A high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material and preparation method thereof

By introducing K+ ions into NaTaO3 ceramics, the Na1-xKxTaO3 ceramic material was designed, which solved the problem of limited selection of microwave dielectric ceramic materials in terms of frequency temperature coefficient compensation, and realized ceramics with high dielectric constant and ultra-high forward temperature coefficient. Material preparation is suitable for frequency temperature coefficient compensation and simplifies the preparation process.

CN116606141BActive Publication Date: 2024-10-15ZHUHAI XINCI PRECISION ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310598918.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-25
Publication Date
2024-10-15
Estimated Expiration
2043-05-25

AI Technical Summary

Technical Problem

Existing microwave dielectric ceramic materials have limited choices in terms of frequency temperature coefficient compensation, making it difficult to design and develop new resonant frequency temperature coefficient compensation materials, which affects the high-temperature stability and frequency selectivity of the device.

Method used

By introducing K+ ions, the Na1-xKxTaO3 ceramic material is designed. Its general chemical formula is Na1-xKxTaO3 (x=0.025-0.15). It is synthesized by the solid-phase method and combined with the solid-phase sintering method to form a ceramic material with high dielectric constant and ultra-high dielectric constant. It is a microwave dielectric ceramic material with a high forward resonant frequency temperature coefficient and is used to adjust the microwave dielectric properties of MgTiO3 to obtain ceramics with a τf value close to zero.

Benefits of technology

A microwave dielectric ceramic material with high dielectric constant, low loss and ultra-high temperature coefficient has been realized, which is suitable for frequency temperature coefficient compensation, and the preparation method is simple and easy for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116606141B_ABST
    Figure CN116606141B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of electronic ceramics and their manufacturing, and specifically relates to a high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material and a preparation method thereof. The raw materials of the high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material of the present invention are Na2CO3, K2CO3 and Ta2O5, and are prepared by a solid phase method, and the chemical formula is Na 1‑x K x TaO3 (x=0.025‑0.15); has a high dielectric constant of 127‑176 and a loss as low as 3.46×10‑ 4 , 730-920ppm / ℃ ultra-high forward temperature coefficient. The present invention introduces K from the raw materials + ions, by adjusting the value of x to change the amount of K+ ion substitution, while ensuring low loss, a microwave dielectric ceramic material with high dielectric and high positive temperature coefficient is obtained; it is especially suitable for frequency temperature coefficient compensation materials, and can be combined with negative frequency temperature coefficient materials to obtain τ f The material has a near-zero cost and is simple to prepare, making it easy for industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of electronic ceramics and their manufacture, and in particular relates to a high-dielectric and high-positive temperature coefficient microwave dielectric ceramic material and a preparation method thereof. Background Art

[0002] Microwave dielectric materials play a key role in global society with a wide range of applications, from terrestrial and satellite communications, including the Internet of Things (IoT), software defined radio, GPS and DBS TV, to environmental monitoring via satellite. Today, low-loss dielectric materials are ubiquitous.

[0003] To be used in the microwave frequency field, dielectric ceramics should have a high dielectric constant, excellent quality factor and near-zero frequency temperature coefficient to promote device miniaturization, improve frequency selectivity and ensure high temperature stability.

[0004] Among the many microwave dielectric ceramics, ABO 3 Perovskite ceramics have been widely studied due to their high reliability and play an important role in the manufacture of electronic components. 3 It is an early ferroelectric compound with an orthorhombic perovskite structure and exhibits excellent dielectric properties. r =113.76,Q×f=8824GHz,andτ f = +645ppm / ℃. Used to adjust MgTiO 3 The microwave dielectric properties of 0.92MgTiO 3 -0.08NaTaO 3 Ceramics, achieving a near-zero τ f However, the choice of frequency temperature coefficient compensation materials is limited, and it is necessary to design and develop new resonant frequency temperature coefficient compensation materials. Summary of the invention

[0005] In view of the above problems or shortcomings, the present invention aims to improve NaTaO 3 The microwave dielectric properties of a new type of resonant frequency temperature coefficient compensation material are developed, and a new type of high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material and its preparation method are provided.

[0006] A high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material, the chemical formula of which is Na 1-x K x TaO 3 (x = 0.025-0.15), the raw material composition is Na 2 CO 3 , K 2 CO 3 and Ta 2 O 5, synthesized by solid phase method; has a high dielectric constant of 127-176 and a loss as low as 3.46×10 -4 , ultra-high forward resonant frequency temperature coefficient of 730-920ppm / ℃.

[0007] Furthermore, the above-mentioned high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material is used as a frequency temperature coefficient compensation material to adjust the MgTiO 3 The microwave dielectric properties of f Ceramics with a value close to zero.

[0008] The preparation method of the above-mentioned high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material comprises the following specific steps:

[0009] Step 1: Sodium carbonate Na 2 CO 3 Potassium carbonate K 2 CO 3 and tantalum pentoxide Ta 2 O 5 The original powder is according to the chemical formula Na 1-x K x TaO 3 (x=0.025-0.15) ratio for material preparation;

[0010] Step 2: Planetarily ball mill the raw materials prepared in step 1 according to the mass ratio of powder, zirconium oxide balls and anhydrous ethanol of 1:4-5:2-3, mix for 4-8 hours, take out and dry at 60°C-90°C, sieve with a 60-200 mesh sieve, and then pre-calculate in an atmospheric atmosphere at 1000°C-1200°C for 3-6 hours.

[0011] Step 3, the powder pre-sintered in step 2 is mixed by planetary ball milling for 2-6 hours according to the mass ratio of powder, zirconium oxide ball and anhydrous ethanol of 1:4-5:1-2, and then taken out and dried at 60°C-90°C; after drying, a PVA solution accounting for 2-5% of the total mass of the dried material is added as a binder to granulate and press into shape; finally, it is sintered in an atmosphere of 1500°C-1550°C for 4-6 hours to obtain a high dielectric and high positive temperature coefficient microwave dielectric ceramic material.

[0012] The present invention introduces K from the raw materials 2 CO 3 , considering K + Ions and Na + The ions have similar ionic radius, so that in the crystal structure, K + Ions can enter the lattice site to form a solid solution. +The introduction of ions helps the densification and grain growth of ceramics, improves its quality factor, and finally produces a new type of high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material. The preparation method is solid phase sintering method, which is simple in process.

[0013] In summary, the Na 1-x K x TaO 3 Ceramics have a large dielectric constant, low loss, and ultra-high forward temperature coefficient, and are particularly suitable for frequency temperature coefficient compensation materials. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 is the XRD diffraction pattern of Example 6-10;

[0015] Figure 2 This is a SEM image of the surface morphology of Example 6-9 after thermal etching at 1500°C for 30 minutes;

[0016] Figure 3 This is a SEM image of the surface morphology of Example 10 after thermal corrosion at 1500°C for 30 minutes. DETAILED DESCRIPTION

[0017] The present invention is described in detail below with reference to the accompanying drawings and embodiments.

[0018] Material chemical formulaNa 1-x K x TaO 3 (x=0.025-0.15), the material of the present invention is prepared by a solid phase method, and the specific steps of the embodiment are as follows:

[0019] Step 1: Add anhydrous sodium carbonate Na 2 CO 3 、Anhydrous potassium carbonate K 2 CO 3 and tantalum pentoxide Ta 2 O 5 The original powder is according to the chemical formula Na 1-x K x TaO 3 (x=0.025-0.15) ratio for material preparation.

[0020] Step 2: Planetarily ball mill the raw materials prepared in step 1 according to the mass ratio of powder, zirconium oxide balls and anhydrous ethanol of 1:5:2, mix for 4 hours, take out and dry at 70°C, sieve with a 60-mesh sieve, and then pre-calculate in an atmospheric atmosphere at 1150°C for 4 hours.

[0021] Step 3, the powder pre-sintered in step 2 is mixed by planetary ball milling for 4 hours according to the mass ratio of powder, zirconium oxide ball and anhydrous ethanol of 1:5:1, and then taken out and dried at 70°C; after drying, a PVA solution accounting for 5% of the total mass of the dried material is added as a binder to granulate and press into shape; finally, it is sintered in an atmosphere of 1500°C-1550°C for 4 hours to obtain a high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material.

[0022] The composition and microwave dielectric properties of each embodiment are as follows:

[0023]

[0024]

[0025]

[0026]

[0027] From the table above, we can see that as x increases from 0.025 to 0.15, the dielectric constant of the sample continues to increase, the quality factor reaches a maximum value at x = 0.05 and then decreases, and the resonant frequency temperature coefficient gradually increases. All samples show lower loss and higher ε r and τ f The best microwave dielectric performance ε was obtained in Example 7. r =163.29, Q×f=9091GHz (f=3.15GHz), tanδ=3.46×10 -4 , τ f =+809.52ppm / ℃.

[0028] Figure 1 (a) shows the XRD diffraction patterns of Examples 6, 7, 8, 9, and 10 (No. 6-10). All the diffraction peaks are consistent with the orthorhombic structure NaTaO with space group Pmcn (62). 3 (PDF#73-0878). In the range of x = 0.025-0.15, the introduction of K+ did not bring about a second phase, and a good Na 1-x K x TaO 3 Solid solution. Figure 1 (b) is the magnified diffraction peaks of the (101) and (121) crystal planes, which move to lower angles. According to the Bragg diffraction law, the left shift of the peak position is caused by the increase in the unit cell volume. 3 For 1-x K x TaO 3 (x=0.025-0.15) K in ceramics +The ionic radius of the ion is larger than that of Na at the same coordination number. + ions, causing the cell volume to increase, so the diffraction peak shifts to the left.

[0029] Figure 2 (a) to (d) and Figure 3 The surface morphology SEM images of Examples 6, 7, 8, 9, and 10 after thermal etching at 1500℃ for 30 minutes are shown in order. + Substitution helps grain growth and ceramic densification, but further increasing the amount of K+ substitution will inhibit grain development, cause microstructural inhomogeneity, and even worse cracking (such as Figure 3 ). In particular, Figure 2 (b) has a larger average grain size (about 3.58 μm), better densification and better uniformity.

[0030] In summary, the present invention adopts K + Ion replacement of Na + Designed by Na 1-x K x TaO 3 Ceramic system, by adjusting the x value to change K + The ion substitution amount ensures low loss while obtaining a microwave dielectric ceramic material with high dielectric constant and high positive temperature coefficient. It is particularly suitable for frequency temperature coefficient compensation materials and can be compounded with negative frequency temperature coefficient materials to obtain materials with near-zero τf. The preparation method is simple and easy to industrialize.

Claims

1. A high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material, characterized in that: The chemical formula is Na 1-x K x TaO3, the raw material composition is Na2CO3, K2CO3 and Ta2O5, synthesized by solid phase method; x = 0.05, pre-sintering at 1150 °C, sintering at 1550 °C; dielectric constant 163.29, loss 3.46 × 10 -4 , resonant frequency temperature coefficient 809.52ppm / ℃.

2. The high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material according to claim 1, characterized in that: Adjusting the microwave dielectric properties of MgTiO3 as a frequency temperature coefficient compensation material to obtain τ f Ceramics with a value close to zero.

3. The method for preparing a high dielectric constant and high positive temperature coefficient microwave dielectric ceramic material according to claim 1, characterized in that: The specific steps are as follows: Step 1: Prepare the original powders of sodium carbonate Na2CO3, potassium carbonate K2CO3 and tantalum pentoxide Ta2O5 according to the chemical formula Na 1- x K x TaO3 is prepared in proportion, x = 0.05; Step 2, the raw materials prepared in step 1 are subjected to planetary ball milling according to the mass ratio of powder, zirconium oxide balls and anhydrous ethanol of 1:4-5:2-3, mixed for 4-8 hours, taken out and dried at 60°C-90°C, sieved with a 60-200 mesh sieve, and then pre-calcined in an atmospheric atmosphere at 1150°C for 3-6 hours; Step 3, the powder pre-sintered in step 2 is mixed by planetary ball milling for 2-6 hours according to the mass ratio of powder, zirconium oxide ball and anhydrous ethanol of 1:4-5:1-2, and then taken out and dried at 60°C-90°C; after drying, a PVA solution accounting for 2-5% of the total mass of the dried material is added as a binder to granulate and press into shape; finally, it is sintered in an atmosphere at 1550°C for 4-6 hours to obtain a high dielectric and high positive temperature coefficient microwave dielectric ceramic material.