Semiconductor structure
By adjusting the etching parameters of the shallow trench isolation structure in the fin-shaped field effect transistor assembly to form a step-like structure, and combining with the virtual gate structure, the problem of the upper limit of the process of the planar field effect transistor assembly is solved, and the upper limit of the process is achieved. Higher structural strength and performance.
Patent Information
- Application Number
- CN202210423638.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-06-01
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-06-01
AI Technical Summary
The existing planar field effect transistor components face process limits in the process of reducing the size, making it difficult to effectively suppress the energy band reduction and short channel effects caused by drain electrodes. The component manufacturing cost is high and the functional diversity is insufficient.
The fin-shaped field effect transistor assembly with a non-planar structure is adopted, and the etching parameters of the shallow trench isolation structure is adjusted to form a shallow trench isolation structure with a step-like cross-sectional structure. In combination with the dummy gate structure, the structural strength of the component is enhanced and stability.
The contact area of the fin structure and the gate structure is improved, the drain-induced band reduction and short channel effect are reduced, the structural strength and quality of the component are enhanced, and the performance and reliability of the component are improved.
Smart Images

Figure CN114744045B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a semiconductor structure, in particular to a stepped shallow trench isolation structure and a grid structure located above the structure. Background Art
[0002] As semiconductor components are developed towards high density, the size of components within a unit area is continuously reduced. Semiconductor components are widely used in the electronics industry due to their small size, multiple functions and / or low manufacturing cost. Semiconductor components are divided into semiconductor components that store logical data, semiconductor logic components that operate and process logical data operations, or hybrid semiconductor components that have the functions of semiconductor storage components and semiconductor logic components and / or other semiconductor components.
[0003] In recent years, as the size of field effect transistors (FETs) components continues to shrink, the development of conventional planar field effect transistor components has faced process limitations. In order to overcome process limitations, replacing planar transistor components with non-planar field effect transistor components, such as fin field effect transistor (Fin FET) components, has become the current mainstream development trend. Since the three-dimensional structure of the fin field effect transistor component can increase the contact area between the gate and the fin structure, the gate's control over the carrier channel region can be further increased, thereby reducing the drain induced barrier lowering (DIBL) effect faced by small-sized components and suppressing the short channel effect (SCE). Furthermore, since the fin field effect transistor component has a wider channel width at the same gate length, a doubled drain drive current can be obtained. Even more, the threshold voltage of the transistor component can be regulated by adjusting the work function of the gate. Summary of the invention
[0004] The present invention discloses a semiconductor structure, comprising a substrate, a fin-shaped structure on the substrate, a shallow trench isolation structure located in the substrate, wherein the shallow trench isolation structure has a stepped top surface, and has a first top surface and a second top surface higher than the first top surface, and a gate structure spanning part of the shallow trench isolation structure and part of the fin-shaped structure, wherein the gate structure has a stepped bottom surface.
[0005] Optionally, the second top surface is lower than a top surface of the fin-shaped structure.
[0006] Optionally, the gate structure includes a liner layer, a conductive layer and a mask layer stacked in sequence from bottom to top.
[0007] Optionally, from the cross-sectional view, the cushion layer has a stepped cross-sectional structure, and the stepped cross-sectional structure has three different levels.
[0008] Optionally, a bottom surface of the conductive layer is lower than a top surface of the fin-shaped structure.
[0009] Optionally, the hard mask layer of the gate structure includes a stepped top surface.
[0010] Optionally, the lowest bottom surface of the gate structure is flush with the first top surface of the shallow trench isolation structure.
[0011] Optionally, it further includes a second gate structure located on the substrate, wherein the second gate structure is not located above the shallow trench isolation structure.
[0012] Optionally, the second gate structure has a flat top surface.
[0013] The present invention is characterized in that the etching parameters when making the shallow trench isolation structure are adjusted to form a shallow trench isolation structure with a stepped cross-section structure. The applicant has found that the stepped shallow trench isolation structure has a higher structural strength and is easy to form a dummy gate structure on the boundary between the shallow trench isolation structure and the fin structure. When the dummy gate structure is subsequently formed on the stepped top surface, the fin structure itself and the gate structure can be protected, thereby improving the quality of the component. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:
[0015] Figures 1 to 3 A schematic diagram of steps for forming a semiconductor structure in a preferred embodiment of the present invention is shown.
[0016] Figure 4 A schematic diagram of a semiconductor structure according to another preferred embodiment of the present invention is shown.
[0017] The above drawings include the following reference numerals:
[0018] 100 Substrate
[0019] 101 Fin Structure
[0020] 102 Ditch
[0021] 104 Insulation layer
[0022] 105 cushion layer
[0023] 106 Shallow Trench Isolation Structure
[0024] 110 Patterned Shielding
[0025] 111 Silicon oxide layer
[0026] 112 Silicon nitride layer
[0027] 113 Silicon oxide layer
[0028] 120 Dummy gate structure
[0029] 121 gate dielectric layer
[0030] 122 gate conductive layer
[0031] 123 Mask layer
[0032] 124 gap wall
[0033] 130 Gate structure
[0034] 131 gate dielectric layer
[0035] 132 gate conductive layer
[0036] 133 Mask layer
[0037] 134 gap wall
[0038] S1 Top
[0039] S2 Top
[0040] S3 Top DETAILED DESCRIPTION
[0041] The following has disclosed enough details to enable those skilled in the art to implement the invention. Furthermore, some object structures and operation processes well known to those skilled in the art will not be described in detail. Of course, other embodiments may also be applied to the present invention, or any structural, logical and electrical changes may be made without departing from the embodiments described herein.
[0042] Likewise, the embodiments of the drawings are only for illustration and are not drawn completely to scale for the purpose of clearly describing some details. In addition, for the sake of simplicity and clarity, when multiple embodiments have partially similar features, these similar features will be represented by the same substantial mark.
[0043] Please refer to Figures 1 to 3 , which is a schematic diagram of the steps of forming a semiconductor structure in a preferred embodiment of the present invention. First, Figure 1As shown, a substrate 100 is provided. The substrate 100 is, for example, a semiconductor substrate such as a silicon substrate, a silicon-containing substrate or a silicon-on-insulator (SOI) substrate. The substrate 100 is formed with at least one fin structure 101. In the implementation of the bulk silicon process, the fin structure 101 is preferably formed by using a sidewall image transfer (SIT) technology, including forming a plurality of patterned sacrificial layers (not shown) on the substrate 100 through a lithography and etching process, and sequentially performing deposition and etching processes to form a spacer (not shown) on the sidewall of each of the patterned sacrificial layers. Subsequently, the patterned sacrificial layers are removed, and an etching process is performed through the coverage of the spacer so that the pattern of the spacer is transferred to a patterned mask 110 of a single-layer or multi-layer structure, for example, a composite structure consisting of a silicon oxide layer 111, a silicon nitride layer 112 and a silicon oxide layer 113. Afterwards, an etching process is performed to transfer the pattern of the patterned mask 110 to the substrate 100 below to form a plurality of trenches 102 and define each fin structure 101. In addition, in another embodiment, a fin structure cutting process (fin cutting) can also be performed to form the desired fin structure 101, such as fin structures 101 in parallel strips.
[0044] In another embodiment, the fin structure 101 may be formed by first forming a patterned hard mask layer (not shown) on the substrate 100, and then using an epitaxial process to grow a semiconductor layer (not shown) such as silicon or silicon germanium on the substrate 100 exposed outside the patterned mask layer to serve as the corresponding fin structure. Alternatively, in other embodiments such as those including a silicon-on-insulator substrate (not shown), a semiconductor layer (not shown) of the substrate 100 may be etched using the patterned mask 110, and the etching may stop at a bottom oxide layer (not shown) below the semiconductor layer to form the fin structures.
[0045] Then, if Figure 2As shown, an insulating material layer (not shown) is formed on the substrate 100 in an all-round manner, preferably by using a flowable chemical vapor deposition (FCVD) process, followed by chemical mechanical polishing (CMP) and etch-back processes, to form an insulating layer 104, such as silicon oxide, in the trench 102. It is worth noting that in the above-mentioned manufacturing process, since the recess 102 occupies a larger area on the entire substrate 100, after the insulating layer 104 is filled into the recess 102, it undergoes CMP and etch-back, which will cause the insulating layer 104 near the central part of the recess 102 to be etched faster, while the insulating layer 104 located in the recess 102 near the fin structure 101 is etched at a slower rate, which easily causes the top surface of the insulating layer 104 in the center of the recess 102 to be lower than the top surface of the surrounding insulating layer 104. The above phenomenon can also be called a dishing phenomenon.
[0046] In this preferred embodiment, the process etching parameters are adjusted to etch the insulating layer 104 in the groove 102 to form a Figure 2 A shallow trench isolation (STI) structure 106 having a stepped top surface is shown. It is noteworthy that the shallow trench isolation structure 106 in this embodiment has two top surfaces of different heights, which are defined as top surface S1 and top surface S2, respectively, wherein top surface S1 is lower than top surface S2, and preferably, top surface S1 and top surface S2 are both horizontal surfaces. Therefore, the shallow trench isolation structure 106 of this preferred embodiment has a stepped top surface. In addition, the top surface of the fin-like structure 101 can be defined as top surface S3, and in this embodiment, top surface S1 and top surface S2 are both lower than top surface S3. Therefore, a stepped area is formed in the area near the edge of the shallow trench isolation structure 106 and the fin-like structure 101, and the stepped area has at least three horizontal surfaces of different heights (i.e., top surface S1, top surface S2, and top surface S3).
[0047] According to the experimental results of the applicant, the shallow trench isolation structure generally produced by the concave phenomenon usually has an arc-shaped concave top surface, and in the preferred embodiment, the etching parameters are deliberately adjusted so that the surface of the shallow trench isolation structure has a step shape, and the angle of each step-shaped plane portion is close to the horizontal (that is, the top surface S1 and the top surface S2 are substantially parallel to the horizontal plane), and there may be a vertical or inclined side between the two top surfaces S1 and S2. In addition to adjusting the etching parameters as mentioned above, the actual manufacturing method can also achieve a shallow trench isolation structure with a stepped top surface by performing back etching multiple times, which will not be elaborated here.
[0048] It should be noted that in one embodiment, when performing chemical mechanical polishing and etching back processes, part of the patterned mask 110 (for example, the silicon nitride layer 112 and the silicon oxide layer 113) may be selectively removed in response to different structural characteristics such as the subsequent formation of a tri-gate transistor component or a dual-gate fin transistor component, but the present invention is not limited thereto. In other embodiments, the patterned mask 110 may also be completely retained or completely removed. In addition, in another embodiment, a dielectric layer may be further formed before forming the insulating layer 104 to serve as a liner 105 to cover the substrate 100 and the fin structure 101. The liner 105 is, for example, a single-layer or multi-layer structure, preferably a dielectric material such as silicon oxide or a suitable high dielectric constant material. The formation method of the liner 105 includes, for example, utilizing an in-situ vapor generation (ISSG) technique to form a liner 105 evenly distributed on the surface of the fin structure 101 and the trench 102, such as Figure 2 In other embodiments, the liner layer 105 may also be formed by an atomic layer deposition (ALD) process, or may include other dielectric materials.
[0049] Then, Figure 3 As shown, after completely removing the patterned mask 110 (silicon oxide layer 111), at least one dummy gate structure 120 across the fin structure 101 and a gate structure 130 located on the fin structure 101 are formed. In the present embodiment, the process of forming the dummy gate structure 120 can be integrated with a commonly used gate process. For example, a gate process can be performed to sequentially form a gate dielectric material layer (not shown), such as an insulating material including silicon oxide, and a gate layer (not shown) on the fin structure 101, and then pattern the gate layer and the gate dielectric material layer to form a gate structure 130 on the fin structure 101. Figure 3 The plurality of gate structures 130 shown include a gate dielectric layer 131, a gate conductive layer 132, and a mask layer 133. The dummy gate structure 120 includes a gate dielectric layer 121, a gate conductive layer 122, and a mask layer 123. In one embodiment, the gate conductive layer 122 of the dummy gate structure 120 is, for example, a polysilicon gate, but its material is not limited thereto and can be determined according to actual needs. Subsequently, spacers 124 and 134 surrounding the dummy gate structure 120 and the gate structure 130 can be formed, wherein the spacers 124 and 134 are, for example, made of materials such as silicon nitride, silicon oxynitride, or silicon carbonitride.
[0050] It is worth mentioning that, because the shallow trench isolation structure 106 has a stepped top surface (the above-mentioned top surface S1 and top surface S2), when the dummy gate structure 120 is completed, because it spans over the stepped area, the dummy gate structure 120 will also present a stepped structure when observed from the cross-sectional view. For example, the dummy gate structure 120 spans over the top surface S1, the top surface S2 and the top surface S3, so the dummy gate structure 120 has a stepped bottom surface and a stepped top surface. A detailed observation includes a stepped gate dielectric layer 121, a stepped gate conductive layer 122 and a stepped mask layer 123, wherein the cross-sectional structures of the above-mentioned gate dielectric layer 121, the gate conductive layer 122 and the mask layer 123 all have three different levels. As shown in FIG. Figure 3 As shown, the bottom surface of the gate conductive layer 122 (level with the top surface S1) is lower than the top surface of the fin structure 101 (i.e., the top surface S3), and the lowest bottom surface of the dummy gate structure 120 is level with the top surface S1 of the shallow trench isolation structure 106. The applicant has found that the dummy gate structure 120 has a stepped bottom surface, which can be stably combined with the stepped top surface of the shallow trench isolation structure 106, thereby strengthening the structural strength of the device in this area and protecting the surrounding fin structure 101 and the gate structure 130 formed above the fin structure 101.
[0051] On the other hand, in this preferred embodiment, the gate structure 130 is completely located above the fin structure 101, but not on the shallow trench isolation structure 106, and therefore does not cover the stepped region. Therefore, the gate structure 130 has a flat bottom surface and a flat top surface.
[0052] like Figure 3 As shown, the dummy gate structure 120 of the present embodiment partially covers the fin structure 101. In other words, the dummy gate structure 120 and the spacer 134 are used to cover the edge of the fin structure 101 after etching, so as to prevent the fin structure 101 from being affected by subsequent processes, such as the source / drain epitaxial growth process, which may cause structural deformation, leakage current or damage to the overall electrical performance.
[0053] The following will describe different implementations of the semiconductor structure of the present invention, and for simplicity, the following description will mainly describe the differences between the embodiments, and will not repeat the same parts. In addition, the same components in the embodiments of the present invention are marked with the same reference numerals to facilitate comparison between the embodiments.
[0054] Figure 4 A schematic diagram of a semiconductor structure of another preferred embodiment of the present invention is shown. Figure 4As shown, the position of the dummy gate structure 120 can be adjusted. In the preferred embodiment, the spacer 124 of the dummy gate structure 120 is located above the junction of the insulating layer 104 of the shallow trench isolation structure 106 and the fin structure 101. In the preferred embodiment, the spacer 124 is still located on the fin structure 101 (the spacer 124 does not cross over the insulating layer 104), but in other preferred embodiments of the present invention, the spacer 124 may cross over the fin structure 101 and the insulating layer 104 at the same time, which also falls within the scope of the present invention.
[0055] In summary, the present invention is characterized in that the etching parameters when making the shallow trench isolation structure are adjusted to form a shallow trench isolation structure with a stepped cross-section structure. The applicant has found that the stepped shallow trench isolation structure has a higher structural strength and is easy to form a dummy gate structure on the boundary between the shallow trench isolation structure and the fin structure. When the dummy gate structure 120 is subsequently formed on the stepped top surface, the fin structure itself and the gate structure can be protected, thereby improving the quality of the component.
[0056] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A semiconductor structure, characterized in that: include: A substrate having a fin structure thereon; A shallow trench isolation structure is located in the substrate, wherein the shallow trench isolation structure has a stepped top surface, and has a first top surface and a second top surface higher than the first top surface; as well as A gate structure spans part of the shallow trench isolation structure and part of the fin structure, wherein the gate structure has a stepped bottom surface, and the gate structure further includes a gate conductive layer and a spacer, the spacer is located on both sides of the gate conductive layer, and the bottom surfaces of the spacer located on both sides of the gate conductive layer are not at the same height.
2. The semiconductor structure according to claim 1, characterized in that The second top surface of the shallow trench isolation structure is lower than the top surface of the fin structure.
3. The semiconductor structure according to claim 1, characterized in that: The gate structure includes a liner layer, a conductive layer and a mask layer which are sequentially stacked from bottom to top.
4. The semiconductor structure according to claim 3, characterized in that: From the cross-sectional view, the liner layer has a stepped cross-sectional structure, and the stepped cross-sectional structure has three different levels.
5. The semiconductor structure according to claim 3, characterized in that: The bottom surface of the conductive layer is lower than the top surface of the fin structure.
6. The semiconductor structure according to claim 3, characterized in that: The mask layer of the gate structure includes a stepped top surface.
7. The semiconductor structure according to claim 1, characterized in that: The lowest bottom surface of the gate structure is flush with the first top surface of the shallow trench isolation structure.
8. The semiconductor structure according to claim 1, characterized in that: The semiconductor structure further includes a second gate structure located on the substrate, wherein the second gate structure is not located above the shallow trench isolation structure.
9. The semiconductor structure according to claim 8, characterized in that: The second gate structure has a flat top surface.
10. The semiconductor structure according to claim 1, wherein: The spacer is located at the junction of the shallow trench isolation structure and the fin structure.
11. The semiconductor structure according to claim 1, characterized in that: The semiconductor structure further includes an insulating layer, and the insulating layer is located on both sides of the fin structure.
12. The semiconductor structure according to claim 11, characterized in that: The spacers include a first spacer and a second spacer located on both sides of the gate conductive layer, the first spacer is located above the fin structure, and the second spacer is located above the insulating layer.
13. The semiconductor structure according to claim 11, characterized in that: The spacers include a first spacer and a second spacer located at both sides of the gate conductive layer, the bottom surface of the first spacer contacts the fin structure, and the bottom surface of the second spacer contacts the insulating layer.
14. The semiconductor structure according to claim 12, characterized in that: A bottom surface of the first spacer is higher than a bottom surface of the second spacer.
Citation Information
Patent Citations
Method of forming integrated circuit structure
CN102054741A
Semiconductor element and manufacturing method thereof
CN106711213A
Semiconductor structure and method of making the same
CN107689394A
Semiconductor device and method for fabricating the same
US9455227B1