A battery and its preparation device and preparation method

By forming a multi-layer diaphragm structure at the starting section of the material belt of the battery core and applying a glue layer, the problem of diaphragm collapse is solved, the stability and welding efficiency of the core hole are improved, and the structural performance and product quality of the battery are improved.

CN117133966BActive Publication Date: 2024-11-08CALB GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311063951.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-22
Publication Date
2024-11-08
Estimated Expiration
2043-08-22

AI Technical Summary

Technical Problem

During the formation of the battery core, the diaphragm close to the core hole is prone to wrinkle and collapse, affecting the quality and efficiency of welding operations.

Method used

By forming a multi-layer diaphragm structure at the starting section of the material tape beyond the electrode sheet, and applying a glue layer on the surface of the diaphragm, the peel strength between the diaphragm is ensured ≥0.04N/cm, and the adhesion effect and stability of the diaphragm are enhanced. Prevent collapse.

Benefits of technology

It improves the structural stability of the core hole, facilitates welding operation, reduces operation difficulty, and improves product yield and battery structural performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117133966B_ABST
    Figure CN117133966B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of battery technology, and proposes a battery and a preparation device and method thereof. The battery includes a cylindrical winding core formed by winding a material strip, the material strip includes a diaphragm and a pole piece, and along the extension direction of the material strip, the diaphragm is arranged beyond the pole piece at the starting section of the material strip; the winding core has a winding core hole, and the part of the diaphragm that exceeds the pole piece surrounds and forms the winding core hole; along the extension direction of the material strip, the part of the diaphragm that exceeds the pole piece forms the innermost circle structure of the winding core in the radial direction, and the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2; the diaphragm is provided with a glue layer, and the peel strength between the diaphragms in the innermost circle structure is ≥0.04N / cm. The battery can improve the shaping effect of the diaphragm in the winding core near the winding core hole, which is convenient for welding operations at the winding core hole to improve the structural performance of the winding core.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a battery and a manufacturing device and method thereof. Background Art

[0002] The battery cell in the battery can be a roll core, that is, the battery cell can be formed by winding the material strip. It is worth noting that in the process of forming the roll core, a winding needle is required to wrap and support the material strip; after the roll core is prepared, the winding needle needs to be pulled out of the roll core to form a roll core hole inside the roll core. However, when the needle is pulled out of the roll core, the diaphragm near the needle is prone to wrinkles, which can easily cause the inner circle diaphragm near the roll core hole to deform and collapse after the needle is pulled out, affecting the subsequent welding operation. Summary of the invention

[0003] The present invention provides a battery and a preparation device and method thereof. The battery can improve the shaping effect of a diaphragm in a winding core near a winding core hole, facilitate welding operations at the winding core hole, and improve the structural performance of the winding core.

[0004] In order to achieve the above object, the present invention provides the following technical solutions:

[0005] According to a first aspect of the present invention, there is provided a battery, comprising a cylindrical winding core formed by winding a material strip, the material strip comprising a diaphragm and a pole piece, wherein the diaphragm is arranged beyond the pole piece at the starting section of the material strip along the extension direction of the material strip; the winding core has a winding core hole, and the portion of the diaphragm exceeding the pole piece surrounds and forms the winding core hole; along the extension direction of the material strip, the portion of the diaphragm exceeding the pole piece forms the innermost circle structure of the winding core in the radial direction, and the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2; the diaphragm is provided with a glue layer, and the peel strength between the diaphragms in the innermost circle structure is ≥0.04N / cm.

[0006] It should be noted that in the battery provided by the present application, the diaphragm at the starting section of the material strip that exceeds the pole piece setting forms the innermost ring structure of the winding core in the radial direction. After winding, the number of turns of the diaphragm located in the innermost ring structure is at least two, and the diaphragms of adjacent ring layers are bonded by the adhesive layer on the surface of the diaphragm so that the peel strength between the diaphragms is ≥0.04N / cm. Accordingly, the battery can improve the relative stability of the diaphragm located in the innermost ring structure, avoid the collapse and deformation of the diaphragm located in the innermost ring structure, so as to ensure that the winding core hole has a stable structural form, facilitate welding operations in the winding core hole, and reduce the difficulty of operation.

[0007] At the same time, it is worth noting that in the process of winding to form a core, the viscosity of the glue layer on the surface of the diaphragm can increase when heated, so as to improve the bonding effect of the glue layer on the diaphragm in the innermost ring structure, reduce the difficulty of bonding between diaphragms, and improve the product yield of the core; at the same time, the diaphragm may shrink due to heat, so as to assist in improving the shaping effect of the multi-layer diaphragm located in the innermost ring structure after bonding, prevent the diaphragm located in the innermost ring structure from collapsing into the core hole, further facilitate welding operations in the core hole, and reduce the difficulty of operation.

[0008] According to a second aspect of the present invention, there is provided a battery preparation device, comprising a winding needle, wherein the outer circumferential surface of the winding needle is used to fix the diaphragm in the material strip to wind it into a cylindrical core; the temperature of the outer circumferential surface of the winding needle is adjustable within the range of 20°C to 150°C to control the peel strength between the diaphragms in the innermost circle structure of the core to be ≥0.04N / cm, wherein the material strip comprises a diaphragm and a pole piece, and along the extension direction of the material strip, the diaphragm is arranged beyond the pole piece at the starting section of the material strip, and the portion of the diaphragm exceeding the pole piece forms the innermost circle structure of the core in the radial direction, the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2, and the diaphragm is provided with a glue layer.

[0009] It should be noted that in the process of winding the battery preparation device provided in the embodiment of the present application to form a core, the diaphragm at the starting section of the material strip is fixed on the outer peripheral surface of the winding needle; after the diaphragm is fixed, the material strip can be rotated and wound with the winding needle to form a core. During the winding of the material strip by the winding needle, the part of the diaphragm beyond the pole piece setting at the starting section of the material strip forms the innermost ring structure of the core in the radial direction, and the viscosity of the adhesive layer on the surface of the diaphragm can be increased when heated to improve the bonding effect of the adhesive layer on the diaphragm in the innermost ring structure, reduce the bonding difficulty between the diaphragms, and improve the product yield of the core; at the same time, the diaphragm may shrink due to heat to assist in improving the shaping effect of the multi-layer diaphragms in the innermost ring structure after bonding, and prevent the diaphragm located in the innermost ring structure from collapsing into the core hole, so as to facilitate welding operations in the core hole and reduce the difficulty of operation.

[0010] At the same time, in the battery prepared by the preparation device, the number of circles of the diaphragm in the innermost circle structure is at least two, and the diaphragms of adjacent circles are bonded by the adhesive layer on the surface of the diaphragm, so that the peel strength between the diaphragms is ≥0.04N / cm. Accordingly, the battery can improve the relative stability of the diaphragm in the innermost circle structure, avoid the collapse and deformation of the diaphragm in the innermost circle structure, so as to ensure that the winding core hole has a stable structural form, facilitate welding operations in the winding core hole, and reduce the difficulty of operation.

[0011] According to a third aspect of the present invention, there is provided a method for preparing a battery, which is used to prepare a battery provided by any technical solution in the first aspect above, and the preparation method comprises:

[0012] Providing a material strip, the material strip comprising a diaphragm and a pole piece, wherein along the extension direction of the material strip, the diaphragm is arranged beyond the pole piece at the starting section of the material strip;

[0013] The material strip is wound to form a cylindrical core, the core having a core hole, wherein the portion of the diaphragm extending beyond the pole piece surrounds and forms the core hole; along the extension direction of the material strip, the portion of the diaphragm extending beyond the pole piece forms the innermost circle structure of the core in the radial direction, the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2; the diaphragm is provided with a glue layer, and the peel strength between the diaphragms in the innermost circle structure is ≥0.04N / cm.

[0014] It should be noted that in the battery prepared by the preparation method of the battery provided in the present application, the diaphragm at the starting section of the material strip beyond the pole piece setting forms the innermost ring structure of the winding core in the radial direction. After winding, the number of turns of the diaphragm located in the innermost ring structure is at least two, and the diaphragms of adjacent rings are bonded by the adhesive layer on the surface of the diaphragm, so that the peel strength between the diaphragms is ≥0.04N / cm. Accordingly, the battery can improve the relative stability of the diaphragm located in the innermost ring structure, avoid the collapse and deformation of the diaphragm located in the innermost ring structure, so as to ensure that the winding core hole has a stable structural form, facilitate welding operations in the winding core hole, and reduce the difficulty of operation.

[0015] At the same time, it is worth noting that in the process of winding to form a core, the viscosity of the glue layer on the surface of the diaphragm can increase when heated, so as to improve the bonding effect of the glue layer on the diaphragm in the innermost ring structure, reduce the difficulty of bonding between diaphragms, and improve the product yield of the core; at the same time, the diaphragm may shrink due to heat, so as to assist in improving the shaping effect of the multi-layer diaphragm located in the innermost ring structure after bonding, prevent the diaphragm located in the innermost ring structure from collapsing into the core hole, further facilitate welding operations in the core hole, and reduce the difficulty of operation. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to better understand the present application, reference may be made to the embodiments shown in the following drawings. The components in the drawings are not necessarily to scale, and related elements may be omitted in order to emphasize and clearly illustrate the technical features of the present application. In addition, related elements or components may have different arrangements as known in the art. In addition, in the drawings, the same reference numerals represent the same or similar components in each drawing. Among them:

[0017] Figure 1 A schematic diagram of the structure of a roll core in a battery provided in an embodiment of the present application;

[0018] Figure 2 for Figure 1 A top view of the structure in the middle;

[0019] Figure 3 A schematic diagram of the structure of a battery manufacturing device provided in an embodiment of the present application;

[0020] Figure 4 A flow chart of a method for preparing a battery provided in an embodiment of the present application.

[0021] The following are the descriptions of the reference numerals:

[0022] 100, winding core; 110, winding core hole; 200, winding needle; 210, outer needle; 220, inner needle; 01, diaphragm; 02, adhesive layer. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the example embodiments of the present application to clearly and completely describe the technical solutions in the example embodiments of the present application. The example embodiments described herein are only for illustrative purposes and are not intended to limit the scope of protection of the present application. Therefore, it should be understood that various modifications and changes can be made to the example embodiments without departing from the scope of protection of the present application.

[0024] In the description of the present application, unless otherwise expressly specified and limited, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; the term "plurality" refers to two or more; the term "and / or" includes any and all combinations of one or more associated listed items. In particular, mentioning "the / " object or "an" object is also intended to indicate one of a possible plurality of such objects.

[0025] Unless otherwise specified or explained, the terms "connection", "fixed", etc. should be understood in a broad sense. For example, "connection" can be a fixed connection, a detachable connection, an integral connection, an electrical connection, or a signal connection; "connection" can be a direct connection or an indirect connection through an intermediate medium. For those skilled in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0026] Further, in the description of the present application, it should be understood that the directional words such as "upper", "lower", "inner", "outer" and the like described in the example embodiments of the present application are described at the angles shown in the accompanying drawings and should not be understood as limitations on the example embodiments of the present application. It should also be understood that, in the context, when it is mentioned that an element or feature is connected to another element (one or more) "upper", "lower", or "inner", "outer", it can not only be directly connected to the other (one or more) elements "upper", "lower", "inner", "outer", but also can be indirectly connected to the other (one or more) elements "upper", "lower", "inner", "outer" through an intermediate element.

[0027] In a first aspect, an embodiment of the present application provides a battery. Figure 1 A schematic diagram of the structure of a roll core in a battery provided in an embodiment of the present application; Figure 2 for Figure 1 Please refer to the top view of the structure. Figure 1 and Figure 2 As shown in the structure, the battery includes a cylindrical core 100 formed by winding a material strip, the material strip includes a diaphragm 01 and a pole piece, and along the extension direction of the material strip, the diaphragm 01 is arranged beyond the pole piece at the starting section of the material strip; the core 100 has a core hole 110, and the part of the diaphragm 01 that exceeds the pole piece surrounds and forms the core hole 110; along the extension direction of the material strip, the part of the diaphragm 01 that exceeds the pole piece forms the innermost circle structure of the core 100 in the radial direction, and the number of circles of the diaphragm 01 in the innermost circle structure is greater than or equal to 2; the diaphragm 01 is provided with a glue layer 02, and the peel strength between the diaphragms 01 in the innermost circle structure is ≥0.04N / cm.

[0028] It should be understood that in the process of forming the winding core 100, the diaphragm 01 at the end of the material strip needs to be fixed on the surface of the support member (such as the winding needle 200), and then the material strip is wound around the support member. After the preparation of the winding core 100, the support member will be withdrawn, and the winding core 100 will form the winding core hole 110 at the corresponding support member position. It is worth noting that the starting part of the material strip only has the diaphragm 01. In other words, the part of the winding core 100 surrounding and forming the side wall of the winding core hole 110 is the diaphragm 01.

[0029] After the material strip is wound to form the core 100, a welding tool is required to be inserted into the core hole 110 to weld the core hole 110 and improve the structural performance of the core 100. It should be noted that in the battery provided in the embodiment of the present application, the diaphragm 01 at the starting section of the material strip beyond the portion where the pole piece is set forms the innermost circle structure of the core 100 in the radial direction. After winding, the number of circles of the diaphragm 01 located in the innermost circle structure is at least two circles, and the diaphragms 01 of adjacent circles are bonded by the adhesive layer 02 on the surface of the diaphragm 01, so that the peel strength between the diaphragms 01 is ≥0.04N / cm. Accordingly, the battery can improve the relative stability of the diaphragm 01 located in the innermost circle structure, avoid collapse and deformation of the diaphragm 01 located in the innermost circle structure, so as to ensure that the core hole 110 has a stable structural form, facilitate welding operations in the core hole 110, and reduce the difficulty of operation.

[0030] At the same time, it is worth noting that in the process of winding to form the core 100, the viscosity of the glue layer 02 on the surface of the diaphragm 01 can increase when heated, so as to improve the bonding effect of the glue layer 02 on the diaphragm 01 in the innermost circle structure, reduce the bonding difficulty between the diaphragms 01, and improve the product yield of the core 100; at the same time, the diaphragm 01 may shrink when heated, so as to assist in improving the shaping effect of the multi-layer diaphragm 01 located in the innermost circle structure after bonding, and prevent the diaphragm 01 located in the innermost circle structure from collapsing toward the core hole 110, further facilitating welding operations in the core hole 110 and reducing operational difficulty.

[0031] For example, the innermost ring structure of the diaphragm 01 in the battery provided in the embodiment of the present application is shaped to prevent the diaphragm 01 at the side wall of the winding core hole 110 from collapsing, so as to provide a larger operating space for the ejector pin for subsequent resistance welding, ultrasonic welding or penetration welding using the winding core hole 110.

[0032] In addition, when specifically setting up the battery provided in the embodiment of the present application, the number of turns of the diaphragm 01 located in the innermost ring structure needs to be greater than 2 turns, so as to form effective protection for the core 100 when the subsequent welding tooling extends into the core hole 110, and to prevent the active coating on the surface of the pole piece in the core 100 from being scratched and falling off. Of course, the number of turns of the diaphragm 01 located in the innermost ring structure cannot be too many, so as to avoid the diaphragm 01 occupying too large a proportion in the core 100 and affecting the energy density of the core 100. Accordingly, in one embodiment, the number of turns of the diaphragm 01 in the innermost ring structure is less than or equal to 12, so as to ensure the energy density of the core 100 and enhance the protective effect of the diaphragm 01 on the pole piece.

[0033] It is worth noting that when preparing the diaphragm 01, the glue layer 02 can be simultaneously formed on the membrane surface to simplify the preparation process.

[0034] For example, with the diaphragm 01 fixed on the surface of the winding needle 200 as the starting point, the next circle of diaphragm 01 can be bonded and fixed by the adhesive layer 02 on the surface of the diaphragm 01 when winding the previous circle of diaphragm 01. Accordingly, the structural setting can reduce the difficulty of winding and improve the preparation rate of the core 100; moreover, the structural setting can avoid the movement and dislocation between adjacent film layers, and can improve the yield of the core 100 obtained by winding, as well as improve the structural yield of the battery using the core 100.

[0035] Of course, the adhesive layer 02 on the surface of the diaphragm 01 can also be prepared on the surface of the diaphragm 01 after the preparation of the diaphragm 01 is completed and before winding; or, the adhesive layer 02 on the surface of the diaphragm 01 can also be sprayed or brushed on the surface of the diaphragm 01 during the winding process when the winding strip forms the winding core 100. The specific settings can be made according to needs and will not be repeated here.

[0036] In one embodiment, please continue to refer to Figure 2In the structure shown, along the radial direction of the winding core 100 , the thickness of the adhesive layer 02 ranges from 1 μm to 4 μm.

[0037] It should be noted that in this embodiment, the upper limit of the thickness of the adhesive layer 02 is 4 μm to prevent the thickness of the adhesive layer 02 from being too thick, resulting in the total thickness of the adhesive layer 02 in the winding core 100 being too large and affecting the battery energy density; the lower limit of the adhesive layer 02 is 1 μm to prevent the thickness of the adhesive layer 02 from being too thin and unable to function. Therefore, in this embodiment, by setting the thickness of the adhesive layer 02 within the above range, the adhesive layer 02 can better play a bonding effect and ensure the energy density of the battery.

[0038] For example, when the thickness of the adhesive layer 02 is specifically set, it can be set to one of the following values.

[0039] 1μm, 1.5μm, 2μm, 2.5μm, 3μm, 3.5μm, 4μm.

[0040] In one implementation, please continue to refer to Figure 2 In the structure shown, the material of the adhesive layer 02 is one of polyvinylidene difluoride (PVDF), polytetrafluoroethylene (PTFE), polymethyl methacrylate (PMMA), polyethylene oxide (PEO) or polyacrylic acid (PAA).

[0041] It is worth noting that when the adhesive layer 02 is a multi-layer structure, the material of each layer structure can be one of the above materials, and the materials of different layer structures can be different.

[0042] In addition, the adhesive layer 02 may be set to be a thermosetting adhesive. Thermosetting adhesive has the advantages of fast curing and high strength, which can improve the bonding effect and thus ensure that the peeling strength between the diaphragms 01 located in the innermost ring structure is greater than a preset value.

[0043] In one embodiment, please continue to refer to Figure 2 In the structure shown, along the radial direction of the winding core 100 , the thickness of the diaphragm 01 ranges from 7 μm to 20 μm.

[0044] It should be noted that, in this embodiment, the upper limit of the thickness of the diaphragm 01 is set to 20 μm to prevent the diaphragm 01 from being too thick and affecting the energy density; the lower limit of the thickness of the diaphragm 01 is set to 7 μm to prevent the diaphragm 01 from being too thin and unable to be heat-formed to form a stable winding core hole 110.

[0045] In one embodiment, please continue to refer to Figure 2 In the structure shown, the diameter range of the winding core 100 is ≥ 40 mm.

[0046] It should be understood that when the diameter of the core 100 is greater than 40 mm, the core 100 can be called a large core 100. When preparing the large core 100, the winding tension is large, and the internal diaphragm 01 is more likely to collapse inward, thereby causing interference welding, affecting exhaust, and the inner ring diaphragm 01 is insufficient to support the inner ring pole piece, and causing problems such as poor bonding of the inner ring positive and negative electrodes, wrinkles of the negative electrode, or lithium precipitation.

[0047] It should be noted that the structural setting in the embodiment of the present application can ensure the shaping effect of the multilayer diaphragm 01 located in the innermost circle structure in the large winding core 100 formed by winding after bonding, prevent the diaphragm 01 located in the innermost circle structure from collapsing toward the winding core hole 110, ensure that the winding core hole 110 has a stable structural form, facilitate welding operations in the winding core hole 110, reduce the difficulty of operation, and improve the structural performance of the battery.

[0048] In one embodiment, the ratio of the diameter of the winding core hole 110 to the diameter of the winding core 100 is 0.06-0.4.

[0049] It should be noted that the larger the proportion of the core hole 110, the stricter the peel strength requirement for the internal diaphragm 01. In the embodiment of the present application, the peel strength between the diaphragms 01 is set to be ≥ 0.04N / cm. Accordingly, when the core hole 110 accounts for a large proportion, the relative stability of the diaphragm 01 in the innermost ring structure can be guaranteed, and the collapse and deformation of the diaphragm 01 located in the innermost ring structure can be avoided, so as to ensure that the core hole 110 has a stable structural form, facilitate welding operations in the core hole 110, and reduce the difficulty of operation.

[0050] In one embodiment, the battery provided in the embodiment of the present application further includes a shell, and the shape of the shell can be cylindrical or hexagonal. The winding core 100 in the above structure is placed inside the shell to form a cylindrical battery or a hexagonal battery.

[0051] It is worth noting that the winding core 100 includes a main body and a pole ear portion extending from the main body, and the pole ear portion is connected to the pole column assembly on the surface of the shell to achieve electrical connection between the internal structure and the external structure of the battery. The main body of the winding core 100 is formed by winding pole sheets, which are specifically divided into positive pole sheets and negative pole sheets, and the positive pole sheets and negative pole sheets are separated by a diaphragm 01 to prevent short circuits. Exemplarily, the positive pole sheet includes a current carrier and a positive polarity active material coated on the surface of the current carrier, wherein the current carrier also has a portion not coated by the active material, which forms a pole ear, and the multi-layer pole ear is folded to form a positive pole ear portion, and the pole ear portion is connected to the pole column assembly at the shell to form a positive electrode; the negative pole sheet includes a current carrier and a negative polarity active material coated on the surface of the current carrier, wherein the portion of the current carrier not coated by the active material forms a pole ear, and the multi-layer pole ear is folded to form a negative pole ear portion, and the pole ear portion is connected to the pole column assembly at the shell to form a negative electrode.

[0052] In one embodiment, the battery provided in the embodiment of the present application further includes an electrolyte, and the electrolyte is filled inside the shell.

[0053] It should be understood that the electrolyte is composed of electrolytes, organic solvents and additives. The electrolyte is an important material inside the battery. It can transport lithium ions and provide the power required by the battery. It is a key component for the battery to exert energy.

[0054] In a second aspect, an embodiment of the present application provides a battery preparation device. Figure 3 This is a schematic diagram of the structure of the battery manufacturing device provided in the embodiment of the present application. Figure 1 and Figure 2 refer to Figure 3 As shown in the structure, the battery preparation device includes a winding needle 200, the outer peripheral surface of the winding needle 200 is used to fix the diaphragm 01 in the material strip to wind up a cylindrical winding core 100; the temperature of the outer peripheral surface of the winding needle 200 is adjustable in the range of 20°C to 150°C to control the peel strength between the diaphragms 01 in the innermost circle structure of the winding core 100 to be ≥0.04N / cm, wherein the material strip includes a diaphragm 01 and a pole piece, and along the extension direction of the material strip, the diaphragm 01 is arranged beyond the pole piece at the starting section of the material strip, and the portion of the diaphragm 01 that exceeds the pole piece forms the innermost circle structure of the winding core 100 in the radial direction, the number of turns of the diaphragm 01 in the innermost circle structure is greater than or equal to 2, and the diaphragm 01 is provided with a glue layer 02.

[0055] It should be understood that in the process of winding to form the core 100, the diaphragm 01 at the starting section of the material strip is fixed on the outer peripheral surface of the winding needle 200; after the diaphragm 01 is fixed, the material strip can be rotated and wound with the winding needle 200 to form the core 100. In the process of the winding needle 200 winding the material strip, the diaphragm 01 at the starting section of the material strip beyond the pole piece setting forms the innermost ring structure of the core 100 in the radial direction, and the adhesive layer 02 on the surface of the diaphragm 01 can increase its viscosity when heated to improve the bonding effect of the adhesive layer 02 on the diaphragm 01 in the innermost ring structure, reduce the bonding difficulty between the diaphragms 01, and improve the product yield of the core 100; at the same time, the diaphragm 01 may shrink when heated to assist in improving the shaping effect of the multi-layer diaphragm 01 located in the innermost ring structure after bonding, prevent the diaphragm 01 located in the innermost ring structure from collapsing toward the core hole 110, and further facilitate welding operations in the core hole 110 to reduce the difficulty of operation.

[0056] At the same time, in the battery prepared by the preparation device, the number of circles of the separator 01 in the innermost circle structure is at least two, and the adjacent circles of the separator 01 are bonded by the adhesive layer 02 on the surface of the separator 01, so that the peel strength between the separators 01 is ≥ 0.04N / cm. Accordingly, the battery can improve the relative stability of the separator 01 in the innermost circle structure, avoid the collapse and deformation of the separator 01 in the innermost circle structure, so as to ensure that the winding core hole 110 has a stable structural form, facilitate welding operations in the winding core hole 110, and reduce the difficulty of operation.

[0057] It should be noted that in the battery preparation device provided in this embodiment, the multilayer diaphragm 01 located in the innermost circle structure can be shaped under heating after bonding, so as to improve the structural stability of the core hole 110 and prevent the diaphragm 01 located in the innermost circle structure from collapsing toward the core hole 110; at the same time, after the diaphragm 01 in the innermost circle structure is shaped, the outer circle of the core 100 can match a higher winding tension, thereby manufacturing a tighter core 100 and improving the energy density of the battery cell.

[0058] It is worth noting that during the winding process of the winding core 100, the temperature of the outer peripheral surface should not be too high. If the temperature is too high, the diaphragm 01 and the winding needle 200 will be too tightly connected to make it difficult to withdraw the needle, or the diaphragm 01 will be deformed and closed due to heat. Therefore, in the embodiment of the present application, the upper limit of the temperature rise of the outer peripheral surface is set to 150°C to ensure the shaping effect of the diaphragm 01 forming the winding core hole 110.

[0059] Of course, the temperature at the peripheral surface should not be too low to prevent the diaphragm 01 and the adhesive layer 02 from being unable to be shaped at low temperatures. Therefore, in the embodiment of the present application, the lower limit of the temperature rise of the peripheral surface is set to 20° C. to ensure the shaping effect of the diaphragm 01 forming the core hole 110 .

[0060] In one embodiment, the winding needle 200 has a winding forming state and a needle withdrawal state. When the winding needle 200 is in the winding forming state, the temperature of the outer circumference of the winding needle 200 rises, and the winding needle 200 can rotatably wind the material strip around its own axis to form a cylindrical winding core 100; when the winding needle 200 is in the needle withdrawal state, the temperature of the outer circumference of the winding needle 200 drops, and the winding needle 200 can be withdrawn from the winding core 100.

[0061] It should be noted that, in the present embodiment, the temperature of the winding needle 200 in the winding forming state is higher than the temperature of the winding needle 200 in the needle withdrawal state, wherein the temperature of the winding needle 200 rises when winding the material strip, thereby heating the diaphragm 01 so that the diaphragms 01 adhere tightly to each other to form a whole, thereby avoiding the collapse of the diaphragm 01 at a later stage; the temperature of the winding needle 200 drops when withdrawing the needle, thereby facilitating the withdrawal of the winding needle 200, thereby improving the yield of the winding core 100 obtained after withdrawing the needle.

[0062] When specifically setting the temperature of the winding needle 200 in the winding state, the temperature range of the winding needle 200 can be adjusted according to the winding degree of the winding core 100 .

[0063] In one embodiment, the winding forming state includes a winding state and a shaping state. When the winding needle 200 is in the winding state, the temperature of the outer circumference of the winding needle 200 is in the range of 20°C to 90°C, and the winding needle 200 can rotatably wind the material strip around its own axis to form an initial winding core 100; when the winding needle 200 is in the shaping state, the temperature of the outer circumference of the winding needle 200 is in the range of 60°C to 120°C, and the winding needle 200 is used to shape the initial winding core 100 formed by the winding state to form a cylindrical winding core 100.

[0064] It is worth noting that, in this embodiment, the temperature of the winding needle 200 in the winding state is lower than or equal to the temperature of the winding needle 200 in the shaping process.

[0065] For example, in a specific embodiment, the temperature of the winding needle 200 rises in the winding state, but the temperature of the winding needle 200 after heating is lower than the temperature in the shaping state. For example, in the process of winding the battery cell, the temperature of the outer peripheral surface of the winding needle 200 is in the range of 60°C to 90°C. After the winding strip is wound to form the winding core 100, the winding core 100 can be kept on the surface of the winding needle 200, and the temperature of the outer peripheral surface of the winding needle 200 is controlled in the range of 70°C to 110°C for 1s to 20s to shape the diaphragm 01 located in the innermost circle.

[0066] In another specific embodiment, the winding needle 200 is heated in the winding state, and the temperature of the winding needle 200 in the winding state is equal to the temperature in the shaping state. For example, during the process of winding the battery cell, the winding needle 200 has been heated to a certain temperature. After the winding strip is formed into the winding core 100, the winding core 100 can be kept on the surface of the winding needle 200, and the innermost circle of the diaphragm 01 can be shaped at the same temperature during the winding process.

[0067] In another specific embodiment, the temperature of the winding needle 200 does not rise in the winding state, and the temperature of the winding needle 200 rises in the shaping state. For example, during the process of winding the battery cell, the temperature of the winding needle 200 remains unchanged. After the winding strip is wound to form the winding core 100, the winding needle 200 can be heated, and the winding core 100 is kept on the surface of the heated winding needle 200 to shape the innermost circle of the diaphragm 01.

[0068] It is worth noting that after the operations in the above three specific embodiments are completed, the temperature of the outer peripheral surface of the winding needle 200 will drop to complete the needle withdrawal operation.

[0069] In another embodiment, the winding needle 200 has a winding forming state and a needle withdrawal state. When the winding needle 200 is in the winding forming state, the winding needle 200 can rotatably wind the material strip around its own axis to form a cylindrical winding core 100; when the winding needle 200 is in the needle withdrawal state, the winding needle 200 can be withdrawn from the winding core 100; when the winding needle 200 is in the winding forming state and the needle withdrawal state, the temperature of the outer peripheral surface of the winding needle 200 is maintained in the range of 60°C to 120°C.

[0070] It should be noted that in this embodiment, during the process of winding the winding needle 200 to form the winding core 100 and during the process of withdrawing the needle, the temperature of the outer peripheral surface of the winding needle 200 remains unchanged and is maintained at a temperature. For example, the temperature can be maintained at a value within the range of 60°C to 120°C.

[0071] In one embodiment, please refer to Figure 3 In the structure shown, the winding needle 200 includes an inner needle 220 and an outer needle 210. The outer needle 210 has a receiving cavity, and the outer peripheral surface of the outer needle 210 forms at least a part of the outer peripheral surface of the winding needle 200; the inner needle 220 can be inserted and pulled relative to the receiving cavity.

[0072] It is worth noting that the material of the outer needle 210 in this embodiment can be elastic, and the cross-sectional size of the outer needle 210 can change with the insertion and extraction of the inner needle 220 in the accommodating cavity. Specifically, when the inner needle 220 is inserted into the accommodating cavity, the cross-sectional size of the outer needle 210 increases, that is, the cross-sectional size of the outer peripheral surface of the winding needle 200 increases; when the inner needle 220 is pulled out of the accommodating cavity, the cross-sectional size of the outer needle 210 decreases, that is, the cross-sectional size of the outer peripheral surface of the winding needle 200 decreases. Alternatively, the outer needle 210 may have a gap along its outer peripheral surface, which can be filled by the inner needle 220 inserted into the accommodating cavity to change the cross-sectional size of the outer peripheral surface of the winding needle 200.

[0073] It should be noted that this embodiment adopts the form of nesting inner and outer needles 210. After the inner needle 220 is pulled out, the cross-sectional size of the outer peripheral surface of the winding needle 200 is reduced, making it convenient to pull out the needle, which can solve the problem of high temperature causing the winding needle 200 and the innermost circle structure diaphragm 01 to adhere and affect the extraction of the needle.

[0074] It is worth noting that the battery preparation device provided in the embodiment of the present application also includes a driving mechanism, which is connected to the inner needle 220 and is used to drive the inner needle 220 to perform insertion and extraction actions relative to the accommodating cavity.

[0075] It should be noted that, in this embodiment, the structural setting of driving the inner needle 220 by the driving mechanism makes the winding needle 200 provided in the embodiment of the present application easier to use and can improve the convenience of plugging and unplugging operations.

[0076] Specifically, the driving mechanism can drive the inner needle 220 to be inserted into the accommodating cavity of the outer needle 210, so that the inner needle 220 supports the outer needle 210. At this time, the outer needle 210 can be rotated to form the core 100 through multiple rotations. The driving mechanism can also drive the inner needle 220 to pull out of the accommodating cavity of the outer needle 210, so that the outer needle 210 can be pulled out from the inner circle of the core 100 that has been wound into shape, thereby reducing the difficulty of needle extraction.

[0077] In one embodiment, the roughness of the outer circumferential surface of the winding needle 200 is less than or equal to ±(2 μm-2.5 μm).

[0078] Specifically, the roughness of the outer circumference of the winding needle 200 is less than or equal to (2μm to 2.5μm); or, the roughness of the outer circumference of the winding needle 200 is less than or equal to -(2μm to 2.5μm). It should be understood that there is a reference line on the outer circumference of the winding needle 200, which is the profile center line used to evaluate the surface roughness parameters. The reference line can also be called the least squares center line of the profile, that is, within the sampling length, the sum of the squares of the profile deviations of each point on the profile line is the smallest, and has a geometric profile shape. Alternatively, the reference line can also be called the arithmetic mean center line of the profile, that is, within the sampling length, the areas of the profiles on both sides of the center line are equal.

[0079] It is worth noting that the roughness "±" of the outer circumference of the winding needle 200 can be understood as: along the direction away from the outer circumference of the winding needle 200, there are protrusions beyond the reference line and depressions that do not exceed the reference line on the outer circumference surface, and the size of the protrusion is represented by "+", and the size of the depression is represented by "-". Exemplarily, the outer surface of the winding needle 200 is provided with a concave-convex microstructure, which includes a groove microstructure and a protrusion microstructure, and the size range of the protrusion microstructure is less than or equal to +2μm to +2.5μm, and the size range of the groove microstructure is less than or equal to -2μm to -2.5μm.

[0080] It should be noted that by setting the roughness of the outer surface of the outer needle 210 to be less than or equal to ±(2μm~1.5μm), the diaphragm 01 can be prevented from sticking when the needle is withdrawn, so as to ensure the yield of the prepared core 100, thereby improving the structural yield of the battery using the core 100.

[0081] When the needle winding structure 200 in the embodiment of the present application is used, the inner needle 220 can be used to first pull out the outer needle 210 and retract it inwards, thereby facilitating the needle withdrawal.

[0082] In a preferred embodiment, the roughness of the outer surface of the winding needle 200 is less than or equal to ±(1.5μm-2μm). In this embodiment, the concave-convex variation of the outer surface of the winding needle 200 is smaller, which can further prevent the diaphragm 01 from adhering when the needle is withdrawn, so as to ensure the yield of the prepared winding core 100, and further improve the structural yield of the battery using the winding core 100.

[0083] In one embodiment, the winding needle 200 further includes a heating element, which is pre-buried in the winding needle 200. Exemplarily, the heating element may be a heating wire or a heating sheet.

[0084] It should be understood that when the winding needle 200 is divided into an outer needle 210 and an inner needle 220 , the heating element can be pre-buried in the inner needle 220 or the outer needle 210 .

[0085] It is worth noting that the battery preparation device provided in the embodiments of the present application is also used to prepare the battery provided by any technical solution in the first aspect above.

[0086] In a third aspect, an embodiment of the present application provides a method for preparing a battery. Figure 4 Flow chart of the method for preparing a battery provided in the embodiment of the present application, please refer to Figures 1 to 3 refer to Figure 4 The structure shown in the figure, the preparation method of the battery is used to prepare the battery provided by any technical solution in the first aspect above. The preparation method comprises:

[0087] Step S402: providing a material strip, the material strip comprising a diaphragm 01 and a pole piece, and along the extension direction of the material strip, the diaphragm 01 is arranged beyond the pole piece at the starting section of the material strip;

[0088] Step S404: Winding the material strip to form a cylindrical core 100, the core 100 has a core hole 110, wherein the portion of the diaphragm 01 extending beyond the pole piece surrounds and forms the core hole 110; along the extension direction of the material strip, the portion of the diaphragm 01 extending beyond the pole piece forms the innermost circle structure of the core 100 in the radial direction, and the number of circles of the diaphragm 01 in the innermost circle structure is greater than or equal to 2; the diaphragm 01 is provided with a glue layer 02, and the peel strength between the diaphragms 01 in the innermost circle structure is ≥0.04N / cm.

[0089] It should be understood that in the process of forming the core 100, the diaphragm 01 at the end of the material strip is fixed on the surface of the support (e.g., the winding needle 200), and then the material strip is wound around the support to form the core 100 structure. After the core 100 is prepared, the support is withdrawn, and the core 100 forms the core hole 110 at the position corresponding to the support. It is worth noting that the starting part of the material strip only has the diaphragm 01. In other words, the part of the core 100 surrounding and forming the side wall of the core hole 110 is the diaphragm 01.

[0090] It is worth noting that after the material strip is wound to form the core 100, a welding tool needs to be used to extend into the core hole 110 to weld the core hole 110 to improve the structural performance of the core 100. It should be noted that in the battery prepared by the preparation method of the battery provided in the embodiment of the present application, the diaphragm 01 at the starting section of the material strip beyond the setting of the pole piece forms the innermost circle structure of the core 100 in the radial direction. After winding, the number of circles of the diaphragm 01 located in the innermost circle structure is at least two circles, and the diaphragms 01 of adjacent circles are bonded by the adhesive layer 02 on the surface of the diaphragm 01, so that the peel strength between the diaphragms 01 is ≥0.04N / cm. Accordingly, the battery can improve the relative stability of the diaphragm 01 located in the innermost circle structure, avoid the collapse and deformation of the diaphragm 01 located in the innermost circle structure, so as to ensure that the core hole 110 has a stable structural form, facilitate welding operations in the core hole 110, and reduce the difficulty of operation.

[0091] It should be noted that, in the process of winding to form the core 100, the viscosity of the glue layer 02 on the surface of the diaphragm 01 can be increased when heated, so as to enhance the bonding effect of the glue layer 02 on the diaphragm 01 in the innermost ring structure, reduce the bonding difficulty between the diaphragms 01, and improve the product yield of the core 100; at the same time, the diaphragm 01 may shrink due to heat, so as to assist in enhancing the shaping effect of the multi-layer diaphragm 01 located in the innermost ring structure after bonding, and prevent the diaphragm 01 located in the innermost ring structure from collapsing toward the core hole 110, further facilitating welding operations in the core hole 110 and reducing operational difficulty.

[0092] In one embodiment, in step S404, the method of winding the material strip to form a cylindrical winding core 100 includes:

[0093] Fix the diaphragm 01 which is arranged beyond the pole piece in the starting section of the material strip to the outer peripheral surface of the winding needle 200;

[0094] The material strip is wound by rotating the winding needle 200 to form a cylindrical winding core 100;

[0095] The winding needle 200 is pulled out from the winding core 100 .

[0096] During the process of winding the material tape by the winding needle 200, the viscosity of the glue layer 02 on the surface of the diaphragm 01 can increase when heated, which can improve the bonding effect of the glue layer 02 on the diaphragm 01 in the innermost circle structure, reduce the bonding difficulty between the diaphragms 01, and improve the product yield of the winding core 100; at the same time, the diaphragm 01 may shrink due to heat, so as to help improve the shaping effect of the multi-layer diaphragm 01 located in the innermost circle structure after bonding.

[0097] It should be noted that in the preparation method of the battery provided in this embodiment, the multilayer diaphragm 01 located in the innermost circle structure can be shaped under high temperature after bonding, so as to improve the structural stability of the core hole 110 and prevent the diaphragm 01 located in the innermost circle structure from collapsing toward the core hole 110; at the same time, after the diaphragm 01 in the innermost circle structure is shaped, the outer circle of the core 100 can match a higher winding tension, thereby manufacturing a tighter core 100 and improving the energy density of the battery cell.

[0098] In one embodiment, during the process of winding the material strip to form a cylindrical winding core 100, the temperature of the outer circumference of the winding needle 200 is adjustable within the range of 20°C to 150°C, so that the diaphragms 01 adhere tightly to form a whole, thereby avoiding the subsequent collapse of the diaphragms 01.

[0099] In one embodiment, during the process of rotating the winding needle 200 to wind the material strip and form the cylindrical winding core 100, the temperature of the outer circumference of the winding needle 200 is adjustable within the range of 20° C. to 120° C. In this embodiment, the temperature range is further narrowed so that the diaphragms 01 adhere tightly to form a whole, thereby preventing the diaphragms 01 from collapsing later.

[0100] Accordingly, on this basis, when specifically setting the temperature of the winding needle 200 in the winding state, the temperature range of the winding needle 200 can also be adjusted according to the winding degree of the core 100 to improve the winding effect on the core 100.

[0101] In one embodiment, the method of winding the material strip by rotating the winding needle 200 to form a cylindrical winding core 100 includes:

[0102] The temperature of the outer peripheral surface of the winding needle 200 is controlled to be within the range of 20° C. to 90° C., so that the winding needle 200 rotates around its own axis to wind the material strip to form the initial winding core 100;

[0103] The temperature of the outer peripheral surface of the winding needle 200 is controlled to be in the range of 60° C. to 120° C., and the initial winding core is shaped by the winding needle 200 to form a cylindrical winding core 100 .

[0104] It is worth noting that in this embodiment, the outer peripheral surface temperature of the winding needle 200 is adjusted within the above range only during the winding process of the winding core 100. Specifically, the temperature of the winding needle 200 during the winding process is lower than or equal to the temperature of the winding needle 200 during the shaping process.

[0105] For example, in a specific embodiment, the temperature of the winding needle 200 rises during the winding process, but the temperature of the winding needle 200 after the temperature rises is lower than the temperature during shaping. For example, during the winding process of the battery cell, the temperature of the outer peripheral surface of the winding needle 200 is in the range of 60°C to 90°C. After the winding strip is formed into the winding core 100, the winding core 100 can be kept on the surface of the winding needle 200, and the temperature of the outer peripheral surface of the winding needle 200 is controlled in the range of 70°C to 110°C for 1s to 20s to shape the diaphragm 01 located in the innermost circle.

[0106] In another specific embodiment, the winding needle 200 is heated during the winding process, and the temperature of the winding needle 200 in the winding state is equal to the temperature during shaping. For example, during the winding process of the battery cell, the winding needle 200 has been heated to a certain temperature. After the winding strip is formed into the winding core 100, the winding core 100 can be kept on the surface of the winding needle 200, and the innermost circle of the diaphragm 01 is shaped at the same temperature during the winding process.

[0107] In another specific embodiment, the temperature of the winding needle 200 does not rise during the winding process, but rises during the shaping process. For example, during the winding process of the battery cell, the temperature of the winding needle 200 remains unchanged. After the winding strip is wound to form the winding core 100, the winding needle 200 may be heated, and the winding core 100 may be kept on the surface of the heated winding needle 200 to shape the innermost circle of the diaphragm 01.

[0108] It is worth noting that after the operations in the above three specific embodiments are completed, the temperature of the outer peripheral surface of the winding needle 200 will drop to facilitate the needle withdrawal operation. That is, the temperature of the outer peripheral surface of the winding needle 200 when it is withdrawn from the winding core 100 is lower than the temperature of the outer peripheral surface of the winding needle 200 when it is winding the material tape.

[0109] It should be noted that the temperature of the winding needle 200 decreases when the winding needle 200 is withdrawn, which facilitates the withdrawal of the winding needle 200 and can improve the yield of the winding core 100 obtained after the withdrawal of the needle.

[0110] In another embodiment, the material strip is wound around the rotating winding needle 200 to form a cylindrical winding core 100, and the outer peripheral surface temperature of the winding needle 200 is always controlled within the range of 60° C. to 120° C. during the process of withdrawing the winding needle 200 from the winding core 100. This structural setting is easy to implement and more efficient.

[0111] Exemplarily, a specific example of the method for preparing a battery in the embodiment of the present application is provided, as follows:

[0112] 1. The winding needle 200 clamps the first section of the diaphragm 01;

[0113] 2. When winding starts, the temperature rises to 60℃~90℃;

[0114] 3. The positive pole piece and the negative pole piece are sequentially inserted into the winding mechanism to be wound with the separator 01 to form a winding core 100;

[0115] 4. Wind to the designed diameter of the core 100, wrap it up with tape;

[0116] 5. Raise the temperature of the coiling needle 200 to 70℃~110℃ and keep it for 1-20s.

[0117] 6. Pull out the inner needle 220, and rotate the outer needle 210 in the opposite direction for ≥0.5 turns before pulling it out.

[0118] 7. After winding is completed, the material is cut to form the final winding core 100.

[0119] Those skilled in the art will readily appreciate other embodiments of the present application after considering the specification and practicing the invention disclosed herein. The present application is intended to cover any variation, use or adaptation of the present invention, which follows the general principles of the present application and includes common knowledge or customary techniques in the art that are not disclosed in the present application. The specification and example embodiments are intended to be exemplary only, and the true scope and spirit of the present application are indicated by the appended claims.

[0120] It should be understood that the present application is not limited to the precise structures described above and shown in the drawings, and that various modifications and changes may be made without departing from its scope. The scope of protection of the present application is limited only by the appended claims.

Claims

1. A battery, characterized in that: It comprises a cylindrical winding core wound by a material strip, wherein the material strip comprises a diaphragm and a pole piece, wherein the diaphragm is arranged beyond the pole piece at the starting section of the material strip along the extension direction of the material strip; the winding core has a winding core hole, and the portion of the diaphragm exceeding the pole piece surrounds and forms the winding core hole; along the extension direction of the material strip, the portion of the diaphragm exceeding the pole piece forms the innermost circle structure of the winding core in the radial direction, and the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2; the diaphragm is provided with an adhesive layer, and the peel strength between the diaphragms in the innermost circle structure is ≥0.04N / cm, the thickness of the adhesive layer is in the range of 1μm to 4μm, and the thickness of the diaphragm is in the range of 7μm to 20μm.

2. The battery according to claim 1, characterized in that The number of turns of the diaphragm in the innermost circle structure is less than or equal to 12.

3. The battery according to claim 1, characterized in that The material of the adhesive layer is one of polyvinylidene fluoride, polytetrafluoroethylene, polymethyl methacrylate, polyethylene oxide or polyacrylic acid.

4. The battery according to any one of claims 1 to 3, characterized in that: The diameter range of the winding core is ≥40 mm.

5. The battery according to claim 4, characterized in that The ratio of the diameter of the winding core hole to the diameter of the winding core is 0.06 to 0.

4.

6. A battery manufacturing device, characterized in that: It comprises a winding needle, the outer circumference of which is used to fix the diaphragm in the material strip to form a cylindrical winding core; the temperature of the outer circumference of the winding needle is adjustable in the range of 20°C to 150°C to control the peel strength between the diaphragms in the innermost circle structure of the winding core to be ≥0.04N / cm, wherein the material strip comprises a diaphragm and a pole piece, and along the extension direction of the material strip, the diaphragm is arranged beyond the pole piece at the starting section of the material strip, and the part of the diaphragm beyond the pole piece forms the innermost circle structure of the winding core in the radial direction, the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2, and the diaphragm is provided with a glue layer, the thickness of the glue layer is in the range of 1μm to 4μm, and the thickness of the diaphragm is in the range of 7μm to 20μm.

7. The battery manufacturing device according to claim 6, characterized in that: The winding needle has a winding forming state and a needle withdrawal state. When the winding needle is in the winding forming state, the temperature of the outer circumference of the winding needle rises, and the winding needle can rotatably wind the material strip around its own axis to form a cylindrical winding core; when the winding needle is in the needle withdrawal state, the temperature of the outer circumference of the winding needle drops, and the winding needle can be withdrawn from the winding core.

8. The battery manufacturing device according to claim 7, characterized in that: The winding forming state includes a winding state and a shaping state. When the winding needle is in the winding state, the temperature of the outer circumferential surface of the winding needle is in the range of 20°C to 90°C, and the winding needle can rotatably wind the material strip around its own axis to form an initial winding core; when the winding needle is in the shaping state, the temperature of the outer circumferential surface of the winding needle is in the range of 60°C to 120°C, and the winding needle is used to shape the initial winding core formed by the winding state to form a cylindrical winding core.

9. The battery manufacturing device according to claim 6, characterized in that: The winding needle has a winding forming state and a needle withdrawal state. When the winding needle is in the winding forming state, the winding needle can rotatably wind the material strip around its own axis to form a cylindrical winding core; when the winding needle is in the needle withdrawal state, the winding needle can be withdrawn from the winding core; When the winding needle is in the needle-drawing state and the winding-forming state, the temperature of the outer peripheral surface of the winding needle is maintained in the range of 60° C. to 120° C.

10. The battery manufacturing device according to any one of claims 6 to 9, characterized in that: The winding needle comprises an inner needle and an outer needle, the outer needle has a receiving cavity, and the outer peripheral surface of the outer needle forms at least a part of the outer peripheral surface of the winding needle; the inner needle can be inserted and pulled out relative to the receiving cavity; The battery preparation device further comprises a driving mechanism, which is connected to the inner needle and is used to drive the inner needle to perform insertion and extraction actions relative to the accommodating cavity.

11. The battery manufacturing device according to claim 10, characterized in that: The roughness of the outer peripheral surface of the winding needle is less than or equal to ±(2μm to 2.5μm).

12. The battery manufacturing device according to any one of claims 6 to 9, characterized in that: The winding needle further comprises a heating element, and the heating element is pre-buried in the winding needle.

13. A method for preparing a battery, characterized in that: For preparing a battery as claimed in any one of claims 1 to 5, the preparation method comprising: Providing a material strip, the material strip comprising a diaphragm and a pole piece, wherein along the extension direction of the material strip, the diaphragm is arranged beyond the pole piece at the starting section of the material strip; The material strip is wound to form a cylindrical core, the core having a core hole, wherein the portion of the diaphragm extending beyond the pole piece surrounds and forms the core hole; along the extension direction of the material strip, the portion of the diaphragm extending beyond the pole piece forms the innermost circle structure of the core in the radial direction, the number of circles of the diaphragm in the innermost circle structure is greater than or equal to 2; the diaphragm is provided with a glue layer, the peel strength between the diaphragms in the innermost circle structure is ≥0.04N / cm, the thickness of the glue layer is in the range of 1μm to 4μm, and the thickness of the diaphragm is in the range of 7μm to 20μm.

14. The method for preparing a battery according to claim 13, characterized in that: The method of winding the material strip to form a cylindrical winding core comprises: Fixing the diaphragm disposed beyond the pole piece in the starting section of the material strip to the outer peripheral surface of the winding needle; The material strip is wound by rotating the winding needle to form a cylindrical winding core; The winding needle is pulled out from the winding core.

15. The method for preparing a battery according to claim 14, characterized in that: During the process of winding the material strip to form a cylindrical winding core, the temperature of the outer peripheral surface of the winding needle can be adjusted within the range of 20° C. to 150° C.

16. The method for preparing a battery according to claim 15, characterized in that: In the process of winding the material strip by rotating the winding needle to form a cylindrical winding core, the temperature of the outer peripheral surface of the winding needle can be adjusted within the range of 20° C. to 120° C.

17. The method for preparing a battery according to claim 16, characterized in that: The method of winding the material strip by rotating the winding needle to form a cylindrical winding core includes: Controlling the temperature of the outer peripheral surface of the winding needle to be within the range of 20° C. to 90° C., so that the winding needle rotates around its own axis to wind the material strip to form an initial winding core; The temperature of the outer peripheral surface of the winding needle is controlled within the range of 60° C. to 120° C., and the initial winding core is shaped by the winding needle to form a cylindrical winding core.

18. The method for preparing a battery according to claim 16 or 17, characterized in that: The temperature of the outer peripheral surface of the winding needle when it is withdrawn from the winding core is lower than the temperature of the outer peripheral surface of the winding needle when it is wound around the material tape.

19. The method for preparing a battery according to claim 15, characterized in that: The material strip is wound by rotating the winding needle to form a cylindrical winding core, and in the process of withdrawing the winding needle from the winding core, the temperature of the outer peripheral surface of the winding needle is always controlled within the range of 60° C. to 120° C.