Electrode material consistency determination method, system, electronic device and storage medium

By conducting electrochemical tests on the negative electrode material, obtaining the target voltage and current parameters, calculating the judgment parameters and comparing them with the benchmark parameters, the problem of low consistency judgment efficiency in the existing technology is solved, and efficient qualitative and quantitative judgment is achieved.

CN114487056BActive Publication Date: 2024-11-05SUNWODA MOBILITY ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210110650.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-01-29
Publication Date
2024-11-05
Estimated Expiration
2042-01-29

AI Technical Summary

Technical Problem

In existing technologies, the consistency determination of negative electrode materials is inefficient, and accurate conclusions cannot be drawn from a single test item; multiple parameters need to be tested.

Method used

By conducting multiple electrochemical tests on the material under test, multiple sets of test parameters are obtained, the target voltage parameter range and current parameter are determined, the judgment parameters are calculated, and the results are compared with the reference parameters to achieve consistency judgment.

Benefits of technology

This improves the efficiency of electrode material consistency determination, avoids the need to test multiple parameters, and enables both qualitative and quantitative determination.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114487056B_ABST
    Figure CN114487056B_ABST
Patent Text Reader

Abstract

The present application discloses a method, system, electronic device and storage medium for determining the consistency of electrode materials. The method for determining the consistency of electrode materials includes: performing multiple electrochemical tests on the material to be tested to obtain multiple groups of test parameter groups; determining the target voltage parameter range from any group of the test parameter groups, and using at least one of the candidate voltage parameters in the target voltage parameter range as the first target parameter; obtaining the candidate current parameter corresponding to the first target parameter from multiple groups of the test parameter groups, and using the candidate current parameter as the second target parameter; calculating the determination parameter based on multiple second target parameters; comparing the determination parameter with the preset reference parameter, and determining the consistency of the material to be tested based on the comparison result. The present application can avoid testing multiple parameter indicators of the material to be tested, thereby improving the efficiency of determining the consistency of the material to be tested.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of consistency determination, and in particular to a method, system, electronic device and storage medium for determining the consistency of an electrode material. Background Art

[0002] At present, with the increasing shortage of fossil energy resources, electric energy storage devices such as batteries and capacitors are widely used in various fields. Among them, negative electrode materials and positive electrode materials are important components of energy storage devices.

[0003] Taking negative electrode materials as an example, in related technologies, when judging the consistency of negative electrode materials, it is necessary to test multiple parameter indicators such as particle size distribution, specific surface area, tap density, morphology, and crystal structure of the negative electrode materials, and determine the consistency of the negative electrode materials based on the test results of the above multiple parameter indicators. That is, this method cannot draw a judgment conclusion through a single test item indicator, which affects the efficiency of consistency judgment. Summary of the invention

[0004] The present application aims to solve at least one of the technical problems existing in the prior art. To this end, the present application proposes a method, system, electronic device and storage medium for determining the consistency of electrode materials, which can avoid testing multiple parameter indicators of the material to be tested, thereby improving the efficiency of determining the consistency of the material to be tested.

[0005] According to the first aspect of the present application, the electrode material consistency determination method includes: performing multiple electrochemical tests on the material to be tested to obtain multiple groups of test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each group of the test parameter groups includes multiple candidate current parameters, and candidate voltage parameters corresponding to the candidate current parameters; determining a target voltage parameter range from any group of the test parameter groups, and taking at least one of the candidate voltage parameters in the target voltage parameter range as a first target parameter; obtaining the candidate current parameter corresponding to the first target parameter from multiple groups of the test parameter groups, and taking the candidate current parameter as a second target parameter; calculating a determination parameter based on multiple second target parameters; comparing the determination parameter with a preset reference parameter, and determining the consistency of the material to be tested based on the comparison result.

[0006] According to the electrode material consistency determination method of the embodiment of the present application, there is at least the following beneficial effect: by performing electrochemical tests on the material to be tested, multiple groups of test parameter groups are obtained, and a target voltage parameter range that can provide a basis for determination of consistency is obtained from any group of test parameter groups. The second target parameter is obtained according to the first target parameter in the target voltage parameter range, and the determination parameter is obtained according to the multiple second target parameters, so as to determine the consistency of the material to be tested according to the comparison result of the determination parameter and the reference parameter. It can be seen that the electrode material consistency determination method provided in the embodiment of the present application avoids the detection of multiple parameter indicators of the material to be tested, and only needs to extract the target parameters (including the first target parameter and the second target parameter) from the test parameter group corresponding to the electrochemical test to obtain the determination parameter. Therefore, the electrode material consistency determination method provided in the embodiment of the present application improves the efficiency of consistency determination.

[0007] According to some embodiments of the present application, the test parameter group includes candidate parameter ranges representing non-oxidation peak ranges and non-reduction peak ranges; determining the target voltage parameter range from any group of the test parameter groups includes: taking the candidate parameter range of any group of the test parameter groups as the target voltage parameter range.

[0008] According to some embodiments of the present application, multiple groups of electrochemical tests are performed on the material to be tested to obtain multiple groups of test parameter groups, including: performing CV tests or LSV tests according to a preset scanning speed to obtain multiple candidate current parameters and multiple candidate voltage parameters; obtaining a group of test parameter groups based on multiple candidate current parameters and multiple candidate voltage parameters; adjusting the scanning speed, and performing the scanning operation according to the preset scanning speed again to obtain multiple groups of test parameter groups.

[0009] According to some embodiments of the present application, the determination parameter is calculated based on multiple second target parameters, including: obtaining the scanning speed corresponding to the second target parameter; in the same scanning direction, the determination parameter is calculated based on multiple second target parameters and the corresponding scanning speeds; wherein the same scanning direction includes any one of a direction of increasing the candidate voltage parameter and a direction of decreasing the candidate voltage parameter.

[0010] According to some embodiments of the present application, the consistency of the material to be tested is determined based on the comparison result, including: if the comparison result indicates that the determination parameter is equal to the reference parameter, then the consistency of the material to be tested is determined to be at the first level; if the comparison result indicates that the determination parameter is not equal to the reference parameter, then the consistency of the material to be tested is determined to be at the second level.

[0011] According to some embodiments of the present application, the consistency of the material to be tested is determined based on the comparison result, including: if the comparison result indicates that the determination parameter is not equal to the reference parameter, obtaining the difference value between the determination parameter and the reference parameter; if the difference value is within a preset range, determining that the consistency of the material to be tested is a preset level corresponding to the preset range.

[0012] According to the second aspect of the present application, the electrode material consistency determination system includes: a test module, which is used to perform multiple electrochemical tests on the material to be tested to obtain multiple groups of test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each group of the test parameter groups includes multiple candidate current parameters, and candidate voltage parameters corresponding to the candidate current parameters; a first query module, which is used to determine the target voltage parameter range from any group of the test parameter groups, and use at least one of the candidate voltage parameters in the target voltage parameter range as the first target parameter; a second query module, which is used to obtain the candidate current parameter corresponding to the first target parameter from multiple groups of the test parameter groups, and use the candidate current parameter as the second target parameter; a calculation module, which is used to calculate the determination parameter based on multiple second target parameters; a determination module, which is used to compare the determination parameter with a preset reference parameter, and determine the consistency of the material to be tested based on the comparison result.

[0013] According to some embodiments of the present application, it also includes: a testing device, which is a three-electrode electrochemical system or a two-electrode electrochemical system; wherein the preparation material of the working electrode of the testing device is the material to be tested; and the testing module is used to perform the electrochemical test on the testing device multiple times.

[0014] According to the electronic device of the embodiment of the third aspect of the present application, it includes: at least one processor; at least one memory for storing at least one program; when the at least one program is executed by the at least one processor, the at least one processor implements the electrode material consistency determination method as described in the first aspect.

[0015] According to the computer-readable storage medium of the fourth aspect embodiment of the present application, processor-executable instructions are stored therein, and the processor-executable instructions, when executed by the processor, are used to implement the electrode material consistency determination method as described in the first aspect.

[0016] The electrode material consistency determination method, system, electronic device and storage medium provided by the present application conduct electrochemical testing on the material to be tested, and select the third candidate parameter range corresponding to the non-Faraday capacitance characteristic signal area in the test parameter group as the target voltage parameter range, thereby obtaining a determination parameter that can characterize the consistency change of the material to be tested according to the target voltage parameter range, and then achieving qualitative and / or quantitative determination of the consistency of the material to be tested according to the comparison result of the determination parameter and the reference parameter. Therefore, the embodiment of the present application avoids testing multiple parameter indicators of the material to be tested, and improves the efficiency of determining the consistency of the material to be tested.

[0017] Additional aspects and advantages of the present application will be given in part in the description below, and in part will become apparent from the description below, or will be learned through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The present application is further described below with reference to the accompanying drawings and embodiments, wherein:

[0019] Figure 1 A schematic diagram of a process of determining the consistency of electrode materials according to an embodiment of the present application;

[0020] Figure 2 This is a schematic diagram of a CV curve of an embodiment of the present application with a scan rate of 0.5 mV / s;

[0021] Figure 3 Another schematic diagram of the process of determining the consistency of electrode materials according to an embodiment of the present application;

[0022] Figure 4 Another schematic diagram of the process of determining the consistency of electrode materials according to an embodiment of the present application;

[0023] Figure 5 This is a schematic diagram of a candidate current parameter-scanning speed curve with 2.5V as the first target parameter in an embodiment of the present application;

[0024] Figure 6 Another schematic diagram of the process of determining the consistency of electrode materials according to an embodiment of the present application;

[0025] Figure 7 Another schematic diagram of the process of determining the consistency of electrode materials according to an embodiment of the present application;

[0026] Figure 8 This is a module block diagram of the electrode material consistency determination system according to an embodiment of the present application. DETAILED DESCRIPTION

[0027] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and cannot be understood as limiting the present application.

[0028] In the description of the present application, it should be understood that descriptions involving orientation, such as up, down, front, back, left, right, etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0029] In the description of this application, "several" means more than one, "more" means more than two, "greater than", "less than", "exceed", etc. are understood to exclude the number itself, and "above", "below", "within", etc. are understood to include the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.

[0030] In the description of this application, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in this application based on the specific content of the technical solution.

[0031] In the description of the present application, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0032] First, some terms used in this application are explained:

[0033] Electrochemical testing refers to the process of applying disturbance or stimulation to the electrochemical system based on electrochemical theory, recording or observing the electrochemical response of the electrochemical system, and analyzing the characteristics, performance, behavior and other particularities of the electrochemical system.

[0034] Electrochemical system, the basic unit of electrochemical system includes working electrode, auxiliary electrode, reference electrode, diaphragm, electrolyte (or electrolyte), etc. Among them, the working electrode refers to the electrode on which the reaction to be studied occurs; the auxiliary electrode is the electrode that forms a circuit with the working electrode; the reference electrode is an electrode with a relatively stable and known potential, and the reference electrode is used to provide a voltage monitoring reference for the working electrode.

[0035] CV test (cyclic voltammetry test) is a test method that controls the electrode voltage to scan at different rates and records the current-voltage curve. The voltage range includes multiple voltages that cause different reduction reactions and oxidation reactions to occur alternately on the electrode. The shape of the current-voltage curve can be used to determine the reversibility of the electrode reaction, the possibility of intermediates, phase boundary adsorption or new phase formation, and the nature of the coupled chemical reaction.

[0036] LSV test (Linear Sweep Voltammetry test) refers to a test method in which a linear potential sweep (a linear relationship between potential and time) is applied between a working electrode and an auxiliary electrode.

[0037] It should be noted that in the present application, the electrode material includes any one of the negative electrode material and the positive electrode material. In the following embodiments, the negative electrode material to be tested is taken as the material to be tested for specific description. However, it should be understood that when the positive electrode material to be tested is taken as the material to be tested, the adaptive modifications made to the following embodiments should also fall within the protection scope of the present application.

[0038] Reference Figure 1 and Figure 2 The present application embodiment provides a method for determining the consistency of electrode materials, which includes but is not limited to steps S110 to S150:

[0039] S110, performing multiple electrochemical tests on the negative electrode material to be tested to obtain multiple test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each test parameter group includes multiple candidate current parameters and candidate voltage parameters corresponding to the candidate current parameters;

[0040] S120, determining a target voltage parameter range from any set of test parameter groups, and taking at least one candidate voltage parameter in the target voltage parameter range as a first target parameter;

[0041] S130, obtaining a candidate current parameter corresponding to the first target parameter from a plurality of test parameter groups, and using the candidate current parameter as the second target parameter;

[0042] S140, calculating and obtaining a determination parameter according to a plurality of second target parameters;

[0043] S150, comparing the determination parameter with a preset reference parameter, and determining the consistency of the negative electrode material to be tested according to the comparison result.

[0044] Specifically, the negative electrode material to be tested is taken as the reaction research object, and the electrochemical system to be tested composed of the negative electrode material to be tested is subjected to electrochemical tests such as CV test or LSV test under different test conditions. Taking CV test as an example, multiple candidate voltage parameters in the test and the candidate current parameters corresponding to each candidate voltage parameter are recorded, and multiple candidate voltage parameters and multiple candidate current parameters under the same test conditions are formed into a group of test parameter groups, thereby obtaining multiple groups of test parameter groups. According to each group of test parameter groups, a corresponding CV curve (i.e., candidate current parameter-candidate voltage parameter curve) is constructed, and a target voltage parameter range is determined from any group of test parameter groups, that is, a target voltage parameter range is determined from any CV curve. Among them, the target voltage parameter range represents the range composed of multiple candidate voltage parameters corresponding to the effective area in the CV curve, and the effective area refers to the area that can provide a basis for determining the consistency of the negative electrode material to be tested. Select any candidate voltage parameter from the target voltage parameter range as the first target parameter, search for the candidate current parameter corresponding to the first target parameter from each group of test parameter groups, and use the candidate current parameter as the second target parameter, thereby obtaining multiple second target parameters. According to the multiple second target parameters, a judgment parameter for characterizing the current consistency of the negative electrode material to be tested is calculated, and the judgment parameter is compared with the reference parameter of the reference electrochemical system to judge the consistency of the negative electrode material to be tested according to the comparison result, so as to obtain a judgment conclusion that the consistency is "good, medium, poor", etc. It can be understood that the reference electrochemical system includes a reference negative electrode material, and the reference negative electrode material is used as the reaction research object. Under the same test conditions, the reference electrochemical system is subjected to the same CV test or LSV test as the electrochemical system to be tested, and the reference parameters are calculated according to the same method as above.

[0045] The electrode material consistency determination method provided in the embodiment of the present application is to obtain multiple groups of test parameter groups by performing electrochemical tests on the negative electrode material to be measured, and obtain a target voltage parameter range that can provide a basis for determination of consistency from any group of test parameter groups. The second target parameter is obtained according to the first target parameter in the target voltage parameter range, and the determination parameter is obtained according to the multiple second target parameters, so as to determine the consistency of the negative electrode material to be measured according to the comparison result of the determination parameter and the reference parameter. It can be seen that the electrode material consistency determination method provided in the embodiment of the present application avoids the detection of multiple parameter indicators of the negative electrode material to be measured, and only needs to extract the target parameter (including the first target parameter and the second target parameter) from the test parameter group corresponding to the electrochemical test to obtain the determination parameter. Therefore, the electrode material consistency determination method provided in the embodiment of the present application improves the efficiency of consistency determination.

[0046] Reference Figure 3 In some embodiments, step S110 includes but is not limited to the following sub-steps:

[0047] S310, performing a CV test or an LSV test according to a preset scanning speed to obtain a plurality of candidate current parameters and a plurality of candidate voltage parameters;

[0048] S320, obtaining a set of test parameter groups according to a plurality of candidate current parameters and a plurality of candidate voltage parameters;

[0049] S330, adjusting the scanning speed, and executing step S310 again to obtain multiple test parameter groups.

[0050] Specifically, a three-electrode electrochemical system or a two-electrode electrochemical system is prepared according to the negative electrode material to be tested, wherein the three-electrode electrochemical system includes a working electrode, a reference electrode and an auxiliary electrode; the two-electrode electrochemical system includes a working electrode and an auxiliary electrode. The negative electrode material to be tested includes the negative electrode materials used in lithium-ion batteries, sodium-ion batteries, magnesium-ion batteries, aluminum-ion batteries, supercapacitors, and pseudocapacitors, that is, the negative electrode material to be tested includes MCMB (mesophase carbon microspheres), soft carbon, hard carbon, graphite, graphite oxide, sulfonated graphite, graphene, graphene oxide, sulfonated graphene, carbon nanotubes, silicon, silicon oxide, metal element, metal oxide, metal sulfide, titanium oxide, titanate, titanium sulfide. The auxiliary electrode includes any one of metal platinum, gold, palladium, lithium, sodium, magnesium, and aluminum. The reference electrode includes any one of metal platinum, gold, palladium, lithium, sodium, magnesium, aluminum, lithium iron phosphate, lithium titanate, calomel electrode, silver-silver chloride electrode, mercury-mercury oxide electrode, and hydrogen electrode.

[0051] Taking the two-electrode electrochemical system as an example, the negative electrode material to be tested is made into a working electrode, for example: graphite is selected as the working electrode, metallic lithium is selected as the auxiliary electrode, and LiPF is selected as the electrolyte. 6 , Celgard2300 is selected as the diaphragm, thereby preparing a test device. The test device is powered on, and a scanning operation is performed on the test device at a preset scanning speed (i.e., test conditions), and multiple candidate current parameters and multiple candidate voltage parameters corresponding to the scanning operation are obtained, thereby obtaining a set of test parameter groups corresponding to the scanning speed. The scanning speed is adjusted, and the above operation is repeated according to multiple different scanning speeds to obtain multiple sets of test parameter groups. It can be understood that the scanning speed can be selected from any value between 0.1mV / s and 100mV / s.

[0052] For example, if the scanning speeds are set to include 0.1mV / s, 0.5mV / s, 1.0mV / s and 2.0mV / s, four test parameter groups can be obtained according to the above method. Each scanning speed only performs one cycle of oxidation reaction and reduction reaction, and the electrochemical test of the negative electrode material to be tested is performed from low scanning speed to high scanning speed until the test completes all the set scanning speeds.

[0053] Secondly, in order to avoid side reactions during the scanning process and unnecessary time consumption, the voltage range of the CV test is limited to 0.01V to 3.00V, that is, the candidate voltage parameters are between 0.01V and 3.00V.

[0054] In some embodiments, the test parameter group includes a first candidate parameter range representing an oxidation peak range, a second candidate parameter range representing a reduction peak range, and a third candidate parameter range representing a non-oxidation peak range and a non-reduction peak range. In step S120, "determining a target voltage parameter range from any set of test parameter groups" includes but is not limited to sub-steps:

[0055] The third candidate parameter range of any test parameter group is used as the target voltage parameter range.

[0056] Specifically, taking the CV test as an example, CV curves are constructed for each of the multiple test parameter groups obtained according to the above method. Figure 2 , taking the CV curve corresponding to a scanning speed of 0.5 mV / s as an example. In the CV test, when the triangular wave voltage (i.e., the candidate voltage parameter) increases (i.e., when the potential is scanned toward the cathode), the electroactive substance is reduced on the working electrode, thereby obtaining the reduction wave in the CV curve (e.g., Figure 2 As shown in 100); when the triangle wave voltage is reduced (i.e., when the potential is scanned toward the anode), the reduction product will be oxidized again on the working electrode, thereby obtaining the oxidation wave in the CV curve (as shown in Figure 2 200). Therefore, the CV curve can be divided into a reduction peak range, an oxidation peak range, and the remaining range, wherein the oxidation peak range corresponds to the first candidate parameter range, the reduction peak range corresponds to the second candidate parameter range, and the remaining range corresponds to the third candidate parameter range.

[0057] When the negative electrode material to be tested changes, that is, when the negative electrode material to be tested is inconsistent with the reference negative electrode material, the characteristic signal area of ​​the non-Faraday capacitor in the CV curve will change accordingly, and the characteristic signal area of ​​the non-Faraday capacitor corresponds to the third candidate parameter range. Therefore, the third candidate parameter range is used as the target voltage parameter range, that is, at least one candidate voltage parameter within the third candidate parameter range is processed to obtain the judgment parameter for characterizing the current consistency of the negative electrode material to be tested.

[0058] Reference Figure 4 In some embodiments, step S140 includes but is not limited to the sub-steps of:

[0059] S410, obtaining a scanning speed corresponding to a second target parameter;

[0060] S420 , in the same scanning direction, calculating a determination parameter according to a plurality of second target parameters and corresponding scanning speeds.

[0061] Specifically, in Figure 2 In the CV curve shown, the target voltage parameter range is the candidate voltage parameters corresponding to 1.2V to 3.0V. From the target voltage parameter range, any candidate voltage parameter is selected as the first target parameter, such as 2.5V is selected as the first target parameter. In the four test parameter groups, the candidate current parameters corresponding to 2.5V are searched respectively, and the searched candidate current parameters are used as the second target parameters, thereby obtaining four second target parameters.

[0062] It can be understood that the characteristic signal region of the non-Faraday capacitor can be expressed as a relationship: I / Vscan=K1, where I represents the candidate current parameter, Vscan represents the scanning speed, and K1 represents the slope (i.e., the determination parameter). Therefore, in the same scanning direction, a current-scanning speed diagram (such as Figure 5 As shown). The same scanning direction includes any one of the directions of increasing the candidate voltage parameter and decreasing the candidate voltage parameter, that is, any one of scanning the potential toward the cathode direction and scanning the potential toward the anode direction. Figure 5 Taking the same scanning direction as the direction of increase of the candidate voltage parameter as an example, a candidate current parameter-scanning speed diagram is constructed according to the candidate current parameters corresponding to 2.5V at scanning speeds of 0.1mV / s, 0.5mV / s, 1.0mV / s and 2.0mV / s, and the slope value K1 corresponding to the candidate current parameter-scanning speed diagram is calculated to obtain the judgment parameter.

[0063] Reference Figure 6 In some embodiments, step S150 includes but is not limited to the sub-steps of:

[0064] S610, if the comparison result indicates that the determination parameter is equal to the reference parameter, then the consistency of the negative electrode material to be tested is determined to be the first level;

[0065] S620: If the comparison result indicates that the determination parameter is not equal to the reference parameter, the consistency of the negative electrode material to be tested is determined to be at the second level.

[0066] Specifically, the judgment parameter is compared with the reference parameter. If the comparison result indicates inequality, it indicates that at least one of the particle size distribution, specific surface area, tap density, morphology, crystal structure, etc. of the negative electrode material to be tested is different from that of the reference negative electrode material. At this time, the consistency of the negative electrode material to be tested is judged to be the first level; if the comparison result indicates equality, it indicates that the particle size distribution, specific surface area, tap density, morphology, crystal structure, etc. of the negative electrode material to be tested are equal to those of the reference negative electrode material. At this time, the consistency of the negative electrode material to be tested is judged to be the second level, thereby achieving a qualitative judgment on the consistency of the negative electrode material to be tested.

[0067] Reference Figure 7 In some other embodiments, step S150 includes but is not limited to sub-steps:

[0068] S710, if the comparison result indicates that the determination parameter and the reference parameter are not equal, obtain the difference value between the determination parameter and the reference parameter;

[0069] S720: If the difference value is within a preset range, it is determined that the consistency of the negative electrode material to be tested is a preset level corresponding to the preset range.

[0070] Specifically, a plurality of preset ranges are pre-set, and each preset range corresponds to a preset level. When it is determined that the judgment parameter is not equal to the reference parameter, the difference value between the judgment parameter and the reference parameter is obtained, and the preset range containing the difference value is searched, so as to determine the consistency of the negative electrode material to be tested according to the preset level corresponding to the preset range, thereby achieving a quantitative judgment on the consistency of the negative electrode material to be tested. It is understandable that the difference value includes any one of a difference value, a rate of change, etc., which is not specifically limited in the embodiments of the present application.

[0071] In the following, taking different types of negative electrode materials to be tested as an example, the quantitative judgment of the consistency of the negative electrode materials to be tested is specifically described.

[0072] First, in some embodiments, graphite is selected as the negative electrode material to be tested, the negative electrode material to be tested is used as the working electrode, the auxiliary electrode is selected as metallic lithium, the electrolyte is selected as LiPF6, and the diaphragm is selected as Celgard2300. The working electrode, the auxiliary electrode, the electrolyte and the diaphragm are assembled to form a two-electrode electrochemical system to be tested. Four scanning speeds are set at 0.1mV / s, 0.5mV / s, 1.0mV / s and 2.0mV / s, and the determination parameters of the negative electrode material to be tested are calculated according to the method described in any of the above embodiments.

[0073] Table 1:

[0074] Slope value K2 Rate of change Preset Level Benchmark anode materials 1.64E-04 0.0% /

[0075] Table 2:

[0076] Negative electrode material to be tested Slope value K1 Rate of change Preset Level Particle size D50 reduced by 1um 1.42E-04 -13.2% middle Particle size D50 increased by 1.5um 2.06E-04 25.7% Difference Particle size D50 increased by 3um 2.43E-04 48.0% Difference Graphitization degree decreased by 1% 1.50E-04 -8.7% good Graphitization degree increased by 1% 1.75E-04 6.5% good Graphitization degree increased by 2% 1.94E-04 18.1% middle 20% reduction in specific surface area 2.08E-04 27.1% Difference Surface area reduced by 10% 1.95E-04 18.8% middle Surface area increased by 10% 1.85E-04 12.9% middle Tap density reduced by 15% 1.86E-04 13.5% middle 15% increase in tap density 1.96E-04 19.4% middle

[0077] Referring to Table 1 and Table 2, taking the rate of change as an example to represent the difference value, three preset ranges of 0≤x<10%, 10%≤x<20%, ​​and x≥20% are pre-set, wherein x represents the absolute value of the rate of change, 0≤x<10% represents the preset level of "good", 10%≤x<20% represents the preset level of "medium", and x≥20% represents the preset level of "poor". It can be understood that, corresponding to the two-electrode electrochemical system to be tested, the reference two-electrode electrochemical system uses the reference negative electrode material as the working electrode, and the components of each part of the reference two-electrode electrochemical system are equal to those of the two-electrode electrochemical system to be tested, that is, the auxiliary electrode of the reference two-electrode electrochemical system uses metallic lithium, and the electrolyte uses LiPF 6 The separator is Celgard 2300. The slope value K2 (i.e., the reference parameter) of the reference negative electrode material calculated according to the method described in any of the above embodiments is 1.64E-04.

[0078] As shown in Table 2, when the particle size D50 of the negative electrode material to be tested is reduced by 1 μm compared to the particle size D50 of the reference negative electrode material, the slope value K1 (i.e., the judgment parameter) of the negative electrode material to be tested is 1.42E-04, and the change rate of the judgment parameter compared to the reference parameter is -13.2%. At this time, the consistency of the negative electrode material to be tested is judged to be medium. When the particle size D50 of the negative electrode material to be tested is increased by 1.5 μm compared to the particle size D50 of the reference negative electrode material, the slope value K1 of the negative electrode material to be tested is 2.06E-04, and the change rate of the judgment parameter compared to the reference parameter is 25.7%. At this time, the consistency of the negative electrode material to be tested is judged to be poor. When the particle size D50 of the negative electrode material to be tested is increased by 3 μm compared to the particle size D50 of the reference negative electrode material, the slope value K1 of the negative electrode material to be tested is 2.43E-04, and the change rate of the judgment parameter compared to the reference parameter is 48.0%. At this time, the consistency of the negative electrode material to be tested is judged to be poor. It can be understood that when the graphitization degree, specific surface area and solid density of the negative electrode material to be tested change, the preset level corresponding to the negative electrode material to be tested can be obtained by referring to Table 2, and this embodiment of the present application will not be repeated.

[0079] Secondly, in some other embodiments, a composite of graphene and iron oxide is selected as the negative electrode material to be tested, the negative electrode material to be tested is used as the working electrode, metal platinum is selected as the auxiliary electrode, 1.0M potassium hydroxide standard titration solution is selected as the electrolyte, and mercuric trioxide electrode is selected as the reference electrode. A three-electrode electrochemical system to be tested is assembled according to the working electrode, the auxiliary electrode, the electrolyte and the reference electrode. Taking the LSV test as an example, four scanning speeds of 0.01mV / s, 1.0mV / s, 10mV / s and 100mV / s are set, and according to the method described in any of the above embodiments, the direction of decreasing the candidate voltage parameter is used as the same scanning direction to calculate the determination parameter of the negative electrode material to be tested.

[0080] Table 3:

[0081] Slope value K2 Rate of change Preset Level Benchmark anode materials 2.71E-02 0.0% /

[0082] Table 4:

[0083]

[0084] Referring to Table 3 and Table 4, taking the rate of change as an example to represent the difference value, three preset ranges of 0≤x<10%, 10%≤x<20%, ​​and x≥20% are pre-set, wherein x represents the absolute value of the rate of change, 0≤x<10% represents the preset level of "good", 10%≤x<20% represents the preset level of "medium", and x≥20% represents the preset level of "poor". It can be understood that, corresponding to the three-electrode electrochemical system to be tested, the reference three-electrode electrochemical system uses the reference negative electrode material as the working electrode, and the components of each part of the reference three-electrode electrochemical system are equal to those of the three-electrode electrochemical system to be tested. The slope value K2 (i.e., the reference parameter) of the reference negative electrode material calculated according to the method described in any of the above embodiments is 2.71E-02.

[0085] As shown in Table 4, when the iron oxide proportion of the negative electrode material to be tested increases by 1wt.% compared to the iron oxide proportion of the reference negative electrode material, the slope value K1 (i.e., the judgment parameter) of the negative electrode material to be tested is 3.04E-02, and the change rate of the judgment parameter compared to the reference parameter is 12.2%. At this time, the consistency of the negative electrode material to be tested is judged to be medium. When the iron oxide proportion of the negative electrode material to be tested decreases by 5wt.% compared to the iron oxide proportion of the reference negative electrode material, the slope value K1 of the negative electrode material to be tested is 1.98E-02, and the change rate of the judgment parameter compared to the reference parameter is -26.8%. At this time, the consistency of the negative electrode material to be tested is judged to be poor. It can be understood that when the iron oxide particle size of the negative electrode material to be tested changes, the preset level corresponding to the negative electrode material to be tested can be obtained by referring to Table 4, and this embodiment of the present application will not be repeated.

[0086] Finally, in other embodiments, molybdenum disulfide is selected as the negative electrode material to be tested, the negative electrode material to be tested is used as the working electrode, the auxiliary electrode is selected as metal magnesium, the electrolyte is selected as 0.5M Mg(BH4)2 (volume ratio DME:THF=1:1), and the diaphragm is selected as Celgard2300. According to the working electrode, the auxiliary electrode, the electrolyte and the diaphragm, a two-electrode electrochemical system to be tested is assembled. Four scanning speeds of 0.1mV / s, 0.5mV / s, 5.0mV / s and 50mV / s are set, and the judgment parameters of the negative electrode material to be tested are calculated according to the method described in any of the above embodiments.

[0087] Table 5:

[0088] Slope value K2 Rate of change Preset Level Benchmark anode materials 9.30E-04 0.0% /

[0089] Table 6:

[0090] Negative electrode material to be tested Slope value K1 Rate of change Preset Level Surface area increased by 10% 1.11E-03 19.2% middle Surface area reduced by 5% 8.31E-04 -10.6% middle 20% increase in tap density 4.67E-04 -49.8% Difference Tap density reduced by 10% 1.09E-03 17.7% middle

[0091] Referring to Tables 5 and 6, taking the rate of change as an example to represent the difference value, three preset ranges of 0≤x<10%, 10%≤x<20%, ​​and x≥20% are pre-set, wherein x represents the absolute value of the rate of change, 0≤x<10% represents the preset level of "good", 10%≤x<20% represents the preset level of "medium", and x≥20% represents the preset level of "poor". It can be understood that, corresponding to the two-electrode electrochemical system to be tested, the reference two-electrode electrochemical system uses the reference negative electrode material as the working electrode, and the components of each part of the reference two-electrode electrochemical system are equal to those of the two-electrode electrochemical system to be tested. The slope value K2 (i.e., the reference parameter) of the reference negative electrode material calculated according to the method described in any of the above embodiments is 9.30E-04.

[0092] As shown in Table 6, when the specific surface area of ​​the negative electrode material to be tested increases by 10% compared to the specific surface area of ​​the reference negative electrode material, the slope value K2 (i.e., the judgment parameter) of the negative electrode material to be tested is 1.11E-03, and the rate of change of the judgment parameter compared to the reference parameter is 19.2%. At this time, the consistency of the negative electrode material to be tested is judged to be medium. When the specific surface area of ​​the negative electrode material to be tested decreases by 5% compared to the specific surface area of ​​the reference negative electrode material, the slope value K2 of the negative electrode material to be tested is 8.31E-04, and the rate of change of the judgment parameter compared to the reference parameter is -10.6%. At this time, the consistency of the negative electrode material to be tested is judged to be medium. It can be understood that when the specific surface area and tap density of the negative electrode material to be tested change, the preset level corresponding to the negative electrode material to be tested can be obtained by referring to Table 6, and this embodiment of the present application will not be repeated.

[0093] The electrode material consistency determination method provided in the embodiment of the present application performs an electrochemical test on the negative electrode material to be tested, and selects the third candidate parameter range corresponding to the non-Faraday capacitance characteristic signal area in the test parameter group as the target voltage parameter range, thereby obtaining a determination parameter that can characterize the consistency change of the negative electrode material to be tested according to the target voltage parameter range, and then realizes the qualitative determination and / or quantitative determination of the consistency of the negative electrode material to be tested according to the comparison result of the determination parameter and the reference parameter. Therefore, the determination method provided in the embodiment of the present application avoids testing multiple parameter indicators of the negative electrode material to be tested, and improves the determination efficiency of the consistency of the negative electrode material to be tested.

[0094] Reference Figure 8 The present application also provides a system for determining the consistency of electrode materials. The system includes:

[0095] The test module 801 is used to perform multiple electrochemical tests on the negative electrode material to obtain multiple test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each test parameter group includes multiple candidate current parameters and candidate voltage parameters corresponding to the candidate current parameters;

[0096] A first query module 802 is used to determine a target voltage parameter range from any set of test parameter groups, and to use at least one candidate voltage parameter in the target voltage parameter range as a first target parameter;

[0097] A second query module 803 is used to obtain candidate current parameters corresponding to the first target parameter from multiple test parameter groups, and use the candidate current parameters as the second target parameter;

[0098] A calculation module 804, configured to calculate a determination parameter according to a plurality of second target parameters;

[0099] The determination module 805 is used to compare the determination parameter with the preset reference parameter, and determine the consistency of the negative electrode material to be tested according to the comparison result.

[0100] Secondly, the determination system also includes a test device, which is a three-electrode electrochemical system or a two-electrode electrochemical system, wherein the preparation material of the working electrode of the test device is the material to be tested, and the test module 801 is used to perform multiple electrochemical tests on the test device.

[0101] It can be seen that the contents of the above-mentioned electrode material consistency determination method embodiment are all applicable to the embodiments of the present electrode material consistency determination system. The functions specifically implemented by the present electrode material consistency determination system embodiment are the same as those in the above-mentioned electrode material consistency determination method embodiment, and the beneficial effects achieved are also the same as those achieved by the above-mentioned electrode material consistency determination method embodiment.

[0102] The embodiment of the present application also provides an electronic device, which includes: at least one processor, and a memory connected to the at least one processor in communication. The memory stores instructions, and the instructions are executed by the at least one processor, so that when the at least one processor executes the instructions, the electrode material consistency determination method described in any of the above embodiments is implemented.

[0103] An embodiment of the present application provides a computer-readable storage medium storing computer-executable instructions, wherein the computer-executable instructions are used to execute the electrode material consistency determination method described in any of the above embodiments.

[0104] The device embodiments described above are merely illustrative, and the units described as separate components may or may not be physically separated, that is, they may be located in one place or distributed on multiple network units. Some or all of the modules may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0105] It will be appreciated by those skilled in the art that all or some of the steps and systems in the disclosed method above may be implemented as software, firmware, hardware and appropriate combinations thereof. Some physical components or all physical components may be implemented as software executed by a processor, such as a central processing unit, a digital signal processor or a microprocessor, or may be implemented as hardware, or may be implemented as an integrated circuit, such as an application specific integrated circuit. Such software may be distributed on a computer-readable medium, which may include a computer storage medium (or a non-transitory medium) and a communication medium (or a temporary medium). As known to those skilled in the art, the term computer storage medium includes volatile and non-volatile, removable and non-removable media implemented in any method or technology for storing information (such as computer-readable instructions, data structures, program modules or other data). Computer storage media include, but are not limited to, RAM, ROM, EEPROM, flash memory or other memory technologies, CD-ROM, digital versatile disks (DVD) or other optical disk storage, magnetic cassettes, magnetic tapes, disk storage or other magnetic storage devices, or any other medium that may be used to store desired information and may be accessed by a computer. Furthermore, it is well known to those skilled in the art that communication media typically embodies computer readable instructions, data structures, program modules, or other data in a modulated data signal such as a carrier wave or other transport mechanism, and may include any information delivery media.

[0106] The embodiments of the present application are described in detail above in conjunction with the accompanying drawings, but the present application is not limited to the above embodiments. Various changes can be made within the knowledge of ordinary technicians in the relevant technical field without departing from the purpose of the present application. In addition, the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.

Claims

1. Method for determining the consistency of electrode materials, It is characterized in that include: Perform multiple electrochemical tests on the material to be tested at different scanning speeds to obtain multiple test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each of the test parameter groups includes multiple candidate current parameters and candidate voltage parameters corresponding to the candidate current parameters; Determine a target voltage parameter range from any one of the test parameter groups, and use at least one of the candidate voltage parameters in the target voltage parameter range as a first target parameter; wherein, determining the target voltage parameter range from any one of the test parameter groups comprises: using a third candidate parameter range of any one of the test parameter groups as the target voltage parameter range; wherein, the third candidate parameter range corresponds to a parameter range other than a range where a redox peak is located in a CV test or an LSV test; Obtaining the candidate current parameter corresponding to the first target parameter from the plurality of test parameter groups, and using the candidate current parameter as the second target parameter; Calculate the determination parameter according to the plurality of second target parameters; Using the determination parameter as the only parameter indicator to determine the consistency of the material to be tested, including: comparing the determination parameter with a preset reference parameter, and determining the consistency of the material to be tested according to the comparison result; The step of calculating the determination parameter based on the multiple second target parameters includes: Acquire the scanning speed corresponding to the second target parameter; In the same scanning direction, the determination parameter is obtained by calculating the slope value according to the plurality of the second target parameters and the corresponding scanning speeds; Wherein, the same scanning direction includes any one of an increasing direction of the candidate voltage parameter and a decreasing direction of the candidate voltage parameter; Wherein, judging the consistency of the material to be tested according to the comparison result includes: If the comparison result indicates that the determination parameter is not equal to the reference parameter, obtaining a difference value between the determination parameter and the reference parameter; If the difference value is within a preset range, the consistency of the material to be tested is determined to be a preset level corresponding to the preset range.

2. The method for determining the consistency of electrode materials according to claim 1, It is characterized in that The test parameter group includes candidate parameter ranges representing non-oxidation peak ranges and non-reduction peak ranges; Determining a target voltage parameter range from any one of the test parameter groups includes: The candidate parameter range of any group of the test parameter groups is used as the target voltage parameter range.

3. The method for determining the consistency of electrode materials according to claim 1, It is characterized in that The method of performing multiple groups of electrochemical tests on the material to be tested to obtain multiple groups of test parameter groups includes: Performing a CV test or an LSV test according to a preset scanning speed to obtain a plurality of the candidate current parameters and a plurality of the candidate voltage parameters; Obtain a set of the test parameter groups according to a plurality of the candidate current parameters and a plurality of the candidate voltage parameters; The scanning speed is adjusted, and the scanning operation according to the preset scanning speed is performed again to obtain multiple groups of the test parameter groups.

4. The method for determining the consistency of electrode materials according to any one of claims 1 to 3, It is characterized in that The determining of the consistency of the material to be tested according to the comparison result includes: If the comparison result indicates that the determination parameter is equal to the reference parameter, then the consistency of the material to be tested is determined to be at the first level; If the comparison result indicates that the determination parameter is not equal to the reference parameter, the consistency of the material to be tested is determined to be at the second level.

5. Electrode material consistency determination system, It is characterized in that include: A test module, used to perform multiple electrochemical tests on the material to be tested at different scanning speeds to obtain multiple test parameter groups; wherein the electrochemical test includes a CV test or an LSV test; each of the test parameter groups includes multiple candidate current parameters and candidate voltage parameters corresponding to the candidate current parameters; A first query module is used to determine a target voltage parameter range from any group of the test parameter groups, and use at least one of the candidate voltage parameters in the target voltage parameter range as the first target parameter; wherein, determining the target voltage parameter range from any group of the test parameter groups includes: using a third candidate parameter range of any of the test parameter groups as the target voltage parameter range; wherein, the third candidate parameter range corresponds to a parameter range other than the range where the redox peak is located in the CV test or the LSV test; A second query module, configured to obtain the candidate current parameter corresponding to the first target parameter from the plurality of test parameter groups, and use the candidate current parameter as the second target parameter; A calculation module, used for calculating a determination parameter according to a plurality of second target parameters; A determination module, used to determine the consistency of the material to be tested by using the determination parameter as the only parameter indicator, including: comparing the determination parameter with a preset reference parameter, and determining the consistency of the material to be tested according to the comparison result; The step of calculating the determination parameter based on the multiple second target parameters includes: Acquire the scanning speed corresponding to the second target parameter; In the same scanning direction, the determination parameter is obtained by calculating the slope value according to the plurality of the second target parameters and the corresponding scanning speeds; Wherein, the same scanning direction includes any one of an increasing direction of the candidate voltage parameter and a decreasing direction of the candidate voltage parameter; Wherein, judging the consistency of the material to be tested according to the comparison result includes: If the comparison result indicates that the determination parameter is not equal to the reference parameter, obtaining a difference value between the determination parameter and the reference parameter; If the difference value is within a preset range, the consistency of the material to be tested is determined to be a preset level corresponding to the preset range.

6. The electrode material consistency determination system according to claim 5, It is characterized in that Also includes: A test device, wherein the test device is a three-electrode electrochemical system or a two-electrode electrochemical system; Wherein, the preparation material of the working electrode of the testing device is the material to be tested; The test module is used to perform the electrochemical test on the test device multiple times.

7. Electronic equipment, It is characterized in that include: at least one processor; at least one memory for storing at least one program; When the at least one program is executed by the at least one processor, the at least one processor implements the electrode material consistency determination method according to any one of claims 1 to 4.

8. A computer-readable storage medium having processor-executable instructions stored therein, It is characterized in that The processor-executable instructions are used to implement the electrode material consistency determination method according to any one of claims 1 to 4 when executed by the processor.