Method for repairing lithium iron phosphate material based on carbon dioxide supercritical reaction

The carbon dioxide supercritical reaction method is used to supplement lithium, iron and phosphorus elements in waste lithium iron phosphate batteries, which solves the problems of cumbersome recycling process and high cost in the existing technology, realizes low-energy consumption and environmentally friendly lithium iron phosphate material repair, and improves improve recovery efficiency and purity.

CN118851133APending Publication Date: 2024-10-29INFORMATION COMM COMPANY STATE GRID SHANDONG ELECTRIC POWER +2
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202411108215.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

When recycling used lithium iron phosphate batteries, the existing technology cannot achieve full component recovery, and the conventional regeneration process has cumbersome steps, high equipment requirements, high costs, and may produce secondary pollution.

Method used

The carbon dioxide supercritical reaction method is used to repair the lithium iron phosphate material. By heating the reaction in the carbon dioxide supercritical fluid, hydrocarbon-based organic matter is used as a reducing agent to supplement lithium, iron and phosphorus elements, and a constant temperature reaction is performed to repair the lithium iron phosphate material.

Benefits of technology

It achieves simple process operation, low energy consumption, no secondary pollutants, reduces recycling costs, and the repaired materials have high purity and the process is controllable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118851133A_ABST
    Figure CN118851133A_ABST
Patent Text Reader

Abstract

The invention discloses a method for repairing a lithium iron phosphate material based on a carbon dioxide supercritical reaction, which comprises the following steps: analyzing the lithium iron phosphate material to be repaired, and calculating to obtain the proportion of missing elements in the lithium iron phosphate material to be repaired; uniformly mixing the lithium iron phosphate material to be repaired with a lithium source, an iron source and a phosphorus source which need to be supplemented; putting the uniformly mixed mixture into a reaction kettle, and adding a hydrocarbon-based organic matter into the reaction kettle; sealing the reaction kettle, and filling carbon dioxide to obtain carbon dioxide supercritical fluid; heating the mixture, and reacting at a constant temperature until the reaction is complete; and cooling the reaction kettle, reducing pressure and recovering carbon dioxide to obtain the repaired lithium iron phosphate material. According to the repairing method of the lithium iron phosphate material disclosed by the invention, the lithium iron phosphate material is re-synthesized by adopting a carbon dioxide supercritical reduction repairing method, and the reduction repairing reaction is promoted by the heat effect under a carbon dioxide supercritical fluid high-pressure medium.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of lithium ion battery positive electrode materials, and in particular to a method for repairing lithium iron phosphate materials based on supercritical carbon dioxide reaction. Background Art

[0002] The lithium-ion battery industry has developed rapidly and is widely used in portable electronic devices such as mobile phones, electric vehicles and renewable energy storage. Among them, lithium-ion batteries using lithium iron phosphate (LiFePO4) as the positive electrode material have a stable structure and high theoretical capacity (170mAh g -1 ), good cycle performance, environmental friendliness, high safety factor and wide material sources, the output of LiFePO4 is growing rapidly, and accordingly, the number of waste lithium iron phosphate batteries is growing rapidly. Therefore, the recycling of waste batteries has become an important problem facing the current society.

[0003] At present, there are two main treatment methods for the recovery of lithium iron phosphate: hydrometallurgy and pyrometallurgy. The lithium, iron and other metals are recycled and reused. Because of its simple operation process and easy industrialization, many scholars have carried out relevant research, but this process cannot recover all components of waste lithium iron phosphate. For environmental protection and resource utilization, repairing the failed lithium iron phosphate positive electrode material through direct regeneration technology is one of the effective strategies for recycling waste batteries. Specifically, by reconstructing the failed and lithium-poor lithium iron phosphate crystals, and by replenishing lithium and repairing the lattice distortion of the recovered positive electrode material, regular olivine-type lithium iron phosphate crystals are re-formed. In the prior art, wet leaching is performed, and then the required raw materials (such as lithium, iron elements, reducing agents, etc.) are added thereto, and then the lithium iron phosphate material is re-synthesized through calcination or ball milling. This method is relatively cumbersome, has high equipment requirements, and has high recovery costs. Some methods have high calcination temperatures, resulting in high recovery costs for waste lithium iron phosphate. Summary of the invention

[0004] The purpose of the present invention is to provide a method for repairing lithium iron phosphate, a positive electrode material of waste lithium batteries, by using carbon dioxide supercritical fluid. The method has simple process operation, easy process control, low energy consumption, is environmentally friendly, and does not generate secondary pollutants.

[0005] A method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction, comprising the following steps:

[0006] Analyze the lithium iron phosphate material to be repaired to determine the ratio of lithium, iron and phosphorus in the lithium iron phosphate material to be repaired; calculate the ratio of missing elements in the lithium iron phosphate material to be repaired;

[0007] According to the ratio of the missing elements in the lithium iron phosphate material to be repaired, the lithium source, iron source and phosphorus source to be supplemented are calculated; the lithium iron phosphate material to be repaired and the lithium source, iron source and phosphorus source to be supplemented are mixed evenly;

[0008] The mixture is placed in a reactor, and hydrocarbon-based organic matter is added into the reactor; the reactor is sealed, and carbon dioxide is charged into the reactor to obtain a carbon dioxide supercritical fluid;

[0009] The mixture in the carbon dioxide supercritical fluid is heated and reacted at a constant temperature until the reaction is complete;

[0010] The reactor is cooled, the pressure is reduced to recover the carbon dioxide, and the repaired lithium iron phosphate material is obtained.

[0011] Furthermore, the ratios of lithium, iron and phosphorus in the lithium iron phosphate material to be repaired are determined by means of XRD and XPS.

[0012] Furthermore, the phosphorus source is selected from one or more of diammonium phosphate, lithium dihydrogen phosphate, and iron phosphate.

[0013] Preferably, the phosphorus source is selected from ammonium hydrogen phosphate and lithium dihydrogen phosphate.

[0014] Ammonium hydrogen phosphate and lithium dihydrogen phosphate have good reducing properties, which are conducive to the repair reaction.

[0015] Furthermore, the lithium source is selected from one or more of lithium nitrate, lithium halide, lithium carbonate and lithium hydroxide.

[0016] Furthermore, the iron source is selected from one or both of iron carbonate and iron acetate.

[0017] Furthermore, the ratio of the added volume of the hydrocarbon-based organic matter to the mass of the lithium iron phosphate to be repaired is (0.2-1) mL:10 g; the hydrocarbon-based organic matter is selected from one or more of ethanol, methanol, and isopropanol.

[0018] The addition of hydrocarbon-based organic matter as a reducing agent is to form a reaction environment for the reduction reaction.

[0019] Furthermore, the volume of the mixture is 1 / 2-3 / 4 of the volume of the reactor.

[0020] Furthermore, the pressure of the carbon dioxide supercritical fluid is maintained at 7.8-12 MPa.

[0021] Furthermore, the reaction temperature of the isothermal reaction is 30-80°C.

[0022] Furthermore, the reaction time of the isothermal reaction is 0.5-6h.

[0023] The repair method of lithium iron phosphate material disclosed in the present invention abandons the conventional water (solvent) heat and high-temperature calcination regeneration technology, and adopts the carbon dioxide supercritical reduction repair method to re-synthesize the lithium iron phosphate material. The thermal effect under the high-pressure medium of carbon dioxide supercritical fluid promotes the reduction repair reaction, avoids the use of solvents such as water, reduces the amount of reagents used, and at the same time, carbon dioxide can be recycled and reused, reducing the cost investment. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 is the XRD diagram of Example 1 before and after repair in the present invention;

[0025] Figure 2 This is the full XPS spectrum of Example 2 before and after repair in the present invention;

[0026] Figure 3 is the XPS graph of Li before and after repair in Example 2 of the present invention;

[0027] Figure 4 It is the XPS graph of Fe before and after repair in Example 2 of the present invention;

[0028] Figure 5 It is the XPS graph of P before and after repair in Example 2. DETAILED DESCRIPTION

[0029] In order to make the technical solution of the present invention clearer, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0030] Example 1

[0031] The waste lithium iron phosphate positive electrode sheets are recycled and crushed to make lithium iron phosphate materials to be repaired.

[0032] The physical phase, chemical state and element ratio of the lithium iron phosphate material to be repaired are determined by XRD, XPS and other methods. Figure 1 XRD shows that the phase of lithium iron phosphate changes after the batch cycle. Figure 1 After the middle cycle, some peaks become weaker or even disappear compared with the standard spectrum, for example, the peak around 24° disappears. Figure 3 , 4 The peak areas of the Li, Fe and P fine spectra before repair in and 5 are 462.1, 513.3 and 486.4 respectively, and the area ratio can be used to calculate that the ratio of Li:Fe:P on the surface of the sample to be repaired after cycling changes from 1:1:1 in theory to 0.9:1:0.95; therefore, 1 mol of the material to be repaired lacks approximately 0.1 mol of lithium and 0.05 mol of phosphorus.

[0033] Pour 100g of the analyzed lithium iron phosphate material to be repaired into a mortar, add the corresponding lithium carbonate (2.34g) and diammonium phosphate (3.62g) according to the deficiency of lithium, iron, phosphate, etc., grind and mix evenly, then add the mixed powder into a 100mL reactor, accounting for about 60% of the volume of the reactor, add 5mL of ethanol, and seal the reactor.

[0034] Inject carbon dioxide gas into the reactor to a pressure of 8 MPa to obtain carbon dioxide supercritical fluid; heat the reactor to a reaction temperature of 50°C, react for 1 hour, and then cool naturally.

[0035] The pressure is released and carbon dioxide is collected to directly obtain lithium iron phosphate material. The obtained lithium iron phosphate material is subjected to XRD detection. The results are as follows Figure 1 shown.

[0036] Example 2

[0037] The same batch of lithium iron phosphate as in Example 1 was used; the step of calculating the missing molar ratio of the elements was omitted.

[0038] Pour 100g of the analyzed lithium iron phosphate material to be repaired into a mortar, add the corresponding lithium dihydrogen phosphate (3.24g) and lithium carbonate (1.27g) according to the deficiency of lithium, iron, phosphate, etc., grind and mix evenly, then add the mixed powder into a 100mL reactor, accounting for about 60% of the volume of the reactor, add 5mL of ethanol, and seal the reactor.

[0039] Inject carbon dioxide gas into the reactor to a pressure of 8 MPa to obtain carbon dioxide supercritical fluid; heat the reactor to a reaction temperature of 60°C, react for 1 hour, and then cool naturally.

[0040] The pressure is released and carbon dioxide is collected to directly obtain lithium iron phosphate material. The obtained lithium iron phosphate material is subjected to XPS detection. The results are as follows Figure 2-Figure 5 shown.

[0041] in conclusion

[0042] like Figure 1 , Figure 2-5 As shown, in Example 1 and Example 2 of the present invention, the lithium iron phosphate material to be repaired and the lithium source and phosphorus source to be supplemented are mixed and placed in an autoclave, and carbon dioxide is introduced under pressure until liquefaction occurs to obtain a supercritical carbon dioxide fluid. In a supercritical carbon dioxide environment, under the action of the reducing agent ethanol, the lithium iron phosphate material to be repaired fully reacts with the lithium source and phosphorus source to be supplemented, and the lithium iron phosphate material is repaired. After the reaction is completed, carbon dioxide gas is collected under reduced pressure, and the repaired material is retained in the kettle. The physical phase purity of the repaired lithium iron phosphate material is high, and the repair effect is good. And the method process is easy to control, has low energy consumption, is environmentally friendly, and does not produce secondary pollutants.

[0043] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction, characterized in that: The following steps are involved: Analyze the lithium iron phosphate material to be repaired to determine the ratio of lithium, iron and phosphorus in the lithium iron phosphate material to be repaired; Calculate and obtain the ratio of missing elements in the lithium iron phosphate material to be repaired; According to the ratio of the missing elements in the lithium iron phosphate material to be repaired, the lithium source, iron source and phosphorus source to be supplemented are calculated; the lithium iron phosphate material to be repaired and the lithium source, iron source and phosphorus source to be supplemented are mixed evenly; The mixture is placed in a reactor, and hydrocarbon-based organic matter is added into the reactor; the reactor is sealed, and carbon dioxide is charged into the reactor to obtain a carbon dioxide supercritical fluid; The mixture in the carbon dioxide supercritical fluid is heated and reacted at a constant temperature until the reaction is complete; The reactor is cooled, the pressure is reduced to recover the carbon dioxide, and the repaired lithium iron phosphate material is obtained.

2. A method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The ratio of lithium, iron and phosphorus in the lithium iron phosphate material to be repaired is determined by XRD and XPS.

3. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The phosphorus source is selected from one or more of diammonium phosphate, lithium dihydrogen phosphate, and iron phosphate.

4. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The lithium source is selected from one or more of lithium nitrate, lithium halide, lithium carbonate and lithium hydroxide.

5. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The iron source is selected from one or both of iron carbonate and iron acetate.

6. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The ratio of the added volume of the hydrocarbon-based organic matter to the mass of the lithium iron phosphate to be repaired is 0.2-1:10; the hydrocarbon-based organic matter is selected from one or more of ethanol, methanol, and isopropanol.

7. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The volume of the mixture is 1 / 2-3 / 4 of the volume of the reactor.

8. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The pressure of the carbon dioxide supercritical fluid is maintained at 7.8-12 MPa.

9. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The reaction temperature of the isothermal reaction is 30-80°C.

10. The method for repairing lithium iron phosphate material based on supercritical carbon dioxide reaction according to claim 1, characterized in that: The reaction time of the isothermal reaction is 0.5-6h.

Citation Information

Cited By

  • Method for assisting recovery of state of health of lithium battery electrode by using helium-4 superfluid

    CN119253115A

  • A method for restoring the health status of lithium battery electrodes using helium-4 superfluid

    CN119253115B

  • Nano single crystal lithium iron phosphate as well as preparation method and application thereof

    CN119352158A

  • Regenerated lithium iron phosphate and repairing method and application thereof

    CN121341985A