Device for continuously producing coated asphalt through multi-stage oxidation and method for continuously producing coated asphalt

Through the multi-stage oxidation series continuous production of asphalt coated asphalt device, the problems of unstable product quality caused by intermittent reactions in the prior art are solved, and efficient large-scale continuous production is achieved, and production efficiency is improved. Oxygen concentration.

CN118956437APending Publication Date: 2024-11-15CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310545044.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing reactor process with stirrer has intermittent reactions, resulting in unstable product quality, small scale of the reactor, unable to achieve large-scale continuous production, and low production efficiency.

Method used

Design a multi-stage oxidation series continuous production of coated asphalt devices, including multi-stage coated asphalt reactors, gas-liquid micromixers, pressure differential control valves, liquid level control valves and coated asphalt stripping towers, through multi-stage oxidation reactions and stripping towers to achieve continuous operation and large-scale production.

Benefits of technology

The oxygen concentration of the oxidation reaction is improved, the reactor specifications are reduced, the product quality stability and large-scale continuous production are achieved, the production efficiency is improved, and energy consumption is saved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118956437A_ABST
    Figure CN118956437A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of petrochemical high-end carbon materials, and relates to a device for continuously producing coated asphalt through multistage oxidation and a method for continuously producing the coated asphalt. The device comprises a multi-stage coated asphalt reactor, a multi-stage gas-liquid micromixer, a multi-stage pressure difference control valve, a multi-stage liquid level control valve, a coated asphalt stripping tower and a stripping tower bottom pump, the gas-liquid micro-mixer is used for mixing raw materials and air, the coated asphalt reactor is used for oxidation reaction, liquid flowing out of the top of the previous-stage reactor enters the bottom of the next-stage coated asphalt reactor from the next-stage gas-liquid micro-mixer under the control of the liquid level control valve, and the pressure difference control valve is used for controlling the pressure difference between the tops of the adjacent coated asphalt reactors. According to the method for continuously producing the coated asphalt through multi-stage oxidation, continuous production of the device is achieved, raw materials which are not subjected to oxidation reaction are forcibly mixed with air again, the oxidation reaction effect is improved, oxidized liquid sequentially flows backwards, and energy consumption of the device is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of high-end carbon materials in petrochemical industry, and more specifically, relates to a device for continuously producing coated asphalt by multi-stage oxidation and a method for continuously producing coated asphalt. Background Art

[0002] As a highly aromatized specialty product, coated asphalt is mainly used for mixing with carbon materials to prepare various graphite carbon products. According to different application scenarios, it can be divided into binders, impregnants, and coating agents. It is widely used in the production of graphite electrodes, carbon blocks for metallurgical furnaces and aluminum electrolytic cells, prebaked anodes and anode pastes for electrolytic aluminum, and electrode pastes required for smelting ferroalloys and calcium carbide. For example: coated asphalt is used as a binder to produce electrodes and anode blocks for aluminum smelting. It has the advantages of low resistivity, good conductivity, low energy consumption, no slag, and long life; it is used to impregnate carbon products, which can greatly reduce the porosity of the products, increase the density of carbon materials, increase the mechanical strength of carbon materials, and improve the electrical and thermal conductivity of carbon materials; coated asphalt is used in the modification of negative electrode materials for lithium-ion batteries, and the cycle performance, rate performance, specific capacity, and life of negative electrode materials have been greatly improved.

[0003] In recent years, with the country's continuous layout in the field of new energy, the demand and production of lithium-ion battery vehicles have shown explosive growth. The current annual output has exceeded 1 million vehicles, and it is expected to reach 5 million vehicles / year in 2025. Driven by the development of new energy vehicles, the market demand for coated asphalt for the modification of negative electrode materials for lithium-ion batteries is huge. At present, the commonly used methods for preparing coated asphalt include chemical catalysis, vacuum flash evaporation, air oxidation, steam blowing, high-temperature thermal polymerization, hydrogenation, co-carbonization and back-matching. In comparison, the air oxidation method has a simple process and mild conditions, and can achieve the regulation of various industrial indicators of coated asphalt by optimizing raw materials and process conditions, becoming the most widely used large-scale production process. However, most coated asphalt reactors are intermittent reactors and cannot achieve continuous production.

[0004] Figure 1 This is a simplified process flow diagram of a conventional reactor with an agitator. As shown in the figure, the raw materials heated to a suitable temperature enter the reactor, and are oxidized with air in the reactor under the stirring of the agitator. The generated reaction tail gas flows out from the top of the reactor. After the reaction, it is stripped with superheated steam. After stripping, the stripping oil and gas flow out from the top of the reactor. After stripping, the coated asphalt is discharged from the bottom of the reactor and sent to the downstream buffer tank.

[0005] In conventional reactor processes with agitators, the reaction is intermittent, the stability of product quality cannot be guaranteed, and due to the influence of the type and manufacturing of the agitator, the reactor cannot be large-scale.

[0006] In summary, the conventional reactor process with a stirrer has the following shortcomings:

[0007] (1) Intermittent reaction and unstable product quality.

[0008] (2) The reactor is small and cannot be used for large-scale production.

[0009] (3) Intermittent operation, low production efficiency.

[0010] The present invention is based on large-scale, continuous and large-scale production, and multiple oxidation units are arranged to carry out multi-stage oxidation reactions to achieve continuous operation of the entire process flow, which can greatly improve production efficiency and realize large-scale and continuous production. Summary of the invention

[0011] The purpose of the present invention is to solve the problem that the current reactor with agitator is difficult to achieve stable product quality, continuous production and large-scale production. The present invention provides a multi-stage oxidation series continuous production device and a method for continuous production of coated asphalt.

[0012] In order to achieve the above-mentioned object, the present invention provides a device for continuously producing coated asphalt by multi-stage oxidation, the device comprising: a multi-stage coated asphalt reactor, a multi-stage gas-liquid micro-mixer, a multi-stage differential pressure control valve, a multi-stage liquid level control valve, a coated asphalt stripping tower and a stripping tower bottom pump;

[0013] The multi-stage coated asphalt reactor is composed of a first-stage coated asphalt reactor, a second-stage coated asphalt reactor, ... and an n-stage coated asphalt reactor connected in series, and each stage of the coated asphalt reactor is provided with a corresponding gas-liquid micro-mixer, a pressure difference control valve and a liquid level control valve; the gas-liquid micro-mixer is used to mix the raw material and air, the coated asphalt reactor is used for oxidation reaction, and the liquid flowing out of the top of the previous stage reactor enters the bottom of the next stage coated asphalt reactor through the next stage gas-liquid micro-mixer under the control of the liquid level control valve, and the pressure difference control valve is used to control the pressure difference at the top of adjacent coated asphalt reactors;

[0014] The n-th stage coated asphalt reactor is provided with a liquid outflow pipeline at the top of the n-th stage coated asphalt reactor, and the liquid outflow pipeline at the top of the n-th stage coated asphalt reactor is connected to the n-th stage liquid level control valve and then connected to the top of the coated asphalt stripping tower; the coated asphalt stripping tower is provided with a superheated steam feed pipeline at the bottom of the coated asphalt stripping tower, a discharge pipeline at the top of the coated asphalt stripping tower and a discharge pipeline at the bottom of the coated asphalt stripping tower, the discharge pipeline at the bottom of the coated asphalt stripping tower is connected to a bottom pump of the stripping tower, the bottom pump of the stripping tower is provided with a product discharge pipeline, and the discharge pipeline at the top of the coated asphalt stripping tower is connected to a gas treatment system.

[0015] The second aspect of the present invention provides a method for continuously producing coated asphalt by multi-stage oxidation. The method is carried out using the device for continuously producing coated asphalt by multi-stage oxidation, and comprises the following steps: the raw materials and air heated to the reaction temperature are mixed in a gas-liquid micro-mixer, and then enter a multi-stage coated asphalt reactor for oxidation reaction, and the reaction tail gas is connected in sequence through a pressure difference control valve to control the pressure difference at the top of adjacent coated asphalt reactors, so that the upper-stage liquid enters the bottom of the next-stage coated asphalt reactor from the next-stage gas-liquid micro-mixer under the control of the liquid level control valve;

[0016] The liquid phase at the top of the n-stage coated asphalt reactor enters the top of the coated asphalt stripping tower under the control of the n-stage liquid level control valve, and superheated steam is introduced into the bottom of the coated asphalt stripping tower. Under the stripping effect of the superheated steam, the coated asphalt at the bottom of the coated asphalt stripping tower is pumped out and pressurized by the bottom pump of the stripping tower. After cooling under the control of the liquid level at the bottom of the stripping tower, the asphalt is formed and then sent to the warehouse.

[0017] The present invention includes the following advantages:

[0018] (1) Multiple groups of oxidation reaction units are set up to carry out multi-stage oxidation reactions to increase the oxygen concentration of the oxidation reaction and reduce the specifications of the reactor, thereby facilitating continuous production of the device and improving production efficiency.

[0019] (2) A gas-liquid micro-mixer is provided to force the unoxidized raw materials to be mixed with air again to improve the oxidation reaction effect.

[0020] (3) A coated asphalt stripping tower is set up, and superheated steam is used for stripping at the bottom of the tower to ensure the quality of the coated asphalt product.

[0021] (4) The gases at the top of the multi-stage oxidation reactors are connected in sequence through pressure difference control valves. By controlling the pressure difference between the tops of two adjacent reactors, the oxidized liquid flows backward in sequence, saving energy consumption of the device.

[0022] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The above and other objects, features and advantages of the present invention will become more apparent through a more detailed description of exemplary embodiments of the present invention in conjunction with the accompanying drawings, wherein like reference numerals generally represent like components throughout the exemplary embodiments of the present invention.

[0024] Figure 1 This is a schematic diagram of the production process flow of coated asphalt in a conventional reactor with an agitator.

[0025] Figure 2 The present invention provides a schematic diagram of the process flow of a process for continuously producing coated asphalt through a multi-stage oxidation reaction.

[0026] Reference numerals

[0027] Equipment: coated asphalt reactor R1, R2...Rn; gas-liquid micro-mixer M1, M2...Mn; multi-stage differential pressure control valve D1, D2...Dn; multi-stage liquid level control valve L1, L2...Ln; coated asphalt stripping tower C; stripping tower bottom pump P; agitator J; anti-backmixing sieve plate N; chimney tower plate oil collecting box X; stripping tower plate B; feed distributor S.

[0028] Logistics: 1 raw materials; 2 air; 3 superheated steam; 4 reaction tail gas; 5 stripping tail gas; 6 mixed tail gas; 7 coated asphalt, 8 fuel gas, liquid flowing out of the top of the reactor 9, 10, 11, 12, ...n+8. DETAILED DESCRIPTION

[0029] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to make the present invention more thorough and complete, and to fully convey the scope of the present invention to those skilled in the art.

[0030] The first aspect of the present invention provides a device for continuously producing coated asphalt by multi-stage oxidation, the device comprising: a multi-stage coated asphalt reactor R1, R2...Rn, a multi-stage gas-liquid micro-mixer M1, M2...Mn, a multi-stage differential pressure control valve D1, D2...Dn, a multi-stage liquid level control valve L1, L2...Ln, a coated asphalt stripping tower C and a stripping tower bottom pump P;

[0031] The multi-stage coated asphalt reactors R1, R2...Rn are composed of a first-stage coated asphalt reactor R1, a second-stage coated asphalt reactor R2... and an nth-stage coated asphalt reactor Rn connected in series, and each stage of the coated asphalt reactor is provided with a corresponding gas-liquid micro-mixer, a pressure difference control valve and a liquid level control valve; the gas-liquid micro-mixer is used to mix the raw material and air, the coated asphalt reactor is used for oxidation reaction, and the liquid flowing out of the top of the previous stage reactor enters the bottom of the next stage coated asphalt reactor through the next stage gas-liquid micro-mixer under the control of the liquid level control valve, and the pressure difference control valve is used to control the pressure difference at the top of adjacent coated asphalt reactors;

[0032] The n-th stage coated asphalt reactor Rn is provided with a liquid outflow pipeline at the top of the n-th stage coated asphalt reactor, and the liquid outflow pipeline at the top of the n-th stage coated asphalt reactor is connected to the n-th stage liquid level control valve Ln and then connected to the top of the coated asphalt stripping tower C; the coated asphalt stripping tower C is provided with a superheated steam feed pipeline at the bottom of the coated asphalt stripping tower, a discharge pipeline at the top of the coated asphalt stripping tower and a discharge pipeline at the bottom of the coated asphalt stripping tower, the discharge pipeline at the bottom of the coated asphalt stripping tower is connected to a stripping tower bottom pump P, the stripping tower bottom pump P is provided with a product discharge pipeline, and the discharge pipeline at the top of the coated asphalt stripping tower is connected to a gas treatment system.

[0033] In the present invention, raw materials suitable for the production of coated asphalt are passed through a multi-stage series-connected air raw material micro-mixer and an oxidation reactor to reach the required oxygen concentration and oxidation time, thereby realizing the continuous production of coated asphalt. The light oil and gas in the coated asphalt are then stripped by steam through a coated asphalt stripping tower to produce a qualified coated asphalt product.

[0034] In the present invention, the multi-stage oxidation reaction is composed of a plurality of oxidation units, each of which includes processes such as gas-liquid micro-mixing of raw materials and air, oxidation of raw materials, and gas-liquid separation. The raw materials heated to the reaction temperature are fully mixed with a certain proportion of air in the first-stage gas-liquid micro-mixer, enter the first-stage oxidation reactor provided with an anti-backmixing sieve plate and flow upward in a plug flow manner, and partial oxidation of the raw materials is achieved through a certain residence time, and then enter the gas-liquid separation section at the top of the reactor through the chimney-type tower plate, and the separated gas is self-pressurized to the gas treatment system, and the separated liquid is self-pressurized to the secondary oxidation unit, and so on. The light oil and gas stripped out of the stripping tower are also self-pressurized to the gas treatment system.

[0035] According to the present invention, preferably, the first-stage gas-liquid micro-mixer M1 is provided with a first-stage gas-liquid micro-mixer raw material feed pipeline, a first-stage gas-liquid micro-mixer air feed pipeline and a first-stage gas-liquid micro-mixer discharge pipeline, the first-stage gas-liquid micro-mixer discharge pipeline is connected to the bottom of the first-stage coated asphalt reactor R1, the first-stage coated asphalt reactor R1 is provided with a first-stage coated asphalt reactor fuel gas feed pipeline, a first-stage coated asphalt reactor top gas outflow pipeline and a first-stage coated asphalt reactor top liquid outflow pipeline, the first-stage coated asphalt reactor top gas outflow pipeline is provided with a first-stage pressure difference control valve D1, and the first-stage coated asphalt reactor top liquid outflow pipeline is provided with a first-stage liquid level control valve L1;

[0036] The 2nd to nth stage gas-liquid micro-mixers M2~Mn are all provided with gas-liquid micro-mixer air feed pipelines, the top liquid outflow pipelines of the upper stage coated asphalt reactor are sequentially connected to the next stage gas-liquid micro-mixer and the bottom of the next stage coated asphalt reactor, and the top liquid outflow pipelines of each stage coated asphalt reactor are provided with a liquid level control valve, and the top gas outflow pipelines of the multi-stage coated asphalt reactors are sequentially merged into tail gas merging pipelines through pressure difference control valves; the last stage tail gas merging pipeline is merged with the top discharge pipeline of the coated asphalt stripping tower and then connected to the gas treatment system, and the gas treatment system is composed of a cooler and a gas-liquid separation tank, etc.

[0037] According to the present invention, preferably, each stage of the coated asphalt reactor is a cylindrical pressure vessel, with a feed distributor S arranged at the lower part, an anti-backmixing screen plate N arranged at the middle part, and a chimney tower plate oil collecting box X arranged at the upper part; preferably, the number of layers of the anti-backmixing screen plate (N) is 3-15 layers, and circular holes with a diameter of 8-20 mm are evenly distributed on the screen plate.

[0038] In the present invention, the oxidation reactor is a cylindrical pressure vessel, and a chimney-type tray oil collecting box is arranged on the upper part thereof to achieve gas-liquid separation.

[0039] In the present invention, the number of circular holes is determined by calculation based on the amount of raw materials, the amount of air and the hole velocity, so that the gas-liquid mixture in the oxidation reactor flows upward in the form of plug flow.

[0040] According to the present invention, preferably, the gas-liquid micro-mixer 3 includes a micro-mixer shell and an internal vortex disperser, the micro-mixer shell is provided with a liquid medium inlet, the coated asphalt circulation pump 2 is connected to the liquid medium inlet, the vortex disperser includes an internal strong mixing vortex element, a gas phase nozzle and a gas phase inlet, and the air feed pipeline and the superheated steam feed pipeline are connected to the gas phase inlet.

[0041] In the present invention, the gas-liquid micro-mixer is a mixer of gas and liquid, and the gas is dispersed in the liquid in the form of microbubbles, so that the raw materials and air are fully mixed, and the oxidation reaction effect is enhanced. The gas-liquid micro-mixer adopts eddy current dispersion technology, firstly, the air is evenly distributed in the circular cross-section of the mixer, and then the velocity gradient and pressure gradient are sheared through the eddy current element to form microbubbles. The advantage is that the bubble generation size is small and uniform, and the internal flow channel size is large, which can ensure long-term operation and reflux operation in emergency situations. The gas-liquid micro-mixer has a simple structure, the liquid medium goes through the main inlet, the gas medium enters the upper branch inlet of the micro-mixer, is inserted into the interior of the micro-mixer, and is provided with a gas phase collision head, and the gas is directly sprayed into the inlet of the eddy current disperser, and the evenly mixed medium flows out from the outlet of the micro-mixer.

[0042] According to the present invention, preferably, the coated asphalt stripping tower C is a cylindrical pressure vessel, and a plurality of inclined stripping tower plates B are arranged from top to bottom inside, and inward guide baffles are arranged on both sides of each stripping tower plate B. 2 to 4 liquid guide curtains are arranged on each stripping tower plate (B), and the inclination angle of the stripping tower plate B is 0° to 15°.

[0043] In the present invention, the stripping tray B adopts a new type of multi-falling liquid film tray technology and a diversion solid valve tray technology suitable for high-viscosity fluids, which can promote the flow of high-viscosity media, continuously generate medium surface renewal, promote the rupture of light oil emulsified film, reduce the thickness of high-viscosity medium falling film, and ensure the integrity of falling film, thereby improving the light oil stripping efficiency and avoiding high-viscosity media and solid particles such as coke powder from clogging the tray. The stripping tray has a certain inclination angle, and a liquid diversion curtain is designed at a certain interval. Generally, 2 to 4 curtains are designed for one tray. Inner diversion baffles are designed on both sides of the tray to gather liquid reflux, prevent liquid from slipping along the tower wall, and avoid wall flow. The inclination angle of the stripping tray B is determined according to the viscosity of the medium, generally 0° to 15°.

[0044] In the present invention, a stripping tray is arranged in the coated asphalt stripping tower to ensure the flow and stripping time of the high-viscosity and high-surface-tension coated asphalt, thereby improving the stripping effect.

[0045] According to the present invention, preferably, the superheated steam feed pipeline at the bottom of the coated asphalt stripping tower is connected to the superheated steam outlet of the superheating section of the heating furnace.

[0046] The second aspect of the present invention provides a method for continuously producing coated asphalt by multi-stage oxidation. The method is carried out using the device for continuously producing coated asphalt by multi-stage oxidation, and comprises the following steps: raw materials 1 and air 2 heated to the reaction temperature enter a multi-stage series-connected coated asphalt reactor for oxidation reaction, and the reaction tail gas 4 is sequentially connected through a pressure difference control valve to control the pressure difference at the top of adjacent coated asphalt reactors, so that the upper-stage liquid enters the bottom of the next-stage coated asphalt reactor from the next-stage gas-liquid micro-mixer under the control of the liquid level control valve;

[0047] The liquid phase n+8 at the top of the nth stage coated asphalt reactor enters the top of the coated asphalt stripping tower C under the control of the nth stage liquid level control valve Ln, and superheated steam 3 is introduced into the bottom of the coated asphalt stripping tower C. Under the stripping effect of the superheated steam, the coated asphalt 7 at the bottom of the coated asphalt stripping tower C is pumped out and pressurized by the stripping tower bottom pump P, and asphalt is molded after cooling under the control of the liquid level at the bottom of the stripping tower, and then sent to the warehouse.

[0048] In the present invention, the gases at the tops of the multi-stage oxidation reactors connected in series are connected in sequence through pressure difference control valves, and the pressure difference at the tops of two adjacent reactors is controlled so that the oxidized liquid flows backward in sequence.

[0049] According to the present invention, preferably, the following steps are included: (1) the raw material 1 heated to the reaction temperature and the preheated air 2 enter the gas-liquid micro-mixer M1, and after forced and sufficient mixing, enter the coated asphalt reactor R1, and a certain flow of fuel gas 8 is introduced into the top of the coated asphalt reactor R1, and an oxidation reaction is carried out at a certain temperature and pressure. The reaction tail gas 4 is discharged from the gas outflow pipeline at the top of the first-stage coated asphalt reactor, and the pressure difference between the top of the coated asphalt reactor R1 and the top of the coated asphalt reactor R2 is controlled by the pressure control valve D1 on the gas outflow pipeline at the top of the first-stage coated asphalt reactor, so that the first-stage coated asphalt reactor R1 is heated to 100 ℃ and the pressure of the coated asphalt reactor R2 is reduced. The unreacted liquid 9 at the top of the asphalt reactor enters the second-stage gas-liquid micro-mixer M2 with the air 2 under the control of the first-stage liquid level control valve L1, and enters the second-stage coated asphalt reactor R2 for oxidation reaction after forced and fully mixed; (2) The unreacted liquid at the top of the upper-stage coated asphalt reactor enters the lower-stage gas-liquid micro-mixer with the air under the control of the upper-stage liquid level control valve, and enters the lower-stage coated asphalt reactor for oxidation reaction after forced and fully mixed; (3) The stripping exhaust gas 5 is mixed with the mixed reaction exhaust gas 4 to obtain a mixed exhaust gas 6, which enters the cooler for cooling and then enters the gas-liquid separation tank for gas-liquid separation.

[0050] In the present invention, the non-condensable gas in the mixed tail gas is recycled to the low-pressure gas recovery system, and the liquid is sent to the downstream device as light oil for further processing and utilization.

[0051] According to the present invention, preferably, the oxidation time required for the production of coated asphalt is determined according to the raw material processing volume, raw material properties, and product quality requirements; preferably, the oxidation time is 3-8 hours.

[0052] In the present invention, multi-stage oxidation is required to achieve the oxidation time and oxygen concentration. The number of oxidation stages depends on the oxidation time of a single-stage oxidation reactor. Multiple reactors are connected in series for multi-stage oxidation to increase the oxygen concentration of the oxidation reaction and reduce the specifications of the reactor.

[0053] According to the present invention, preferably, the air and steam used in the device are superheated to the temperature and pressure required by the reactor.

[0054] Example 1

[0055] Ethylene tar is used as raw material 1. It is first heated to a suitable temperature by an upstream heating furnace, and then enters the gas-liquid micro-mixer M1 together with the preheated air 2. After forced and sufficient mixing, it enters the coated asphalt reactor R1 through the feed distributor S1. At a certain temperature and pressure, an oxidation reaction is carried out from bottom to top on the anti-reverse mixing screen plate N. A certain flow of fuel gas 8 is introduced into the top of the reactor. The gas pipeline at the top of the reactor is equipped with a pressure control valve D to control the pressure at the top of the tower. A special chimney plate oil collecting box X is set at the top of the reactor. The unreacted liquid 9 at the top enters the next-level gas-liquid micro-mixer M2 together with the air b under the control of the liquid level L. After forced and sufficient mixing, it enters the coated asphalt reactor M2 through the feed distributor S2. This is repeated. The liquid phase n at the top of the last reactor Rn enters the top stripping tower plate B of the coated asphalt stripping tower C under the control of the liquid level Ln. The bottom stripping tower plate B of the coated asphalt stripping tower C is introduced into superheated steam 3. Under the stripping action of the superheated steam, The unreacted light oil and oil gas 5 carried on the coated asphalt are stripped out and flow out from the top of the stripper. Together with the oil gas at the top of each reactor R, they enter the oil and gas cooler of the downstream gas treatment system under pressure control for cooling and separation. Oil gas and light oil are separated. The oil gas is sent to the gas system or sent to the heating furnace for combustion after adsorption. The light oil is sent to the device for further processing. The coated asphalt 7 at the bottom of the stripper C is pumped out and pressurized by the stripper bottom pump P. It is cooled and asphalt-molded under the control of the liquid level at the bottom of the stripper, and then sent to the warehouse. The air and steam used in the device are superheated to the temperature and pressure required by the reactor.

[0056] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments.

Claims

1. A device for continuously producing coated asphalt by multi-stage oxidation, characterized in that: The device comprises: a multi-stage coated asphalt reactor (R1, R2...Rn), a multi-stage gas-liquid micro-mixer (M1, M2...Mn), a multi-stage differential pressure control valve (D1, D2...Dn), a multi-stage liquid level control valve (L1, L2...Ln), a coated asphalt stripping tower (C) and a stripping tower bottom pump (P); The multi-stage coated asphalt reactor (R1, R2...Rn) is composed of a first-stage coated asphalt reactor (R1), a second-stage coated asphalt reactor (R2)... and an nth-stage coated asphalt reactor (Rn) connected in series, and each stage of the coated asphalt reactor is provided with a corresponding gas-liquid micro-mixer, a pressure difference control valve and a liquid level control valve; the gas-liquid micro-mixer is used to mix the raw material and air, the coated asphalt reactor is used for oxidation reaction, and the liquid flowing out of the top of the previous stage reactor enters the bottom of the next stage coated asphalt reactor through the next stage gas-liquid micro-mixer under the control of the liquid level control valve, and the pressure difference control valve is used to control the pressure difference at the top of adjacent coated asphalt reactors; The nth stage coated asphalt reactor (Rn) is provided with a liquid outflow pipeline at the top of the nth stage coated asphalt reactor, and the liquid outflow pipeline at the top of the nth stage coated asphalt reactor is connected to the nth stage liquid level control valve (Ln) and then connected to the top of the coated asphalt stripping tower (C); the coated asphalt stripping tower (C) is provided with a superheated steam feed pipeline at the bottom of the coated asphalt stripping tower, a discharge pipeline at the top of the coated asphalt stripping tower and a discharge pipeline at the bottom of the coated asphalt stripping tower, the discharge pipeline at the bottom of the coated asphalt stripping tower is connected to a stripping tower bottom pump (P), and the stripping tower bottom pump (P) is provided with a product discharge pipeline, and the discharge pipeline at the top of the coated asphalt stripping tower is connected to a gas treatment system.

2. The device for continuously producing coated asphalt by multi-stage oxidation according to claim 1, wherein: The first-stage gas-liquid micro-mixer (M1) is provided with a first-stage gas-liquid micro-mixer raw material feed pipeline, a first-stage gas-liquid micro-mixer air feed pipeline and a first-stage gas-liquid micro-mixer discharge pipeline, the first-stage gas-liquid micro-mixer discharge pipeline is connected to the bottom of the first-stage coated asphalt reactor (R1), the first-stage coated asphalt reactor (R1) is provided with a first-stage coated asphalt reactor fuel gas feed pipeline, a first-stage coated asphalt reactor top gas outflow pipeline and a first-stage coated asphalt reactor top liquid outflow pipeline, the first-stage coated asphalt reactor top gas outflow pipeline is provided with a first-stage pressure difference control valve (D1), and the first-stage coated asphalt reactor top liquid outflow pipeline is provided with a first-stage liquid level control valve (L1); The 2nd to nth stage gas-liquid micro-mixers (M2~Mn) are all provided with gas-liquid micro-mixer air feed pipelines, the top liquid outflow pipelines of the upper stage coated asphalt reactor are sequentially connected to the next stage gas-liquid micro-mixer and the bottom of the next stage coated asphalt reactor, and the top liquid outflow pipelines of each stage coated asphalt reactor are provided with a liquid level control valve, and the top gas outflow pipelines of the multi-stage coated asphalt reactors are sequentially merged into tail gas merging pipelines through pressure difference control valves; the last stage tail gas merging pipeline is merged with the top discharge pipeline of the coated asphalt stripping tower and then connected to the gas treatment system, and the gas treatment system is composed of a cooler and a gas-liquid separation tank, etc.

3. The device for continuously producing coated asphalt by multi-stage oxidation according to claim 1 or 2, wherein: Each stage of the coated asphalt reactor is a cylindrical pressure vessel, with a feed distributor (S) arranged at the bottom, an anti-backmixing screen plate (N) arranged in the middle, and a chimney tower plate oil collecting box (X) arranged at the top; preferably, the number of layers of the anti-backmixing screen plate (N) is 3-15 layers, and circular holes with a diameter of 8-20 mm are evenly distributed on the screen plate.

4. The device for continuously producing coated asphalt by multi-stage oxidation according to claim 1 or 2, wherein: The gas-liquid micro-mixer (3) comprises a micro-mixer shell and an internal vortex disperser, the micro-mixer shell is provided with a liquid medium inlet, the coated asphalt circulation pump (2) is connected to the liquid medium inlet, the vortex disperser comprises an internal strong mixing vortex element, a gas phase nozzle and a gas phase inlet, and the air feed pipeline and the superheated steam feed pipeline are connected to the gas phase inlet.

5. The device for continuously producing coated asphalt by multi-stage oxidation according to claim 1 or 2, wherein: The coated asphalt stripping tower (C) is a cylindrical pressure vessel, and multiple inclined stripping tower plates (B) are arranged from top to bottom inside, and inward guide baffles are arranged on both sides of each stripping tower plate (B). 2 to 4 liquid guide curtains are arranged on each stripping tower plate (B), and the inclination angle of the stripping tower plate (B) is 0° to 15°.

6. The device for continuously producing coated asphalt by multi-stage oxidation according to claim 1 or 2, wherein: The superheated steam feed pipeline at the bottom of the coated asphalt stripping tower is connected to the superheated steam outlet of the superheating section of the heating furnace.

7. A method for continuously producing coated asphalt by multi-stage oxidation, characterized in that: The method is carried out using the device for continuously producing coated asphalt by multi-stage oxidation as described in any one of claims 1 to 6, and comprises the following steps: The raw materials (1) and air (2) heated to the reaction temperature enter the multi-stage coated asphalt reactors connected in series for oxidation reaction, and the reaction tail gas (4) is connected in sequence through the pressure difference control valve to control the pressure difference at the top of the adjacent coated asphalt reactors, so that the liquid of the previous stage enters the bottom of the next stage coated asphalt reactor through the gas-liquid micro-mixer of the next stage under the control of the liquid level control valve; The liquid phase (n+8) at the top of the n-th stage coated asphalt reactor enters the top of the coated asphalt stripping tower (C) under the control of the n-th stage liquid level control valve (Ln), and superheated steam (3) is introduced into the bottom of the coated asphalt stripping tower (C). Under the stripping effect of the superheated steam, the coated asphalt (7) at the bottom of the coated asphalt stripping tower (C) is pumped out and pressurized by the stripping tower bottom pump (P), and asphalt is molded after being cooled under the control of the liquid level at the bottom of the stripping tower, and then sent to the warehouse.

8. The method for continuously producing coated asphalt by multi-stage oxidation according to claim 7, wherein: The following steps are involved: (1) The raw material (1) heated to the reaction temperature and the preheated air (2) enter the gas-liquid micro-mixer (M1), and after forced and sufficient mixing, enter the coated asphalt reactor (R1), and a certain flow of fuel gas (8) is introduced into the top of the coated asphalt reactor (R1), and an oxidation reaction is carried out at a certain temperature and pressure. The reaction tail gas (4) is discharged from the gas outflow pipeline at the top of the first-stage coated asphalt reactor. The pressure control valve (D1) on the gas outflow pipeline at the top of the first-stage coated asphalt reactor controls the pressure difference between the top of the coated asphalt reactor (R1) and the top of the coated asphalt reactor (R2), so that the unreacted liquid (9) at the top of the first-stage coated asphalt reactor enters the second-stage gas-liquid micro-mixer (M2) with the air (2) under the control of the first-stage liquid level control valve (L1), and after forced and sufficient mixing, enters the second-stage coated asphalt reactor (R2) for oxidation reaction; (2) The unreacted liquid at the top of the upper-stage coated asphalt reactor is controlled by the upper-stage liquid level control valve and enters the lower-stage gas-liquid micro-mixer with air, where it is forced and fully mixed before entering the lower-stage coated asphalt reactor for oxidation reaction; (3) The stripping tail gas (5) is mixed with the mixed reaction tail gas (4) to obtain a mixed tail gas (6), which enters a cooler for cooling and then enters a gas-liquid separation tank for gas-liquid separation.

9. The method for continuously producing coated asphalt by multi-stage oxidation according to claim 7, wherein: The oxidation time required for the production of coated asphalt is determined according to the raw material processing volume, raw material properties, and product quality requirements; preferably, the oxidation time is 3-8 hours.

10. The method for continuously producing coated asphalt by multi-stage oxidation according to claim 7, wherein: The air (2) and the superheated steam (3) are both superheated to the reaction temperature.

Citation Information

Cited By

  • Process for producing isotropic pitch

    WO2026161802A1