A post-processing method for improving the soldering strength of bumps in flip-chip devices

By using post-processing methods in the flip-chip bonding process, including flux coating and temperature control, the problem of bump strength and reliability in the micro-bump and small-pitch flip-chip bonding process is solved, and the welding strength is significantly improved. , suitable for highly integrated and miniaturized devices.

CN118073276BActive Publication Date: 2024-10-15WUXI ZHONGWEI GAOKE ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410231970.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-01
Publication Date
2024-10-15
Estimated Expiration
2044-03-01

AI Technical Summary

Technical Problem

Micro-bump, small-pitch flip-chip bonding process products have the risk of strength failure and poor reliability due to the small bump diameter, and the problem of bump breakage caused by residual stress.

Method used

A post-processing method is adopted to improve the bump soldering strength of flip-flip soldered devices, including providing chips and substrates with the same bump structure, applying flux for soldering, and then rapidly heating and holding at a specific temperature to promote the release of residual stress. and atomic diffusion, control the growth of the intermetallic compound layer, and ensure the improvement of welding strength.

Benefits of technology

Through this method, the bump welding strength is significantly improved, making up for the strength defects and reliability problems of highly integrated and miniaturized devices, and is suitable for flip-chip bonding processes with micro-bumps and small pitches.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118073276B_ABST
    Figure CN118073276B_ABST
Patent Text Reader

Abstract

The present invention provides a post-processing method for improving the welding strength of the bumps of a flip-chip device, comprising the following steps: step S1. providing a chip and a substrate with the same bump structure, the chip comprising a silicon layer and a first bump spaced on the silicon layer, the substrate comprising a base layer and a second bump spaced on the base layer, the first bump and the second bump being made of the same material, and coating a layer of flux on the welding surface of the first bump and the second bump; step S2. aligning and assembling the first bump of the chip and the second bump of the substrate, after the assembly is completed, flip-chip bonding to obtain the device; step S3. rapidly heating the device at a temperature of T1 for 1 min, then keeping the device at a temperature of T2 for t1, and finally cooling the device to a temperature of T3 and taking it out. The present invention can release the residual stress inside the bump and strengthen the diffusion interface strength by post-processing the bump welding, thereby improving the welding strength, is greatly suitable for the welding process of micro bumps, and can make up for the strength defects and reliability problems of highly integrated and miniaturized devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of integrated circuit packaging, in particular to a post-processing method for improving the welding strength of bumps of an inverted soldering device. Background Art

[0002] With the rapid development of big data, 5G, artificial intelligence, and mobile Internet, especially after the process node reaches 7nm, physical effects and cost constraints have significantly slowed down Moore's Law. In the "post-Moore era", relying on the innovation of advanced packaging and interconnection technology to meet the needs of system miniaturization and multi-functionality will be one of the important directions for the development of the integrated circuit manufacturing industry.

[0003] In order to meet the application needs of high-performance chips, advanced packaging interconnection technology will continue to develop in the direction of high density and high reliability in the future. High density means that the solder joint pitch will continue to decrease to below 10μm. Cu-Cu bonding is a new method that has developed rapidly. Cu is low-cost, has excellent electrical and thermal conductivity, good anti-electromigration ability and thermal mechanical reliability. Moreover, Cu is always in a solid state during the bonding process, without the overflow problem of soft soldering, and narrow pitch interconnection can be achieved. Cu-Cu bonding technology can meet high-density and high-reliability interconnection, and may be widely used in the future.

[0004] Micro-bump and small pitch packaging interconnect technology has gradually become a trend. However, due to the reduction in bump diameter and shortened pitch, the contact area between bumps becomes smaller during the welding process, which will directly affect the bump welding strength and cause strength risks in the device. Therefore, the welding strength of micro-bump and small pitch products has become an issue that needs to be urgently addressed. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention provides a post-processing method for improving the soldering strength of the bumps of a flip-chip device, so as to solve the problems of strength failure risk and poor reliability of highly integrated micro-bumps and small-pitch flip-chip bonding process products due to the small bump diameter, as well as the bump breakage problem caused by residual stress.

[0006] The technical solution adopted by the present invention is:

[0007] A post-processing method for improving the soldering strength of a bump of a flip-chip solder joint device, comprising the following steps:

[0008] Step S1. Provide a chip and a substrate with the same bump structure, wherein the chip comprises a silicon layer and first bumps spaced apart on the silicon layer, and the substrate comprises a base layer and second bumps spaced apart on the base layer, wherein the first bump and the second bump are made of the same material, and a layer of soldering flux is applied to the welding surfaces of the first bump and the second bump;

[0009] Step S2. Align and assemble the first bump of the chip and the second bump of the substrate. After the assembly is completed, perform flip-chip bonding by welding, clean and remove the flux, and obtain a device;

[0010] Step S3: The device is rapidly heated at temperature T1 for 1 min, and then the device is placed in an oven and kept at temperature T2 for t1. Finally, the device is cooled to temperature T3 along with the oven and then taken out.

[0011] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, the first bumps and the second bumps are made of copper, and the chip and the substrate are flip-chip bonded by hot-pressing welding.

[0012] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, the diameters of the first bumps and the second bumps are both 8-40 μm, and the bump spacing is ≥10 μm.

[0013] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, T1 is 300°C to 310°C.

[0014] Preferably, the post-processing method for improving the soldering strength of the bumps of the flip-chip soldering device, wherein: the first bump and the second bump are made of copper and tin, the first bump and the second bump both include a copper column and a tin cap, the silicon layer and the substrate layer are both provided with a copper column, the copper column is provided with a tin cap, the copper column has a thickness of not less than 3 μm, the tin cap has a thickness of not less than 2 μm, and the chip and the substrate are flip-chip bonded by reflow soldering to form an intermetallic compound Cu x Sn y .

[0015] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, the diameters of the first bumps and the second bumps are greater than 40 μm.

[0016] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, T1 is 252°C to 282°C.

[0017] Preferably, in the post-processing method for improving the soldering strength of bumps of flip-chip devices, in step S3, T2 is 145-155°C, t1 is 25-35min; and T3 is 60-80°C.

[0018] Preferably, in the post-processing method for improving the soldering strength of the bumps of flip-chip devices, t1 and the total time of cooling in the oven are less than 1 hour.

[0019] Flux is used to assist welding and remove oxides from the surface of the bumps. After flip-chip bonding is completed, the device is rapidly heated at temperature T1 (solid-liquid diffusion temperature of the bump material) for 1 min to allow the bumps to reach the solid-liquid diffusion temperature. The device is moved into a 150±5°C oven and kept warm for 30±5 min. This process promotes the release of residual stress of the bumps, atomic diffusion, and regrowth of grains. After the insulation is completed, the device is cooled from 150°C to 60~80°C with the furnace and then taken out. The growth of the IMC layer and the residual stress release process are controlled by temperature regulation. However, in order to avoid excessive growth of the IMC layer and a decrease in welding strength, the total upper limit time of the insulation stage and the furnace cooling stage must be controlled to not exceed 1h to determine the safety threshold for the growth of the IMC layer.

[0020] The post-processing method for improving the welding strength of the bumps of a flip-chip device of the present invention can greatly compensate for and improve the welding strength of the bumps for circuits with known insufficient strength or residual stress risk, effectively remove the residual stress inside the bumps and strengthen the diffusion interface strength, thereby improving the welding strength, and is extremely suitable for flip-chip bonding processes of micro-bumps and small-pitch devices.

[0021] Advantages of the present invention:

[0022] The post-processing method for improving the welding strength of the bumps of the flip-chip device of the present invention can release the residual stress inside the bumps and strengthen the diffusion interface strength through post-processing of the bump welding, thereby improving the welding strength. It is very suitable for the welding process of micro-bumps and can make up for the strength defects and reliability problems of highly integrated and miniaturized devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a schematic diagram of the chip bump structure of Example 1 of the present invention.

[0024] Figure 2 Schematic diagram of the substrate bump structure of Example 1 of the present invention.

[0025] Figure 3 Schematic diagram of the flip-chip bonding process of the chip and substrate in Example 1 of the present invention.

[0026] Figure 4 This is a schematic diagram of the device structure after the substrate and chip are welded in Example 1 and Example 2 of the present invention.

[0027] Figure 5 This is a schematic diagram of the chip bump structure of Example 2 of the present invention.

[0028] Figure 6 Schematic diagram of the substrate bump structure of Example 2 of the present invention.

[0029] Figure 7 This is a schematic diagram of the reflux curve of Example 2.

[0030] Figure 8 The present invention is a process curve diagram of the rapid heating, heat preservation process and furnace cooling process of the flip-chip device welding in the oven. DETAILED DESCRIPTION

[0031] The present invention will be further described below in conjunction with specific drawings and embodiments.

[0032] Example 1

[0033] A post-processing method for improving the soldering strength of a bump of a flip-chip solder joint device, comprising the following steps:

[0034] like Figure 1-2 Step S1. Provide a chip 1 and a substrate 2 with the same bump structure, wherein the chip 1 includes a silicon layer 1-1 and first bumps 1-2 spaced apart on the silicon layer, and the substrate 2 includes a base layer 2-1 and second bumps 2-2 spaced apart on the base layer; the materials of the first bumps 1-1 and the second bumps 2-2 are both Cu, and a 20 μm thick soldering flux is coated on the soldering surfaces of the first bumps 1-2 and the second bumps 2-2, respectively. The soldering flux is manufactured by Senju Corporation and has a brand name of WF-6070SP. The first bumps 1-2 and the second bumps 2-2 are micro bumps, and the diameters of the first bumps 1-2 and the second bumps 2-2 are 15 μm, and the spacing between the first bumps 1-2 and the second bumps 2-2 is 20 μm;

[0035] Step S2. Figure 3-4 , align and assemble the first bump 1-2 of the chip 1 and the second bump 2-2 of the substrate 2. After the assembly is completed, the chip 1 and the substrate 2 are flip-chip bonded by hot pressing welding. After the welding is completed, the flux is cleaned and removed to obtain a device. The flip-chip bonding equipment used is FC300, the hot pressing welding temperature is 320°C, the hot pressing pressure is 2.3N, the pressing time is 10min, and the first bump 1-2 and the second bump 2-2 are welded;

[0036] Step S3. Figure 8 , Cu-Cu hot pressing bonding is low-temperature diffusion bonding, and the temperature range of solid-liquid diffusion bonding is 300℃~310℃, so T1 is selected as 305℃, and the device is quickly heated at 305℃ for 1min, and then the device is placed in an oven and kept at 150℃ for 30min. This process promotes the release of residual stress of the bumps, atomic diffusion and grain regrowth. Finally, the device is taken out after cooling to 70℃ with the oven. The total time of the insulation stage and the cooling stage with the oven does not exceed 1h. After this post-processing process, the chip shear strength can be increased to 2~3 times of the original. The process curves of the device's rapid heating, insulation process and furnace cooling process in the oven are as follows Figure 8 shown.

[0037] Example 2

[0038] A post-processing method for improving the soldering strength of a bump of a flip-chip solder joint device, comprising the following steps:

[0039] like Figure 5-6 Step S1. Provide a chip 1 and a substrate 2 with the same bump structure, wherein the chip 1 comprises a silicon layer 1-1 and first bumps 1-2 spaced apart on the silicon layer 1-1, and the substrate 2 comprises a base layer 2-1 and second bumps 2-2 spaced apart on the base layer, wherein the materials of the first bumps 1-2 and the second bumps 2-2 are both copper and tin, and the structures of the first bumps 1-2 and the second bumps 2-2 are both copper pillars 1-3 electroplated with tin caps 1-4, presenting a "copper pillar + tin cap" type, wherein the copper pillars 1-3 are thick The thickness of the solder cap 1-4 is 40 μm, the thickness of the solder cap 1-4 is 20 μm, and a 20 μm thick solder flux is coated on the soldering surface of the first bump 1-2 and the second bump 2-2 respectively. The solder flux is manufactured by Senju Company and the brand is WF-6070SP. The size type of the first bump 1-2 and the second bump 2-2 is a conventional bump. The diameter of the first bump 1-2 and the second bump 2-2 is 80 μm, and the spacing between the first bump 1-2 and the second bump 2-2 is 100 μm.

[0040] Step S2. Figure 4 and Figure 7 The first bump 1-2 of the chip 1 and the second bump 2-2 of the substrate 2 are aligned and assembled. After the assembly is completed, the chip 1 and the substrate 2 are flip-chip bonded by reflow soldering to form an intermetallic compound Cu x Sn y , cleaning and removing the flux, obtaining the device, flip-chip bonding using a placement machine, reflow temperature of 265°C, reflow time of 60s, the first bump 1-2 and the second bump 2-2 are welded;

[0041] Step S3. Figure 8 , reflow soldering is solid-liquid diffusion bonding, and the solid-liquid diffusion bonding temperature range is 252℃~282℃, so T1 is selected as 260℃, the device is quickly heated at 260℃ for 1min, and then the device is placed in an oven and kept at 150℃ for 30min, and finally the device is cooled to 70℃ with the oven and taken out. The total time of the heat preservation stage and the cooling stage with the oven does not exceed 1h. After this post-processing process, the chip shear strength can be increased to 2~3 times of the original. The process curves of the device's rapid heating, heat preservation process and furnace cooling process in the oven are as follows Figure 8 shown.

[0042] Comparative Example 1

[0043] A post-processing method for improving the soldering strength of a bump of a flip-chip solder joint device, comprising the following steps:

[0044] like Figure 1-2Step S1. Provide a chip 1 and a substrate 2 with the same bump structure, wherein the chip 1 includes a silicon layer 1-1 and first bumps 1-2 spaced apart on the silicon layer, and the substrate 2 includes a base layer 2-1 and second bumps 2-2 spaced apart on the base layer, wherein the materials of the first bump 1-1 and the second bump 2-2 are both Cu, and a 20 μm thick soldering flux is coated on the soldering surfaces of the first bump 1-1 and the second bump 2-2, respectively. The soldering flux is manufactured by Senju Corporation and has a brand name of WF-6070SP. The first bump 1-2 and the second bump 2-2 are micro bumps, and the diameters of the first bump 1-2 and the second bump 2-2 are 15 μm, and the bump spacings of the first bump 1-2 and the second bump 2-2 are both 20 μm;

[0045] Step S2. Figure 4 , align and assemble the first bump 1-2 of the chip and the second bump 2-2 of the substrate 2. After the assembly is completed, the chip 1 and the substrate 2 are flip-chip bonded by hot pressing welding, and the flux is cleaned and removed to obtain the device. The flip-chip bonding equipment used is FC300, the hot pressing welding temperature is 320℃, the hot pressing pressure is 2.3N, the pressing time is 10min, and the first bump 1-2 and the second bump 2-2 are welded.

[0046] Comparative Example 2

[0047] A post-processing method for improving the soldering strength of a bump of a flip-chip solder joint device, comprising the following steps:

[0048] like Figure 5-6 , providing a chip 1 and a substrate 2 with the same bump structure, wherein the chip 1 comprises a silicon layer 1-1 and a first bump 1-2 spaced apart on the silicon layer, the substrate 2 comprises a base layer 2-1 and a second bump 2-2 spaced apart on the base layer, the materials of the first bump 1-2 and the second bump 2-2 are both copper and tin, the structures of the first bump 1-2 and the second bump 2-2 are both electroplated tin caps 1-4 on copper pillars 1-3, presenting a "copper pillar + tin cap" type, wherein the copper pillar 1-3 has a thickness of 40 μm, and the tin cap 1-4 has a thickness of 20 μm, a layer of 20 μm thick soldering flux is coated on the welding surfaces of the first bump 1-1 and the second bump 2-2 respectively, the soldering flux manufacturer is Senju Co., Ltd., the brand is WF-6070SP, the size type of the first bump and the second bump are conventional bumps, the diameters of the first bump 1-2 and the second bump 2-2 are both 80 μm, and the spacing between the first bump 1-2 and the second bump 2-2 is both 100 μm;

[0049] Step S2. Figure 4 The first bump 1-2 of the chip 1 and the second bump 2-2 of the substrate 2 are aligned and assembled. After the assembly is completed, the chip 1 and the substrate 2 are flip-chip bonded by reflow soldering to form an intermetallic compound Cu x Sn y, clean and remove the flux, obtain the device, flip-chip bonding using a placement machine, reflow temperature of 265 ° C, reflow time of 60s, the first bump 1-2 and the second bump 2-2 are welded.

[0050] The shear strength of the chip in comparative example 1 that has not been post-processed is 0.9 kg, and the shear strength of the chip in embodiment 1 that has been post-processed is 2.1 kg; the shear strength of the chip in comparative example 2 that has not been post-processed is 1.7 kg, and the shear strength of the chip in embodiment 2 that has been post-processed is 4.1 kg.

[0051] The post-processing method for improving the welding strength of the bumps of the flip-chip device of the present invention can release the residual stress inside the bumps and strengthen the diffusion interface strength through post-processing of the bump welding, thereby improving the welding strength. It is very suitable for the welding process of micro-bumps and can make up for the strength defects and reliability problems of highly integrated and miniaturized devices.

[0052] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A post-processing method for improving the soldering strength of bumps of flip-chip devices, characterized in that: The following steps are involved: Step S1. providing a chip (1) and a substrate (2) having the same bump structure, wherein the chip (1) comprises a silicon layer (1-1) and first bumps (1-2) arranged at intervals on the silicon layer (1-1), and the substrate (2) comprises a base layer (2-1) and second bumps (2-2) arranged at intervals on the base layer (2-1), wherein the first bumps (1-2) and the second bumps (2-2) are made of the same material, and a layer of soldering flux is coated on the welding surfaces of the first bumps (1-2) and the second bumps (2-2); Step S2. aligning and assembling the first bump (1-2) of the chip (1) and the second bump (2-2) of the substrate (2); after the assembly is completed, performing flip-chip bonding by welding, and cleaning and removing the solder flux to obtain a device; Step S3. The device is rapidly heated at temperature T1 for 1 min, then the device is placed in an oven and kept at temperature T2 for t1, and finally the device is cooled to temperature T3 along with the oven and then taken out; The materials of the first bump (1-2) and the second bump (2-2) are both copper and tin. The first bump (1-2) and the second bump (2-2) both include a copper column (1-3) and a tin cap (1-4). The copper column (1-3) is disposed on the silicon layer (1-1) and the substrate layer (2-1). The tin cap (1-4) is disposed on the copper column. The thickness of the copper column (1-3) is not less than 3 μm. The thickness of the tin cap (1-4) is not less than 2 μm. The chip (1) and the substrate (2) are flip-chip bonded by reflow soldering to form an intermetallic compound Cu x Sn y ; In step S3, T1 is 260° C., T2 is 150° C., t1 is 30 min, and T3 is 70° C.; the total time of t1 and cooling in the oven is less than 1 h.