Salt mud neutralizer and preparation method thereof

By adjusting the pH value and filtration treatment, controlling the trace ion content, and preparing a high reaction efficiency salt sludge neutralizer, the problems of resource waste and environmental pollution in salt sludge treatment are solved, and efficient utilization and environmental protection of salt sludge are achieved.

CN115650398BActive Publication Date: 2024-11-15CHINASALT JINTAN +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211367387.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-03
Publication Date
2024-11-15
Estimated Expiration
2042-11-03

AI Technical Summary

Technical Problem

In the prior art, salt sludge treatment methods lead to waste of resources and environmental pollution, and impurity ions affect the nucleation process of calcium carbonate crystals, making it difficult to prepare high-purity and highly reactive salt sludge neutralizers.

Method used

By stirring the salt raw halogen and caustic soda, adjust the pH value, and use ceramic membrane filtration and CO2 adjustment to control the trace ion content, add excessive soda ash to react, and gradually filter and wash to prepare a salt sludge neutralizer with high reaction efficiency.

Benefits of technology

It significantly improves the neutralization efficiency of salt sludge neutralizer, reduces production costs, realizes comprehensive utilization of resources and environmental protection, and provides high-purity, high-reactive salt sludge neutralizer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115650398B_ABST
    Figure CN115650398B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of environmental protection and resource utilization of solid waste, and particularly relates to a salt mud neutralizer and a preparation method. First, salt-making brine and caustic soda are stirred and reacted at room temperature, and then the reaction system is filtered through a ceramic membrane, a small amount of CO2 is introduced into the filtrate and filtered twice through the ceramic membrane, and then the filtrate is stirred and reacted with soda ash, and the reaction system is filtered three times to obtain a filtrate as salt-making brine to an evaporation system for salt production, and the filter residue is washed and dehydrated to obtain a salt mud neutralizer. The method of the present invention removes impurities such as iron and manganese, and controls the content of magnesium ions during the impurity removal process. The trace magnesium ions present in the salt mud have an inhibitory effect on the growth of calcium carbonate crystals in the salt mud, and can reduce the particle size of calcium carbonate in the salt mud and increase the specific surface area of ​​calcium carbonate in the salt mud. The method of the present invention realizes the recycling of salt mud solid waste, turns waste into treasure, improves the neutralization efficiency of the salt mud neutralizer, and makes the salt mud easier to use for neutralization reaction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of environmental protection and solid waste resource utilization, and in particular relates to a salt mud neutralizer and a preparation method thereof. Background Art

[0002] Brine purification, also known as brine pretreatment, is one of the key processes in the vacuum salt production process. Its purpose is to remove Ca 2+ Mg 2+ , Fe 2+ , Mn 2+ The plasma is separated before entering the heating chamber.

[0003] The two-alkali method is a commonly used process in the purification of brine for salt production. The main principle is to use caustic soda (NaOH) to remove Mg in brine. 2+ , Fe 2+ , Mn 2+ , remove it by hydroxide precipitation, and use soda ash (Na2CO3) to remove the Ca 2+ Removed as CaCO3 precipitate.

[0004] The basic reaction formula of this method is as follows:

[0005] 2OH-+X 2+ →X(OH)2↓ (1)

[0006] Ca 2+ +CO3 2- →CaCO3↓ (2)

[0007] X is a divalent metal ion such as Mg, Fe, or Mn

[0008] Salt mud is the general term for various inorganic salts discharged during the brine purification process. At present, the common treatment method used by most enterprises is to landfill salt mud as waste, which not only wastes resources but also pollutes the production environment and natural environment of enterprises. The main component of two-alkali salt mud is calcium carbonate (CaCO3). Calcium carbonate (CaCO3) reacts with all strong acids to produce water and corresponding calcium salts. The calcium carbonate (CaCO3) in the two-alkali salt mud belongs to light calcium carbonate. Light calcium carbonate has a large sedimentation volume, fine particles, a rough surface, and a large specific surface area. It is very suitable as a neutralizer raw material, so it is feasible to use salt mud as an acidic waste liquid neutralizer. However, there are still some trace impurity ions in the salt mud. The presence of impurities will affect the nucleation process of calcium carbonate crystals and wrap the surface of calcium carbonate crystals, affecting the subsequent neutralization reaction application. How to balance the influence of impurities in the preparation process and produce a method for producing a salt mud neutralizer with high purity and high reactivity has become an urgent problem to be solved. Summary of the invention

[0009] In order to solve the defects existing in the related art, the present invention provides a method for preparing a salt mud neutralizer, which not only comprehensively utilizes the effective ingredients in the salt mud, but also can make full use of resources to turn waste into treasure, greatly reduce the production cost of the salt mud neutralizer, and control the content of some trace ions, which has a significant effect on improving the neutralization efficiency of the salt mud neutralizer.

[0010] To achieve the above objectives,

[0011] On the one hand, the present invention provides a method for preparing a salt mud neutralizer, wherein the method can control the content of trace ions in the salt mud neutralizer, and the method comprises the following steps:

[0012] (1) Stir the salt-making brine and caustic soda at room temperature, adjust the pH of the reaction system to 11.0-12.2, and sample the supernatant of the reaction system to detect Mg 2+ Content, control Mg 2+ The content is 10-20 mg / L, and then the reaction system is filtered once with a ceramic membrane;

[0013] (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.0-8.5, and then performing secondary filtration with a ceramic membrane;

[0014] (3) adding excess soda ash to the filtrate obtained in step (2) and stirring the mixture to react, and adjusting the pH of the reaction system to 9.5 to 10;

[0015] (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine for salt production;

[0016] (5) The filter residue salt mud obtained in step (4) is washed with washing water at a mass ratio of 1:10 to 1:15, and then dehydrated to obtain a salt mud neutralizer.

[0017] Optionally, the method further comprises transferring the refined brine for salt production obtained in step (4) to a multiple-effect evaporation system for evaporation to produce salt.

[0018] Optionally, the components of the salt mud neutralizer are respectively as follows in parts by weight:

[0019] CaCO3 96.0~98.0 parts by weight

[0020] MgCO3 0.5~1.0 parts by weight

[0021] NaCl 0.1~0.5 weight part

[0022] Na2SO4 0.1~0.2 parts by weight.

[0023] Optionally, in step (1), the salt-making brine comprises at least the following components, and the mass concentration of each component is respectively:

[0024] NaCl297~300g / L;

[0025] Ca 2+ 0.52~0.57g / L;

[0026] Mg 2+ 0.02~0.07g / L;

[0027] SO4 2- 12.0~12.2g / L.

[0028] Optionally, in step (4), the components of the obtained salt-making refined brine are respectively as follows in terms of mass concentration:

[0029] NaCl292~295g / L;

[0030] Ca 2+ 1.0~2.0mg / L;

[0031] Mg 2+ 0.5~0.8mg / L;

[0032] SO4 2- 3.5~3.8g / L.

[0033] Optionally, in step (2), the reaction time after CO2 is introduced is at least 2 hours.

[0034] Optionally, the pore size of the ceramic membrane is 30 to 50 nm.

[0035] On the other hand, the present invention provides a salt mud neutralizer, which is prepared by any of the above methods, wherein the components of the salt mud neutralizer are respectively:

[0036] CaCO3 96.0~98.0 parts by weight;

[0037] MgCO3 0.5-1.0 parts by weight;

[0038] NaCl 0.1-0.5 parts by weight;

[0039] Na2SO4 0.1~0.2 parts by weight.

[0040] On the other hand, the present invention provides a salt-making refined brine, which is prepared by any of the above methods, wherein the components in the salt-making refined brine are respectively as follows in terms of mass concentration:

[0041] NaCl292~295g / L;

[0042] Ca 2+ 1.0~2.0mg / L;

[0043] Mg 2+ 0.5~0.8mg / L;

[0044] SO4 2- 3.5~3.8g / L.

[0045] The present invention has at least the following beneficial effects:

[0046] (1) The present invention proposes for the first time to use the salt mud produced in the brine purification process of the two-alkali method to prepare a neutralizer for acid-base neutralization, comprehensive utilization of solid waste, energy conservation and emission reduction, and protection of natural resources. Due to the needs of application, the prepared salt mud neutralizer must have a relatively high reaction efficiency. The present invention puts forward higher requirements on raw materials, process conditions such as pH, moisture, and operating conditions during the preparation process.

[0047] (2) The scheme of the present invention can regulate the content of Fe, Mn, Mg and other ions, so that the main component CaCO3 in the prepared salt mud neutralizer has a small particle size, irregular morphology, and a large specific surface area, which is easier to use for neutralization reaction and improves the efficiency of neutralization reaction.

[0048] (3) The components of the product are CaCO3 and MgCO3. MgCO3 inhibits the dissolution of CaCO3 in water, which can increase the effective content of salt mud neutralizer CaCO3, increase the pH of the product reaction, and further improve the efficiency of the neutralization reaction.

[0049] (4) The process of the present invention is reasonable, easy to prepare, and the process is safe and reliable. It provides a new way to treat salt mud and solid waste, and provides experience for the solid waste treatment industry. The solid waste recycling and waste treatment are in line with the national policies on energy conservation, emission reduction, and green environmental protection. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] Figure 1 The particle size distribution diagram of the salt mud neutralizer prepared by the exemplary embodiment of the present invention and the comparative example;

[0051] Figure 2 Microscopic microscope photos of salt mud neutralizers prepared according to exemplary embodiments of the present invention and comparative examples;

[0052] Figure 3 The pH-time curves of the salt mud neutralizers prepared in the exemplary embodiments of the present invention and the comparative examples; DETAILED DESCRIPTION

[0053] The method for preparing a salt mud neutralizer according to a specific embodiment of the present invention can control the content of trace ions in the salt mud neutralizer:

[0054] (1) First, the salt-making brine and caustic soda were stirred and reacted at room temperature, the pH of the reaction system was adjusted to 11.0-12.2, and the supernatant of the reaction system was sampled and tested for Mg 2+ Content, control Mg 2+ The content is 10 to 20 mg / L, and then the reaction system is filtered once with a ceramic membrane;

[0055] (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.0-8.5, and then performing a secondary filtration with a ceramic membrane;

[0056] (3) then adding excess soda ash to the filtrate obtained in step (2) and stirring the mixture to react, and adjusting the pH of the reaction system to 9.5-10;

[0057] (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine for salt production;

[0058] (5) The filter residue salt mud obtained in step (4) is then washed with washing water at a mass ratio of 1:10 to 1:15, and then dehydrated to obtain a salt mud neutralizer.

[0059] Since the main component of salt mud is calcium carbonate, the nucleation, growth and growth rate of calcium carbonate crystals are greatly affected by internal and external factors. When using salt mud, a by-product of salt production, to prepare a neutralizer, it is necessary to fully consider the impact of the type and content of impurities in the salt mud on the main component calcium carbonate. Therefore, the impurity content can be controlled by the method provided by the present invention.

[0060] The method for preparing a salt mud neutralizer according to a specific embodiment of the present invention may further include transferring the salt-making brine obtained in step (4) to a multi-effect evaporation system for evaporation and salt production. After the reaction is completed, the salt-making brine obtained has Ca 2+ The content is controlled at ≤10mg / L, Mg 2+ The content is controlled at ≤2mg / L, and then enters the multi-effect evaporation system to evaporate and produce salt to achieve resource utilization.

[0061] The method for preparing a salt mud neutralizer according to a specific embodiment of the present invention, wherein the components of the salt mud neutralizer are, by weight, respectively:

[0062] CaCO3 96.0~98.0 parts by weight

[0063] MgCO3 0.5~1.0 parts by weight

[0064] NaCl 0.1~0.5 weight part

[0065] Na2SO4 0.1~0.2 parts by weight.

[0066] In the method for preparing a salt mud neutralizer according to a specific embodiment of the present invention, in step (1), the raw brine for salt production contains the following components, and the components are respectively, by mass concentration:

[0067] NaCl297~300g / L;

[0068] Ca 2+ 0.52~0.57g / L;

[0069] Mg 2+ 0.02~0.07g / L;

[0070] SO4 2- 12.0~12.2g / L, and a small amount of Fe and Mn impurities.

[0071] According to the precipitation equilibrium constant Ksp, the precipitation pH ranges of Fe(OH)3, Fe(OH)2, Mn(OH)2, and Mg(OH)2 are 1.5-4.1, 8.0-8.4, 7.8-10.4, and 10.4-12.4, respectively. Meanwhile, Fe(OH)3, Fe(OH)2, and Mn(OH)2 will reversely dissolve in alkaline solutions of pH≥14, pH≥13.5, and pH≥14, respectively. Therefore, in step (1), caustic soda NaOH solution is used to adjust the pH to 11.0-12.2 to ensure that the impurities of Fe(OH)3, Fe(OH)2, and Mn(OH)2 are completely precipitated. Under this pH condition, the Mg 2+ Most of it is precipitated as Mg(OH)2, and a small amount of Mg is left in the solution. 2+ .

[0072] Step (2) uses CO2 to adjust the solution pH to 8.0-8.5 in order to remove excess NaOH and allow a small amount of Mg in step (1) to 2+ The reaction produces Mg(HCO3)2 which is soluble in water.

[0073] In step (3), the soda ash reacts with the Ca 2+ The reaction generates CaCO3, and due to adsorption, Mg 2+ Will replace Ca to some extent 2+ , occupying the lattice position for normal crystal growth at the kink position, hindering the nucleus and normal growth of CaCO3, forming irregular small crystals of CaCO3. At the same time, Mg(HCO3)2 reacts with excess soda ash to generate a small amount of MgCO3. The presence of MgCO3 is due to CO3 2- The common ion effect can inhibit the dissolution of CaCO3 and play a synergistic role in the polarization of calcium ions and the increase in the pH of calcium carbonate solution.

[0074] The filter residue is washed with water to remove most of the soluble impurities, which is the salt mud neutralizer. By utilizing the characteristics of the impurities in the salt mud itself and controlling the trace ion content through pH adjustment, the synergistic effect is exerted.

[0075] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0076] Example 1

[0077] After testing, the raw halogen composition of this embodiment is calculated by mass concentration as follows: NaCl 297g / L, Ca 2+ 0.52g / L, Mg 2+ 0.05g / L, SO4 2- 12.0g / L and a small amount of Fe and Mn impurities.

[0078] (1) Stir the salt-making brine and caustic soda at room temperature, fine-tune the pH of the reaction system within the pH range of 11.0 to 12.2, and take the supernatant of the reaction system to detect Mg 2+ Content, after testing Mg 2+ The content was 10 mg / L, and then the reaction system was filtered through a ceramic membrane;

[0079] (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.0, and filtering it again with a ceramic membrane after the adjustment is completed;

[0080] (3) adding an excess of soda ash to the filtrate obtained in step (2) and stirring the mixture to react, and fine-tuning the pH of the reaction system at a pH value of 9.5 to 10;

[0081] (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine;

[0082] (5) sending the salt-making refined brine obtained in step (4) to a multi-effect evaporation system for evaporation to make salt;

[0083] (6) Add washing water in a mass ratio of 1:10 to the filter residue salt mud obtained in step (4) for washing, and dehydrate to obtain a salt mud neutralizer.

[0084] Example 2

[0085] After testing, the raw halogen composition of this embodiment is calculated by mass concentration as follows: NaCl 300g / L, Ca 2+ 0.55g / L, Mg 2+ 0.04g / L, SO4 2-12.2g / L and a small amount of Fe and Mn impurities:

[0086] (1) Stir the salt-making brine and caustic soda at room temperature, fine-tune the pH of the reaction system within the pH range of 11.0 to 12.2, and take the supernatant of the reaction system to detect Mg 2+ Content, after testing Mg 2+ The content was 15 mg / L, and then the reaction system was filtered through a ceramic membrane;

[0087] (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.5, and filtering it again with a ceramic membrane after the adjustment is completed;

[0088] (3) adding an excess of soda ash to the filtrate obtained in step (2) and stirring the mixture to react, and fine-tuning the pH of the reaction system at a pH value of 9.5 to 10;

[0089] (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine;

[0090] (5) sending the salt-making refined brine obtained in step (4) to a multi-effect evaporation system for evaporation to make salt;

[0091] (6) Add washing water with a mass ratio of 1:15 to the filter residue salt mud obtained in step (4) for washing, and dehydrate to obtain a salt mud neutralizer.

[0092] Comparative Example 1

[0093] According to Example 1, the composition of the original halogen is calculated by mass concentration as follows: NaCl 297g / L, Ca 2+ 0.52g / L, Mg 2+ 0.05g / L, SO4 2- 12.0 g / L and a small amount of Fe and Mn impurities. Step (1) Adjust the pH to alkaline, without controlling the specific value.

[0094] (1) stirring the salt-making brine and caustic soda at room temperature, reacting the caustic soda in excess until the pH of the system is alkaline, and then filtering the reaction system with a ceramic membrane;

[0095] (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.0, and filtering it again with a ceramic membrane after the adjustment is completed;

[0096] (3) adding an excess of soda ash to the filtrate obtained in step (2) and stirring the mixture to react, and fine-tuning the pH of the reaction system at a pH value of 9.5 to 10;

[0097] (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine;

[0098] (5) sending the salt-making refined brine obtained in step (4) to a multi-effect evaporation system for evaporation to make salt;

[0099] (6) Add washing water in a mass ratio of 1:10 to the filter residue salt mud obtained in step (4) for washing, and dehydrate to obtain a salt mud neutralizer.

[0100] Comparative Example 2

[0101] According to Example 2, the composition of the original halogen is calculated by mass concentration: NaCl 300g / L, Ca 2+ 0.55g / L, Mg 2+ 0.04g / L, SO4 2- 12.2 g / L and a small amount of Fe and Mn impurities. Step (2) of introducing CO2 to adjust the pH value is eliminated.

[0102] (1) Stir the salt-making brine and caustic soda at room temperature, adjust the pH of the reaction system to 12.2, and sample the supernatant of the reaction system to detect Mg 2+ Content, control Mg 2+ The content was 15 mg / L, and then the reaction system was filtered through a ceramic membrane;

[0103] (2) adding an excess of soda ash to the filtrate obtained in step (1) and stirring the mixture to react, and fine-tuning the pH of the reaction system at a pH value of 9.5 to 10;

[0104] (3) The reaction system obtained in step (2) is filtered three times with a ceramic membrane, the filter residue is salt mud, and the filtrate is refined brine.

Claims

1. A method for preparing a salt mud neutralizer, characterized in that: The method can control the content of trace ions in the salt mud neutralizer, and comprises the following steps: (1) Stir the salt-making brine and caustic soda at room temperature, adjust the pH of the reaction system to 11.0-12.2, and sample the supernatant of the reaction system to detect Mg 2+ Content, control Mg 2+ The content is 10-20 mg / L, and then the reaction system is filtered once with a ceramic membrane; The salt-making raw brine comprises at least the following components, each of which is measured by mass concentration, respectively: NaCl 297~300g / L; That 2+ 0.52~0.57g / L; Mg 2+ 0.02~0.07g / L; SO4 2- 12.0~12.2g / L; (2) passing CO2 into the filtrate obtained in step (1) to adjust the pH of the solution to 8.0-8.5, and then performing secondary filtration with a ceramic membrane; (3) adding excess soda ash to the filtrate obtained in step (2) and stirring to react, and adjusting the pH of the reaction system to 9.5-10; (4) filtering the reaction system obtained in step (3) three times with a ceramic membrane, wherein the filter residue is salt mud and the filtrate is refined brine for salt production; (5) The filter residue salt mud obtained in step (4) is washed with washing water at a mass ratio of 1:10 to 1:15, and then dehydrated to obtain a salt mud neutralizer.

2. The method for preparing a salt mud neutralizer according to claim 1, characterized in that: The method further comprises transferring the refined brine obtained in step (4) to a multiple-effect evaporation system for evaporation to produce salt.

3. The method for preparing a salt mud neutralizer according to claim 1, characterized in that: The components of the salt mud neutralizer are, by weight, respectively: CaCO3 96.0-98.0 parts by weight; MgCO3 0.5-1.0 parts by weight; NaCl 0.1-0.5 parts by weight; Na2SO4 0.1~0.2 parts by weight.

4. The method for preparing a salt mud neutralizer according to claim 3, characterized in that: In step (4), the components of the obtained salt-making refined brine are respectively as follows in terms of mass concentration: NaCl 292~295g / L; That 2+ 1.0~2.0mg / L; Mg 2+ 0.5~0.8mg / L; SO4 2- 3.5~3.8g / L。 5. The method for preparing a salt mud neutralizer according to claim 4, characterized in that: In step (2), the reaction time after CO2 is introduced is at least 2 hours.

6. The method for preparing a salt mud neutralizer according to claim 5, characterized in that: The pore size of the ceramic membrane is 30-50 nm.

7. A salt mud neutralizer, characterized in that: Prepared by the method according to any one of claims 1 to 6, the components of the salt mud neutralizer are, by weight, respectively: CaCO3 96.0-98.0 parts by weight; MgCO3 0.5-1.0 parts by weight; NaCl 0.1-0.5 parts by weight; Na2SO4 0.1~0.2 parts by weight.

8. A salt-making refined brine prepared by the method according to any one of claims 1 to 6, wherein the components in the salt-making refined brine are, by mass concentration, respectively: NaCl 292~295g / L; That 2+ 1.0~2.0mg / L; Mg 2+ 0.5~0.8mg / L; SO4 2- 3.5~3.8g / L。