AMOLED display panel and preparation method thereof
By not setting a buffer layer in the capacitance area of the AMOLED display panel and using IGZO or ITZO active layer materials, combined with the same layer design of gate, source and drain, the low flatness of the capacitance area in the traditional top luminescent AMOLED display panel is solved. The problem has improved the yield and production efficiency of the panel.
Patent Information
- Application Number
- CN202110006806.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-01-05
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2041-01-05
AI Technical Summary
The interlayer capacitance structure in the traditional top luminescent AMOLED display panel results in low flatness of the pixel luminescent area, affecting the yield of the AMOLED display panel.
There is no buffer layer in the capacitance region of the TFT array substrate. The second light shielding layer is used as the lower electrode plate of the capacitor. It is designed through the same layer of the gate, source and drain, combined with IGZO, ITZO or IGZTO active layer materials to form High capacitive and flat top luminous OLED display panel.
It effectively improves the flatness of the pixel luminous area of the AMOLED display panel, improves the yield of the panel, and reduces the production cost and manufacturing process complexity.
Smart Images

Figure CN112786667B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to an AMOLED display panel and a preparation method thereof. Background Art
[0002] Organic Light-Emitting Diode (OLED) is an active light-emitting device. Compared with the current mainstream flat panel display technology, Liquid Crystal Display (LCD), OLED has the advantages of high contrast, wide viewing angle, low power consumption, and thinner volume. It is expected to become the next generation of flat panel display technology after LCD and is one of the most popular technologies in flat panel display technology. Among them, AMOLED (Active-matrix organic light-emitting diode) has the characteristics of large size, low power consumption, high resolution, and long panel life, so it has received great attention in the field of display technology.
[0003] The existing AMOLED display panel includes: a TFT array substrate including a thin film transistor (Thin Film Transistor, TFT) driving circuit, and a plurality of OLED display devices arranged on the TFT array substrate, and each OLED display device is controlled by a corresponding TFT. The current process of top-gate thin film transistor (Top-gate Thin Film Transistor, Top-gate TFT) has a complex structure and a large number of layers. Each additional array process not only increases the time cost and material cost, but also reduces the yield. Therefore, it is necessary to reduce the process and propose a new process of gate, source, and drain in the same layer (Gate Source Drain one Layer Thin Film Transistor, GSD one Layer TFT). Combined with inkjet printing (Ink Jet Printin, IJP) technology, it can not only further reduce the time cost of preparation but also effectively improve the feasibility of mass production. Compared with the bottom-emitting AMOLED display technology, the top-emitting technology can achieve a higher aperture ratio and improve display performance because the light emission does not need to be independent of the driving circuit area. Such as Figure 1As shown, the array substrate of this GSD one Layer TFT generally includes: a substrate 11, which is divided into a plurality of driving TFT areas A, a plurality of capacitor areas B and a plurality of metal wiring areas C; a light shielding layer 12, which is arranged on the substrate 11 and is located in the driving TFT area A, the capacitor area B and the metal wiring area C; a buffer layer 13, which is arranged on the light shielding layer 12 and is located in the driving TFT area A, the capacitor area B and the metal wiring area C; an active layer 14, which is arranged on the buffer layer 13 and is located in the driving TFT area A, the capacitor area B and the metal wiring area C; a gate insulating layer 15, which is arranged on the active layer 14 and is located in the driving TFT area A and the metal wiring area C; a metal layer 16, which is arranged on the gate insulating layer 15 and is located in the driving TFT area A and the metal wiring area C, and the metal layer of the driving TFT area A includes a gate 162, a source 163 and a drain 161 on the same layer; and a passivation layer 17 located above the metal layer 16. The structure of the capacitor in the capacitor area B is a sandwich capacitor structure of three-layer electrode plates, wherein the upper electrode plate is the anode 19 located above the flat layer 18, the middle electrode plate is the flat layer, and the lower electrode plate is the shading layer.
[0004] However, the use of this traditional design of not placing the capacitor directly under the OLED display device will affect the pixel resolution. If the capacitor is placed directly under the OLED display device, the inkjet printing technology has very high requirements for the flatness of the pixel light-emitting area, especially the anode of the pixel light-emitting area. If the traditional sandwich capacitor structure is used, the low flatness will inevitably cause the AMOLED yield to decrease. Summary of the invention
[0005] The embodiment of the present invention provides an AMOLED display panel and a method for manufacturing the same, so as to improve the AMOLED yield reduction phenomenon caused by low flatness of the interlayer capacitor structure of the conventional top-emitting AMOLED display panel.
[0006] To solve the above problems, in a first aspect, the present application provides an AMOLED display panel, comprising: a TFT array substrate and a plurality of top-emitting OLED devices arranged on the TFT array substrate,
[0007] The TFT array substrate comprises:
[0008] The substrate is divided into a plurality of driving TFT areas, a plurality of capacitor areas and a plurality of metal wiring areas; wherein the driving TFT area is provided with driving TFTs, the capacitor area is provided with capacitors, and the metal wiring area is provided with metal wirings,
[0009] A light shielding layer, disposed on the substrate, comprising a first light shielding layer located in the driving TFT area and a second light shielding layer located in the capacitor area, wherein the second light shielding layer serves as a lower electrode plate of a capacitor in the capacitor area;
[0010] a buffer layer, disposed on the light shielding layer, comprising a first buffer layer located in the driving TFT region, wherein the capacitor region is not provided with a buffer layer;
[0011] An active layer, disposed on the buffer layer, comprising a first active layer located in the driving TFT region;
[0012] a gate insulating layer, disposed on the active layer, comprising a first gate insulating layer located in the driving TFT region and a second gate insulating layer located in the capacitor region, wherein the second gate insulating layer serves as a capacitor dielectric layer of a capacitor in the capacitor region; and
[0013] A metal layer is arranged on the gate insulating layer, comprising a first metal layer located in the driving TFT area and a second metal layer located in the capacitor area, wherein the first metal layer includes a gate 162, a source 163 and a drain 161 on the same layer, and the second metal layer serves as an upper electrode plate of a capacitor in the capacitor area.
[0014] Furthermore, in the metal routing area, the shading layer further includes a third shading layer, the buffer layer further includes a second buffer layer, the active layer further includes a second active layer, the gate insulating layer further includes a third gate insulating layer, and the metal layer further includes a third metal layer.
[0015] Further, the top-emitting OLED device comprises: an anode, the anode is located above the capacitor region and is electrically connected to the driving TFT region, and the orthographic projection of the anode on the AMOLED display panel covers the capacitor region;
[0016] a light-emitting material layer, the light-emitting material layer being located on the anode; and
[0017] A cathode covers the light emitting material layer.
[0018] Furthermore, the gate, source and drain are divided into two layers, the lower layer contains an alloy of one or more of Mo, Ti and Ni, and the upper layer contains Cu or a Cu-containing alloy. Thickness range of upper layer
[0019] Furthermore, the light shielding layer is divided into three layers, the lower layer contains one or more alloys of Mo, Ti, and Ni, the middle layer is Cu or a Cu alloy, and the upper layer contains one or more alloys of Mo, Ti, and Ni. Thickness range of the middle layer Thickness range of upper layer
[0020] Furthermore, the active layer material is IGZO, ITZO or IGZTO.
[0021] In a second aspect, the present application provides a method for preparing an AMOLED display panel, comprising the following steps:
[0022] Providing a substrate, dividing a plurality of driving TFT areas, a plurality of capacitor areas and a plurality of metal wiring areas on the substrate;
[0023] Depositing a light shielding layer, a buffer layer and an active layer in sequence on the substrate, and removing the buffer layer in the capacitor region;
[0024] A gate insulating layer, a metal layer and a top-emitting OLED device are sequentially deposited on the light shielding layer, the buffer layer and the active layer.
[0025] Furthermore, the step of sequentially depositing a light shielding layer, a buffer layer and an active layer on the substrate and removing the buffer layer in the capacitor region comprises the following steps:
[0026] Depositing a whole-surface light-shielding layer on the substrate, and etching and patterning the whole-surface light-shielding metal layer using a first yellow light process to form a first light-shielding layer in the driving TFT area, a second light-shielding layer in the capacitor area, and a third light-shielding layer in the metal wiring area;
[0027] Sequentially depositing a buffer layer and an active layer on the entire surface above the light-shielding metal layer, and etching and patterning the entire surface of the active layer using a second yellow light process to form a first active layer in the driving TFT area and a second active layer in the metal wiring area;
[0028] The first active layer and the second active layer are used to etch the lower buffer layer, remove the buffer layer in the capacitor area, and form the first buffer layer in the driving TFT area and the second buffer layer in the metal wiring area.
[0029] Furthermore, the step of sequentially depositing a gate insulating layer, a metal layer and a top-emitting OLED device on the light-shielding layer, the buffer layer and the active layer comprises the following steps:
[0030] Depositing a whole gate insulating layer on the active layer, and performing a third yellow light process on the gate insulating layer of the driving TFT area to open holes and perform a conductor process, so as to form a first gate insulating layer of the driving TFT area, a second gate insulating layer of the capacitor area, and a third gate insulating layer of the metal wiring area;
[0031] Depositing a metal layer on the gate insulating layer, patterning it using a fourth yellow light process, and etching the metal layer to form a first metal layer in the driving TFT area, a second metal layer in the capacitor area, and a third metal layer in the metal wiring area, wherein the first metal layer includes a gate, a source, and a drain on the same layer;
[0032] Performing self-aligned etching on the gate insulating layer using the patterned metal layer to form a self-aligned channel region in the driving TFT region;
[0033] A passivation layer and a planarization layer are sequentially deposited, the passivation layer and the planarization layer are patterned and opened, an anode of a top-emitting OLED device is deposited and patterned, an organic photoresist layer is deposited again, and the OLED light-emitting area is defined by patterning.
[0034] Furthermore, the material of the active layer is IGZO, ITZO or IGZTO.
[0035] The present invention provides a top-emitting OLED display panel with a gate, a source and a drain on the same layer, wherein the thickness of the capacitor in the capacitor area is reduced by not arranging a buffer layer in the capacitor area, and high capacitance is ensured without changing the area of the capacitor and without using an interlayer capacitor, thereby ensuring the flatness under the anode of the top-emitting OLED device, thereby improving the yield of the panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for describing the embodiments are briefly introduced below.
[0037] Figure 1 It is a structural schematic diagram of an existing AMOLED display panel;
[0038] Figure 2 is a schematic structural diagram of an AMOLED display panel provided by an embodiment of the present invention;
[0039] Figure 3 is a schematic diagram of the structure of an AMOLED display panel after step S11 implemented in an embodiment of the present invention;
[0040] Figure 4 is a schematic diagram of the structure of an AMOLED display panel after step S12 implemented in an embodiment of the present invention;
[0041] Figure 5 is a schematic diagram of the structure of an AMOLED display panel after step S13 implemented in an embodiment of the present invention;
[0042] Figure 6 is a schematic diagram of the structure of an AMOLED display panel after step S14 implemented in an embodiment of the present invention;
[0043] Figure 7 is a schematic diagram of the structure of an AMOLED display panel after step S15 implemented in an embodiment of the present invention;
[0044] Figure 8 It is a schematic diagram of the structure of the AMOLED display panel after step S16 implemented in an embodiment of the present invention.
[0045] Description of the accompanying drawings:
[0046] A-driving TFT area; B-capacitor area; C-metal wiring area; 11-substrate; 12-light shielding layer; 121-first light shielding layer; 122-second light shielding layer; 123-third light shielding layer; 13-buffer layer; 131-first buffer layer; 132-second buffer layer; 14-active layer; 141-first active layer; 142-second active layer; 15-gate insulating layer; 151-first gate insulating layer; 152-second gate insulating layer; 153-third gate insulating layer; 16-metal layer; 160-first metal layer; 161-drain; 162-gate; 163-source; 164-second metal layer; 165-third metal layer; 17-passivation layer; 18-flat layer; 19-anode; 10-photoresistive layer. DETAILED DESCRIPTION
[0047] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0048] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0049] The embodiments of the present invention provide an AMOLED display panel and a method for manufacturing the same, which are described in detail below.
[0050] First, see Figure 2-Figure 7 In an embodiment of the present invention, an AMOLED display panel is provided, comprising: a TFT array substrate, and a plurality of top-emitting OLED devices arranged on the TFT array substrate, wherein the TFT array substrate comprises: a substrate 11, a light shielding layer 12, a buffer layer 13, an active layer 14, a gate insulator 15 (GI) and a metal layer 16. In one embodiment, the TFT array substrate further comprises: a passivation layer 17 and a planarization layer 18.
[0051] The substrate 11 can be divided into a plurality of driving TFT areas A, a plurality of capacitor areas B and a plurality of metal wiring areas C. The driving TFT area A is provided with driving TFTs, the capacitor area B is provided with capacitors, and the metal wiring area C is provided with metal wirings.
[0052] Specifically, the capacitor is two capacitor electrode plates, and a capacitor dielectric layer directly arranged between two adjacent capacitor electrode plates.
[0053] It is understandable that the above-mentioned substrate 11 may also be divided into other areas, such as a switch TFT area, which is not specifically limited here.
[0054] Specifically, the shading layer 12 is a shading metal layer, which is arranged on the substrate 11, and includes a first shading layer 121 located in the driving TFT area A and a second shading layer 122 located in the capacitor area B; the second shading layer 122 serves as the lower electrode plate of the capacitor in the capacitor area B.
[0055] Specifically, the buffer layer 13 is disposed on the light shielding layer 12, and includes a first buffer layer 131 located in the driving TFT area A, wherein the capacitor area B is not provided with a buffer layer 13, so as to reduce the thickness of the capacitor in the capacitor area B, thereby ensuring high capacitance.
[0056] Specifically, the active layer 14 is disposed on the buffer layer 13 , and includes a first active layer 141 located in the driving TFT region A.
[0057] Specifically, the gate insulating layer 15 is disposed on the active layer 14, and includes a first gate insulating layer 151 located in the driving TFT region A and a second gate insulating layer 152 located in the capacitor region B, and the second gate insulating layer 152 serves as a capacitor dielectric layer of the capacitor in the capacitor region B;
[0058] Specifically, the metal layer 16 is disposed on the gate insulating layer 15, and includes a first metal layer 160 located in the driving TFT area A and a second metal layer 164 located in the capacitor area B, wherein the first metal layer 160 includes a gate 162, a source 163 and a drain 161 on the same layer, and this same-layer design is used to reduce the number of yellow light processes. The second metal layer 164 serves as an upper electrode plate of the capacitor in the capacitor area B.
[0059] Top-emitting technology can achieve a higher aperture ratio and improve display performance. The design of the gate 162, source 163, and drain 161 on the same layer can reduce the cost of AMOLED display panel production, but the design of the gate 162, source 163, and drain 161 on the same layer requires the capacitor to adopt a sandwich capacitor structure, and the sandwich capacitor will produce low flatness. This low flatness is bound to affect the anode 19 of the top-emitting OLED device above the capacitor, which has a high flatness requirement, thereby affecting the yield of the AMOLED display panel.
[0060] In an embodiment of the present invention, a top-emitting AMOLED display panel is provided in which a gate electrode 162, a source electrode 163, and a drain electrode 161 are on the same layer. The thickness of the capacitor in the capacitor area B is reduced by not providing a buffer layer 13 in the capacitor area B, the second light shielding layer 122 is used as the lower electrode plate of the capacitor, and the second metal layer 164 is used as the upper electrode plate. High capacitance is ensured without changing the area of the capacitor and without using an interlayer capacitor. The traditional method of using a top-emitting AMOLED device anode 19 as the upper electrode plate to produce low flatness is broken through, and the flatness below the anode 19 is ensured, thereby improving the yield of the panel.
[0061] Based on the above embodiments, Figure 2 As shown, in another specific embodiment of the present application, in the metal routing area C, the shading layer 12 further includes a third shading layer 123, the buffer layer 13 further includes a second buffer layer 132, the active layer 14 further includes a second active layer 142, the gate insulating layer 15 further includes a third gate insulating layer 153, and the metal layer 16 further includes a third metal layer 165.
[0062] In the above embodiment of the present invention, in order to avoid the loss of the buffer layer 13 in the capacitor region B during the etching process of the buffer layer 13, an active layer 14 is present above the region to reduce the risk of short circuit between the metal layer 16 and the light shielding layer 12 due to the reduction of the dielectric layer thickness caused by the etching of the buffer layer 13, thereby improving the process yield.
[0063] In one embodiment, Figure 2 As shown, the top-emitting OLED device comprises:
[0064] an anode 19, wherein the anode 19 is located above the capacitor region B and is electrically connected to the driving TFT region A;
[0065] a light-emitting material layer, wherein the light-emitting material layer is located on the anode 19; and
[0066] A cathode covers the light emitting material layer.
[0067] Specifically, the orthographic projection of the anode 19 on the AMOLED display panel covers the capacitor area B. The covering refers to partial covering or complete covering.
[0068] The anode 19 is a three-layer structure of an indium tin oxide (ITO) layer, a silver (Ag) metal layer 16 and an ITO layer (ITO / Ag / ITO).
[0069] In the embodiment of the present invention, the anode 19 is located directly above the capacitor region B, which is different from the conventional top-emitting OLED device in that the anode 19 is not located directly above the capacitor region B. Therefore, the resolution of the display panel can be higher.
[0070] In another specific embodiment of the present application, the gate, source 163 and drain 161 are divided into two layers, the lower layer is a contact enhancement layer, containing one or more alloys of molybdenum (Mo), titanium (Ti), nickel (Ni), and the thickness range is The upper layer is the main metal wiring layer, containing copper (Cu) or Cu alloy, with a thickness range of
[0071] In another specific embodiment of the present application, the light shielding layer 12 is divided into three layers, the upper layer is a contact enhancement layer, containing one or more alloys of Mo, Ti, and Ni, the middle layer is a main metal wiring layer, containing Cu or Cu alloy, and the upper layer is an oxidation protection layer to prevent the middle main wiring layer from oxidation failure during the array substrate (Array) process, containing one or more alloys of Mo, Ti, and Ni. Among them, the thickness range of the lower layer is Thickness range of the middle layer Thickness range of upper layer
[0072] In another specific embodiment of the present application, the material of the active layer 14 is indium gallium zinc oxide (IGZO), indium tin zinc oxide (ITZO) or indium gallium zinc tin oxide (IGZTO).
[0073] It should be noted that the above display panel embodiment only describes the above structure. It can be understood that in addition to the above structure, the display panel of the embodiment of the present invention may also include any other necessary structures as needed, such as a polarizer and a cover plate, etc., which are not specifically limited here.
[0074] The present invention also provides a method for preparing an AMOLED display panel, comprising the following steps:
[0075] (1) providing a substrate 11, on which a plurality of driving TFT regions A, a plurality of capacitor regions B, and a plurality of metal wiring regions C are divided;
[0076] (2) depositing a light shielding layer 12, a buffer layer 13 and an active layer 14 on the substrate 11 in sequence, and removing the buffer layer 13 in the capacitor region B;
[0077] (3) A gate insulating layer 15, a metal layer 16 and a top-emitting OLED device are sequentially deposited on the light-shielding layer 12, the buffer layer 13 and the active layer 14.
[0078] Specifically, the step of sequentially depositing the light shielding layer 12, the buffer layer 13 and the active layer 14 on the substrate 11 and removing the buffer layer 13 in the capacitor region B comprises the following steps:
[0079] S11 Figure 3 As shown, a whole-surface light shielding layer 12 is deposited on the substrate 11, and the whole-surface light shielding layer 12 is etched and patterned using a first yellow light process to form a first light shielding layer 121 in the driving TFT area A, a second light shielding layer 122 in the capacitor area B, and a third light shielding layer 123 in the metal wiring area C;
[0080] S12 Figure 4 As shown, a buffer layer 13 and an active layer 14 are sequentially deposited on the light-shielding metal layer 16, an organic photoresist layer 10 is deposited on the active layer 14, and a second yellow light process is used to etch and pattern the active layer 14 to form a first active layer 141 of the driving TFT area A and a second active layer 142 of the metal wiring area C;
[0081] S13 Figure 5 As shown, the first active layer 141 and the second active layer 142 are used to etch the lower buffer layer 13 to remove the buffer layer 13 of the capacitor area B, thereby forming the first buffer layer 131 of the driving TFT area A and the second buffer layer 132 of the metal wiring area C.
[0082] Specifically, the gate insulating layer 15, the metal layer 16 and the top-emitting OLED device are sequentially deposited on the light shielding layer 12, the buffer layer 13 and the active layer 14, comprising the steps of:
[0083] S14 Figure 6 As shown, a gate insulating layer 15 is deposited on the entire surface of the active layer 14, and a third yellow light process is used to perform a hole opening and a conductor process on the gate insulating layer 15 of the driving TFT area A to form a first gate insulating layer 151 of the driving TFT area A, a second gate insulating layer 152 of the capacitor area B, and a third gate insulating layer 153 of the metal wiring area C;
[0084] S15 Figure 7 As shown, a metal layer 16 is deposited on the gate insulating layer 15, an organic photoresist layer 10 is deposited on the metal layer 16, and a fourth yellow light process is used for patterning, and the metal layer 16 is etched to form a first metal layer 160 of the driving TFT area A, a second metal layer 164 of the capacitor area B, and a third metal layer 165 of the metal wiring area C, wherein the first metal layer 160 includes a gate 162, a source 163, and a drain 161 on the same layer;
[0085] S16 Figure 8 As shown, the gate insulating layer 15 is self-aligned and etched using the patterned metal layer 16 to form a self-aligned channel region in the driving TFT region A;
[0086] S17 sequentially deposits a passivation layer 17 and a planarization layer 18, patterns and perforates the passivation layer 17 and the planarization layer 18, deposits and patterns an anode 19 of a top-emitting OLED device, deposits an organic photoresist layer 10 again, and patterns and defines an OLED light-emitting area, and obtains Figure 2 The AMOLED display panel shown.
[0087] Specifically, the material of the active layer 14 is IGZO, ITZO or IGZTO.
[0088] In order to better implement the method for preparing the AMOLED display panel of the present invention, the present invention also provides a more specific embodiment, including the steps of:
[0089] S21: Clean the glass substrate 11, divide it into a plurality of driving TFT areas A, a plurality of capacitor areas B and a plurality of metal wiring areas C, and deposit a whole-surface light shielding layer 12 on the glass substrate 11. The whole-surface light shielding layer 12 adopts a three-layer wiring structure, the lower layer is a contact enhancement layer, and contains one or more alloys of Mo, Ti and Ni, with a thickness range of The middle layer is the main metal wiring layer, made of Cu or Cu alloy, with a thickness range of The upper metal layer is an oxidation protection layer to prevent the middle main wiring layer from oxidation failure during the array process. It contains one or more alloys of Mo, Ti, and Ni. The thickness range is Using the first yellow light process, wet etching (Wet) is used to pattern the entire light shielding layer 12 to form a light shielding layer 12 pattern with routing and light shielding functions;
[0090] S22 uses a plasma enhanced chemical vapor deposition (PECVD) process to deposit a buffer layer 13 on the patterned light shielding layer 12 substrate 11. The buffer layer 13 can be a single layer of Si3N4, a single layer of SiO2, a single layer of SiON, or a double layer structure of the above film layers, with a total thickness of
[0091] S23 Physical vapor deposition (PVD) process is used to deposit the active layer 14, which can be IGZO, ITZO or IGZTO, etc. The active layer 14 is patterned using a second yellow light process to define the active area and the light shielding layer 12 wiring area. The thickness of the active layer 14 is
[0092] S24: using the yellow light pattern of the active layer 14, etching the buffer layer 23, ensuring that the buffer layer 13 above the light shielding layer 12 in the capacitor region B is removed, while the buffer layer 13 is retained in the metal wiring region C due to the presence of the yellow light pattern of the active layer 14;
[0093] S25 PECVD process is used to deposit the entire gate insulating layer 15, the material of which is SiOx, wherein the oxygen content can be controlled by the PECVD process technology. The gate insulating layer 15 is used as a dielectric layer of the capacitor in the capacitor region B. Since the thickness of the gate insulating layer 15 is significantly lower than that of the buffer layer 13, the capacitance value can be effectively increased.
[0094] S26 uses the third yellow light process to perform a hole opening process on the GI of the TFT area to form metal contact holes in the S / D area and perform conductor processing to reduce the resistance value of the AOS in the S / D area;
[0095] S27 PVD process deposits metal layer 16, the metal is a double-layer metal structure, the lower layer is a contact enhancement layer, containing one or more alloys of Mo, Ti, Ni, and the thickness range is The upper layer is the main metal trace, made of Cu or Cu alloy, with a thickness of The two layers of metal are patterned by a fourth yellow light process, and the two layers of metal wiring are etched by a Wet process to form the metal layer 16 of the driving TFT area A, the capacitor area B and the metal wiring area C, wherein the metal layer 16 of the driving TFT area A includes a gate electrode 162, a source electrode 163 and a drain electrode 161 on the same layer, and the metal layer 16 of the capacitor area B can be used as an upper electrode plate of the capacitor area B;
[0096] S28: using the metal layer 16 pattern as a pattern for dry etching the gate insulating layer 15, etching the gate insulating layer 15, forming a gate 162 / gate insulating layer 15 / active layer 14 (Gate / GI / IGZO) channel region structure by self-alignment, and performing a conductorization process to reduce the IGZO resistance value of the source 163 / drain 161 (S / D) region;
[0097] S29 uses PECVD process to deposit a passivation layer 17 (PV) SiO2 film with a thickness of Used to protect the underlying TFT devices;
[0098] S210 deposits an organic planar layer 18 (PLN), and uses the fifth yellow light process to pattern the PLN layer, and uses the PLN pattern to etch the PV opening to form a contact hole;
[0099] S211 deposits the first OLED device electrode layer, and patterns the electrode layer using the sixth yellow light process;
[0100] S212 The electrode layer of the patterned OLED device is covered with an organic photoresist layer, and a yellow light process is used to define the light-emitting area of the OLED device, which is used for the inkjet printing technology in the post-process to prepare the OLED device.
[0101] In the embodiment of the present invention, a method for preparing an AMOLED display panel is provided. The buffer layer 13 is not set in the capacitor area B to reduce the thickness of the capacitor in the capacitor area B, and high capacitance is ensured without changing the area of the capacitor and without using an interlayer capacitor, thereby ensuring the flatness under the anode 19 of the top-emitting OLED device. Compared with the traditional preparation method, the capacitor in the capacitor area B does not need to be set with a buffer layer 13 and an active layer 14, thereby effectively reducing the complexity of the manufacturing process and improving production efficiency.
[0102] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, please refer to the detailed description in other embodiments above, and will not be repeated here.
[0103] In specific implementation, the above units or structures can be implemented as independent entities, or can be arbitrarily combined to be implemented as the same or several entities. The specific implementation of the above units or structures can refer to the previous method embodiments, which will not be repeated here.
[0104] The specific implementation of the above operations can be found in the previous embodiments, which will not be described in detail here.
[0105] An AMOLED display panel and a preparation method thereof provided by an embodiment of the present invention are introduced in detail above. Specific examples are used herein to illustrate the principle and implementation mode of the present invention. The description of the above embodiments is only used to help understand the method and core idea of the present invention. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation mode and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. An AMOLED display panel, characterized in that: include: A TFT array substrate and a plurality of top-emitting OLED devices disposed on the TFT array substrate, wherein the top-emitting OLED devices include an anode, The TFT array substrate comprises: The substrate is divided into a plurality of driving TFT areas, a plurality of capacitor areas and a plurality of metal wiring areas, wherein a capacitor is provided in the capacitor area, and the capacitor is composed of a lower electrode plate, a capacitor dielectric layer and an upper electrode plate stacked in sequence, and the anode is located directly above the capacitor area, and the positive projection of the anode on the AMOLED display panel covers the capacitor area; A light-shielding metal layer is arranged on the substrate, comprising a first light-shielding layer located in the driving TFT area and a second light-shielding layer located in the capacitor area, wherein the second light-shielding layer is a lower electrode plate of the capacitor, and the light-shielding metal layer is divided into three layers, wherein the lower layer is a contact enhancement layer, the middle layer is a main metal wiring layer, and the upper layer is an oxidation protection layer; A buffer layer is disposed on the light-shielding metal layer, comprising a first buffer layer located in the driving TFT region, wherein the capacitor region is not provided with a buffer layer; An active layer, disposed on the buffer layer, comprising a first active layer located in the driving TFT region; a gate insulating layer, disposed on the active layer, comprising a first gate insulating layer located in the driving TFT region and a second gate insulating layer located in the capacitor region, wherein the second gate insulating layer is a capacitor dielectric layer of the capacitor; and A metal layer, disposed on the gate insulating layer, comprising a first metal layer located in the driving TFT region and a second metal layer located in the capacitor region, wherein the first metal layer includes a gate, a source and a drain on the same layer, and the second metal layer is an upper electrode plate of the capacitor; In the metal wiring area, the light-shielding metal layer further includes a third light-shielding layer, the buffer layer further includes a second buffer layer, the active layer further includes a second active layer, the gate insulating layer further includes a third gate insulating layer, the metal layer further includes a third metal layer, the first active layer and the second active layer are arranged in the same layer; two ends of the third metal layer are bent toward a side close to the substrate; The first light-shielding layer, the second light-shielding layer and the third light-shielding layer are spaced apart from each other, the first gate insulating layer, the second gate insulating layer and the third gate insulating layer are spaced apart from each other, and the first metal layer, the second metal layer and the third metal layer are spaced apart from each other.
2. The AMOLED display panel according to claim 1, characterized in that: The top-emitting OLED device comprises: an anode, the anode being located above the capacitor region and electrically connected to the driving TFT region, wherein the orthographic projection of the anode on the AMOLED display panel covers the capacitor region; a light-emitting material layer, the light-emitting material layer being located on the anode; and A cathode covers the light emitting material layer.
3. The AMOLED display panel according to claim 1, characterized in that: The gate, source and drain are divided into two layers, the lower layer contains one or more alloys of Mo, Ti and Ni, and the upper layer contains Cu or a Cu-containing alloy.
4. The AMOLED display panel according to claim 1, characterized in that: The lower layer contains an alloy of one or more of Mo, Ti, and Ni, the middle layer contains Cu or an alloy containing Cu, and the upper layer contains an alloy of one or more of Mo, Ti, and Ni.
5. The AMOLED display panel according to claim 1, characterized in that: The active layer material is IGZO, ITZO or IGZTO.
6. A method for preparing an AMOLED display panel, characterized in that: Includes steps: A substrate is provided, on which a plurality of driving TFT areas, a plurality of capacitor areas and a plurality of metal wiring areas are divided, wherein a capacitor is provided in the capacitor area, and the capacitor is composed of a lower electrode plate, a capacitor dielectric layer and an upper electrode plate stacked in sequence; Depositing a whole surface of a light-shielding metal layer on a substrate, and using a first yellow light process to etch and pattern the whole surface of the light-shielding metal layer to form a first light-shielding layer in the driving TFT area, a second light-shielding layer in the capacitor area, and a third light-shielding layer in the metal wiring area which are spaced apart from each other, wherein the second light-shielding layer is a lower electrode plate of the capacitor, and the light-shielding metal layer is divided into three layers, wherein the lower layer is a contact enhancement layer, the middle layer is a main metal wiring layer, and the upper layer is an oxidation protection layer; Sequentially depositing a buffer layer and an active layer on the entire surface above the light-shielding metal layer, and etching and patterning the entire surface of the active layer using a second yellow light process to form a first active layer in the driving TFT area and a second active layer in the metal wiring area, wherein the first active layer and the second active layer are arranged in the same layer; Using the yellow light patterns of the first active layer and the second active layer, etching the lower buffer layer, removing the buffer layer in the capacitor area, and forming the first buffer layer in the driving TFT area and the second buffer layer in the metal wiring area; A gate insulating layer, a metal layer and a top-emitting OLED device are sequentially deposited on the light-shielding metal layer, the buffer layer and the active layer, comprising: depositing a whole surface of the gate insulating layer above the active layer, performing a hole-opening and conductorization process on the gate insulating layer of the driving TFT region using a third yellow light process, so as to form a first gate insulating layer of the driving TFT region, a second gate insulating layer of the capacitor region and a third gate insulating layer of the metal wiring region which are arranged at intervals from each other, wherein the second gate insulating layer is a capacitor dielectric layer of the capacitor; Depositing a metal layer on the gate insulating layer, patterning it using a fourth yellow light process, and etching the metal layer to form a first metal layer in the driving TFT area, a second metal layer in the capacitor area, and a third metal layer in the metal wiring area which are spaced apart from each other, wherein the second metal layer is an upper electrode plate of the capacitor, the first metal layer includes a gate, a source, and a drain on the same layer, and both ends of the third metal layer are bent toward a side close to the substrate; Performing self-aligned etching on the gate insulating layer using the patterned metal layer to form a self-aligned channel region in the driving TFT region; A passivation layer and a planarization layer are deposited in sequence, the passivation layer and the planarization layer are patterned and holes are opened, an anode of a top-emitting OLED device is deposited and patterned, an organic photoresist layer is deposited again, and the OLED light-emitting area is defined by patterning, the anode is located directly above the capacitor area, and the positive projection of the anode on the AMOLED display panel covers the capacitor area.
7. The method for preparing an AMOLED display panel according to claim 6, characterized in that: The material of the active layer is IGZO, ITZO or IGZTO.