Preparation and use method of an environmentally friendly coking inhibitor for styrene devices

The environmentally friendly tar retardant composed of amine compounds and hydroxybenzophenone solves the problems of large dosage, high toxicity and tar formation of DNBP in the existing technology, and achieves low dosage, non-toxic and non-polluting tar formation prevention effect. , extending the unit operation time and increasing the styrene yield.

CN114349592BActive Publication Date: 2024-10-15BEIJING SBL S&D CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210056430.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-18
Publication Date
2024-10-15
Estimated Expiration
2042-01-18

AI Technical Summary

Technical Problem

The retarder DNBP used in existing styrene plants has problems such as large dosage, high toxicity, and easy environmental pollution. Moreover, traditional retarder cannot effectively prevent the formation of tar, resulting in increased polymer content and high tar yield.

Method used

It is an environmentally friendly scorch retardant composed of amine compounds and hydroxybenzophenone. It prevents the generation of free radicals by chelating metal ions and resisting oxygen. It works synergistically to inhibit the polymerization of styrene. It has the characteristics of low dosage, non-toxic and non-polluting. .

Benefits of technology

It effectively extends the operating time of the styrene unit, reduces the tar yield, reduces environmental pollution and harm to the health of operators, increases the styrene yield, and reduces costs.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to the preparation and use of an environmentally friendly coke inhibitor for a styrene device. The coke inhibitor contains amine compounds and hydroxybenzophenones, which can effectively extend the operation time of the styrene device, improve the output and quality of styrene products, reduce the tar yield, and has a small amount of use and good effect, so that the production process of the styrene distillation device can obtain better economic benefits. At the same time, the coke inhibitor is non-toxic, does not cause any adverse effects on the subsequent product processing, is safe and environmentally friendly, and belongs to a green environmentally friendly product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a preparation method and a use method of an environment-friendly coking inhibitor for a styrene device. Background Art

[0002] Styrene is an important basic raw material in the petrochemical industry and has a wide range of uses. It is mainly used in the production of styrene resins and styrene-butadiene rubber. It can also be used in the production of benzene, dyes, pesticides, and mineral processing industries.

[0003] Styrene has the properties of vinyl olefins and is highly reactive. It can polymerize at room temperature to produce tar. The higher the temperature, the faster the polymerization rate and the more tar is produced. In order to reduce the polymerization loss and polymerization fouling of styrene monomer during the styrene distillation process and ensure the normal operation of the distillation system, inhibitors that prevent tar generation must be added during the distillation process.

[0004] In the 1970s and 1980s, nitrobenzene compound 2,4-dinitrophenol (DNP) was used as a styrene retarder at home and abroad. In the late 1980s, by introducing methyl and ethyl groups into the DNP structure to improve its solubility in styrene, 2,6-dinitro-p-cresol (DNPC) and 4,6-dinitro-2-sec-butylphenol (DNBP) began to be used in styrene units. However, these retarders cannot extend the polymerization induction period, but can only reduce the polymerization rate. As the heating time of styrene increases, the polymer content has been slowly increasing, and it is impossible to completely prevent the formation of polymers and achieve the purpose of reducing tar yield. Since the 1990s, true retarders have begun to be used in styrene units, such as phenols and hydroxylamine compounds. Although true retarders can extend the induction period of the polymerization reaction, they are consumed by the reaction of retarders with free radicals during the induction period, resulting in a shortened service life of the retarders. In recent years, most styrene plants at home and abroad have used a combination of retarders and true retarders. Through the synergistic effect of each component, the inhibition efficiency is high. However, there are still certain defects, that is, DNBP is difficult to add, the dosage is large, the toxicity is high, and it is easy to pollute the environment.

[0005] Pure DNBP must be diluted with ethylbenzene during use, and it is very easy to produce carcinogens under high temperature conditions, which not only increases the energy consumption of the device and reduces the yield of styrene, but also causes great harm to the health of on-site operators. In recent years, since the production of DNBP requires a large amount of concentrated sulfuric acid and concentrated nitric acid, a large amount of acidic wastewater will be generated in the washing and dehydration process during the production process, which is particularly polluting to the environment. Faced with the new situation where the country's environmental protection requirements are becoming increasingly stringent, manufacturers of DNBP have successively stopped production and reduced production, so it has become inevitable to produce new products to replace DNBP. Summary of the invention

[0006] The purpose of the present invention is to provide an environmentally friendly coke inhibitor for a styrene device and a method of using the same. The coke inhibitor can effectively prevent the generation of coke dirt and has a good effect of reducing the yield of tar. At the same time, the dosage is small, the cost is low, and the agent is non-toxic and pollution-free. Amine compounds and hydroxybenzophenone are used, and the traditional polluting retarder DNBP or DNPC is no longer used. The dosage is only two-thirds to one-half of the original DNBP dosage, thereby effectively extending the operating time of the styrene device, improving the styrene yield, reducing the yield of tar, reducing pollution to the environment, eliminating the impact on the health of operators, and enabling the production process of the styrene device to obtain better economic benefits.

[0007] The invention is an environmentally friendly anti-scorch agent for replacing DNBP, which is composed of active ingredients A component, B component and organic solvent, characterized in that the mass ratio of A component to B component is 0.1~10:1, preferably 0.5~1:1, wherein A component is an amine compound, which can be selected from N,N'-bis(1-ethyl-3-methylpentyl)-p-phenylenediamine and N,N'-dimethyl-N,N'-di(1-methylpropyl)-p-phenylenediamine; B component is a hydroxybenzophenone, which can be selected from 2,4-dihydroxybenzophenone and 2-hydroxy-4-methoxybenzophenone. The organic solvent is C5~C 10 The amount of hydrocarbons used is not strictly required, so that components A and B are completely dissolved, and the kinematic viscosity of the above-mentioned anti-scorch agent is maintained at ≤8mm at 30℃ 2 / s range is good.

[0008] The present invention also provides a method for using the environment-friendly coking inhibitor for a styrene device, wherein the environment-friendly coking inhibitor of the present invention is added to a crude styrene material in a distillation tower at a mass concentration of not less than 5 ppm.

[0009] The present invention is obtained on the basis of studying the causes of styrene polymerization and the polymerization mechanism of styrene. The study shows that the factors initiating styrene polymerization include oxygen, metal impurities, heat, etc., and the polymerization of styrene follows a free radical polymerization mechanism.

[0010] Styrene monomer will catalyze the generation of free radicals at higher temperatures or in contact with metals, and accelerate the polymerization process in two ways. If oxygen is present, free radicals react with monomers to generate peroxy radicals, and peroxy radicals will further react with monomers to generate more free radicals. This process will continue to generate more free radicals. Once free radicals are generated, polymerization will occur. The higher the concentration of free radicals, the faster the polymerization rate. The coke inhibitor of the present invention contains a metal passivation component that can chelate with metal ions to form a stable complex, inhibiting the generation of free radicals induced by metal ions; it also contains a clean dispersing component that can be adsorbed on the surface of fine polymers that have been formed in the upstream material to form a protective film to prevent the polymerization reaction from continuing; the antioxidant coke inhibitor contained in the coke inhibitor of the present invention is resistant to high temperatures, can not only capture peroxy radicals, but also can combine with alkyl radicals, thereby effectively inhibiting styrene polymerization. The most important thing is that the synergistic effect between the two types of components in the coke inhibitor of the present invention is obvious, it has good compatibility with the medium, small dosage, non-toxicity, no pollution, will not have any adverse effects on subsequent products, and the coke inhibitor of the present invention also has the advantage of low cost. DETAILED DESCRIPTION

[0011] Embodiment 1-10:

[0012] Under constant stirring, the commercially available 2# solvent (commercial number, the main component is C5~C 10 The component A and the component B shown in Table 1 are respectively added into the mixture of the hydrocarbons (including the hydrocarbons) and mixed evenly to obtain the novel environmentally friendly coking inhibitor for the styrene device of the present invention.

[0013] Table 1: Components and proportions of the scorch inhibitors of Examples 1 to 8 (data in the table are all in mass fractions)

[0014] Example Component A Component A Component B Component B Organic solvents N,N'-Bis(1-ethyl-3-methylpentyl)-p-phenylenediamine N,N'-Dimethyl-N,N'-di(1-methylpropyl)-p-phenylenediamine 2,4-Dihydroxybenzophenone 2-Hydroxy-4-methoxybenzophenone 2#Solvent 1 40 servings 20 servings 40 servings 2 35 servings 20 servings 45 servings 3 35 servings 25 servings 40 servings 4 30 servings 30 servings 40 servings 5 15 servings 10 servings 40 servings 35 servings 6 10 servings 10 servings 40 servings 40 servings 7 15 servings 25 servings 25 servings 35 servings 8 10 servings 20 servings 20 servings 50 servings

[0015] Embodiment 9:

[0016] The coke inhibitor of Example 1 was added at 600 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was measured according to GB / T509-88 standard and was 4.28 mg / gSM.

[0017] Embodiment 10:

[0018] The coke inhibitor of Example 2 was added at 250ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5Mpa, the tar content was measured according to GB / T509-88 standard and was 4.33mg / gSM.

[0019] Embodiment 11:

[0020] The coke inhibitor of Example 3 was added at 100 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation unit for the actual industrial preparation of styrene, with a mass composition of 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, and 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was determined in accordance with GB / T509-88 standard to be 4.36 mg / gSM.

[0021] Embodiment 12:

[0022] The coke inhibitor of Example 4 was added at 50 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was measured according to GB / T 509-88 standard and was 4.32 mg / gSM.

[0023] Embodiment 13:

[0024] The coke inhibitor of Example 5 was added at 50 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was measured according to GB / T 509-88 standard and was 4.30 mg / gSM.

[0025] Embodiment 14:

[0026] The coke inhibitor of Example 6 was added at 50 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was measured according to GB / T 509-88 standard and was 4.34 mg / gSM.

[0027] Embodiment 15:

[0028] The coke inhibitor of Example 7 was added at 20 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was determined in accordance with GB / T 509-88 standard to be 4.42 mg / gSM.

[0029] Embodiment 16:

[0030] The coke inhibitor of Example 8 was added at 10 ppm to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation device for the actual industrial preparation of styrene, and its mass composition is: 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, 54% styrene). After 12 hours at a temperature of 120°C and a pressure of 2.5 MPa, the tar content was determined in accordance with GB / T 509-88 standard to be 4.58 mg / gSM.

[0031] Blank comparison test

[0032] Without adding any coke inhibitor to the evaluation raw material (the evaluation raw material is the crude styrene material entering the distillation unit for the actual industrial preparation of styrene, with a mass composition of 0.6% benzene, 1.8% toluene, 0.2% xylene, 42% ethylbenzene, and 54% styrene), the tar content was measured at a temperature of 120°C and a pressure of 2.5 MPa after 12 hours in accordance with GB / T 509-88 standard and was found to be 6.85 mg / gSM.

[0033] From the results of the above application evaluation experiment and blank comparison experiment, it can be seen that after using the novel environmentally friendly coking inhibitor of the present invention, the styrene polymerization rate is significantly reduced, the styrene polymer is effectively inhibited, and the tar yield is significantly reduced. This shows that the coking inhibitor of the present invention has a good effect in preventing tar from being generated. In addition, the environment will not be polluted during use.

Claims

1. An environmentally friendly coking inhibitor for a styrene device, comprising component A, component B and an organic solvent, characterized in that The mass ratio of component A to component B is 0.1-10:1, and the amount of the organic solvent is such that the kinematic viscosity of the scorch inhibitor at 30°C is maintained at ≤8mm 2 / s; wherein: component A is selected from one of N,N'-bis(1-ethyl-3-methylpentyl)-p-phenylenediamine and N,N'-dimethyl-N,N'-di(1-methylpropyl)-p-phenylenediamine; component B is selected from one of 2,4-dihydroxybenzophenone and 2-hydroxy-4-methoxybenzophenone; the organic solvent is C5~C 10 of hydrocarbons.

2. The environmentally friendly coking inhibitor for styrene device according to claim 1, characterized in that: The mass ratio of component A to component B is 0.5~1:

1.

3. A method for using an environmentally friendly coking inhibitor for a styrene device, comprising adding the coking inhibitor of claim 1 or 2 into a crude styrene material in a styrene distillation tower at a mass concentration of not less than 5 ppm.

4. The method of use according to claim 3, characterized in that: The coke inhibitor is added into the crude styrene material in the styrene distillation tower at a mass concentration of 5 to 1000 ppm.

5. The method of use according to claim 4, characterized in that: The coke inhibitor is added into the crude styrene material in the styrene distillation tower at a mass concentration of 5 to 100 ppm.