Semiconductor structure and method for forming the same
By forming a recessed node contact layer in the contact window of the semiconductor structure and adding contact plugs, the problem of increased contact resistance in DRAM devices is solved, and the performance and yield of the semiconductor structure are improved.
Patent Information
- Application Number
- CN201910644881.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-07-17
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2039-07-17
AI Technical Summary
As the DRAM size decreases, the resistance value of the contact window increases, resulting in slowing down the DRAM device speed, and even failing to test the chip electrical performance and low yield.
By forming a node contact layer with recesses within the contact window of the semiconductor structure, and forming a contact plug on the recesses, the contact area between the plug and the contact layer is increased and the contact resistance is reduced.
It effectively reduces the contact resistance of the semiconductor structure and improves the performance and product yield of DRAM devices.
Smart Images

Figure CN112242346B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing technology, and in particular to a semiconductor structure and a forming method thereof. Background Art
[0002] Dynamic Random Access Memory (DRAM) is a semiconductor device commonly used in electronic devices such as computers. It is composed of multiple storage cells, each of which usually includes a transistor and a capacitor. The gate of the transistor is electrically connected to the word line, the source is electrically connected to the bit line, and the drain is electrically connected to the capacitor. The word line voltage on the word line can control the opening and closing of the transistor, so that the data information stored in the capacitor can be read through the bit line, or the data information can be written into the capacitor.
[0003] The transistor and capacitor in each memory cell in the DRAM are electrically connected through a contact window. As the size of the DRAM becomes smaller and smaller, the size of the contact window is also reduced accordingly, which leads to an exponential increase in the contact resistance between the transistor and the capacitor. The high resistance of the contact window often causes the speed of the entire DRAM device to slow down, and even causes the failure of the chip electrical performance test, and sometimes even leads to a low yield or even a zero yield of the chip.
[0004] Therefore, how to reduce the resistance of the contact window and improve the performance of DRAM devices has become a technical problem that needs to be urgently solved in the current advanced semiconductor process. Summary of the invention
[0005] The present invention provides a semiconductor structure and a method for forming the same, which are used to solve the problem of relatively large internal contact resistance of the existing semiconductor structure, so as to improve the performance of the semiconductor structure and increase the yield of the semiconductor structure.
[0006] In order to solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising the following steps:
[0007] Providing a substrate, wherein the substrate has a dielectric layer and a contact window penetrating the dielectric layer;
[0008] forming a node contact layer in the contact window, wherein the node contact layer has a gap inside;
[0009] Etching the node contact layer to form a recess in the node contact layer using the gap;
[0010] A contact plug is formed on the recessed node contact layer.
[0011] Preferably, the characteristic size of the bottom of the depression is 10% to 60% of the characteristic size of the top of the depression.
[0012] Preferably, it also includes:
[0013] A metal silicide is formed in the surface region of the node contact layer.
[0014] Preferably, it also includes:
[0015] An isolation layer is formed on the sidewalls of the contact window.
[0016] In order to solve the above problem, the present invention further provides a method for forming a semiconductor structure, comprising the following steps:
[0017] Providing a substrate, wherein the substrate has a dielectric layer and a contact window penetrating the dielectric layer;
[0018] forming a node contact layer in the contact window;
[0019] forming a sidewall mask layer on the sidewall of the contact window;
[0020] Etching the node contact layer using the sidewall mask layer to form a recess in the node contact layer;
[0021] A contact plug is formed on the recessed node contact layer.
[0022] Preferably, it also includes:
[0023] The sidewall mask layer includes an isolation mask layer and a protection mask layer;
[0024] forming a lower recess in the node contact layer using the protection mask layer;
[0025] An upper recess is formed in the node contact using the isolation mask layer.
[0026] Preferably, it also includes:
[0027] The sidewall mask layer includes a multi-layer mask layer, and the multi-layer mask layer is used to form the stepped recess in the node contact layer.
[0028] Preferably, it also includes:
[0029] A metal silicide is formed in the surface region of the node contact layer.
[0030] Preferably, it also includes:
[0031] An isolation layer is formed on the sidewalls of the contact window.
[0032] In order to solve the above problem, the present invention further provides a semiconductor structure, comprising:
[0033] A substrate having a dielectric layer and a contact window penetrating the dielectric layer;
[0034] A node contact layer is located in the contact window, and a top of the node contact layer has a depression;
[0035] A contact plug is connected to the node contact layer.
[0036] Preferably, the side wall of the recess has an inflection point.
[0037] Preferably, the height of the inflection point ranges from 10% to 80% of the height of the depression.
[0038] Preferably, the characteristic size of the bottom of the depression is 10% to 60% of the characteristic size of the top of the depression.
[0039] In order to solve the above problem, the present invention further provides a semiconductor structure, comprising:
[0040] A substrate having a dielectric layer and a contact window penetrating the dielectric layer;
[0041] A node contact layer, located in the contact window, wherein the top of the node contact layer has a stepped depression;
[0042] A contact plug is connected to the node contact layer.
[0043] Preferably, the stepped recess comprises an upper recess and a lower recess, and the opening width of the upper recess is greater than that of the lower recess.
[0044] Preferably, it also includes:
[0045] An isolation layer, located on the sidewall surface of the contact window;
[0046] The metal silicide is located between the node contact layer and the contact plug.
[0047] The semiconductor structure and the method for forming the same provided by the present invention form a node contact layer with a recess so that part of the contact plug is located in the recess, thereby increasing the contact area between the contact plug and the node contact layer, achieving a reduction in the contact resistance between the node contact layer and the contact plug, and improving the performance of the semiconductor structure and the product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] Attached Figure 1 is a flow chart of a method for forming a semiconductor structure in a first embodiment of the present invention;
[0049] Attached Figure 2A-2G It is a schematic cross-sectional view of the main processes in the process of forming a semiconductor structure in the first embodiment of the present invention;
[0050] Attached Figure 3is a flow chart of a method for forming a semiconductor structure in a second embodiment of the present invention;
[0051] Attached Figures 4A-4K It is a schematic cross-sectional view of the main processes in the process of forming a semiconductor structure according to the second embodiment of the present invention. DETAILED DESCRIPTION
[0052] The specific implementation of the method for forming a semiconductor structure provided by the present invention is described in detail below with reference to the accompanying drawings.
[0053] Implementation Method 1
[0054] This embodiment provides a method for forming a semiconductor structure. Figure 1 is a flow chart of a method for forming a semiconductor structure in a first embodiment of the present invention, Figure 2A-2G 1 is a schematic cross-sectional view of the main process in the process of forming a semiconductor structure in the first embodiment of the present invention. The semiconductor structure described in this embodiment can be, but is not limited to, a DRAM device. Figure 1 , Figure 2A-2G As shown, the method for forming a semiconductor structure provided in this embodiment includes the following steps:
[0055] Step S11, providing a substrate 20, wherein the substrate 20 has a dielectric layer 21 and a contact window 24 penetrating the dielectric layer 21, such as Figure 2B shown.
[0056] Specifically, the substrate 20 may be a Si substrate, a Ge substrate, a SiGe substrate, SOI (Silicon On Insulator) or GOI (Germanium On Insulator), etc. In this embodiment, the substrate 20 is preferably a Si substrate.
[0057] The specific method for forming the contact window 24 on the substrate 20 may be: first, depositing a first mask layer 221 and a second mask layer 222 on the surface of the dielectric layer 21 in sequence, and forming a photoresist layer 223 with an opening on the surface of the second mask layer 222, such as Figure 2A Then, the dielectric layer 21 is etched from the opening to the surface of the substrate 20 to form the contact window 24; finally, the first mask layer 221, the second mask layer 222 and the photoresist layer 223 are removed to obtain Figure 2BThe structure shown in FIG. The material of the first mask layer 221 may be a carbon material; the material of the second mask layer 222 may be a silicon oxynitride material. A barrier layer 23 formed of a material such as silicon nitride may be provided between the substrate 20 and the dielectric layer 21, and the contact window 24 sequentially penetrates the dielectric layer 21 and the barrier layer 23 in a direction perpendicular to the substrate 20.
[0058] Step S12, forming a node contact layer 25 in the contact window 24, wherein the node contact layer 25 has a gap 251 inside. Figure 2C shown.
[0059] Specifically, the node contact layer 25 can be formed by filling the first conductive material in the contact window 24. The first conductive material can be a conductive material such as polysilicon, silicon germanium, etc. When the formed contact window 24 has a high aspect ratio, specifically, when the aspect ratio is greater than 5, in the process of filling the first conductive material in the contact window 24 using a thin film process such as a chemical vapor deposition process and a physical vapor deposition process, a gap 251 is generated in the node contact layer 25 due to insufficient filling. In one example, the distance H1 between the gap 251 and the substrate 20 is 80nm to 120nm.
[0060] Step S13, etching the node contact layer 25, and forming a recess 26 in the node contact layer 25 by using the gap 251, as shown in FIG. Figure 2D shown.
[0061] In this embodiment, the node contact layer 25 can be directly etched by dry etching process. Due to the presence of the gap 251, the V-shaped or U-shaped recess 26 is directly formed after etching. In the direction parallel to the substrate 20, the width of the bottom 262 of the recess 26 is smaller than the opening width of the top 261 of the recess 26, that is, the characteristic size of the bottom 262 of the recess 26 is smaller than the characteristic size of the top 261. Preferably, the distance H2 between the bottom 262 of the recess 26 and the substrate 20 is 70nm to 90nm.
[0062] In this embodiment, since the recess 26 is formed by etching to the gap 251, the sidewall surface of the recess 26 is not a smooth surface, but has a Figure 2DThe inflection point (i.e., turning point) structure shown in the dotted circle. The position of the inflection point is not limited and depends on the actual process requirements. Preferably, the side wall slope of the recess 26 above the inflection point is smaller than the side wall slope of the recess 26 below the inflection point. The height range of the inflection point is 10% to 80% of the height of the recess, and as an example, it can be 15%, 30%, 45%, and 60%. The recess height is the length in the vertical direction from the lowest point to the highest point on the surface of the node contact layer 25 of the recess 26, and the height of the inflection point is the length in the vertical direction from the lowest point on the surface of the node contact layer 25 of the recess 26 to the inflection point. The position is beneficial to both increasing the surface area of the node contact layer in the recessed area and filling the contact plug 29.
[0063] Those skilled in the art can adjust the relative proportional relationship between the characteristic dimensions of the bottom 262 and the top 261 of the recess 26 according to actual needs. In order to further effectively reduce the contact resistance inside the semiconductor structure and increase the process window for forming the contact plug 29, preferably, the characteristic dimension of the bottom 262 of the recess 26 is 10% to 60% of the characteristic dimension of the top 261 thereof.
[0064] Step S14, forming a contact plug 29 on the node contact layer 25 of the recess 26, such as Figure 2G shown.
[0065] Preferably, before forming the contact plug 29, the method for forming the semiconductor structure further includes the following steps:
[0066] A metal silicide 28 is formed on the surface region of the node contact layer 25 .
[0067] More preferably, the method for forming the semiconductor structure further comprises the following steps:
[0068] An isolation layer 27 is formed on the sidewalls of the contact window 24 .
[0069] Specifically, the dielectric layer 21 includes a first surface 211 facing the substrate 20 and a second surface 212 opposite to the first surface 211; in a direction perpendicular to the substrate 20, the top 261 of the recess 26 is located below the second surface 212, so that the contact window 24 exposes a portion of the dielectric layer 21. By controlling the etching time and / or the amount of etchant for etching the node contact layer 25, the height of the node contact layer 25 is lower than the dielectric layer 21 after etching, that is, the top 261 of the recess 26 located in the node contact layer 25 is below the second surface 212 of the dielectric layer 21.
[0070] The first conductive material forming the node contact layer 25 may be, but is not limited to, polysilicon. The following description will be made by taking the first conductive material being polysilicon as an example. After forming the recess 26, an atomic layer deposition process is used to deposit a first dielectric material to form the isolation layer 27 covering the surface of the contact window 24 (including the surface of the recess 26, the exposed sidewall surface of the dielectric layer 21, and the second surface 212 of the dielectric layer 21). Figure 2E As shown; then, the second surface 212 covering the dielectric layer 21 and the isolation layer 27 covering the surface of the recess 26 are removed by a dry etching process, and only the isolation layer 27 covering the side wall surface of the dielectric layer 21 exposed to the contact window 24 is retained; thereafter, metal ions are implanted along the recess 26 by an ion implantation process and an annealing process to form the metal silicide 28 in the surface area of the node contact layer 25, as shown Figure 2F Finally, the second conductive material is filled in the contact window 24, and combined with a chemical mechanical polishing (Chemical Mechanical Polishing, CMP) process, to form the contact plug 29 electrically contacting the metal silicide 28, such as Figure 2G As shown. The first dielectric material can be a metal compound such as TiN, TaN, or a non-metal compound such as silicon nitride, silicon oxide, etc. The metal ions injected along the recess 26 can be any one or a combination of cobalt ions, germanium ions, and nickel ions. The second conductive material can be, but is not limited to, tungsten metal.
[0071] In this embodiment, the filling process of the first conductive material is only performed once. By utilizing the gap 251 formed during deposition, the node contact layer 25 only needs to be etched once to form the recess 26 in the node contact layer 25, thereby greatly reducing the process flow and saving the production cost of the semiconductor structure. Moreover, since the recess 26 is formed on the top of the node contact layer 25, on the one hand, it is beneficial to form a larger area of the metal silicide 28 by subsequent ion implantation, thereby reducing the contact resistance between the node contact layer 25 and the contact plug 29; on the other hand, the characteristic size of the bottom 262 of the recess 26 is 10% to 60% of the characteristic size of the top 261 thereof, which is beneficial to the full filling of the contact plug 29, thereby ensuring the electrical performance of the semiconductor structure. In addition, by utilizing the feature that there are gaps in the filling process of the through hole with a high aspect ratio, the etching process can be simplified, and the V-shaped or U-shaped recess 26 can be formed by etching once, thereby further helping to reduce the contact resistance and improve the performance of the semiconductor structure.
[0072] This embodiment also provides a semiconductor structure. The schematic diagram of the semiconductor structure can be seen in Figure 2GThe semiconductor structure may be as follows: Figure 1 , Figure 2A-2G The method shown is formed. Figure 1 , Figure 2A-2G As shown, the semiconductor structure provided in this embodiment includes:
[0073] A substrate 20 having a dielectric layer 21 and a contact window 24 penetrating the dielectric layer 21;
[0074] A node contact layer 25 is located in the contact window 24, and a top of the node contact layer 25 has a depression;
[0075] The contact plug 29 is connected to the node contact layer 25 .
[0076] Preferably, the side wall of the recess has an inflection point.
[0077] Preferably, the height of the inflection point ranges from 10% to 80% of the height of the depression.
[0078] Preferably, the recess has a V-shape or a U-shape in a cross section along a direction perpendicular to the substrate.
[0079] Preferably, the characteristic size of the bottom 262 of the recess 26 is 10% to 60% of the characteristic size of the top 261 thereof.
[0080] The semiconductor structure and the method for forming the same provided in this embodiment form a node contact layer having a depression on the top so that part of the contact plug is located in the depression. By increasing the contact area between the contact plug and the node contact layer, the contact resistance between the node contact layer and the contact plug is reduced, thereby improving the performance of the semiconductor structure and the product yield.
[0081] Implementation Method 2
[0082] This embodiment provides a method for forming a semiconductor structure. Figure 3 is a flow chart of a method for forming a semiconductor structure in a second embodiment of the present invention, Figures 4A-4K This is a schematic cross-sectional view of the main processes in the process of forming a semiconductor structure in the second embodiment of the present invention. The same points as the first embodiment will not be described in detail in this embodiment, and the differences from the first embodiment will be mainly described below.
[0083] like Figure 3 , Figure 4A-Figure 4K As shown, this embodiment provides a method for forming a semiconductor structure, comprising the following steps:
[0084] Step S31, providing a substrate 30, wherein the substrate 30 has a dielectric layer 31 and a contact window 34 penetrating the dielectric layer 31, wherein the dielectric layer 31 includes a first surface 311 facing the substrate 30 and a second surface 312 opposite to the first surface 311, such as Figure 4B and Figure 4D shown.
[0085] Specifically, the substrate 30 may be a Si substrate, a Ge substrate, a SiGe substrate, SOI (Silicon On Insulator) or GOI (Germanium On Insulator), etc. In this embodiment, the substrate 30 is preferably a Si substrate.
[0086] The specific method for forming the contact window 34 on the substrate 30 may be: first, depositing a first mask layer 321 and a second mask layer 322 on the surface of the dielectric layer 31 in sequence, and forming a photoresist layer 323 with an opening on the surface of the second mask layer 322, such as Figure 4A Then, the dielectric layer 31 is etched from the opening to the surface of the substrate 30 to form the contact window 34; finally, the first mask layer 321, the second mask layer 322 and the photoresist layer 323 are removed to obtain Figure 4B The structure shown in FIG. The material of the first mask layer 321 may be a carbon material; the material of the second mask layer 322 may be a silicon oxynitride material. A barrier layer 33 formed of a material such as silicon nitride may be provided between the substrate 30 and the dielectric layer 31, and the contact window 34 sequentially penetrates the dielectric layer 31 and the barrier layer 33 in a direction perpendicular to the substrate 30.
[0087] Step S32, forming a node contact layer 35 in the contact window 34, such as Figure 4F shown.
[0088] Step S33, forming a sidewall mask layer on the sidewall of the contact window 34, such as Figure 4G shown.
[0089] Step S34, etching the node contact layer 35 using the sidewall mask layer to form a recess in the node contact layer 35, such as Figure 4J shown.
[0090] The present embodiment does not limit the specific shape of the recess. As long as the recess can be formed on the top of the node contact layer 35 , the contact resistance can be reduced by increasing the subsequent contact area with the contact plug 41 .
[0091] Preferably, the method for forming the node contact layer 35 comprises the following steps:
[0092] A node contact layer 35 is formed in the contact window 34, such as Figure 4E As shown, specifically, a node contact layer 35 is formed in the contact window 34 and on the second surface 312 of the dielectric layer 31 by using a thin film process such as CVD, PVD or ALD; a portion of the node contact layer 35 on the second surface 312 of the dielectric layer 31 and in the contact window 34 is removed by an etching process, and a groove 36 is formed in the contact window 34, as shown in FIG. Figure 4F shown.
[0093] Preferably, the method for forming the node contact layer 35 further comprises the following steps:
[0094] A node contact layer 35 is formed in the contact window 34, and a gap 351 is formed in the node contact layer 35. Figure 4C As shown;
[0095] The node contact layer 35 is etched back to the gap 351 to form an initial trench 352. Figure 4D As shown;
[0096] A first conductive material is filled along the contact window 34. Preferably, the first conductive material is the same as the node contact layer material. The first conductive material covers the initial groove 352 to form a node contact layer 35 without gaps. Figure 4E As shown; the node contact layer 35 without gaps is etched back again to form the groove 36, as shown Figure 4F shown.
[0097] Specifically, since the formed contact window 34 has a high aspect ratio, when a thin film process such as CVD, PVD or ALD is used to form a node contact layer 35 in the contact window 34, the gap 351 will be generated in the node contact layer 35 due to insufficient filling. Among them, the distance H1 between the gap 351 and the substrate 30 is 80nm to 120nm. After the node contact layer 35 is filled in the contact window 34, first, the node contact layer 35 having the gap 351 is etched back for the first time by a dry etching process to expose the gap 351, and the node contact layer 35 having the gap 351 is formed in the contact window 34. Figure 4D Then, the first conductive material is filled into the contact window 34 again. Since the filling height of this step is small, the first conductive material can completely fill the initial groove 352 to form the node contact layer 35 without gaps. Figure 4EAs shown; then, the node contact layer 35 without a gap is etched back by a dry etching process until the height H3 from the substrate 30 is 120nm to 150nm, forming the groove 36 (that is, the distance between the bottom of the groove 36 and the substrate 30 is 120nm to 150nm), as shown Figure 4F As shown, during the second back etching, there is no void inside the node contact layer 35 because the characteristic size of the bottom of the formed trench 36 is the same as or similar to the characteristic size of the top.
[0098] Preferably, the method for forming the semiconductor structure further comprises:
[0099] A first dielectric material is deposited on the bottom surface of the trench, the sidewall of the trench and the surface of the substrate, and the first dielectric material on the bottom surface of the trench and the surface of the substrate is removed by a dry etching process.
[0100] Specifically, the first dielectric material may be silicon oxide, silicon nitride, etc. The first dielectric material retained on the sidewall of the trench is a sidewall mask layer, and a portion of the node contact layer is etched using the sidewall mask layer to form a recess in the node contact layer.
[0101] Preferably, the method for forming the semiconductor structure further comprises the following steps:
[0102] The sidewall mask layer includes an isolation mask layer 37 and a protection mask layer 38, and the protection mask layer 38 is located on the surface of the isolation mask layer 37;
[0103] Using the protective mask layer 38 to form a lower recess 391 in the node contact layer;
[0104] Using the isolation mask layer 37 to form an upper recess 392 in the node contact layer;
[0105] The bottom of the upper recess 392 is higher than the bottom of the lower recess 391 .
[0106] Specifically, after forming the groove 36, the first dielectric material and the second dielectric material are sequentially deposited along the groove 36 by an atomic layer deposition process to form the isolation mask layer 37 and the protection mask layer 38 covering the surface of the isolation mask layer 37. Figure 4G As shown;
[0107] Then, the second surface of the dielectric layer 31 and the protective mask layer 38 at the bottom of the groove 36 are removed by a dry etching process, and only the protective mask layer 38 located at the side wall of the contact window 34 is retained; then, the isolation mask layer 37 and the node contact layer 35 at the bottom of the groove 36 are etched back until the height H4 from the substrate 30 is 90nm to 140nm, forming a Figure 4H The lower recess 391 shown (ie, the distance between the bottom of the lower recess 391 and the substrate 30 is 90 nm to 140 nm), in the direction parallel to the substrate 30, the width W1 of the lower recess 391 is preferably 10 nm to 20 nm.
[0108] Afterwards, the protective mask layer 38 is removed by a wet etching process or a dry etching process with a high selectivity ratio to obtain the following Fig. 4I The structure shown in FIG. 1 is shown in FIG. 2 ; Next, the isolation mask layer 37 covering the second surface of the dielectric layer 31 and the bottom of the groove 36 is removed by dry etching, and only the isolation mask layer 37 located at the side wall of the contact window 34 is retained; Finally, the node contact layer 35 is etched back again by dry etching, and the etching depth of this step is less than the depth of the lower recess 391, and the upper recess 392 is formed at the top of the lower recess 391, so that in the direction parallel to the substrate 30, the width W2 of the top of the recess finally formed is greater than the width W1 of the bottom. Among them, the width W2 of the top of the recess can be 20nm to 40nm. That is, the recess finally formed includes an upper recess 392 and a lower recess 391 that are interconnected, and the opening width W2 of the upper recess 392 is greater than the opening width W1 of the lower recess, so that the entire recess is "concave".
[0109] The above is only an example. Those skilled in the art can also adjust the relative proportional relationship between the top width and the bottom width of the recess according to actual needs, for example, according to the thickness of the deposited isolation layer 37 and the protective layer 38. The first dielectric material can be but not limited to silicon nitride, and the second dielectric material can be but not limited to silicon oxide, so that the isolation layer 37 and the protective layer 38 have different etching selectivities. The thickness of the isolation layer 37 formed by the atomic layer deposition process is 3nm to 10nm, and the thickness of the protective layer 38 can also be 3nm to 10nm. The thickness of the isolation layer 37 and the protective layer 38 can be the same or different, and those skilled in the art can choose according to actual needs.
[0110] Preferably, the sidewall mask layer comprises a multi-layer mask layer, and the multi-layer mask layer is used to form the stepped recess in the node contact layer. The step may comprise a plurality of stepped structures, and the number of the steps is determined by the number of the sidewall mask layers.
[0111] Step S35, forming a contact plug 41 on the recessed node contact layer 35, such as Figure 4K shown.
[0112] Preferably, the method for forming the semiconductor structure further comprises:
[0113] Before forming the contact plug 41 , a metal silicide 40 is formed on the surface region of the node contact layer 35 .
[0114] Specifically, metal ions are implanted along the recess to form metal silicide 40 on the surface of the recess, such as Figure 4J Afterwards, the contact window 34 is filled with a second conductive material, and a chemical mechanical polishing (CMP) process is combined to form the contact plug 41 electrically contacting the metal silicide 40, as shown in FIG. Figure 4K As shown. The metal ions implanted along the recess may be any one or a combination of cobalt ions, germanium ions and nickel ions. The second conductive material may be, but is not limited to, tungsten metal.
[0115] Preferably, the process of forming the metal silicide further comprises:
[0116] An isolation layer is formed on the sidewalls of the contact window 34 .
[0117] Specifically, during the process of forming the upper recess 392 , the isolation mask layer 37 remaining on the sidewall surface of the contact window 34 forms the isolation layer, thereby saving process steps.
[0118] Optionally, the isolation layer is different from the isolation mask layer 37. Specifically, the isolation mask layer 37 is removed by wet etching, the isolation layer is formed by a thin film process such as ALD, and a dry etching process is performed to remove the isolation layer on the surface of the substrate 31 and the surface of the metal silicide 40, and the isolation layer on the side wall of the contact window 34 is retained. The isolation layer can be a metal compound such as TiN or TaN, or a non-metal compound such as silicon nitride and silicon oxide.
[0119] In this embodiment, the node contact layer 35 is etched back multiple times, so that the relative proportional relationship between the top width and the bottom width of the recess can be accurately controlled. Moreover, since the characteristic size of the bottom of the recess is smaller than the top, the entire recess is stepped, such as a "concave" shape. On the one hand, it is beneficial for subsequent ion implantation to form a larger area of the metal silicide 40, thereby reducing the contact resistance between the node contact layer 35 and the contact plug 41; on the other hand, it is also beneficial for the full filling of the contact plug 41, thereby ensuring the electrical performance of the semiconductor structure.
[0120] This embodiment also provides a semiconductor structure. The schematic diagram of the semiconductor structure can be seen in Figure 4K The semiconductor structure may be as follows: Figure 3 , Figure 4A-Figure 4K The method shown is formed. Figure 3 , Figure 4A-Figure 4K As shown, the semiconductor structure comprises:
[0121] A substrate 30 having a dielectric layer 31 and a contact window 34 penetrating the dielectric layer 31;
[0122] A node contact layer 35 is located in the contact window 34, and the top of the node contact layer 35 has a stepped depression;
[0123] The contact plug 41 is connected to the node contact layer 35 .
[0124] Preferably, the stepped recess includes an upper recess 392 and a lower recess 391 , and the opening width of the upper recess 392 is greater than that of the lower recess 391 .
[0125] Preferably, the semiconductor structure further comprises:
[0126] An isolation layer, located on the sidewall surface of the contact window 34;
[0127] The metal silicide 40 is located between the node contact layer 35 and the contact plug 41 .
[0128] The above is only a preferred embodiment of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for forming a semiconductor structure, characterized in that: The steps include: Providing a substrate, wherein the substrate has a dielectric layer and a contact window penetrating the dielectric layer; A node contact layer is formed in the contact window; the upper portion of the contact window is not filled with the node contact layer and a groove is formed in the contact window; forming a sidewall mask layer on the sidewall of the contact window; Etching the node contact layer using the sidewall mask layer to form a recess in the node contact layer; forming a contact plug on the recessed node contact layer; Wherein, the sidewall mask layer includes a multi-layer mask layer, and the multi-layer mask layer is used to form the stepped recess in the node contact layer.
2. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: A metal silicide is formed in the surface region of the node contact layer.
3. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: An isolation layer is formed on the sidewalls of the contact window.
Citation Information
Patent Citations
Semiconductor structure
CN209993595U