach a metastable phase.

[0009] Preferably, the rear end of the flash tube has a spiral diaphragm clamping structure, which is composed of a chassis, an airway, a spiral Bourdon tube, and a sealing cover; the spiral Bourdon tube is formed by overlapping multiple circles, and is provided with a channel for injecting gas inside, while the tail is sealed; when the gas pressure in the flash tube rises, the internal pressure of the spiral Bourdon tube increases, and the inner diameter of the spiral gradually decreases, expanding and pressurizing the side of the diaphragm, and when the pressure on the side of the diaphragm increases, the diaphragm is in a state of unbalanced compression height, similar to an unbalanced pressure rod, and when the gas pressure in the flash tube increases a little, the diaphragm can reach the critical condition of buckling failure; there is an airway on the inner wall of the chassis for connecting the spiral Bourdon tube, and the spiral Bourdon tube is fixed in the chassis groove, so that it can only expand in the radial direction of the diaphragm; V-shaped groove openings are made at the inner diameters of the circular grooves of the pipeline and the spiral Bourdon tube, and a stopper is provided at the front end of the chassis.

[0010] Preferably, the outer layer of the flash tube is equipped with an electromagnetic coil, which can heat the gas and powder material inside the flash tube; through the heating of the electromagnetic coil, the internal energy of the gas can be increased before the impact test, and the impact heating of the gas by the projectile ensures that the powder material can reach the phase change temperature requirement at a specific pressure.

[0011] Preferably, the diaphragm is located at the end of the flash tube, and the diaphragm material has high hardness and brittleness. The membrane surface of the diaphragm is subjected to a specific molding process to form a weak point in the center; when the pressure on both sides of the diaphragm exceeds the designed limit pressure difference, the diaphragm will break along the preset weak path.

[0012] Preferably, the material collection bin is composed of a bin body, a liquid nitrogen dripper, a liquid nitrogen nozzle, and a filter screen; the material collection bin is equipped with a plurality of liquid nitrogen drippers connected to a liquid nitrogen storage device, which are evenly distributed on the top of the material collection bin; at the front end of the material collection bin, a plurality of hydraulic nozzles distributed in a mirror-symmetrical manner are arranged; the material collection bin also contains a plurality of layers of filter screens, the filter screens are formed by winding and arranging mesh wires with serrated protrusions on the outer surface, the outer ring is a gasket with threads, which can be spirally entered into the bin body, the filter screen has multiple layers, and the mesh aperture of each layer is different, and the mesh aperture of the filter screen changes layer by layer as it moves away from the material release port; a gas channel is arranged at the tail of the material collection bin, the channel is connected to the low-pressure chamber, and the low-pressure chamber is connected to the vacuum pump.

[0013] Preferably, as the number of layers of the multi-layer filter increases, the filter aperture decreases layer by layer and the filter mesh increases; the filter mesh wire is made of high-quality alloy fiber, which can still maintain good mechanical toughness in a low temperature environment, and the fiber surface has a convex structure.

[0014] The utility model provides a gas gun flash evaporation device based on powder surface quenching control, and the beneficial technical effects are:

[0015] (1) Compared with the traditional method of obtaining the metastable phase of materials, the dynamic high pressure technology can shorten the material heating time to the microsecond level during the high-speed loading process of the material, significantly improving the phase change rate of the powder surface; when the outside of the powder material has been transformed into a metastable phase, the inside of the material can still maintain a stable phase, making it possible to achieve a metastable phase-stable coating structure.

[0016] (2) In the collection chamber, the powder material can be quickly cooled by contact with liquid nitrogen. At the same time, due to the addition of a rigid filter, the powder particles collide with the rigid mesh fibers, destroying the gaseous protective layer formed on the surface of the powder material particles, significantly increasing the supercooling of the powder surface, and ultimately forming a coating process of the metastable phase on the powder surface with the internal stable phase.

[0017] (3) The diaphragm crushing stress threshold is designed based on the buckling failure rupture mechanism of the diaphragm. By controlling the force on the side of the diaphragm, the diaphragm crushing time point is controlled, thereby controlling the impact phase change process; changing the protruding shape of the mesh fiber of the rigid filter and the mesh density of the weaving can control the retention ratio of the metastable phase material of the powder particles after quenching and cooling; through the effective control of the three variable factors, the metastable phase of the material generated under the impact high temperature and high pressure conditions can be preserved and recycled under normal conditions.

[0018] (4) Since dynamic high pressure technology will increase the temperature and pressure of the impact powder simultaneously, in order to enable the powder material to better overcome the latent heat barrier of phase change, the introduction of electromagnetic coils can heat the powder to a specific initial temperature at the initial stage, driving more metastable phases to form under low pressure, saving a lot of impact power. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the powder material modification process;

[0020] Figure 2 It is a schematic diagram of the structure of a gas gun flash evaporation device based on powder surface quenching control;

[0021] Figure 3 It is the front view and side profile of the projectile;

[0022] Figure 4 It is a structural schematic diagram of a material collection and cooling device;

[0023] Figure 5 It is a schematic diagram of the structure of part a of the diaphragm clamping mechanism and the diaphragm;

[0024] Figure 6 It is a schematic diagram of the structure of the material collection bin and the filter screen;

[0025] Figure 7 It is a schematic diagram of the flow chart of an embodiment;

[0026] Figure numerals: 1. light gas gun, 2. projectile, 21. vortex structure, 3. flash tube, 31. electromagnetic coil, 32. diaphragm clamping mechanism, 321. chassis, 322. air duct, 323. spiral Bourdon tube, 324. sealing cover, 33. diaphragm, 34. material stacking trough, 35. pneumatic joint, 36. flash tube body, 4. material collection bin, 41. bin body, 42. liquid nitrogen nozzle, 43. liquid nitrogen dripper, 44. filter, 45. end cover, 5. liquid nitrogen storage tank, 6. vacuum pump, 7. low-pressure chamber. DETAILED DESCRIPTION

[0027] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0028] like Figure 1 As shown in the experiment, the phase change process of powder material can be divided into 4 stages: Figure 1 (o) represents the original form of the powder material; Figure 1 (a) represents the second stage of phase change. At this time, the powder particles absorb a certain amount of energy, and the atoms in the outer layer of the particles break through the phase change barrier and reach a high-energy excited state. While continuing to absorb energy, they transfer energy to the inner layer. As the reaction time increases, the proportion of atoms in the high-energy excited state gradually increases, and the transformation to the third stage begins. Figure 1 (b) represents the third stage of phase change. The inner layer of the particle also begins to gradually transform. The atoms of the outer material and the environment reach the same high temperature state. According to the high-pressure phase transition theory, the Gibbs free energy of the thermodynamic system spontaneously transforms to a lower state. The Gibbs free energy of the metastable phase of the powder particles is lower. Under high temperature and high pressure conditions, driven by the change of Gibbs free energy, the powder will generate a metastable phase that only exists in this extreme environment of high temperature and high pressure. Figure 1 In the fourth stage represented by (c), the diaphragm breaks instantly, the powder material particles are released into the supercooled environment, and the melt on the powder surface begins to vitrify. The vitrification incubation time is closely related to the powder supercooling. Different supercooling leads to different energy barriers that can be broken through during the phase change of the material. Therefore, the preferential nucleation of a certain phase can be achieved by controlling the supercooling. Under the condition of the same system energy, the supercooling is closely related to the preset weak path curvature coefficient of the diaphragm, the groove depth, the number of filter mesh layers and the mesh size. The relationship between these variables can be expressed as:

[0029]

[0030] Where ΔT is the thermodynamic undercooling, ΔH and C Pare melting enthalpy and specific heat respectively, Г is the curvature function of the weak path of the diaphragm, d is the average depth of the groove of the weak path of the diaphragm, and n is the fiber correction coefficient of the filter, which is determined by the weaving material of the mesh fiber, the shape of the surface protrusions and the weaving aperture; when the same phase change material is selected, the above formula shows ΔT∝d,n. In the experiment, the supercooling degree can be controlled by pretreating the weak path of the diaphragm and controlling the fiber correction coefficient of the filter. Due to the collision between the powder particles and the mesh fibers, the gaseous protective layer on the surface of the powder material particles is destroyed, resulting in accelerated heat exchange of the particles in the supercooled environment. As a result, the cooling time is shortened to microseconds. In actual operation, the supercooling degree can be close to 1000K, which is much higher than the threshold required for the vitrification process.

[0031] like Figure 2 A gas gun flash device based on powder surface quenching control is shown, comprising a light gas gun 1, a projectile 2, a flash tube 3, a material collection bin 4, a liquid nitrogen storage 5, a vacuum pump 6, and a low-pressure chamber 7; the projectile 2 obtains initial kinetic energy through the light gas gun 1, and then enters the flash tube 3 to compress the gas and powder material therein; when the pressure inside the flash tube 3 reaches the buckling failure stress threshold of the diaphragm 33, the diaphragm 33 ruptures, allowing the powder material to quickly enter the material collection bin 4 and be rapidly cooled. The liquid nitrogen storage device 5 injects liquid nitrogen into the material collection bin 4 to reduce its internal temperature; at the same time, the vacuum pump 6 runs continuously to maintain the low pressure in the low pressure chamber 7 to guide the flow of the powder material after it is released; the light gas gun 1 is connected to the flash tube 3 through a flange, and a sealing ring is provided in the middle to ensure the air tightness of the entire device; wherein, the inner diameter of the muzzle of the light gas gun 1, the inner diameter of the flash tube 3 and the outer diameter of the projectile 2 are the same, so the projectile 2 can smoothly enter the flash tube 3 from the light gas gun 1; a threaded connection is adopted between the flash tube 3 and the material collection bin 4, and a gas pipeline is provided at the tail of the material collection bin 4, which is connected to the low pressure chamber 7, and the low pressure chamber 7 is connected to the vacuum pump 6 through the gas pipeline, and this connection can be controlled by a switch; the liquid nitrogen storage device 5 is connected to the liquid nitrogen nozzle 42 and the liquid nitrogen dripper 43 through a pipeline, and the connection can also be controlled by a switch.

[0032] like Figure 3 As shown in the front view and side cross-sectional view of the projectile, the front end of the projectile 2 is provided with a vortex structure 21, which forms a vortex groove, the groove direction is spiral, the vortex head is wide and deep, and the groove is shallow and narrow structure developing forward; when the projectile 2 moves forward, after the gas enters the vortex structure, the flow state is transformed into a vortex state, and twisting and rotational motion is introduced in the gas flow direction to promote the fluid to form a strong vortex, and these vortices can significantly enhance the heat transfer effect.

[0033] like Figure 4As shown, the flash tube 3 is used for material phase transformation, and the electromagnetic coil 31 is used to increase the initial temperature of the phase change of the gas and powder material inside the pipeline; the diaphragm clamping mechanism 32 clamps the diaphragm 33 and is placed at the rear end of the flash tube 3. When the pressure in the flash tube 3 increases, a radial compression load is applied to the diaphragm 33; the experimental powder material is evenly filled on the middle platform of the material stacking groove 34 located on the bottom curved surface, and the flash tube 3 is evenly distributed with material stacking grooves 34 in the same direction; gas is injected into the flash tube body 36 through the pneumatic joint 35 to form a phase change environment; wherein, the flash tube body 36 and the diaphragm clamping mechanism 32 are flange-connected, and the inner diameter of the flash tube body 36, the inner diameter of the diaphragm clamping mechanism 32 and the outer diameter of the projectile 2 are the same, so the projectile 2 can smoothly transition from the flash tube body 36 to the diaphragm clamping mechanism 32 and compress the gas;

[0034] Specifically, the tail of the flash tube body 36 is equipped with a plurality of material stacking grooves 34, which are grooves processed on the inner wall surface of the tail of the flash tube body 36. These grooves present a spiral overall tendency inside the pipe. With the traveling direction of the projectile, the depth of the material stacking groove gradually decreases and finally becomes flush with the pipe surface. The depth transition process is smooth. The flash tube body 36 is connected to the light gas gun 1 with a sealing gasket flange.

[0035] Specifically, there is an air channel 322 on the inner wall of the diaphragm clamping mechanism 32, and the air channel 322 connects the flash tube 3 and the spiral Bourdon tube 323. The spiral Bourdon tube 323 is placed in the annular groove of the chassis 321 and the sealing cover 324. After the chassis 321 and the sealing cover 324 are connected, the spiral Bourdon tube 323 is restricted and can only expand along the radial direction of the diaphragm 33; the diaphragm 33 is molded before the experiment to form a weak path. When the diaphragm 33 yields and fails to break, the existence of the weak path causes the diaphragm 33 to rupture along the path, avoiding the splashing of diaphragm 33 fragments and preventing damage to other structures of the device; wherein, the inner diameter of the front end channel of the chassis 321 is the same as the outer diameter of the projectile 2, and the tail is provided with a tenon, and there is a circle of buffer gasket in front of the tenon to limit the projectile 2 from continuing to move. , and can also absorb the kinetic energy of the projectile to prevent the rebound and deviation of the projectile 2 after compression; the pipe 322 and the spiral Bourdon tube 323 are connected by a threaded pipe joint; the chassis 321 and the sealing cover 324 have an annular groove with the same inner diameter, the outer ring diameter of the annular groove is the same as the outer ring diameter of the spiral Bourdon tube 323, the groove depth is the same as the width of the spiral Bourdon tube 323, on both sides of the diaphragm 33, the inner ring steps on both sides of the annular groove are V-shaped chamfered openings are processed, and sealing gaskets are placed, and the sealing gaskets cooperate with the diaphragm 33 to seal the space inside the flash tube 3; the chassis 321 and the sealing cover 324 are threadedly connected, and a sealing groove is set at the connection tail to place the sealing gasket; the weak path of the diaphragm 33 is spiral, and the depth of the compression groove gradually increases as it approaches the center.

[0036] like Figure 6As shown, the sealing cover 324 of the flash tube 3 is connected to the front end connection port of the warehouse body 41, the powder material is released from the connection port, and the liquid nitrogen nozzle 42 sprays liquid nitrogen, which can drive the powder material to impact and cool the filter screen 44 covered by the liquid nitrogen dripper 43; the end cover 45 is used to seal the warehouse body, and has a connection hole in the center for extracting the gasified liquid nitrogen during the cooling process to prevent excessive gas disturbance in the material collection warehouse from interfering with the experiment; the front end of the warehouse body 41 has an internal thread and a sealing gasket groove, which can be threadedly sealed with the spiral sealing cover 324 of the flash tube 3; the liquid nitrogen nozzle 42 and the liquid nitrogen dripper 43 are connected to the liquid nitrogen through a liquid nitrogen pipeline In the storage device 5, whether liquid nitrogen passes through is controlled by a switch and can be controlled as needed; the outer ring of the filter screen 44 is a gasket with a thread, which can be screwed into the bin body 41; the surface of the mesh fiber of the multi-layer filter screen 44 has protrusions, and when it comes into contact with the powder material with a gaseous protective layer, the protrusions make it easier to pierce the protective layer, and the apertures of the multi-layer filter screen 44 are different, and the apertures decrease layer by layer as they move away from the material release port; the end cover 45 and the bin body 41 are connected by threads, and a sealing groove is provided at the connection tail for placing a sealing gasket; a gas pipeline extends from the central opening of the end cover 45, which is connected to the low-pressure chamber 7 through the pipeline.

[0037] like Figure 7 As shown, the utility model also provides a method for rapid cooling of powder material modification technology, using the above-mentioned gas gun flash evaporation device based on powder surface quenching control, including the following steps:

[0038] S1: Check the reliability of each component of the device to ensure that the liquid nitrogen nozzle 42 and the liquid nitrogen dripper 43 are not blocked, the sealing gaskets at various parts are free of cracks, the pipeline switches at various parts are in normal use, and the barrel and flash tube 3 of the light gas gun 1 are cleaned; put the projectile 2 into the light gas gun 1, with the side of the projectile 2 having the vortex structure 21 facing the pipe mouth; connect the flash tube body 36 and the light gas gun 1 through the cooperation of the flange and the sealing gasket; connect the liquid nitrogen dripper 43 and the liquid nitrogen nozzle 42 to the liquid nitrogen storage 5, and spirally place multiple filter screens 44 in the order of pore size from large to small into the warehouse body 41; install the gas pipeline at the opening of the end cover 45, and finally, connect the end cover 45 and the sealing gasket to the warehouse body 41 by spiral connection;

[0039] S2: Use a threaded pipe joint to connect the spiral Bourdon tube 323 and the airway 322; place a sealing gasket on the V-shaped groove inside the circular groove of the bottom plate 321, and embed the diaphragm 33 into the inner wall of the inner ring of the spiral Bourdon tube 323; put the spiral Bourdon tube 323 and the diaphragm 33 into the bottom plate 321, place the sealing gasket again on the V-shaped groove inside the circular groove of the sealing cover 324, and connect the sealing cover 324 and the bottom plate 321 with the sealing gasket in a spiral manner; after connection, the diaphragm clamping mechanism 32 is spirally connected with the material collection bin 4 in cooperation with the sealing gasket; divide the powder material into multiple portions, and respectively put them into the middle section of multiple material stacking grooves 34 at the bottom of the flash tube 3;

[0040] S3: A buffer gasket is placed at the inner stopper at the front end of the diaphragm clamping mechanism 32, and the flash tube body 36 is connected to the diaphragm clamping mechanism 32 with a flange in cooperation with the sealing gasket; the liquid nitrogen dripper 43 is turned on to cool the multi-layer filter screen 44, and at the same time, the pipeline connecting the material collection bin 4 to the low-pressure chamber 7 is opened, and the vacuum pump 6 starts to operate to continuously extract the gasified nitrogen from the material collection bin 4; when the filter screen 44 reaches the specified temperature, the liquid nitrogen dripper 43 is turned off;

[0041] S4: When the air pressure in the material collection bin 4 is lower than the set threshold, the projectile 2 is fired and the liquid nitrogen nozzle 42 is opened at the same time;

[0042] S5: Observe and record the experimental phenomena and results, observe the diaphragm fragmentation morphology, ensure that the diaphragm is torn along the preset weak path, and the length of the tearing path cannot exceed the total length of the preset fragmentation path; secondly, ensure that there is no residual powder agglomerate material in the flash tube 3. If the requirements are not met, the diaphragm related parameters need to be redesigned;

[0043] S6: Perform X-ray diffraction (XRD) analysis on the powder material after the experiment to observe whether a new diffraction peak is generated. If the diffraction peak is the same as the original powder material spectrum, try to increase the initial internal energy of the powder material and the flash evaporation environment through the electromagnetic coil 31, or give the projectile 2 a larger initial kinetic energy, and conduct multiple experiments to find the initial parameters that will cause the diffraction peak to change in the XRD spectrum;

[0044] S7: Determine whether to continue the experiment based on the experimental results and XRD analysis. If the existing materials meet the requirements, there is no need to continue the experiment and the device is disassembled; if the existing materials do not meet the requirements, proceed to the subsequent steps:

[0045] S8: Observe the adhesion of powder materials on each layer of the multi-layer filter screen 44, determine whether the multi-layer filter screen 44 has the preset effect, and consider the rationality of the layout; ensure that the material is successfully attached to the filter screen 44 far away from the material release port, that is, the rear of the warehouse body 41: if the material is not attached, and the material is mostly concentrated on the filter screen 44 at the front end of the warehouse body 41 and near the material release port, it is because the weaving aperture setting of the filter screen 44 is unreasonable, resulting in excessive flow resistance when the expanded gas passes through the filter screen 44, making it difficult to pass through the filter screen 44 into the low-pressure chamber 7, and the weaving aperture of the filter screen 44 should be increased; if the material is mostly concentrated at the rear of the warehouse body 41, it is necessary to increase the number of filter screen 44 layers to effectively intercept the material while keeping the weaving aperture unchanged, and the added filter screen 44 should meet different phase angles;

[0046] S9: If the XRD analysis shows a change in the diffraction peaks and the material is effectively intercepted and collected by the filter, you should consider changing the protrusion structure on the mesh fiber and seek a greater degree of supercooling by changing the arrangement distance and protrusion height. Continue the experiment after the changes are completed.

Claims

1. A gas gun flash evaporation device based on powder surface quenching control, Features: It includes a light gas gun, a projectile, a flash tube, a material collection bin, a liquid nitrogen storage, a low-pressure chamber, and a vacuum pump; the surface of the projectile facing the muzzle is treated to form a vortex groove, the groove is spiral-shaped, the vortex head is wide and deep, and the groove is shallow and narrow and develops forward; The flash tube includes a flash tube body, an electromagnetic coil, a diaphragm clamping mechanism, a diaphragm, a material stacking groove, and a pneumatic joint; the material stacking groove is a groove on the inner wall surface of the rear part of the flash tube body after treatment, and these grooves present a spiral overall tendency inside the pipe; the depth of the material stacking groove gradually decreases with the direction of the projectile; the diaphragm clamping mechanism includes a chassis, a spiral Bourdon tube, and a sealing cover; there is an airway on the inner wall of the chassis for connecting the spiral Bourdon tube, and the spiral Bourdon tube is fixed in the chassis groove and can only expand along the radial direction of the diaphragm; the inner diameter of the circular groove of the pipeline and the spiral Bourdon tube is V-shaped groove opening, and the front end of the chassis has a stop tenon; The material collection bin comprises a bin body, a liquid nitrogen nozzle, a liquid nitrogen dripper, a filter screen and an end cover; the filter screen is formed by winding and arranging a mesh wire with serrated protrusions on the outer surface, and the outer ring is a gasket with threads that can be spirally inserted into the bin body; the filter screen has multiple layers, and the mesh apertures of the multiple layers are different in size, and the mesh apertures of the filter screen decrease layer by layer as it moves away from the material release port.

2. A gas gun flash evaporation device based on powder surface quenching control according to claim 1, Features: The diaphragm is subjected to a molding process so that the weak path of the diaphragm is spiral-shaped, and the depth of the groove on the diaphragm gradually increases as it approaches the center.

3. A gas gun flash evaporation device based on powder surface quenching control according to claim 1, Features: The spiral Bourdon tube is formed by overlapping multiple circles, and is provided with a channel for injecting gas inside, while the tail is sealed. After gas is injected, the spiral Bourdon tube expands, causing the inner diameter of the spiral to gradually decrease.