Ceramic copper clad laminate surface treatment agent and ceramic copper clad laminate surface treatment working fluid

By using the ceramic copper clad surface treatment agent with α-substituted organic acids and heterocyclic amines and other components, the complexing agent and organic film are formed, and the problems of low micro-etching treatment efficiency and uneven surface of the ceramic copper clad are solved, and the further development is achieved. Efficient copper surface treatment and good silver sinking effect.

CN118028814BActive Publication Date: 2024-11-12HUIZHOU XINWEIYA NANOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311654426.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-05
Publication Date
2024-11-12
Estimated Expiration
2043-12-05

AI Technical Summary

Technical Problem

In the prior art, the micro-etching treatment efficiency of ceramic copper clad plates is low, the copper surface roughness is poor and the surface is uneven, especially the problem of falling silver layer falling off on AMB ceramic copper clad plates.

Method used

Using a ceramic copper clad surface treatment agent, including α-substituted organic acids, heterocyclic amines and PEG-600, through the combination of these components, a complexing agent and an organic film are formed, which promotes the oxidation reaction of the copper surface and reduces the surface tension. Improve micro-etching rate and uniformity.

Benefits of technology

The micro-etching rate and uniformity of the ceramic copper clad plate are significantly improved, the roughness of the copper surface is increased, and the organic film is easy to remove in subsequent processes without affecting the quality of the silver deposited.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The present application provides a surface treatment agent for a ceramic copper-clad laminate and a surface treatment working liquid for a ceramic copper-clad laminate. The surface treatment agent for a ceramic copper-clad laminate comprises an α-substituted organic acid, a heterocyclic amine, PEG-600 and deionized water. The α-substituted organic acid in the treatment agent acts as a complexing agent. On the one hand, it inhibits the hydrolysis of ferric iron by weakly complexing it with ferric iron, thereby promoting the oxidation reaction of ferric iron on copper. On the other hand, the α-substituted organic acid further promotes the oxidation reaction of ferric iron on copper by complexing the generated divalent iron, thereby increasing the rate of micro-etching of the copper surface by the working liquid. The heterocyclic amine increases the roughness of the copper surface after the reaction by complexing its amino group with copper ions. The wetting effect of PEG-600 reduces the tension of the copper surface, so that each position on the copper surface can react evenly, thereby improving the uniformity of the copper surface reaction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of ceramic plate manufacturing process, and in particular to a ceramic copper-clad plate surface treatment agent and a ceramic copper-clad plate surface treatment working liquid. Background Art

[0002] Ceramic board (also called ceramic substrate circuit board) is made of ceramic copper clad laminate as the substrate to make circuits. Ceramic copper clad laminate can be generally divided into DBC (Direct bonded copper, direct copper clad ceramic substrate), DPC (Direct plating copper, direct electroplating ceramic substrate), AMB (Active metal brazing, active metal brazing ceramic substrate), etc. According to the process, AMB ceramic copper clad laminate uses metal brazing materials containing a small amount of active elements to tightly weld the copper foil and the ceramic substrate under high temperature and high pressure conditions.

[0003] Different from the DPC or DBC process, the AMB ceramic copper clad laminate is affected by high temperature and high pressure. The metal crystal structure of copper is very different from the crystal structure of ordinary electrolytic copper foil. The resulting change is that the copper surface is difficult to be treated with ordinary micro-etching solutions.

[0004] The final surface treatment of ceramic boards usually uses nickel-gold or immersion silver. Before depositing the plating layer, the copper surface of the ceramic copper-clad board needs to be micro-etched. In the prior art, a micro-etching agent of a potassium persulfate system, a ferric sulfate system or a hydrogen peroxide system is generally used to micro-etch the copper surface. When the above-mentioned micro-etching agent is used to treat the surface of ceramic copper-clad boards, especially AMB ceramic copper-clad boards, the following problems exist: 1. The treatment efficiency is low, and it is often necessary to extend the treatment time by more than four times to micro-etch the copper surface; 2. The roughness of the copper surface after micro-etching is poor. Even if the treatment time is extended several times, a certain proportion of the immersion silver layer will fall off; 3. The micro-etching of the surface of the ceramic copper-clad board is uneven. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present application provides a surface treatment agent for a ceramic copper clad laminate.

[0006] The present application discloses a surface treatment agent for a ceramic copper-clad laminate comprising: 1.0-5.5 parts of an α-substituted organic acid, 0.05-0.5 parts of a heterocyclic amine, 0.1-1.0 parts of PEG-600 and 3.5-7.0 parts of deionized water.

[0007] Preferably, the α-substituted organic acid includes at least one of tartaric acid and alanine.

[0008] Preferably, the heterocyclic amine is at least one of 2-aminothiazole and 5-aminotetrazolyl.

[0009] Preferably, the tartaric acid is at least one of DL-tartaric acid, D-tartaric acid and L-tartaric acid.

[0010] Preferably, the alanine is at least one of DL-alanine, D-alanine and L-alanine.

[0011] Preferably, the α-substituted organic acid comprises 0.8-4.0 parts of tartaric acid and 0.2-1.5 parts of alanine.

[0012] Preferably, the tartaric acid is 1.5-3.0 parts and the alanine is 0.6-1.2 parts.

[0013] Preferably, the heterocyclic amine comprises 0.03-0.3 parts of 2-aminothiazole and 0.02-0.2 parts of 5-aminotetrazolyl.

[0014] Preferably, the amount of 2-aminothiazole is 0.08-0.15 parts, and the amount of 5-aminotetrazolyl is 0.07-0.14 parts.

[0015] According to a second aspect of the present invention, the present application provides a working liquid for surface treatment of a ceramic copper-clad laminate.

[0016] The present application discloses a ceramic copper-clad laminate surface treatment working solution comprising 85.5-94.5 g / l of sulfuric acid, 57-63 g / l of ferric sulfate, 95-105 ml / l of a ceramic copper-clad laminate surface treatment agent and the remainder of deionized water.

[0017] The beneficial effects of the present application are as follows: during the micro-etching process, the α-substituted organic acid in the working solution acts as a complexing agent. On the one hand, it inhibits the hydrolysis of ferric iron through weak complexing with ferric iron, and promotes the oxidation reaction of ferric iron to copper. On the other hand, the α-substituted organic acid further promotes the oxidation reaction of ferric iron to copper through complexing with the generated divalent iron, thereby increasing the rate of micro-etching of the copper surface by the working solution; the heterocyclic amine can form an organic film with copper ions through the complexing of its amino group with copper ions. Since the copper surface is a rough surface, this organic film is more likely to form at the crest of the copper rough surface, and the organic film protects the copper surface. Therefore, the reaction rate at the trough of the copper rough surface is faster than the reaction rate at the crest, thereby increasing the roughness of the copper surface after the reaction. Furthermore, this organic film can be easily removed by pickling in the subsequent process without affecting the quality of subsequent silver deposition; through the wetting effect of PEG-600, the tension of the copper surface is reduced, so that each position of the copper surface can react evenly, thereby improving the uniformity of the copper surface reaction. DETAILED DESCRIPTION

[0018] In order to further understand the application content, characteristics and functions of the present application, the following embodiments are cited. The technical solutions between the various embodiments can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the protection scope required by this application.

[0019] Embodiment 1

[0020] The surface treatment agent for the ceramic copper clad laminate in this example is prepared from the following raw materials in parts by weight: 2.5 parts of DL-tartaric acid, 1.0 parts of DL-alanine, 0.13 parts of 2-aminothiazole, 0.1 parts of 5-aminotetrazole, 0.4 parts of PEG-600 and 5.88 parts of deionized water. The above parts are all mass ratios, for example, the mass ratio of DL-tartaric acid to DL-alanine is 2.5:1.

[0021] The surface treatment agent for ceramic copper clad boards in the present invention is based on oxidizing compounds such as ferric sulfate, potassium persulfate or hydrogen peroxide, and is a treatment agent for micro-etching the copper surface of ceramic copper clad boards, especially AMB ceramic copper clad boards, under acidic conditions. The treatment agent is applied before silver plating or nickel-gold plating in the production process of ceramic copper clad boards, and aims to improve the silver plating quality of ceramic copper clad boards. Different oxide systems use different treatment agents, and the surface treatment agent for ceramic copper clad boards in the present invention is suitable for the ferric sulfate system.

[0022] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0023] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0024] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0025] Before the silver deposition process of the AMB ceramic copper-clad laminate, the copper surface is treated with the ceramic copper-clad laminate surface treatment working liquid prepared with the above-mentioned ceramic copper-clad laminate surface treatment agent, wherein the α-substituted organic acid is used as a complexing agent to inhibit the hydrolysis of trivalent iron through the weak complexing effect of its carboxyl group on trivalent iron ions, and the heterocyclic amine is used as an inhibitor to complex copper through the amino group so that the working liquid can selectively react with the copper surface, PEG is used as a wetting agent to reduce the tension of the copper surface so that each position of the copper surface can react evenly, and deionized water is used as a solvent.

[0026] During the micro-etching process, the α-substituted organic acid in the working solution acts as a complexing agent. On the one hand, it inhibits the hydrolysis of ferric iron through weak complexing with ferric iron and promotes the oxidation reaction of ferric iron to copper. On the other hand, through the complexing of the generated divalent iron by the α-substituted organic acid, the oxidation reaction of ferric iron to copper is further promoted, thereby increasing the rate of micro-etching of the copper surface by the working solution. The heterocyclic amine can form an organic film with copper ions through the complexing of its amino group with copper ions. Since the copper surface is a rough surface, this organic film is more likely to form at the peak of the copper rough surface. The organic film protects the copper surface. Therefore, the reaction rate at the trough of the copper rough surface is faster than that at the peak, thereby increasing the roughness of the copper surface after the reaction. Moreover, this organic film can be easily removed by pickling in the subsequent process without affecting the quality of subsequent silver deposition. Through the wetting effect of PEG-600, the tension of the copper surface is reduced, so that each position of the copper surface can react evenly, thereby improving the uniformity of the copper surface reaction.

[0027] Embodiment 2

[0028] The surface treatment agent for the ceramic copper clad laminate in this example is prepared from the following raw materials in parts by weight: 3.0 parts of DL-tartaric acid, 0.8 parts of DL-alanine, 0.08 parts of 2-aminothiazole, 0.1 parts of 5-aminotetrazole, 0.4 parts of PEG-600 and 5.55 parts of deionized water, all of which are weight ratios.

[0029] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0030] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0031] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0032] Embodiment 3

[0033] The ceramic copper clad laminate surface treatment agent in this example is prepared from the following raw materials in parts by weight: 1.5 parts of DL-tartaric acid, 1.5 parts of DL-alanine, 0.12 parts of 2-aminothiazole, 0.08 parts of 5-aminotetrazole, 0.4 parts of PEG-600 and 6.36 parts of deionized water, all of which are weight ratios.

[0034] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0035] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0036] Embodiment 4

[0037] The surface treatment agent for the ceramic copper clad laminate in this example is prepared from the following raw materials in parts by weight: 0.8 parts of DL-tartaric acid and / or D-tartaric acid and / or L-tartaric acid, 0.2 parts of DL-alanine and / or D-alanine and / or L-alanine, 0.03 parts of 2-aminothiazole, 0.02 parts of 5-aminotetrazole, 0.1 parts of PEG-600 and 3.5 parts of deionized water, and the above parts are all by mass ratio.

[0038] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0039] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0040] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0041] Embodiment 5

[0042] The surface treatment agent for the ceramic copper clad laminate in this example is prepared from the following raw materials in parts by weight: 4.0 parts of DL-tartaric acid, 1.5 parts of DL-alanine, 0.3 parts of 2-aminothiazole, 0.2 parts of 5-aminotetrazole, 1.0 parts of PEG-600 and 7.0 parts of deionized water, all of which are weight ratios.

[0043] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0044] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0045] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0046] Embodiment 6

[0047] The ceramic copper clad laminate surface treatment agent in this example is prepared from the following raw materials in parts by weight: 1.3 parts of DL-tartaric acid, 0.5 parts of DL-alanine, 0.08 parts of 2-aminothiazole, 0.01 parts of 5-aminotetrazole, 0.4 parts of PEG-600 and 5.55 parts of deionized water, and the above parts are all weight ratios.

[0048] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0049] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0050] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0051] Embodiment 7

[0052] The ceramic copper clad laminate surface treatment agent in this example is prepared from the following raw materials in parts by weight: 1.5 parts of DL-tartaric acid, 0.5 parts of DL-alanine, 0.05 parts of 2-aminothiazole, 0.05 parts of 5-aminotetrazole, 0.4 parts of PEG-600 and 6.36 parts of deionized water, and the above parts are all weight ratios.

[0053] The surface treatment liquid of the ceramic copper clad laminate is prepared by using the above-mentioned surface treatment agent of the ceramic copper clad laminate as follows:

[0054] Sulfuric acid: 90g / l, ferrous sulfate: 60g / l, ceramic copper clad laminate surface treatment agent: 100ml / l, deionized water: balance.

[0055] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0056] Comparative Example 1

[0057] The silver pretreatment solution is prepared using the potassium persulfate system on the market as follows:

[0058] Sulfuric acid: 70 g / l, potassium persulfate: 90 g / l, citric acid: 5 g / l, potassium persulfate stabilizing additive: 100 ml / l, deionized water: balance.

[0059] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0060] Comparative Example 2

[0061] The silver pretreatment working solution is prepared using the hydrogen peroxide system on the market as follows:

[0062] The traditional micro-etching agent working solution is prepared as follows:

[0063] Sulfuric acid: 70g / l, hydrogen peroxide: 40ml / l, hydrogen peroxide stabilizing additive: 40ml / l, deionized water: balance.

[0064] The above-prepared working solution is used for silver immersion pretreatment and silver immersion performance testing.

[0065] Immersion silver performance test data

[0066] 1. Copper surface roughness test:

[0067] The AMB ceramic plate after circuit etching was pre-treated with silver deposition using the working solution prepared in the above embodiments, and the surface roughness of the resulting plate was tested. The results are shown in Table 1 below:

[0068]

[0069]

[0070] Table 1

[0071] 2. Silver bonding test:

[0072] The AMB ceramic plate after circuit etching was pre-treated with the working solution prepared in the above embodiments, and the treatment time of the working solution prepared in each embodiment was controlled to be the same, and the ceramic plate was chemically silvered, and the resulting plate was tested for silver bonding strength, and the bonding strength was tested by pulling with 3M tape. The results are shown in Table 2:

[0073]

[0074]

[0075] Table 2

[0076] 3. Thickness uniformity test:

[0077] The AMB ceramic plate after circuit etching was pre-treated with the working solution prepared in the above embodiments, and the ceramic plate was chemically silvered. The resulting plate was tested for thickness uniformity. The silver thickness was tested with an XRF thickness tester. The results are shown in Table 3:

[0078]

[0079]

[0080] Table 3

[0081] In summary, during the micro-etching process, the α-substituted organic acid in the working solution acts as a complexing agent. On the one hand, it inhibits the hydrolysis of ferric iron through weak complexing with ferric iron and promotes the oxidation reaction of ferric iron to copper. On the other hand, through the complexing of the generated divalent iron by the α-substituted organic acid, the oxidation reaction of ferric iron to copper is further promoted, thereby increasing the rate of micro-etching of the copper surface by the working solution; heterocyclic amines can form organic films with copper ions through the complexing of their amino groups with copper ions. Since the copper surface is a rough surface, this organic film is more likely to form at the crest of the copper rough surface, and the organic film protects the copper surface. Therefore, the reaction rate at the trough of the copper rough surface is faster than that at the crest, thereby increasing the roughness of the copper surface after the reaction. Furthermore, this organic film can be easily removed by pickling in the subsequent process without affecting the quality of subsequent silver deposition; through the wetting effect of PEG-600, the tension of the copper surface is reduced, so that each position of the copper surface can react evenly, thereby improving the uniformity of the copper surface reaction.

[0082] The above is only the implementation mode of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.

Claims

1. A surface treatment agent for ceramic copper clad laminates, It is characterized in that include: 1.0-5.5 parts of α-substituted organic acid, 0.05-0.5 parts of heterocyclic amine, 0.1-1.0 parts of PEG-600 and 3.5-7.0 parts of deionized water; the α-substituted organic acid includes 0.8-4.0 parts of tartaric acid and 0.2-1.5 parts of alanine; the heterocyclic amine includes 0.03-0.3 parts of 2-aminothiazole and 0.02-0.2 parts of 5-aminotetrazolyl.

2. The surface treatment agent for ceramic copper clad laminate according to claim 1, It is characterized in that The tartaric acid is at least one of DL-tartaric acid, D-tartaric acid and L-tartaric acid.

3. The surface treatment agent for ceramic copper clad laminate according to claim 1, It is characterized in that The alanine is at least one of DL-alanine, D-alanine and L-alanine.

4. The surface treatment agent for ceramic copper clad laminate according to claim 1, It is characterized in that The tartaric acid is 1.5-3.0 parts, and the alanine is 0.6-1.2 parts.

5. The surface treatment agent for ceramic copper clad laminate according to claim 1, It is characterized in that The 2-aminothiazole is 0.08-0.15 parts, and the 5-aminotetrazolyl is 0.07-0.14 parts.

6. A working fluid for surface treatment of ceramic copper-clad laminates, It is characterized in that The method comprises 85.5-94.5 g / l of sulfuric acid, 57-63 g / l of ferric sulfate, 95-105 ml / l of the surface treatment agent for the ceramic copper clad plate according to any one of claims 1 to 5, and the balance of deionized water.