A junction field effect transistor device and a method for manufacturing the same
By designing the structure in the SiC junction field effect transistor device, the gate is located between the sources and the gate conductivity region is shallower, the problem of large driving circuit pressure caused by avalanche current passing through the gate is solved, and the device production is simplified , achieving more reliable avalanche breakdown and simplicity of production.
Patent Information
- Application Number
- CN202011245808.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-11-10
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-11-10
AI Technical Summary
When the SiC junction field effect transistor device breaks down by avalanche, the avalanche current passes through the gate electrode directly, resulting in high pressure on the gate driving circuit and even burning. The trench structure is complex and easy to form a subtrench structure, resulting in advance breakdown.
Design a junction field effect transistor device, in which the gate is located between two adjacent sources, the conductivity region of the gate is shallower than the conductivity region of the source, so that the avalanche current passes through the source without passing through the gate and simplify the production using a flat structure.
It protects the gate driving circuit, improves the avalanche breakdown reliability of the device, and simplifies the device manufacturing process.
Smart Images

Figure CN112289855B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of semiconductor technology, and more specifically, to a junction field effect transistor device and a preparation method thereof. Background Art
[0002] The bandgap width of SiC material is about 3 times that of silicon, and the critical breakdown field strength is about 10 times that of silicon, so it is very suitable for applications in high voltage and high frequency fields. Compared with the low channel mobility and gate reliability problems caused by the high MOS interface state of SiC MOSFET, there is no MOS gate structure in SiC junction field effect transistor (JFET), so the device is relatively simple and mature.
[0003] Conventional SiC junction field effect transistors (JFETs) are trench-type structures, such as Figure 1 As shown. The gate is at the bottom of the trench, and the p+ region at the bottom of the trench is used to deplete the conductive channel, thereby turning off the device. However, in conventional structures, since the p+ region is only electrically connected to the gate, when an avalanche breakdown occurs in the device, the avalanche current directly enters the gate through the p+ region. When the avalanche current is large, the gate will pass a very large current, which will cause great pressure on the gate drive circuit and even directly burn the gate drive circuit. At the same time, the etching of the trench is prone to form a sub-trench structure, which will cause the device to break down prematurely. Therefore, the production of trench field effect transistors is also difficult. Summary of the invention
[0004] The present invention provides a junction field effect transistor device, aiming to improve the above problems.
[0005] In order to achieve the above object, the technical solution adopted by the present invention is: a junction field effect transistor device, the device comprising:
[0006] Ⅰ - A conductive drift layer;
[0007] Ⅱ + Conductive region, formed in Ⅰ - In the conductive drift layer, the middle position II + The depth of the conductive area is lower than that of the Ⅱ + Conductive type area;
[0008] The gate ohmic contact area is formed in the middle of the II + On the conductive area,
[0009] The source ohmic contact region is formed on both sides of the II + On the conductive area;
[0010] In I - Conductivity type is n - Conductive type, Ⅱ+ The conductivity type is p + Conductive type, in Ⅰ - Conductivity type is p - Conductive type, Ⅱ + The conductivity type is n + Conductive type.
[0011] Furthermore, the device also includes:
[0012] Ⅰ + Conductive area, formed on both sides of the Ⅱ + In the conductive area, Ⅰ + The depth of the conductive zone is lower than that of the II + Conductive zone and the middle position Ⅱ + Conductive type area;
[0013] Ⅱ on both sides + Conductive zone and the middle position Ⅱ + The conductive areas are directly opposite to each other, and the opposite areas are gate-controlled conductive channels.
[0014] Furthermore, the source ohmic contact region is directly formed on I + Conductive type area and corresponding Ⅱ + On the conductive area.
[0015] Furthermore, the device also includes:
[0016] The field oxide layer is located between the gate ohmic contact region and the source ohmic contact region, and the thickness of the field oxide layer is higher than the heights of the gate ohmic contact and the source ohmic contact.
[0017] Furthermore, the device also includes:
[0018] The first interconnect metal layer formed on the gate ohmic contact region and the source ohmic contact region are respectively referred to as the gate interconnect metal layer and the source interconnect metal layer.
[0019] Furthermore, the device also includes:
[0020] An isolation dielectric layer is formed on the first interconnect metal layer, and the isolation dielectric layer on the source interconnect metal layer and a portion of the gate interconnect metal layer is etched to form an isolation window;
[0021] And a second interconnect metal layer is formed on the isolation dielectric layer and its window.
[0022] Furthermore, the device also includes:
[0023] Ⅰ + Conductive substrate;
[0024] Formed in I + I on conductive substrate+ Conductive buffer layer, Ⅰ - The conductive drift layer is formed in I + On the conductive buffer layer.
[0025] Furthermore, the device also includes:
[0026] The drain electrode is composed of an ohmic contact and a pressed metal. + Conductive substrate contact, block metal is used to connect to the external circuit.
[0027] The present invention is implemented in this way, a method for preparing a junction field effect transistor device, which is specifically as follows:
[0028] In the growth of - Conductive drift layer is formed on the epitaxial wafer by ion implantation II + Conductive area and II formed on both sides + Conductivity type I + Conductive region; injecting type I doping ions into the gate-controlled conductive channel, then depositing a thin carbon layer, performing high-temperature annealing to activate the injected doping ions, removing the carbon layer, and performing sacrificial oxidation to remove the defect layer on the semiconductor surface; depositing and forming a field oxide layer, depositing metal and performing rapid thermal annealing to form a source ohmic contact and a gate ohmic contact on the source and gate respectively; forming a first interconnect metal layer, including a source interconnect metal and a gate interconnect metal; forming an isolation dielectric layer, etching the isolation dielectric layer on the source interconnect metal layer and part of the gate interconnect metal layer to form an isolation window; forming a second interconnect metal layer on the isolation dielectric layer and its window; applying a passivation dielectric and polyimide on the terminal area of the chip; depositing metal on the back of the device and performing laser annealing to form an ohmic contact, and then depositing a block metal to complete the preparation of a junction field effect transistor device.
[0029] The junction field effect transistor device provided by the present invention has a gate located between two adjacent source electrodes, and the gate II + The conductivity type of the region is greater than that of the source II + The conductive region is shallower, so the avalanche of the device occurs at the source II + Conductive region. Avalanche current directly passes through the source without passing through the gate, protecting the gate drive circuit. At the same time, the device has a planar structure and is easy to manufacture. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the structure of an existing trench SiC junction field effect transistor;
[0031] Figure 2 A schematic diagram of the structure of a junction field effect transistor device provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0032] The specific implementation modes of the present invention are further explained in detail below by describing the embodiments with reference to the accompanying drawings, so as to help those skilled in the art to have a more complete, accurate and in-depth understanding of the inventive concept and technical solution of the present invention.
[0033] The method of the present invention is applicable to junction field effect transistors (JFETs) of various SiC and other semiconductor materials, such as Si, GaN, Ga2O3 and other semiconductor materials. The following is an explanation using SiC JFET as an example.
[0034] The present invention proposes a junction field effect transistor device, wherein the gate of the device is located between two adjacent source electrodes, and the gate II + The conductivity type of the region is greater than that of the source II + The conductive region is shallower, so the avalanche of the device occurs at the source II + Conductive region. Avalanche current directly passes through the source without passing through the gate, protecting the gate drive circuit. At the same time, the device has a planar structure and is easy to manufacture.
[0035] Embodiment 1:
[0036] The junction field effect transistor device of the embodiment of the present invention is as follows Figure 2 As shown, the device's primitive cell includes drain electrodes 1, n + Conductive substrate 2, n + Conductive buffer layer 3, n - Conductive drift layer 4, formed on n - The p-type conductive drift layer 4 + Conductive area, located on both sides of the p + The first p + Conductive zone 5, p located in the middle + The conductivity type region is the second p + Conductive type regions 6 are formed in the first p + Conductive region 5, second p + The source ohmic contact region 901 and the gate ohmic contact region 902 on the conductive region 6. + The conductive region 7 is formed in the first p + Conductive type region 5. + The depth of the conductive region 7 is lower than the first p + Conductive type region 5 is also lower than the second p + The depth of the conductive region 6; the first p + The conductive region 5 is connected to the second p + The second conductive region 6 is directly opposite to the second conductive region 6. + The conductive region 6 and the first p +The opposite region between the conductive regions 5 is the gate-controlled conductive channel 401 .
[0037] For SiC devices, n + The concentration of conductive substrate 2 is greater than 1E18cm -3 , n + The concentration of the conductive buffer layer 3 is about 1E18 cm -3 , with a thickness of several microns, the buffer layer can reduce the defects of subsequent drift layer growth. - The concentration of the conductive drift region 4 is about 1E14cm -3 ~1E17cm -3 The thickness is greater than 5 microns, depending on the withstand voltage of the device design.
[0038] Second p + Conductive type region 6 and the first p + The conductive area 5 has a high doping concentration, and the doping concentration is greater than 1E19cm -3 , and the second p + The depth of the conductive region 6 is less than the first p + The depth of the conductive region 5 is such that when the device is blocked, the maximum electric field will appear in the first p + At the edge of conductive region 5, avalanche breakdown also occurs at the first p + The edge of the conductive region 5, the avalanche current flows through the first p + The conductive area 5 flows directly into the source. The avalanche breakdown is more reliable, and the avalanche current no longer flows into the gate drive, which also protects the gate drive circuit.
[0039] Second p + The depth of conductive region 6 is greater than n + The depth of the conductive region 7, i.e. the second p + The conductive region 6 and the first p + Part of the conductive area 5 is directly opposite to each other, with an n-type conductive area in between. The n-type conductive area in the middle is the gate-controlled conductive channel 401. The device is turned off by depleting the gate-controlled conductive channel 401. Therefore, the doping concentration, width and length of the middle gate-controlled conductive channel 401 determine the threshold voltage of the device. The relevant parameters need to be designed according to the threshold voltage of the device. The doping concentration of the gate-controlled conductive channel 401 is greater than the n-type conductive area. - The doping concentration of the conductive drift region 4 further reduces the resistance of the conductive channel.
[0040] In the embodiment of the present invention, the source ohmic contact region 901 is directly formed on n + Conductive type region 7 and the corresponding first p + On the conductive region 5, an n-type ohmic contact and a p-type ohmic contact are formed simultaneously. +The conductive region 7 is in the first p + The conductive region 5 is inside, and the source ohmic contact region 901 is in the n + Conductive type region 7 and the first p + The first p + The conductive region 5 is directly electrically connected to the source ohmic contact region 901. + The doping concentration of conductive area 7 is greater than 1E19cm -3 The thickness is generally greater than 0.2 microns. The source ohmic contact 901 can be formed by depositing Ni or TiNi and then performing rapid thermal annealing.
[0041] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0042] The field oxide layer 8 is located between the gate ohmic contact region 902 and the source ohmic contact region 901, and the thickness of the field oxide layer 8 is generally greater than 0.2 microns. On the one hand, the field oxide layer 8 is used to protect the junction terminal region of the device from the influence of subsequent processes, and on the other hand, it is used to isolate the gate ohmic contact region 902 from the source ohmic contact region 901. The interval between the gate ohmic contact region 902 and the source ohmic contact region 901 (i.e., the width of the field oxide layer 8) is greater than the absolute value of the designed maximum gate breakdown voltage. The field oxide layer 8 can be grown by CVD. The gate ohmic contact region 902 can be formed simultaneously with the source ohmic contact region 901, and Ni or TiNi is deposited at the same time, and then formed by rapid thermal annealing. The process is simplified.
[0043] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0044] The first interconnect metal layer 10 formed on the gate ohmic contact region 902 and the source ohmic contact region 901 are respectively referred to as the gate interconnect metal layer 102 and the source interconnect metal layer 101. After the gate ohmic contact region 902 is formed, the first interconnect metal layer 10 is deposited, including the source interconnect metal 101 and the gate interconnect metal 102. The source interconnect metal 101 and the gate interconnect metal 102 are the same and are formed at the same time to simplify the process. The first interconnect metal layer 10 can be Al or Cu, Ag, etc., and the thickness is generally greater than 0.2 microns to reduce the resistance of the interconnection. Through the low-resistance interconnect metal, the resistance of the gate loop on the chip can be reduced, and the uniformity of the gate voltage of each unit cell on the chip can be achieved.
[0045] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0046] An isolation dielectric layer is formed on the first interconnect metal layer, a window is formed by etching the isolation dielectric layer on the source interconnect metal layer and part of the gate interconnect metal layer, and a second interconnect metal layer is formed on the isolation dielectric layer and its window; the second interconnect metal layer is a pressed block metal for the source and gate of the device. The source of each unit cell of the device is interconnected, and a large pressed block metal is formed on the gate for connecting the source and gate to the external circuit. The second interconnect metal layer is generally Al or Ag, Cu, Au, etc., with a thickness greater than 1 micron.
[0047] In the embodiment of the present invention, the drain 1 is composed of an ohmic contact and a pressed metal. The ohmic contact is used to form a very low resistivity connection with the SiC substrate, and the pressed metal is used to connect the back drain with an external circuit. The ohmic contact can be formed by depositing Ni and performing rapid annealing, or by laser annealing. The pressed metal can be TiNiAg, or CrTiAg, TiNiAu, etc.
[0048] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0049] After the second interconnect metal layer is completed, the terminal area of the chip is made of passivation medium and polyimide to protect the device from damage by moisture, scratches or other ion contamination. The passivation medium is generally SiO2 and SiN, with a total thickness greater than 0.5 microns, and the thickness of polyimide is greater than 1 micron.
[0050] In an embodiment of the present invention, the method for preparing the above-mentioned junction field effect transistor device specifically comprises the following steps:
[0051] First, the first p + Conductive type region 5, second p + Conductivity type region 6, n +Conductive region 7; n-type doping ions are injected into the conductive channel 401, which can generally be nitrogen ions or phosphorus ions, to reduce the resistance of the conductive channel. Subsequently, a thin carbon layer is deposited, and high-temperature annealing is performed to activate the injected doping ions, and the annealing temperature is greater than 1600°C. The carbon layer is removed, and sacrificial oxidation is performed to remove the defective layer on the surface of the semiconductor. A field oxide layer 8 is deposited and formed, metal Ni is deposited and rapidly thermally annealed, and a source ohmic contact 901 and a gate ohmic contact 902 are formed on the source and gate at the same time; a first interconnect metal layer 10 is formed, including a source interconnect metal 101 and a gate interconnect metal 102, which are formed at the same time. The isolation dielectric layer is formed, and the isolation dielectric layer on the source interconnection metal layer and part of the gate interconnection metal layer is etched to form an isolation window; a second interconnection metal layer is formed on the isolation dielectric layer and its window; a passivation dielectric and polyimide are made on the terminal area of the chip; metal Ni is deposited on the back of the device and laser annealed to form an ohmic contact, and then a block metal is deposited, which can be TiNiAg, CrTiAg, TiNiAu, etc., thereby completing the preparation of the chip.
[0052] Embodiment 2
[0053] The junction field effect transistor device of the embodiment of the present invention is as follows Figure 2 As shown, the device's primitive cell includes drain electrode 1, p + Conductive substrate 2, p + Conductive buffer layer 3, p - Conductive drift layer 4, formed on p - The n-type conductive drift layer 4 + Conductive area, located on both sides of the n + The first n + Conductive zone 5, n located in the middle + The conductivity type region is the second n + Conductive type regions 6 are formed in the first n + Conductive type region 5, second n + The source ohmic contact region 901 and the gate ohmic contact region 902 on the conductive region 6. + The conductive region 7 is formed in the first n + Conductive type region 5. + The depth of the conductive region 7 is lower than the first n + Conductive type region 5, and also lower than the second n + The depth of the conductive region 6; the first n + The conductive region 5 is connected to the second n + The conductive area 6 is directly opposite to the second n + The conductive region 6 and the first n + The opposite region between the conductive regions 5 is the gate-controlled conductive channel 401 .
[0054] For SiC devices, p + The concentration of conductive substrate 2 is greater than 1E18cm -3 , p + The concentration of the conductive buffer layer 3 is about 1E18 cm -3 , with a thickness of several microns, the buffer layer can reduce the defects of subsequent drift layer growth. - The concentration of the conductive drift region 4 is about 1E14cm -3 ~1E17cm -3 The thickness is greater than 5 microns, depending on the withstand voltage of the device design.
[0055] Second n + Conductive type region 6 and the first n + The conductive area 5 has a high doping concentration, and the doping concentration is greater than 1E19cm -3 , and the second n + The depth of the conductive region 6 is less than the first n + The depth of the conductive region 5 is such that when the device is blocked, the maximum electric field will appear in the first n + At the edge of conductive region 5, avalanche breakdown also occurs at the first n + The edge of the conductive region 5, the avalanche current flows through the first n + The conductive area 5 flows directly into the source. The avalanche breakdown is more reliable, and the avalanche current no longer flows into the gate drive, which also protects the gate drive circuit.
[0056] Second n + The depth of the conductive region 6 is greater than that of the p + The depth of the conductive region 7, that is, the second n + The conductive region 6 and the first n + Part of the conductive area 5 is directly opposite to each other, with a p-type conductive area in between. The p-type conductive area in the middle is the gate-controlled conductive channel 401. The device is turned off by depleting the gate-controlled conductive channel 401. Therefore, the doping concentration, width and length of the middle gate-controlled conductive channel 401 determine the threshold voltage of the device. The relevant parameters need to be designed according to the threshold voltage of the device. The doping concentration of the gate-controlled conductive channel 401 is greater than the p-type conductive area. - The doping concentration of the conductive drift region 4 further reduces the resistance of the conductive channel.
[0057] In the embodiment of the present invention, the source ohmic contact region 901 is directly formed on the p + Conductive type region 7 and the corresponding first n + On the conductive region 5, an n-type ohmic contact and a p-type ohmic contact are formed simultaneously. + The conductive region 7 is in the first n +The conductive region 5 is inside, and the source ohmic contact region 901 is in the p + Conductive type region 7 and the first n + The first n + The conductive region 5 is directly electrically connected to the source ohmic contact region 901. + The doping concentration of conductive area 7 is greater than 1E19cm -3 The thickness is generally greater than 0.2 microns. The source ohmic contact 901 can be formed by depositing Ni or TiNi and then performing rapid thermal annealing.
[0058] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0059] The field oxide layer 8 is located between the gate ohmic contact region 902 and the source ohmic contact region 901, and the thickness of the field oxide layer 8 is generally greater than 0.2 microns. On the one hand, the field oxide layer 8 is used to protect the junction terminal region of the device from the influence of subsequent processes, and on the other hand, it is used to isolate the gate ohmic contact region 902 from the source ohmic contact region 901. The interval between the gate ohmic contact region 902 and the source ohmic contact region 901 (i.e., the width of the field oxide layer 8) is greater than the absolute value of the designed maximum gate breakdown voltage. The field oxide layer 8 can be grown by CVD. The gate ohmic contact region 902 can be formed simultaneously with the source ohmic contact region 901, and Ni or TiNi is deposited at the same time, and then formed by rapid thermal annealing. The process is simplified.
[0060] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0061] The first interconnect metal layer 10 formed on the gate ohmic contact region 902 and the source ohmic contact region 901 are respectively referred to as the gate interconnect metal layer 102 and the source interconnect metal layer 101. After the gate ohmic contact region 902 is formed, the first interconnect metal layer 10 is deposited, including the source interconnect metal 101 and the gate interconnect metal 102. The source interconnect metal 101 and the gate interconnect metal 102 are the same and are formed at the same time to simplify the process. The first interconnect metal layer 10 can be Al or Cu, Ag, etc., and the thickness is generally greater than 0.2 microns to reduce the resistance of the interconnection. Through the low-resistance interconnect metal, the resistance of the gate loop on the chip can be reduced, and the uniformity of the gate voltage of each unit cell on the chip can be achieved.
[0062] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0063] An isolation dielectric layer is formed on the first interconnect metal layer, a window is formed by etching the isolation dielectric layer on the source interconnect metal layer and part of the gate interconnect metal layer, and a second interconnect metal layer is formed on the isolation dielectric layer and its window; the second interconnect metal layer is a pressed block metal for the source and gate of the device. The source of each unit cell of the device is interconnected, and a large pressed block metal is formed on the gate for connecting the source and gate to the external circuit. The second interconnect metal layer is generally Al or Ag, Cu, Au, etc., with a thickness greater than 1 micron.
[0064] In the embodiment of the present invention, the drain 1 is composed of an ohmic contact and a pressed metal. The ohmic contact is used to form a very low resistivity connection with the SiC substrate, and the pressed metal is used to connect the back drain with an external circuit. The ohmic contact can be formed by depositing Ni and performing rapid annealing, or by laser annealing. The pressed metal can be TiNiAg, or CrTiAg, TiNiAu, etc.
[0065] In an embodiment of the present invention, the junction field effect transistor device further includes:
[0066] After the second interconnect metal layer is completed, the terminal area of the chip is made of passivation medium and polyimide to protect the device from damage by moisture, scratches or other ion contamination. The passivation medium is generally SiO2 and SiN, with a total thickness greater than 0.5 microns, and the thickness of polyimide is greater than 1 micron.
[0067] In an embodiment of the present invention, the method for preparing the above-mentioned junction field effect transistor device specifically comprises the following steps:
[0068] First, the first n is formed on the epitaxial wafer with the drift layer by ion implantation. + Conductive type region 5, second n + Conductive type region 6, p +Conductive region 7; p-type doping ions are injected into the conductive channel 401, which can generally be aluminum ions, to reduce the resistance of the conductive channel. Subsequently, a thin carbon layer is deposited, and a high-temperature annealing is performed to activate the injected doping ions, and the annealing temperature is greater than 1600°C. The carbon layer is removed, and sacrificial oxidation is performed to remove the defective layer on the surface of the semiconductor. A field oxide layer 8 is deposited and formed, metal Ni is deposited and rapidly thermally annealed, and a source ohmic contact 901 and a gate ohmic contact 902 are formed on the source and gate at the same time; a first interconnect metal layer 10 is formed, including a source interconnect metal 101 and a gate interconnect metal 102, which are formed at the same time. The isolation dielectric layer is formed, and the isolation dielectric layer on the source interconnection metal layer and part of the gate interconnection metal layer is etched to form an isolation window; a second interconnection metal layer is formed on the isolation dielectric layer and its window; a passivation dielectric and polyimide are made on the terminal area of the chip; metal Ni is deposited on the back of the device and laser annealed to form an ohmic contact, and then a block metal is deposited, which can be TiNiAg, CrTiAg, TiNiAu, etc., thereby completing the preparation of the chip.
[0069] The present invention is described above by way of example in conjunction with the accompanying drawings. It is obvious that the specific implementation of the present invention is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the method concept and technical solution of the present invention, or the concept and technical solution of the present invention are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.
Claims
1. A junction field effect transistor device, characterized in that: The device comprises: Ⅰ - A conductive drift layer; Ⅱ + Conductive region, formed in Ⅰ - In the conductive drift layer, the middle position II + The depth of the conductive area is lower than that of the Ⅱ + Conductive type area; The gate ohmic contact area is formed in the middle of the II + On the conductive area, The source ohmic contact region is formed on both sides of the II + On the conductive area; In I - Conductivity type is n - Conductive type, Ⅱ + The conductivity type is p + Conductive type, in Ⅰ - Conductivity type is p - Conductive type, Ⅱ + The conductivity type is n + Conductive type; The device further comprises: Ⅰ + Conductive area, formed on both sides of the Ⅱ + In the conductive area, Ⅰ + The depth of the conductive zone is lower than that of the II + Conductive zone and the middle position Ⅱ + Conductive type area; Ⅱ on both sides + Conductive zone and the middle position Ⅱ + The conductive type regions are directly opposite to each other, and the opposite regions are gate-controlled conductive channels; The device further comprises: Ⅰ + Conductive substrate; Formed in I + I on conductive substrate + Conductive buffer layer, Ⅰ - The conductive drift layer is formed in I + On the conductive buffer layer; The drain electrode is composed of an ohmic contact and a pressed metal. + Conductive substrate contact, the block metal is used to connect with the external circuit; The device further comprises: The field oxide layer is located between the gate ohmic contact region and the source ohmic contact region, and the thickness of the field oxide layer is higher than the heights of the gate ohmic contact and the source ohmic contact.
2. The junction field effect transistor device according to claim 1, characterized in that: The source ohmic contact region is formed directly on I + Conductive type area and corresponding Ⅱ + On the conductive area.
3. The junction field effect transistor device according to any one of claims 1 to 2, characterized in that: The device further comprises: The first interconnect metal layer formed on the gate ohmic contact region and the source ohmic contact region are respectively referred to as the gate interconnect metal layer and the source interconnect metal layer.
4. The junction field effect transistor device according to claim 3, characterized in that: The device further comprises: An isolation dielectric layer is formed on the first interconnect metal layer, and the isolation dielectric layer on the source interconnect metal layer and a portion of the gate interconnect metal layer is etched to form an isolation window; And a second interconnect metal layer is formed on the isolation dielectric layer and its window.
5. The method for preparing the junction field effect transistor device according to any one of claims 1 to 4 is as follows: In the growth of - Conductive drift layer is formed on the epitaxial wafer by ion implantation II + Conductive area and II formed on both sides + Conductivity type I + Conductive type region: injecting type I doping ions into the gate-controlled conductive channel, then depositing a thin carbon layer, performing high temperature annealing to activate the injected doping ions, removing the carbon layer, and performing sacrificial oxidation to remove the defective layer on the semiconductor surface; Depositing and forming a field oxide layer, depositing metal and performing rapid thermal annealing, and forming a source ohmic contact and a gate ohmic contact on the source and the gate at the same time; forming a first interconnect metal layer, including a source interconnect metal and a gate interconnect metal; forming an isolation dielectric layer, and etching the isolation dielectric layer on the source interconnection metal layer and a portion of the gate interconnection metal layer to form an isolation window; Forming a second interconnect metal layer on the isolation dielectric layer and its window; applying passivation dielectric and polyimide on the terminal area of the chip; Metal is deposited on the back of the device and laser annealed to form an ohmic contact, and then a compression block metal is deposited to complete the preparation of the junction field effect transistor device.