A method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil
Through the multi-step treatment of Fischer-Tropsch synthetic oil, including hydrorefining, hydroisomerization, molecular sieve adsorption and urea complexing, the problems of low yields of isomer alkanes and many side reactions in the prior art were solved, and the problem of low yields of isomer alkanes and many side reactions was achieved. Method for efficient preparation of high-purity isomer alkanes.
Patent Information
- Application Number
- CN202310214410.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-02-28
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2043-02-28
AI Technical Summary
In the prior art, when using Fischer-Tropsch synthetic oil to prepare high-purity isomer alkanes, the yield is low, the efficiency is low, and the side reactions are many, making it difficult to achieve the goal of high purity and high yield.
Using the 125-350°C fraction of Fischer-Tropsch synthetic oil as raw material, multiple fractionation and separation are carried out through steps such as hydrorefining, hydroisomerization, molecular sieve adsorption and urea complexing, combined with specific catalysts and process conditions, to improve the Purity and yield of isomer alkanes.
Highly efficient and high yield preparation of high-purity isomer alkanes is achieved, reducing side reactions, and improving the conversion rate of normal alkanes and the yield of isomer alkanes.
Smart Images

Figure BDA0004114433410000051 
Figure BDA0004114433410000061 
Figure BDA0004114433410000062
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of organic chemical industry, and in particular relates to a method for preparing high-purity isoparaffins by utilizing Fischer-Tropsch synthetic oil. Background Art
[0002] Isoalkanes have good low-temperature fluidity, stability, compatibility, spreadability and water retention. Low surface tension ensures excellent wetting and surface spreading. High-purity isoalkanes contain almost no harmful impurities, have little odor, have high chemical stability, have a long shelf life, are easy to recycle and reuse, and have good comfort and safety. Moreover, the flash point and volatility of narrow-fraction isoalkanes match, and the application effect in professional fields is better. Isoalkanes are widely used in lubricants for various instruments, metalworking fluids, daily chemicals, polymerization reactants, oilfield drilling fluids, aviation kerosene blending components, clean high cetane number diesel blending components and many other fields.
[0003] CN 101921621 A discloses a method for preparing isoparaffin solvent oil by using a hydrorefining-hydroisomerization process with petroleum-based distillate oil or deasphalted oil as raw materials. Since the petroleum-based raw oil contains a large amount of harmful compounds such as sulfur, nitrogen, and aromatics, which cannot be completely removed, the cleanliness of the product is affected.
[0004] Invention patents such as CN 111471488 A, CN 113980701 A, and CN 200410048351 disclose methods for separating isoparaffins from Fischer-Tropsch synthetic oil to purify normal paraffins or prepare isoparaffins by using molecular sieve adsorption separation. A series and X series molecular sieves such as 3A, 5A, 10X, and 13X are used as adsorbents. The isoparaffin content in Fischer-Tropsch synthetic oil generally does not exceed 10%, and the pore size of the selected molecular sieve is not ideal for the adsorption selectivity of normal paraffins, resulting in low adsorption separation efficiency and low isoparaffin yield.
[0005] US 5866748 discloses a method for preparing isoparaffin solvent oil. The method uses normal alkanes rich in carbon atoms of 8 to 20 in the liquid product of Fischer-Tropsch synthesis as raw materials, uses a catalyst with amorphous silicon aluminum as a carrier and a precious metal or non-precious metal as an active metal, and prepares isoparaffin solvent oil through a hydrogenation isomerization reaction under suitable process conditions. Since the irregular pore size carrier has poor selectivity for the reactants, the conversion rate and selectivity are reduced, the yield of the target product is low, and the purity of the isoparaffin is not more than 90%.
[0006] CN 108315051 B, CN 103897718 A, CN102464998 A, and US 8058492, US8198492, US 7232935B2, US 20100076238A1, US 20090163744A1 and US 20090163744A1, US20090031617A1, WO 2010053468 A1, WO 2006075057, WO2009117337, etc. disclose a method for preparing bio-jet fuel and biodiesel by hydrogenation saturation and hydrodeoxygenation of bio-oil as raw material, and then performing hydroisomerization reaction of the bio-oil. Due to the limitation of conversion rate and selectivity of hydroisomerization reaction, the purity of the obtained isoparaffin is not more than 90%.
[0007] In order to further improve the isomerization rate of the product, the method disclosed in US 20100000908A1 uses animal and vegetable oils as raw materials to prepare bio-jet fuel and biodiesel with good low temperature performance through hydrodeoxygenation and hydroisomerization reactions. + Compared with the one-pass process, this method has a high product isomerization rate, but the process of partial product recycling reduces production efficiency. In addition, the 200℃ of the one-pass hydrogenation isomerization product + The fraction is a mixture of normal alkanes and isoalkanes. When the isoalkanes therein undergo a second hydrogenation isomerization reaction, it is easy to cause an increase in hydrocracking side reactions and a decrease in the yield of the target product. Summary of the invention
[0008] In view of the above problems existing in the prior art, the technical problem to be solved by the present invention is to provide a method for preparing high-purity isoalkanes using Fischer-Tropsch synthetic oil, which can prepare high-purity isoalkanes with high efficiency, high yield and few side reactions.
[0009] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows:
[0010] A method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil comprises the following steps:
[0011] (1) a step of selecting a feedstock oil, wherein a 125-350° C. fraction of Fischer-Tropsch synthetic oil or any fraction within the distillation range is selected as the feedstock oil;
[0012] (2) Hydrofining step, in which the olefins in the feedstock are hydrogenated and saturated by hydrofining, and the oxygenated compounds and aromatics that may exist are removed to less than 50 μg / g, and the hydrofining reaction product is subjected to gas-liquid separation by thermal high separation to obtain n-C5 +; Preferably, the oxygen-containing compounds and aromatics that may be present are removed to less than 10 μg / g;
[0013] (3) Hydroisomerization reaction step, the n-C5 + Converted into normal and isomeric mixed alkanes, the conversion rate of normal alkane reactants is over 60%;
[0014] (4) Atmospheric pressure fractionation step, the C5 + Normal and isomerized mixed alkanes are separated into light and heavy fractions. The 100-270℃ fraction is light normal and isomerized mixed alkanes, and the 270℃ fraction is light normal and isomerized mixed alkanes. + The fractions are heavy normal and isomeric mixed alkanes;
[0015] (5) separating the normal and isoalkanes of the light normal-isomerized mixed alkanes at 100 to 270° C. obtained in the fractionation step by a molecular sieve adsorption method;
[0016] (6) using a urea complexation method to separate the normal and iso-alkanes from the 270°C+ heavy mixed alkanes obtained in the fractionation step;
[0017] (7) a secondary hydroisomerization step, wherein the normal alkanes obtained by the adsorption separation of normal and isomerized molecular sieves and the urea complex separation are recycled back to the hydroisomerization step for a secondary hydroisomerization reaction;
[0018] (8) a fractionation step, wherein the isoparaffins obtained by the adsorption separation of normal and isomeric molecular sieves and the urea complex separation are fractionated to prepare isoparaffins with different distillation ranges; the isoparaffins with different distillation ranges can be extracted from the system as isoparaffin products, or light and heavy fraction isoparaffins can be obtained by fractionation, or narrow fraction isoparaffin products can be obtained by rectification, or the light fraction, heavy fraction and narrow fraction isoparaffins obtained by fractionation and rectification are blended to obtain isoparaffin products with different carbon number distributions.
[0019] In the method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, in step (2), alumina is used as a carrier for the hydrorefining catalyst, and at least one of Ni, Co, Mo, and W is used as a hydrogenation active metal component, and the active metal content in oxidation state is 5% to 25% of the carrier mass, preferably, the active metal content in oxidation state is 15% to 25% of the carrier mass.
[0020] The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, step (2), the hydrofining reaction temperature is 300-400°C, the hydrogen partial pressure is 3-18MPa, the liquid hourly volume space velocity is 0.5-3.0h -1 , hydrogen-oil ratio is 500~1500Nm 3 / m 3Preferably, the reaction temperature is 340-380°C, the hydrogen partial pressure is 6-10 MPa, and the liquid hourly volume space velocity is 1.0-2.0 h -1 , hydrogen-oil ratio is 800~1200Nm 3 / m 3 .
[0021] The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, step (3), the catalyst for the hydroisomerization reaction uses at least one of ZSM-12, ZSM-22, ZSM-23, ZSM-35, ZSM-48, SAPO-11, SAPO-41 as a carrier, Pt and / or Pd as hydrogenation active metal components, the active metal content in elemental form is 0.1% to 1.0% of the carrier mass, preferably, the active metal content in elemental form is 0.3% to 0.7% of the carrier mass.
[0022] The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, step (3), the hydroisomerization reaction temperature is 280-380°C, the hydrogen partial pressure is 3-18 MPa, and the liquid hourly volume space velocity is 0.5-3.0 h -1 , hydrogen to oil ratio 300~1000Nm 3 / m 3 Preferably, the reaction temperature is 300-350°C, the hydrogen partial pressure is 4-8 MPa, and the liquid hourly volume space velocity is 1.0-2.0 h -1 , hydrogen-to-oil ratio 300~800Nm 3 / m 3 .
[0023] In the method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, in step (5), the molecular sieve is a 10-membered ring mesoporous molecular sieve, and the minor axis size of its elliptical pores is 0.4-0.52 nm, and the major axis size is 0.52-0.54 m.
[0024] In the method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, in step (5), the molecular sieve is any one of AlPO-41, UCSB-15GaGe, EU-1, ECNU-21, Laumontite, ZSM-23 or IST-1.
[0025] The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, step (6), using a urea solution with a mass ratio of urea: isopropanol: water of 30-45: 35-40: 15-30 as a complexing agent, a mass ratio of urea solution to alkane of 5-15: 1, a complexing time of 2-10 hours, and a complexing temperature of 10-50° C. Preferably, the mass ratio of urea solution to alkane is 5-10: 1, the complexing time is 2-6 hours, and the complexing temperature is 20-40° C.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] Most of the normal alkanes are converted into isoalkanes by the hydroisomerization reaction, and then the normal and isoalkanes are separated by molecular sieve adsorption and / or urea complexation, so that high-purity isoalkanes can be prepared with high yield. Compared with the method of producing isoalkanes as by-products during the purification of normal alkanes, the method used in the present invention has high efficiency and high yield; compared with the method of increasing the severity of the hydroisomerization reaction, the method used in the present invention has fewer side reactions. Moreover, the present invention uses a method for secondary isomerization of the normal alkanes obtained by separating the normal and isoalkanes, which improves the conversion rate of normal alkanes and further improves the yield of isoalkanes. DETAILED DESCRIPTION
[0028] The present invention is further described below in conjunction with specific examples. In the examples, the substances described in each calculation formula refer to liquid hydrocarbons having a carbon number of not less than 5. The yield of liquid hydrocarbons in the hydroisomerization reaction (Y ISO )、100℃ - Fraction yield (Y L )、100~270℃ fraction yield (Y M )、270℃ fraction yield (Y H ), the isoparaffin yield of normal isoparaffin separation (X ISO ), isoparaffin purity (P ISO ), etc., calculated by the following formula:
[0029] Y ISO (%) = total weight of hydrocarbon products ÷ total weight of hydrocarbon feedstock × 100%;
[0030] Y L (%) = 100°C in hydrogenated isomerized product - Fraction weight ÷ total weight of hydroisomerization products × Y ISO ×100%;
[0031] Y M (%) = weight of fraction at 100-270°C in hydroisomerization product / total weight of hydroisomerization product × Y ISO ×100%;
[0032] Y H (%) = 270℃ in hydrogenation isomerization product + Fraction weight ÷ total weight of hydroisomerization products × Y ISO ×100%;
[0033] X ISO (%) = total weight of isoparaffin products ÷ total weight of hydrocarbon feedstock × 100%;
[0034] P ISO(%) = weight of isoparaffins in hydrocarbon products ÷ (weight of isoparaffin products + weight of normal paraffin products) × 100%.
[0035] Analysis of alkane composition in Tables 1 to 8: First, Agilent 5973MS was used for qualitative analysis, and then Varian CP-3800GC was used for detection. The chromatographic column used was a 50m×200μm×0.5μm PONA column, FID detector, injection volume 0.2μL, split ratio 150:1, column box temperature 60℃, injection port temperature 300℃, and the temperature was increased to 180℃ at a rate of 5℃ / min, and then increased to 220℃ at a rate of 2℃ / min.
[0036] Example 1
[0037] A method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil comprises the following steps:
[0038] (1) Using 125-350°C distillate of Fischer-Tropsch oil as raw material;
[0039] (2) A tubular fixed bed reactor hydrogenation test device with a catalyst loading of 200 ml was used to carry out a 5% NiO-20% MoO 3 / Al 2 O 3 In a fixed bed reactor with a catalyst volume of 200 ml, the reaction pressure was 8.0 MPa, the reaction temperature was 360°C, and the liquid hourly volume space velocity was 1,0 h -1 、Hydrogen oil volume ratio 800Nm 3 / m 3 The hydrofining reaction was carried out under the process conditions of , and no oxygen-containing compounds, aromatics and olefins were detected in the liquid phase product. The composition of the feedstock oil and the hydrofining liquid product is shown in Table 1;
[0040] (3) The liquid phase product of the hydrofining reaction in step (2) was used as the raw material, and the reaction temperature was 360° C., the reaction pressure was 8.0 MPa, and the liquid hourly volume space velocity was 2.0 h in a fixed bed reactor equipped with 200 ml of 0.5% Pt / SAPO-11 catalyst. -1 , hydrogen oil volume ratio 500Nm 3 / m 3 The hydroisomerization reaction was carried out under the process conditions of , and the yield and physicochemical properties of the product are shown in Table 2.
[0041] (4) The obtained liquid product is fractionated by a real boiling point distillation apparatus to obtain a light fraction with a distillation range of less than 100°C, a medium fraction with a distillation range of 100 to 270°C, and a high-quality product with a distillation range of 270°C. + The carbon number distribution and composition of the latter two are shown in Tables 3 and 4;
[0042] (5) The medium-quality product with a distillation range of 100 to 270° C. in step (4) is used as a raw material, and a ZSM-23 molecular sieve is selected as an adsorbent. The molecular sieve is a one-dimensional 10-membered ring molecular sieve, and its elliptical pore minor axis size is 4.5 nm and major axis size is 5.2 nm. The normal alkanes and isoalkanes are separated by adsorption and desorption processes, and adsorption separation and purification are carried out under the conditions of an adsorption tower temperature of 200° C. and a pressure of 2.5 MPa. A mixture of normal pentane and isoheptane in a mass ratio of 2.5:1 is used as a desorbent. Under the conditions of a hydrogen flow rate of 0.025 m / s, a desorption temperature of 360° C., and a desorption pressure of 0.1 MPa, the normal alkanes adsorbed on the molecular sieve are desorbed, and the desorbent is removed by fractionation to obtain normal alkanes. The isoalkanes are not adsorbed by the molecular sieve. The purity and yield of the prepared isoalkanes are shown in Table 5.
[0043] (6) Using the heavy product with a distillation range of 270°C+ in step (4) as a raw material, the normal alkanes and the isoalkanes are separated by urea complexation. The mass ratio of the urea complexing agent is urea: isopropanol: water = 40: 40: 20, the mass ratio of the complexing agent to the alkane is 8: 1, the complexing temperature is 40°C, the complexing reaction time is 2 hours, and the composition and yield of the isoalkanes obtained after washing with water are shown in Table 6.
[0044] (7) The light isoparaffins with a temperature of 100 to 270° C. obtained in step (5) are separated by three-tower distillation. The first distillation tower is set at 40 plates, an operating pressure of 0.06 MPa, a reflux ratio of 5, a tower top temperature of 105° C., and a tower bottom temperature of 185° C. to separate C 7 ~C 15 Light isoparaffins are separated into C 7 ~C 9 With C 10 + Two components, C 7 ~C 9 As a product extracted from the system, C 10 + The components enter the second distillation tower for further separation; the second distillation tower is set at 40 plates, 0.06 MPa operating pressure, 5 reflux ratio, 158 ° C tower top temperature, and 212 ° C tower bottom temperature. 15 + The components were separated into C 10 ~C 11 and C 12 + Two components, C 10 ~C 11 As a product extracted from the system, C 12 +Enter the third distillation tower for further separation; the third distillation tower is set at 40 plates, 0.04 MPa operating pressure, 5 reflux ratio, 185 ° C tower top temperature, and 220 ° C tower bottom temperature. 12 + The components were separated to obtain C 12 ~C 13 and C 14 ~C 15 The purity and yield of the two components are shown in Table 7.
[0045] (8) The 270°C solution obtained in step (6) is treated by double tower distillation. + The first distillation tower is set at 40 plates, 0.02 MPa operating pressure, 12 reflux ratio, 222°C tower top temperature, and 257°C tower bottom temperature to separate the heavy isoparaffins. 16 + Separation of heavy isoparaffins into C 15 ~C 17 With C 18 + Two components, C 15 ~C 17 As a product extracted from the system, C 18 + The components enter the second distillation tower for further separation. The second distillation tower is set at 40 plates, 0.06 MPa operating pressure, 5 reflux ratio, 250°C tower top temperature, and 273°C tower bottom temperature. 18 + The components were separated into C 18 ~C 19 and C 20 + Two components are extracted from the system as products, respectively. The purity and yield of each component are shown in Table 8.
[0046] Table 1 Composition of 125-350℃ fraction and hydrofining liquid product of Fischer-Tropsch synthetic oil
[0047]
[0048]
[0049] Table 2 Hydroisomerization product yield and general properties of the product
[0050] project Yield, % Liquid hydrocarbons 98.98 Gaseous hydrocarbons 1.02 100℃-Distillation 8.42 100~270℃ fraction 58.60 <![CDATA[270℃ + Fraction]]> 31.96 Liquid product physicochemical properties Pour point, ℃ -32 Olefin content, μg / g Not detected Aromatic content, μg / g Not detected Oxygen content, μg / g Not detected
[0051] Table 3 Carbon number distribution and composition of the middle fraction of the hydroisomerization reaction product at 100-270°C
[0052] Carbon number Isoparaffin content, % Normal alkane content, % Purity of isoparaffins, % <![CDATA[C 7 ]]> 1.03 0.91 53.09 <![CDATA[C 8 ]]> 4.48 3.93 53.27 <![CDATA[C 9 ]]> 5.80 3.98 59.30 <![CDATA[C 10 ]]> 6.94 4.22 62.19 <![CDATA[C 11 ]]> 8.74 3.86 69.37 <![CDATA[C 12 ]]> 9.58 3.78 71.71 <![CDATA[C 13 ]]> 11.02 3.09 78.10 <![CDATA[C 14 ]]> 10.94 2.70 80.21 <![CDATA[C 15 ]]> 10.70 2.48 81.18 <![CDATA[C 16 ]]> 1.53 0.29 84.07 total 70.76 29.24 70.76
[0053] Table 4 Hydroisomerization reaction products 270℃ + Heavy fraction carbon number distribution and composition
[0054]
[0055]
[0056] Table 5 Purity and yield of isoparaffins obtained by molecular sieve adsorption separation of the middle fraction at 100-270℃
[0057]
[0058] Table 6 270℃ + Purity and yield of isoparaffins obtained by urea complex separation of heavy fractions
[0059]
[0060] Table 7 Yield and purity of narrow-fraction isoparaffins obtained by distillation of the middle mass components at 100-270℃
[0061]
[0062]
[0063] Table 8 270℃+Hydrogen fraction distillation to obtain narrow fraction isoparaffin yield and purity
[0064]
Claims
1. A method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil, characterized in that: The following steps are involved: (1) A step of selecting a feedstock oil, wherein a 125-350° C. fraction of the Fischer-Tropsch synthetic oil or any fraction within the 125-350° C. fraction of the Fischer-Tropsch synthetic oil is selected as the feedstock oil; (2) Hydrofining step, in which the olefins in the feed oil are hydrogenated and saturated, and the oxygenated compounds and aromatics present are removed to below 50 μg / g, and the hydrofining reaction product is subjected to gas-liquid separation by thermal high separation to obtain n-C5 + ; (3) Hydroisomerization reaction step, the n-C5 + Converted into normal and isomeric mixed alkanes; (4) Atmospheric pressure fractionation step, the C5 + Normal and isomerized mixed alkanes are separated into light and heavy fractions. The 100~270℃ fraction is light normal and isomerized mixed alkanes, and the 270℃ fraction is + The fractions are heavy normal and isomeric mixed alkanes; (5) Separating the normal and isoalkanes of the light normal isomerized mixed alkanes at 100 to 270° C. obtained in the fractionation step by a molecular sieve adsorption method; the molecular sieve is a 10-membered ring mesoporous molecular sieve having an elliptical pore having a minor axis size of 0.4 to 0.52 nm and a major axis size of 0.52 to 0.54 nm; (6) Using the urea complexation method, the 270°C + Separation of normal and iso-alkanes in heavy mixed alkanes; (7) A secondary hydroisomerization step, wherein the normal alkanes obtained by the adsorption separation of normal and isomerized molecular sieves and the urea complexation separation are recycled back to the hydroisomerization step for a secondary hydroisomerization reaction; (8) A fractionation step for fractionating the isoparaffins obtained by the adsorption separation of normal and isoparaffins and the separation by urea complexation to prepare isoparaffins with different distillation ranges.
2. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: In step (2), the catalyst for hydrotreating uses alumina as a carrier and at least one of Ni, Co, Mo and W as a hydrogenation active metal component, wherein the active metal content in oxidation state is 5% to 25% of the carrier mass.
3. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: Step (2), the hydrofining reaction temperature is 300-400°C, the hydrogen partial pressure is 3-18 MPa, and the liquid hourly volume space velocity is 0.5-3.0 h -1 , hydrogen-oil ratio is 500~1500Nm 3 / m 3 .
4. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: In step (3), the catalyst for the hydroisomerization reaction uses at least one of ZSM-12, ZSM-22, ZSM-23, ZSM-35, ZSM-48, SAPO-11, and SAPO-41 as a carrier, uses Pt and / or Pd as hydrogenation active metal components, and the active metal content in the form of a single substance is 0.1% to 1.0% of the carrier mass.
5. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: Step (3), the hydroisomerization reaction temperature is 280-380°C, the hydrogen partial pressure is 3-18 MPa, and the liquid hourly volume space velocity is 0.5-3.0 h -1 , hydrogen to oil ratio 300~1000 Nm 3 / m 3 .
6. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: In step (5), the molecular sieve is any one of AlPO-41, EU-1, ECNU-21 or ZSM-23.
7. The method for preparing high-purity isoparaffins using Fischer-Tropsch synthetic oil according to claim 1, characterized in that: In step (6), a urea solution having a mass ratio of urea: isopropanol: water of 30-45:35-40:15-30 is used as a complexing agent, a mass ratio of urea solution to alkane of 5-15:1, a complexing time of 2-10 hours, and a complexing temperature of 10-50°C is used.