Flexible circuit board manufacturing method for intelligent video field

By making through holes and circuit patterns in the gold finger functional area of ​​the flexible circuit board, combining blue glue layer debrowning and high-temperature and high-pressure compression technology, the problems of high wiring density and poor reinforcement fit of the flexible circuit board are solved, and the problem of poor lamination of the flexible circuit board is achieved. Higher line density and functionality are achieved, and the binding force between the cover film and the connecting line area is improved, avoiding layering and bubble problems.

CN118973095AActive Publication Date: 2024-11-15深せん市実锐泰科技有限公司

Patent Information

Application Number
CN202410984308.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-15
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

During the high wiring density and reinforced bonding process, existing flexible circuit boards are prone to problems such as unclear line etching or poor reinforced bonding, resulting in excessive process capability or coating film delamination and bubbles.

Method used

The double-sided flexible copper clad plate design is adopted. Through holes are made in the gold finger functional area and electroplating process to form through holes, and then line graphic production and browning are carried out to form graphic browned flexible boards, and made in the reinforcement area. The blue glue layer is subjected to debrowning, followed by vacuum compression and high-temperature and high-pressure compression, increasing the compensation copper skin to improve the binding force between the covering film and the connecting line area.

Benefits of technology

Effectively improve the circuit density and functionality of the flexible circuit board, preventing the problem of imperfect etching or exceeding the process capability, and at the same time, enhancing the surface bonding of the cover film in the reinforcement area, avoiding the layering between the cover film and the connecting line area and The foaming problem ensures the surface color difference and bonding force of the finished product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973095A_ABST
    Figure CN118973095A_ABST
Patent Text Reader

Abstract

The invention discloses a method for manufacturing a flexible circuit board in the field of smart video, which comprises the following steps of: taking a double-sided flexible copper-clad plate, manufacturing a conducting hole in a golden finger functional region, manufacturing a circuit pattern, browning, manufacturing a blue glue layer in a reinforcing region, de-browning, tearing off the blue glue layer, pasting a cover film on double sides, performing primary lamination, and pasting and reinforcing the reinforcing region. Pressing for the second time to form a flexible circuit board; the additional function circuit is moved to the second surface, so that a larger wiring space is provided for the first surface, and the problem of incomplete etching or super process capability is prevented; after total browning and local de-browning are carried out, a browning effect is formed in the reinforcing area, the bonding force is higher, and the whole processing flow can enable the flexible circuit board to have stronger function support and higher reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of flexible circuit board manufacturing, and in particular to a method for manufacturing a flexible circuit board for the field of smart video. Background Art

[0002] In some digital AI video fields and smart camera fields, the flexible circuit boards used are relatively small in size, but have relatively more functional requirements, resulting in an increasing wiring density of the flexible circuit boards used inside them. In addition, there is a need to transmit instantaneous large currents and higher voltages during the application process. Therefore, the copper layer thickness of the flexible circuit boards is thicker than that of ordinary flexible circuit boards.

[0003] When the flexible circuit board is a single-layer board with a single-sided gold finger (plug circuit), the gold finger plug circuit needs to connect more board circuits, design a larger wiring density in a smaller space, and there are certain requirements for the thickness of the circuit copper layer. This can easily lead to problems such as incomplete etching or exceeding the process capability during processing.

[0004] And generally, the gold finger line position of the flexible circuit board needs to be reinforced to improve the hardness support and facilitate plug-in. The reinforcement is generally pasted on the covering film of the non-plug-in surface of the gold finger line. The reinforcement needs to be pressed to ensure firmness. If the reinforcement area is large and the thickness is thick, the use of rapid pressing process is likely to cause the reinforcement to be loose. After pressing, the covering film is easily affected by the high temperature too much, resulting in delamination and blistering between the inner layer of the flexible circuit board, resulting in scrapping and other problems.

[0005] Therefore, in order to solve the problems raised by the above background technology, a new method for manufacturing a flexible circuit board for the field of smart video is provided. Summary of the invention

[0006] The present invention aims to solve the problem that the existing high wiring density rigid-flexible boards with gold fingers are prone to incomplete circuit etching or poor reinforcement bonding during circuit manufacturing and reinforcement bonding, and proposes a new flexible circuit board manufacturing method for the smart video field, which comprises the following steps: S10: Take a double-sided flexible copper clad laminate, wherein the first side of the double-sided flexible copper clad laminate comprises a gold finger area, a gold finger functional area and a first connection line area adjacent to each other in sequence, and the second side comprises a patch reinforcement area and a second connection line area adjacent to each other in sequence, and the gold finger area and the gold finger functional area correspond to the patch reinforcement area; Making through holes in the gold finger functional area and performing electroplating processing, the through holes form conductive holes, and then performing circuit pattern making and browning processing to form a patterned browning flexible board; The circuit pattern includes a first-side circuit pattern and a second-side circuit pattern. The first circuit pattern includes a gold finger pattern located in the gold finger area and the gold finger function area. The second side circuit pattern includes a functional circuit pattern; S20: forming a blue glue layer on the pasting reinforcement area of ​​the patterned brown flexible board, then performing a browning treatment, and then tearing off the blue glue layer to form a partitioned browned patterned flexible board; S30: pasting cover films on both sides of the partitioned browning pattern flexible board, and performing a first lamination to form a cover film flexible board; S40: attaching and reinforcing the reinforcing area of ​​the cover film flexible board, and performing a second lamination to form the flexible circuit board.

[0007] Furthermore, the second-side circuit pattern also includes a compensation copper foil located between the functional circuit patterns of the supplementary reinforcement area.

[0008] Furthermore, the conducting hole is located on the gold finger pattern of the gold finger functional area corresponding to the functional circuit pattern.

[0009] Furthermore, the blue glue layer is made by screen printing blue glue or attaching a blue glue film.

[0010] Furthermore, the covering film is attached to the gold finger functional area and the first connecting line area, and further, the first pressing is performed by vacuum pressing and rapid pressing, and the pressing parameters are a temperature of 160°C to 180°C and a pressure of 15kg / cm 2 Up to 25kg / cm 2 The pressure is applied for 7 to 15 minutes.

[0011] Optionally, the first lamination is performed using a rigid plate lamination device, the lamination heating rate is 2°C / min to 5°C / min, the maximum temperature is 160°C to 185°C, and the pressure is 20kg / cm 2 Up to 30kg / cm 2 , the cooling rate is 8℃ / min to 12℃ / min.

[0012] Furthermore, before the attachment and reinforcement, the cover film flexible board is subjected to plasma treatment.

[0013] Furthermore, the second lamination is performed using a rigid plate lamination device, the lamination heating rate is 2°C / min to 6°C / min, the maximum temperature is 170°C to 190°C, and the pressure is 25kg / cm 2 Up to 35kg / cm 2 , the cooling rate is 10℃ / min to 20℃ / min.

[0014] Optionally, the first pressing is performed at a temperature of 130°C to 150°C and a pressure of 15kg / cm 2 Up to 20kg / cm 2 The pressure is set to 100%, and the pre-pressing is performed for 60 to 90 seconds.

[0015] The manufacturing method of the technical solution of the present invention moves the additional functional circuit to the second surface, provides a larger wiring space for the first surface, prevents the problem of incomplete etching or exceeding the process capacity due to excessive circuit density, and enables the flexible circuit board with the same area to form more circuit functions; the method of first browning the whole area and then partially de-browning is used to form a browning effect in the reinforcement area, effectively improving the surface bonding force between the covering film and the connecting line area when the reinforcement is applied to the surface of the reinforcement area, and preventing the problem of the covering film and the connecting line area not being able to fit together and delamination after the reinforcement is pressed. The connecting line area is first browned and then de-browned. The brown-black color of the circuit surface after the reinforcement and covering browning will not cause the color difference problem on the surface of the finished flexible circuit board. The roughness of the circuit surface in the connecting line area can be formed by browning, and the color difference problem of the circuit surface in the connecting line area of ​​the finished flexible circuit board can be prevented. Further, the compensation copper foil is added between the functional circuit patterns in the reinforcement area, and the rough surface formed by the copper foil after browning can be effectively used to improve the bonding strength of the covering film. Further, pre-pressing and then high-temperature and high-pressure pressing with rigid board pressing equipment can effectively form a covering film and reinforced pressing, thereby improving the bonding strength between layers. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0017] Figure 1 It is a process flow chart of the production method of the present invention; Figure 2 It is a schematic diagram of the planar structure of the circuit pattern on the first side of the pattern browning flexible board according to the manufacturing method of the present invention; Figure 3 The present invention is attached Figure 2 Schematic diagram of the AA cross-section structure; Figure 4 The present invention is attached Figure 2 Schematic diagram of BB cross-section structure; Figure 5 It is a schematic diagram of the planar structure of the circuit pattern on the second side of the pattern browning flexible board according to the manufacturing method of the present invention; Figure 6It is a schematic diagram of the planar structure of the second surface of the blue glue layer after it turns brown in the manufacturing method of the present invention; Figure 7 It is a schematic diagram of the planar structure of the browning circuit pattern on the first side of the partitioned browning pattern flexible board according to the manufacturing method of the present invention; Figure 8 It is a schematic diagram of the planar structure of the browning circuit pattern on the second side of the partitioned browning pattern flexible board according to the manufacturing method of the present invention; Fig. 9 A schematic diagram of the planar structure of the first covering film graphic surface of the covering film flexible board of the manufacturing method of the present invention; Fig.10 The present invention is attached Fig. 9 Schematic diagram of CC cross-section structure; Fig.11 It is a schematic diagram of the planar structure of the second covering film pattern surface of the covering film flexible board of the manufacturing method of the present invention; Fig.12 A schematic diagram of the planar structure of the second surface of the flexible circuit board according to the manufacturing method of the present invention; Fig.13 The present invention is attached Fig.12 Schematic diagram of the DD cross-section structure.

[0018] Description of Figure Numbers: Label name Label name 10A First side line graphics 3210 Functional line graphics 110 Goldfinger Area 20A Browning circuit pattern on the first side 1110 Gold Finger Graphics 20B Brown circuit pattern on the second side 210 Gold Finger Function Area 30A First covering film graphic surface 2110 Via holes 410 First cover film 310 First connection line area 4110 Covering film protective layer 3110 Original wiring 4120 Covering film adhesive layer 3120 New wiring 30B Second covering film graphic surface 3130 Surface brown layer 420 Second side cover film 10J Insulation dielectric layer 40 Flexible circuit board 10B Second side line graphics 510 Reinforcement 120 Subsidy for strong areas 4210 Reinforced protective layer 1210 Compensation copper 4220 Reinforced adhesive layer 320 Second connection line / / The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0020] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, inside, outside...) are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0021] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0022] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0023] See also Figure 1 , Figure 1 It is a process flow chart of the production method of the present invention.

[0024] The method for manufacturing a flexible circuit board according to the embodiment of the present invention adopts Figure 1 The process shown is carried out for processing. Figure 1 The processing flow is the process with technical features of this embodiment, not the entire process flow; the following is Figure 1 The process flow is described in detail.

[0025] Please also read Figures 2 to 5 ; Figure 2 It is a schematic diagram of the planar structure of the circuit pattern on the first side of the pattern browning flexible board according to the manufacturing method of the present invention; Figure 3 The present invention is attached Figure 2 Schematic diagram of the AA cross-section structure; Figure 4 The present invention is attached Figure 2 Schematic diagram of BB cross-section structure; Figure 5 This is a schematic diagram of the planar structure of the circuit pattern on the second side of the pattern browned flexible board according to the manufacturing method of the present invention.

[0026] Step S10: A double-sided flexible copper clad laminate is taken, including an insulating dielectric layer 10J. The first side of the double-sided flexible copper clad laminate includes a gold finger area 110, a gold finger functional area 210 and a first connecting line area 310 adjacent to each other in sequence. The second side includes a patch reinforcement area 120 and a second connecting line area 320 adjacent to each other in sequence. The gold finger area 110 and the gold finger functional area 210 correspond to the patch reinforcement area 120.

[0027] Different from the prior art, this embodiment adjusts the single-layer board with gold finger design into a double-sided board, and moves some auxiliary function circuit patterns such as grounding wires, heat dissipation wires, auxiliary wires, etc. to the second side, providing a larger design space for the circuit patterns with direct functions such as conduction, signal transmission, and welding components on the first side. New circuits 3120 can be set on the first side based on the original wiring 3110, thereby improving the functionality and processability of the flexible circuit board and preventing etching problems or exceeding process capability caused by excessive single-sided wiring density.

[0028] A through hole is made in the gold finger functional area, and electroplating is performed to form a conductive hole 2110. In this embodiment, the conductive hole 2110 is located on the gold finger pattern of the gold finger functional area corresponding to the functional circuit pattern.

[0029] Then, the circuit pattern is produced. The circuit pattern includes a first circuit pattern 10A and a second circuit pattern 10B. The first circuit pattern 10A includes a gold finger pattern 1110 located in the gold finger area 110 and the gold finger functional area 120 , and the second circuit pattern 10B includes a functional circuit pattern 3210 .

[0030] Since part of the circuit is moved to the second side, but the functional circuit pattern 3210 still needs to be connected to the gold finger pattern 1110 to achieve the plug-in connection effect during application, a gold finger functional area 210 is set between the gold finger area 110 and the first connecting line area 310, and a via 2110 is made in this area. The gold finger functional area 210 is subsequently formed so that the via 2110 can be covered with a covering film without affecting the appearance and performance. The via 2110 forms an effect of connecting the functional circuit pattern 3210 to the gold finger pattern 1110.

[0031] In this embodiment, the second-side circuit pattern 10B further includes a compensation copper sheet 1210 located between the functional circuit patterns in the supplementary reinforcement area.

[0032] The compensation copper sheet 1210 is provided. Since the bonding force between the copper sheet and the covering film is greater than the bonding force between the covering film and the insulating medium layer 10J, the bonding force between the subsequent covering film layer and the core board layer of the flexible circuit board can be effectively improved to prevent problems such as delamination and blistering.

[0033] A browning treatment is then performed to form a surface browning layer 3130, and the whole is processed to form a patterned browning flexible board.

[0034] The surface browning layer 3130 has a dense and uniform rough surface structure, which can greatly improve the bonding strength between the cover film layer and the circuit pattern, and provide a good basic surface condition for the subsequent attachment of the cover film and the production of reinforcement.

[0035] Please also read Figures 6 to 8 ; Figure 6 It is a schematic diagram of the planar structure of the second surface of the blue glue layer after it turns brown in the manufacturing method of the present invention; Figure 7 It is a schematic diagram of the planar structure of the browning circuit pattern on the first side of the partitioned browning pattern flexible board according to the manufacturing method of the present invention; Figure 8 It is a schematic planar structural diagram of the browning circuit pattern on the second side of the partitioned browning pattern flexible board according to the manufacturing method of the present invention.

[0036] Step S20: A blue glue layer 1220 is formed on the reinforcement area 120 of the patterned brown flexible board, and then a de-browning treatment is performed. Thereafter, the blue glue layer 1220 is torn off to form a partitioned browned patterned flexible board, wherein the first-side circuit pattern 10A forms a first-side browned circuit pattern 20A, and the second-side circuit pattern 10B forms a second-side browned circuit pattern 20B. In this embodiment, the blue glue layer is formed by screen printing blue glue or attaching a blue glue film.

[0037] The blue glue layer 1220 is only made on the patch reinforcement area 120 to protect the surface brown layer 3130 of the patch reinforcement area 120. After the other areas are de-brownized, the surface brown layer 3130 is de-brownized. The reason for this production method is that the patch reinforcement area 120 needs to be attached with a covering film and then reinforced, so a greater surface bonding force is required, so the surface brown layer 3130 of the area is retained. At the same time, the reinforcement is generally an opaque solid layer, which can effectively cover the dark brown color of the copper surface produced after the browning of the area. The surface browning layer 3130 is relatively fragile and easily scratched and abraded, so fading the surface browning layer 3130 in other areas can effectively prevent scratches and abrasions in subsequent processing. At the same time, the color of the covering film is translucent, and when attached to the surface, it cannot completely cover the scratched and abraded surface browning layer 3130, which will cause color difference on the surface of the finished flexible circuit board, resulting in poor visual inspection.

[0038] It is worth mentioning that the reason why the production method of first browning the entire surface and then partially de-browning is adopted, rather than the production method of first applying a dry film protection layer 3130 without the need for a surface browning layer and then browning the patch reinforcement area 120 alone, is because the rough surface (roughness, roughness uniformity) of the copper surface formed by browning first and then de-browning is far better than the rough surface effect of the original copper layer (or the copper layer after electroplating), so that the copper surface and the subsequent covering film have better bonding, ensuring that the covering film will not delaminate or bubble during the subsequent secondary pressing of the patch reinforcement.

[0039] If the blue glue layer 1220 is made of liquid blue glue, it can be processed by silk-screen printing of blue glue. If it is made of blue tape, it can be made by attaching blue glue film.

[0040] Please also read Figures 9 to 11 ; Fig. 9 A schematic diagram of the planar structure of the first covering film graphic surface of the covering film flexible board of the manufacturing method of the present invention; Fig.10 The present invention is attached Fig. 9 Schematic diagram of CC cross-section structure; Fig.11 It is a schematic plan view of the structure of the second covering film pattern surface of the covering film flexible board in the manufacturing method of the present invention.

[0041] Step S30: A covering film is pasted on both sides of the partitioned brown-colored patterned flexible board, wherein a first-side covering film 410 is attached to the first-side brown-colored circuit pattern 20A to form a first covering film pattern surface 30A, and a second-side covering film 420 is attached to the second-side brown-colored circuit pattern 20B to form a second covering film pattern surface 30B; in this embodiment, the covering film is pasted to the gold finger function area 120 and the first connecting line area 310, and the covering film is pasted to the reinforcement area 120 and the second connecting line area 320; and then the first pressing is performed to form a covering film flexible board.

[0042] Since the gold finger functional area 120 is a newly added area relative to the prior art, it does not need to be exposed like the gold finger pattern 1110. At the same time, there is a conductive hole 2110 in this area, so using a covering film to cover this area can, on the one hand, keep the original size and pattern of the gold finger pattern 1110 unchanged. On the other hand, since the first-side covering film is composed of a covering film protective layer 4110 and a covering film adhesive layer 4120 (the second-side covering film 420 is also composed of a protective layer and an adhesive layer), after the first lamination, the covering film adhesive layer 4120 can effectively fill the conductive hole 2110 to form a solid hole, thereby preventing the problem of burst holes and burst boards caused by the expansion of gas in the hole during subsequent attachment and lamination reinforcement.

[0043] In this embodiment, the first pressing is performed by vacuum pressing and rapid pressing. The pressing parameters are a temperature of 160° C. to 180° C. and a pressure of 15 kg / cm 2 Up to 25kg / cm 2 The pressure is applied for 7 to 15 minutes.

[0044] The first pressing uses vacuum pressing, which can effectively ensure that no gas is hidden in the conductive hole 2110. Using pressing parameters relative to the existing technology, appropriately increasing the temperature, increasing the pressure, and extending the pressing time can effectively melt the covering film glue layer 4120 and fill the conductive hole 2110. It is worth noting that due to the browning and de-browning processing, the surface of the copper layer and the surface of the wall of the conductive hole 2110 form a uniform rough surface. Whether higher temperature, greater pressure, and longer pressing time can improve the bonding strength between the covering film and the copper surface.

[0045] In this embodiment, the first lamination is performed using a rigid plate lamination device, the lamination heating rate is 2°C / min to 5°C / min, the maximum temperature is 160°C to 185°C, and the pressure is 20kg / cm 2 Up to 30kg / cm 2 , the cooling rate is 8℃ / min to 12℃ / min.

[0046] When the thickness of the partitioned browning graphic flexible board is relatively thick and the covering film adhesive layer 4120 is relatively thick, the first pressing can optionally use a rigid board pressing device for pressing, which has relatively greater pressure and pressing temperature, and the temperature rise is relatively gentle, which effectively improves the expansion and contraction performance of the covering film pressing and the interlayer bonding strength.

[0047] See also Fig.12 and Fig.13 ; Fig.12 A schematic diagram of the planar structure of the second surface of the flexible circuit board according to the manufacturing method of the present invention; Fig.13 The present invention is attached Fig.12 Schematic diagram of the DD cross-section structure.

[0048] Step S40: The reinforcement 510 is attached to the reinforcement area of ​​the cover film flexible board, and a second lamination is performed to form a flexible circuit board 40.

[0049] In this embodiment, before attaching the reinforcement 510 , the cover film flexible board is subjected to plasma treatment.

[0050] Since the reinforcement 510 is attached to the cover film, and the surface of the cover film is generally smooth, and the cover film material is generally a relatively inert polyimide material, plasma treatment of the cover film can form a rough surface on the cover film surface to improve the bonding strength of the reinforcement attachment.

[0051] In this embodiment, the second lamination is performed using a rigid plate lamination device, the lamination heating rate is 2°C / min to 6°C / min, the maximum temperature is 170°C to 190°C, and the pressure is 25kg / cm 2 Up to 35kg / cm 2 , the cooling rate is 10℃ / min to 20℃ / min.

[0052] Since this embodiment requires a stronger bonding force between the reinforcement and the covering film, and therefore when there is good bonding force between the covering film and the partitioned browned graphic flexible board, the second lamination can optionally be performed using a rigid board lamination device, which also has relatively greater pressure and lamination temperature, and a relatively gentle temperature rise, effectively improving the expansion and contraction performance of the covering film lamination and the interlayer bonding force.

[0053] In this embodiment, the first pressing step is performed at a temperature of 130°C to 150°C and a pressure of 10 kg / cm 2 Up to 20kg / cm 2 The pressure is set to 100%, and the pre-pressing is performed for 60 to 90 seconds.

[0054] It is worth noting that when the thickness of the partitioned browned graphic flexible board is relatively thin and the covering film adhesive layer 4120 can easily fill the conductive hole 2110, the first pressing can be used as pre-pressing, and the second pressing can be used as a manufacturing method using a pressing device for a rigid board for pressing. The first pressing uses a pre-pressing device, and the covering film is pre-pressed to the surface of the partitioned browned graphic flexible board under relatively low temperature and relatively small pressure, especially in a short time. The covering film and the partitioned browned graphic flexible board, as well as the reinforcement and the covering film are completely pressed at one time through the second pressing, which can effectively improve the production efficiency and save production energy.

[0055] It is worth noting that since flexible circuit boards are generally more precise, the actual structure diagram and the thickness of each layer, line width and other dimensions are all at the micron level. If they are drawn according to the actual proportion, there will be a problem of unclear diagrams. Therefore, in order to more clearly show the implementation process of the manufacturing method of this embodiment, the drawings of this embodiment are all schematic diagrams that enlarge the technical features, which do not represent the size of the actual structure diagram, nor do they represent enlarged views of the actual structure diagram in proportion.

[0056] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings, or directly / indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.

Claims

1. A method for manufacturing a flexible circuit board for the field of smart video. It is characterized in that The method for manufacturing a flexible circuit board comprises the following steps: S10: Take a double-sided flexible copper clad laminate, wherein the first side of the double-sided flexible copper clad laminate comprises a gold finger area, a gold finger functional area and a first connection line area adjacent to each other in sequence, and the second side comprises a patch reinforcement area and a second connection line area adjacent to each other in sequence, and the gold finger area and the gold finger functional area correspond to the patch reinforcement area; Making through holes in the gold finger functional area and performing electroplating processing, the through holes form conductive holes, and then performing circuit pattern making and browning processing to form a patterned browning flexible board; The circuit pattern includes a first-side circuit pattern and a second-side circuit pattern. The first circuit pattern includes a gold finger pattern located in the gold finger area and the gold finger function area. The second side circuit pattern includes a functional circuit pattern; S20: forming a blue glue layer on the pasting reinforcement area of ​​the patterned brown flexible board, then performing a browning treatment, and then tearing off the blue glue layer to form a partitioned browned patterned flexible board; S30: pasting cover films on both sides of the partitioned browning pattern flexible board, and performing a first lamination to form a cover film flexible board; S40: attaching and reinforcing the reinforcing area of ​​the cover film flexible board, and performing a second lamination to form the flexible circuit board.

2. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 1, It is characterized in that The second-side circuit pattern also includes a compensation copper foil located between the functional circuit patterns in the supplementary reinforcement area.

3. A method for manufacturing a flexible circuit board for the field of intelligent video communication as claimed in claim 1, It is characterized in that The conducting hole is located on the gold finger pattern of the gold finger functional area corresponding to the functional circuit pattern.

4. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 1 or 2, It is characterized in that The blue glue layer is made by silk-screening blue glue or attaching a blue glue film.

5. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 1 or 2, It is characterized in that The covering film is attached to the gold finger functional area and the first connecting line area, and the covering film is attached to the reinforcing area and the second connecting line area.

6. A method for manufacturing a flexible circuit board for the field of intelligent video communication as claimed in claim 1, It is characterized in that The first pressing is performed by vacuum pressing and rapid pressing, and the pressing parameters are a temperature of 160°C to 180°C and a pressure of 15kg / cm 2 Up to 25kg / cm 2 The pressure is applied for 7 to 15 minutes.

7. A method for manufacturing a flexible circuit board for the field of intelligent video communication as claimed in claim 1, It is characterized in that The first lamination is performed using a rigid plate lamination device, the lamination heating rate is 2°C / min to 5°C / min, the maximum temperature is 160°C to 185°C, and the pressure is 20kg / cm 2 Up to 30kg / cm 2 , the cooling rate is 8℃ / min to 12℃ / min.

8. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 1, It is characterized in that Before the attachment and reinforcement, the cover film flexible board is subjected to plasma treatment.

9. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 1, It is characterized in that The second lamination is performed using a rigid plate lamination device, with a lamination heating rate of 2°C / min to 6°C / min, a maximum temperature of 170°C to 190°C, and a pressure of 25kg / cm 2 Up to 35kg / cm 2 , the cooling rate is 10℃ / min to 20℃ / min.

10. A method for manufacturing a flexible circuit board for the smart video field as claimed in claim 9, It is characterized in that The first pressing step is performed at a temperature of 130°C to 150°C and a pressure of 15 kg / cm 2 Up to 20kg / cm 2 The pressure is set to 100%, and the pre-pressing is performed for 60 to 90 seconds.

Citation Information

Patent Citations

  • Flexible printed circuit board

    CN103118480A

  • Processing method for suspended gold finger, and circuit board

    CN109379840A

  • FPC welding golden finger

    CN215379338U

  • Multilayer printed circuit board and its manufacturing method

    JP2006287007A

Cited By

  • Manufacturing method of voltage-resistant flexible circuit board for new energy automobile

    CN119865974A

  • Manufacturing Method of a Voltage-Resistant Flexible Circuit Board for a New Energy Vehicle

    CN119865974B