A fan-out packaging structure with reduced warpage
By adjusting the thickness of the epoxy plastic seal material on both sides of the chip in the fan-out package and designing the metal interconnect structure, the problem of wafer warpage control in the prior art is solved, and the effect of effectively reducing warpage is achieved.
Patent Information
- Application Number
- CN202111471260.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-03
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2041-12-03
AI Technical Summary
The existing fan-out packaging technology has difficulties in wafer warping control, mainly because the thermal expansion coefficients of epoxy plastic packaging materials and silicon materials are too large, which makes it difficult to solve the warping problem after packaging.
By adjusting the thickness of the epoxy plastic sealing material on both sides of the chip, changing the thickness ratio of the plastic sealing layer on the front and back of the chip, reducing the stress caused by different thicknesses, and using metal columns, metal interconnection lines and convex structures to improve warpage. The specific process includes A protective layer is made, a metal column and a plastic seal layer are arranged, and a convex structure is arranged on the upper metal interconnection line through electroplating or ball planting process.
The wafer warpage is effectively reduced. By adjusting the thickness ratio of the plastic seal layer, the stress caused by different thicknesses of epoxy plastic seals is reduced, and the warpage problem of fanout packaging is significantly improved. The method is simple and the effect is obvious.
Smart Images

Figure CN114188290B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor packaging, and in particular to a fan-out packaging structure capable of reducing warping. Background Art
[0002] As the integration of electronic devices becomes higher and higher, electronic products are developing in the direction of lightness and miniaturization, and IC chip packaging is also tending to be thinner and smaller, which places higher and higher requirements on packaging technology. With the continuous advancement of wafer-level fan-out packaging technology, the proportion of fan-out wafer-level packaging in electronic products has increased year by year, and has gradually become the mainstream direction of the development of advanced packaging technology. Fan-out wafer-level packaging is an embedded packaging processed at the wafer level. Fan-out wafer-level packaging technology generally uses a single microchip cut from the wafer and then embedded in a new "artificial" wafer. At present, fan-out packaging using plastic packaging technology is very difficult in terms of wafer warpage control.
[0003] The characteristic of fan-out wafer-level packaging is that the chip is encapsulated on three sides with epoxy molding compound (EMC) and the interconnection structure is manufactured on the pin surface of the chip. However, due to the large difference in thermal expansion coefficients between EMC and silicon materials and the fact that the EMC material is mainly on one side of the chip, the fan-out wafer will warp after encapsulation. At present, fan-out packaging using the encapsulation process is very difficult to control wafer warpage.
[0004] A new design idea and solution are needed to solve the wafer warpage problem of existing fan-out packaging. Summary of the invention
[0005] Based on the prior art, the task of the present invention is to provide a fan-out packaging structure that reduces warpage. By changing the thickness of the epoxy molding compound (EMC) on both sides of the chip, the stress caused by the different thickness of the EMC on the front and back of the chip is reduced, thereby improving the wafer warpage.
[0006] In a first aspect of the present invention, in view of the problems existing in the prior art, the present invention provides a fan-out packaging structure with reduced warpage, comprising:
[0007] a chip having a front side and a back side opposite to the front side;
[0008] A pin, which is on the front side of the chip;
[0009] A metal column, which is arranged on the pin and electrically interconnected with the pin;
[0010] A plastic encapsulation layer, which wraps the chip and the metal pillar, wherein the thickness of the plastic encapsulation layer on the front side of the chip is determined by the height of the metal pillar;
[0011] A metal interconnection line, which is arranged on the metal pillar and electrically interconnected with the metal pillar; and
[0012] A bump structure is electrically interconnected with the metal interconnection line.
[0013] In a preferred embodiment of the present invention, it is provided that the present invention further comprises:
[0014] A protective layer covering the front side of the chip, the protective layer being used for the pins;
[0015] An insulating layer wraps the metal interconnection line.
[0016] In another preferred embodiment of the present invention, it is provided that the metal interconnection line comprises a lower metal interconnection line and an upper metal interconnection line;
[0017] The lower metal interconnection line is located above the plastic packaging layer and is electrically interconnected with the metal pillar;
[0018] The upper metal interconnection line is located above the lower metal interconnection line and is electrically interconnected with the lower metal interconnection line.
[0019] In another preferred embodiment of the present invention, it is stipulated that the chip is a central processing unit, a graphics processing unit, a memory array or an image sensor.
[0020] In another preferred embodiment of the present invention, it is provided that the stress generated on the front and back sides of the chip due to the different thicknesses of the plastic encapsulation layers is reduced by adjusting the thickness ratio of the plastic encapsulation layers on the front and back sides of the chip.
[0021] In another preferred embodiment of the present invention, it is provided that the thickness of the plastic encapsulation layer on the front and back sides of the chip is determined and / or adjusted according to the calculation formula of the warpage D of the fan-out package:
[0022] D=A×(1+2x+x 2 ) / (4+6x+4x 2 +x 3 y+1 / xy),
[0023] Where A is a constant, x is the ratio of chip thickness to plastic layer thickness, and y is the ratio of Young's modulus of silicon and plastic layer materials.
[0024] In another preferred embodiment of the present invention, it is provided that x=(T1-T2) / Tsi
[0025] Where T1 is the thickness of the plastic layer on the back of the chip, T2 is the thickness of the plastic layer on the front of the chip, and Tsi is the thickness of the chip.
[0026] In another preferred embodiment of the present invention, it is provided that the bump structure is arranged on the upper metal interconnection line by electroplating or ball planting process, and is electrically interconnected with the upper metal interconnection line.
[0027] In a second aspect of the present invention, in view of the problems existing in the prior art, the present invention provides a method for manufacturing a fan-out packaging structure with reduced warpage, comprising:
[0028] Making a protective layer on the front side of the chip;
[0029] Arrange metal posts on the pins;
[0030] Making a plastic encapsulation layer to encapsulate the chip and metal pillars;
[0031] Manufacturing lower metal interconnection lines and upper metal interconnection lines;
[0032] forming an insulating layer wrapping the lower metal interconnection line and the upper metal interconnection line; and
[0033] The bump structure is arranged on the upper metal interconnection line through electroplating or ball planting process.
[0034] In a preferred embodiment of the present invention, when making lower metal interconnects and upper metal interconnects, a seed layer is first deposited, the seed layer is made of Ti, Cu or Al, then the circuits are photolithographically formed, and then Ti, Cu or Al is deposited to form metal interconnects.
[0035] The present invention has at least the following beneficial effects: The present invention proposes a fan-out packaging structure for reducing warpage, which reduces the stress on the front and back sides of the chip due to the different thicknesses of the epoxy molding compound by changing the thickness of the epoxy molding compound on both sides of the chip, thereby effectively improving the wafer warpage, and the method is simple and the effect is obvious. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to further illustrate the above and other advantages and features of various embodiments of the present invention, a more specific description of various embodiments of the present invention will be presented with reference to the accompanying drawings. It will be understood that these drawings only depict typical embodiments of the present invention and are therefore not to be considered as limiting the scope thereof. In the accompanying drawings, for clarity, identical or corresponding parts will be represented by identical or similar reference numerals.
[0037] Figure 1 A schematic diagram of the calculation principle of wafer warpage of a fan-out package according to the present invention is shown.
[0038] Figure 2 A schematic diagram of a fan-out packaging structure with reduced warpage according to an embodiment of the present invention is shown.
[0039] FIG. 3A to FIG. 3E A schematic cross-sectional view of a process for manufacturing a fan-out package structure 100 with reduced warpage according to an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0040] It should be noted that the components in the figures may be shown exaggeratedly for the sake of illustration and are not necessarily true to scale. In the figures, identical or functionally identical components are provided with the same reference numerals.
[0041] In the present invention, each embodiment is only intended to illustrate the aspects of the present invention and should not be construed as limiting.
[0042] In the present invention, unless otherwise specified, the quantifiers "a", "an" and "an" do not exclude the presence of a plurality of elements.
[0043] It should also be pointed out that in the embodiments of the present invention, for the sake of clarity and simplicity, only a portion of the parts or components may be shown, but a person of ordinary skill in the art will understand that under the teachings of the present invention, required parts or components may be added as needed in specific scenarios.
[0044] It should also be pointed out that within the scope of the present invention, the terms "same", "equal", "equal to" and the like do not mean that the two values are absolutely equal, but allow a certain reasonable error, that is, the terms also cover "substantially the same", "substantially equal", and "substantially equal to".
[0045] It should also be pointed out that in the description of the present invention, the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than explicitly or implicitly indicating that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as explicitly or implicitly indicating relative importance.
[0046] In addition, the embodiments of the present invention describe the process steps in a specific order, but this is only for the convenience of distinguishing the steps, and does not limit the sequence of the steps. In different embodiments of the present invention, the sequence of the steps can be adjusted according to the adjustment of the process.
[0047] An embodiment of the present invention proposes a fan-out packaging structure that reduces warpage, and reduces stress caused by different thicknesses on the front and back sides of the chip by changing the thickness of epoxy molding compound on both sides of the chip, thereby effectively improving wafer warpage.
[0048] Figure 1 FIG. 2 shows a schematic diagram of the calculation principle of wafer warpage of a fan-out package according to the present invention. Figure 1As shown, T1 is the thickness of the EMC material on the back of the chip, T2 is the thickness of the EMC material on the front of the chip, and Tsi is the thickness of the chip. With the chip as the interface, the EMC material distributed on the front and back of the silicon chip will produce shrinkage forces in opposite directions on the silicon chip during the high-temperature baking process. Therefore, when the package thickness is required to be certain, the effective MEC thickness that actually causes warping is T1-T2. By changing the values of T1 and T2 and adjusting the thickness ratio of the EMC material on the front and back of the chip, the warping can be improved. Based on the above principle, the inventor first sets the chip thickness Tsi to the effective EMC thickness ratio as x=(T1-T2) / Tsi.
[0049] Then, there is a corresponding relationship between the warpage D and the chip thickness Tsi and the EMC effective thickness T1-T2 ratio x. By adjusting the EMC thickness on the front and back of the chip to change the x value, the warpage of the fan-out package can be improved. The calculation formula for the warpage D of the fan-out package is:
[0050] D=A×(1+2x+x 2 ) / (4+6x+4x 2 +x 3 y+1 / xy),
[0051] Among them, the thermal expansion coefficient, length, total package thickness and curing temperature are constants under certain conditions, x is the ratio of chip thickness to EMC material thickness, and y is the ratio of Young's modulus of silicon and EMC material. Since the Young's modulus of silicon and EMC material is constant, y is a fixed value.
[0052] According to the above calculation formula of warpage D, by changing the values of T1 and T2, the thickness ratio of the EMC material on the front and back sides of the chip is adjusted to improve the warpage.
[0053] Figure 2 A schematic diagram of a fan-out packaging structure with reduced warpage according to an embodiment of the present invention is shown.
[0054] like Figure 2 As shown, a fan-out package structure 200 for reducing warpage includes a chip 210, a protective layer 220, a pin 230, a metal pillar 240, an EMC plastic layer 250, an interconnection structure layer 260 and a bump structure 270. The interconnection structure layer 260 includes an insulating layer 261, a lower metal interconnection line 262 and an upper metal interconnection line 263.
[0055] The chip 210 may be a central processing unit, a graphics processing unit, a memory array, an image sensor, or other devices.
[0056] The pin 230 is located on the front side of the chip 210. In one embodiment of the present invention, the pin 230 may be made of aluminum metal.
[0057] The protection layer 220 covers the front side of the chip 210 to protect the pins 230. In one embodiment of the present invention, the material of the protection layer 220 may include silicon oxide, silicon nitride, polyimide PI, etc.
[0058] The metal pillar 240 is disposed on the pin 230 and is electrically interconnected with the pin 230. In one embodiment of the present invention, the material of the metal pillar 240 may be a metal material such as Al, Cu, or W.
[0059] The EMC plastic layer 250 wraps the chip 210 and the metal pillar 240. The thickness of the EMC material on the back of the chip is T1, and the thickness of the EMC material on the front of the chip is T2. The EMC material on the front of the chip and the metal pillar 240 are in the same plane, so the EMC thickness T2 on the front is determined by the height of the metal pillar 240. By changing the height of the metal pillar 140, the thickness T2 can be changed, that is, the thickness of the EMC material on the front of the chip 210 can be adjusted. By changing the thickness of the EMC material on the front and back of the chip 210, the thickness ratio of the EMC material on the front and back of the chip is adjusted, and the stress generated by the different EMC thicknesses on the front and back of the chip is reduced, thereby achieving the purpose of improving the wafer warpage. The values of T1 and T2 are set and / or adjusted by the warpage D of the fan-out package mentioned above.
[0060] The interconnection structure layer 260 includes 261, a lower metal interconnection line 262 and an upper metal interconnection line 263. The lower metal interconnection line 262 is located above the EMC plastic packaging layer 250 and is electrically interconnected with the metal pillar 240. The upper metal interconnection line 263 is located above the lower metal interconnection line 262 and is electrically interconnected with the lower metal interconnection line 262. The insulating layer 261 wraps the lower metal interconnection line 262 and the upper metal interconnection line 263. The material of the insulating layer 261 can be an oxide layer, polyimide PI, phenylbenzobisoxazole resin PBO or resin organic matter. The material of the lower metal interconnection line 262 and the upper metal interconnection line 263 is a metal such as Al, Cu, and Ti.
[0061] The bump structure 270 is arranged on the upper metal interconnection line 263 by electroplating or ball planting process, and is electrically interconnected with the upper metal interconnection line 263.
[0062] FIG. 3A to FIG. 3E A schematic cross-sectional view of a process for manufacturing a fan-out package structure 100 with reduced warpage according to an embodiment of the present invention is shown.
[0063] In step 1, if Figure 3A As shown, a protection layer 320 is formed on the front side of the chip 310 . The main materials of the protection layer 320 include silicon oxide, silicon nitride, polyimide PI, etc., and the manufacturing method includes spraying, vapor deposition, etc. The protection layer 320 is used to protect the pins 330 .
[0064] In step 2, if Figure 3B As shown, a metal column 340 is arranged on the pin 330. The metal column 340 is arranged on the pin 330 by electroplating or welding. The material of the metal column 340 can be a metal material such as Al, Cu, W, etc.
[0065] In step 3, if Figure 3C As shown, an EMC plastic layer 350 is made to wrap the chip 310 and the metal pillar 340 to form a plastic package. The thickness of the EMC material on the back of the chip is T1, and the thickness of the EMC material on the front of the chip is T2. The EMC material on the front of the chip is in the same plane as the metal pillar 240. The values of T1 and T2 are set and / or adjusted by the warpage D of the fan-out package mentioned above.
[0066] In step 4, if Figure 3D As shown, the lower metal interconnection line 362 and the upper metal interconnection line 363 are manufactured. When manufacturing the lower metal interconnection line 362 and the upper metal interconnection line 363, a seed layer is first deposited, the seed layer uses Ti, Cu or Al, then the line is photolithographically formed, and then Ti, Cu or Al is deposited to form the lower metal interconnection line.
[0067] In step 5, if Figure 3D As shown, an insulating layer 361 is formed to wrap the lower metal interconnection line 362 and the upper metal interconnection line 363. The material of the insulating layer 361 can be an oxide layer, polyimide PI, phenylbenzobisoxazole resin PBO or resin organic matter. The method for forming the insulating layer includes spraying, vapor deposition, etc.
[0068] In step 6, if Figure 3E As shown, a bump structure 370 is arranged on the upper metal interconnection line 363 by electroplating or ball planting process.
[0069] The present invention has at least the following beneficial effects: The present invention proposes a fan-out packaging structure for reducing warpage, which reduces the stress on the front and back sides of the chip due to the different thicknesses of the epoxy molding compound by changing the thickness of the epoxy molding compound on both sides of the chip, thereby effectively improving the wafer warpage, and the method is simple and the effect is obvious.
[0070] Although some embodiments of the present invention have been described in this application document, it will be appreciated by those skilled in the art that these embodiments are merely shown as examples. Those skilled in the art may conceive of numerous variations, alternatives, and improvements under the teachings of the present invention without departing from the scope of the present invention. The appended claims are intended to define the scope of the present invention and thereby cover methods and structures within the scope of these claims themselves and their equivalents.
Claims
1. A fan-out packaging structure with reduced warpage, include: a chip having a front side and a back side opposite to the front side; A pin, which is on the front side of the chip; A metal column, which is arranged on the pin and electrically interconnected with the pin; A plastic encapsulation layer, which wraps the chip and the metal pillar, wherein the thickness of the plastic encapsulation layer on the front side of the chip is determined by the height of the metal pillar; A metal interconnection line, which is arranged on the metal pillar and electrically interconnected with the metal pillar; as well as a bump structure electrically interconnected with the metal interconnection line; By adjusting the thickness ratio of the plastic sealing layer on the front side and the back side of the chip, the stress generated by the different thickness of the plastic sealing layer on the front side and the back side of the chip can be reduced; The thickness of the plastic encapsulation layer on the front and back sides of the chip is determined and / or adjusted according to the calculation formula of the warpage D of the fan-out package: D=A×(1+2x+x 2 ) / (4+6x+4x 2 +x 3 y+1 / xy), Where A is a constant, x is the ratio of chip thickness to plastic layer thickness, and y is the ratio of Young's modulus of silicon and plastic layer materials; x=(T 1 -T 2 ) / Tsi Where T 1 is the thickness of the plastic layer on the back of the chip, T 2 is the thickness of the plastic layer on the front of the chip, and Tsi is the thickness of the chip.
2. The fan-out packaging structure with reduced warpage as claimed in claim 1, It is characterized in that Also includes: A protective layer covering the front side of the chip, the protective layer being used for the pins; An insulating layer wraps the metal interconnection line.
3. The fan-out packaging structure with reduced warpage as claimed in claim 1, It is characterized in that The metal interconnection line includes a lower metal interconnection line and an upper metal interconnection line; The lower metal interconnection line is located above the plastic packaging layer and is electrically interconnected with the metal pillar; The upper metal interconnection line is located above the lower metal interconnection line and is electrically interconnected with the lower metal interconnection line.
4. The fan-out packaging structure with reduced warpage as claimed in claim 1, It is characterized in that The chip is a central processing unit, a graphics processing unit, a memory array or an image sensor.
5. The fan-out packaging structure with reduced warpage as claimed in claim 3, It is characterized in that The bump structure is arranged on the upper metal interconnection line through electroplating or ball planting process, and is electrically interconnected with the upper metal interconnection line.
6. A method for manufacturing a fan-out packaging structure with reduced warpage, include: Making a protective layer on the front side of the chip; Arrange metal posts on the pins; Making a plastic encapsulation layer to encapsulate the chip and metal pillars; Manufacturing lower metal interconnection lines and upper metal interconnection lines; Making an insulating layer covering the lower metal interconnection line and the upper metal interconnection line; as well as Arranging a bump structure on the upper metal interconnection line by electroplating or ball planting process; By adjusting the thickness ratio of the plastic sealing layer on the front side and the back side of the chip, the stress generated by the different thickness of the plastic sealing layer on the front side and the back side of the chip can be reduced; The thickness of the plastic encapsulation layer on the front and back sides of the chip is determined and / or adjusted according to the calculation formula of the warpage D of the fan-out package: D=A×(1+2x+x 2 ) / (4+6x+4x 2 +x 3 y+1 / xy), Where A is a constant, x is the ratio of chip thickness to plastic layer thickness, and y is the ratio of Young's modulus of silicon and plastic layer materials; x=(T 1 -T 2 ) / Tsi Where T 1 is the thickness of the plastic layer on the back of the chip, T 2 is the thickness of the plastic layer on the front of the chip, and Tsi is the thickness of the chip.
7. The method for manufacturing a fan-out package structure with reduced warpage according to claim 6, It is characterized in that When making lower-layer metal interconnects and upper-layer metal interconnects, a seed layer is first deposited, the seed layer uses Ti, Cu or Al, then the circuit is photolithographically patterned, and then Ti, Cu or Al is deposited to form metal interconnects.