Blade wear-resistant layer laser cladding device and method

The wear-resistant layer of the blade is formed through laser cladding technology, which solves the problem of unstable quality of the wear-resistant layer in the existing technology, improves the consistency and processing efficiency of the blade, and is suitable for mass production.

CN115595576BActive Publication Date: 2024-10-29AVIC BEIJING INST OF AERONAUTICAL MATERIALS
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211278585.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-10-19
Publication Date
2024-10-29
Estimated Expiration
2042-10-19

AI Technical Summary

Technical Problem

In the existing technology, the wear-resistant layer of low-pressure turbine working blades often suffers from quality problems such as shedding, falling pieces, and mutual adhesion during machining, commissioning, and flight testing, resulting in poor consistency of the blades and making them unsuitable for batch production.

Method used

Laser cladding technology is used to laser clad the wear-resistant layer of the blade through a device composed of a laser and a powder feeder. High-energy laser beams and cladding powder are used to form a strong metallurgical bonding layer to improve the hardness and wear resistance of the blade.

Benefits of technology

It significantly improves the uniformity of the structure of the blade's wear-resistant layer and the bonding strength of the weld, reduces the impact of the welder's operating proficiency, improves the consistency and processing efficiency of the blade, and is suitable for batch processing and manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115595576B_ABST
    Figure CN115595576B_ABST
Patent Text Reader

Abstract

The present invention discloses a blade wear-resistant layer laser cladding device and method. The blade wear-resistant layer laser cladding device comprises a laser; a powder feeder for storing and conveying cladding powder; a cladding head connected to the laser through an optical fiber and connected to the powder feeder through a pipeline; and a positioning mechanism for positioning the blade to be clad. The blade wear-resistant layer laser cladding device uses laser cladding instead of manual argon arc welding for wear-resistant layer surfacing, so that the wear-resistant layer has uniform structure and high weld bonding strength. Compared with the traditional method of cladding the blade wear-resistant layer by manual argon arc welding, it reduces the large difference in the uniformity of the wear-resistant layer structure and the weld bonding strength caused by the different operating proficiency of the welder, improves the consistency of the blade wear-resistant layer, and improves the consistency of the low-pressure turbine working blade.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of laser cladding of blade wear-resistant layers, and in particular to a device and method for laser cladding of blade wear-resistant layers. Background Art

[0002] In the prior art, the first-stage working blades of the low-pressure turbine of the engine are usually formed by precision casting of DD6 single crystal material, and the blade crown is a Z-shaped tooth structure (such as the attached Figure 1 As shown in the figure). The turbine blades of the engine work in a high-temperature gas environment and under fatigue vibration conditions. Each blade is inserted into the tenon groove of the turbine disc in a tenon-tooth manner, and the serrated crowns mesh with each other to form an outer ring of the wheel rim. During flight, the blade crowns collide with each other, and the damping surface is worn. Under the action of high-temperature environment and high-pressure gas, the blade root bending moment increases, causing cracks at the blade root and blade breakage accidents.

[0003] Therefore, a wear-resistant layer is usually added to the blade crown to increase the service life of the blade. However, during machining, test runs and test flights, the wear-resistant layer often falls off, blocks fall off and sticks to each other, making it unsuitable for batch production.

[0004] At present, the wear-resistant layer is usually clad by manual argon arc welding in China. The cladding quality of the wear-resistant layer depends on the operator's proficiency. The uniformity of the structure and the weld strength of the wear-resistant layer processed by different welders vary greatly, resulting in poor consistency of the blades.

[0005] Therefore, how to improve the consistency of low-pressure turbine working blades is a technical problem that technical personnel in this field currently need to solve. Summary of the invention

[0006] In view of this, an object of the present invention is to provide a blade wear-resistant layer laser cladding device to improve the consistency of the blade.

[0007] In order to achieve the above object, the present invention provides the following technical solutions:

[0008] A blade wear-resistant layer laser cladding device, comprising:

[0009] Lasers;

[0010] A powder feeder, used to store and transport cladding powder;

[0011] a cladding head connected to the laser through an optical fiber and connected to the powder feeder through a pipeline; and

[0012] The positioning mechanism is used to position the blade to be clad.

[0013] Optionally, in the above-mentioned blade wear-resistant layer laser cladding device, it also includes a mechanical arm and a controller, the cladding head is arranged on the mechanical arm, and the laser, the powder feeder and the mechanical arm are all electrically connected to the controller.

[0014] Optionally, the above-mentioned blade wear-resistant layer laser cladding device further includes a spectrometer electrically connected to the controller and a LIBS device electrically connected to the spectrometer.

[0015] Optionally, in the above-mentioned blade wear-resistant layer laser cladding device, the positioning mechanism includes:

[0016] A fixture assembly, used for clamping and positioning the blade to be clad;

[0017] A position adjusting member, used for supporting the clamp assembly, and the position adjusting member is provided with an adjusting slide groove;

[0018] The clamping member is used to clamp and fix the clamp assembly on the position adjusting member, and the clamping member is slidably connected to the adjusting sliding groove.

[0019] Optionally, in the above-mentioned blade wear-resistant layer laser cladding device, the fixture assembly includes:

[0020] A first positioning block, provided with a first positioning groove matching the blade root of the blade to be clad;

[0021] A second positioning block is provided with a second positioning groove matching the blade crown of the blade to be clad;

[0022] The auxiliary positioning plate is arranged on the second positioning block, and is used for abutting against the blade crown of the blade to be clad, so as to limit the relative position of the blade crown of the blade to be clad in the second positioning groove.

[0023] Optionally, in the above-mentioned blade wear-resistant layer laser cladding device, the auxiliary positioning plate is rotatably disposed on the second positioning block, and an elastic reset element is disposed between the auxiliary positioning plate and the second positioning block.

[0024] Optionally, in the above-mentioned blade wear-resistant layer laser cladding device, the second positioning block is further provided with a clearance groove for avoiding the operating space of the cladding head.

[0025] A blade wear-resistant layer laser cladding method, using the blade wear-resistant layer laser cladding device as described above, comprises the following steps:

[0026] S1: Positioning the blade to be clad by means of a positioning mechanism;

[0027] S2: preheating the to-be-clad portion of the blade by means of a cladding head;

[0028] S3: The powder feeder transmits cladding powder to the cladding head, and the laser transmits laser light to the cladding head through an optical fiber. The cladding head performs laser cladding on the to-be-clad portion of the blade.

[0029] Optionally, in the above-mentioned blade wear-resistant layer laser cladding method, in step S3, the process parameters of laser cladding are: laser power is 1000W~2000W, laser scanning speed is 300~1000mm / min, forming line energy is 1.2~2.4KJ / cm, powder feeding method is coaxial high-purity argon powder feeding, powder feeding speed is 3~12g / min, overlap rate between passes is 35~70%, argon powder feeding protection method is coaxial dual-channel high-purity argon protection: inner protection argon flow rate is 15~35L / min, outer protection argon flow rate is 0~40L / min.

[0030] Optionally, in the above-mentioned laser cladding method for the wear-resistant layer of the blade, in the step S3, the cladding powder is a cobalt-based alloy powder with a particle size of φ15 to φ300 μm, and the chemical composition and mass percentage of the cobalt-based alloy powder are C≤0.08%, Si: 3.0% to 3.8%, Cr: 16.5% to 18.5%, Mo: 27.0% to 30.0%, and the rest is Co.

[0031] When using the blade wear-resistant layer laser cladding device provided by the present invention, the blade to be clad is pre-positioned by a positioning mechanism. Since the cladding head is connected to the laser through an optical fiber and is connected to the powder feeder through a pipeline, when the blade wear-resistant layer is laser clad, first, the blade portion to be clad is preheated by the cladding head to reduce the crack tendency of the cladding portion, then, the laser is emitted by the laser and the high-energy laser beam is transmitted to the cladding head through the optical fiber, and the cladding powder is transmitted to the cladding head through the powder feeder. The high-energy laser beam transmitted to the cladding head by the laser quickly scans the blade coating, and the cladding powder melts and solidifies in an instant, and the blade base metal melts into a thin layer. The interface between the two quickly produces molecular or atomic-level cross-diffusion in a very narrow area, and at the same time forms a strong metallurgical bonding layer, that is, a wear-resistant layer, thereby significantly improving the hardness and wear resistance of the blade base.

[0032] It can be seen that the blade wear-resistant layer laser cladding device provided by the present invention adopts laser cladding instead of manual argon arc welding for wear-resistant layer surfacing, so that the wear-resistant layer has uniform structure and high weld bonding strength. On the one hand, compared with the traditional method of cladding the wear-resistant layer of the blade by manual argon arc welding, it reduces the phenomenon of large differences in the uniformity of the wear-resistant layer structure and the weld bonding strength caused by the different operating proficiency of the welders, improves the consistency of the blade wear-resistant layer, and improves the consistency of the low-pressure turbine working blade; on the other hand, it improves the cladding efficiency of the blade wear-resistant layer, so that the processing efficiency of the blade is improved, which is suitable for batch processing and manufacturing. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0034] Figure 1 It is a structural schematic diagram of a part to be clad of an existing turbine blade;

[0035] Figure 2 A schematic structural diagram of a blade wear-resistant layer laser cladding device provided by an embodiment of the present invention;

[0036] Figure 3 A schematic diagram of the structure of a positioning mechanism provided by an embodiment of the present invention;

[0037] Figure 4 A schematic structural diagram of a clamp assembly provided by an embodiment of the present invention;

[0038] Figure 5 A schematic structural diagram of a clamp assembly provided in an embodiment of the present invention for clamping a blade to be clad.

[0039] Among them, 100 is a laser, 200 is a powder feeder, 300 is a cladding head, 400 is a positioning mechanism, 401 is a fixture assembly, 4011 is a first positioning block, 4011-a is a first positioning groove, 4012 is a second positioning block, 4012-a is a second positioning groove, 4012-b is a give way groove, 4013 is an auxiliary positioning plate, 402 is a position adjustment member, 4021 is an adjustment slide groove, 403 is a clamping member, 500 is a robotic arm, 600 is a controller, 700 is a spectrometer, 800 is a LIBS device, 900 is a blade to be clad, and 901 is a part to be clad. DETAILED DESCRIPTION

[0040] In view of this, the core of the present invention is to provide a blade wear-resistant layer laser cladding device to improve the consistency of the blade.

[0041] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0042] like Figures 1 to 5As shown, an embodiment of the present invention discloses a blade wear-resistant layer laser cladding device, including a laser 100, a powder feeder 200, a cladding head 300 and a positioning mechanism 400.

[0043] The powder feeder 200 is used to store and transport cladding powder; the cladding head 300 is connected to the laser 100 via an optical fiber and is connected to the powder feeder 200 via a pipeline; the positioning mechanism 400 is used to position the blade 900 to be clad.

[0044] When using the blade wear-resistant layer laser cladding device provided by the present invention, the blade 900 to be clad is pre-positioned by the positioning mechanism 400. Since the cladding head 300 is connected to the laser 100 through an optical fiber and is connected to the powder feeder 200 through a pipeline, when the blade wear-resistant layer is laser clad, first, the blade portion 901 to be clad is preheated by the cladding head 300 to reduce the crack tendency of the cladding portion. Then, the laser 100 emits a laser and transmits a high-energy laser beam to the cladding head 300 through an optical fiber. The cladding powder is transmitted to the cladding head 300 through the powder feeder 200. The high-energy laser beam transmitted by the laser 100 to the cladding head 300 quickly scans the blade coating, and the cladding powder melts and solidifies in an instant. The blade base metal melts into a thin layer, and the interface between the two quickly produces molecular or atomic-level cross-diffusion in a very narrow area, and at the same time forms a strong metallurgical bonding layer, that is, a wear-resistant layer, thereby significantly improving the hardness and wear resistance of the blade base.

[0045] It can be seen that the blade wear-resistant layer laser cladding device provided by the present invention adopts laser cladding instead of manual argon arc welding for wear-resistant layer surfacing, so that the wear-resistant layer has uniform structure and high weld bonding strength. On the one hand, compared with the traditional method of cladding the wear-resistant layer of the blade by manual argon arc welding, it reduces the phenomenon of large differences in the uniformity of the wear-resistant layer structure and the weld bonding strength caused by the different operating proficiency of the welders, improves the consistency of the blade wear-resistant layer, and improves the consistency of the low-pressure turbine working blade; on the other hand, it improves the cladding efficiency of the blade wear-resistant layer, so that the processing efficiency of the blade is improved, which is suitable for batch processing and manufacturing.

[0046] It should be noted that the present invention does not specifically limit the above laser cladding parameters. As long as the cladding parameters that can meet the use requirements are within the protection scope of the present invention; the preferred laser cladding parameters are as follows: laser power is 1000W-2000W, laser scanning speed is 300-1000mm / min, forming line energy is 1.2-2.4KJ / cm, powder feeding method is coaxial high-purity argon powder feeding, powder feeding speed is 3-12g / min, overlap rate between passes is 35- 70%, the argon powder feeding protection mode is coaxial double-channel high-purity argon protection: the inner protection argon flow rate is 15-35L / min, and the outer protection argon flow rate is 0-40L / min; the cladding powder is a cobalt-based alloy powder with a particle size of φ15-φ300μm, and the chemical composition and mass percentage of the cobalt-based alloy powder are C≤0.08%, Si: 3.0%-3.8%, Cr: 16.5%-18.5%, Mo: 27.0%-30.0%, and the rest is Co.

[0047] In a specific embodiment of the present invention, the equipment used is Arnold 6KW three-dimensional laser processing and manufacturing system, and the set process parameters are as follows: laser power is 1100-1600W, laser scanning speed is 500-750mm / min, forming line energy is 1.3-1.8KJ / cm, powder feeding method is coaxial high-purity argon powder feeding, powder feeding speed is 3.5-6.5g / min, overlap rate between passes is 40-55%, gas protection method is coaxial double-channel high-purity argon protection: inner protection argon flow rate is 15-25L / min, outer protection argon flow rate is 0-20L / min; cladding powder is spherical cobalt-based alloy powder with a particle size of φ53-φ150μm.

[0048] In addition, the above-mentioned blade wear-resistant layer laser cladding device also includes a robot arm 500 and a controller 600. The cladding head 300 is arranged on the robot arm 500, so that the position of the cladding head 300 can be adjusted through the robot arm 500, thereby improving the flexibility of the cladding head 300; the laser 100, the powder feeder 200 and the robot arm 500 are all electrically connected to the controller 600, so that the laser 100, the powder feeder 200 and the robot arm 500 can be controlled by the controller 600, thereby improving the degree of automation of the blade wear-resistant layer laser cladding device.

[0049] It should be understood that the above-mentioned controller 600 can be a control unit integrated with the robot arm 500, or it can be a separately arranged computer or PLC controller 600 and the like. As long as it is a type that can meet the control requirements, it belongs to the protection scope of the present invention; optionally, the controller 600 provided in an embodiment of the present invention is a computer.

[0050] Furthermore, the above-mentioned blade wear-resistant layer laser cladding device also includes a spectrometer 700 electrically connected to the controller 600 and a LIBS device 800 (LIBS is the abbreviation of Laser-Induced Breakdown Spectroscopy, which refers to laser induced breakdown spectroscopy) electrically connected to the spectrometer 700, so that the LIBS device 800 uses the spectrometer 700 to analyze the emitted spectrum to identify the elemental composition in the sample, and then can perform material identification, classification, qualitative and quantitative analysis.

[0051] like Figure 3 As shown, the positioning mechanism 400 includes a clamp assembly 401, a position adjustment member 402 and a clamping member 403; wherein, the clamp assembly 401 is used to clamp and position the blade 900 to be clad, the position adjustment member 402 is used to support the clamp assembly 401, and the position adjustment member 402 is provided with an adjustment slot 4021, the clamping member 403 is used to clamp and fix the clamp assembly 401 on the position adjustment member 402, and the clamping member 403 is slidably connected to the adjustment slot 4021, so that the clamp assembly 401 is clamped on the position adjustment member 402 through the clamping member 403, when the position of the clamp assembly 401 needs to be adjusted, the clamping member 403 is slid along the adjustment slot 4021 to a preset position, and then the clamp assembly 401 is re-clamped on the position adjustment member 402 through the clamping member 403, so as to achieve the position adjustment of the clamp assembly 401.

[0052] like Figure 4 and Figure 5 As described above, the fixture assembly 401 includes a first positioning block 4011 , a second positioning block 4012 and an auxiliary positioning plate 4013 , so as to position the blade 900 to be clad by means of the first positioning block 4011 , the second positioning block 4012 and the auxiliary positioning plate 4013 .

[0053] Specifically, the first positioning block 4011 is provided with a first positioning groove 4011-a matching the blade root of the blade 900 to be clad, so as to position the blade root of the blade 900 to be clad through the first positioning groove 4011-a; the second positioning block 4012 is provided with a second positioning groove 4012-a matching the blade crown of the blade 900 to be clad, so as to position the blade crown of the blade 900 to be clad through the second positioning groove 4012-a; the auxiliary positioning plate 4013 is arranged on the second positioning block 4012 and is located on one side of the second positioning groove 4012-a, and is used to abut against the blade crown of the blade 900 to be clad, limit the relative position of the blade crown of the blade 900 to be clad in the second positioning groove 4012-a, and play a role of auxiliary positioning, thereby improving the positioning stability of the fixture assembly 401 on the blade 900 to be clad, and improving the positioning accuracy.

[0054] It should be understood that the present invention does not limit the specific shapes of the first positioning groove 4011-a and the second positioning groove 4012-a. In practical applications, the shapes of the first positioning groove 4011-a and the second positioning groove 4012-a can be adaptively modified according to the specific shapes of the blade root and the blade crown. As long as the shapes can meet the positioning requirements, they are within the protection scope of the present invention. Optionally, in the embodiment of the present invention, the first positioning groove 4011-a is a V-shaped groove, so that the blade 900 to be clad is placed in the first positioning groove. 4011-a and the second positioning groove 4012-a, the to-be-clad portion 901 of the blade 900 to be clad is in a horizontal state, and the to-be-clad portion 901 is in the optimal cladding position of the cladding head 300, which is convenient for the cladding head 300 to clad the to-be-clad portion 901. The second positioning groove 4012-a is a shape that matches the blade crown of the blade 900 to be clad, and can realize the positive and negative placement of the blade 900 to be clad on the second positioning groove 4012-a, so as to realize the positive and negative cladding of the blade 900 to be clad.

[0055] In addition, the auxiliary positioning plate 4013 can be fixedly set on the second positioning block 4012, or can be movably set on the second positioning block 4012. As long as the setting method can meet the use requirements, it belongs to the protection scope of the present invention; optionally, in an embodiment of the present invention, the auxiliary positioning plate 4013 is rotatably set on the second positioning block 4012, and an elastic reset element is provided between the auxiliary positioning plate 4013 and the second positioning block 4012, so as to apply a pulling force to the auxiliary positioning plate 4013 through the elastic reset element, so that the auxiliary positioning plate 4013 can always abut against the blade 900 to be clad, thereby improving the positioning stability of the clamp assembly 401 on the blade 900 to be clad.

[0056] It should be understood that the above-mentioned elastic reset element can be a spring or a tension rope type part, and as long as the part type can meet the use requirements, it belongs to the protection scope of the present invention; optionally, the elastic reset element provided in the embodiment of the present invention is a spring with a strong tensile deformation force.

[0057] The second positioning block 4012 provided in the embodiment of the present invention is also provided with a clearance groove 4012-b, which is used to avoid the operating space of the cladding head 300 and avoid interference with the cladding head 300. At the same time, it is convenient to dissipate the heat generated in the cladding process to the part to be clad 901 through the clearance groove 4012-b, thereby preventing the blade 900 to be clad from cracking due to overheating of the substrate, reducing the quality of the blade, and extending the service life of the blade.

[0058] In addition, an embodiment of the present invention further discloses a blade wear-resistant layer laser cladding method, using the blade wear-resistant layer laser cladding device as described above, comprising the steps of:

[0059] S1: The blade 900 to be clad is positioned by the positioning mechanism 400 to fix the blade 900 to be clad.

[0060] S2: Preheating the to-be-clad portion 901 of the blade 900 by the cladding head 300 to reduce the crack tendency of the cladding portion and reduce the generation of cracks.

[0061] S3: The powder feeder 200 transmits cladding powder to the cladding head 300, and the laser 100 transmits laser light to the cladding head 300 through an optical fiber. The cladding head 300 performs laser cladding on the portion to be clad 901 of the blade.

[0062] When using the blade wear-resistant layer laser cladding method provided by the present invention, the blade 900 to be clad is fixed in advance by the positioning mechanism 400, and the blade portion 901 to be clad is preheated by the cladding head 300 to reduce the crack tendency of the cladding portion. Then, the laser is emitted by the laser 100 and the high-energy laser beam is transmitted to the cladding head 300 by the optical fiber, and the cladding powder is transmitted to the cladding head 300 by the powder feeder 200. The high-energy laser beam transmitted by the laser 100 to the cladding head 300 quickly scans the blade coating, and the cladding powder melts and solidifies in an instant, and the blade base metal melts into a thin layer. The interface between the two quickly produces molecular or atomic-level cross-diffusion in a very narrow area, and at the same time forms a strong metallurgical bonding layer, that is, a wear-resistant layer, thereby significantly improving the hardness and wear resistance of the blade base.

[0063] It can be seen that the laser cladding method for the wear-resistant layer of the blade provided by the present invention adopts laser cladding instead of manual argon arc welding for wear-resistant layer surfacing, so that the wear-resistant layer has uniform structure and high weld bonding strength. On the one hand, compared with the traditional method of cladding the wear-resistant layer of the blade by manual argon arc welding, the phenomenon of large differences in the uniformity of the wear-resistant layer structure and the weld bonding strength caused by the different operating proficiency of the welders is reduced, the consistency of the blade wear-resistant layer is improved, and the consistency of the low-pressure turbine working blade is improved; on the other hand, the cladding efficiency of the blade wear-resistant layer is improved, so that the processing efficiency of the blade is improved, which is suitable for batch processing and manufacturing.

[0064] It should be noted that the present invention does not specifically limit the above laser cladding parameters. As long as the cladding parameters that can meet the use requirements are within the protection scope of the present invention; the preferred laser cladding parameters are as follows: laser power is 1000W-2000W, laser scanning speed is 300-1000mm / min, forming line energy is 1.2-2.4KJ / cm, powder feeding method is coaxial high-purity argon powder feeding, powder feeding speed is 3-12g / min, overlap rate between passes is 35- 70%, the argon powder feeding protection mode is coaxial double-channel high-purity argon protection: the inner protection argon flow rate is 15-35L / min, and the outer protection argon flow rate is 0-40L / min; the cladding powder is a cobalt-based alloy powder with a particle size of φ15-φ300μm, and the chemical composition and mass percentage of the cobalt-based alloy powder are C≤0.08%, Si: 3.0%-3.8%, Cr: 16.5%-18.5%, Mo: 27.0%-30.0%, and the rest is Co.

[0065] In a specific embodiment of the present invention, the equipment used is Arnold 6KW three-dimensional laser processing and manufacturing system, and the set process parameters are as follows: laser power is 1100-1600W, laser scanning speed is 500-750mm / min, forming line energy is 1.3-1.8KJ / cm, powder feeding method is coaxial high-purity argon powder feeding, powder feeding speed is 3.5-6.5g / min, overlap rate between passes is 40-55%, gas protection method is coaxial double-channel high-purity argon protection: inner protection argon flow rate is 15-25L / min, outer protection argon flow rate is 0-20L / min; cladding powder is spherical cobalt-based alloy powder with a particle size of φ53-φ150μm.

[0066] The terms "first" and "second" and the like in the specification and claims of the present invention and the above drawings are used to distinguish different objects, rather than to describe a specific order. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device including a series of steps or units is not limited to the listed steps or units, but may include steps or units that are not listed.

[0067] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A blade wear-resistant layer laser cladding device, characterized in that: include: Lasers; A powder feeder, used to store and transport cladding powder; A cladding head, connected to the laser through an optical fiber, and connected to the powder feeder through a pipeline; as well as A positioning mechanism, used for positioning the blade to be clad; The positioning mechanism comprises: A fixture assembly, used for clamping and positioning the blade to be clad; A position adjusting member, used for supporting the clamp assembly, and the position adjusting member is provided with a plurality of adjusting slots; the adjusting slots are arranged along the radial direction of the position adjusting member; A clamping member, used for clamping and fixing the clamp assembly on the position adjusting member, wherein the clamping members are multiple, and different clamping members are slidably connected to different adjusting slide grooves; The cladding head first preheats the part to be clad of the blade to reduce the crack tendency of the part to be clad; then, the laser emits laser and transmits the high-energy laser beam to the cladding head through the optical fiber, and the powder feeder transmits the cladding powder to the cladding head. The high-energy laser beam transmitted by the laser to the cladding head quickly scans the blade coating, and the cladding powder transmitted by the powder feeder to the part to be clad through the cladding head melts and solidifies in an instant, and the blade base metal melts into a thin layer, and the interface between the two quickly produces molecular or atomic-level cross-diffusion in a very narrow area, and a strong metallurgical bonding layer is formed at the same time.

2. The blade wear-resistant layer laser cladding device according to claim 1 is characterized in that: It also includes a mechanical arm and a controller, the cladding head is arranged on the mechanical arm, and the laser, the powder feeder and the mechanical arm are all electrically connected to the controller.

3. The blade wear-resistant layer laser cladding device according to claim 2 is characterized in that: Also included is a spectrometer electrically connected to the controller and a LIBS device electrically connected to the spectrometer.

4. The blade wear-resistant layer laser cladding device according to claim 1 is characterized in that: The clamp assembly comprises: A first positioning block, provided with a first positioning groove matching the blade root of the blade to be clad; A second positioning block is provided with a second positioning groove matching the blade crown of the blade to be clad; The auxiliary positioning plate is arranged on the second positioning block, and is used for abutting against the blade crown of the blade to be clad, so as to limit the relative position of the blade crown of the blade to be clad in the second positioning groove.

5. The blade wear-resistant layer laser cladding device according to claim 4 is characterized in that: The auxiliary positioning plate is rotatably arranged on the second positioning block, and an elastic reset element is arranged between the auxiliary positioning plate and the second positioning block.

6. The blade wear-resistant layer laser cladding device according to claim 4 is characterized in that: The second positioning block is also provided with a clearance groove for avoiding the operating space of the cladding head.

7. A method for laser cladding of a blade wear-resistant layer, characterized in that: The blade wear-resistant layer laser cladding device according to any one of claims 1 to 6 comprises the following steps: S1: Positioning the blade to be clad by means of a positioning mechanism; S2: preheating the to-be-clad portion of the blade by means of a cladding head; S3: The powder feeder transmits cladding powder to the cladding head, and the laser transmits laser light to the cladding head through an optical fiber. The cladding head performs laser cladding on the part to be clad of the blade, so that the part to be clad is The cladding powder melts instantly under the action of the laser and solidifies, and the blade base metal melts into a thin layer. The interface between the two rapidly produces molecular or atomic-level cross-diffusion in a very narrow area, while forming a strong metallurgical bonding layer.

8. The blade wear-resistant layer laser cladding method according to claim 7, characterized in that: In step S3, the process parameters of laser cladding are: laser power of 1000 W to 2000 W, laser scanning speed of 300 to 1000 mm / min, forming line energy of 1.2 to 2.4 KJ / cm, powder feeding method of coaxial high-purity argon powder feeding, powder feeding speed of 3 to 12 g / min, overlap rate between passes of 35 to 70%, argon powder feeding protection method of coaxial dual-channel high-purity argon protection: inner protection argon flow rate of 15 to 35 L / min, outer protection argon flow rate of 0 to 40 L / min.

9. The blade wear-resistant layer laser cladding method according to claim 7, characterized in that: In step S3, the cladding powder is a cobalt-based alloy powder with a particle size of φ15 to φ300 μm, and the chemical composition and mass percentage of the cobalt-based alloy powder are C≤0.08%, Si: 3.0% to 3.8%, Cr: 16.5% to 18.5%, Mo: 27.0% to 30.0%, and the rest is Co.

Citation Information

Patent Citations

  • Dynamic gradient cladding process and device based on plane subarea space layering

    CN108559997A

  • Surfacing tool for wear-resistant layer of blade crown of high-temperature alloy turbine blade