Method for manufacturing semiconductor device
By forming hollow grooves on the first substrate of the semiconductor device and attaching the second substrate, using alkaline hydroxide and hydrogen fluoride compound etching technology, the problem of low device yield in the prior art is solved, and efficient thin film structure separation is achieved and manufacture.
Patent Information
- Application Number
- CN202011491189.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-12-23
- Filing Date
- 2020-12-16
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-12-16
AI Technical Summary
In the conventional MEMS pressure sensor manufacturing method, a structural layer is formed on the upper part of the sacrificial layer, making it difficult for etching substances to penetrate into the lower part of the device, resulting in a low device yield.
By forming a hollow groove on one side surface of the first substrate, attaching the second substrate, and forming a thin film structure on its surface, etching is performed using alkaline hydroxide and hydrogen fluoride compound, and finally separating the second substrate by vacuum adsorption or tweezers to form Film structure.
The separation yield of the thin film structure of semiconductor devices is improved, the process is simplified, and the manufacturing efficiency of the device is improved.
Smart Images

Figure CN113086942B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing a semiconductor device, and more particularly, to a method for forming a hollow groove structure at the bottom of a semiconductor device during a manufacturing process of the semiconductor device to facilitate device separation. Background Art
[0002] Recently, with the development of science and technology, electronic products such as smartphones, laptops, and built-in devices have gradually developed in a trend of miniaturization. On the other hand, as the number of components configured in an electronic product increases, the size requirement for each component has also developed in a trend of miniaturization.
[0003] Sensors are very important for electronic products because they can measure external signals such as position and acceleration to provide basic data that allows a central processing unit to provide necessary information to users.
[0004] Among them, the pressure sensor is a device that can receive the magnitude of the force applied to the sensor as a physical quantity and convert it into an electrical signal output. It can be divided into a piezoresistive sensor and an electrostatic capacitance sensor according to the pressure detection method. That is, when a thin film is formed by a semiconductor process and a silicon piezoresistive body is formed in the middle of the substrate to cause the thin film to deform due to pressure, the above-mentioned piezoresistive sensor can utilize the change in resistance of the piezoresistive body. When the interval between the electrode plates changes due to external stress, the above-mentioned electrostatic capacitance sensor can utilize the change in electrostatic capacitance between the electrodes.
[0005] This MEMS pressure sensor is formed by evaporating a structural layer and a sacrificial layer on a non-conductive substrate such as a silicon substrate, a III-V compound substrate such as a gallium arsenic compound, or a sapphire substrate, and then separating the structural layer from the substrate through an etching process for removing the sacrificial layer.
[0006] However, the prior art of manufacturing MEMS pressure sensors based on sacrificial layers has the following problem: since the structural layer is formed on the upper part of the sacrificial layer, it is difficult for etching materials to penetrate into the lower part of the device, thereby damaging the structural layer, resulting in low yield.
[0007] Prior art literature
[0008] Patent Literature
[0009] Patent Document 0001: Korean Patent Publication No. 10-1923671 Summary of the invention
[0010] Technical issues
[0011] The present invention is proposed to improve the problems of the conventional method for manufacturing a semiconductor device as described above, and an object of the present invention is to provide a method for manufacturing a semiconductor device that facilitates device separation.
[0012] Technical Solution
[0013] In order to achieve the purpose as described above, a semiconductor device can be provided by the following method. The manufacturing method of the semiconductor device of the present invention is characterized in that it includes: a step of forming a hollow groove by etching a side surface of a first substrate; a step of attaching a second substrate to the first substrate having the hollow groove formed thereon; a step of retaining only the silicon active layer by etching the second substrate; a step of forming a thin film structure on the surface of the silicon active layer of the second substrate; and a step of separating the second substrate having the thin film structure formed thereon from the first substrate.
[0014] The present invention is characterized in that the first substrate is a III-V compound composed of gallium arsenic compound or gallium nitride, silicon, silicon carbide, silicon oxide (SiOx) or aluminum oxide (AlOx) substrate.
[0015] The present invention is characterized in that the second substrate 20 is a silicon substrate or a silicon on insulator (SOI) substrate having an insulating oxide layer and a single crystal silicon layer formed on a silicon substrate.
[0016] The present invention is characterized in that in the step of forming the hollow groove of the first substrate, an alkaline aqueous solution containing an alkaline hydroxide such as potassium hydroxide, sodium hydroxide, ethylenediamine pyrocatechol (EDP) or tetramethylammonium hydroxide, hydroxylamine and thiourea is used.
[0017] The present invention is characterized in that, in the step of attaching the second substrate to the first substrate, the attachment is performed by fusion welding or hybrid welding.
[0018] The present invention is characterized in that, in the step of retaining only the silicon layer by etching the above-mentioned second substrate, etching is performed using an alkaline aqueous solution containing alkaline hydroxides, hydroxylamine and thiourea, and then etching is performed using an aqueous solution containing a hydrogen fluoride compound or a gas containing a hydrogen fluoride compound, wherein the above-mentioned alkaline hydroxide contains potassium hydroxide, sodium hydroxide, ethylenediamine pyrocatechol (EDP) and tetramethylammonium hydroxide.
[0019] The present invention is characterized in that, in the step of forming a thin film structure on one side surface of the above-mentioned second substrate, a silicon oxide (SiOx) layer formed by oxidizing a portion of the silicon layer through a thermal oxidation process and a silicon oxide (SiOx) layer and a silicon nitride (SiNx) layer formed by chemical reaction on the surface of the silicon layer using a low-temperature chemical vapor deposition method (LPCVD) are stacked on the surface of the silicon layer of the above-mentioned second substrate.
[0020] The present invention is characterized in that, in the step of forming a thin film structure on one side surface of the second substrate, heat treatment is performed after the thin film structure is doped with a P-type dopant containing boron.
[0021] The present invention is characterized in that, in the step of forming a thin film structure on one side surface of the second substrate, a reaction gas containing at least one of argon or a boron compound is used to etch the thin film structure.
[0022] The present invention is characterized in that in the step of forming a thin film structure on one side surface of the second substrate, any one of aluminum, copper and tungsten is evaporated.
[0023] The present invention is characterized in that, in the step of separating the second substrate from the first substrate, vacuum suction or tweezers are used to separate the second substrate from the first substrate.
[0024] Effects of the Invention
[0025] As described above, the manufacturing method of the semiconductor device of the present invention has the following effect, that is, before the step of forming the thin film structure of the semiconductor device is performed, after a hollow groove structure is formed on one side surface of the above-mentioned first substrate, the above-mentioned second substrate and the above-mentioned first substrate formed with the thin film structure can be easily separated, thereby improving the yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 The flowchart is used to illustrate the method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0027] Figure 2 It is a schematic diagram showing a cross section of a first substrate having a hollow groove formed therein in a method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0028] Figure 3 The diagram is a simplified diagram showing a cross section of a second substrate combined with a first substrate in a method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0029] Figure 4 A simplified diagram showing cross sections of a second substrate and a first substrate in which only a silicon layer is left by etching in a method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0030] Figure 5The diagram is a simplified diagram showing cross sections of a second substrate and a first substrate on which a thin film structure is formed in a method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0031] Figure 6 It is a simplified diagram showing the cross-sections of the second substrate and the first substrate formed by doping the thin film structure with a P-type dopant containing boron and then performing a heat treatment in the method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0032] Figure 7 The diagram is a simplified cross-sectional view of the second substrate and the first substrate showing etching of a portion of the thin film structure in the method for manufacturing a semiconductor device according to an embodiment of the present invention.
[0033] Figure 8 It is a schematic diagram showing the cross-section of the second substrate and the first substrate in the method for manufacturing a semiconductor device according to an embodiment of the present invention, in which metal is evaporated onto the thin film structure.
[0034] Fig. 9 The diagram is a schematic cross-sectional view of the second substrate and the first substrate showing etching of a part of the side surface of the thin film structure in the method for manufacturing a semiconductor device according to the embodiment of the present invention.
[0035] Fig.10 The diagram is a schematic diagram showing a cross section of the second substrate separated from the first substrate in the method for manufacturing a semiconductor device according to the embodiment of the present invention.
[0036] Description of Reference Numerals
[0037] 10: First substrate
[0038] 11: First support layer
[0039] 12: Hollow slot
[0040] 20: Second substrate
[0041] 21: Silicon active layer
[0042] 22: First insulating film
[0043] 23: Second support layer
[0044] 24: Second insulating film
[0045] 25: Nitride film
[0046] 26: Doping Department
[0047] 27: Electrode DETAILED DESCRIPTION
[0048] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.
[0049] The present invention can be modified in many ways and has many embodiments. The drawings illustrate specific embodiments, which will be described in detail in the detailed description. However, this does not limit the present invention to specific embodiments, and should be interpreted as including all modifications, equivalent technical solutions and alternative technical solutions within the scope of the concept and technology of the present invention.
[0050] When describing the present invention, the terms "first", "second", etc. are only used to describe various structural elements, and the above terms do not limit the above structural elements. The above terms are only used to distinguish between other structural elements and one structural element. For example, without departing from the scope of protection of the invention claimed in the present invention, the first structural element may also be named as the second structural element, and similarly, the second structural element may also be named as the first structural element.
[0051] The term "and / or" has a meaning that may include a combination of a plurality of related recited items or any combination of a plurality of related recited items.
[0052] When it is said that a certain structural element is "connected" or "coupled" to other structural elements, it can be understood that it is directly connected or directly coupled to other structural elements, but it can also be understood that other structural elements exist in between. Conversely, when it is said that a certain structural element is "directly connected" or "directly coupled" to other structural elements, it can be understood that there are no other structural elements in between.
[0053] The terms used in this application are only used to illustrate specific embodiments and do not have the meaning of limiting the present invention. Unless clearly indicated in the context, a singular expression may include a plural expression.
[0054] In the present application, it should be understood that terms such as "including" or "having" are only used to specify the existence of features, numbers, steps, actions, structural elements, parts or combinations thereof recorded in the specification, and do not preclude the existence or additional possibilities of one or more other features, numbers, steps, actions, structural elements, parts or combinations thereof.
[0055] Unless otherwise defined, all terms used herein, including technical or scientific terms, may have the same meaning as those generally understood by a person of ordinary skill in the art to which the present invention belongs. Terms defined in commonly used dictionaries may be interpreted as having the same meaning as that in the context of the relevant art, and unless clearly defined in this application, should not be interpreted in an ideal or overly formal sense.
[0056] Moreover, the following embodiments are provided only for those skilled in the art to more completely illustrate the present invention. For further clarity of the description, the shapes and sizes of the structural elements in the drawings may be magnified.
[0057] Reference Figure 1 A method for manufacturing a semiconductor device according to an embodiment of the present invention may include: step S10 of forming a hollow groove by etching a side surface of a first substrate; step S20 of attaching a second substrate including a silicon layer to a side surface of the first substrate having the hollow groove formed thereon; step S30 of etching the second substrate to retain only the silicon layer; step S40 of forming a thin film structure on a surface of the silicon layer of the second substrate; and step S50 of separating the second substrate having the thin film structure formed thereon from the first substrate.
[0058] Although in Figure 1 The manufacturing method of the semiconductor device is shown in 5 steps, but the present invention is not limited to this. It can be divided or repeatedly implemented according to specific processes, which can be regarded as belonging to the scope of the present invention. For the convenience of explanation, the following 5 steps are used to illustrate the manufacturing method of the semiconductor device. Figures 2 to 10 .
[0059] Reference Figure 2 According to one embodiment of the present invention, in step S10 of forming a hollow groove by etching one side surface of the first substrate, one of III-V compounds composed of gallium arsenic compounds or gallium nitride, silicon, silicon carbide, silicon oxide (SiOx) or aluminum oxide (AlOx) can be used as the substrate. For example, a p-type single crystal silicon substrate containing boron, aluminum, gallium, and indium elements commonly used in semiconductor processes or an n-type single crystal silicon substrate containing phosphorus, antimony, and bismuth elements can be used. As another example, a quartz substrate or a sapphire substrate commonly used in light emitting diode (LED) or thin film field effect transistor type display (TET) processes can be used.
[0060] According to one embodiment of the present invention, in step S10 of etching a side surface of the first substrate to form a hollow groove, after coating the first substrate with an alkaline aqueous solution containing an alkaline hydroxide selected from potassium hydroxide, sodium hydroxide, ethylenediaminepyrocatechol (EDP) or tetramethylammonium hydroxide, hydroxylamine and thiourea and immersing the first substrate for a predetermined time, a hollow groove having a desired height and width can be formed by washing. For example, a potassium hydroxide standard solution containing 0.1M potassium hydroxide can be used in the process to form a hollow groove having a height of 1 to 50 microns.
[0061] Reference Figure 3The step S20 of attaching a second substrate including a silicon layer to a surface of one side of a first substrate having a hollow groove formed thereon according to an embodiment of the present invention is characterized in that an epitaxial silicon-on-insulator substrate including a silicon active layer 21, a first insulating film 22, and a second supporting layer 23 can be used as the second substrate 20, and during the process of the silicon active layer 21, the first insulating film 22 blocks the influence of the second supporting layer 23. For example, the epitaxial silicon-on-insulator substrate can be a structure in which a silicon oxide film is formed on the upper part of the silicon supporting layer and a single crystal silicon active layer is formed on the upper part of the silicon oxide film.
[0062] According to one embodiment of the present invention, the step S20 of attaching a second substrate including a silicon layer to a side surface of a first substrate having a hollow groove is characterized in that the first substrate 10 and the second substrate 20 are formed by chemical bonding and melting welding in a heating process without an additional intermediate layer. For example, by heating the hydroxyl groups (-OH) formed on the surface of the first substrate 10 composed of silicon and the surface of the second substrate 20 composed of silicon to form an ether bond (-O-) and attach them, not only can the process be simplified, but also the economic efficiency can be improved because no additional materials are required.
[0063] Reference Figure 4 According to one embodiment of the present invention, in step S30 of etching the second substrate to retain only the silicon layer, after the first substrate is coated with or immersed in an alkaline aqueous solution containing an alkaline hydroxide selected from potassium hydroxide, sodium hydroxide, ethylenediaminepyrocatechol (EDP) or tetramethylammonium hydroxide, hydroxylamine and thiourea and maintained for a predetermined time, the second support layer 23 can be removed by washing. For example, the entire silicon support layer can be removed by using a potassium hydroxide standard solution containing 0.1M potassium hydroxide in the process.
[0064] According to an embodiment of the present invention, in step S30 of etching the second substrate to retain only the silicon layer, an aqueous solution containing a hydrogen fluoride compound or a gas containing a hydrogen fluoride compound may be used for etching. For example, a solution containing 49% hydrogen fluoride in water and ammonium fluoride may be used for etching.
[0065] Reference Figure 5 According to one embodiment of the present invention, in the step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate, a portion of the silicon active layer 21 may be oxidized by a thermal oxidation process to form the second insulating film 24. For example, oxygen or water may be injected and heated within a temperature range of 800°C to 1000°C, so that the silicon active layer 21 forms silicon oxide through a chemical reaction. Under the same temperature condition, when water is injected, a thicker oxide film may be formed compared to the case where only oxygen is injected.
[0066] According to one embodiment of the present invention, the step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate is characterized in that a second insulating film 24 and a nitride film 25 are formed on the surface of the silicon active layer 21 using a low temperature chemical vapor deposition method (LPCVD), wherein the insulating film and the nitride film can be repeatedly stacked. For example, an insulating film composed of silicon oxide can be formed by thermally decomposing tetraethyl orthosilicate (TEOS). As another example, a nitride film composed of silicon oxide can be formed by reacting silane gas with ammonia gas.
[0067] Reference Figure 6 According to one embodiment of the present invention, the step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate is characterized in that heat treatment is performed after the above-mentioned thin film structure is doped with a P-type dopant containing boron. For example, a photosensitive film, oxide, nitride, polysilicon, or metal film is evaporated on the surface of the thin film structure as a mask material, and after the boron trifluoride gas is ionized in a high vacuum environment, it can be accelerated to 5000 keV to be injected into the thin film layer and heat treated. As another example, the resistance can be locally adjusted by changing the concentration of boron used as a P-type dopant and performing multiple doping. It can be divided or repeatedly implemented according to specific processes, and these can be regarded as belonging to the scope of the present invention.
[0068] Reference Figure 7 According to one embodiment of the present invention, the step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate is characterized in that a reaction gas containing at least one of argon or a boron compound is used to etch the thin film structure. For example, under the condition of a gas pressure of 0.01 to 0.1 Torr, a voltage of 250 to 500 V can be used to ionize the reaction gas containing carbon tetrafluoride to etch silicon oxide. As another example, a reaction gas containing carbon tetrafluoride and oxygen is used, and the reaction rate can be adjusted according to the oxygen concentration.
[0069] Reference Figure 8 According to one embodiment of the present invention, the step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate is characterized in that any one of aluminum, copper, and tungsten can be evaporated. For example, a metal target containing one of aluminum, copper, and tungsten can be used, and the evaporation is performed by a sputtering process using argon gas. As another example, a metal target containing one of aluminum, copper, and tungsten can be used, and the evaporation and evaporation are performed by arc discharge. The electrode portion 27 can be formed by this process.
[0070] Reference Fig. 9According to one embodiment of the present invention, in step S40 of forming a thin film structure on the surface of the silicon layer of the second substrate, a reaction gas containing at least one of argon or boron compounds can be used to etch a portion of the silicon active layer. For example, under the condition of a gas pressure of 0.01 to 0.1 Torr, a voltage of 250 to 500 V can be used to ionize the reaction gas containing carbon tetrafluoride, so that the silicon active layer without a thin film structure can be etched. In step S50, the second substrate in which a portion of the silicon active layer is etched to form a thin film structure can be easily separated from the first substrate.
[0071] Reference Fig.10 The step S50 of separating the second substrate having the thin film structure formed thereon from the first substrate is characterized in that the second substrate is separated from the first substrate using vacuum adsorption or tweezers. For example, a device for fixing the product by adsorbing the product is used, that is, after the first substrate is adsorbed by a vacuum suction cup, an external force can be applied to the upper part of the first substrate to separate the second substrate from the second substrate.
[0072] As described above, it should be understood that, without changing the technical concept or essential features of the present invention, a person skilled in the art can implement the technical structure of the present invention in other specific embodiments.
[0073] Therefore, it should be understood that the multiple embodiments described above are merely examples at all levels and have no restrictive meaning. The scope of the present invention should be expressed according to the scope of protection claimed in the invention rather than the detailed invention described above. The meaning and scope of the scope of protection claimed in the invention and all changes or modified embodiments derived from equivalent technical solutions belong to the scope of the present invention.
Claims
1. A method for manufacturing a semiconductor device, It is characterized in that include: A step (S10) of forming a hollow groove (12) by etching a surface of one side of the first substrate (10); A step (S20) of attaching a second substrate (20) including a silicon active layer (21) to a surface of one side of the first substrate having the hollow groove formed thereon; A step of etching the second substrate to retain only the silicon active layer (S30); A step (S40) of forming a thin film structure consisting of at least one layer on the surface of the silicon active layer of the second substrate; and a step (S50) of separating the second substrate having a thin film structure from the first substrate, In the step (S40) of forming a thin film structure on one side surface of the second substrate (20), a silicon oxide layer (24) formed by oxidizing a portion of the silicon active layer by a thermal oxidation process and a silicon oxide layer and a silicon nitride layer (25) formed by chemical reaction on the surface of the silicon layer by a low-temperature chemical vapor deposition method are stacked on the surface of the silicon layer of the second substrate. In the step (S40) of forming a thin film structure on one side surface of the second substrate, a portion of the silicon active layer where the thin film structure is not formed is etched using a reaction gas containing at least one of argon or a fluorine-based compound to form a groove, so that in the step (S50) of separating the second substrate having the thin film structure formed thereon from the first substrate, separation is achieved, The second substrate (20) is an epitaxial silicon-on-insulator substrate.
2. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that At least one of the group consisting of a III-V compound composed of a gallium arsenic compound or gallium nitride, silicon, silicon carbide, silicon oxide or aluminum oxide is used as the first substrate (10).
3. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the step (S10) of forming the hollow groove (12) of the first substrate (10), an alkaline aqueous solution containing at least one alkaline hydroxide selected from potassium hydroxide, sodium hydroxide, catechol ethylenediamine or tetramethylammonium hydroxide, hydroxylamine and thiourea is used.
4. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the step (S20) of attaching the second substrate (20) to the first substrate (10) formed with the hollow groove (12), the attachment is performed by fusion welding or hybrid welding.
5. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that The step (S30) of etching the second substrate (20) to retain only the silicon active layer (21) comprises: The step of etching using at least one alkaline aqueous solution containing an alkaline hydroxide selected from potassium hydroxide, sodium hydroxide, catechol ethylenediamine and tetramethylammonium hydroxide, hydroxylamine and thiourea; and The step of performing etching using an aqueous solution containing a hydrogen fluoride compound or a gas containing a hydrogen fluoride compound.
6. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the step (S40) of forming a thin film structure on one side surface of the second substrate, a heat treatment is performed after the thin film structure is doped with a P-type dopant containing boron.
7. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the step (S40) of forming a thin film structure on one side surface of the second substrate, any one of aluminum, copper and tungsten is evaporated.
8. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the step ( S50 ) of separating the second substrate from the first substrate, the second substrate is separated from the first substrate using vacuum suction or tweezers.