A constrained geometry nitrogen-containing sidearm indene metal derivative and a synthesis method thereof

Through one-pot preparation technology, the synthesis of nitrogen-containing side-arm indecane metal catalysts is simplified, the problem of complex process and heavy metal pollution is solved, high purity and low cost production is achieved, and a variety of CGC-based production is suitable for a variety of CGC-based products. Synthesis of indene compounds.

CN115894573BActive Publication Date: 2024-11-12TIANJIN UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211411409.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-11
Publication Date
2024-11-12
Estimated Expiration
2042-11-11

AI Technical Summary

Technical Problem

The preparation process of the metallocene catalyst with nitrogen-containing side arm restricted geometric configurations is complicated in the prior art, and is prone to isomer and heavy metal contamination, and the traditional method uses heavy metal salts to cause environmental pollution.

Method used

The one-pot preparation technology is used to control the reaction sequence and conditions, and use cheap tetravalent metal salts such as TiCl4 and ZrCl4 to avoid intermediate separation, simplify the process, improve product purity, reduce equipment investment, and eliminate heavy metal pollution.

Benefits of technology

It has achieved simplified processes, improved product purity, reduced equipment investment, avoided heavy metal pollution, and has good atomic economy and green chemical properties. It is suitable for the synthesis of a variety of CGC indene compounds.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115894573B_ABST
    Figure CN115894573B_ABST
Patent Text Reader

Abstract

The present invention proposes a restricted geometry nitrogen-containing sidearm indene metal derivative and a synthesis method thereof, belonging to the technical field of olefin polymerization catalysts. The synthesis method comprises the following steps: 1) under the protection of an inert gas, in a first solvent, a lithium salt of a compound having a structure shown in formula (I-1) is reacted with a compound having a structure shown in formula (I-2) to obtain a reaction solution containing a compound having a structure shown in formula (II-1); 2) after adding a lithium salt of a compound having a structure shown in formula (II-2) to the reaction solution obtained in step 1), an alkyl lithium is added to react, and a reaction solution containing a double lithium salt of a compound having a structure shown in formula (III-1) is obtained; 3) a metal salt is added to the reaction solution obtained in step 2), and a second solvent is added at the same time, and the reaction is performed to obtain an indene metal compound having a structure shown in formula (III-2); the process effectively simplifies the reaction process and improves the purity of the product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to olefin polymerization catalysts, and in particular relates to a restricted geometry nitrogen-containing side arm indene metal derivative and a synthesis method thereof. Background Art

[0002] Polyolefin resins are widely used in various fields of daily life and industrial production. As an organic material, it has the advantages of strong corrosion resistance, stable structural performance, and easy processing. At present, my country's demand for polyolefin resin products is very huge and increasing every year. Industrial production is also facing the process transformation from traditional ZN catalytic olefin polymerization technology to metallocene catalytic olefin polymerization technology.

[0003] Compared with ZN catalysts, metallocene catalysts have the advantages of single active center, high catalytic activity, narrow polymer molecular weight distribution, good copolymerization performance, etc. In the development process of metallocene catalysts, they have experienced various classic configurations such as non-bridged dimetallocene, bridged dimetallocene, single metallocene and constrained geometry (CGC) metallocene catalysts.

[0004] Among them, the typical CGC metallocene has excellent performance in catalyzing ethylene homopolymerization and copolymerization. Metallocene catalysts have also developed from traditional cyclopentadiene derivatives to indene and fluorene derivatives. Dow and Exxon were the first to develop the production technology of CGC metallocene and catalytic olefin polymerization. For example, in 2112, Jerzy K (Jerzy K, Nickias PN, Jorge S, et al. Substituted group 4 metal complexes, catalysts and olefin polymerization process:, EP1253158A1[P].2112.); (J Klosin, WJ Kruper, PN Nickias, JT patton, DR Wilson. 3-heteroatom substituted cyclopentadienyl-containing metal complexes and olefin polymerization Process:, TW455595B[P].2111) team reported the synthesis method of restricted geometry nitrogen-containing sidearm single metallocene catalyst, and used it in the polymerization reaction of ethylene and α-olefin, and obtained good polymerization results.

[0005] However, the above reaction conditions are relatively harsh, the preparation process is relatively complicated, and the heavy metal salt PbCl 2The use of oxidized trivalent titanium compounds and heavy metal lead salts will pollute the environment. In addition, when synthesizing large sterically hindered carbonyl ligands (such as aromatic substitution), the intermediates are prone to produce isomers, and there are certain difficulties in purifying the ligands. Summary of the invention

[0006] The invention provides a method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative. By controlling the reaction sequence and reaction conditions of various raw materials, etc., an in-situ preparation process and a one-pot reaction of metal salts such as zirconium and titanium are adopted to synthesize the constrained geometry nitrogen-containing sidearm indene metal derivative, thereby effectively simplifying the reaction process and improving the purity of the product.

[0007] The present invention provides a method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps:

[0008] 1) Under the protection of an inert gas, in a first solvent, reacting a lithium salt of a compound having a structure represented by formula (I-1) with a compound having a structure represented by formula (I-2) to obtain a reaction solution containing a compound having a structure represented by formula (II-1);

[0009] 2) adding a lithium salt of a compound having a structure represented by formula (II-2) to the reaction solution obtained in step 1) to react, thereby obtaining a reaction solution containing a compound having a structure represented by formula (III-1), and adding alkyl lithium to react, thereby obtaining a reaction solution containing a dilithium salt of a compound having a structure represented by formula (III-1);

[0010] 3) adding a metal salt to the reaction solution obtained in step 2) and simultaneously adding a second solvent to react to obtain an indene metal compound having a structure represented by formula (III-2);

[0011]

[0012] in,

[0013] R 1 are independently selected from nitrogen-containing groups, R 2 Independently selected from hydrogen, methyl;

[0014] R 3 , R 4 are independently selected from substituted or unsubstituted alkyl, substituted or unsubstituted aryl;

[0015] R 5 Independently selected from substituted or unsubstituted alkyl, aryl;

[0016] M is independently selected from titanium, zirconium and hafnium.

[0017] Furthermore, R 1 Independently selected from nitrogen-containing alkyl groups or aromatic amine groups.

[0018] Furthermore, the metal salt includes tetrachlorobis(tetrahydrofuran)titanium, zirconium tetrachloride or hafnium tetrachloride.

[0019] Furthermore, the molar ratio of the lithium salt of the compound having the structure represented by formula (I-1) to the compound having the structure represented by formula (I-2) is 1:1-5.

[0020] Furthermore, the molar ratio of the compound having the structure represented by formula (II-1) to the lithium salt of the compound having the structure represented by formula (II-2) is 1:1-5;

[0021] Preferably, the molar ratio of the compound having the structure represented by formula (III-1) to the alkyl lithium is 1:2 to 2.5.

[0022] Furthermore, the molar ratio of the dilithium salt of the compound having the structure represented by formula (III-1) to the metal salt is 1:1-5.

[0023] Further, the first solvent includes at least one of aromatic hydrocarbons, ethers and alkane solvents;

[0024] Preferably, the alkane solvent includes at least one of toluene, tetrahydrofuran, diethyl ether and n-hexane;

[0025] More preferably, the alkane solvent is n-hexane;

[0026] The second solvent includes tetrahydrofuran.

[0027] Further, in step 1) and step 2), the reaction temperature is -78-100°C;

[0028] In step 3), the reaction temperature is -30-35°C.

[0029] Furthermore, the inert gas includes at least one of nitrogen, helium or argon.

[0030] The present invention also provides a restricted geometry nitrogen-containing sidearm monoindenyl metal catalyst derivative synthesized by any of the above-mentioned synthesis methods.

[0031] The present invention has the following advantages:

[0032] The production process of the restricted geometry nitrogen-containing sidearm indene metal derivative of the present invention adopts a one-pot preparation technology, has a simple route, does not require intermediate separation, effectively reduces the required equipment, reduces equipment investment, and significantly improves the purity of the obtained product. In addition, the raw materials of the production process are cheap and easy to obtain, the reaction conditions are relatively mild, the reaction stability and selectivity are good, and it has good atom economy, which complies with sustainable green chemistry. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:

[0034] Figure 1 The NMR image of the compound corresponding to the compound 4b prepared in Comparative Example 1 of the present invention;

[0035] Figure 2 The NMR image of the compound corresponding to the compound 5b prepared in Comparative Example 1 of the present invention;

[0036] Figure 3 The NMR image of the compound corresponding to compound 4b prepared in Example 2 of the present invention;

[0037] Figure 4 The NMR spectrum of the compound corresponding to compound 5b prepared in Example 2 of the present invention. DETAILED DESCRIPTION

[0038] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

[0039] In the prior art, the amine ligand of the compound having the structure shown in formula (II-2) first reacts with the compound having the structure shown in formula (I-2) with large steric hindrance, and then reacts with the compound having the structure shown in formula (I-1), which easily produces different isomers and is difficult to purify. 3 (THF) 3 After reacting with the lithium salt of the compound having the structure shown in formula (III-1), PbCl 2 Oxidation of trivalent titanium will result in incomplete oxidation, generation of by-products, and heavy metal pollution.

[0040] An embodiment of the present invention provides a method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps:

[0041] 1) Under the protection of an inert gas, in a first solvent, reacting a lithium salt of a compound having a structure represented by formula (I-1) with a compound having a structure represented by formula (I-2) to obtain a reaction solution containing a compound having a structure represented by formula (II-1);

[0042] 2) adding a lithium salt of a compound having a structure represented by formula (II-2) to the reaction solution obtained in step 1) to react, thereby obtaining a reaction solution containing a compound having a structure represented by formula (III-1), and adding alkyl lithium to react, thereby obtaining a reaction solution containing a dilithium salt of a compound having a structure represented by formula (III-1);

[0043] 3) adding a metal salt to the reaction solution obtained in step 2) and simultaneously adding a second solvent to react to obtain an indene metal compound having a structure represented by formula (III-2);

[0044]

[0045]

[0046] in,

[0047] R 1 are independently selected from nitrogen-containing groups, R 2 Independently selected from hydrogen, methyl;

[0048] R 3 , R 4 are independently selected from substituted or unsubstituted alkyl, substituted or unsubstituted aryl;

[0049] R 5 Independently selected from substituted or unsubstituted alkyl, aryl;

[0050] M is independently selected from titanium, zirconium and hafnium.

[0051] The production process of the restricted geometry nitrogen-containing sidearm indene metal derivatives proposed in the embodiment of the present invention adopts a one-pot preparation technology, does not require the separation of intermediates, can greatly reduce the required equipment, reduce equipment investment, and has certain industrial application value. In addition, the production process effectively solves the technical problem that the existing process is prone to produce isomers and other by-products, and the obtained product has a high purity.

[0052] The raw materials of the production process proposed in the embodiment of the present invention are cheap and easy to obtain, and the cheap tetravalent metal salt MCl is used. 4 (M=Ti,Zr,Hf), which has a price advantage. For example, when synthesizing indole titanium derivatives, TiCl 4 (THF) 2 TiCl 3 (THF) 3 Cheaper and no heavy metal oxidant PbCl 2 The use of it avoids the subsequent heavy metal environmental pollution problem.

[0053] The production process proposed in the embodiment of the present invention can be used for the synthesis of various CGC indene compounds and derivatives, and has good universality. The obtained CGC indene titanium compound is used in ethylene and α-olefin copolymerization experiments, and its copolymerization performance and catalyst activity are excellent.

[0054] In one embodiment of the present invention, R 1 Independently selected from nitrogen-containing alkyl groups or aromatic amine groups.

[0055] In one embodiment of the present invention, the metal salt includes tetrachlorobis(tetrahydrofuran)titanium, zirconium tetrachloride or hafnium tetrachloride.

[0056] Specifically, the metal salt also includes titanium tetrahydrofuran adduct generated in situ in the reactor.

[0057] In one embodiment of the present invention, the molar ratio of the lithium salt of the compound having the structure represented by formula (I-1) to the compound having the structure represented by formula (I-2) is 1:1-5. Preferably, the molar ratio of the lithium salt of the compound having the structure represented by formula (I-1) to the compound having the structure represented by formula (I-2) is 1:1-1.15.

[0058] In one embodiment of the present invention, the molar ratio of the compound having the structure represented by formula (II-1) to the lithium salt of the compound having the structure represented by formula (II-2) is 1:1-5. Preferably, the molar ratio of the compound having the structure represented by formula (II-1) to the lithium salt of the compound having the structure represented by formula (II-2) is 1:1-1.15.

[0059] It should be noted that since the present invention adopts a one-pot method for the reaction, the molar amount of the compound having the structure represented by formula (II-1) is calculated according to the theoretical value.

[0060] In one embodiment of the present invention, the molar ratio of the compound having the structure represented by formula (III-1) to the alkyl lithium is 1:2 to 2.5. Preferably, the molar ratio of the compound having the structure represented by formula (III-1) to the alkyl lithium is 1:2 to 2.1.

[0061] It should be noted that since the present invention adopts a one-pot method for the reaction, the molar amount of the compound having the structure represented by formula (III-1) is also calculated according to the theoretical value.

[0062] In one embodiment of the present invention, the molar ratio of the dilithium salt of the compound having the structure shown in formula (III-1) to the metal salt is 1:1-5. Preferably, the molar ratio of the dilithium salt of the compound having the structure shown in formula (III-1) to the metal salt is 1:1-1.15.

[0063] It should be noted that since the present invention adopts a one-pot method for the reaction, the molar amount of the dilithium salt of the compound having the structure represented by formula (III-1) is also calculated according to the theoretical value.

[0064] In one embodiment of the present invention, the first solvent includes at least one of aromatic hydrocarbons, ethers and alkane solvents. Preferably, the alkane solvent includes at least one of toluene, tetrahydrofuran, ether and n-hexane. More preferably, the alkane solvent is n-hexane.

[0065] In one embodiment of the present invention, the second solvent includes tetrahydrofuran. The purity of the product obtained by selecting tetrahydrofuran as the second solvent in the embodiment of the present invention is higher.

[0066] In one embodiment of the present invention, in step 1) and step 2), the reaction temperature is -78-111°C.

[0067] Preferably, in step 1) and step 2), the reaction temperature is 31-35°C.

[0068] In one embodiment of the present invention, in step 3), the reaction temperature is -31-1° C. Low temperature is more conducive to the reaction between the metal salt and the dilithium salt having the structure of the compound represented by formula (III-1).

[0069] In one embodiment of the present invention, in step 1), step 2), and step 3), the reaction time is 3-48 hours. Preferably, in step 1), step 2), and step 3), the reaction time is 6-8 hours.

[0070] In one embodiment of the present invention, the inert gas includes at least one of nitrogen, helium or argon. The synthesis method discussed in the embodiment of the present invention is sensitive to water and oxygen. The inert gas of the present invention is a gas with stable properties and does not participate in chemical reactions.

[0071] In one embodiment of the present invention, the method further comprises step 4), wherein after the reaction is completed, the solvent is removed in vacuo, the product is extracted, and the product is purified.

[0072] Specifically, step 4) is as follows: vacuumizing the reaction liquid obtained in step 3) to remove all solvents, extracting the residue with an aromatic solvent, vacuumizing again to remove the aromatic solvent, and washing the remaining solid with an alkane solvent to obtain an indene metal compound having a structure shown in formula (III-2).

[0073] An embodiment of the present invention further provides a constrained geometry nitrogen-containing sidearm monoindenyl metal catalyst derivative synthesized by any of the above-mentioned synthesis methods.

[0074] The present invention will be described in detail below with reference to embodiments.

[0075] Example 1 A synthesis of a constrained geometry nitrogen-containing sidearm monoindenyl titanium catalyst comprises the following steps:

[0076] Step 1):

[0077]

[0078] At room temperature, in a nitrogen atmosphere, compound 1a (484.3 mg, 2.61 mmol) was placed in a 111 ml eggplant-shaped bottle, 41 ml of n-hexane was added, and 2.4 M n-butyl lithium hexane solution (1.14 mL, 2.74 mmol) was added under stirring, and stirred for 6 hours to obtain a yellow precipitate 2a. 2 SiCl 2 (337.4 mg, 2.61 mmol) was slowly added dropwise to the reaction solution, and the solution changed from a yellow suspension to a brown turbid liquid. After stirring overnight, 3a was generated. After sampling, the hexane solvent was drained, and the NMR analysis results of 3a were: 1 HNMR (411 MHz, C 6 D 6 )δ7.59(t,J=7.1Hz,2H),7.23–7.12(m,2H),5.12(d,J=2.4Hz,1H),3.51(d,J=2 .1Hz,1H),3.12(t,J=6.4Hz,4H),1.54–1.45(m,5H),1.12(s,3H),-1.11(s,3H).

[0079] Step 2):

[0080]

[0081] Under nitrogen atmosphere, add equimolar lithium tert-butylamine to the hexane solution of the intermediate compound 3a in a 100 ml eggplant-shaped bottle, stir and react for 8 hours, take samples and monitor the completion of the reaction by NMR, and generate the cyclopentadienyl ligand 4a. The NMR characterization data are as follows: 1 H NMR (411 MHz, C 6 D 6 )δ7.75(t,J=6.5Hz,1H),7.66(d,J=7.1Hz,1H),7.36–7.23(m,2H),5.44(d,J=2.2Hz,1H),3.47(d,J=1. 5Hz,1H),3.29(dd,J=12.9,6.5Hz,5H),1.68–1.61(m,5H),1.17–1.19(m,9H),1.13(s,3H),1.11(s,3H).

[0082] Step 3):

[0083]

[0084] Under nitrogen atmosphere, 2.1 eq of n-butyl lithium hexane solution was added to the 100 ml hexane solution of intermediate compound 4a in an eggplant-shaped flask. After stirring overnight, a large amount of yellow precipitate 4a dilithium salt was produced. The reaction solution was cooled to -20 °C and an equimolar amount of TiCl4 (THF) 2 Solid, the color of the solution changed from yellow to dark black, slowly warmed to room temperature, stirred overnight, vacuum removed the solvent, extracted with toluene to filter out the lithium salt, vacuum distilled to remove toluene, recrystallized, washed with n-hexane to obtain a black solid 5a with a yield of 74.8%. NMR characterization is as follows: 1 H NMR (411 MHz, C 6 D 6 )δ7.38(d,J=8.8Hz,2H),6.89–6.78(m,2H),5.43(s,1H),3.33(s,2H),2.97(s,2H),1.22(s,4H),1.16(s,9H),1.42(s,3H),1.32(s,3H).

[0085] Example 2 A synthesis of a constrained geometry nitrogen-containing sidearm monoindenyl titanium catalyst comprises the following steps:

[0086] Step 1):

[0087]

[0088] At room temperature, in a nitrogen atmosphere, compound 1a (411 mg, 2.1 mmol) was placed in a 111 mL eggplant-shaped bottle, 41 ml of n-hexane was added, and 2.4 M n-butyl lithium hexane solution (1.92 mL, 2.215 mmol) was added under stirring, and stirred for 6 hours to obtain a yellow precipitate 2a. 2 SiCl 2 (337.4 mg, 2.61 mmol) was slowly added dropwise to the reaction solution, and the solution changed from a yellow suspension to a brown turbid liquid. After stirring overnight, 3b was generated. After sampling, the hexane solvent was drained. The NMR characterization of 3b was 1 H NMR (411 MHz, CDCl 3 )δ7.49(dd,J=11.4,7.4Hz,3H),7.45–7.37(m,3H),7.35(d,J=7.2Hz,2H),7.35 (d,J=7.2Hz,2H),7.31(s,2H),7.32–7.24(m,2H),7.29–7.17(m,3H),7.24–7.1 8(m,1H),7.11(t,J=7.4Hz,1H),7.11(t,J=7.4Hz,1H),5.21(d,J=2.1Hz,1H),4 .17(s,1H),3.31(dd,J=14.4,6.5Hz,2H),3.22–3.19(m,2H),1.95–1.78(m,4H).

[0089] Step 2):

[0090]

[0091] Under nitrogen atmosphere, an equal amount of lithium tert-butylamine was added to a 100 ml eggplant-shaped bottle containing the generated compound intermediate 3b in hexane solution, and the mixture was stirred for 6 hours. The reaction was completed by sampling and NMR monitoring to generate the cyclopentadienyl ligand 4b. The NMR image of the obtained product is shown in Figure 3 As shown, the NMR characterization data are as follows: 1 H NMR (411 MHz, C 6 D 6 )δ7.71(dd,J=6.4,2.9Hz,2H),7.63–7.48(m,5H),7.19(dd,J=7.4,4.6Hz,4H),7.15–7.17(m,5H),5.47(d,J=2.1H z,1H),4.15(d,J=1.2Hz,1H),3.11(q,J=7.1Hz,2H),3.11–2.89(m,2H),1.54(dd,J=12.8,5.8Hz,4H),1.18(s,9H).

[0092] Step 3):

[0093]

[0094] Under nitrogen atmosphere, add 2.1 times the amount of n-butyl lithium hexane solution to the 100 ml eggplant-shaped bottle containing the generated compound intermediate 4b. After stirring overnight, a large amount of yellow precipitate 4b dilithium salt is generated. The reaction solution is cooled to -20 °C and an equimolar amount of TiCl 4 (THF) 2 Solid, the color of the solution changed from yellow to dark black, slowly warmed to room temperature, stirred overnight, vacuum removed the solvent, extracted with toluene to filter out the lithium salt, vacuum distilled to remove toluene, recrystallized, washed with n-hexane to obtain a black solid 5b with a yield of 75%. The NMR image of the obtained product is as follows Figure 4 As shown, the NMR characterization is as follows: 1 H NMR (411 MHz, C 6 D 6 )δ8.11(ddd,J=9.4,7.6,2.7Hz,4H),7.58(d,J=8.7Hz,1H),7.41–7.24(m,7H),7.18–6.99( m,1H),6.89–6.79(m,1H),5.91(s,1H),3.51(s,2H),3.11(s,2H),1.61(s,9H),1.41(s,4H).

[0095] Example 3A synthesis of a constrained geometry nitrogen-containing sidearm monoindenyl titanium catalyst comprises the following steps:

[0096] Step 1):

[0097]

[0098] At room temperature, in a nitrogen atmosphere, compound 1a (511 mg, 2.62 mmol) was placed in a 100 mL eggplant-shaped bottle, 61 ml of n-hexane was added, and 2.5 M n-butyl lithium hexane solution (1.11 mL, 2.75 mmol) was added under stirring, and stirred for 6 hours to obtain a yellow precipitate 2a. 2 SiCl 2 (372.3 mg, 2.88 mmol) was slowly added dropwise to the reaction solution, and the solution changed from a yellow suspension to a brown turbid liquid. After stirring overnight, 3b was generated. After sampling, the hexane solvent was drained. The nuclear magnetic resonance characterization of 3b was 1H NMR (411 MHz, CDCl3) δ7.49 (dd, J = 11.4, 7.4 Hz, 3H), 7.45–7.37 (m, 3H), 7.35 (d, J = 7.2 Hz, 2H), 7.35 (d, J = 7.2 Hz, 2H), 7.31 (s, 2H), 7.32–7.24 (m, 2H), 7.29–7.17 (m, 3H), 7.24–7.18(m,1H),7.11(t,J=7.4Hz,1H),7.11(t,J=7.4Hz,1H),5.21(d,J=2.1Hz,1 H),4.17(s,1H),3.31(dd,J=14.4,6.5Hz,2H),3.22–3.19(m,2H),1.95–1.78(m,4H).

[0099] Step 2):

[0100]

[0101] Under nitrogen atmosphere, an equal mole of lithium cyclopentylamine was added to the hexane solution of the intermediate compound 3b in a 111 mL eggplant-shaped bottle, and the mixture was stirred for 8 hours. The reaction was completed by sampling and NMR monitoring to generate the cyclopentyl ligand 4c. The NMR characterization data are as follows: 1 H NMR (411 MHz, C 6 D 6)δ7.75–7.59(m,5H),7.37(d,J=7.6Hz,1H),7.22(dd,J=4.9,1.6Hz,3H),7.19(dd,J=6.3,2.6Hz,3H),7.17(t,J=7.4Hz,1H),5.49(d,J=2.2Hz,1H), 4.12(d,J=1.5Hz,1H),3.21–3.15(m,5H),1.71–1.58(m,2H),1.58–1.51( m,4H),1.43(dd,J=8.7,4.3Hz,2H),1.31–1.17(m,3H),1.12–1.11(m,2H).

[0102] Step 3):

[0103]

[0104] Under nitrogen atmosphere, add 2.1 times the amount of n-butyl lithium n-hexane solution to the 111 ml eggplant-shaped bottle containing the generated compound intermediate 4c. After stirring overnight, a large amount of yellow precipitate 4c dilithium salt is produced. The reaction solution is cooled to -30 °C and an equimolar amount of TiCl 4 (THF) 2 Solid, the color of the solution changed from yellow to dark black, slowly warmed to room temperature, stirred overnight, vacuum removed the solvent, extracted with toluene and filtered off the lithium salt, vacuum distilled to remove toluene, recrystallized, washed with n-hexane, and obtained a black solid 5c with a yield of 79%. NMR characterization is as follows: 1 H NMR (411 MHz, C 6 D 6 )δ8.17–8.11(m,2H),7.97(dd,J=6.7,2.8Hz,2H),7.61(d,J=8.8Hz,1H),7.37–7 .32(m,2H),7.32(s,1H),7.31–7.26(m,4H),6.99(dd,J=16.7,8.8Hz,3H),6.85–6 .79(m,1H),5.85(s,1H),3.58(t,J=6.5Hz,1H),3.45(d,J=8.2Hz,2H),3.18(s,2H ),2.19(s,2H),1.86(dd,J=12.5,9.1Hz,3H),1.58(s,3H),1.41(d,J=7.1Hz,6H).

[0105] Example 4 A synthesis of a constrained geometry nitrogen-containing sidearm monoindenyl titanium catalyst comprises the following steps:

[0106] Step 1):

[0107]

[0108] At room temperature, in a nitrogen atmosphere, compound 1a (311 mg, 1.62 mmol) was placed in a 100 ml eggplant-shaped bottle, 41 ml of n-hexane was added, and 2.5 M n-butyl lithium hexane solution (1.72 mL, 1.78 mmol) was added under stirring, and stirred for 6 hours to obtain a yellow precipitate 2a. 2 SiCl 2 (219 mg, 1.62 mmol) was slowly added dropwise to the reaction solution, and the solution changed from a yellow suspension to a brown turbid liquid. After stirring overnight, 3a was generated. After sampling, the hexane solvent was drained, and the NMR analysis results of 3a were: 1 H NMR (411 MHz, C 6 D 6 )δ7.59(t,J=7.1Hz,2H),7.23–7.12(m,2H),5.12(d,J=2.4Hz,1H),3.51(d,J=2 .1Hz,1H),3.12(t,J=6.4Hz,4H),1.54–1.45(m,5H),1.12(s,3H),-1.11(s,3H).

[0109] Step 2):

[0110]

[0111] Under nitrogen atmosphere, add equimolar lithium tert-butylamine to the hexane solution of the intermediate compound 3a in a 100 ml eggplant-shaped bottle, stir and react for 8 hours, take samples and monitor the completion of the reaction by NMR, and generate the cyclopentadienyl ligand 4a. The NMR characterization data are as follows: 1 HNMR (411 MHz, C 6 D 6 )δ7.75(t,J=6.5Hz,1H),7.66(d,J=7.1Hz,1H),7.36–7.23(m,2H),5.44(d,J=2.2Hz,1H),3.47(d,J=1. 5Hz,1H),3.29(dd,J=12.9,6.5Hz,5H),1.68–1.61(m,5H),1.17–1.19(m,9H),1.13(s,3H),1.11(s,3H).

[0112] Step 3)

[0113]

[0114] Under nitrogen atmosphere, 2.1 eq of n-butyl lithium hexane solution was added to the 100 ml eggplant-shaped bottle containing the generated compound intermediate 4a. After stirring overnight, a large amount of yellow precipitate 4a dilithium salt was produced. The reaction solution was cooled to -30 °C and an equimolar amount of ZrCl 4 Solid, the color of the solution changed from yellow to yellow-brown, slowly warmed to room temperature, stirred overnight, vacuum removed the solvent, extracted with toluene to filter out the lithium salt, vacuum distilled to remove toluene, washed with n-hexane to obtain a yellow crystalline solid 5d, with a yield of 65.3%. NMR characterization is as follows: 1 HNMR (C 6 D 6 )δ1.51(s,3H),1.69(s,3H).1.33(s,9H),1.7-1.7(m,4H),3.1-3.2(m,2H) ,3.4-3.5(m,2H),5.59(s,1H).6.9-7.1(m,2H),7.6-7.7(m,1H),7.63(d,1H 3 J HH =8.5Hz).

[0115] Comparative Example 1 The catalyst having the same structure as that in Example 2 is prepared, comprising the following steps:

[0116] Under nitrogen atmosphere, the intermediate Ph 2 SiCl 2 To a solution of 1 g, 1.114 mol, in 21 ml of hexane, add lithium tert-butylamine (312 mg, 1.114 mol). After stirring overnight, filter out the lithium salt and drain the solvent to obtain an oily product 1d with a yield of 91%.

[0117]

[0118] 1d (511 mg, 1.724 mmol) was added with an equal molar amount of lithium salt solid 1a. The color of the solution changed from yellow to yellow-brown. After stirring overnight, the solvent was removed by filtration and vacuum to obtain product 4b. The NMR results of the obtained product are as follows: Figure 1 shown.

[0119]

[0120] After adding twice the amount of n-butyl lithium solution to the product 4b, the mixture was filtered and dried, and then the dilithium salt solid (487 mg, 1.18 mmol) was added to a mixture containing an equimolar amount of TiCl 3 (THF) 3 After stirring for 2 hours, PbCl 2(155 mg, 1.54 mmol), the solution turned from yellow to black, stirred overnight, and then vacuum distilled to remove THF, extracted with toluene, filtered, and washed with n-hexane to obtain black solid 5b with a yield of 71.3%. The NMR results of the obtained product are as follows Figure 2 shown.

[0121]

[0122] Depend on Figure 1-4 By comparison, the ligand 4b synthesized by the method proposed in Comparative Example 1 has a NMR Figure 1 It can be seen that there are multiple peaks of isomers at 4.1-5.5 ppm, and the ligand 4b synthesized by the embodiment method Figure 3 It can be seen that the generation of isomerization peaks at 4.1-5.5 ppm is reduced. The NMR of catalyst 5b obtained by the comparative method is Figure 2 Comparative Example Catalyst 5b NMR Figure 4 At 7.1-8.5ppm and 1.2-1.5ppm, the comparative method has many impurity peaks that cannot be removed, which are the peaks of the products of incomplete oxidation of trivalent titanium. At 4.1-5.5ppm, the peaks of isomers are not completely removed, and the purity is low.

[0123] Test Example 1 Ethylene-octene copolymerization experiment

[0124] The preferred catalysts for the ethylene-octene polymerization experiment of the present invention are the catalyst M1 (5a) prepared in Example 1 and the catalyst M2 (5b) prepared in Example 2.

[0125] Instruments and equipment: high temperature and high pressure intermittent reactor, hot press, electronic density meter, melt flow rate meter, high temperature gel permeation chromatograph (GPC).

[0126] In the ethylene-octene polymerization experiment of M1 catalyst, the experiment of the effect of temperature factor on the polymerization of M1 and M2 catalysts was preferred (polymerization temperature was selected as 91°C, 121°C, 141°C, 161°C), wherein the pressure was 2MPa, the octene concentration was 1.5M, the catalyst concentration was 3.1umol, the reaction time was 11min, the total solvent volume was 31mL, and the cocatalyst was [Ph 3 C][B(C 6 F 5 ) 4 ], concentration ratio: B / Ti = 1.1, Al / Ti = 151, main catalyst pre-alkylation concentration ratio: Al / Ti = 5. Catalyst, co-catalyst, triisobutylaluminum are all selected in toluene solution.

[0127] The catalyst polymerization experiment is as follows:

[0128] The reactor was preheated at 151°C and ethylene was used to replace the reaction system. When the temperature dropped below 61°C, 16.4 mL of n-hexane, 7.1 mL of octene, and 4.5 mL of triisobutylaluminum were added in sequence. After stirring for 1 minute, 1 mL of catalyst M1 (catalyst M2) and co-catalyst [Ph 3 C][B(C 6 F 5 ) 4 ], open the ethylene flow valve, keep the ethylene pressure of the system at 2MPa, and react for 11 minutes. After the reaction is completed, add a fire extinguishing agent. The polymer solution is precipitated with acidified ethanol. After drying, the tablets are pressed and subjected to density, melt index determination, GPC and other analytical tests. The results are shown in Tables 1 and 2, wherein Table 1 is the catalytic characteristic data of M1, and Table 2 is the catalytic characteristic data of M2.

[0129] Table 1 Catalytic properties of M1

[0130]

[0131] Table 2 Catalytic properties data of M2

[0132]

Claims

1. A method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps: 1) Under inert gas protection, in a first solvent, a lithium salt of a compound having a structure represented by formula I-1 is reacted with a compound having a structure represented by formula I-2 to obtain a reaction solution containing a compound having a structure represented by formula II-1; the first solvent is n-hexane; the reaction temperature is -78-100° C.; wherein, The compound having the structure shown in formula II-1 is selected from 3a; Formula I-1; Formula I-2; Formula II-1; 2) Under nitrogen atmosphere, add equimolar lithium tert-butylamine to a 100 ml hexane solution of the intermediate compound 3a in an eggplant-shaped bottle, stir and react for 8 hours, take a sample and monitor the completion of the reaction by NMR, and generate the cyclopentadienyl ligand 4a; ; ; 3) Under nitrogen atmosphere, 2.1 eq of n-butyl lithium hexane solution was added to a 100 ml eggplant-shaped bottle containing the generated compound intermediate 4a. After stirring overnight, dilithium salt was generated. The reaction solution was cooled to -20°C, an equimolar amount of TiCl4(THF)2 solid was added, the temperature was raised to room temperature, stirred overnight, the solvent was removed in vacuo, the lithium salt was filtered out by toluene extraction, the toluene was removed by vacuum distillation, the mixture was recrystallized, and washed with n-hexane to obtain a black solid 5a. 。 2. A method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps: 1) Under inert gas protection, in a first solvent, a lithium salt of a compound having a structure represented by formula I-1 is reacted with a compound having a structure represented by formula I-2 to obtain a reaction solution containing a compound having a structure represented by formula II-1; the first solvent is n-hexane; the reaction temperature is -78-100° C.; wherein, The compound having the structure shown in formula II-1 is selected from 3b; Formula I-1; Formula I-2; Formula II-1; 2) Under nitrogen atmosphere, add equimolar lithium tert-butylamine to a 100 ml hexane solution of intermediate 3b in an eggplant-shaped flask, and stir to react for 6 hours to generate cyclopentadienyl ligand 4b; ; ; 3) Under nitrogen atmosphere, add 2.1 times the amount of n-butyl lithium hexane solution to the 100 ml eggplant-shaped bottle containing the generated compound intermediate 4b. After stirring overnight, a large amount of yellow precipitate 4b dilithium salt is generated. The reaction solution is cooled to -20 o C, add an equal mole of TiCl4(THF)2 solid, warm to room temperature, stir overnight, remove the solvent in vacuo, extract with toluene to filter out the lithium salt, remove toluene by distillation under reduced pressure, recrystallize, and wash with n-hexane to obtain a black solid 5b; 。 3. A method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps: 1) Under inert gas protection, in a first solvent, a lithium salt of a compound having a structure represented by formula I-1 is reacted with a compound having a structure represented by formula I-2 to obtain a reaction solution containing a compound having a structure represented by formula II-1; the first solvent is n-hexane; the reaction temperature is -78-100° C.; wherein, The compound having the structure shown in formula II-1 is selected from 3b; Formula I-1; Formula I-2; Formula II-1; 2) Under nitrogen atmosphere, add equimolar lithium cyclopentylamine to a 100 mL hexane solution of intermediate 3b in an eggplant-shaped flask, and stir to react for 8 hours to generate cyclopentylamine ligand 4c; ; ; 3) Under nitrogen atmosphere, add 2.1 times the amount of n-butyl lithium n-hexane solution to the 100 ml eggplant-shaped bottle containing the generated compound intermediate 4c. After stirring overnight, a large amount of yellow precipitate 4c dilithium salt is generated. The reaction solution is cooled to -30 o C, add an equimolar amount of TiCl4(THF)2 solid, warm to room temperature, stir overnight, remove the solvent in vacuo, extract with toluene and filter out the lithium salt, remove toluene by distillation under reduced pressure, recrystallize, and wash with n-hexane to obtain a black solid 5c; 。 4. A method for synthesizing a constrained geometry nitrogen-containing sidearm indene metal derivative, comprising the following steps: 1) Under inert gas protection, in a first solvent, a lithium salt of a compound having a structure represented by formula I-1 is reacted with a compound having a structure represented by formula I-2 to obtain a reaction solution containing a compound having a structure represented by formula II-1; the first solvent is n-hexane; the reaction temperature is -78-100° C.; wherein, The compound having the structure shown in formula II-1 is selected from 3a; Formula I-1; Formula I-2; Formula II-1; 2) Under nitrogen atmosphere, add equimolar lithium tert-butylamine to the hexane solution of the intermediate compound 3a in a 100 ml eggplant-shaped bottle, and stir to react for 8 hours to generate the cyclopentadienyl ligand 4a; ; ; 3) Under nitrogen atmosphere, 2.1 eq of n-butyl lithium hexane solution was added to the 100 ml eggplant-shaped bottle containing the generated compound intermediate 4a. After stirring overnight, a large amount of yellow precipitate 4a dilithium salt was produced. The reaction solution was cooled to -30 o C, add an equal mole of ZrCl4 solid, warm to room temperature, stir overnight, remove the solvent in vacuo, extract with toluene to filter out the lithium salt, remove toluene by vacuum distillation, wash with n-hexane to obtain a yellow crystalline solid 5d; 。 5. The synthesis method according to any one of claims 1 to 4, characterized in that The molar ratio of the lithium salt of the compound having the structure represented by formula I-1 to the compound having the structure represented by formula I-2 is 1:1-5.