Alloy steel plate strip surface hot-dip tinning device
By introducing atomized spray heads and scrapers into the hot-dip plating device on the alloy steel plate belt, the problem of impurities on the surface of the steel plate belt affecting the plating quality is solved, efficient cleaning is achieved, and the adhesion and uniformity of the plating layer are improved. , thereby improving product processing quality.
Patent Information
- Application Number
- CN202421000843.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-09
- Publication Date
- 2025-02-07
- Estimated Expiration
- 2034-05-09
AI Technical Summary
The existing hot-dip tin plating device on the surface of the alloy steel plate belt is not cleaned and pretreated before the steel plate belt enters the tin liquid pool, resulting in oil stains, dust and other impurities adhesion on the surface of the steel plate belt, affecting the uniformity and adhesion of the plating and reducing the product. Processing quality.
Design a hot-dip plating device for alloy steel plate belt surface, including atomizing spray head and scraper, through a water pump, water is passed through the delivery pipe and U-shaped tube to the atomizing spray head, spraying water to cover the surface of the steel plate belt, dissolve or soften impurities, and then The scraper cleans up impurities to ensure that the surface is clean and free of impurities.
Through cleaning treatment, the adhesion and uniformity of the tin plating layer are improved and the product processing quality is improved.
Smart Images

Figure CN222434590U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of hot-dip tinning of alloy steel strips, in particular to a device for hot-dip tinning of the surface of an alloy steel strip. Background Art
[0002] Alloy steel strip is a special steel product composed of iron, carbon and other alloy elements. During the production and processing of steel strip, it is necessary to use hot-dip tinning process to cover the molten tin on the surface of the steel strip in order to improve the corrosion resistance, aesthetics and other properties of the steel strip.
[0003] The existing hot-dip tinning device for alloy steel strip surface is mainly composed of a conveying mechanism, a tin liquid pool and a cooling system. During the tinning process, the steel strip is first sent into the tin liquid pool through the conveying mechanism. In the tin liquid pool, the steel strip contacts with the molten tin liquid. After immersion, the steel strip leaves the tin melting furnace and enters the cooling system. During the cooling process, the tinned layer gradually solidifies and fixes on the surface of the steel strip. Finally, the cooled steel strip is rolled up by the winding device to complete the entire hot-dip tinning process.
[0004] The existing hot-dip tinning device for the surface of alloy steel strips does not perform cleaning pretreatment before the steel strips enter the tin liquid pool, so that oil, dust and other particulate matter may adhere to the surface of the steel strips, thereby affecting the uniformity and adhesion of the molten tin and reducing the quality of product processing; therefore, a hot-dip tinning device for the surface of alloy steel strips is proposed to address the above problems. Utility Model Content
[0005] In order to make up for the deficiencies of the prior art and solve the problems raised by the above-mentioned background technology, the utility model proposes a device for hot-dip tinning on the surface of an alloy steel plate or strip.
[0006] The technical solution adopted by the utility model to solve its technical problems is: the utility model describes a device for hot-dip tinning on the surface of an alloy steel plate strip, comprising a base; a bending plate is fixedly connected to the base, two hollow tubes are fixedly connected to the bending plate, each hollow tube is connected to a plurality of atomizing nozzles, the two hollow tubes are connected via a U-shaped tube, a support frame is fixedly connected to the base, a water tank is installed on the support frame, a water pump is installed on the water tank, an input hole of the water pump is connected to a water pumping pipe, an output hole of the water pump is connected to a delivery pipe, and the other end of the delivery pipe is fixedly connected to the U-shaped pipe, a filter screen is arranged in the water tank, a through opening is opened on the base, and the water tank is arranged directly below the through opening, and a filter screen is arranged in the water tank, a through opening is opened on the base, and the water tank is arranged directly below the through opening, and a filter screen is fixedly connected to the base There are two vertical plates, and two scrapers are rotatably installed between the two vertical plates, and the two scrapers are respectively located on the upper and lower sides of the steel strip. Before the steel strip enters the tin liquid pool, it is necessary to remove the impurities remaining on the surface of the steel strip. Through the operation of the water pump, the water in the water tank flows into the U-shaped tube through the conveying pipe, and finally sprayed out through the atomizing nozzle 4, so that the water is evenly covered on the entire surface of the steel strip, so that it can effectively dissolve or soften the oil, rust and other impurities on its surface. Subsequently, through the action of the scraper, the surface of the steel strip can be scraped and cleaned, so that these impurities can be quickly and thoroughly removed, and efficient cleaning is achieved to ensure that the surface of the steel strip is clean and free of impurities, thereby improving the adhesion and uniformity of the tin plating layer, thereby improving the processing quality of the product.
[0007] Preferably, two inclined plates are fixedly connected between the two vertical plates, and three springs are fixedly connected between the inclined plates and the scraper. When the device is used, the scraper can always be in contact with the surface of the steel strip by setting the springs, so that scraping and cleaning can be performed better.
[0008] Preferably, a tin liquid pool is provided on the base, and a sinking roller is rotatably installed in the tin liquid pool. When the device is used, the sinking roller is provided to facilitate the immersion of the steel plate strip into the molten tin liquid in the tin liquid pool.
[0009] Preferably, two short plates are fixedly connected to both sides of the port of the tin liquid pool, and auxiliary rollers are rotatably mounted on the two short plates. When the device is used, auxiliary rollers are provided to facilitate auxiliary conveying operations on the steel strip.
[0010] Preferably, two first vertical plates are fixedly connected to one end of the base, and two first guide rollers are rotatably installed on the two first vertical plates. Two second vertical plates are fixedly connected to the base, and the second vertical plates are arranged between the first vertical plates and the vertical plates. Two second guide rollers are rotatably installed on the two second vertical plates. When the device is used, the guide rollers are arranged to facilitate the conveying operation of the steel plate strip.
[0011] The utility model is beneficial in that:
[0012] The utility model needs to remove the impurities remaining on the surface of the steel strip before the steel strip enters the tin liquid pool, and through the operation of the water pump, the water in the water tank flows into the U-shaped tube through the conveying pipe, and finally is sprayed out through the atomizing nozzle, so that the water is evenly covered on the entire surface of the steel strip, thereby effectively dissolving or softening the oil, rust and other impurities on the surface thereof, and then, through the action of the scraper, the surface of the steel strip can be scraped and cleaned, so that these impurities can be quickly and thoroughly removed, and efficient cleaning is achieved to ensure that the surface of the steel strip is clean and free of impurities, thereby improving the adhesion and uniformity of the tin-plated layer, and further improving the processing quality of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0014] Figure 1 It is a schematic diagram of the overall three-dimensional structure of hot-dip tinning equipment;
[0015] Figure 2 It is a schematic diagram of the three-dimensional structure of the cleaning mechanism;
[0016] Figure 3 It is a schematic diagram of the three-dimensional structure of the spray mechanism;
[0017] Figure 4 It is a schematic diagram of the three-dimensional structure of the scraping and cleaning component;
[0018] Figure 5 It is a schematic diagram of the three-dimensional structure of the transmission mechanism;
[0019] Figure 6 It is a schematic diagram of the three-dimensional structure of the tin liquid pool in cross section.
[0020] In the figure: 1. base; 2. bending plate; 3. hollow tube; 4. atomizing nozzle; 5. U-shaped tube; 6. support frame; 7. water tank; 8. filter screen; 9. water pump; 10. suction pipe; 11. conveying pipeline; 12. through port; 13. vertical plate; 14. scraper; 15. inclined plate; 16. spring; 17. tin liquid pool; 18. sinking roller; 19. short plate; 20. auxiliary roller; 21. first vertical plate; 22. first guide roller; 23. second vertical plate; 24. second guide roller. DETAILED DESCRIPTION
[0021] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0022] See also Figure 1-4 As shown, a device for hot-dip tinning on the surface of an alloy steel strip comprises a base 1; a bending plate 2 is fixedly connected to the base 1, two hollow tubes 3 are fixedly connected to the bending plate 2, each hollow tube 3 is connected to a plurality of atomizing nozzles 4, and the two hollow tubes 3 are connected through a U-shaped tube 5; a support frame 6 is fixedly connected to the base 1, a water tank 7 is installed on the support frame 6, a water pump 9 is installed on the water tank 7, an input hole of the water pump 9 is connected to a water pumping pipe 10, an output hole of the water pump 9 is connected to a delivery pipe 11, and the other end of the delivery pipe 11 is fixedly connected to the U-shaped tube 5, a filter screen plate 8 is arranged in the water tank 7, a through port 12 is opened on the base 1, and the water tank 7 is arranged directly below the through port 12, two vertical plates 13 are fixedly connected to the base 1, two scrapers 14 are rotatably installed between the two vertical plates 13, and the two scrapers 14 are respectively located on the upper and lower ends of the steel strip. On the lower two sides, two inclined plates 15 are fixedly connected between the two vertical plates 13, and three springs 16 are fixedly connected between the inclined plates 15 and the scraper 14; before the steel strip enters the tin liquid pool 17, it is necessary to remove the impurities remaining on the surface of the steel strip, and the water in the water tank 7 is pumped out through the suction pipe 10 by the water pump 9, and flows into the U-shaped tube 5 through the conveying pipe 11, and finally sprayed out through the atomizing nozzle 4, so that the water is evenly covered on the entire surface of the steel strip, so that it can effectively dissolve or soften the oil, rust and other impurities on its surface, and then, through the action of the scraper 14, the surface of the steel strip can be scraped and cleaned, so that these impurities can be quickly and thoroughly removed, and efficient cleaning can be achieved to ensure that the surface of the steel strip is clean and free of impurities, thereby improving the adhesion and uniformity of the tin plating layer, and thus improving the processing quality of the product.
[0023] See also Figure 5-6As shown, a tin liquid pool 17 is provided on the base 1, and a sinking roller 18 is rotatably installed in the tin liquid pool 17. Two short plates 19 are fixedly connected to both sides of the port of the tin liquid pool 17, and auxiliary rollers 20 are rotatably installed on the two short plates 19. Two first vertical plates 21 are fixedly connected to one end of the base 1, and two first guide rollers 22 are rotatably installed on the two first vertical plates 21. Two second vertical plates 23 are fixedly connected to the base 1, and the second vertical plates 23 are arranged between the first vertical plates 21 and the vertical plates 13. Two second guide rollers 24 are rotatably installed on the two second vertical plates 23; when tinning, the steel strip is first passed through the two first guide rollers 22, between the two second guide rollers 24, the top of the auxiliary roller 20 and the bottom of the sinking roller 18 in sequence. When the steel strip after cleaning is sent into the tin liquid pool 17 through the conveying mechanism, with the cooperation of the sinking roller 18, the steel strip can be sunk into the tin liquid pool 17, so that the steel strip contacts with the molten tin liquid, thereby achieving the purpose of tinning.
[0024] Working principle: the existing hot-dip tinning device for alloy steel strip surface does not perform cleaning pretreatment before the steel strip enters the tin liquid pool 17, so that oil, dust and other particulate matter may adhere to the surface of the steel strip, thereby affecting the uniformity and adhesion of the molten tin and reducing the quality of product processing; therefore, a hot-dip tinning device for alloy steel strip surface is proposed to address the above problems; before the steel strip enters the tin liquid pool 17, it is necessary to remove the impurities remaining on the surface of the steel strip, and the water in the water tank 7 is pumped out through the pumping pipe 10 through the water pump 9, and flows into the U-shaped tube 5 through the conveying pipe 11, and finally sprayed out through the atomizing nozzle 4, so that the water is evenly covered on the entire surface of the steel strip, so that the oil, rust and other impurities on its surface can be effectively dissolved or softened, and then, the scraper 14 can scrape and clean the surface of the steel strip, so that these impurities can be quickly and thoroughly removed, and efficient cleaning can be achieved to ensure that the surface of the steel strip is clean and free of impurities, thereby improving the adhesion and uniformity of the tin plating layer, and thus improving the processing quality of the product;
[0025] During tin plating, the steel strip is first passed through the two first guide rollers 22, between the two second guide rollers 24, the top of the auxiliary roller 20 and the bottom of the sinking roller 18 in sequence. When the steel strip after cleaning is sent into the tin liquid pool 17 through the conveying mechanism, with the cooperation of the sinking roller 18, the steel strip can be sunk into the tin liquid pool 17, so that the steel strip is in contact with the molten tin liquid, thereby achieving the purpose of tin plating.
[0026] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the utility model. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0027] The above shows and describes the basic principle, main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments, and the above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, and these changes and improvements fall within the scope of the utility model to be protected.
Claims
1. A device for hot-dip tinning of alloy steel strips, characterized in that: The invention comprises a base (1); a bent plate (2) is fixedly connected to the base (1); two hollow tubes (3) are fixedly connected to the bent plate (2); each hollow tube (3) is connected to a plurality of atomizing nozzles (4); the two hollow tubes (3) are connected to each other via a U-shaped tube (5); a support frame (6) is fixedly connected to the base (1); a water tank (7) is installed on the support frame (6); a water pump (9) is installed on the water tank (7); an input hole of the water pump (9) is connected to a water pump pipe (10); the water pump (9) is connected to a water pump (11); The output hole of the pump (9) is connected to a delivery pipe (11), and the other end of the delivery pipe (11) is fixedly connected to the U-shaped tube (5). A filter screen (8) is arranged in the water tank (7). A through opening (12) is opened on the base (1), and the water tank (7) is arranged directly below the through opening (12). Two vertical plates (13) are fixedly connected to the base (1), and two scrapers (14) are rotatably installed between the two vertical plates (13), and the two scrapers (14) are respectively located on the upper and lower sides of the steel plate strip.
2. The device for hot-dip tinning of alloy steel strip according to claim 1, characterized in that: Two inclined plates (15) are fixedly connected between the two vertical plates (13), and three springs (16) are fixedly connected between the inclined plates (15) and the scraper plates (14).
3. The device for hot-dip tinning of alloy steel strip according to claim 1, characterized in that: A tin liquid pool (17) is arranged on the base (1), and a sinking roller (18) is rotatably installed in the tin liquid pool (17).
4. The device for hot-dip tinning of alloy steel strip according to claim 3, characterized in that: Two short plates (19) are fixedly connected to both sides of the port of the tin liquid pool (17), and auxiliary rollers (20) are rotatably mounted on the two short plates (19).
5. The device for hot-dip tinning of alloy steel strip according to claim 1, characterized in that: Two first vertical plates (21) are fixedly connected to one end of the base (1), and two first vertical plates (21) are rotatably mounted with two first guide rollers (22).
6. The device for hot-dip tinning of alloy steel strip according to claim 1, characterized in that: Two second vertical plates (23) are fixedly connected to the base (1), and the second vertical plates (23) are arranged between the first vertical plate (21) and the vertical plate (13). The two second vertical plates (23) are rotatably mounted with two second guide rollers (24).