Production method of wear-resistant layer on tooth surface of new steel tooth roller drill
By pre-filling wear-resistant materials and sintered metal powder in the tooth mold of the tooth drill bit, the wear-resistant layer on the tooth surface is made by using the sintering process, which solves the problem of welding layer multiplying spherical due to oxyacetylene surfacing, and improves wear resistance and breakage Rock efficiency.
Patent Information
- Application Number
- CN202211673285.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-26
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2042-12-26
AI Technical Summary
The wear-resistant layer of the conventional tooth drill bit tooth surface is limited due to the welding material spread of oxyacetylene surfacing, which leads to the welding layer being spherical, affecting the rock-breaking penetration and drilling efficiency.
A mixed powder of pre-filled wear-resistant materials and sintered metal is used to prepare a tooth surface wear-resistant layer through the sintering process, and the mold is used to control the appearance of the welding layer to be flat, and diamond single crystal particles can be added to improve wear resistance.
The wear-resistant layer produced through the sintering process can effectively improve wear resistance, avoid the problem of welding layer multiplying spherical shape, and improve rock breaking and drilling efficiency.
Smart Images

Figure CN115921864B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil drilling tools, in particular to a method for producing a new type of wear-resistant layer on the tooth surface of a steel-toothed roller drill bit. Background Art
[0002] The roller drill bit is a common tool for oil drilling. It is connected to the top drive or the mud motor to rotate and perform rock breaking operations. Common roller drill bits include insert tooth roller drill bits and steel tooth roller drill bits. Insert tooth roller drill bits use carbide sintered formed teeth, which are pressed into the prefabricated tooth holes of the roller body by some hydraulic tools, and the alloy teeth are fixed by interference fit. The steel tooth roller drill bit is processed by milling the steel matrix directly to form the tooth shape, and then wear-resistant welding materials, usually tubular tungsten carbide welding materials or sintered tungsten carbide rod welding materials, are heated and melted by oxyacetylene and welded on the tooth surface of the drill bit. Both drill bits are universal excavation tools. In addition, the roller single piece can be used as a trenchless tool or a crossing tool to construct some trenchless holes or crossing holes by combining with a specific matrix. It can also be used as a pile hole excavation tool in the construction industry or to complete some municipal pipeline hole operations, etc. It has a wide range of uses.
[0003] The wear-resistant layer on the tooth surface of conventional roller drill bits is welded with oxyacetylene and wear-resistant electrodes. The disadvantages of this production process are: the tooth area is small, the spread of the welding material of oxyacetylene welding is limited, resulting in problems such as spherical shape of the weld layer after welding, which affects the rock breaking penetration and drilling efficiency. Summary of the invention
[0004] In order to effectively solve the problems in the above-mentioned background technology, the present invention proposes a method for producing a new type of wear-resistant layer on the tooth surface of a steel-tooth roller drill.
[0005] The specific technical solutions are as follows:
[0006] A novel method for producing a wear-resistant layer on the tooth surface of a steel-tooth roller drill comprises the following steps: Step 1, pre-filling a tooth die with mixed powder of a wear-resistant material and a sintered metal;
[0007] Step 2: Place the tooth wheel in the tooth mold, leaving space for powder in advance, and the inner cavity space of the mold is larger than the volume of the tooth;
[0008] Step 3: Put the batch of sintering molds into an atmosphere furnace or a vacuum furnace for sintering. The sintering process is carried out according to the melting point of the added low-temperature metal powder;
[0009] Step 4: After sintering, since the tooth mold will not be bonded to the metal material, it can be directly removed to complete the wear-resistant layer.
[0010] Preferably, the wear-resistant material is cast tungsten carbide with a hardness greater than 1000 HV or spherical tungsten carbide with a hardness greater than 2000 HV or cobalt-containing sintered spherical alloy, or it can be crushed powder of cemented carbide.
[0011] Preferably, the sintered metal is Cu—Mn—Ni low temperature alloy powder, or Cu—Mn—Co alloy powder, or Cu—Mn—Ni—Sn.
[0012] Preferably, the metal powder accounts for 30% or 40% or 50% or more of the total proportion.
[0013] Preferably, in step one, diamond single crystal particles are also added, the diamond single crystal particles are coated diamond single crystals, and the added proportion of diamond can be 10%, 20%, 25% or more than 25%.
[0014] Preferably, in step 2, the gear is fixed in the tooth mold by a tooling.
[0015] Preferably, in step 2, the outside of each layer of tooth mold is fixed by an outer ring.
[0016] Preferably, adjacent outer rings are fixed by white latex or slots.
[0017] Preferably, the tooth mold is made of graphite material.
[0018] Compared with the prior art, the invention has the following beneficial effects: the process can control the appearance of the weld layer to be smooth through the tooth mold. This process can further improve the wear resistance by adjusting the formula and the addition ratio of hard materials, such as adding diamond particles, which is not available in conventional surfacing methods. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of the present invention;
[0020] Figure 2 It is a structural schematic diagram of a tooth mold in the present invention;
[0021] Figure 3 It is a schematic diagram of the left mold structure of another tooth mold in the present invention;
[0022] Figure 4 It is a right structural schematic diagram of another tooth mold in the present invention;
[0023] Figure 5 This is a diagram showing another tooth mold in use in the present invention;
[0024] Figure 6 An exploded view of the present invention;
[0025] Figure 7 A perspective view of the present invention;
[0026] Figure 8 This is the finished product picture. DETAILED DESCRIPTION
[0027] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used herein to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below other devices or structures". Thus, the exemplary term "above" may include both "above" and "below". The device may also be positioned in other different ways, rotated 90 degrees or in other orientations, and the spatially relative descriptions used herein are interpreted accordingly.
[0028] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings and preferred embodiments. Figure 1 As shown, a new method for producing the wear-resistant layer on the tooth surface of a steel-toothed roller drill bit is provided. A mixed powder of wear-resistant material and bonding metal is pre-filled inside the tooth mold, and the wear-resistant layer on the tooth surface is produced by sintering. The above is a schematic assembly diagram. The steel teeth of the roller base 1 have been milled, and the processing state of the inner hole can be determined according to one's own production conditions. For example, heat treatment can be directly performed after the wear-resistant layer is produced, such as a multi-purpose furnace with vacuum carburizing and quenching. The inner hole of a conventional roller needs to be carburized, and the inner hole can be in a state before carburizing. Other non-tooth positions on the outer surface are not carburized, and the anti-seepage layer can be brushed in advance.
[0029] If carburizing needs to be performed after sintering is completed, the processing of the inner hole can basically be ignored and can be determined according to the process arrangement.
[0030] like Figure 2 and 3 As shown, the movable tooth mold 2, the three rows of teeth of the gear wheel often have slightly different tooth shapes. The tooth mold mold can be easily made by a small machining center and a CNC program, and even a fixed tooling can be made to arrange the raw materials into an array and batch produce multiple tooth molds at a time. Reference numeral 3 is a ring tooling for the auxiliary tooth mold. Reference numeral 5 is a schematic support gear wheel positioning structure. Reference numeral 4 is the loaded wear-resistant sintered powder.
[0031] The material of the tooth mold can be graphite, or other materials that are easy to process and resistant to high temperatures. Take graphite as an example.
[0032] like Figure 2 and 3 As shown, the movable tooth molds are the left mold 21 and the right mold 22, with a powder filling gap 23 in the middle. This mold has a high efficiency of mass production using a small processing center, and the edges of the vertical seams have a staggered design to prevent the liquid metal material from seeping out after sintering. If further reliability is required, the vertical seams on the back can also be added with this structure, but it is not limited to this structure. The adjusted process may not require staggered grooves, or other types of design structures are required to prevent seepage.
[0033] Figures 4 to 6 The figure shows the mold for the top teeth, the material can also be graphite or other high temperature resistant and easy to process materials, the bottom also has a staggered groove anti-seepage design, and the necessary side can also be added.
[0034] When installing with the steel teeth of the gear, the left and right molds are assembled to wrap the teeth inside. Taking graphite as an example, white glue with a specific viscosity or other glues can be used to bond and fix.
[0035] After the tooth mold is assembled, the mixed powder can be loaded into it. The powder is a wear-resistant material, such as conventional cast tungsten carbide (hardness > 1000HV) or spherical tungsten carbide (hardness > 2000HV) or cobalt-containing sintered spherical alloy. It can also be crushed powder of cemented carbide, or single crystal tungsten carbide can be added to improve a certain toughness. It can also be a mixture of several tungsten carbide materials in a certain proportion.
[0036] At the same time, a certain proportion of sintered metal powder is mixed. The metal powder can be Cu-Mn-Ni low-temperature alloy powder, Cu-Mn-Co alloy powder, or Cu-Mn-Ni-Sn, etc. The metal powder can account for 30%, 40% or even 50% or more of the total proportion, which can be adjusted as needed.
[0037] As mentioned above, diamond single crystal particles can be added. If diamond is sintered in an atmosphere protection state or a vacuum state, it can be graphitized at a higher temperature. Diamond can be coated diamond single crystal. The coated diamond currently sold on the market, for example, has titanium, silicon, nickel and other materials on the surface of the diamond. The addition ratio of diamond can be 10%, 20%, 25% or more according to the selection.
[0038] The mixed metal powder and tungsten carbide powder (or adding diamond single crystal) is referred to as sintered powder.
[0039] The cone can be fixed by a fixed tool (positioned as needed, and after being installed with the bottom tooth mold, the space for powder loading is fixed), and then the bottom mold is installed. The bottom mold can be separated at this time, and then the mold is closed after adjustment at the top tooth position. Then the sintering powder is loaded into the gap above.
[0040] The mold has reserved space for powder filling in advance. The inner cavity of the mold is larger than the volume of the tooth. The thickness of the powder filling can also be adjusted by adjusting the size of the inner cavity of the tooth mold, thereby controlling the thickness of the wear-resistant layer, such as 2mm, 3mm or more.
[0041] like Figure 6 and 7 As shown above, this is a schematic diagram of this method. Each tooth mold is split, and the tooth mold can be wrapped from both sides of the tooth, and then sintering powder can be loaded. After each layer of tooth wrapping and powder loading is completed, an outer ring fixed tooth mold can be added, which is the number 3 in the general diagram, and repeated layer by layer. Or when the process is mature and the product is fixed, the positioning groove of the tooth mold can be processed at the fixed position of each layer of the outer ring, which can quickly locate and improve efficiency.
[0042] After the assembly and sintering powder filling are completed, each layer of outer ring can be fixed with white glue or fixed by a specific slot or other limiting design as needed or for easy movement, which will not be described in detail.
[0043] Then the batch of sintering molds are placed in an atmosphere furnace or a vacuum furnace for sintering. The sintering process is carried out according to the melting point of the added low-temperature metal powder. The sintering is usually completed by adjusting the metal powder to be in a molten state. For example, the melting point of conventional Cu-Mn-Co is around 1000°C. After sintering, since the graphite mold will not adhere to the metal material, it can be directly removed and the wear-resistant layer is completed. Figure 8 shown.
[0044] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for producing a wear-resistant layer on the tooth surface of a steel-toothed roller drill bit, Features: The method comprises the following steps: Step 1, pre-filling a mixed powder of wear-resistant material and sintered metal in a tooth die; Step 2: Place the tooth wheel in the tooth mold, leaving space for powder in advance, and the inner cavity space of the mold is larger than the volume of the tooth; Step 3: Put the batch of sintering molds into an atmosphere furnace or a vacuum furnace for sintering. The sintering process is carried out according to the melting point of the added low-temperature metal powder; Step 4: After sintering, since the tooth mold will not be bonded to the metal material, the wear-resistant layer can be directly removed and made; In step 1, diamond single crystal particles are also added, the diamond single crystal particles are coated diamond single crystals, and the addition ratio of diamond is 10%, 20% or 25%; In step 2, the gear is fixed in the tooth mold by a tooling; In step 2, the outside of each layer of tooth mold is fixed by an outer ring.
2. The method for producing the wear-resistant layer on the tooth surface of a steel-tooth roller drill according to claim 1, It is characterized in that The wear-resistant material is cast tungsten carbide with a hardness greater than 1000 HV, or spherical tungsten carbide with a hardness greater than 2000 HV, or cobalt-containing sintered spherical alloy, or crushed powder of cemented carbide.
3. The method for producing the wear-resistant layer on the tooth surface of a steel-tooth roller drill according to claim 1, It is characterized in that The sintered metal is Cu Mn Ni low temperature alloy powder, or Cu Mn Co alloy powder, or Cu Mn Ni Sn.
4. The method for producing the wear-resistant layer on the tooth surface of a steel-tooth roller drill according to claim 1, It is characterized in that The metal powder accounts for more than 30%, 40% or 50% of the total proportion.
5. The method for producing the wear-resistant layer on the tooth surface of a steel-tooth roller drill according to claim 1, It is characterized in that Adjacent outer rings are fixed by white glue or slots.