Composite floor for railway passenger car, manufacturing method therefor and railway passenger car
By adopting a laminated structure of carbon fiber composite panels and plastic panels, the problem of complex floor structure in rail passenger vehicles was solved, achieving lightweighting, noise reduction, and vibration damping, reducing the vehicle body weight and improving sound insulation performance.
Patent Information
- Application Number
- PCT/CN2024/094877
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-23
- Filing Date
- 2024-05-23
- Publication Date
- 2024-11-28
AI Technical Summary
The existing rail passenger vehicle floor structure is complex and cannot simultaneously meet the requirements of lightweight, noise reduction, vibration reduction, fire resistance and low cost.
The composite flooring structure consists of a first carbon fiber composite plate, a reinforcing plate, a second carbon fiber composite plate, and a plastic plate. The laminated flooring is formed through hot pressing and a specific layup sequence. Modified carbon fiber reinforced thermoplastic resin material is used to improve interfacial bonding and mechanical strength, and the plastic plate provides shock absorption.
It achieves a reduction of 8-15% in vehicle body weight, an increase of 3-10dB in sound insulation, an increase of 10-15% in impact resistance, and a reduction of 2-8dBA in radiated sound power, meeting the requirements for lightweighting and vibration reduction.
Smart Images

Figure CN2024094877_28112024_PF_FP_ABST
Abstract
Description
Composite floor for rail passenger car, preparation method thereof and rail passenger car
[0001] This application claims priority to the Chinese patent application filed with the Patent Office of China on May 23, 2023, with application number 202310586799.6 and invention name “A composite floor for rail passenger cars, its preparation method and rail passenger car”, the entire contents of which are incorporated by reference into this application. Technical Field
[0002] The present invention belongs to the field of rail passenger vehicles, and in particular relates to a composite floor for a rail passenger vehicle, a preparation method thereof, and a rail passenger vehicle. Background Art
[0003] Ordinary rail passenger car floors are mostly made of plywood as the main material, with hardwood ribs used as support at the bottom of the floor. Mechanical connections are used between the floor, ribs, and car body frame. As railways enter the era of high-speed EMUs, higher requirements are placed on the floor structure. To meet the requirements of passenger comfort, the floor must have good vibration damping and sound insulation performance. In addition, in terms of safety, it must also meet flame retardant performance requirements.
[0004] CN202046316U discloses an existing floor structure as shown in Figure 1. The floor structure uses aluminum honeycomb composite panels, with aluminum honeycomb material in the middle. Aluminum plates are provided on the upper and lower surfaces of the aluminum honeycomb material, and the aluminum plates and the aluminum honeycomb material are connected by adhesive. The floor design adopts a structure with bonded rubber support blocks, and foam material is bonded between the support blocks for heat insulation and noise absorption under the vehicle. The floor is covered with flame-retardant floor cloth, and an aluminum profile edge is provided between the two floor panels. The floor panels are directly connected by screws. This floor structure can improve fire resistance and reduce noise inside the vehicle, but its composition is relatively complex, which is not conducive to achieving the requirements of low cost and lightweight, and there are certain problems in practical application.
[0005] Summary of the Invention
[0006] In view of this, the object of the present invention is to provide a composite floor for a railway passenger car, a preparation method thereof, and a railway passenger car. The composite floor has the characteristics of high strength, impact resistance, noise reduction, lightness, etc., and has excellent comprehensive performance.
[0007] To achieve this object, the present invention adopts the following technical solutions:
[0008] In a first aspect, the present invention provides a composite floor for a railway passenger car, comprising, in sequence, a first carbon fiber composite board, a reinforcement board, a second carbon fiber composite board, and a plastic board.
[0009] Preferably, the first carbon fiber composite plate and the second carbon fiber composite plate are independently made of modified carbon fiber reinforced thermoplastic resin materials.
[0010] Preferably, polar groups exist on the surface of the modified carbon fiber.
[0011] Preferably, the content of the modified carbon fiber in the first carbon fiber composite plate and the second carbon fiber composite plate is independently 10 to 30 wt%.
[0012] Preferably, the first carbon fiber composite plate and the second carbon fiber composite plate independently include a first thermoplastic resin layer, a modified carbon fiber layer and a second thermoplastic resin layer.
[0013] Preferably, the reinforcement board is a foam board and / or a honeycomb board.
[0014] Preferably, the foam board is made of polymer foam material.
[0015] Preferably, the polymer foam material is selected from any one or more of polyimide foam, polyurethane foam, polypropylene foam or polyethylene foam.
[0016] Preferably, the foam plate is made of aluminum honeycomb reinforced polymer foam material and / or carbon fiber reinforced polymer foam material.
[0017] Preferably, the thickness of the first carbon fiber composite plate is 6 to 12 mm.
[0018] Preferably, the second carbon fiber composite plate has a thickness of 6 to 12 mm.
[0019] Preferably, the thickness of the reinforcement plate is 16 to 30 mm.
[0020] Preferably, the thickness of the plastic plate is 8 to 16 mm.
[0021] In a second aspect, the present invention provides a method for preparing the above-mentioned composite floor, comprising the following steps:
[0022] (1) mixing a thermoplastic resin material with a modified carbon fiber having a polar group on its surface, and subjecting the obtained mixture to a hot pressing process to obtain a first carbon fiber composite plate and a second carbon fiber composite plate;
[0023] (2) The first carbon fiber composite plate, the reinforcement plate, the second carbon fiber composite plate and the plastic plate are stacked in sequence according to the layering order, and after hot pressing treatment, a composite floor is obtained.
[0024] Preferably, the ply laying sequence is a 0° / 90° alternating ply laying sequence.
[0025] In a third aspect, the present invention provides a railway passenger car comprising the composite floor involved in the above technical solution.
[0026] Preferably, each of the composite floors is glued together by a counter-rotationally symmetrical single bevel, and the angle between the bevel and the horizontal direction is 30 to 60 degrees.
[0027] Preferably, the plastic plate in the composite floor is connected to the upper surface of the vehicle body chassis of the railway vehicle by means of an adhesive resin.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] The present invention provides a composite floor, which is obtained by sequentially laminating a first carbon fiber composite sheet, a reinforcement sheet, a second carbon fiber composite sheet, and a plastic sheet. The reinforcement sheet provides support, filling, and shock absorption. The first and second carbon fiber composite sheets are disposed on the upper and lower sides of the reinforcement sheet, respectively. The first and second carbon fiber composite sheets are made of a thermoplastic resin material reinforced with modified carbon fibers. Polar groups on the surface of the modified carbon fibers enhance the interfacial bonding between the carbon fibers and the thermoplastic resin, resulting in a 12-25% increase in tensile strength and a 10-20% increase in interlaminar shear strength compared to unmodified carbon fiber composite sheets. Furthermore, the carbon fibers and thermoplastic resin in the first and second carbon fiber composite sheets effectively enhance the mechanical strength and noise reduction of the composite floor. The presence of the thermoplastic resin also provides a certain degree of shock absorption. A plastic sheet is further disposed below the second carbon fiber sheet, contacting the upper surface of the vehicle underframe to further provide shock absorption. The composite floor provided by the present invention has a simple structure and low cost, meeting the demand for lightweight vehicles. Research has shown that compared with the existing traditional rail passenger car floor structure (i.e., the floor shown in Figure 1), the composite floor provided by the present invention can reduce the car body weight by 8-15%, increase the sound insulation by 3-10dB, and improve the impact resistance by 10-15%. The structure of the composite floor avoids the main frequency range of car body vibration during installation, meets the vibration reduction requirements, and reduces the radiated sound power by 2-8dBA. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 is a schematic structural diagram of an existing floor;
[0031] Among them, 1 is the floor cloth; 2 is the adhesive; 3 is the aluminum profile frame; 4 is the screw; 5 is the aluminum honeycomb; 6 is the melamine foam board; 7 is the fireproof fiber felt; 8 is the rubber support block; 9 is the vehicle body frame; 10 is the upper surface of the vehicle body frame;
[0032] FIG2 is a schematic structural diagram of a composite floor provided by the present invention;
[0033] Reference numeral 9 denotes a vehicle body underframe; 10 denotes an upper surface of the vehicle body underframe; 11a denotes an integrated composite material floor panel I; 11b denotes an integrated composite material floor panel II; 12 denotes an upper carbon fiber composite panel; 13 denotes a foam panel; 14 denotes a corrugated plastic panel; 15 denotes an inclined surface II; 16 denotes an inclined surface I; 17 denotes an adhesive resin; and 18 denotes a lower carbon fiber composite panel. DETAILED DESCRIPTION
[0034] The following will clearly and completely describe the technical solutions of the present invention in conjunction with the embodiments of the present invention. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. All other embodiments derived by persons of ordinary skill in the art based on the embodiments of the present invention without inventive effort are intended to fall within the scope of protection of the present invention.
[0035] In view of the complex structure of existing flooring, which cannot simultaneously meet the requirements of fire protection, noise reduction, vibration reduction, low cost and lightweight, the present invention provides a composite flooring, which comprises a first carbon fiber composite plate, a reinforcement plate, a second carbon fiber composite plate and a plastic plate. The thickness of each plate can be selected by those skilled in the art according to actual needs. In the present invention, the thickness of the first carbon fiber composite plate is 6 to 12 mm, which can be 6 mm, 7 mm, 8 mm, 9 mm, 10 mm, 11 mm or 12 mm; the thickness of the second carbon fiber composite plate is 6 to 12 mm, which can be 6 mm, 7 mm, 8 mm, 9 mm, 10 mm, 11 mm or 12 mm; the thickness of the reinforcement plate is 16 to 30 mm, which can be 16 mm, 18 mm, 20 mm, 22 mm, 24 mm, 26 mm, 28 mm or 30 mm; and the thickness of the plastic plate is 8 to 16 mm, which can be 8 mm, 9 mm, 10 mm, 11 mm, 12 mm, 13 mm, 14 mm, 15 mm or 16 mm. The above point values are merely enumerated and are not limited thereto. Other point values within the above numerical range are applicable and will not be detailed here.
[0036] In the present invention, the first carbon fiber composite plate and the second carbon fiber composite plate are independently modified carbon fiber reinforced thermoplastic resin materials, and polar groups are present on the surface of the modified carbon fibers, and the polar groups are hydroxyl groups, carboxyl groups, amino groups, amide groups, or acid groups well known to those skilled in the art. In the modified carbon fiber reinforced thermoplastic resin material, if the modified carbon fibers are used as reinforcements, too high a content will increase the cost and will not significantly improve the performance of the floor. If the content is too low, the reinforcing effect will not be achieved. Therefore, in some embodiments of the present invention, the content of the modified carbon fibers in the first carbon fiber composite plate and the second carbon fiber composite plate is independently 10 to 30 wt%, preferably 13 to 25 wt%, and more preferably 15 to 20 wt%. The present invention has no particular restrictions on the source of the carbon fibers, and any commercially available products can be used, such as T300 carbon fiber, T400 carbon fiber, or M30 carbon fiber. The thermoplastic resin material can be selected from any one or more of polyethylene, polypropylene, nylon PA6, nylon PA66, or polyetheretherketone, all of which are commercially available products. In some embodiments of the present invention, the surface modification of carbon fibers is achieved by some modifiers, such as any one or more of potassium permanganate, nitric acid, silane coupling agent or sizing agent can be selected, and the surface of the carbon fibers is provided with corresponding polar groups by means of liquid phase oxidation method or surface coating modification method. When the modifier is potassium permanganate or nitric acid, the liquid phase oxidation method is generally used; when the modifier is potassium permanganate or nitric acid, the surface coating modification method is generally adopted. The liquid phase oxidation method or surface coating modification method can be carried out according to the technical means well known to those skilled in the art, and will not be described in detail here. The present invention compounds carbon fibers and thermoplastic resins to prepare carbon fiber composite boards, which can effectively enhance the mechanical strength and anti-noise effect of the composite floor. At the same time, the presence of the thermoplastic resin gives the carbon fiber composite board a certain shock-absorbing effect.
[0037] In some embodiments of the present invention, the first carbon fiber composite plate and the second carbon fiber composite plate independently include a first thermoplastic resin layer, a modified carbon fiber layer, and a second thermoplastic resin layer. The thickness of the first thermoplastic resin layer, the modified carbon fiber layer, and the second thermoplastic resin layer are independently 2 to 4 mm, specifically 2 mm, 2.5 mm, 3 mm, 3.5 mm, or 4 mm. It should be noted that the present invention designs the first carbon fiber composite plate and the second carbon fiber composite plate into a "sandwich" structure, which can further enhance the performance of the first carbon fiber composite plate and the second carbon fiber composite plate, thereby improving the overall performance of the composite floor.
[0038] In the present invention, the point values listed above are merely for illustrative purposes and are not limited thereto. Other point values within the numerical range are applicable, and to avoid complexity, they will not be described one by one.
[0039] In the present invention, the reinforcing plate is a foam plate and / or a honeycomb plate, that is, the reinforcing plate can be a separate foam plate or a separate honeycomb plate, or a combination of a foam plate and a honeycomb plate. There is no particular restriction on the order of the upper and lower positions of the foam plate and the honeycomb plate. The foam plate is made of a polymer foam material, which can be a commonly available commercial product. Specifically, it can be selected from any one or more of polyimide foam, polyurethane foam, polypropylene foam, or polyethylene foam. As a preferred technical solution, the present invention uses aluminum honeycomb reinforced polymer foam material and / or carbon fiber reinforced polymer foam material to prepare the foam plate. The foam plate can achieve sound insulation and heat insulation effects, and the fireproof foam plate can also have a fireproof function. The present invention has no particular restrictions on the honeycomb plate, and any one familiar to those skilled in the art can be used. Specifically, it can be selected from aramid honeycomb plates and / or aluminum honeycomb plates. The aramid honeycomb plates and / or aluminum honeycomb plates can be commonly available commercial products. The honeycomb plate can achieve effective sound insulation, heat insulation, and fireproof effects.
[0040] In the present invention, the plastic plate is made of thermoplastic resin, which is preferably flame-retardant thermoplastic resin as described in the above technical solution, so as to have excellent flame retardant properties while providing shock absorption. In some embodiments of the present invention, the plastic plate is preferably a corrugated structure.
[0041] The composite floor provided by the present invention has a simple structure and low cost, meeting the demand for lightweight vehicle bodies. Research has shown that compared with existing conventional rail passenger car floor structures (i.e., the floor structure shown in Figure 1), the composite floor provided by the present invention can reduce vehicle body weight by 8-15%, improve sound insulation by 3-10dB, and enhance impact resistance by 10-15%. The composite floor structure avoids the main vibration frequency range of the vehicle body, achieving the required vibration reduction range, and reduces radiated sound power by 2-8dBA.
[0042] The above-mentioned composite flooring is prepared in a simple manner. After placing the individual panels according to their positions and a certain plying order, the laminate is laminated. In some embodiments of the present invention, the composite flooring is prepared according to the following method:
[0043] (1) mixing a thermoplastic resin material with a modified carbon fiber having a polar group on its surface, and subjecting the obtained mixture to a hot pressing process to obtain a first carbon fiber composite plate and a second carbon fiber composite plate;
[0044] (2) The first carbon fiber composite plate, the reinforcement plate, the second carbon fiber composite plate and the plastic plate are stacked in sequence according to the layering order, and after hot pressing treatment, a composite floor is obtained.
[0045] According to the present invention, a thermoplastic resin material is first mixed with a modified carbon fiber having a polar group on its surface, and the resulting mixture is hot-pressed to obtain a first carbon fiber composite plate and a second carbon fiber composite plate. The temperature of the hot-pressing treatment is 200-280°C, preferably 240-260°C; the pressure is 4-10 MPa, preferably 6-80 MPa; and the time is 5-15 min, preferably 5-10 min. In some embodiments of the present invention, the modified carbon fiber is prepared by modifying carbon fiber to form modified carbon fiber, and the carbon fiber is preferably chopped carbon fiber. The modification treatment can be performed using a variety of modifiers to treat the carbon fiber, such as specifically including the following steps: cutting the carbon fiber into chopped carbon fiber (SCF), placing it in an acetone solution, and reflux treatment at 80-100°C for 10-15 hours to remove the sizing agent on the surface of the carbon fiber to obtain a carbon fiber fabric (CFF). It is then washed thoroughly with ethanol or deionized water, preferably ethanol, and vacuum dried at 100-120°C for 12-20 hours. Use acetone to reflux at 80-100°C for 10-15h to treat CFF to remove the surface slurry. Take out the CFF treated with acetone, wash it with ethanol or deionized water, preferably deionized water, 2-3 times, and finally put it into a vacuum drying oven at 100-120°C for 12-20h, take it out and place it in a dryer filled with desiccant for standby use. Add the desized and dried carbon fiber and liquid-phase oxidant concentrated nitric acid into the container, reflux at 100-150°C for 10-15h, take out the oxidized carbon fiber, and wash it thoroughly with deionized water until the pH is 7. Then immerse the desized carbon fiber in the sizing agent for 5-10min, take it out and air-dry it at room temperature for 2-5h, and then dry it in a vacuum oven for 2-5h for standby use. In other embodiments of the present invention, the modified carbon fiber is treated with a silane coupling agent, preferably a silane coupling agent KH570, specifically comprising the following steps: 1) preparing a mixed solution of anhydrous ethanol and water, preferably anhydrous ethanol and water in a volume ratio of 9:1, adjusting the pH to 5 with dilute hydrochloric acid, adding the silane coupling agent KH570 to the mixed solution, and ultrasonically treating for 5 to 10 minutes to prepare a KH570 solution with a concentration of 1 to 3 wt%; 2) taking the carbon fiber treated with nitric acid and adding it to the silane solution, ultrasonically treating it for 10 to 20 minutes, and standing it at room temperature for 12 to 20 hours. Then, take out the carbon fiber and place it in a vacuum drying oven and react it at 100 to 120°C for 10 to 30 minutes. Finally, place it in a vacuum drying oven and dry it at 80 to 100°C for 12 to 20 hours for standby use.
[0046] After obtaining the modified carbon fibers, the modified carbon fibers can be mixed with a thermoplastic resin, or the modified carbon fibers and a thermoplastic resin film can be laminated to form a modified carbon fiber reinforced thermoplastic resin prepreg. In some embodiments of the present invention, the modified carbon fiber reinforced thermoplastic resin prepreg and carbon fiber composite plate are preferably prepared by a compression molding process on a flat vulcanizer. First, a modified carbon fiber / thermoplastic resin prepreg is prepared according to a sandwich structure, that is, the upper and lower layers are thermoplastic resin layers, and the middle layer is a modified carbon fiber layer. It is molded at high temperature, and the molding parameters are: molding temperature 240°C, pressure 6MPa, molding time 5min. The pressed prepreg is naturally cooled to room temperature in the mold and then taken out. Finally, according to needs, multiple pieces (specifically 6 to 10 pieces, preferably 6 to 8 pieces) of prepreg are taken out and the first carbon fiber composite plate is molded on a flat vulcanizer in a ply order of [0° / 90° / 0° / 90° alternating]. Multiple pieces (specifically 4 to 8 pieces, preferably 6 to 8 pieces) of prepreg are taken out and the second carbon fiber composite plate is molded on a flat vulcanizer in a ply order of [0° / 90° / 0° / 90° alternating]. The molding parameters refer to the above settings.
[0047] In the present invention, the reinforcing plate (i.e., foam plate and / or honeycomb plate) and plastic plate can be purchased as finished products on the market or prepared by themselves. In the present invention, the foam plate can be obtained by hot pressing a foam material. Among them, the foam plate made of a polymer foam material reinforced with aluminum honeycomb and / or a polymer foam material reinforced with carbon fiber, the present invention preferably disperses the aluminum honeycomb and / or carbon fiber in the polymer foam material, makes it uniformly dispersed, and then prepares the foam plate by hot pressing. The plastic plate can be made into a resin film after a certain treatment of a thermoplastic resin, and then hot pressed to prepare a plastic plate, and then further prepared into a corrugated plastic plate according to the corrugated plate manufacturing method. The above-mentioned hot pressing is preferably carried out on a flat vulcanizer. The temperature, time and pressure of the hot pressing can be set according to the parameters commonly used by those skilled in the art.
[0048] According to the present invention, after obtaining a first carbon fiber composite sheet, a second carbon fiber composite sheet, a reinforcing sheet, and a plastic sheet, the first carbon fiber composite sheet, the reinforcing sheet, the second carbon fiber composite sheet, and the plastic sheet are stacked in a plying order and subjected to hot pressing to obtain a composite floor. The plying order is preferably a 0° / 90° alternating plying order. The hot pressing temperature is 200-280°C, preferably 240-260°C; the pressure is 8-20 MPa, preferably 10-16 MPa; and the time is 5-15 minutes, preferably 6-10 minutes. In some embodiments of the present invention, after the hot pressing is completed, the composite floor is preferably formed by cold pressing at the same pressure for 5-10 minutes.
[0049] The structure of the formed composite floor is shown in Figure 2, where 9 is the vehicle body underframe; 10 is the upper surface of the vehicle body underframe; 11a is the integrated composite floor I; 11b is the integrated composite floor II; 12 is the first carbon fiber composite board; 13 is the foam board; 14 is the corrugated plastic board; 15 is the inclined surface II; 16 is the inclined surface I; 17 is the adhesive resin; and 18 is the second carbon fiber composite board.
[0050] The present invention also provides a railway passenger car comprising the composite flooring described in the above technical solution. It should be noted that the length of a single carriage in a railway passenger car is relatively long. During the preparation of the composite flooring, it is not convenient to directly prepare flooring of corresponding length. Therefore, individual composite floorings must be glued together. To avoid gaps caused by parallel gluing of individual composite floorings, each composite flooring is preferably glued together using a single, counter-rotationally symmetrical bevel. The angle between the bevel and the horizontal is preferably 30 to 60°, more preferably 30 to 50°, and even more preferably 35 to 45°. In some embodiments of the present invention, an ultra-high-speed water jet cutter is preferably used to cut the composite flooring into an integrated composite material flooring I (i.e., 11a in FIG. 2 ) and an integrated composite material flooring II (i.e., 11b in FIG. 2 ), each with a 45° angled surface at one end. The right end of 11a is 45° angled surface I, and the left end of 11b is 45° angled surface II. Bevel I and bevel II are anti-rotationally symmetrical. Bevel I of 11a and bevel II of 11b are surface treated separately. An adhesive resin is then applied to the overlapping bevels. The two floorings are bonded together at the overlapping location under a pressure of 2 to 5 MPa and then cured at room temperature for 2 to 5 hours. The surface treatment is mechanical, specifically, grinding or polishing.
[0051] In the present invention, the plastic plate of the composite floor and the upper surface of the vehicle body chassis of the railway vehicle can be connected by various means, such as mechanical connection or bonding, etc. In the present invention, the connection is preferably through adhesive resin.
[0052] The above-mentioned rail passenger car provided by the present invention meets the requirements of lightweight and low cost, and at the same time has certain fire prevention, noise reduction, shock absorption, flame retardancy and other properties, which is convenient for practical application.
[0053] In order to further illustrate the present invention, the following examples are provided for detailed description. The experimental raw materials used in the following examples of the present invention can be purchased from the market or prepared according to conventional methods well known to those skilled in the art. The T300 carbon fiber was purchased from the T series carbon fiber produced by Toray Industries, Japan, with the model number T300; the nylon PA66 FR was purchased from the Dartek series nylon 66 resin produced by DuPont in the United States, with the model number PA66 FR50; the aluminum honeycomb was purchased from Shanghai Gufeng Honeycomb Products Co., Ltd., with a specification of 1500*3000mm; the polyimide precursor powder was purchased from Qinyang Tianyi Chemical Co., Ltd.
[0054] Example 1
[0055] This embodiment provides a composite floor for a railway passenger car. Its structural schematic is shown in Figure 2 , where 9 represents the vehicle body underframe; 10 represents the upper surface of the vehicle body underframe; 11a represents integrated composite floor I; 11b represents integrated composite floor II; 12 represents a first carbon fiber composite board; 13 represents a foam board; 14 represents a corrugated plastic board; 15 represents inclined surface II; 16 represents inclined surface I; 17 represents adhesive resin; and 18 represents a second carbon fiber composite board. The specific preparation method is as follows:
[0056] (1) Cut T300 carbon fiber into 10cm long short carbon fiber (SCF), place it in acetone solution, and reflux it at 80℃ for 10h to remove the sizing agent on the surface of the carbon fiber. Then wash it thoroughly with ethanol and vacuum dry it at 100℃ for 12h. Use acetone to reflux at 80℃ for 10h to treat CFF to remove the sizing on its surface. Take out the CFF treated with acetone, wash it with deionized water 3 times, and finally put it into a vacuum drying oven at 100℃ for 12h, take it out and place it in a dryer filled with desiccant for later use. Add the desized and dried carbon fiber and liquid-phase oxidant concentrated nitric acid into the container, reflux it at 100℃ for 10h, take out the oxidized carbon fiber, and wash it thoroughly with deionized water until pH=7. Then immerse the desized carbon fiber in the sizing agent for 5min, take it out, air-dry it at room temperature for 2h, and then dry it in a vacuum oven for 2h for later use;
[0057] (2) Nylon PA66 FR was made into a resin film, and then molded on a flat vulcanizer to prepare a plastic plate. The molding parameters were: molding temperature 245°C, pressure 5 MPa, and molding time 2 min. Then, a corrugated plastic plate was prepared according to the corrugated plate manufacturing method.
[0058] (3) Carbon fiber prepreg and carbon fiber composite board are prepared by compression molding process on a flat vulcanizer. First, a sandwich structure is used to prepare CFF / PA66 FR prepreg, that is, the upper and lower layers are flame retardant nylon film PA66 FR, and the middle layer is carbon fiber CFF. The prepreg is compression molded at high temperature. The compression parameters are: compression temperature 240°C, pressure 6MPa, and compression time 5min. The pressed prepreg is naturally cooled to room temperature in the mold and then taken out. Finally, 8 pieces of the pressed prepreg are taken out and molded into a first carbon fiber composite board 12 on a flat vulcanizer in a layering order of [0° / 90° / 0° / 90° cycle]. 6 pieces of the prepreg are taken out and molded into a second carbon fiber composite board on a flat vulcanizer in a layering order of [0° / 90° / 0° / 90° cycle]. The compression parameters refer to the above settings.
[0059] (4) The SCF treated in step 1 was added to the polyimide precursor powder to uniformly disperse the SCF, and then molded on a flat vulcanizer to prepare a plastic plate. The molding parameters were: molding temperature 250°C, pressure 0.1 MPa, and molding time 6 min to prepare a foam plate with flame retardant properties.
[0060] (5) The first carbon fiber composite board, the foam board, the corrugated plastic board, and the second carbon fiber composite board are sequentially stacked and placed in a mold cavity of a flat-plate vulcanizer. The PA66 FR resin film can also be added between the boards. The boards are then placed in a flat-plate vulcanizer and molded again to prepare an integrated composite material floor. The molding parameters are: molding temperature 240° C., pressure 16 MPa, molding time 6 min, and finally cold pressing for 5 min under the same pressure to form the composite material floor.
[0061] (6) Using an ultra-high-speed water jet cutting machine, the integrated composite material floor for rail passenger cars is cut into an integrated composite material floor I and an integrated composite material floor II with a 45° angle bevel at one end as required, wherein the right end of the 11a is the 45° angle bevel I, and the left end of the 11b is the 45° angle bevel II, and the bevel I and the bevel II are anti-rotationally symmetrical. The bevel I of the floor 11a and the bevel II of the floor 11b are surface-treated (specifically, mechanically treated, such as grinding, polishing, etc.), and then adhesive resin is applied to the bevels of the overlapping area. The two floors coated with glue are bonded at the overlapping position under a pressure of 2MPa, and finally cured at room temperature for 2h to obtain the bonded composite floor.
[0062] Example 2
[0063] This embodiment provides a composite floor for a railway passenger car, the structural diagram of which is shown in FIG2 , and the preparation method is as follows:
[0064] (1) First, a mixed solution of anhydrous ethanol and water was prepared in a volume ratio of 9:1, and the pH was adjusted to 5 with dilute hydrochloric acid. The silane coupling agent KH570 was added to the mixed solution and ultrasonically treated for 5 minutes to prepare a KH570 solution with a concentration of 1 wt%; the carbon fiber treated with nitric acid was added to the silane solution and ultrasonically treated for 10 minutes. After standing at room temperature for 12 hours, the carbon fiber was taken out and placed in a vacuum drying oven at 100°C for reaction for 10 minutes, and finally placed in a vacuum drying oven at 80°C for drying for 12 hours for standby use;
[0065] (2) Nylon PA66 FR was made into a resin film, and then molded on a flat vulcanizer to prepare a plastic plate. The molding parameters were: molding temperature 245°C, pressure 5 MPa, and molding time 2 min. Then, a corrugated plastic plate was prepared according to the corrugated plate manufacturing method.
[0066] (3) Carbon fiber prepreg and carbon fiber composite board are prepared by compression molding process on a flat vulcanizer. First, a sandwich structure is used to prepare CFF / PA66 FR prepreg, that is, the upper and lower layers are flame retardant nylon film PA66 FR, and the middle layer is carbon fiber CFF. The prepreg is compression molded at high temperature. The compression parameters are: compression temperature 240°C, pressure 6MPa, and compression time 5min. The pressed prepreg is naturally cooled to room temperature in the mold and then taken out. Finally, 8 pieces of the pressed prepreg are taken out and molded into a first carbon fiber composite board 12 on a flat vulcanizer in a layering order of [0° / 90° / 0° / 90° cycle]. 6 pieces of the prepreg are taken out and molded into a second carbon fiber composite board on a flat vulcanizer in a layering order of [0° / 90° / 0° / 90° cycle]. The compression parameters refer to the above settings.
[0067] (4) Cut the aluminum honeycomb into 10 mm thick pieces as needed and place them in a flat mold cavity. Then, add the PA66 FR solution into the mold cavity so that the solution is dispersed in the various holes of the honeycomb. Heat it to 150°C for foaming. After foaming, treat it at 250°C for 1 hour to prepare a foam board.
[0068] (5) The first carbon fiber composite board, the foam board, the corrugated plastic board, and the second carbon fiber composite board are sequentially stacked and placed in a mold cavity of a flat-plate vulcanizer. The PA66 FR resin film can also be added between the boards. The boards are then placed in a flat-plate vulcanizer and molded again to prepare an integrated composite material floor. The molding parameters are: molding temperature 240° C., pressure 16 MPa, molding time 6 min, and finally cold pressing for 5 min under the same pressure to form the composite material floor.
[0069] (6) Using an ultra-high-speed water jet cutting machine, the integrated composite material floor for rail passenger cars is cut into an integrated composite material floor I and an integrated composite material floor II with a 45° angle bevel at one end as required, wherein the right end of the 11a is the 45° angle bevel I, and the left end of the 11b is the 45° angle bevel II, and the bevel I and the bevel II are anti-rotationally symmetrical. The bevel I of 11a and the bevel II of 11b are surface-treated (specifically, mechanically treated, such as grinding, polishing, etc.), and then adhesive resin is applied to the bevels of the overlapping area. The two floors coated with glue are bonded at the overlapping position under a pressure of 2MPa, and finally cured at room temperature for 2h to obtain the bonded composite floor.
[0070] The composite floorings obtained in Examples 1 and 2 were tested for quality, sound insulation, impact resistance, and shock absorption using standard testing methods for railway passenger car floors. The results showed that, compared to conventional railway passenger car floors (the floor structure shown in FIG1 ), the composite flooring provided in Example 1 of the present invention reduced vehicle body mass by 12%, increased sound insulation by 6 dB, improved impact resistance by 12%, and reduced radiated sound power by 5 dBA. The composite flooring provided in Example 2 of the present invention also reduced vehicle body mass by 12%, increased sound insulation by 5 dB, and improved impact resistance by 10%. The composite flooring's structure avoids the dominant vibration frequency range of the vehicle body, meeting the required vibration damping range, and reduced radiated sound power by 4 dBA.
[0071] The above description of the disclosed embodiments will enable one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be readily apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention is not limited to the embodiments shown herein but is to be construed in the widest manner consistent with the principles and novel features disclosed herein.
Claims
1. A composite floor for a railway passenger car, characterized in that: It includes a first carbon fiber composite plate, a reinforcement plate, a second carbon fiber composite plate and a plastic plate in sequence; The first carbon fiber composite plate and the second carbon fiber composite plate are independently thermoplastic resin materials reinforced with modified carbon fibers; Polar groups exist on the surface of the modified carbon fiber.
2. The composite floor according to claim 1, characterized in that: The content of the modified carbon fiber in the first carbon fiber composite plate and the second carbon fiber composite plate is independently 10 to 30 wt %.
3. The composite floor according to claim 1, characterized in that: The first carbon fiber composite plate and the second carbon fiber composite plate independently include a first thermoplastic resin layer, a modified carbon fiber layer and a second thermoplastic resin layer.
4. The composite flooring according to claim 1, characterized in that: The reinforcement board is a foam board and / or a honeycomb board.
5. The composite floor according to claim 4, characterized in that: The foam board is made of polymer foam material; The polymer foam material is selected from any one or more of polyimide foam, polyurethane foam, polypropylene foam or polyethylene foam.
6. The composite flooring according to claim 5, characterized in that: The foam plate is made of aluminum honeycomb reinforced polymer foam material and / or carbon fiber reinforced polymer foam material.
7. The composite flooring according to claim 1, characterized in that: The thickness of the first carbon fiber composite plate is 6 to 12 mm; The thickness of the second carbon fiber composite plate is 6 to 12 mm; The thickness of the reinforcing plate is 16 to 30 mm; The thickness of the plastic plate is 8-16 mm.
8. The method for preparing a composite floor according to any one of claims 1 to 7, characterized in that: The following steps are involved: (1) mixing a thermoplastic resin material with a modified carbon fiber having a polar group on the surface, and subjecting the obtained mixture to a hot pressing treatment to obtain a first carbon fiber composite plate and a second carbon fiber composite plate; (2) Lay the first carbon fiber composite plate, the reinforcement plate, the second carbon fiber composite plate and the plastic plate in a manner as follows: The layers are stacked in sequence and after heat pressing, a composite floor is obtained.
9. The preparation method according to claim 8, characterized in that: The ply laying sequence is a 0° / 90° alternating ply laying sequence.
10. A rail passenger car, characterized in that: A composite floor comprising any one of claims 1 to 7 or a composite floor prepared by the preparation method according to claim 8 or 9; Each of the composite floors is glued by a counter-rotationally symmetrical single bevel, and the angle between the bevel and the horizontal direction is 30 to 60 degrees; The plastic plate in the composite floor is connected to the upper surface of the vehicle body underframe of the rail passenger vehicle through an adhesive resin.
Citation Information
Patent Citations
Preparation method of carbon fiber modified phenolic resin and phenolic moulding plastic
CN105754056A
Composite floor for rail transit vehicle
CN108909126A
Composite floor for railway passenger car, preparation method of composite floor and railway passenger car
CN116619851A
Based on fire -retardant rail transit car of a foaming technology preparation interior trim floor
CN208484332U
Surface coating method for carbon fiber and surface-coated carbon fiber
JP1991113075A