Small-caliber smoothing toner bottle body mold

The small-caliber softening water bottle mold addresses fit and deformation issues by using a clamping mechanism with guide and molding blocks, ensuring precise alignment and preventing scalding, thus enhancing product quality.

CN222116018UActive Publication Date: 2024-12-06SHANGHAI JIXIAOPAI BIOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323528301.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-25
Publication Date
2024-12-06
Estimated Expiration
2033-12-25

AI Technical Summary

Technical Problem

Existing blow molding molds for small-caliber toner bottles suffer from poor fit between mold parts, leading to deformation and scalding issues at the mold line, which compromises product quality.

Method used

A small-caliber softening water bottle mold design featuring a clamping mechanism with guide blocks and grooves, molding mechanisms with top and bottle mouth blocks, and auxiliary mechanisms with bottom blocks, ensuring precise alignment and fit of mold parts to prevent deformation and scalding during blow molding.

Benefits of technology

The design enhances the uniformity of bottle thickness and prevents scalding and scratching, improving the overall quality of the molded products by maintaining accurate fit and alignment of mold components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222116018U_ABST
    Figure CN222116018U_ABST
Patent Text Reader

Abstract

The utility model provides a small-caliber smoothing toner bottle body mould, which relates to the technical field of small-caliber smoothing toner bottle body moulds and comprises a clamping mechanism, the clamping mechanism comprises a first mould, a second mould is arranged on one side face of the first mould, a guide block is arranged on one side face, close to the second mould, of the first mould, and the guide block is arranged on the other side face of the first mould. The number of the guide blocks is two, the guide blocks are fixedly connected with the first mold, and as a preferable implementation mode, a forming mechanism is arranged at the tops of the guide blocks, and the forming mechanism comprises a top block. According to the small-caliber smoothing toner bottle body mold, due to the arrangement of the clamping mechanism, when the small-caliber smoothing toner bottle body mold is used for blow molding, edges and corners of a bottle opening and a bottle body can be better reflected, the thickness of each part of the bottle body is more uniform, and in addition, due to the arrangement of the two filling blocks and the two bottle opening mold blocks, the production efficiency is improved. Therefore, the soft water bottle is prevented from being scalded during blow molding.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of small-caliber skin softening water bottle molds, in particular to a small-caliber skin softening water bottle mold. Background Art

[0002] Blow molding, here mainly refers to hollow blow molding, which is a method of using gas pressure to inflate the hot melt parison closed in the mold to form a hollow product. It is the third most commonly used plastic processing method and also a rapidly developing plastic molding method. The mold used for blow molding is only a female mold. Compared with injection molding, the equipment cost is lower, the adaptability is stronger, the molding performance is good, and the products with complex undulating curves can be molded.

[0003] The existing blow molding mold for small-caliber toner bottle is usually composed of multiple mold parts. However, when multiple mold parts are used in combination, the fit is not high. Therefore, during blow molding, the bottle mouth and the bottle body will be burned from the mold line, causing the bottle mouth or the bottle body to deform, resulting in reduced product quality. For this reason, we provide a small-caliber toner bottle mold. Utility Model Content

[0004] The utility model aims to solve the defect that the mold part of the existing blow molding mold for the small-caliber softening water bottle in the prior art causes scalding to the product at the mold line, and provides a small-caliber softening water bottle mold.

[0005] In order to achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a small-caliber softening water bottle mold, comprising: a clamping mechanism, the clamping mechanism comprising a first mold, a second mold is provided on one side of the first mold, a guide block is provided on a side of the first mold close to the second mold, the number of the guide blocks is two, and the guide block is fixedly connected to the first mold. As a preferred embodiment, a molding mechanism is provided on the top of the guide block, the molding mechanism comprises a top block, a bottle mouth mold block is provided at the bottom of the top block, the number of the top block and the bottle mouth mold block are both two, the top block and the bottle mouth mold block are both placed in a first placement groove opened on the first mold and the second mold, the top block is provided with a blow molding groove, the bottle mouth mold block is provided with a bottle mouth groove, and an auxiliary mechanism is provided at the bottom of the guide block, the auxiliary mechanism comprises a bottom block, and the number of the bottom blocks is two.

[0006] As a preferred embodiment, a guide groove matched with the guide block is formed on the second mold, and a first placement groove is formed on both the first mold and the second mold.

[0007] As a preferred embodiment, the first mold and the second mold are both provided with a second mounting groove, and the first mold and the second mold are both provided with a bottle body groove.

[0008] As a preferred embodiment, the bottom block is placed in a second mounting groove provided on the first mold and the second mold, and a bottle bottom groove is provided on the bottom block.

[0009] Compared with the prior art, the advantages and positive effects of the utility model are:

[0010] The utility model provides a clamping mechanism so that the small-caliber skin softening water bottle mold can better reflect the edges and corners of the bottle mouth and the bottle body during blow molding, and makes the thickness of the bottle body more uniform. In addition, two filling blocks and two bottle mouth mold blocks are provided, so that the skin softening water bottle will not cause burns during blow molding, and at the same time, the two bottom blocks in the auxiliary mechanism are used to prevent the surface of the formed bottle body from being scratched during demoulding, thereby improving the quality of product production. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 The utility model provides a three-dimensional diagram of a small-caliber skin softening water bottle mold.

[0012] Figure 2 The utility model is a schematic diagram of the disassembly of a small-caliber skin softening water bottle mold.

[0013] Figure 3 The utility model provides a schematic diagram of the installation of a top block of a small-caliber skin softening water bottle mold.

[0014] Figure 4 The utility model provides a schematic diagram of the installation of a bottle mouth mold block of a small-caliber softening water bottle mold.

[0015] Figure 5 The utility model provides a schematic diagram of the bottom block structure of a small-caliber skin softening water bottle mold.

[0016] Figure 6 The utility model provides a schematic diagram of the installation of a guide block of a small-caliber skin softening water bottle mold.

[0017] Figure 7 The utility model is a three-dimensional diagram of an auxiliary mechanism of a small-caliber skin softening water bottle mold.

[0018] Legend:

[0019] 1. Clamping mechanism; 2. Forming mechanism; 3. Auxiliary mechanism; 11. First mold;

[0020] 12. Second mold; 13. Guide block; 14. First mounting groove; 15. Second mounting groove;

[0021] 16. Bottle body groove; 17. Guide groove; 21. Top block; 22. Blow molding groove; 23. Bottle mouth mold block;

[0022] 24. Bottle mouth groove; 31. Bottom block; 32. Bottle bottom groove. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0024] Example 1

[0025] like Figure 1 , Figure 2 , Figure 6 and Figure 7 As shown, the utility model provides a technical solution: a small-caliber softening water bottle mold, comprising: a clamping mechanism 1, the clamping mechanism 1 comprises a first mold 11, a second mold 12 is provided on one side of the first mold 11, a guide block 13 is provided on the side of the first mold 11 close to the second mold 12, the number of the guide blocks 13 is two, the guide blocks 13 are fixedly connected to the first mold 11, a guide groove 17 matched with the guide block 13 is provided on the second mold 12, a first placement groove 14 is provided on the first mold 11 and the second mold 12, a second installation groove 15 is provided on the first mold 11 and the second mold 12, and a bottle body groove 16 is provided on the first mold 11 and the second mold 12.

[0026] In this embodiment, by setting a clamping mechanism 1, and the clamping mechanism 1 is provided with a first placement groove 14 and a second installation groove 15 that match the molding mechanism 2 and the auxiliary mechanism 3, under the stable clamping of the first mold 11 and the second mold 12, the auxiliary mechanism 3 and the molding mechanism 2 will not cause a decrease in product quality due to insufficient fit of the components when blow-molding the bottle body and the bottle mouth, and a guide block 13 is provided on the first mold 11, and a guide groove 17 is opened on the second mold 12, so that the first mold 11 and the second mold 12 are more accurate and fit during installation, and the guide block 13 will enter the guide groove 17, thereby ensuring that the first mold 11 and the second mold 12 will not deviate after alignment, thereby ensuring the fit of each component in the auxiliary mechanism 3 and the molding mechanism 2.

[0027] Example 2

[0028] like Figure 1-Figure 5As shown, a molding mechanism 2 is provided on the top of the guide block 13, and the molding mechanism 2 includes a top block 21. A bottle mouth mold block 23 is provided at the bottom of the top block 21. The number of the top block 21 and the bottle mouth mold block 23 are both two. The top block 21 and the bottle mouth mold block 23 are both placed in the first placement groove 14 opened on the first mold 11 and the second mold 12. A blow molding groove 22 is opened on the top block 21, and a bottle mouth mold block 23 is opened on the bottle mouth groove 24. An auxiliary mechanism 3 is provided at the bottom of the guide block 13. The auxiliary mechanism 3 includes a bottom block 31. The number of the bottom blocks 31 is two. The bottom blocks 31 are placed in the second installation groove 15 opened on the first mold 11 and the second mold 12, and a bottle bottom groove 32 is opened on the bottom block 31.

[0029] In this embodiment, by setting the molding mechanism 2 and the auxiliary mechanism 3, and the number of the top block 21, the bottle mouth mold block 23 and the bottom block 31 are all two, so that the type of skin softening water bottle will not directly rub against the molded bottle body during demoulding, thereby ensuring the smoothness of the bottle body and making the quality of the bottle body higher, and by setting the blow molding groove 22 on the top block 21 and the bottle mouth mold block 23. The positions where the blow molding groove 22 and the bottle mouth groove 24 are set are located in the central part of the top block 21 and the bottle mouth mold block 23, and there is a thicker peripheral part to protect the bottle mouth, so that the bottle mouth will not be scalded at the mold line between the two top blocks 21 and the two bottle mouth mold blocks 23 and the two bottom blocks 31, and the edges of the bottle bottom groove 32 and the bottle mouth groove 24 opened on the bottom block 31 are both in line with the bottle body groove 16, so as to ensure the molding effect of the body, the bottle mouth and the bottle bottom.

[0030] Working principle:

[0031] like Figure 1-Figure 7 As shown, when the utility model is used, the first mold 11 and the second mold 12 in the clamping mechanism 1 are firstly accurately aligned. Under the action of the guide block 13 and the guide groove 17, the first mold 11 and the second mold 12 are closely and fittingly aligned. At the same time, the guide block 13 fits with the guide groove 17 to ensure the stability of the connection between the first mold 11 and the second mold 12, and the two bottom blocks 31 are installed in the second installation grooves 15 opened on the first mold 11 and the second mold 12. Under the restriction of the second installation grooves 15, the fit of the bottle bottom grooves 32 opened on the two bottom blocks 31 can be ensured. Afterwards, the first mold 11 and the second mold 12 are erected, and the two bottom blocks 31 are placed in the second installation groove 15, and then the two bottle mouth mold blocks 23 are first placed in the first placement groove 14, and the surface of the bottle mouth groove 24 that fits with the bottle body groove 16 is placed at the bottom, and then the two top blocks 21 are placed in the first placement groove 14. At this time, the two top blocks 21 and the two bottle mouth mold blocks 23 are placed. At this time, the bottle mouth groove 24 is in a fit state with the bottle body groove 16 and the bottle bottom groove 32, ensuring that the blow molding fit between the bottle body and the bottle mouth and the bottle bottom is higher, and then the blow molding operation can be carried out through the blow molding groove 22.

[0032] The above are only preferred embodiments of the present invention, and are not intended to limit the present invention in other forms. Any technician familiar with the profession may use the technical contents disclosed above to change or modify them into equivalent embodiments with equivalent changes and apply them to other fields. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the technical solution of the present invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. A small-caliber skin softening water bottle mold, characterized in that: include: A clamping mechanism (1), the clamping mechanism (1) comprising a first mold (11), a second mold (12) being provided on one side of the first mold (11), a guide block (13) being provided on one side of the first mold (11) close to the second mold (12), two guide blocks (13) being provided, the guide blocks (13) being fixedly connected to the first mold (11), a molding mechanism (2) being provided on the top of the guide blocks (13), the molding mechanism (2) comprising a top block (21), a bottle mouth mold being provided on the bottom of the top block (21) The guide block (23) comprises a top block (21) and a bottle mouth mold block (23), each of which is two in number. The top block (21) and the bottle mouth mold block (23) are both placed in first placement grooves (14) provided on the first mold (11) and the second mold (12). The top block (21) is provided with a blow molding groove (22), and the bottle mouth mold block (23) is provided with a bottle mouth groove (24). An auxiliary mechanism (3) is provided at the bottom of the guide block (13), and the auxiliary mechanism (3) comprises a bottom block (31). The bottom blocks (31) are two in number.

2. A small-caliber skin softening water bottle mold according to claim 1, characterized in that: The second mold (12) is provided with a guide groove (17) that matches the guide block (13), and the first mold (11) and the second mold (12) are both provided with a first placement groove (14).

3. A small-caliber skin softening water bottle mold according to claim 2, characterized in that: The first mold (11) and the second mold (12) are both provided with a second installation groove (15), and the first mold (11) and the second mold (12) are both provided with a bottle body groove (16).

4. The small-caliber skin softening water bottle mold according to claim 1, characterized in that: The bottom block (31) is placed in a second mounting groove (15) provided on the first mold (11) and the second mold (12), and a bottle bottom groove (32) is provided on the bottom block (31).