Semiconductor structure and method for forming the same
The electrode contact layer of the semiconductor structure is formed through the atomic layer deposition process, which solves the problem that the dielectric layer is easily broken down due to high surface roughness of the electrode layer, and improves electrical performance and reliability.
Patent Information
- Application Number
- CN201910471955.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-05-31
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2039-05-31
AI Technical Summary
The surface roughness of the electrode layer in the existing semiconductor structure is high, resulting in the dielectric layer being easily broken down and affecting electrical properties.
The first electrode contact layer and the second electrode contact layer are formed by atomic layer deposition process to reduce surface roughness, increase the thickness and stability of the dielectric layer, avoid protrusion points, and extend the shortest distance between the electrode layers.
It improves the electrical performance of the semiconductor structure, reduces the risk of breakdown of the dielectric layer, and enhances the reliability of the capacitor.
Smart Images

Figure CN112018241B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] A capacitor is a passive two-terminal electrical device used to store energy in an electric field. A capacitor comprises at least two electrodes separated by a dielectric layer. The capacitance of a capacitor is proportional to the area between the two electrodes and inversely proportional to the distance between the two electrodes (e.g., the thickness of the dielectric layer). Therefore, the capacitance of a capacitor can be increased by increasing the area of the electrodes, and / or by reducing the distance between them.
[0003] In today's VLSI, capacitors are commonly used passive devices. Because in analog RF circuits, capacitors with greater capacitance density and higher reliability are required, analog capacitors have shifted from polysilicon-insulator-polysilicon (PIP) to metal-insulator-metal (MIM). Summary of the invention
[0004] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, so as to optimize the electrical performance of the semiconductor structure.
[0005] To solve the above problems, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate; forming a first electrode layer on the substrate, the first electrode layer being a single-layer or multi-layer structure; forming a dielectric layer on the first electrode layer; forming a second electrode layer on the dielectric layer, the second electrode layer being a single-layer or multi-layer structure; the first electrode layer in contact with the dielectric layer is a first electrode contact layer, the second electrode layer in contact with the dielectric layer is a second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed using an atomic layer deposition process.
[0006] Correspondingly, an embodiment of the present invention also provides a semiconductor structure, including: a substrate; a first electrode layer, located on the substrate, the first electrode layer is a single-layer or multi-layer structure; a dielectric layer, located on the first electrode layer; a second electrode layer, located on the dielectric layer, the second electrode layer is a single-layer or multi-layer structure; the first electrode layer that contacts the dielectric layer is a first electrode contact layer, the second electrode layer that contacts the dielectric layer is a second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed using an atomic layer deposition process.
[0007] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0008] In the embodiment of the present invention, the first electrode layer in contact with the dielectric layer is the first electrode contact layer, and the second electrode layer in contact with the dielectric layer is the second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed by an atomic layer deposition process. The first electrode layer contact layer, or the second electrode layer contact layer, or the first electrode layer contact layer and the second electrode contact layer are formed by an atomic layer deposition process. The surface roughness of the layer structure formed by the atomic layer deposition process is low. Compared with the process method in which the first electrode contact layer and the second electrode contact layer simultaneously use a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer and the second electrode layer contact layer to have protrusions that protrude toward the dielectric layer at the same time, and the shortest distance between the first electrode layer contact layer and the second electrode layer contact layer becomes larger, so that the dielectric layer is not easy to be broken down, thereby improving the electrical performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 It is a schematic diagram of the structure of a semiconductor structure;
[0010] Figures 2 to 5 It is a schematic structural diagram corresponding to each step in the method for forming a semiconductor structure according to the first embodiment of the present invention;
[0011] Figure 6 is a structural schematic diagram of a method for forming a semiconductor structure in a second embodiment of the present invention;
[0012] Figure 7 It is a structural schematic diagram of a method for forming a semiconductor structure according to a third embodiment of the present invention. DETAILED DESCRIPTION
[0013] As can be seen from the background technology, the devices currently formed still have the problem of poor performance. The reasons for the poor performance of the devices are now analyzed in combination with a method for forming a semiconductor structure.
[0014] refer to Figure 1 A schematic structural diagram of a semiconductor structure is shown.
[0015] like Figure 1 As shown, the semiconductor structure includes: a substrate and a capacitor 1 located on the substrate. Specifically, the capacitor 1 includes a first metal layer 11 , a dielectric layer 12 located on the first metal layer 11 , and a second metal layer 13 located on the dielectric layer 12 .
[0016] The capacitor 1 is a MIM capacitor structure, the thickness of the dielectric layer 12 is only a dozen nanometers, or even several nanometers, and the first metal layer 11 and the second metal layer 13 are usually formed by a physical vapor deposition process (Physical Vapor Deposition, PVD), and the surfaces of the first metal layer 11 and the second metal layer 13 are in a columnar crystalline state, so that the surfaces of the first metal layer 11 and the second metal layer 13 have a high roughness. In the same area on the substrate, there are protrusions in the first metal layer 11 and the second metal layer 13 that are simultaneously protruding toward the dielectric layer 12. In this case, the shortest distance between the first metal layer 11 and the second metal layer 13 is much smaller than the design value, and thus the dielectric layer 12 is easily broken down, resulting in the MIM capacitor structure being prone to breakdown.
[0017] In order to solve the technical problem, an embodiment of the present invention provides a method for forming a semiconductor structure, including: providing a substrate; forming a first electrode layer on the substrate, the first electrode layer being a single-layer or multi-layer structure; forming a dielectric layer on the first electrode layer; forming a second electrode layer on the dielectric layer, the second electrode layer being a single-layer or multi-layer structure; the first electrode layer in contact with the dielectric layer is a first electrode contact layer, the second electrode layer in contact with the dielectric layer is a second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed using an atomic layer deposition process.
[0018] In order to solve the technical problem, in the embodiment of the present invention, the first electrode layer in contact with the dielectric layer is the first electrode contact layer, the second electrode layer in contact with the dielectric layer is the second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed by an atomic layer deposition process. The first electrode layer contact layer, or the second electrode layer contact layer, or the first electrode layer contact layer and the second electrode contact layer are formed by an atomic layer deposition process. The surface roughness of the layer structure formed by the atomic layer deposition process is low. Compared with the process method in which the first electrode contact layer and the second electrode contact layer are simultaneously formed with a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer and the second electrode layer contact layer to have protrusions that protrude toward the dielectric layer at the same time, and the shortest distance between the first electrode layer contact layer and the second electrode layer contact layer becomes larger, so that the dielectric layer is not easy to be broken down, thereby improving the electrical performance of the semiconductor structure.
[0019] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and easy to understand, specific embodiments of the embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0020] Figures 2 to 5 It is a schematic structural diagram corresponding to each step in the first embodiment of the method for forming a semiconductor structure according to an embodiment of the present invention.
[0021] refer to Figure 2 , providing a substrate.
[0022] The substrate provides a process foundation for the subsequent formation of semiconductor structures.
[0023] Specifically, the substrate includes an interlayer dielectric layer 100 , a connection metal layer 101 located in the interlayer dielectric layer 100 , and an anti-etching layer 102 located on the interlayer dielectric layer 100 and the connection metal layer 101 .
[0024] The connection metal layer 101 is a structure to be connected, and the connection metal layer 101 is used to electrically connect to a capacitor formed subsequently.
[0025] In this embodiment, the material of the connection metal layer 101 is Cu. In other embodiments, the material of the connection metal layer includes Al, Co or W.
[0026] It should be noted that there are multiple connecting metal layers 101 .
[0027] The interlayer dielectric layer 100 is used to achieve electrical isolation between multiple connection metal layers 101 .
[0028] The material of the interlayer dielectric layer 100 is an ultra low K dielectric material (ULK), where the ultra low k dielectric material refers to a dielectric material with a relative dielectric constant less than 2.6. The use of the ultra low K dielectric material for the interlayer dielectric layer 100 can effectively reduce the parasitic capacitance of the connecting metal layer 101, thereby reducing the back end of line (BEOL) RC delay.
[0029] In this embodiment, the material of the interlayer dielectric layer 100 is porous silicon oxide. In other embodiments, the material of the interlayer dielectric layer may also be SiOCH.
[0030] Subsequently, a capacitor connected to the connection metal layer 101 is formed on the anti-etching layer 102 . The etch stop layer 102 is used to define the position where the etching stops during the formation of the capacitor, and to protect the connection metal layer 101 and the interlayer dielectric layer 100 .
[0031] Specifically, the material of the anti-etching layer 102 includes one or more materials selected from silicon oxide, silicon carbonitride, silicon carbon nitride oxide, silicon nitride oxide, boron nitride, boron carbonitride and silicon nitride containing C. In this embodiment, the material of the anti-etching layer 102 is silicon nitride containing C.
[0032] It should be noted that the thermal expansion coefficient of the material of the anti-etching layer 102 and the material of the first electrode layer in the capacitor formed subsequently is quite different. If the first electrode layer is directly formed on the anti-etching layer 102, the first electrode layer is prone to delamination or even cracking from the anti-etching layer 102, resulting in poor quality of capacitor formation. Therefore, in this embodiment, the formation method further includes: forming a buffer layer 103 between the anti-etching layer 102 and the first electrode layer, and the buffer layer 103 plays a role of stress buffering.
[0033] In this embodiment, the material of the buffer layer 103 is silicon oxide.
[0034] It should be noted that the density of the buffer layer 103 is greater than that of the interlayer dielectric layer 100 . The higher density of silicon oxide is beneficial to improving the adhesion between the buffer layer 103 and the anti-etching layer 102 and the subsequent first electrode layer, thereby improving the formation quality of the semiconductor structure.
[0035] In other embodiments, the material of the buffer layer includes a low-k dielectric material (a low-k dielectric material refers to a dielectric material having a relative dielectric constant greater than or equal to 2.6 and less than or equal to 3.9) or an ultra-low-k dielectric material (an ultra-low-k dielectric material refers to a dielectric material having a relative dielectric constant less than 2.6), for example: SiOH, SiOCH, FSG, BSG, PSG, BPSG, hydrogenated silsesquioxane or methyl silsesquioxane.
[0036] refer to Figure 3 , a first electrode layer 104 is formed on the substrate, and the first electrode layer 104 is a single-layer or multi-layer structure.
[0037] The first electrode layer 104 , the subsequently formed dielectric layer, and the second electrode layer together form a capacitor, which is a MIM capacitor.
[0038] The first electrode layer 104 is used as a bottom plate of the MIM capacitor and is connected to the connection metal layer 101 .
[0039] It should be noted that the first electrode layer 104 that contacts the subsequently formed dielectric layer is the first electrode contact layer 1041 .
[0040] In this embodiment, the material of the first electrode contact layer 1041 is a metal material.
[0041] Specifically, the material of the first electrode contact layer 1041 is metal nitride, which is an inert metal. Thus, the first electrode contact layer 1041 has high stability, making it difficult for metal ions to diffuse.
[0042] In this embodiment, the material of the first electrode contact layer 1041 is one or both of TiN and TaN. The work functions of TaN and TiN are relatively high, so that electrons are not likely to transition, and the capacitor formed subsequently is not likely to leak. In this embodiment, the material of the first electrode contact layer 1041 includes TiN.
[0043] In this embodiment, the first electrode contact layer 1041 is formed by an atomic layer deposition (ALD) process. The atomic layer deposition process includes performing multiple atomic layer deposition cycles to form the first electrode contact layer 1041 of the desired thickness. By selecting the atomic layer deposition process, it is beneficial to improve the thickness uniformity of the first electrode contact layer 1041, so that the thickness of the first electrode contact layer 1041 can be accurately controlled; in addition, the atomic layer deposition process has good gap filling performance and step coverage, which correspondingly improves the conformal coverage ability of the first electrode contact layer 1041. In other embodiments, other deposition processes may also be used to form the first electrode contact layer, such as: organic metal chemical vapor deposition method, etc.
[0044] It should be noted that the first electrode contact layer 1041 should not be too thick or too thin. If the first electrode contact layer 1041 is too thick, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. If the first electrode contact layer 1041 is too thin, it is easy to reduce the thickness uniformity and film quality of the first electrode contact layer 1041, as well as the covering ability of the first electrode contact layer 1041 on the substrate. The first electrode contact layer 1041 is not easy to cover the rough points of the layer structure below the first electrode contact layer 1041, so that there are protruding points in the first electrode contact layer 1041 that protrude toward the dielectric layer 106. Subsequently, a second electrode layer is formed on the dielectric layer, and the second electrode contact layer is in contact with the dielectric layer in the second electrode layer. Therefore, in the same area, the distance between the first electrode contact layer 1041 and the second electrode contact layer is the shortest and closer, and then the dielectric layer 106 is prone to breakdown. In this embodiment, the thickness of the first electrode contact layer 1041 is 1 nanometer to 15 nanometers.
[0045] The step of forming the first electrode layer 104 further includes: before forming the first electrode contact layer 1041 , forming a third electrode film 1042 on the substrate.
[0046] The first electrode contact layer 1041 and the third electrode film 1042 are used together as the lower plate of the MIM capacitor.
[0047] In this embodiment, the material of the third electrode film 1042 is a metal material.
[0048] Specifically, the material of the third electrode film 1042 is metal nitride, which is an inert metal. Thus, the third electrode film 1042 has high stability, making it difficult for metal ions to diffuse.
[0049] In this embodiment, the material of the third electrode film 1042 is one or both of TiN and TaN. TaN and TiN have relatively high work functions, so that electrons are not likely to transition, and thus the capacitor formed subsequently is not likely to leak electricity. In this embodiment, the material of the third electrode film 1042 includes TiN.
[0050] The first electrode contact layer 1041 and the third electrode film 1042 are made of the same material, which effectively avoids interface problems and electrical performance degradation problems caused by different materials and improves process compatibility and semiconductor structure stability.
[0051] It should be noted that the thickness of the third electrode film 1042 should not be too small or too large. If the thickness of the third electrode film 1042 is too small, the film quality of the third electrode film 1042 is poor, which may reduce the quality of the first electrode contact layer 1041; if the thickness of the third electrode film 1042 is too large, the height of the device may be too large, which may have an adverse effect on the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the third electrode film 1042 is 30 nanometers to 80 nanometers.
[0052] In this embodiment, the third electrode film 1042 is formed by a physical vapor deposition process, which has the advantages of simple process, low pollution, low process cost, dense film formation, and strong bonding with other film structures.
[0053] It should be noted that the MIM capacitor is formed between adjacent metal layers in the back-end process, so the first electrode layer 104 is located in a partial area on the substrate.
[0054] It should also be noted that after forming the third electrode film 1042, the third electrode film 1042 is also cleaned and dried with an inert gas, so that the surface of the third electrode film 1042 is not easily contaminated, which is beneficial to improving the reliability of the semiconductor MIM capacitor.
[0055] like Figure 4 As shown, a dielectric layer 106 is formed on the first electrode layer 104 .
[0056] The dielectric layer 106 is used as an insulating layer in the MIM capacitor.
[0057] In this embodiment, the material of the dielectric layer 106 is a high-k dielectric material, wherein the high-k dielectric material refers to a dielectric material having a relative dielectric constant greater than that of silicon oxide. The use of a high-k dielectric material is conducive to increasing the capacitance value of the MIM capacitor.
[0058] Specifically, the dielectric layer 106 is a high-k dielectric layer formed by stacking, that is, the dielectric layer 106 is a high-k composite dielectric layer. When the thickness of the high-k dielectric layer reaches a certain value, its formation quality tends to deteriorate. Therefore, by using a high-k composite dielectric layer, the thickness of the dielectric layer 106 meets the process requirements while having better formation quality.
[0059] The material of the dielectric layer 106 includes binary oxides and ternary oxides.
[0060] Specifically, the binary oxide includes one or more of hafnium oxide, tantalum oxide, titanium oxide, hafnium oxide or lanthanum oxide; the ternary oxide includes one or more of SrTiO3, Zn2GeO4, NiCo2O4, Zn2SnO4, ZnFe2O4, ZnMnO3 and Fe2GeO4. In this embodiment, the material of the dielectric layer 106 includes hafnium oxide.
[0061] It should be noted that the dielectric layer 106 should not be too thick or too thin. It can be seen from the capacitance formula that the capacitance value of a single capacitor is inversely proportional to the thickness of the dielectric layer 106. If the dielectric layer 106 is too thick, the capacitance density becomes smaller, and it is not easy to meet the device requirements. If the dielectric layer 106 is too thin, it is easy to reduce the thickness uniformity and film quality of the dielectric layer 106, as well as the coverage ability of the dielectric layer 106 on the first electrode layer 104. In addition, it is also easy to cause the linearity between the capacitance value and the thickness of the dielectric layer 106 to decrease, breakdown and other problems. In this embodiment, the thickness of the material of the dielectric layer 106 is 5 nanometers to 12 nanometers.
[0062] In this embodiment, the dielectric layer 106 is formed by an atomic layer deposition process. The atomic layer deposition process includes performing multiple atomic layer deposition cycles to form a dielectric layer 106 of a desired thickness. By selecting the atomic layer deposition process, it is beneficial to improve the thickness uniformity of the dielectric layer 106, so that the thickness of the dielectric layer 106 can be accurately controlled; in addition, the atomic layer deposition process has good gap filling performance and step coverage, which correspondingly improves the conformal coverage ability of the dielectric layer 106. In other embodiments, when the dielectric layer is thicker, other deposition processes can also be used to form it, such as chemical vapor deposition.
[0063] refer to Figure 5 , a second electrode layer 105 is formed on the dielectric layer 106, and the second electrode layer 105 is a single-layer or multi-layer structure.
[0064] The second electrode layer 105 , the first electrode layer 104 and the dielectric layer 106 together form a capacitor, which is a MIM capacitor.
[0065] The second electrode layer 105 is used as a top plate of the MIM capacitor and is connected to a metal layer subsequently formed on the capacitor.
[0066] It should be noted that the second electrode layer 105 that contacts the dielectric layer 106 is the second electrode contact layer 1051 .
[0067] In this embodiment, the second electrode contact layer 1051 is formed by an atomic layer deposition process. The atomic layer deposition process includes performing multiple atomic layer deposition cycles to form the second electrode contact layer 1051 of the desired thickness. By selecting the atomic layer deposition process, it is beneficial to improve the thickness uniformity of the second electrode contact layer 1051, so that the thickness of the second electrode contact layer 1051 can be accurately controlled; in addition, the atomic layer deposition process has good gap filling performance and step coverage, which correspondingly improves the conformal coverage ability of the second electrode contact layer 1051. In other embodiments, other deposition processes can also be used to form the second electrode contact layer, such as: organic metal chemical vapor deposition method, etc.
[0068] The first electrode contact layer 1041 and the second electrode contact layer 1051 are both formed by an atomic layer deposition process, so the surface roughness of the first electrode contact layer 1041 and the second electrode contact layer 1051 is relatively low. Compared with a process method in which the first electrode contact layer and the second electrode contact layer are simultaneously formed by a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer 104 contact layer and the second electrode layer 105 contact layer to have protrusions that simultaneously protrude toward the dielectric layer 106, and the shortest distance between the first electrode layer 104 contact layer and the second electrode layer 105 contact layer becomes larger, so that the dielectric layer 106 is not easy to be punctured, thereby improving the electrical performance of the semiconductor structure.
[0069] In this embodiment, the shortest distance refers to the distance between the upper surface of the first electrode contact layer 1041 and the lower surface of the second electrode contact layer 1051 .
[0070] In this embodiment, the material of the second electrode contact layer 1051 is a metal material.
[0071] Specifically, the material of the second electrode contact layer 1051 is metal nitride, which is an inert metal. Thus, the second electrode contact layer 1051 has high stability, making it difficult for metal ions to diffuse.
[0072] In this embodiment, the material of the second electrode contact layer 1051 is one or both of TiN and TaN. The work functions of TaN and TiN are relatively high, so that electrons are not easy to transition, and the capacitor formed subsequently is not easy to leak. In this embodiment, the material of the second electrode contact layer 1051 includes TiN.
[0073] It should be noted that the second electrode contact layer 1051 should not be too thick or too thin. If the second electrode contact layer 1051 is too thick, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. If the second electrode contact layer 1051 is too thin, it is easy to reduce the thickness uniformity and film quality of the second electrode contact layer 1051, as well as the covering ability of the second electrode contact layer 1051 on the dielectric layer 106. The second electrode contact layer 1051 is not easy to cover the rough spots on the fourth electrode film formed subsequently, so that in the same area, the shortest distance between the second electrode contact layer 1051 and the second electrode contact layer is closer, and then the dielectric layer 106 is prone to breakdown. In this embodiment, the thickness of the second electrode contact layer 1051 is 1 nanometer to 15 nanometers.
[0074] The step of forming the second electrode layer 105 further includes: after forming the second electrode contact layer 1051 , forming a fourth electrode film 1052 on the second electrode contact layer 1051 .
[0075] The second electrode contact layer 1051 and the fourth electrode film 1052 together serve as the upper plate of the MIM capacitor. The second electrode layer 105 is connected to a metal subsequently formed on the capacitor.
[0076] To this end, the fourth electrode film 1052 is made of metal material.
[0077] Specifically, the material of the fourth electrode film 1052 is metal nitride, which is an inert metal. Thus, the fourth electrode film 1052 has high stability, making it difficult for metal ions to diffuse.
[0078] In this embodiment, the material of the fourth electrode film 1052 is one or both of TiN and TaN. TaN and TiN have relatively high work functions, so that electrons are not likely to transition, and the capacitor formed subsequently is not likely to leak. In this embodiment, the material of the fourth electrode film 1052 includes TiN.
[0079] The second electrode contact layer 1051 and the fourth electrode film 1052 are made of the same material, which effectively avoids interface problems and electrical performance degradation problems caused by different materials and improves process compatibility and semiconductor structure stability.
[0080] In this embodiment, the fourth electrode film 1052 is formed by a physical vapor deposition process. For specific advantages, reference may be made to the corresponding description of the third electrode film 1042, which will not be repeated here.
[0081] It should be noted that the thickness of the fourth electrode film 1052 should not be too small or too large. If the thickness of the fourth electrode film 1052 is too small, it is easy to cause the film quality of the fourth electrode film 1052 to be poor, and thus it is easy to reduce the formation quality of the formed MIM capacitor; if the thickness of the fourth electrode film 1052 is too large, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the fourth electrode film 1052 is 30 nanometers to 80 nanometers.
[0082] It should also be noted that after forming the fourth electrode film 1052, the fourth electrode film 1052 is also cleaned and dried with an inert gas so that the surface of the fourth electrode film 1052 is not easily contaminated, which is beneficial to improving the reliability of the semiconductor MIM capacitor.
[0083] In other embodiments, the method for forming the semiconductor structure may further include: forming a first electrode contact layer and a second electrode contact layer in contact with the dielectric layer by an atomic layer deposition process, without forming a third electrode film and a fourth electrode film, and accordingly, the thickness of the first electrode contact layer and the second electrode contact layer is adaptively adjusted according to design requirements;
[0084] Alternatively, the third electrode film is not formed, and the fourth electrode film is formed, and the thickness of the first electrode contact layer is adaptively adjusted according to design requirements;
[0085] Alternatively, the third electrode film is formed but the fourth electrode film is not formed, and the thickness of the second electrode contact layer is adaptively adjusted according to design requirements.
[0086] refer to Figure 6 The present invention also proposes a second method for forming a semiconductor structure, the specific contents of which are as follows:
[0087] The similarities between the embodiment of the present invention and the first embodiment are not repeated here. The difference between the embodiment of the present invention and the first embodiment is that the first electrode layer 204 in contact with the dielectric layer 206 is the first electrode contact layer 2041, the second electrode layer in contact with the dielectric layer 206 is the second electrode contact layer 2051, and the first electrode contact layer 2041 is formed by an atomic layer deposition process.
[0088] The first electrode contact layer 2041 is formed by an atomic layer deposition process. The surface roughness of the first electrode layer contact layer 2041 is relatively low. Compared with a process method in which the first electrode contact layer and the second electrode contact layer are simultaneously formed by a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer 2041 and the second electrode layer contact layer 2051 to have protrusions that simultaneously protrude toward the dielectric layer 206. The shortest distance between the first electrode layer contact layer 2041 and the second electrode layer contact layer 2051 becomes larger, and thus the dielectric layer 206 is not easy to be punctured, thereby improving the electrical performance of the semiconductor structure.
[0089] In this embodiment, the material, thickness and formation method of the first electrode contact layer 2041 are as described in the first embodiment and will not be described again herein.
[0090] In this embodiment, the material, thickness and formation method of the third electrode film are as described in the first embodiment and will not be repeated here.
[0091] In this embodiment, the second electrode contact layer 2051 is formed by physical vapor deposition process. The physical vapor deposition process has the advantages of simple process, low pollution, low process cost, dense film formation, and strong bonding with other film structures.
[0092] It should be noted that the thickness of the second electrode contact layer 2051 should not be too small or too large. If the thickness of the second electrode contact layer 2051 is too small, the film quality of the second electrode contact layer 2051 is likely to be poor, which may reduce the quality of the formed MIM capacitor; if the thickness of the second electrode contact layer 2051 is too large, the process time may be too long, and the height of the formed device may be too large, which may be detrimental to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the second electrode contact layer 2051 is 31 nanometers to 95 nanometers.
[0093] In this embodiment, the material of the second electrode contact layer 2051 is not described in detail here.
[0094] In this embodiment, the fourth electrode film is not formed.
[0095] In other embodiments, the method for forming the semiconductor structure may further include: forming the first electrode contact layer only by atomic layer deposition process, without forming the third electrode film and the fourth electrode film, and adaptively adjusting the thickness of the first electrode contact layer and the second electrode contact layer.
[0096] refer to Figure 7 The present invention also proposes a third method for forming a semiconductor structure, the specific contents of which are as follows:
[0097] The similarities between the embodiment of the present invention and the first embodiment are not repeated here. The difference between the embodiment of the present invention and the first embodiment is that the first electrode layer in contact with the dielectric layer 306 is the first electrode contact layer 3041, and the second electrode layer 305 in contact with the dielectric layer 306 is the second electrode contact layer 3051, and the second electrode contact layer 3051 is formed by an atomic layer deposition process.
[0098] The second electrode contact layer 3051 is formed by an atomic layer deposition process. The surface roughness of the second electrode layer contact layer 3051 is relatively low. Compared with the first electrode contact layer and the second electrode contact layer simultaneously using a process method with a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer 3041 and the second electrode layer contact layer 3051 to have protrusions that protrude toward the dielectric layer 306 at the same time, and the shortest distance between the first electrode layer contact layer 3041 and the second electrode layer contact layer 3051 becomes larger, so that the dielectric layer 306 is not easy to be punctured, thereby improving the electrical performance of the semiconductor structure.
[0099] In this embodiment, the material, thickness and formation method of the second electrode contact layer 3051 are as described in the first embodiment and will not be described again herein.
[0100] In this embodiment, the material, thickness and formation method of the fourth electrode film are as described in the first embodiment and will not be repeated here.
[0101] In this embodiment, the first electrode contact layer 3041 is formed by a physical vapor deposition process. The physical vapor deposition process has the advantages of simple process, low pollution, low process cost, dense film formation, and strong bonding with other film structures.
[0102] It should be noted that the thickness of the first electrode contact layer 3041 should not be too small or too large. If the thickness of the first electrode contact layer 3041 is too small, it is easy to cause the film quality of the first electrode contact layer 3041 to be poor, and then it is easy to reduce the formation quality of the dielectric layer 306; if the thickness of the first electrode contact layer 3041 is too large, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the first electrode contact layer 3041 is 31 nanometers to 95 nanometers.
[0103] In this embodiment, the material of the first electrode contact layer 3041 is not described in detail here.
[0104] In this embodiment, the third electrode film is not formed.
[0105] In other embodiments, the method for forming the semiconductor structure may further include: forming the second electrode contact layer only by atomic layer deposition process, without forming the third electrode film and the fourth electrode film, and adaptively adjusting the thickness of the first electrode contact layer and the second electrode contact layer.
[0106] Correspondingly, an embodiment of the present invention further provides a semiconductor structure. Figure 5 FIG. 4 is a schematic structural diagram of a first embodiment of a semiconductor structure of the present invention.
[0107] refer to Figure 5 The semiconductor structure includes: a substrate; a first electrode layer 104, located on the substrate, and the first electrode layer 104 is a single-layer or multi-layer structure; a dielectric layer 106, located on the first electrode layer 104; a second electrode layer 105, located on the dielectric layer 106, and the second electrode layer 105 is a single-layer or multi-layer structure; the first electrode layer 104 in contact with the dielectric layer 106 is a first electrode contact layer 1041, and the second electrode layer 105 in contact with the dielectric layer 106 is a second electrode contact layer 1051, and at least one of the first electrode contact layer 1041 and the second electrode contact layer 1051 is formed by an atomic layer deposition process.
[0108] In the embodiment of the present invention, the first electrode layer 104 in contact with the dielectric layer 106 is the first electrode contact layer 1041, and the second electrode layer 105 in contact with the dielectric layer 106 is the second electrode contact layer 1051. The first electrode contact layer 1041 and the second electrode contact layer 1051 are both formed by atomic layer deposition process, so the surface roughness of the first electrode contact layer 1041 and the second electrode contact layer 1051 is relatively low. Compared with the process method in which the first electrode contact layer and the second electrode contact layer are simultaneously formed by atomic layer deposition, in the same area, it is not easy for protrusions that protrude toward the dielectric layer 106 at the same time in the first electrode layer 104 contact layer and the second electrode layer 105 contact layer, and the shortest distance between the first electrode layer 104 contact layer and the second electrode layer 105 contact layer becomes larger, so that the dielectric layer 106 is not easy to be broken down, thereby improving the electrical performance of the semiconductor structure.
[0109] The substrate provides the process basis for forming the semiconductor structure.
[0110] Specifically, the substrate includes an interlayer dielectric layer 100 , a connection metal layer 101 located in the interlayer dielectric layer 100 , and an anti-etching layer 102 located on the interlayer dielectric layer 100 and the connection metal layer 101 .
[0111] The connection metal layer 101 is a structure to be connected, and the connection metal layer 101 is used to be electrically connected to the capacitor.
[0112] In this embodiment, the material of the connection metal layer 101 is Cu. In other embodiments, the material of the connection metal layer includes Al, Co or W.
[0113] It should be noted that there are multiple connecting metal layers 101 .
[0114] The interlayer dielectric layer 100 is used to achieve electrical isolation between multiple connection metal layers 101 .
[0115] The material of the interlayer dielectric layer 100 is an ultra-low K dielectric material, where the ultra-low K dielectric material refers to a dielectric material with a relative dielectric constant less than 2.6. The use of the ultra-low K dielectric material for the interlayer dielectric layer 100 can effectively reduce the parasitic capacitance of the connecting metal layer 101, thereby reducing the back-end RC delay.
[0116] In this embodiment, the material of the interlayer dielectric layer 100 is porous silicon oxide. In other embodiments, the material of the interlayer dielectric layer may also be SiOCH.
[0117] The etching stop layer 102 is used to define the etching stop position in the process of forming the capacitor, and to protect the connection metal layer 101 and the interlayer dielectric layer 100 .
[0118] Specifically, the material of the anti-etching layer 102 includes one or more materials selected from silicon oxide, silicon carbonitride, silicon carbon nitride oxide, silicon nitride oxide, boron nitride, boron carbonitride and silicon nitride containing C. In this embodiment, the material of the anti-etching layer 102 is silicon nitride containing C.
[0119] It should be noted that the thermal expansion coefficients of the material of the anti-etching layer 102 and the material of the first electrode layer 104 are quite different. If the first electrode layer 104 is directly formed on the anti-etching layer 102, the first electrode layer 104 is prone to delamination or even cracking from the anti-etching layer 102, resulting in poor quality of capacitor formation. Therefore, a buffer layer 103 is formed between the anti-etching layer 102 and the first electrode layer 104, and the buffer layer 103 plays a role of stress buffering.
[0120] In this embodiment, the material of the buffer layer 103 is silicon oxide.
[0121] It should be noted that the density of the buffer layer 103 is greater than that of the interlayer dielectric layer 100 . The higher density of silicon oxide is beneficial to improving the adhesion between the buffer layer 103 and the anti-etching layer 102 and the first electrode layer 104 , thereby improving the formation quality of the semiconductor structure.
[0122] In other embodiments, the material of the buffer layer includes a low-k dielectric material (a low-k dielectric material refers to a dielectric material having a relative dielectric constant greater than or equal to 2.6 and less than or equal to 3.9) or an ultra-low-k dielectric material (an ultra-low-k dielectric material refers to a dielectric material having a relative dielectric constant less than 2.6), for example: SiOH, SiOCH, FSG, BSG, PSG, BPSG, hydrogenated silsesquioxane or methyl silsesquioxane.
[0123] The first electrode layer 104 , the dielectric layer 106 and the second electrode layer 105 together form a capacitor, which is a MIM capacitor.
[0124] The first electrode layer 104 is used as a lower plate of the MIM capacitor and is connected to the connection metal layer 101 .
[0125] It should be noted that the first electrode layer 104 that contacts the dielectric layer 106 is the first electrode contact layer 1041 .
[0126] In this embodiment, the material of the first electrode contact layer 1041 is a metal material.
[0127] Specifically, the material of the first electrode contact layer 1041 is metal nitride, which is an inert metal. Thus, the first electrode contact layer 1041 has high stability, making it difficult for metal ions to diffuse.
[0128] In this embodiment, the material of the first electrode contact layer 1041 is one or both of TiN and TaN. The work functions of TaN and TiN are relatively high, so that electrons are not easy to transition, and thus the capacitor is not easy to leak. In this embodiment, the material of the first electrode contact layer 1041 includes TiN.
[0129] In this embodiment, the first electrode contact layer 1041 is formed by an atomic layer deposition process, wherein the atomic layer deposition process includes performing multiple atomic layer deposition cycles, and the surface roughness of the first electrode contact layer 1041 is relatively low.
[0130] It should be noted that the first electrode contact layer 1041 should not be too thick or too thin. If the first electrode contact layer 1041 is too thick, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. If the first electrode contact layer 1041 is too thin, it is easy to reduce the thickness uniformity and film quality of the first electrode contact layer 1041. The first electrode contact layer 1041 is not easy to cover the rough points of the layer structure below the first electrode contact layer 1041, so that there are protruding points protruding toward the dielectric layer 106 in the first electrode contact layer 1041, and the second electrode contact layer 1041 is in contact with the dielectric layer 106 in the second electrode layer 105, so that in the same area, the shortest distance between the first electrode contact layer 1041 and the second electrode contact layer is close, and the dielectric layer 106 is prone to breakdown. In this embodiment, the thickness of the first electrode contact layer 1041 is 1 nanometer to 15 nanometers.
[0131] The first electrode layer 104 further includes: a third electrode film 1042 located below the first electrode contact layer 1041 .
[0132] The first electrode contact layer 1041 and the third electrode film 1042 are used together as the lower plate of the MIM capacitor.
[0133] In this embodiment, the material of the third electrode film 1042 is a metal material.
[0134] Specifically, the material of the third electrode film 1042 is metal nitride, which is an inert metal. Thus, the third electrode film 1042 has high stability, making it difficult for metal ions to diffuse.
[0135] In this embodiment, the material of the third electrode film 1042 is one or both of TiN and TaN. TaN and TiN have relatively high work functions, so that electrons are not likely to transition, and thus the capacitor is not likely to leak electricity. In this embodiment, the material of the third electrode film 1042 includes TiN.
[0136] The first electrode contact layer 1041 and the third electrode film 1042 are made of the same material, which effectively avoids interface problems and electrical performance degradation problems caused by different materials, and improves process compatibility and semiconductor structure stability.
[0137] It should be noted that the thickness of the third electrode film 1042 should not be too small or too large. If the thickness of the third electrode film 1042 is too small, it is easy to cause the film quality of the third electrode film 1042 to be poor, resulting in poor formation quality of the first electrode contact layer 1041; if the thickness of the third electrode film 1042 is too large, it will cause the height of the device to be too large, which is easy to have an adverse effect on the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the third electrode film 1042 is 30 nanometers to 80 nanometers.
[0138] It should be noted that the MIM capacitor is formed between adjacent metal layers, so the first electrode layer 104 is located in a partial area on the substrate.
[0139] The dielectric layer 106 is used as an insulating layer in the MIM capacitor.
[0140] In this embodiment, the material of the dielectric layer 106 is a high-k dielectric material, wherein the high-k dielectric material refers to a dielectric material having a relative dielectric constant greater than that of silicon oxide. The use of a high-k dielectric material is conducive to increasing the capacitance value of the MIM capacitor.
[0141] Specifically, the dielectric layer 106 is a high-k dielectric layer formed by stacking, that is, the dielectric layer 106 is a high-k composite dielectric layer. When the thickness of the high-k dielectric layer reaches a certain value, its formation quality tends to deteriorate. Therefore, by using a high-k composite dielectric layer, the thickness of the dielectric layer 106 meets the process requirements while having better formation quality.
[0142] The material of the dielectric layer 106 includes binary oxides and ternary oxides.
[0143] Specifically, the binary oxide includes one or more of hafnium oxide, tantalum oxide, titanium oxide, hafnium oxide or lanthanum oxide; the ternary oxide includes one or more of SrTiO3, Zn2GeO4, NiCo2O4, Zn2SnO4, ZnFe2O4, ZnMnO3 and Fe2GeO4. In this embodiment, the material of the dielectric layer 106 includes hafnium oxide.
[0144] It should be noted that the dielectric layer 106 should not be too thick or too thin. It can be seen from the capacitance formula that the capacitance value of a single capacitor is inversely proportional to the thickness of the dielectric layer 106. If the dielectric layer 106 is too thick, the capacitance density becomes smaller, and it is not easy to meet the device requirements. If the dielectric layer 106 is too thin, it is easy to cause the thickness uniformity and film quality of the dielectric layer 106 to be poor. In addition, it is also easy to cause the linearity between the capacitance value and the thickness of the dielectric layer 106 to decrease, breakdown and other problems. In this embodiment, the thickness of the material of the dielectric layer 106 is 5 nanometers to 12 nanometers.
[0145] The second electrode layer 105 is used as the upper plate of the MIM capacitor and is connected to a metal layer subsequently formed on the capacitor.
[0146] It should be noted that the second electrode layer 105 that contacts the dielectric layer 106 is the second electrode contact layer 1051 .
[0147] In this embodiment, the material of the second electrode contact layer 1051 is a metal material.
[0148] Specifically, the material of the second electrode contact layer 1051 is metal nitride, which is an inert metal. Thus, the second electrode contact layer 1051 has high stability, making it difficult for metal ions to diffuse.
[0149] In this embodiment, the material of the second electrode contact layer 1051 is one or both of TiN and TaN. The work functions of TaN and TiN are relatively high, so that electrons are not likely to transition, and thus the capacitor is not likely to leak electricity. In this embodiment, the material of the second electrode contact layer 1051 includes TiN.
[0150] In this embodiment, the second electrode contact layer 1051 is formed by an atomic layer deposition process, and the atomic layer deposition process includes performing multiple atomic layer deposition cycles, so that the surface roughness of the second electrode contact layer 1051 is relatively low.
[0151] It should be noted that the second electrode contact layer 1051 should not be too thick or too thin. If the second electrode contact layer 1051 is too thick, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. If the second electrode contact layer 1051 is too thin, it is easy to reduce the thickness uniformity and film quality of the second electrode contact layer 1051, as well as the covering ability of the second electrode contact layer 1051 on the dielectric layer 106. The second electrode contact layer 1051 is not easy to cover the rough spots on the fourth electrode film 1052, so that in the same area, the shortest distance between the second electrode contact layer 1051 and the first electrode contact layer 1041 is closer, and the dielectric layer 106 is prone to breakdown. In this embodiment, the thickness of the second electrode contact layer 1051 is 1 nanometer to 15 nanometers.
[0152] The second electrode layer 105 further includes: a fourth electrode film 1052 located on the second electrode contact layer 1051 .
[0153] The second electrode contact layer 1051 and the fourth electrode film 1052 together serve as the upper plate of the MIM capacitor. The second electrode layer 105 is connected to a metal subsequently formed on the capacitor.
[0154] To this end, the fourth electrode film 1052 is made of metal material.
[0155] Specifically, the material of the fourth electrode film 1052 is metal nitride, which is an inert metal. Thus, the fourth electrode film 1052 has high stability, making it difficult for metal ions to diffuse.
[0156] Specifically, the material of the fourth electrode film 1052 is one or both of TiN and TaN. The work functions of TaN and TiN are relatively high, so that electrons are not likely to transition, and thus the capacitor is not likely to leak electricity. In this embodiment, the material of the fourth electrode film 1052 includes TiN.
[0157] The second electrode contact layer 1051 and the fourth electrode film 1052 are made of the same material, which effectively avoids interface problems and electrical performance degradation problems caused by different materials, and improves process compatibility and semiconductor structure stability.
[0158] It should be noted that the thickness of the fourth electrode film 1052 should not be too small or too large. If the thickness of the fourth electrode film 1052 is too small, it is easy to cause the film quality of the fourth electrode film 1052 to be poor, and thus it is easy to reduce the formation quality of the formed MIM capacitor; if the thickness of the fourth electrode film 1052 is too large, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the fourth electrode film 1052 is 30 nanometers to 80 nanometers.
[0159] In other embodiments, the semiconductor structure includes: a first electrode contact layer and a second electrode contact layer in contact with the dielectric layer formed by an atomic layer deposition process, and does not include a third electrode film and a fourth electrode film, and accordingly, the thicknesses of the first electrode contact layer and the second electrode contact layer are adaptively adjusted;
[0160] Alternatively, the third electrode film is not included but the fourth electrode film is included, and the thickness of the first electrode contact layer is adaptively adjusted;
[0161] Alternatively, the third electrode film is included but the fourth electrode film is not included, and the thickness of the second electrode contact layer is adaptively adjusted.
[0162] refer to Figure 6 It is a schematic diagram of the corresponding structure in the second embodiment of the semiconductor structure of the present invention.
[0163] The similarities between this embodiment and the first embodiment are not repeated here. The difference between this embodiment and the first embodiment is that the first electrode layer 204 is in contact with the dielectric layer 206 is the first electrode contact layer 2041, the second electrode layer is in contact with the dielectric layer 206 is the second electrode contact layer 2051, and the first electrode contact layer 2041 is formed by an atomic layer deposition process.
[0164] The first electrode contact layer 2041 is formed by an atomic layer deposition process. The surface roughness of the first electrode layer contact layer 2041 is relatively low. Compared with a process method in which the first electrode contact layer and the second electrode contact layer are simultaneously formed by a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer 2041 and the second electrode layer contact layer 2051 to have protrusions that simultaneously protrude toward the dielectric layer 206. The shortest distance between the first electrode layer contact layer 2041 and the second electrode layer contact layer 2051 becomes larger, and thus the dielectric layer 206 is not easy to be punctured, thereby improving the electrical performance of the semiconductor structure.
[0165] In this embodiment, the material and thickness of the first electrode contact layer 2041 are the same as those described in the first embodiment and will not be described again herein.
[0166] In this embodiment, the material and thickness of the third electrode film are the same as those described in the first embodiment and will not be described in detail herein.
[0167] It should be noted that the thickness of the second electrode contact layer 2051 should not be too small or too large. If the thickness of the second electrode contact layer 2051 is too small, it is easy to cause the film quality of the second electrode contact layer 2051 to be poor, and thus it is easy to reduce the formation quality of the formed MIM capacitor; if the thickness of the second electrode contact layer 2051 is too large, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the second electrode contact layer 2051 is 31 nanometers to 95 nanometers.
[0168] In this embodiment, the material of the second electrode contact layer 2051 is not described in detail here.
[0169] In this embodiment, the fourth electrode film is not included.
[0170] In other embodiments, the semiconductor structure includes: only the first electrode contact layer is formed by an atomic layer deposition process, and does not include a third electrode film and a fourth electrode film, and the thicknesses of the first electrode contact layer and the second electrode contact layer are adaptively adjusted.
[0171] refer to Figure 7 It is a schematic diagram of the corresponding structure in the second embodiment of the semiconductor structure of the present invention.
[0172] The similarities between this embodiment and the first embodiment are not repeated here. The difference between this embodiment and the first embodiment is that the first electrode layer in contact with the dielectric layer 306 is the first electrode contact layer 3041, and the second electrode layer 305 in contact with the dielectric layer 306 is the second electrode contact layer 3051, and the second electrode contact layer 3051 is formed by an atomic layer deposition process.
[0173] The second electrode contact layer 3051 is formed by an atomic layer deposition process. The surface roughness of the second electrode layer contact layer 3051 is relatively low. Compared with the first electrode contact layer and the second electrode contact layer simultaneously using a process method with a roughness greater than that of atomic layer deposition, in the same area, it is not easy for the first electrode layer contact layer 3041 and the second electrode layer contact layer 3051 to have protrusions that protrude toward the dielectric layer 306 at the same time, and the shortest distance between the first electrode layer contact layer 3041 and the second electrode layer contact layer 3051 becomes larger, so that the dielectric layer 306 is not easy to be punctured, thereby improving the electrical performance of the semiconductor structure.
[0174] In this embodiment, the material and thickness of the second electrode contact layer 3051 are the same as those described in the first embodiment and will not be described in detail herein.
[0175] In this embodiment, the material and thickness of the fourth electrode film are the same as those described in the first embodiment and will not be described in detail herein.
[0176] It should be noted that the thickness of the first electrode contact layer 3041 should not be too small or too large. If the thickness of the first electrode contact layer 3041 is too small, it is easy to cause the film quality of the first electrode contact layer 3041 to be poor, and then it is easy to reduce the formation quality of the dielectric layer 306; if the thickness of the first electrode contact layer 3041 is too large, it is easy to cause the process time to be too long, and the height of the formed device is too large, which is not conducive to the subsequent semiconductor process. For this reason, in this embodiment, the thickness of the first electrode contact layer 3041 is 31 nanometers to 95 nanometers.
[0177] In this embodiment, the material of the first electrode contact layer 3041 is not described in detail here.
[0178] In this embodiment, the third electrode film is not included.
[0179] In other embodiments, the semiconductor structure includes: only the second electrode contact layer is formed by an atomic layer deposition process, and does not include a third electrode film and a fourth electrode film, and the thicknesses of the first electrode contact layer and the second electrode contact layer are adaptively adjusted.
[0180] The semiconductor structure can be formed by the formation method described in the above embodiment, or by other formation methods. For the specific description of the semiconductor structure described in this embodiment, reference can be made to the corresponding description in the above embodiment, and this embodiment will not be repeated here.
[0181] Although the embodiments of the present invention are disclosed above, the embodiments of the present invention are not limited thereto. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the embodiments of the present invention. Therefore, the protection scope of the embodiments of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising an anti-etching layer; forming a first electrode layer on the substrate, wherein the first electrode layer is a multi-layer structure; The forming method further comprises: forming a buffer layer between the anti-etching layer and the first electrode layer; forming a dielectric layer on the first electrode layer; forming a second electrode layer on the dielectric layer, wherein the second electrode layer is a multi-layer structure; The portion of the first electrode layer in contact with the dielectric layer is a first electrode contact layer, and the material of the first electrode contact layer includes: one or both of TiN and TaN; the portion of the second electrode layer in contact with the dielectric layer is a second electrode contact layer, and at least one of the first electrode contact layer and the second electrode contact layer is formed by an atomic layer deposition process; The step of forming the first electrode layer also includes: before forming the first electrode contact layer, forming a third electrode film on the substrate, the first electrode contact layer and the third electrode film have the same material; the step of forming the second electrode layer also includes: after forming the second electrode contact layer, forming a fourth electrode film on the second electrode contact layer, the second electrode contact layer and the fourth electrode film have the same material.
2. The method for forming a semiconductor structure according to claim 1, wherein: The first electrode contact layer and the second electrode contact layer are both formed by an atomic layer deposition process.
3. The method for forming a semiconductor structure according to claim 2, wherein: The thickness of the first electrode contact layer is 1 nanometer to 15 nanometers.
4. The method for forming a semiconductor structure according to claim 2, wherein: The thickness of the second electrode contact layer is 1 nanometer to 15 nanometers.
5. The method for forming a semiconductor structure according to claim 1, wherein: The first electrode contact layer is a metal film.
6. The method for forming a semiconductor structure according to claim 1, wherein: The second electrode contact layer is a metal film.
7. The method for forming a semiconductor structure according to claim 5 or 6, characterized in that: The material of the metal film is metal nitride.
8. The method for forming a semiconductor structure according to claim 2, wherein: Forming the third electrode film by a physical vapor deposition process; The fourth electrode film is formed by a physical vapor deposition process.
9. The method for forming a semiconductor structure according to claim 2, wherein: The third electrode film is a metal film; The fourth electrode film is a metal film.
10. A semiconductor structure, characterized in that: include: A substrate, wherein the substrate comprises an anti-etching layer; A first electrode layer, located on the substrate, wherein the first electrode layer is a multi-layer structure; A buffer layer, located between the anti-etching layer and the first electrode layer; a dielectric layer, located on the first electrode layer; A second electrode layer, located on the dielectric layer, wherein the second electrode layer is a multi-layer structure; The portion of the first electrode layer in contact with the dielectric layer is a first electrode contact layer, and the portion of the second electrode layer in contact with the dielectric layer is a second electrode contact layer, at least one of the first electrode contact layer and the second electrode contact layer is formed by an atomic layer deposition process, and a material of the first electrode contact layer includes: one or both of TiN and TaN; The first electrode layer further includes: a third electrode film, located between the substrate and the first electrode contact layer, the first electrode contact layer and the third electrode film being made of the same material; The second electrode layer further includes: a fourth electrode film located on the second electrode contact layer, and the second electrode contact layer and the fourth electrode film are made of the same material.
11. The semiconductor structure according to claim 10, wherein: The first electrode contact layer and the second electrode contact layer are both formed by an atomic layer deposition process.
12. The semiconductor structure according to claim 11, wherein: The thickness of the first electrode contact layer is 1 nanometer to 15 nanometers.
13. The semiconductor structure according to claim 11, wherein: The thickness of the second electrode contact layer is 1 nanometer to 15 nanometers.
14. The semiconductor structure according to claim 10, wherein: The first electrode contact layer is a metal film.
15. The semiconductor structure according to claim 11, wherein: The second electrode contact layer is a metal film.
16. The semiconductor structure according to claim 14 or 15, characterized in that: The material of the metal film is metal nitride.
17. The semiconductor structure according to claim 11, wherein: The third electrode film is a metal film; The fourth electrode film is a metal film.