A semiconductor structure and a method for manufacturing the same
By forming an insulating channel with a narrow top and a wide cross-section in the semiconductor structure, the leakage problem in the shallow channel isolation structure is solved, the active area area and landing area are increased, and better insulation and application range are achieved, which is suitable for Industrial production.
Patent Information
- Application Number
- CN202011051597.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-09-29
AI Technical Summary
The shallow trench isolation structure in existing semiconductor manufacturing has leakage problems, and as the integration level increases, the active area area and landing area are smaller, which is not conducive to storage node contact or other device electrical contact.
A semiconductor structure manufacturing method is used to form a first trench by etching on the substrate, filling it with an oxide layer, and then etching the sidewalls of the oxide layer to form a second trench to form a supplementary layer and increase the density of the active area. area and landing area. The method includes protective layer treatment before and after etching to form the first trench, and ion implantation to optimize the structure when forming the supplementary layer.
It significantly improves the STI insulation, reduces the resistance, increases the area of the active area and landing area, and improves the electrical contact performance of storage nodes or other devices. It has a wide range of applications and is suitable for industrial mass production.
Smart Images

Figure CN114334790B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor structures, and in particular to a semiconductor structure and a manufacturing method thereof. Background Art
[0002] Semiconductor memory chips generally have an array area and a peripheral area; a memory cell array is formed in the array area; and the peripheral area includes peripheral area devices. At present, the mainstream shallow trench isolation (STI) structure in semiconductor manufacturing generally includes a number of U-shaped trenches arranged in sequence and an active area (AA) defined by the trenches. In this STI structure, the cross-section of the trench is theoretically the same from top to bottom, and the corresponding cross-section of the AA is also theoretically the same from top to bottom. Subsequently, the buried word line (BWL) is etched as needed, and then connected to generate the bit line (BL) through the bit line contact plug (BLC). With the improvement of the integration of semiconductor devices, the size of AA and STI is getting smaller and smaller, and this existing STI structure often has leakage problems. Summary of the invention
[0003] In order to overcome the shortcomings of the prior art, the present invention provides a method for manufacturing a semiconductor structure, forming an insulating channel with a narrow upper and wide lower cross-section. The deeper and wider STI bottom can significantly improve the STI insulation, better solve the leakage problem, form a supplementary layer of AA, increase the area of AA, reduce the resistance and increase the landing area of the active area, which is beneficial to the landing of subsequent storage node contact (Storage Node Contact, SNC) or other device electrical contact, and has the advantages of simple operation and easy industrial large-scale production.
[0004] A method for manufacturing a semiconductor structure, comprising:
[0005] Providing a substrate, and etching a first trench on the substrate;
[0006] Filling an oxide layer in the first trench, wherein a top surface of the oxide layer is not lower than a top surface of the substrate;
[0007] Etching downwardly a region of the oxide layer adjacent to the sidewall of the first trench to form a second trench, wherein the depth of the second trench is less than the depth of the first trench, and the width of the second trench is less than half of the width of the first trench;
[0008] A supplementary layer is formed in the second trench.
[0009] Optionally, the depth of the first groove is 300nm-400nm, and the depth of the second groove is 150nm-200nm.
[0010] Optionally, the oxide layer may be made of oxides commonly used in the art, such as silicon dioxide.
[0011] Optionally, the supplementary layer includes single crystal silicon epitaxially grown directly from the substrate or deposited doped polysilicon.
[0012] Optionally, the substrate is a conventional substrate in the art, such as a silicon substrate or a silicon germanium substrate.
[0013] Optionally, the substrate includes an array region and a peripheral region.
[0014] Optionally, the first groove is formed in the array region, the width of the first groove is 20 nm to 40 nm, and the width of the second groove is 5 nm to 15 nm.
[0015] Optionally, the first trench is formed in the peripheral region, the width of the first trench is 70 nm to 110 nm, and the width of the second trench is 30 nm to 50 nm.
[0016] Optionally, the method for manufacturing the semiconductor structure further includes: forming a protection layer on the substrate before etching to form the first trench;
[0017] When etching to form the first groove, the protective layer and the substrate are etched together so that the first groove passes through the protective layer. The protective layer can not only protect the top surface of the substrate, but also promote the growth of the supplementary layer only on the side wall of the second groove, but not on the top surface of the substrate, when epitaxially growing the supplementary layer.
[0018] Optionally, the method for manufacturing the semiconductor structure further includes: performing a first ion implantation on the substrate after forming the oxide layer and before forming the second trench.
[0019] Optionally, the method for manufacturing the semiconductor structure further includes: after forming the supplementary layer, performing a second ion implantation on the substrate, wherein the ion doping type of the second ion implantation is opposite to that of the first ion implantation.
[0020] Optionally, the supplementary layer is formed by epitaxially growing the sidewall of the second trench close to the substrate; and while the second ion implantation is performed on the substrate, the second ion implantation is also performed on the supplementary layer.
[0021] Optionally, the supplementary layer is a deposited doped polysilicon layer, and the doping type of the doped polysilicon layer is consistent with the ion doping type of the second ion implantation.
[0022] The ion type of the ion implantation is selected from the ion type commonly used in the art, such as group III (N-type) element ions or group V (P-type) element ions; group III (N-type) element ions and group V (P-type) element ions are mutually counter-type ions. The ion doping type of the second ion implantation is opposite to that of the first ion implantation, and mutually counter-type ions can be selected as needed.
[0023] Optionally, the method for manufacturing the semiconductor structure further includes: forming a third trench in the array region after forming the supplementary layer;
[0024] forming a word line structure in the third trench;
[0025] Wherein, the depth of the third groove is less than or equal to the depth of the second groove.
[0026] A semiconductor structure is manufactured by adopting the manufacturing method of the semiconductor structure.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] The manufacturing method of the semiconductor structure of the present invention forms an insulating channel with a narrow upper section and a wide lower section. The deeper and wider STI bottom can significantly improve the STI insulation, better solve the leakage problem, form a supplementary layer of AA, increase the area of AA, reduce the resistance value and increase the landing area of the active area, which is beneficial to the landing of subsequent storage node contacts or other device electrical contacts.
[0029] The manufacturing method of the semiconductor structure of the present invention has the advantages of simple operation and easy industrial large-scale production.
[0030] The semiconductor structure of the present invention is not only applicable to the array area of a dynamic random access memory (DRAM), but also applicable to the peripheral area of the DRAM.
[0031] The manufacturing method of the semiconductor structure of the present invention is applicable to extreme ultraviolet lithography (EUV) or pitch doubling technology, and has a wide range of applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] The specific features of the invention involved in this application are shown in the attached claims. The features and advantages of the invention involved in this application can be better understood by referring to the exemplary embodiments and drawings described in detail below. The drawings are briefly described as follows:
[0033] Figure 1a An example of forming a first trench in the method for manufacturing a semiconductor structure of the present invention;
[0034] Figure 1b for Figure 1a Middle AA section view;
[0035] Figure 1c for Figure 1a Middle BB cross section;
[0036] Figure 2a This is an example of forming an oxide layer in the method for manufacturing a semiconductor structure of the present invention;
[0037] Figure 2b for Figure 2a Middle AA section view;
[0038] Figure 2c for Figure 2a Middle BB cross section;
[0039] Figure 3a An example of forming a second trench in the method for manufacturing a semiconductor structure of the present invention;
[0040] Figure 3b for Figure 4a Middle AA section view;
[0041] Figure 3c for Figure 4a Middle BB cross section;
[0042] Figure 4a An example of forming a supplementary layer in the method for manufacturing a semiconductor structure of the present invention;
[0043] Figure 4b for Figure 4a Middle AA section view;
[0044] Figure 4c for Figure 4a Middle BB cross section;
[0045] Figure 5a An example of forming a third trench and a word line structure in a method for manufacturing a semiconductor structure of the present invention;
[0046] Figure 5b for Figure 5a Middle AA section view;
[0047] Figure 5c for Figure 5a Middle BB cross section;
[0048] Figure 6 is an example of the semiconductor structure of the present invention; Figure 5c for Figure 6 Middle local CC cross section;
[0049] In the figure: substrate 1, first trench 2, active area 3, supplementary layer 4, second trench 5, oxide layer 6, third trench 7, word line structure 8. DETAILED DESCRIPTION
[0050] The following is an explanation of the implementation of the present application by means of specific embodiments. Those skilled in the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification.
[0051] In order to make the purpose, technical features and beneficial effects of the present invention more obvious and understandable, the specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings. The described embodiments are only part of the embodiments of the present invention, not all of them, and should not be understood as being limited to the embodiments described herein; on the contrary, these embodiments are provided so that the present invention will be comprehensive and complete, and the concept of the example embodiments will be fully conveyed to those skilled in the art. When describing the embodiments of the present invention in detail, for ease of explanation, the schematic diagrams are only examples, which should not limit the scope of protection of the present invention here; in actual production, the three-dimensional dimensions of length, width and depth should be included. The same figure marks in the figures represent the same or similar structures, and their detailed descriptions will be omitted.
[0052] The terms "a", "an", "the" and "said" are used to indicate the presence of one or more elements / components / etc.; the terms "including" and "having" are used to indicate an open-ended inclusive meaning and mean that there may be additional elements / components / etc. in addition to the listed elements / components / etc. The terms "first" and "second" are used only as labels and are not intended to limit the quantity of their objects.
[0053] There are many leakage problems in the existing semiconductor structures. The existing shallow trench isolation region structure causes the area of the active region to be relatively small, and the area of the active region landing area is also relatively small, which is not conducive to the subsequent landing of storage node contacts or other device electrical contacts. For example, the existing semiconductor structure generally includes a shallow trench isolation region composed of a number of sequentially arranged U-shaped trenches and an active region defined by the shallow trench isolation region. In this shallow trench isolation structure, the cross-section of the trench is theoretically the same width from top to bottom, and the cross-section of the corresponding active region is also theoretically the same width from top to bottom. As the integration of semiconductor devices becomes higher and higher, this existing semiconductor structure often has leakage problems, and the area of the active region is relatively small, and the area of the active region landing area is also relatively small, which is not conducive to the subsequent landing of storage node contacts or other device electrical contacts.
[0054] The existing semiconductor structure manufacturing method is usually applicable to a small range. For example, according to different manufacturing precisions, the semiconductor structure manufacturing method is usually only applicable to extreme ultraviolet lithography technology or only applicable to one technology such as pitch multiplication technology. It is necessary to equip corresponding equipment according to different manufacturing precisions, which increases the cost of enterprises and greatly limits industrial production. If a semiconductor structure manufacturing method with a wide range of applications can be developed, it will have a beneficial application effect.
[0055] The present invention discloses a method for manufacturing a semiconductor structure. By improving the existing manufacturing method, the insulation of STI is significantly improved, the leakage problem is better solved, a supplementary layer of AA is formed, the area of AA is increased, the resistance value is reduced and the landing area of the active area is increased, which is beneficial to the landing of subsequent storage node contacts or other device electrical contacts.
[0056] See also Figure 1a , Figure 1b and Figure 1c , which is an example of forming the first trench 2 in the method for manufacturing the semiconductor structure of the present invention. Figure 1a , Figure 1b and Figure 1c As shown, including:
[0057] A substrate 1 is provided, and a first trench 2 is formed by etching on the substrate 1 .
[0058] The substrate 1 is a conventional substrate 1 in the art, such as a silicon substrate or a silicon germanium substrate.
[0059] The first groove 2 may be formed by etching. In a specific implementation, exposure and development (PHOTO) may be used to define the etching area, and then etching (ETCH) may be used to etch the oxide layer to a required depth.
[0060] See also Figure 2a , Figure 2b and Figure 2c , which is an example of forming an oxide layer 6 in the method for manufacturing a semiconductor structure of the present invention. Figure 2a , Figure 2b and Figure 2c As shown, including:
[0061] A complete oxide layer 6 is filled in the first trench 2 , and the oxide layer is ground to adjust the surface flatness so that the top surface of the oxide layer 6 is not lower than the top surface of the substrate 1 .
[0062] The oxide layer 6 may be made of oxides commonly used in the art, such as silicon dioxide.
[0063] See also Figure 3a , Figure 3b and Figure 3c, which is an example of forming the second trench 5 in the method for manufacturing the semiconductor structure of the present invention. Figure 3a , Figure 3b and Figure 3c As shown, including:
[0064] The area of the oxide layer 6 adjacent to the side wall of the first trench 1 is etched downward to form a second trench 5 , wherein the depth of the second trench 5 is less than the depth of the first trench 2 , and the width of the second trench 5 is less than half of the width of the first trench 2 .
[0065] The depth of the first groove 2 is 300 nm to 400 nm, and the depth of the second groove 5 is 150 nm to 200 nm.
[0066] The substrate 1 includes an array region and a peripheral region. The array region includes an active region 3 and a shallow trench isolation region.
[0067] When the first trench 2 is formed in the array region, the width of the first trench 2 is 20 nm to 40 nm, and the width of the second trench 5 is 5 nm to 15 nm.
[0068] When the first trench 2 is formed in the peripheral region, the width of the first trench 2 is 70 nm to 110 nm, and the width of the second trench 5 is 30 nm to 50 nm.
[0069] The second groove 5 may be formed by etching. In a specific implementation, photolithography (PH) may be used to define the etching area, and then etching (ETCH) may be used to etch OX to a desired depth.
[0070] The etching of the second trench 5 can be defined according to the depth of the word line (Word Line, WL for short) structure in the subsequent specific application, and the critical dimension (CD, usually refers to the strip width) is etched twice.
[0071] See also Figure 4a , Figure 4b and Figure 4c , which is an example of forming the supplementary layer 4 in the method for manufacturing the semiconductor structure of the present invention. Figure 4a , Figure 4b and Figure 4c As shown, including:
[0072] A supplementary layer 4 is formed in the second trench 5 .
[0073] The supplementary layer 4 comprises single crystal silicon epitaxially grown directly from the substrate 1 or deposited doped polysilicon.
[0074] The method for manufacturing the semiconductor structure further includes: forming a protective layer on the substrate 1 before etching to form the first trench 2;
[0075] In one implementation, the protective layer and the substrate 1 are etched together when the first trench 2 is etched, so that the first trench 2 penetrates the protective layer. The protective layer can not only protect the top surface of the substrate 1, but also promote the growth of the supplementary layer 4 only on the side wall of the second trench 5, but not on the top surface of the substrate 1, when the supplementary layer 4 is epitaxially grown.
[0076] In one implementation, the method for manufacturing the semiconductor structure further includes: performing a first ion implantation on the substrate 1 after forming the oxide layer 6 and before forming the second trench 5 .
[0077] In one implementation, the method for manufacturing the semiconductor structure further includes: after forming the supplementary layer 4, performing a second ion implantation on the substrate 1, wherein the ion doping type of the second ion implantation is opposite to that of the first ion implantation.
[0078] In one implementation, the supplementary layer 4 is formed by epitaxially growing the sidewall of the second trench 5 close to the substrate; and while the second ion implantation is performed on the substrate 1, the second ion implantation is also performed on the supplementary layer 4.
[0079] The supplementary layer 4 is a deposited doped polysilicon layer, and the doping type of the doped polysilicon layer is consistent with the ion doping type of the second ion implantation.
[0080] The ion type of the ion implantation is selected from the ion type commonly used in the art, such as group III (N-type) element ions or group V (P-type) element ions; group III (N-type) element ions and group V (P-type) element ions are mutually counter-type ions. The ion doping type of the second ion implantation is opposite to that of the first ion implantation, and mutually counter-type ions can be selected as needed.
[0081] In one implementation, reverse ion implantation (opposite to the ion implantation type in the AA region 3) is performed around the STI, which can increase the isolation effect of the STI and better prevent leakage. A further implementation is: reverse doping ion implantation is performed around the wider area at the bottom of the STI, which can better prevent leakage between the AA regions through the bottom of the STI. If the ion doping type of the AA region is N-type, the ion doping type around the STI is P-type, and the ion implantation can further increase the isolation effect of the STI to prevent leakage.
[0082] See also Figure 5a , Figure 5b and Figure 5c , which is an example of forming the third trench 7 and the word line structure 8 in the method for manufacturing the semiconductor structure of the present invention. Figure 5a , Figure 5b and Figure 5cAs shown, including:
[0083] After forming the supplementary layer 4, forming a third trench 7 in the array region;
[0084] The depth of the third groove 7 is less than or equal to the depth of the second groove 5 .
[0085] forming a word line structure 8 in the third trench 7;
[0086] The formation of the word line structure 8 includes sequentially forming a gate dielectric layer, a metal electrode layer, a metal barrier layer and an insulating cap layer, wherein the insulating cap layer covers the metal electrode layer and the metal barrier layer, and the top of the insulating cap layer is flush with the upper surface of the substrate.
[0087] In the manufacturing method of the present invention, etching, filling, grinding and growth are preferably carried out by conventional techniques in the art, and are suitable for industrial production. For example, etching can be carried out by exposure and development to define the etching area, and then etching to the required depth by etching technology, or one of the existing technologies such as spacing multiplication technology and extreme ultraviolet lithography technology can be used. Filling can be carried out by chemical vapor deposition (CVD) technology and thermal oxidation growth or in-situ water vapor growth oxide layer technology, or other general film deposition technology. Grinding can be carried out by chemical mechanical polishing (CMP); growing crystals can be carried out by silicon epitaxial growth technology or polysilicon deposition technology.
[0088] See also Figure 6 , which is shown as an example of the semiconductor structure array region of the present invention; Figure 5c for Figure 6 Partial CC cross-section view.
[0089] The manufacturing method of the semiconductor structure of the present invention forms an insulating channel with a narrow upper section and a wide lower section. The deeper and wider STI bottom can significantly improve the STI insulation, better solve the leakage problem, form a supplementary layer of AA, increase the area of AA, reduce the resistance value and increase the landing area of the active area, which is beneficial to the landing of subsequent storage node contacts or other device electrical contacts.
[0090] The manufacturing method of the semiconductor structure of the present invention has the advantages of simple operation and easy industrial large-scale production.
[0091] The semiconductor structure of the present invention is not only applicable to the array area of a dynamic random access memory (DRAM), but also applicable to the peripheral area of the DRAM.
[0092] The manufacturing method of the semiconductor structure of the present invention is applicable to extreme ultraviolet lithography (EUV) or pitch doubling technology, and has a wide range of applications.
Claims
1. A method for manufacturing a semiconductor structure, characterized in that: include: Providing a substrate, and etching a first trench on the substrate; Filling an oxide layer in the first trench, wherein a top surface of the oxide layer is not lower than a top surface of the substrate; Etching downwardly a region of the oxide layer adjacent to the sidewall of the first trench to form a second trench, wherein the depth of the second trench is less than the depth of the first trench, and the width of the second trench is less than half of the width of the first trench; forming a supplementary layer in the second trench; Wherein, after forming the oxide layer and before forming the second trench, a first ion implantation is performed on the substrate.
2. The manufacturing method according to claim 1, characterized in that: The depth of the first groove is 300nm-400nm, and the depth of the second groove is 150nm-200nm.
3. The manufacturing method according to claim 1, characterized in that: The substrate includes an array region and a peripheral region.
4. The manufacturing method according to claim 3, characterized in that: The first groove is formed in the array region, the width of the first groove is 20nm-40nm, and the width of the second groove is 5nm-15nm.
5. The manufacturing method according to claim 3, characterized in that: The first trench is formed in the peripheral region, the width of the first trench is 70nm-110nm, and the width of the second trench is 30nm-50nm.
6. The manufacturing method according to claim 1, characterized in that: Also includes: Before etching to form the first groove, forming a protection layer on the substrate; When the first trench is formed by etching, the protection layer and the substrate are etched together so that the first trench penetrates the protection layer.
7. The manufacturing method according to claim 1, characterized in that: Also includes: After forming the supplementary layer, a second ion implantation is performed on the substrate, wherein the ion doping type of the second ion implantation is opposite to that of the first ion implantation.
8. The manufacturing method according to claim 7, characterized in that: The supplementary layer is formed by epitaxially growing the side wall of the second trench close to the substrate; while the second ion implantation is performed on the substrate, the second ion implantation is also performed on the supplementary layer.
9. The manufacturing method according to claim 7, characterized in that: The supplementary layer is a deposited doped polysilicon layer, and the doping type of the doped polysilicon layer is consistent with the ion doping type of the second ion implantation.
10. The manufacturing method according to claim 4, characterized in that: Also includes: After forming the supplementary layer, forming a third trench in the array region; forming a word line structure in the third trench; Wherein, the depth of the third groove is less than or equal to the depth of the second groove.
11. A semiconductor structure, characterized in that: The method is manufactured by the manufacturing method according to any one of claims 1 to 10.
Citation Information
Patent Citations
Manufacturing method of semiconductor device shallow-trench isolation structure
CN104282612A
Semiconductor device structure and preparation method thereof
CN110880510A