Surface treatment-free anti-warping protective cover and coil structure

By arranging grooves and L-shaped structures on the base material of the smartphone camera protective cover, and combining it with a double-sided adhesive layer and a transparent antistatic protective film, the problems of high surface treatment costs and roll warping in the existing technology are solved. Improved strength and detection efficiency are achieved.

CN111347749BActive Publication Date: 2024-10-01SUZHOU YIBANG ELECTRONICS MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010344184.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-04-27
Publication Date
2024-10-01
Estimated Expiration
2040-04-27

AI Technical Summary

Technical Problem

Existing smartphone camera protective covers require surface treatment when the layer structure is compounded, which increases process costs, and is prone to warping when forming a roll structure, affecting subsequent use.

Method used

Using an anti-warp protective cover that requires no surface treatment, by setting up grooves and L-shaped structures on the base material, combined with a double-sided adhesive layer (silicone side and acrylic adhesive side) and a transparent anti-static protective film, warping is avoided and Improved viscosity adaptability.

Benefits of technology

It is possible to improve the strength and detection efficiency of the protective cover without increasing process costs, avoid warping of the roll structure, and ensure the accuracy and efficiency of camera detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111347749B_ABST
    Figure CN111347749B_ABST
Patent Text Reader

Abstract

The present invention provides a surface treatment-free anti-warping protective cover and a roll structure, wherein the surface treatment-free anti-warping protective cover comprises: a substrate and a light-shielding protective layer bonded to one side of the substrate; the substrate has three detection channels that are identical or different, and a broken groove is formed on the surface of the connection between any two adjacent detection channels, and any broken groove extends to the edge positions of both sides of the connection in the length direction; the light-shielding protective layer is bonded to one side of the substrate through a double-sided adhesive layer, one side of the double-sided adhesive layer is a silicone surface, and the other side is an acrylic adhesive surface, the silicone surface is bonded to one side of the substrate, and the acrylic adhesive surface is bonded to the light-shielding protective layer. The protective cover of the present invention has a double-sided adhesive layer with high viscosity, and the two sides of the double-sided adhesive layer have different viscosities to meet the different requirements for viscosity when the two layer structures are compounded. In addition, by arranging the broken groove on the substrate, warping of the protective cover when forming a roll is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a protective cover, in particular to a surface treatment-free anti-warping protective cover and a coiled material structure. Background Art

[0002] A smartphone is a general term for mobile phones that, like a personal computer, have an independent operating system and independent running space, on which users can install software, games, navigation and other programs provided by third-party service providers, and can access wireless networks through mobile communication networks.

[0003] Currently, all smart phones are equipped with cameras. Before leaving the factory, mobile phone cameras need to go through multiple turnovers and also need to undergo quality inspections. Therefore, faced with the problem of how to protect mobile phone cameras and facilitate inspection of mobile phone cameras, the prior art provides a protective cover that can be put on mobile phone cameras and facilitate inspection.

[0004] However, the existing protective cover has a layer structure. In order to achieve the composite between the layers, the adhesive layer between the two layers needs to be surface treated so that the two sides have different viscosities, which increases the process cost of the protective cover. In addition, the existing protective cover is prone to warping when forming a roll material structure, which affects the subsequent use of the roll material. Therefore, it is necessary to propose a further solution to the above problems. Summary of the invention

[0005] The present invention aims to provide a surface treatment-free anti-warping protective cover and a coiled material structure to overcome the deficiencies in the prior art.

[0006] In order to solve the above technical problems, the technical solution of the present invention is:

[0007] A surface treatment-free anti-warping protective cover, comprising: a substrate and a light-shielding protective layer combined with one side of the substrate;

[0008] The substrate has three detection channels that are identical or different and are arranged through the substrate, and a broken groove is formed on the surface of the connecting portion between any two adjacent detection channels, and any broken groove extends to the edge positions of both sides of the connecting portion where it is located in the length direction;

[0009] The light-shielding protective layer is bonded to one surface of the substrate through a double-sided adhesive layer, one surface of the double-sided adhesive layer is a silicone surface, and the other surface is an acrylic adhesive surface. The silicone surface is bonded to one surface of the substrate, and the acrylic adhesive surface is bonded to the light-shielding protective layer.

[0010] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the depth of the broken groove is 1 / 5 to 1 / 4 of the thickness of the substrate.

[0011] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the substrate is L-shaped, and the detection channels are respectively arranged at both ends and the middle corner position of the L-shaped substrate.

[0012] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, an arc-shaped avoidance structure recessed inwardly is further provided on the inner side of the corner of the L-shaped substrate.

[0013] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the substrate and the light-shielding protective layer thereon are further provided with pull ears which are stacked together, and a protrusion is also provided on the pull ear of the substrate.

[0014] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the light-shielding protective layer is a red Mylar tape layer.

[0015] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, a double-sided antistatic light-transmitting protective film is also combined on the light-shielding protective layer.

[0016] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the surface treatment-free anti-warping protective cover also includes: a double-sided antistatic silicone protective film, which is bonded to the other side of the substrate through another double-sided adhesive layer, one side of the double-sided adhesive layer is a silicone surface, and the other side is an acrylic adhesive surface, the silicone surface is bonded to the other side of the substrate, the acrylic adhesive surface is bonded to the double-sided antistatic silicone protective film, and the double-sided antistatic silicone protective film has a first hollow structure at a position corresponding to the detection channel.

[0017] As an improvement of the surface treatment-free anti-warping protective cover of the present invention, the position of the double-sided antistatic silicone protective film corresponding to the broken groove has a second hollow structure, and the second hollow structure has one end extending to one side edge of the double-sided antistatic silicone protective film in the length direction, and the other end is close to the other side edge of the double-sided antistatic silicone protective film. In order to solve the above technical problems, the technical solution of the present invention is:

[0018] A coiled material structure comprises: a material strip and the above-mentioned surface treatment-free anti-warping protective cover adhered to the material strip.

[0019] Compared with the prior art, the invention has the following beneficial effects: the protective cover of the invention can be put on the camera to protect the mobile phone camera, and it has good strength and can withstand certain external forces. Moreover, the protective cover of the invention adopts a transparent protective film, so when the camera is inspected, it is not necessary to tear off the protective film to directly inspect, thereby improving the efficiency of inspection.

[0020] At the same time, the protective cover of the present invention has a double-sided adhesive layer with high viscosity, and the two sides of the double-sided adhesive layer have different viscosities to meet the different requirements for adhesive force when the two layer structures are compounded. In addition, the protective cover of the present invention has a broken groove on the substrate to avoid warping when the protective cover is formed into a roll. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figure 1 This is a schematic diagram of an exploded view of a surface treatment-free anti-warping protective cover in Example 1 of the present invention;

[0023] Figure 2 It is a plan view schematically showing the coil structure in Example 2 of the present invention. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] Example 1

[0026] like Figure 1 As shown, the surface treatment-free anti-warping protective cover 100 of the present embodiment 1 includes: a substrate 1 and a light shielding protective layer 2 combined with one side of the substrate 1 .

[0027] The substrate 1 forms the main structure of the protective cover of this embodiment, and protects the camera by being mounted on the camera. In one embodiment, the substrate 1 can be a rubber substrate.

[0028] In order to protect the camera and achieve the purpose of detection at the same time, the substrate 1 has three identical or different detection channels 11, so that the protective cover of this embodiment is suitable for the protection and detection of the camera of a triple-camera mobile phone. The identical or different refers to the identical or different shapes of the detection channels 11 and the identical or different sizes of the detection channels 11.

[0029] According to the structure of the triple-camera mobile phone, in one embodiment, the substrate 1 is L-shaped, and the detection channels 11 are respectively provided at the two ends and the middle corner of the L-shaped substrate 1. At the same time, in order to avoid interference when the protective cover 100 is installed, an arc-shaped avoidance structure 12 is also provided on the inner side of the corner of the L-shaped substrate 1.

[0030] In order to prevent the protective cover from warping when forming a coil, a broken groove 13 is formed on the surface of the connection between any two adjacent detection channels 11, and the broken groove 13 is located on the other side of the substrate 1. And any broken groove 13 extends to the edge positions on both sides of the connection part where it is located in the length direction to ensure that the broken groove 13 completely cuts off the connection part in the length direction. Therefore, when the protective cover is bent, the broken groove 13 on the substrate 1 can absorb the deformation generated when the substrate 1 is curled, which can reduce the stress generated when the substrate 1 is curled, thereby avoiding the substrate 1 from warping and ensuring the normal use of the coil. In one embodiment, the depth of the broken groove 13 is 1 / 5 to 1 / 4 of the thickness of the substrate 1.

[0031] The light-shielding protective layer 2 is bonded to one side of the substrate 1 through a double-sided adhesive layer 3. The light-shielding protective layer 2 can be a red Mylar tape layer, and its model is JY-312RDF. By providing the light-shielding protective layer 2, it is beneficial for external interference light to be taken into the detection channel 11, thereby ensuring the accuracy of the detection result.

[0032] In order to adapt to the different requirements for adhesion when the two layer structures are compounded, one side of the double-sided adhesive layer 3 is a silicone surface, and the other side is an acrylic adhesive surface. Considering that the substrate 1 requires a relatively larger adhesive force, the light-shielding protective layer 2 requires a relatively smaller adhesive force, and the viscosity of the silicone surface is greater than that of the acrylic adhesive surface, the corresponding silicone surface is combined with one side of the substrate 1, and the acrylic adhesive surface is combined on the light-shielding protective layer 2, so as to facilitate the compounding of the substrate 1 and the light-shielding protective layer 2 thereon.

[0033] In addition, the substrate 1 and the light shielding protective layer 2 thereon are provided with a pull ear 14 stacked together, and the pull ear 14 of the substrate 1 is also provided with a protrusion 141. The pull ear 14 with the protrusion 141 is provided, so that the pull ear 14 is convenient to hold when picking up the protective cover, and slipping can be prevented.

[0034] At the same time, a double-sided antistatic light-transmitting protective film 4 is also combined on the light-shielding protective layer 2, so that when the camera detects, it is not necessary to tear off the protective film to directly detect, thereby improving the efficiency of detection. In one embodiment, the double-sided antistatic light-transmitting protective film 4 includes: a PE film layer, a PET layer, and a PE film layer stacked in sequence.

[0035] In order to protect the other side of the substrate 1, the surface treatment-free anti-warping protective cover further includes: a double-sided antistatic silicone protective film 5, which is bonded to the other side of the substrate 1 through another double-sided adhesive layer 3. At this time, the broken groove 11 on the other side of the substrate 1 also has the function of assisting exhaust when the double-sided antistatic silicone protective film 5 is attached.

[0036] One side of the double-sided adhesive layer 3 is a silicone surface, and the other side is an acrylic adhesive surface. The silicone surface is bonded to the other side of the substrate 1 , and the acrylic adhesive surface is bonded to the double-sided antistatic silicone protective film 5 .

[0037] In addition, in order to avoid affecting the detection of the camera, the double-sided antistatic silicone protective film 5 has a first hollow structure 51 at a position corresponding to the detection channel 11, and the shape of the first hollow structure 51 is consistent with the radial cross-sectional shape of the detection channel 11. In one embodiment, the double-sided antistatic silicone protective film 5 includes: an electrostatic liquid coating, a PET blue magic, a double antistatic silicone, and a PET substrate 1 arranged in sequence.

[0038] In order to match with the broken groove 13 on the substrate 1, the double-sided antistatic silicone protective film 5 has a second hollow structure 52 at a position corresponding to the broken groove 13. In the length direction, one end of the second hollow structure 52 extends to one side edge of the double-sided antistatic silicone protective film 5, and the other end is close to the other side edge of the double-sided antistatic silicone protective film 5. That is, the second hollow structure 52 does not cut off the double-sided antistatic silicone protective film 5, so it is easy to control the double-sided antistatic silicone protective film 5 to be composited on the substrate 1.

[0039] Example 2

[0040] like Figure 2 As shown, based on the requirement of continuous feeding of surface-free anti-warping protective sleeves in actual production, Embodiment 2 also provides a roll material structure 200, which comprises: a material strip 201, and a plurality of surface-free anti-warping protective sleeves 100 as described above adhered to the material strip 201.

[0041] In addition, in order to further facilitate the peeling between each protective cover and the coil, another low-viscosity Mylar strip 6 is also provided at the edge of the double-sided antistatic silicone protective film 5. Preferably, the Mylar strip 6 is provided at the edge of the double-sided antistatic silicone protective film 5 close to the pull ear 14, so that when peeling, the Mylar strip 6 can easily separate the edge of the protective cover 100 from the material tape 201 to prevent the occurrence of adhesive problems.

[0042] In summary, the protective cover of the present invention can be mounted on the camera to protect the mobile phone camera. It has good strength and can withstand certain external forces. In addition, the protective cover of the present invention adopts a transparent protective film, so that when the camera is inspected, it is not necessary to tear off the protective film to directly inspect, thereby improving the efficiency of inspection. At the same time, the protective cover of the present invention has a double-sided adhesive layer with high viscosity, and the two sides of the double-sided adhesive layer have different viscosities to meet the different requirements for viscosity when the two layer structures are compounded. In addition, the protective cover of the present invention avoids warping when the protective cover is formed into a coil by arranging a broken groove on the substrate.

[0043] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.

[0044] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A surface treatment-free anti-warping protective cover, characterized in that: The surface treatment-free anti-warping protective cover comprises: a substrate and a light-shielding protective layer combined with one side of the substrate; The substrate has three detection channels that are identical or different and are arranged through the substrate. A broken groove is formed on the surface of the connecting portion between any two adjacent detection channels. Any broken groove extends to the edge positions of both sides of the connecting portion where it is located in the length direction. The depth of the broken groove is 1 / 5 to 1 / 4 of the thickness of the substrate. The light-shielding protective layer is bonded to one side of the substrate through a double-sided adhesive layer, one side of the double-sided adhesive layer is a silicone surface, and the other side is an acrylic adhesive surface, the silicone surface is bonded to one side of the substrate, and the acrylic adhesive surface is bonded to the light-shielding protective layer; The substrate and the light-shielding protective layer thereon are also provided with pull ears which are stacked together, and a protrusion is also provided on the pull ear of the substrate; the light-shielding protective layer is a red Mylar tape layer; The surface treatment-free anti-warping protective cover also includes: a double-sided antistatic silicone protective film, which is bonded to the other side of the substrate through another double-sided adhesive layer, one side of the double-sided adhesive layer is a silicone surface, and the other side is an acrylic adhesive surface, the silicone surface is bonded to the other side of the substrate, and the acrylic adhesive surface is bonded to the double-sided antistatic silicone protective film, and the double-sided antistatic silicone protective film has a first hollow structure at a position corresponding to the detection channel; the double-sided antistatic silicone protective film has a second hollow structure at a position corresponding to the broken groove, and the second hollow structure has one end extending to one side edge of the double-sided antistatic silicone protective film in the length direction, and the other end is close to the other side edge of the double-sided antistatic silicone protective film.

2. The surface treatment-free anti-warping protective cover according to claim 1, characterized in that: The substrate is L-shaped, and the detection channels are respectively arranged at the two ends and the middle corner positions of the L-shaped substrate.

3. The surface treatment-free anti-warping protective cover according to claim 2, characterized in that: An arc-shaped avoidance structure recessed inwardly is also provided on the inner side of the corner of the L-shaped substrate.

4. The surface treatment-free anti-warping protective cover according to claim 1, characterized in that: The light-shielding protective layer is also combined with a double-sided antistatic light-transmitting protective film.

5. A coil structure, characterized in that: The coiled material structure comprises: a material strip, and a surface treatment-free anti-warping protective cover as described in any one of claims 1 to 4 adhered to the material strip.