In-mold foaming molding die and golf head cover molding method
Through the bonding technology of the barrier guide rib strip and top core of the in-mold foam forming mold, the manufacturing process of golf head cover is simplified, the problem of cumbersome manufacturing and unclear joints in the existing technology is solved, and the product quality is improved Appearance finish.
Patent Information
- Application Number
- CN201910948475.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-09-30
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2039-09-30
AI Technical Summary
The manufacturing process of existing golf ball head covers is complicated and there are slit marks at the joints, which affects the appearance and may scratch the ball head, and there is a potential for damage.
Use in-mold foam forming molds, including bottom molds and top molds, to prevent the spill of foamed materials and define the foamed molding cavity by blocking the fit of the guide rib strips and the top mold core, to replace the traditional braided sleeves and leather. Sewing process simplifies manufacturing process and improves quality.
The manufacturing process of golf ball head covers has been simplified, the finish of the junction between the foamed shell and the braided sleeve has been improved, gas residue has been prevented, and product quality and molding yield has been improved.
Smart Images

Figure CN110539443B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a molding die, and in particular to an in-mold foaming molding die for molding a golf head cover and a golf head cover molding method. Background Art
[0002] As we all know, golf is an elegant, leisure, and healthy green sport, but it is also a high-consumption sport. One of the reasons for its high consumption is that golf clubs are expensive, and golf clubs are essential sports equipment for golf.
[0003] In order to protect the expensive golf clubs, a common practice is to place the golf clubs in a golf bag. When a golf bag contains multiple golf clubs at the same time, the golf clubs will inevitably collide with each other during transportation, which will cause great damage to the golf clubs. Therefore, a golf head cover for individually protecting the head of each golf club came into being.
[0004] At present, for the existing golf head covers made of woven covers and leather, the woven covers and the leather are fixed together by sewing, so that the existing golf head covers have the defect of complicated manufacturing process; in addition, because the woven cover and the leather are fixed together by sewing, there are sewing marks at the joint between the two, which is not smooth enough, affecting the appearance and also has the risk of scratching the golf head.
[0005] Therefore, there is an urgent need for an in-mold foaming mold and a golf head cover molding method that can simplify the manufacturing process and improve the quality to overcome the above-mentioned defects. Summary of the invention
[0006] An object of the present invention is to provide an in-mold foaming mold that can simplify the manufacturing process and improve the quality.
[0007] Another object of the present invention is to provide a golf head cover molding method that can simplify the manufacturing process and improve the quality.
[0008] In order to achieve the above-mentioned purpose, the in-mold foaming molding mold of the present invention is suitable for molding a foam shell whose contour matches the golf club head on a braided sleeve, and includes a bottom mold and a top mold that cooperate with each other in opening and closing. The bottom mold is provided with a matching cavity with a cavity opening facing upward, and the top mold has a top mold core that cooperates with the matching cavity and allows the braided sleeve to be fitted from the outside, and the top mold core moves into the matching cavity when the mold is closed; wherein, the side cavity wall of the matching cavity has a side wall protruding toward the top mold core and is used to prevent the foaming material in the matching cavity from overflowing from the cavity during the in-mold foaming process, and the blocking guide rib is matched with the gap of the top mold core from the side when the mold is closed, and the blocking guide rib and the top mold core both make the matching cavity define a foaming molding cavity whose contour matches the foam shell when the mold is closed.
[0009] Preferably, a soft protective layer is provided on the top mold core, and the protective layer is gap-matched with the blocking and guiding ribs from the side when the mold is closed, or the protective layer is against the blocking and guiding ribs from the side when the mold is closed.
[0010] Preferably, the protective layer covers the top mold core.
[0011] Preferably, the bottom mold includes a bottom mold base body and a bottom mold top cover that opens and closes with the top front end of the bottom mold base body, the matching cavity includes a first matching cavity formed in the bottom mold base body and a second matching cavity formed in the bottom mold top cover, the first matching cavity passes through the top surface of the bottom mold base body, the first matching cavity also extends along the front and rear directions of the bottom mold base body, the second matching cavity passes through the bottom surface and rear side surface of the bottom mold top cover, the second matching cavity is spliced with the front end of the first matching cavity when the bottom mold top cover and the bottom mold base body are covered, and the top mold core is located in the first matching cavity and the second matching cavity when the mold is closed.
[0012] Preferably, the blocking and guiding ribs are respectively formed at the left cavity wall and the right cavity wall of the first matching cavity, and the blocking and guiding ribs also extend along the front-to-rear direction of the bottom mold base to the top surface of the bottom mold base.
[0013] Preferably, the junction between the blocking and guiding ribs and the side cavity wall of the matching cavity is an inwardly concave arc-shaped smooth transition structure.
[0014] Preferably, the matching cavity is arranged to be low at the front and high at the back, and the matching cavity is also arranged to be tapered from large at the front to small at the back.
[0015] To achieve the above-mentioned purpose, the golf head cover molding method of the present invention comprises the following steps:
[0016] (1) Injecting liquid foaming material into the matching cavity of the bottom mold;
[0017] (2) The bottom mold and the top mold are molded together so that the top mold core and the braided sleeve sleeved in the top mold core are moved into the matching cavity;
[0018] (3) heating and maintaining pressure on the in-mold foaming mold so that the foaming material is formed on the woven sleeve into a foam shell that is integrated with the woven sleeve, so that the foam shell and the woven sleeve constitute a golf head cover; and
[0019] (4) The bottom mold and the top mold are opened to remove the golf head cover from the top mold core;
[0020] Among them, in steps (1) to (3), the foaming material flows along the side cavity wall of the matching cavity toward the cavity mouth during the foaming process, and is blocked and guided by the blocking and guiding ribs to flow back to the foaming molding cavity, while the gas in the matching cavity and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs and the top mold core.
[0021] Preferably, in step (2), the top mold core together with the woven sleeve mounted on the top mold core is first moved into the first matching cavity of the bottom mold base, and then the bottom mold top cover is closed on the top front end of the bottom mold base, and the bottom mold top cover is locked with the bottom mold base; in step (4), the bottom mold top cover is first opened relative to the top front end of the bottom mold base, and then the top mold core together with the golf head cover is moved away from the bottom mold base.
[0022] To achieve the above-mentioned purpose, the golf head cover molding method of the present invention comprises the following steps:
[0023] (1) The bottom mold and the top mold are molded together, so that the top mold core and the braided sleeve sleeved in the top mold core are moved into the matching cavity, and the matching cavity is defined as a foaming molding cavity by the top mold core and the blocking and guiding ribs;
[0024] (2) injecting liquid foaming material into the foaming molding cavity;
[0025] (3) heating and maintaining pressure on the in-mold foaming mold so that the foaming material is formed on the woven sleeve into a foam shell that is integrated with the woven sleeve, so that the foam shell and the woven sleeve constitute a golf head cover; and
[0026] (4) The bottom mold and the top mold are opened to remove the golf head cover from the top mold core;
[0027] Among them, in steps (2) to (3), the foaming material flows along the side cavity wall of the matching cavity toward the cavity mouth during the foaming process, and is blocked and guided by the blocking guide ribs to flow back to the foaming molding cavity, while the gas in the matching cavity and the gas mixed in the foaming material are discharged from the gap between the blocking guide ribs and the top mold core.
[0028] Compared with the prior art, since the side cavity wall of the matching cavity has a side wall convex toward the top mold core and is used to block the foaming material in the matching cavity from overflowing from the cavity mouth during the in-mold foaming process, the blocking and guiding ribs are matched with the gap of the top mold core from the side when the mold is closed, and the blocking and guiding ribs and the top mold core define a foaming molding cavity with a contour matching the foam shell when the mold is closed; therefore, in the process of molding the foam shell on the woven sleeve, the foaming material flowing along the side cavity wall of the matching cavity to the cavity mouth is blocked by the blocking and guiding ribs, and the foaming material blocked by the blocking and guiding ribs flows back to the foaming molding cavity under the guidance of the blocking and guiding ribs, thereby realizing the in-mold foaming molding method to form a foam shell integrated with the woven sleeve on the woven sleeve, replacing the traditional sewing process between the woven sleeve and the leather, on the one hand, improving the smoothness of the joint between the foam shell and the woven sleeve, on the other hand, simplifying the manufacturing process of the golf head cover. At the same time, the gas in the matching cavity and the gas mixed in the foaming material are discharged from the gap between the blocking guide rib and the top mold core, preventing the gas from remaining in the foaming shell, thereby improving the quality of the golf head cover. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a schematic diagram of the three-dimensional structure of the in-mold foaming molding mold of the present invention when the mold is closed.
[0030] Figure 2 It is a schematic diagram of the three-dimensional structure of the in-mold foaming molding mold of the present invention when the top mold and the bottom mold are separated.
[0031] Figure 3 is along Figure 1 Schematic diagram of the internal structure after cutting along the AA line.
[0032] Figure 4 is along Figure 1 Schematic diagram of the internal structure after sectioning along the midline BB.
[0033] Figure 5 It is a schematic diagram of the internal structure of the top mold in the in-mold foaming molding mold of the present invention after being longitudinally cut at its center position.
[0034] Figure 6 yes Figure 3 The schematic diagram of the state of the in-mold foaming molding mold when molding a foam shell on a woven sleeve is shown.
[0035] Figure 7 It is a schematic diagram of the three-dimensional structure of a golf head cover formed by the in-mold foaming molding die of the present invention.
[0036] Figure 8 FIG. 1 is a flow chart of a golf head cover molding method according to a first embodiment of the present invention.
[0037] Fig. 9FIG. 4 is a flow chart of a golf head cover molding method according to a second embodiment of the present invention. DETAILED DESCRIPTION
[0038] In order to explain the technical content and structural features of the present invention in detail, further description will be given below in combination with the implementation modes and the accompanying drawings.
[0039] See also Figures 1 to 3 ,as well as Figures 5 to 7 The in-mold foaming mold 100 of the present invention is suitable for forming a foam shell 220 with a contour matching the golf club head on the braided cover 210, so that the foam shell 220 and the braided cover 210 together form a golf club head cover 200. Figure 6 and Figure 7 shown.
[0040] The in-mold foaming mold 100 of the present invention comprises a bottom mold 10 and a top mold 20 that are mutually opened and closed. The bottom mold 10 is provided with a matching cavity 11 with the cavity opening 111 facing upward, and the top mold 20 has a top mold core 21 that matches with the matching cavity 11 and is provided for the braided sleeve 210 to be fitted from the outside, so that the operator can fit the braided sleeve 210 on the top mold core 21 from the outside, and then the braided sleeve 210 can be stabilized and shaped by the top mold core 21; the top mold core 21 is moved into the matching cavity 11 when the mold is closed, and the state is shown in FIG. Figure 1 and Figure 2 The side cavity wall 112 of the matching cavity 11 has a side wall convex to the top mold core 21 and is used to prevent the foaming material in the matching cavity 11 from overflowing from the cavity opening 111 during the in-mold foaming process. Preferably, the blocking and guiding rib 113 is adjacent to the cavity opening 111, and the upper side surface 1131 of the blocking and guiding rib 113 is an outwardly convex arc surface to ensure that the top mold core 21 and the braided sleeve 210 can move into or out of the matching cavity 11 smoothly; the blocking and guiding rib 113 is in clearance fit with the top mold core 21 from the side when the mold is closed (see the state Figure 3 ), the gap is to provide a suitable escape space for the braided sleeve 210 sleeved on the top mold core 21, so that the braided sleeve 210 sleeved on the top mold core 21 can abut against the blocking guide rib 113 from the side when the mold is closed, effectively preventing the foaming material from overflowing from the gap and facilitating the gas discharge in the matching cavity 11; at the same time, the blocking guide rib 113 and the top mold core 21 both make the matching cavity 11 define a foaming molding cavity 114 whose contour matches the foam shell 220 when the mold is closed, and the state is shown in FIG. Figure 3 Specifically, a soft protective layer 22 is provided on the top mold core 21. Preferably, the protective layer 22 covers the top mold core 21 to improve the reliability of the combination of the two. When the mold is closed, the protective layer 22 is gap-matched with the blocking guide rib 113 from the side (see the state Figure 3), such a design can further reduce the gap between the top mold core 21 and the blocking guide rib 113 in the lateral direction, so that the woven sleeve 210 sleeved on the top mold core 21 can be more tightly abutted against the blocking guide rib 113 from the lateral direction when the mold is closed, and further prevent the foaming material from overflowing from the gap while ensuring that the gas in the matching cavity 11 can be discharged normally; and because the protective layer 22 is soft, it can also prevent the woven sleeve 210 sleeved on the top mold core 21 from being damaged due to the rigid collision between the top mold core 21 and the bottom mold 10 when the mold is closed, thereby better protecting the woven sleeve 210 sleeved on the top mold core 21, thereby improving the yield rate of product molding. It is understandable that, since the protective layer 22 is soft, when the protective layer 22 is made to abut against the blocking guide rib 113 from the side when the mold is closed, the blocking guide rib 113 is also slightly embedded in the protective layer 22 when the mold is closed. Correspondingly, the woven sleeve 210 mounted on the top mold core 21 is also slightly embedded in the protective layer 22 due to the abutment of the blocking guide rib 113 when the mold is closed. This design can further reduce the gap between the blocking guide rib 113 and the top mold core 21 from the side, and more effectively prevent the foaming material from overflowing from the gap to the cavity 111, but it is not limited to this example. It is worth noting that when the protective layer 22 is removed (that is, the top mold core 21 is not provided with the protective layer 22), the purpose of the woven sleeve 210 mounted on the top mold core 21 abutting against the blocking guide rib 113 from the side when the mold is closed can also be achieved. More specifically, as follows:
[0041] like Figures 1 to 4 As shown, the bottom mold 10 includes a bottom mold base body 10a and a bottom mold top cover 10b that opens and closes with the top front end of the bottom mold base body 10a. The matching cavity 11 includes a first matching cavity 11a formed in the bottom mold base body 10a and a second matching cavity 11b formed in the bottom mold top cover 10b. The first matching cavity 11a passes through the top surface 115 of the bottom mold base body 10a, and the first matching cavity 11a also extends along the front and rear direction of the bottom mold base body 10a; the second matching cavity 11b passes through the bottom surface 116 and the rear side surface 117 of the bottom mold top cover 10b, and the second matching cavity 11b is spliced with the front end of the first matching cavity 11a when the bottom mold top cover 10b and the bottom mold base body 10a are covered. The top mold core 21 is located in the first matching cavity 11a and the second matching cavity 11b when the mold is closed. The state is shown in FIG. Figure 3As shown. Therefore, with the help of the opening and closing cooperation between the bottom mold base 10a and the bottom mold top cover 10b, the top mold core 21 can be moved into the cooperation cavity 11 when the mold is closed, and moved out of the cooperation cavity 11 when the mold is opened. Specifically, the bottom mold base 10a and the bottom mold top cover 10b are hinged by hinges 30, so that the bottom mold base 10a and the bottom mold top cover 10b can be opened and closed by flipping, so that the opening and closing cooperation between the bottom mold top cover 10b and the bottom mold base 10a is more convenient; preferably, the hinges 30 are located at the front side walls on both sides of the bottom mold base 10a and the bottom mold top cover 10b, but not limited to this.
[0042] like Figure 2 , Figure 3 and Figure 6 As shown, the blocking and guiding ribs 113 are respectively formed on the left and right walls of the first matching cavity 11a, that is, the left and right walls of the first matching cavity 11a each have a blocking and guiding rib 113. Preferably, the blocking and guiding ribs 113 on the left and right walls of the first matching cavity 11a are aligned with each other, which is determined by the combination position between the foam shell 220 and the braided sleeve 210, so it is not limited to this; and the blocking and guiding ribs 113 also extend along the front-to-back direction of the bottom mold base 10a to the top surface 115 of the bottom mold base 10a, so as to more effectively prevent the foaming material in the matching cavity 11 from overflowing from the cavity opening 111. Specifically, the intersection of the blocking and guiding ribs 113 and the side cavity wall 112 of the matching cavity 11 is an inwardly concave arc-shaped smooth transition structure 14, so that the blocking and guiding ribs 113 can block and guide the foaming material more stably and reliably, but it is not limited to this. For example, the matching cavity 11 is arranged in a low front and high back configuration, and the matching cavity 11 is also arranged in a tapered configuration with a large front and a small back configuration (see the state). Figure 2 ) to ensure that a foam shell 220 with a spherical contour is formed on the woven sleeve 210 on the top mold core 21, so this example is not limited to this.
[0043] It should be noted that before the in-mold foaming molding mold 100 of the present invention works, the bottom mold 10 needs to be fixed on an external workbench, and the top mold 20 needs to be installed on an existing power mechanism outside, and the power mechanism drives the top mold 20 and the bottom mold 10 to automatically open and close the molds; and the opening and closing of the bottom mold base 10a and the bottom mold top cover 10b in the bottom mold 10 can be manually operated by the operator, and can also be achieved by setting an existing automatic opening and closing mechanism to realize the automatic opening and closing of the bottom mold top cover 10b relative to the bottom mold base 10a, so it is not limited to this.
[0044] See also Figure 8 , shows a golf head cover molding method according to a first embodiment of the present invention, the method comprising the steps of:
[0045] S001. Inject liquid foaming material into the matching cavity 11 of the bottom mold 10. Preferably, the foaming material can be PU foaming material, but it is not limited to this. It should be noted that the capacity of the foaming material injected into the matching cavity 11 each time is well known to ordinary technicians in this field, so it will not be described in detail here.
[0046] S002, the bottom mold 10 and the top mold 20 are molded together, so that the top mold core 21 together with the braided sleeve 210 sleeved in the top mold core 21 is moved into the matching cavity 11, and the state is shown in FIG. Figure 6 As shown; specifically, in step S002, the top mold core 21 together with the braided sleeve 210 mounted on the top mold core 21 is first moved into the first matching cavity 11a of the bottom mold base 10a, and then the bottom mold top cover 10b is covered on the top front end of the bottom mold base 10a, and the bottom mold top cover 10b is locked with the bottom mold base 10a.
[0047] S003, heating and maintaining the pressure of the in-mold foaming mold 100, so that the foaming material is formed on the braided sleeve 210 to form a foam shell 220 that is integrated with the braided sleeve 210 (see Figure 6 As shown), the foam shell 220 and the braided sleeve 210 form a golf head cover 200, as shown in FIG. Figure 7 It should be noted that the parameters of heating and holding pressure are well known to ordinary technicians in this field, so they will not be described in detail here.
[0048] And S004, the bottom mold 10 and the top mold 20 are opened with each other, and the golf head cover 200 is removed from the top mold core 21 to complete the molding of the golf head cover 200; specifically, in step S004, the bottom mold top cover 10b is first opened relative to the top front end of the bottom mold base 10a, and then the top mold core 21 is moved away from the bottom mold base 10a together with the golf head cover 200.
[0049] Among them, in steps S001 to S003, the foaming material flows along the side cavity wall 112 of the matching cavity 11 toward the cavity opening 111 during the foaming process, and is blocked and guided by the blocking and guiding ribs 113 to flow back to the foaming molding cavity 114, while the gas in the matching cavity 11 and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs 113 and the top mold core 21 to prevent gas from remaining in the foam shell 220 of the golf head cover 200.
[0050] See also Fig. 9 , shows a golf head cover molding method according to a second embodiment of the present invention, the method comprising the steps of:
[0051] P001, the bottom mold 10 and the top mold 20 are molded together, so that the top mold core 21 together with the woven sleeve 210 sleeved in the top mold core 21 is moved into the matching cavity 11, and the matching cavity 11 is defined as a foaming molding cavity 114 by the top mold core 21 and the blocking guide rib 113; specifically, in step P001, the top mold core 21 together with the woven sleeve 210 sleeved on the top mold core 21 is first moved into the first matching cavity 11a of the bottom mold base body 10a, and then the bottom mold top cover 10b is covered on the top front end of the bottom mold base body 10a, and the bottom mold top cover 10b and the bottom mold base body 10a are locked.
[0052] P002. Inject liquid foaming material into the foaming molding cavity 114. Preferably, the foaming material can be PU foaming material, but it is not limited to this. It should be noted that the capacity of the foaming material injected into the foaming molding cavity 114 each time is well known to ordinary technicians in the field, so it will not be described in detail here. Since the golf head cover molding method of the second embodiment is to inject foaming material into the foaming molding cavity 114, an injection channel can be provided on the bottom mold base 10a of the bottom mold 10.
[0053] P003, heating and maintaining the pressure of the in-mold foaming mold 100, so that the foaming material is formed on the braided sleeve 210 to form a foam shell 220 that is integrated with the braided sleeve 210 (see Figure 6 ), so that the foam shell 220 and the braided cover 210 form a golf head cover 200, the state is shown in FIG. Figure 7 It should be noted that the parameters of heating and holding pressure are well known to ordinary technicians in this field, so they will not be described in detail here.
[0054] And P004, the bottom mold 10 and the top mold 20 are opened with each other, and the golf head cover 200 is removed from the top mold core 21 to complete the molding of the golf head cover 200; specifically, in step P004, the bottom mold top cover 10b is first opened relative to the top front end of the bottom mold base 10a, and then the top mold core 21 is moved away from the bottom mold base 10a together with the golf head cover 200.
[0055] Among them, in steps P002 to P003, the foaming material flows along the side cavity wall 112 of the matching cavity 11 toward the cavity opening 111 during the foaming process, and is blocked and guided by the blocking and guiding ribs 113 to flow back to the foaming molding cavity 114, while the gas in the matching cavity 11 and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs 113 and the top mold core 21 to prevent gas from remaining in the foaming shell 220 of the golf head cover 200.
[0056] Compared with the prior art, since the side cavity wall 112 of the matching cavity 11 has a side wall protruding toward the top mold core 21 and is used to prevent the foaming material in the matching cavity 11 from overflowing from the cavity opening 111 during the foaming process in the mold, the blocking and guiding ribs 113 are gap-matched with the top mold core 21 from the side when the mold is closed, and the blocking and guiding ribs 113 and the top mold core 21 define a foaming molding cavity 114 of the matching cavity 11 with a contour matching the foam shell 220 when the mold is closed; therefore, in the process of forming the foam shell 220 on the braided sleeve 210, the blocking and guiding ribs 113 are used to prevent the foaming material in the matching cavity 11 from overflowing from the cavity opening 111 during the foaming process in the mold. The foaming material flowing along the side cavity wall 112 of the matching cavity 11 toward the cavity opening 111 is blocked, and the foaming material blocked by the blocking and guiding ribs 113 is guided by the blocking and guiding ribs 113 to flow back to the foaming molding cavity 114, so that the foaming shell 220 integrated with the braided sleeve 210 is formed on the braided sleeve 210 by the in-mold foaming molding method, replacing the traditional sewing process between the braided sleeve and the leather, on the one hand, improving the smoothness of the joint between the foaming shell 220 and the braided sleeve 210, and on the other hand, simplifying the manufacturing process of the golf head cover 200. At the same time, the gas in the matching cavity 11 and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs 113 and the top mold core 21, preventing the gas from remaining in the foaming shell 220, thereby improving the quality of the golf head cover 200.
[0057] The above disclosure is only a preferred embodiment of the present invention, which cannot be used to limit the scope of the present invention. Therefore, equivalent changes made according to the claims of the present invention are all within the scope of the present invention.
Claims
1. An in-mold foaming mold for forming a golf head cover, which is suitable for forming a foam shell with a contour matching the golf club head on a braided cover, the in-mold foaming mold comprises a bottom mold and a top mold that are mutually opened and closed, the bottom mold is provided with a matching cavity with a cavity opening facing upward, the top mold has a top mold core that matches the matching cavity and is provided for the braided cover to be covered from the outside, the top mold core moves into the matching cavity when the mold is closed, and is characterized in that: The side cavity wall of the matching cavity has a blocking guide rib protruding toward the side wall of the top mold core and used to prevent the foaming material in the matching cavity from overflowing from the cavity opening during the in-mold foaming process. The blocking guide rib is matched with the gap of the top mold core from the side when the mold is closed, and the blocking guide rib and the top mold core together make the matching cavity define a foaming molding cavity whose contour matches the foam shell when the mold is closed; Wherein, the matching cavity is arranged with the front lower and the back higher; The bottom mold includes a bottom mold base body and a bottom mold top cover that opens and closes with the top front end of the bottom mold base body, the matching cavity includes a first matching cavity formed in the bottom mold base body and a second matching cavity formed in the bottom mold top cover, the first matching cavity passes through the top surface of the bottom mold base body, the first matching cavity also extends along the front and rear directions of the bottom mold base body, the second matching cavity passes through the bottom surface and rear side surface of the bottom mold top cover, the second matching cavity is spliced with the front end of the first matching cavity when the bottom mold top cover and the bottom mold base body are covered, and the top mold core is located in the first matching cavity and the second matching cavity when the mold is closed.
2. The in-mold foaming mold according to claim 1, characterized in that: A soft protective layer is provided on the top mold core, and the protective layer is gap-matched with the blocking and guiding ribs from the side when the mold is closed, or the protective layer is against the blocking and guiding ribs from the side when the mold is closed.
3. The in-mold foaming mold according to claim 2, characterized in that: The protective layer covers the top mold core.
4. The in-mold foaming mold according to claim 1, characterized in that: The blocking and guiding ribs are respectively formed at the left cavity wall and the right cavity wall of the first matching cavity, and the blocking and guiding ribs also extend along the front-to-rear direction of the bottom mold base to the top surface of the bottom mold base.
5. The in-mold foaming mold according to claim 1, characterized in that: The intersection of the blocking and guiding ribs and the side cavity wall of the matching cavity is an inwardly concave arc-shaped smooth transition structure.
6. The in-mold foaming mold according to claim 1, characterized in that: The matching cavity is also arranged in a tapered manner with a larger front and a smaller rear.
7. A method for forming a golf head cover using an in-mold foaming mold according to claim 1, characterized in that: The steps include: (1) Injecting liquid foaming material into the matching cavity of the bottom mold; (2) The bottom mold and the top mold are molded together so that the top mold core and the braided sleeve sleeved in the top mold core are moved into the matching cavity; (3) heating and maintaining pressure on the in-mold foaming mold so that the foaming material is formed on the woven sleeve into a foam shell that is integrated with the woven sleeve, so that the foam shell and the woven sleeve constitute a golf head cover; and (4) The bottom mold and the top mold are opened from each other, and the golf head cover is removed from the top mold core; In steps (1) to (3), the foaming material flows along the side cavity wall of the matching cavity toward the cavity opening during the foaming process, and the blocking and guiding ribs block and guide the foaming material to flow back to the foaming molding cavity, while the gas in the matching cavity and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs and the top mold core.
8. The golf head cover molding method according to claim 7, characterized in that: In step (2), the top mold core together with the braided sleeve mounted on the top mold core is first moved into the first matching cavity of the bottom mold base body, and then the bottom mold top cover is closed on the top front end of the bottom mold base body, and the bottom mold top cover is locked with the bottom mold base body; in step (4), the bottom mold top cover is first opened relative to the top front end of the bottom mold base body, and then the top mold core together with the golf head cover is moved away from the bottom mold base body.
9. A method for forming a golf head cover using an in-mold foaming mold according to claim 1, characterized in that: The steps include: (1) The bottom mold and the top mold are molded together so that the top mold core and the braided sleeve sleeved in the top mold core are moved into the matching cavity, and the matching cavity is defined as a foaming molding cavity by the top mold core and the blocking and guide ribs; (2) Injecting liquid foaming material into the foaming molding cavity; (3) heating and maintaining pressure on the in-mold foaming mold so that the foaming material is formed on the woven sleeve into a foam shell that is integrated with the woven sleeve, so that the foam shell and the woven sleeve constitute a golf head cover; and (4) The bottom mold and the top mold are opened from each other, and the golf head cover is removed from the top mold core; In steps (2) to (3), the foaming material flows along the side cavity wall of the matching cavity toward the cavity opening during the foaming process, and is blocked and guided by the blocking and guiding ribs to flow back to the foaming molding cavity, while the gas in the matching cavity and the gas mixed in the foaming material are discharged from the gap between the blocking and guiding ribs and the top mold core.