Method for manufacturing silicon carbide semiconductor device, silicon carbide semiconductor device, and power conversion device
In the manufacturing process of the silicon carbide semiconductor device, the design of the drift layer and well region is used, and the polysilicon film in the Schottky trench is removed in combination with wet etching method, the material residue and pollution problems are solved, and the silicon carbide semiconductor device is improved Reliability and lack of defects.
Patent Information
- Application Number
- CN202080105419.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-30
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2040-09-30
AI Technical Summary
When manufacturing silicon carbide semiconductor devices, holes or cracks are easily formed during the filling process of the interlayer insulating film in the Schottky trench, resulting in residual materials such as polycrystalline silicon and Ni, causing pollution; at the same time, dry etching methods are used in silicon oxide and polycrystalline silicon The process will also cause the formation of silicides in places that should not exist, affecting the reliability of the device.
The drift layer and well region are formed on the silicon carbide semiconductor substrate to form a through gate trench and Schottky trench, a built-in silicon oxide film and a polysilicon film, and the polysilicon in the Schottky trench is removed by wet etching. The film reduces foreign matter residues and improves the purity of the manufacturing process.
It is realized that the silicon carbide semiconductor device has reduced defects and improved reliability, prevented residual contamination of silicide and insulating film, and produced a silicon carbide semiconductor device with few defects and reliability.
Smart Images

Figure CN116195070B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a method for manufacturing a silicon carbide semiconductor device having a trench gate and a power conversion device using the silicon carbide semiconductor device. Background Art
[0002] It is known that there are semiconductor devices for electric power that have built-in unipolar switching elements such as MOSFET (Metal-Oxide-Semiconductor Field-Effect-Transistor) and unipolar freewheeling diodes such as Schottky barrier diodes (SBD). Such semiconductor devices can be realized by configuring MOSFET units and SBD units in parallel on the same chip. Generally speaking, they can be realized by providing a Schottky electrode in a specific area within the chip and operating the area as an SBD.
[0003] By making the freewheeling diode built into the chip of the switching element, the cost can be reduced compared with the case where the freewheeling diode is external to the switching element. In particular, in MOSFET using silicon carbide (SiC) as the base material, the bipolar operation caused by the parasitic pn diode can be suppressed by building in the SBD, which is also one of the advantages. This is because in silicon carbide semiconductor devices, the expansion of crystal defects caused by the recombination energy of carriers generated by the operation of the parasitic pn diode sometimes damages the reliability of the element.
[0004] In addition, in a trench-gate MOSFET having a structure in which a gate electrode is buried in a trench formed in a semiconductor layer, a channel can be formed on the side wall of the trench, and the channel width density can be increased accordingly, thereby reducing the on-resistance.
[0005] When manufacturing such a trench MOSFET with a built-in SBD, after forming a Schottky trench in which a Schottky electrode is buried and a gate trench in which a gate electrode is buried by etching, a gate insulating film and a gate electrode are formed in the gate trench, an interlayer insulating film is formed thereon, and then a contact hole is formed in the interlayer insulating film. At the same time, while leaving a portion of the interlayer insulating film on the side wall of the Schottky trench, a Ni film is deposited and heat treated to form a silicide layer (for example, Patent Document 1).
[0006] Patent Document 1: Japanese Patent Application Publication No. 2018-182235 ( Figure 6 wait) Summary of the invention
[0007] Technical issues to be solved by the invention
[0008] When polysilicon is formed in the gate trench as a gate electrode while the Schottky trench is filled with an interlayer insulating film after the Schottky trench is formed, or when silicides such as metal silicide are formed on the source region, polysilicon and Ni sometimes remain in the holes (voids, cracks) formed by the interlayer insulating film filling the Schottky trench. Polysilicon, metal and silicides thereof remain in places where they should not be there, and are released as foreign matter when the interlayer insulating film is removed, causing contamination.
[0009] In addition, when a gate insulating film of silicon oxide and a gate electrode of polycrystalline silicon are formed in the gate trench, the polycrystalline silicon is mostly processed by dry etching. When silicon oxide and polycrystalline silicon are temporarily formed in the Schottky trench in the same way as in the gate trench and the polycrystalline silicon in the Schottky trench is removed by dry etching, sometimes a portion of the polycrystalline silicon remains on the gate insulating film at the bottom of the Schottky trench. If a metal layer is deposited and heated in this state to perform silicidation, silicide may sometimes be formed at the bottom of the Schottky trench. The silicide may sometimes be released in subsequent processes to cause contamination.
[0010] The present disclosure has been made to solve the above-mentioned technical problems, and an object of the present disclosure is to provide a method for manufacturing a silicon carbide semiconductor device with few defects and high reliability, which can prevent polysilicon material or metal silicide material from remaining in unexpected locations.
[0011] Technical solutions for solving technical problems
[0012] The manufacturing method of the silicon carbide semiconductor device disclosed in the present invention comprises: a step of forming a drift layer on a silicon carbide semiconductor substrate; a step of forming a well region on the drift layer; a step of forming a source region on the upper layer of the well region; a step of forming a gate trench penetrating the source region and the well region and reaching the drift layer; a step of forming a Schottky trench reaching the drift layer at a position separated from the gate trench; a step of forming a silicon oxide film on the inner wall of the gate trench and the Schottky trench; a step of forming a polysilicon film on the inner side of the silicon oxide film in the gate trench and the Schottky trench; a step of removing the gate trench and the Schottky trench by etching back the polysilicon film; The invention relates to a process for forming a gate electrode in a gate trench by forming a polysilicon film outside the trench; a process for forming an interlayer insulating film on the gate electrode in the gate trench; a process for removing the polysilicon film in the Schottky trench by wet etching after a hole is opened in the interlayer insulating film; a process for forming an ohmic electrode on the source region after removing the polysilicon film in the Schottky trench; a process for removing the silicon oxide film in the Schottky trench after forming the ohmic electrode; and a process for forming a source electrode in the Schottky trench that is Schottky-connected to the drift layer.
[0013] Effects of the Invention
[0014] According to the method for manufacturing a silicon carbide semiconductor device disclosed in the present invention, a silicon carbide semiconductor device with few defects and high reliability can be manufactured. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 This is a cross-sectional view of a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to the first embodiment.
[0016] Figure 2 This is a top view of a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to the first embodiment.
[0017] Figure 3 This is a cross-sectional view of a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to the first embodiment.
[0018] Figure 4 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0019] Figure 5 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0020] Figure 6 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0021] Figure 7 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0022] Figure 8 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0023] Fig. 9 It is a cross-sectional view for explaining the method for manufacturing the silicon carbide semiconductor device according to the first embodiment.
[0024] Fig.10 It is a cross-sectional view for explaining a manufacturing method when the manufacturing method of the silicon carbide semiconductor device of the first embodiment is not adopted.
[0025] Fig.11 It is a cross-sectional view for explaining a manufacturing method when the manufacturing method of the silicon carbide semiconductor device of the first embodiment is not adopted.
[0026] Fig.12 It is a cross-sectional view for explaining a manufacturing method when the manufacturing method of the silicon carbide semiconductor device of the first embodiment is not adopted.
[0027] Fig.13It is a cross-sectional view for explaining a manufacturing method when the manufacturing method of the silicon carbide semiconductor device of the first embodiment is not adopted.
[0028] Fig.14 This is a cross-sectional view of a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to the first embodiment.
[0029] Fig.15 This is a top view of a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to the first embodiment.
[0030] Fig.16 This is a cross-sectional view of the silicon carbide semiconductor device according to the first embodiment.
[0031] Fig.17 This is a cross-sectional view of a silicon carbide semiconductor device according to a second embodiment.
[0032] Fig.18 This is a cross-sectional view of a silicon carbide semiconductor device according to a second embodiment.
[0033] Fig.19 It is a cross-sectional view for explaining the method for manufacturing a silicon carbide semiconductor device according to the second embodiment.
[0034] Fig. 20 It is a cross-sectional view for explaining the method for manufacturing a silicon carbide semiconductor device according to the second embodiment.
[0035] Fig.21 It is a cross-sectional view for explaining the method for manufacturing a silicon carbide semiconductor device according to the second embodiment.
[0036] Fig. 22 It is a cross-sectional view for explaining the method for manufacturing a silicon carbide semiconductor device according to the second embodiment.
[0037] Fig.23 This is a cross-sectional view of a silicon carbide semiconductor device according to a second embodiment.
[0038] Fig.24 This is a schematic diagram showing the structure of a power conversion device manufactured by the method for manufacturing a power conversion device according to the third embodiment. DETAILED DESCRIPTION
[0039] Hereinafter, the embodiments will be described with reference to the accompanying drawings. In addition, the accompanying drawings are schematically shown, and the relationship between the sizes and positions of the images shown in different drawings may not be accurately recorded, but may be appropriately changed. In addition, in the following description, the same components are illustrated with the same symbols, and their names and functions are assumed to be the same. Therefore, their detailed description may be omitted in some cases.
[0040] Implementation method 1.
[0041] First, the structure of a silicon carbide semiconductor device manufactured by the manufacturing method according to the first embodiment of the present disclosure will be described.
[0042] Figure 1 This is a cross-sectional view of a portion of an active region of a trench-type silicon carbide MOSFET with built-in Schottky barrier diode (SiC trench MOSFET with built-in SBD), which is a silicon carbide semiconductor device manufactured using the manufacturing method of Embodiment 1. Figure 2 yes Figure 1 The top view of the SiC trench MOSFET with built-in SBD shown is a top view at a certain depth where a trench is formed.
[0043] exist Figure 1 In the embodiment, a drift layer 20 composed of n-type silicon carbide is formed on the surface of a semiconductor substrate 10 composed of n-type and low-resistance silicon carbide. A well region 30 composed of p-type silicon carbide is provided on the surface of the drift layer 20. A source region 40 composed of n-type silicon carbide is formed on the upper layer of the well region 30. In addition, a contact region 35 composed of low-resistance p-type silicon carbide is formed on the surface of the well region 30 next to the source region 40. Here, regardless of whether ion implantation is performed, the region composed of silicon carbide (the region formed as the drift layer 20) is referred to as a silicon carbide layer.
[0044] A gate trench is formed at a portion of the well region 30 where the source region 40 is formed, penetrating the source region 40 and the well region 30 and reaching the drift layer 20. In addition, a Schottky trench is formed at a portion of the well region 30 where the source region 40 is not formed and separated from the gate trench, penetrating the well region 30 and reaching the drift layer 20.
[0045] A gate electrode 60 made of low-resistance polysilicon is formed inside the gate trench via a gate insulating film 50. A p-type first protection region 31 is formed in the drift layer 20 at the bottom of the gate trench. A p-type second protection region 32 is formed in the drift layer 20 at the bottom of the Schottky trench.
[0046] An interlayer insulating film 55 is formed on the gate electrode 60 and the gate insulating film 50 of the gate trench and near the opening of the Schottky trench. In addition, an ohmic electrode 70 composed of metal silicide is formed on the source region 40 and the contact region 35. A source electrode 80 is formed inside the Schottky trench, on the ohmic electrode 70, and on the interlayer insulating film 55, and the source electrode 80 inside the Schottky trench is Schottky-bonded with the drift layer 20. A back ohmic electrode 71 is formed on the surface of the semiconductor substrate 10 on the opposite side of the drift layer 20 where the drift layer 20 is not formed, and a drain electrode 85 is formed outside it.
[0047] At a position where the source electrode 80 contacts the drift layer 20 in the Schottky trench, the source electrode 80 is made of any material among Ti, Mo, W, and Ni.
[0048] like Figure 2 As shown in the top view of , the gate trench having the gate electrode 60 formed therein and the Schottky trench having the source electrode 80 formed therein are formed linearly in a certain direction and are alternately arranged. The interval between the gate trench and the Schottky trench is fixed. Here, in the gate trench, a p-type first connection region 33 is formed from the gate trench to the drift layer 20 along a direction orthogonal to the extension direction of the gate trench, and in the Schottky trench, a p-type second connection region 34 is formed from the Schottky trench to the drift layer 20 along a direction orthogonal to the extension direction of the Schottky trench.
[0049] Figure 3 FIG. 1 is a cross-sectional view of a SiC trench MOSFET with built-in SBD manufactured by the manufacturing method of the first embodiment at a position where a first connection region 33 and a second connection region 34 are formed. Figure 3 As shown, the first connection region 33 connects the first protection region 31 and the well region 30. In addition, the second connection region 34 connects the second protection region 32 and the well region 30. A plurality of first connection regions 33 and second connection regions 34 are formed at predetermined intervals along the extending direction of the gate trench and the Schottky trench.
[0050] Below, use Figure 1 The cross section shown corresponds to Figures 4 to 16 A method for manufacturing the silicon carbide semiconductor device, i.e., the SiC-MOSFET with built-in SBD according to the first embodiment of the present disclosure is described with reference to a cross-sectional view of FIG.
[0051] First, a 1×10 15 cm -3 Above and 1×10 17 cm -3 At an impurity concentration below 50 μm, an n-type drift layer 20 made of silicon carbide having a thickness of 5 μm or more and 50 μm or less is epitaxially grown.
[0052] Next, Al (aluminum) is ion-implanted as a p-type impurity into the surface of the drift layer 20. At this time, the Al ion implantation depth is set to be not less than 0.5 μm and not more than 3 μm, which is not more than the thickness of the drift layer 20. In addition, the impurity concentration of the Al ion implanted is set to 1×10 17 cm-3 Above and 1×10 19 cm -3 The impurity concentration of the drift layer 20 is higher than that of the impurity of the drift layer 20. The region implanted with Al ions in this step becomes the well region 30, and the Figure 4 The structure of the cross-sectional view is shown in FIG.
[0053] Next, an implantation mask is formed by using a photoresist or the like so as to open a predetermined portion of the well region 30 on the surface of the drift layer 20, and ions are implanted with N (nitrogen) as an n-type impurity. The implantation depth of N is made shallower than the thickness of the well region 30. In addition, the impurity concentration of the implanted N is set to 1×10 18 cm -3 Above and 1×10 21 cm -3 The following range exceeds the p-type impurity concentration of the well region 30. The region exhibiting n-type among the regions implanted with N in this step becomes the source region 40. Thereafter, the implantation mask is removed.
[0054] In addition, by the same method, a predetermined region of the well region 30 adjacent to the source region 40 is subjected to an impurity concentration higher than that of the well region 30 by 1×10 19 cm -3 Above and 1×10 21 cm -3 The contact region 35 is formed by ion implanting Al in a manner of impurity concentration in the range below. Figure 5 The structure of the cross-section shown.
[0055] Next, a resist mask is formed to open a portion of the region where the source region 40 is formed, and a gate trench is formed by dry etching to penetrate the source region 40 and the well region 30 and reach the drift layer 20. Similarly, a resist mask is formed to open a portion of the region where the source region 40 is not formed, and a Schottky trench is formed by dry etching to penetrate the well region 30 and reach the drift layer 20.
[0056] The gate trench and the Schottky trench can be formed at the same depth in the same dry etching process. Figure 6 The structure of the cross-section shown.
[0057] Then, if Figure 7As shown in the cross-sectional schematic diagram in FIG, p-type impurities are ion-implanted into the drift layer 20 at the bottom of the gate trench and the Schottky trench to form the first protection region 31 and the second protection region 32, respectively. The resist mask is removed after the ion implantation. In addition, a resist mask is formed to open the portion where the first connection region 33 and the second connection region 34 are formed, and the first connection region 33 and the second connection region 34 are formed by obliquely ion-implanting p-type impurities. The resist mask is removed after the ion implantation.
[0058] Next, annealing is performed at 1300° C. to 1900° C. for 30 seconds to 1 hour in an inert gas atmosphere such as argon (Ar) gas using a heat treatment apparatus. The annealing electrically activates the ion-implanted N and Al.
[0059] Next, the surface of the silicon carbide layer including the inside of the gate trench and the Schottky trench is thermally oxidized to form a silicon oxide film 51 having a thickness of 10 nm to 300 nm. The silicon oxide film 51 is formed in contact with the inner wall of the gate trench and the Schottky trench. The silicon oxide film 51 can be formed by the CVD method. Through the steps up to this step, a silicon oxide film 51 having a thickness of 10 nm to 300 nm is obtained. Figure 8 The structure of the cross-section shown.
[0060] Next, a polysilicon film 61 having conductivity is formed on the silicon oxide film 51 by a reduced pressure CVD method to a thickness of 300 nm to 2000 nm, thereby forming Fig. 9 Next, the polysilicon film 61 is etched back to leave only the gate trench and the Schottky trench inside. Fig.10 The polysilicon film 61 in the gate trench serves as the gate electrode 60 .
[0061] Then, if Fig.11 As shown in the schematic cross-sectional view in FIG, an interlayer insulating film 55 made of silicon oxide is formed by a reduced pressure CVD method to a thickness of 500 nm to 3000 nm.
[0062] Next, the interlayer insulating film 55 and the silicon oxide film 51 are patterned so as to open the regions where the source region 40 and the contact region 35 are formed and the Schottky trenches. Fig.12 The cross-sectional structure shown.
[0063] Then, if Fig.13 As shown in the cross-sectional view in FIG. 2 , the polysilicon film 61 in the Schottky trench is removed by wet etching using an alkaline etching solution such as an alkaline developer.
[0064] Next, by depositing metals such as Ni and performing annealing and other processes, such as Fig.14As shown in the cross-sectional view thereof, an ohmic electrode 70 made of silicide is formed on the source region 40 and the contact region 35 .
[0065] Then, if Fig.15 As shown in the cross-sectional view in FIG. 1 , the silicon oxide film 51 in the Schottky trench and a portion (surface) of the interlayer insulating film 55 are removed by wet etching using hydrofluoric acid or the like. At this time, the natural oxide film on the surface of the ohmic electrode 70 can also be removed at the same time. The silicon oxide film 51 remaining in the gate trench becomes the gate insulating film 50.
[0066] Next, a source electrode 80 is formed inside the Schottky trench and on the ohmic electrode 70 of the gate trench to form a Schottky junction with the drift layer 20, and a back ohmic electrode 71 and a drain electrode 85 are formed on the back side, thereby manufacturing Figure 2 FIG. 8 is a cross-sectional view of a SiC-MOSFET with a built-in SBD. FIG.
[0067] In one of the conventional methods, when a contact hole connected to the ohmic electrode 70 is formed in the interlayer insulating film 55 while the Schottky trench is filled with the interlayer insulating film 55, it is necessary to form the contact hole while covering the Schottky trench with a resist mask, and then form another resist mask to remove the interlayer insulating film 55 in the Schottky trench. However, by manufacturing the SiC-MOSFET with built-in SBD using the manufacturing method of this embodiment, the number of times the resist mask is formed can be reduced to manufacture the SiC-MOSFET with built-in SBD, and the manufacturing cost can be reduced.
[0068] When the SiC-MOSFET with built-in SBD is manufactured by the manufacturing method of this embodiment, when the silicon oxide film 51 inside the Schottky trench is wet-etched, the silicon oxide film 51 and a part (surface) of the interlayer insulating film 55 are wet-etched. Fig.16 As shown in the cross-sectional view thereof, a portion where the source electrode 80 is in direct contact with the source region 40 or the contact region 35 is formed on the gate trench side around the ohmic electrode 70 .
[0069] According to the method for manufacturing a silicon carbide semiconductor device of the present embodiment, it is possible to prevent silicide and gate insulating film from remaining in the Schottky trench and prevent foreign matter causing contamination from being generated during the process, thereby manufacturing a silicon carbide semiconductor device with few defects.
[0070] Implementation method 2.
[0071] First, the structure of a silicon carbide semiconductor device manufactured by the manufacturing method according to the second embodiment of the present disclosure will be described.
[0072] Fig.17This is a schematic cross-sectional view of a unit cell of an active region of a silicon carbide semiconductor device, i.e., a silicon carbide MOSFET with a built-in Schottky barrier diode (SiC-MOSFET with a built-in SBD), manufactured using the manufacturing method of Embodiment 2. Fig.18 1 is a cross-sectional view of the SiC-MOSFET with built-in SBD at the position where the first connection region 33 and the second connection region 34 are formed. Figure 2 same.
[0073] In the first embodiment, the ohmic electrode 70 of the MOSFET in the gate trench is formed in a hole formed at a position away from the hole of the interlayer insulating film 55 in the upper part of the Schottky trench in the cross-sectional view, but in the method for manufacturing a silicon carbide semiconductor device of the present embodiment, the ohmic electrode 70 of the MOSFET in the gate trench and the source electrode 80 in the Schottky trench are formed in the same hole of the interlayer insulating film 55, that is, the interlayer insulating film 55 is not provided between the adjacent ohmic electrode 70 and the Schottky trench. As for other aspects, they are the same as those in the first embodiment, and thus detailed description is omitted.
[0074] exist Fig.17 In the embodiment, a drift layer 20 is formed on the surface of a semiconductor substrate 10. A well region 30 is provided on the surface of the drift layer 20, and a source region 40 and a contact region 35 are formed on the upper layer of the well region 30. A gate trench is formed at a portion of the well region 30 where the source region 40 is formed, penetrating the source region 40 and the well region 30 and reaching the drift layer 20. In addition, a Schottky trench is formed at a portion of the well region 30 where the source region 40 is not formed, penetrating the well region 30 and reaching the drift layer 20.
[0075] A gate insulating film 50 is formed inside the gate trench, and a gate electrode 60 is formed inside the gate trench. A p-type first protection region 31 is formed in the drift layer 20 at the bottom of the gate trench. A p-type second protection region 32 is formed in the drift layer 20 at the bottom of the Schottky trench.
[0076] An interlayer insulating film 55 is formed on the gate electrode 60 and the gate insulating film 50 of the gate trench. In addition, an ohmic electrode 70 is formed on the source region 40, the contact region 35, and the well region 30 near the Schottky trench. The interlayer insulating film 55 is not formed between the adjacent ohmic electrode 70 and the Schottky trench. A source electrode 80 is formed inside the Schottky trench, on the ohmic electrode 70, and on the interlayer insulating film 55, and the source electrode 80 inside the Schottky trench is Schottky-bonded to the drift layer 20. A back ohmic electrode 71 is formed on the surface of the semiconductor substrate 10 on the opposite side of the drift layer 20 where the drift layer 20 is not formed, and a drain electrode 85 is formed outside it.
[0077] In addition, the cross-sectional view at the position where the first protection region 31 and the second protection region 32 are formed is Fig.18 In addition to Fig.17 In addition to the structure, a first protection region 31 is formed in the drift layer 20 on the side wall of the gate trench, and a second protection region 32 is formed in the drift layer 20 on the side wall of the Schottky trench.
[0078] Below, use Fig.17 The cross section shown corresponds to Figure 19 to Figure 23 A method for manufacturing a silicon carbide semiconductor device, i.e., a SiC-MOSFET with built-in SBD, according to a second embodiment of the present disclosure will be described with reference to a cross-sectional view of FIG.
[0079] In the method for manufacturing a silicon carbide semiconductor device of this embodiment, Figures 4 to 11 The process is the same as that of embodiment 1. Fig.11 After the construction of Fig.19 As shown in the cross-sectional view in FIG. 1 , the interlayer insulating film 55 and the silicon oxide film 51 except for the gate electrode 60 and the silicon oxide film 51 of the gate trench are etched. The etching can be performed by plasma etching or by combining plasma etching with wet etching. At this time, the polysilicon film 61 in the Schottky trench is basically not etched, and a part of the upper side of the silicon oxide film of the same material as the gate insulating film 50 in the Schottky trench is etched. The silicon oxide film 51 remains in the lower part of the Schottky trench.
[0080] Then, if Fig. 20 As shown in the cross-sectional view in FIG. 2 , the polysilicon film 61 in the Schottky trench is selectively etched by wet etching.
[0081] Next, the metal constituting the ohmic electrode 70 is deposited and annealed. Fig.21 As shown in the cross-sectional view in FIG. 2 , an ohmic electrode 70 made of silicide is formed on the source region 40 , on the contact region 35 , on the well region 30 near the Schottky trench, and on the side surface of the well region 30 near the upper end of the Schottky trench.
[0082] Then, if Fig. 22 As shown in the cross-sectional view in FIG. 2 , the silicon oxide film 51 in the Schottky trench is wet-etched using hydrofluoric acid or the like.
[0083] Next, a source electrode 80 is formed on the interlayer insulating film 55, inside the Schottky trench and on the ohmic electrode 70 of the gate trench to form a Schottky junction with the drift layer 20, and a back ohmic electrode 71 and a drain electrode 85 are formed on the back side, thereby manufacturing a Fig.17FIG. 8 is a cross-sectional view of a SiC-MOSFET with a built-in SBD. FIG.
[0084] Here, the ohmic electrode 70 may be formed from outside the opening of the Schottky trench to a part of the inside, such as Fig.23 As shown in the cross-sectional view in FIG. 2 , an ohmic electrode 70 may also be formed in the upper portion of the Schottky trench.
[0085] In addition, when the silicon oxide film 51 inside the Schottky trench is wet-etched, the silicon oxide film 51 and a portion (surface) of the interlayer insulating film 55 are wet-etched. Fig. 22 As shown in the cross-sectional view thereof, a portion where the source electrode 80 is in direct contact with the source region 40 or the contact region 35 is formed on the gate trench side around the ohmic electrode 70 .
[0086] According to the manufacturing method of the silicon carbide semiconductor device, i.e., the SiC-MOSFET with built-in SBD of this embodiment, it is also possible to prevent silicide and gate insulating film from remaining in the Schottky trench, and it is possible to prevent foreign matter that causes contamination from being generated during the process, thereby enabling the manufacture of a silicon carbide semiconductor device with fewer defects.
[0087] In addition, according to the silicon carbide semiconductor device of this embodiment, there is no need to form an interlayer insulating film 55 near the Schottky trench, so there is no need to ensure space for forming the interlayer insulating film 55, the interval between the trenches can be made smaller, and a silicon carbide semiconductor device with a higher current density can be manufactured.
[0088] In addition, although the method of forming the well region 30 and the source region 40 by ion implantation is described in Embodiments 1 and 2, the well region 30 and the source region 40 may be formed by other methods, for example, by epitaxy. In addition, although the example of forming the well region 30 on the entire surface is described, the well region 30 may be formed in a part of the upper layer of the drift layer 20. In this case, the Schottky trench may not be provided in a manner of penetrating the well region 30, but may be provided directly in the drift layer 20 from the surface.
[0089] In Embodiments 1 and 2, the first protection region 31 and the second protection region 32 are provided in the lower portion of the trench, but depending on the situation, the first protection region 31 and the second protection region 32 may not be provided. In this case, the first connection region 33 and the second connection region 34 may not be provided.
[0090] Furthermore, although aluminum (Al) is used as a p-type impurity in embodiments 1 to 2, the p-type impurity may be boron (B) or gallium (Ga). The n-type impurity may be phosphorus (P) instead of nitrogen (N). In the MOSFET described in embodiments 1 to 2, the gate insulating film does not necessarily have to be an oxide film such as SiO2, but may be an insulating film other than an oxide film, or a film formed by combining an insulating film other than an oxide film with an oxide film. In addition, in the above embodiments, specific examples are used to illustrate the crystal structure, the plane orientation of the main surface, the deviation angle, and each injection condition, but the scope of application is not limited to these numerical ranges.
[0091] In addition, although the above embodiment describes a device in which a so-called vertical MOSFET silicon carbide semiconductor device having a drain electrode 85 formed on the back surface of the semiconductor substrate 10 is built with an SBD, it can also be applied to a device in which a so-called horizontal MOSFET such as a RESURF (Reduced SURface Field) type MOSFET having a drain electrode 85 formed on the surface of the drift layer 20 is built with an SBD. Furthermore, the silicon carbide semiconductor device can also be a device in which an insulated gate bipolar transistor (IGBT) is built with an SBD. In addition, it can also be applied to a device in which a MOSFET or IGBT having a superjunction structure is built with an SBD.
[0092] Implementation method 3.
[0093] In this embodiment, the manufacturing method of the silicon carbide semiconductor device of the above-mentioned embodiments 1 and 2 is applied to the manufacturing of a power conversion device. The present disclosure is not limited to a specific method for manufacturing a power conversion device, and the following is a description of the case where the present disclosure is applied to a method for manufacturing a three-phase inverter as embodiment 3.
[0094] Fig.24 1 is a block diagram showing a configuration of a power conversion system to which the power conversion device according to the present embodiment is applied.
[0095] Fig.24 The power conversion system shown includes a power supply 100, a power conversion device 200, and a load 300. The power supply 100 is a DC power supply, and supplies DC power to the power conversion device 200. The power supply 100 can be configured by various power supplies, for example, it can be configured by a DC system, a solar cell, a storage battery, or it can be configured by a rectifier circuit connected to an AC system, and an AC / DC converter. In addition, the power supply 100 can also be configured by a DC / DC converter that converts the DC power output from the DC system into a specified power.
[0096] The power conversion device 200 is a three-phase inverter connected between the power source 100 and the load 300, converts the DC power supplied from the power source 100 into AC power and supplies the AC power to the load 300. Fig.24 As shown, the power conversion device 200 includes: a main conversion circuit 201, which converts DC power into AC power and outputs it; a drive circuit 202, which outputs a drive signal for driving each switching element of the main conversion circuit 201; and a control circuit 203, which outputs a control signal of the drive circuit 202 to the drive circuit 202.
[0097] The drive circuit 202 performs off control on each normally-off switching element by making the voltage of the gate electrode and the voltage of the source electrode the same potential.
[0098] Load 300 is a three-phase motor driven by AC power supplied from power converter 200. Load 300 is not limited to a specific use, but is a motor mounted on various electrical devices, such as a hybrid car, an electric car, a railway vehicle, an elevator, or an air conditioner.
[0099] The following describes the details of the power conversion device 200. The main conversion circuit 201 includes a switching element and a freewheeling diode (not shown), and the DC power supplied from the power supply 100 is converted into AC power by the switching action of the switching element and supplied to the load 300. There are various structures for the specific circuit structure of the main conversion circuit 201, and the main conversion circuit 201 of this embodiment is a two-level three-phase full-bridge circuit, which can be composed of 6 switching elements and 6 freewheeling diodes connected in anti-parallel to each switching element. As each switching element of the main conversion circuit 201, a silicon carbide semiconductor device manufactured by the manufacturing method of the silicon carbide semiconductor device of any of the above-mentioned embodiments 1 to 2 is applied. Among the 6 switching elements, every two switching elements are connected in series to form upper and lower arms, and each upper and lower arm constitutes each phase (U phase, V phase, W phase) of the full bridge circuit. Then, the output terminal of each upper and lower arm, that is, the three output terminals of the main conversion circuit 201, is connected to the load 300.
[0100] The drive circuit 202 generates a drive signal for driving the switch element of the main conversion circuit 201, and supplies it to the control electrode of the switch element of the main conversion circuit 201. Specifically, according to the control signal from the control circuit 203 described later, the drive signal for turning on the switch element and the drive signal for turning off the switch element are output to the control electrode of each switch element. When the switch element is maintained in the on state, the drive signal is a voltage signal (on signal) above the threshold voltage of the switch element, and when the switch element is maintained in the off state, the drive signal is a voltage signal (off signal) below the threshold voltage of the switch element.
[0101] The control circuit 203 controls the switch elements of the main conversion circuit 201 to supply the desired power to the load 300. Specifically, based on the power to be supplied to the load 300, the time (on time) that each switch element of the main conversion circuit 201 should be in the on state is calculated. For example, the main conversion circuit 201 can be controlled by PWM control that modulates the on time of the switch element according to the voltage to be output. Then, a control instruction (control signal) is output to the drive circuit 202 so that at each time point, an on signal is output for the switch element that should be in the on state, and an off signal is output for the switch element that should be in the off state. The drive circuit 202 outputs an on signal or an off signal as a drive signal to the control electrode of each switch element in accordance with the control signal.
[0102] In the power conversion device of this embodiment, since a silicon carbide semiconductor device manufactured using the manufacturing method of a silicon carbide semiconductor device of embodiments 1 to 2 is used as a switching element of the main conversion circuit 201, a power conversion device with low loss and improved reliability of high-speed switching operation can be realized.
[0103] In this embodiment, an example of applying the present disclosure to a two-level three-phase inverter is described, but the present disclosure is not limited thereto and can be applied to various power conversion devices. Although a two-level power conversion device is used in this embodiment, a three-level or multi-level power conversion device may also be used, and the present disclosure may also be applied to a single-phase inverter when power is supplied to a single-phase load. In addition, when power is supplied to a DC load, the present disclosure may also be applied to a DC / DC converter or an AC / DC converter.
[0104] In addition, the power conversion device to which the present invention is applied is not limited to the case where the load is an electric motor as described above. For example, it can also be used as a power supply device for an electric discharge machine, a laser processing machine, an induction heating cooker, or a contactless power supply system, and can also be used as a power conditioner for a solar power generation system, a power storage system, etc.
[0105] Description of Reference Numerals
[0106] 10: semiconductor substrate; 20: drift layer; 30: well region; 31: first protection region; 32: second protection region; 33: first connection region; 34: second connection region; 35: contact region; 40: source region; 50: gate insulating film; 51: silicon oxide film; 55: interlayer insulating film; 60: gate electrode; 61: polysilicon film; 70: ohmic electrode; 71: back ohmic electrode; 80: source electrode; 85: drain electrode; 90: resist mask; 100: power supply; 200; power conversion device; 201: main conversion circuit; 202: drive circuit; 203: control circuit; 300: load.
Claims
1. A method for manufacturing a silicon carbide semiconductor device, characterized in that: have: forming a drift layer of a first conductivity type on a silicon carbide semiconductor substrate; forming a well region of a second conductivity type on the drift layer; A step of forming a source region of a first conductivity type in an upper portion of the well region; forming a gate trench penetrating the source region and the well region and reaching the drift layer; A step of forming a Schottky trench reaching the drift layer at a position separated from the gate trench; forming a silicon oxide film in contact with inner walls of the gate trench and the Schottky trench; forming a polysilicon film inside the silicon oxide film in the gate trench and the Schottky trench; The step of removing the polysilicon film outside the gate trench and the Schottky trench by etching back the polysilicon film to form a gate electrode in the gate trench; forming an interlayer insulating film on the gate electrode in the gate trench; After the hole is opened in the interlayer insulating film, the polysilicon film in the Schottky trench is removed by wet etching; After removing the polysilicon film in the Schottky trench, forming an ohmic electrode on the source region; After the step of forming the ohmic electrode, a step of removing the silicon oxide film in the Schottky trench and the silicon oxide film on the gate electrode side of the ohmic electrode; as well as After the step of removing the silicon oxide film in the Schottky trench and the silicon oxide film on the gate electrode side of the ohmic electrode, a step of forming a source electrode in the Schottky trench that makes Schottky connection with the drift layer.
2. The method for manufacturing a silicon carbide semiconductor device according to claim 1, wherein: The interlayer insulating film is not provided between the adjacent ohmic electrodes and the Schottky trenches.
3. The method for manufacturing a silicon carbide semiconductor device according to claim 1 or 2, characterized in that: A second conductivity type protection region is further formed in the drift layer at the bottom of the gate trench and the Schottky trench.
4. The method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 3, characterized in that: The ohmic electrode is made of silicide.
5. The method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 4, characterized in that: The step of removing the polysilicon film in the Schottky trench by wet etching after the hole is opened in the interlayer insulating film is performed in a state where the interlayer insulating film is formed on the gate electrode.
6. The method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 5, characterized in that: The step of removing the silicon oxide film in the Schottky trench is performed by wet etching using an etching solution containing hydrofluoric acid.
7. The method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 6, characterized in that: The step of removing the polysilicon film in the Schottky trench by wet etching is performed by wet etching using an alkaline etching solution.
8. The method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 7, characterized in that: The ohmic electrode is formed in a hole opened in the interlayer insulating film in a self-aligned manner.
9. A silicon carbide semiconductor device, characterized in that: have: Silicon carbide semiconductor substrate; A drift layer of a first conductivity type is formed on the silicon carbide semiconductor substrate; A well region of a second conductivity type is formed on the drift layer; A source region of the first conductivity type is formed in an upper portion of the well region of the second conductivity type; a gate trench formed in a manner of penetrating the source region and the well region and reaching the drift layer; A Schottky trench is formed in such a way as to reach the drift layer; a gate electrode formed in the gate trench via a gate insulating film; an interlayer insulating film formed on the gate electrode and near the Schottky trench opening; an ohmic electrode formed on the source region; as well as The source electrode is formed on the interlayer insulating film, the ohmic electrode and in the Schottky trench, directly contacts the source region on the gate trench side of the ohmic electrode, and is Schottky-connected to the drift layer.
10. A power conversion device comprising: A main conversion circuit, comprising a silicon carbide semiconductor device manufactured by the method for manufacturing a silicon carbide semiconductor device according to any one of claims 1 to 8, or a silicon carbide semiconductor device according to claim 9, wherein the main conversion circuit converts input power and outputs the power; a drive circuit that makes the silicon carbide semiconductor device perform an off operation by making the voltage of the gate electrode and the voltage of the source electrode of the silicon carbide semiconductor device the same, and outputs a drive signal for driving the silicon carbide semiconductor device to the silicon carbide semiconductor device; as well as The control circuit outputs a control signal for controlling the drive circuit to the drive circuit.