A plant disease-resistant agent containing antimicrobial peptides and preparation method thereof
Through the combination of carriers and composite nanowires formed by cross-linking of block copolymers and chitosan microspheres, the problem of unstable disease resistance of antimicrobial peptide plant disease resistance agents under the influence of temperature and soil salinity has been solved, and a good Dispersibility and disease resistance.
Patent Information
- Application Number
- CN202410948919.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-09-27
- Estimated Expiration
- 2044-07-16
AI Technical Summary
The anti-disease effect of existing antimicrobial peptide plant disease-resistant agents is unstable under the influence of temperature and soil salt content, and the carrier has poor dispersion in water, resulting in difficulty in spraying and clogging problems.
A carrier combining block copolymer and chitosan microspheres is used. A carrier with high porosity is formed through cross-linking of block copolymer and chitosan microspheres, and composite nanowires are added to improve dispersion and disease resistance.
It improves the slow-release and protective effects of antimicrobial peptides, reduces the effects of temperature and soil salinity on disease-resistant agents, enhances plants' ability to absorb antimicrobial peptides, and has good dispersion in water, avoiding aggregation.
Smart Images

Figure SMS_3 
Figure SMS_8 
Figure SMS_9
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plant disease-resistant agents, and in particular to a plant disease-resistant agent containing an antimicrobial peptide and a preparation method thereof. Background Art
[0002] Antimicrobial peptides are a class of alkaline polypeptide substances with antimicrobial activity, with a molecular weight of about 2000-7000, and are composed of 20-60 amino acid residues. According to structural classification, antimicrobial peptides can be divided into: linear polypeptides with a helical structure, linear polypeptides rich in certain amino acids, polypeptides containing one disulfide bond, polypeptides containing two or more disulfide bonds, and lantibiotics. Antimicrobial peptides have the advantages of strong alkalinity, thermal stability, and broad-spectrum antibacterial properties. They can quickly detect and kill targets and are widely used in genetic engineering, medicine, agriculture, food, animal husbandry and other fields. When used in the agricultural field, antimicrobial peptides are mainly used as biological pesticides and plant disease resistance agents to inhibit the growth and reproduction of plant pathogens, promote plant growth and enhance plant resistance.
[0003] When antimicrobial peptides are used as plant disease resistance agents, the mechanism of action is that antimicrobial peptides stimulate plant gene expression, affect plant immune response, and improve plant resistance to pathogens. For example, antimicrobial peptide Thionins stimulate plant gene expression by binding to plant cell walls, thereby enhancing plant immunity to pathogens. At present, there are two most commonly used methods for applying antimicrobial peptides: the first application method is to transfer antimicrobial peptide genes into plants for expression, so that plants have disease resistance, but this method is complicated to operate, and due to the low expression of antimicrobial peptides in plants, the expression level of antimicrobial peptide genes in plants is low; the second application method is to use antimicrobial peptides to directly soak plant seeds or spray plants. This method is simple to operate, but in the process of antimicrobial peptide absorption, it is greatly affected by environmental factors. Temperature and salt content in the soil will affect the activity of antimicrobial peptides and the absorption of antimicrobial peptides by plant seeds or plants, thereby affecting the antimicrobial effect of antimicrobial peptides.
[0004] In order to solve the problems existing in the second application method mentioned above, the most commonly used method is to use a carrier to load the antimicrobial peptide to make a plant disease-resistant agent, and then soak the plant seeds or spray the plant plants, so as to protect the antimicrobial peptide while releasing it slowly, and avoid the influence of environmental factors on the activity of the antimicrobial peptide. However, after many experiments, it was found that this method has the following shortcomings: when the carrier releases the antimicrobial peptide slowly, the release amount is greatly affected by temperature, resulting in the disease-resistant effect of the plant disease-resistant agent being greatly affected by temperature; in order to increase the loading amount of the antimicrobial peptide, a carrier with a large specific surface area and a small particle size is generally selected, but the surface energy of the carrier with a large specific surface area and a small particle size is large, and it is easy to agglomerate during use, which affects the release of the antimicrobial peptide, thereby affecting the disease-resistant effect of the antimicrobial peptide; the carrier has poor dispersibility in water, which leads to easy clogging of the nozzle when spraying the plant plants. Summary of the invention
[0005] In view of the shortcomings of the prior art, the present invention provides a plant disease-resistant agent containing antimicrobial peptides and a preparation method thereof. The disease-resistant effect of the prepared plant disease-resistant agent containing antimicrobial peptides is less affected by temperature and salt content in the soil, is not easy to agglomerate during use, and has good dispersibility in water.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows:
[0007] A method for preparing a plant disease-resistant agent containing antimicrobial peptides, comprising the following steps: preparing a carrier, preparing a composite nanowire, preparing an antimicrobial peptide solution, loading, and mixing;
[0008] The preparation of the carrier comprises the following steps: preparing a block copolymer, preparing a chitosan acetic acid solution, preparing chitosan microspheres, and grafting;
[0009] The block copolymer is prepared by mixing methoxypolyethylene glycol amino and N,N-dimethylformamide under the protection of nitrogen, stirring at 40-50° C. and 50-100 rpm for 10-20 min, adding N6-benzyloxycarbonyl-L-lysine cyclic anhydride, stirring at 40-50° C. and 50-100 rpm for 45-50 h, adding ether for precipitation, filtering, taking the filter residue, washing the filter residue with ether for 3-4 times, placing it at -40° C. to -35° C. and freeze-drying it for 25-30 h to obtain the block copolymer;
[0010] In the preparation of the block copolymer, the mass volume ratio of methoxy polyethylene glycol amino, N,N-dimethylformamide, N6-benzyloxycarbonyl-L-lysine cyclic anhydride, and ether is 5-5.5g:1000-1200mL:7-8g:6000-7000mL;
[0011] The weight average molecular weight of the methoxy polyethylene glycol amino group is 2×10 3 ;
[0012] The chitosan acetic acid solution is prepared by mixing chitosan and acetic acid aqueous solution, and stirring at room temperature at a stirring speed of 50-100 rpm for 20-30 minutes to obtain the chitosan acetic acid solution;
[0013] In the preparation of the chitosan acetic acid solution, the mass volume ratio of chitosan to acetic acid aqueous solution is 2-2.5 g: 200-300 mL;
[0014] The mass concentration of acetic acid aqueous solution is 1.5-2%;
[0015] The weight average molecular weight of the chitosan is 1×10 4 , the degree of deacetylation is 90%;
[0016] The chitosan microspheres are prepared by dropping chitosan acetic acid solution into liquid paraffin at room temperature, stirring the liquid paraffin at a stirring speed of 300-400 rpm, stirring at room temperature at a stirring speed of 300-400 rpm for 30-40 minutes after the dropping is completed, stirring at a stirring speed of 300-400 rpm for 20-30 minutes at 40-50° C., dropping polysorbate 80 while keeping the temperature and stirring speed unchanged, stirring at a stirring speed of 300-400 rpm for 20-30 minutes at 40-50° C. after the dropping is completed, adding glutaraldehyde aqueous solution and calcium carbonate in sequence, stirring at a stirring speed of 300-400 rpm at 40-50° C. Stir at a stirring speed of 50-60 min, add sodium hydroxide aqueous solution to adjust the pH to 9-9.5, stir at a stirring speed of 300-400 rpm for 3-3.5 h at 60-65 ° C, centrifuge at a speed of 8000-9000 rpm for 8-10 min, take the precipitate, wash the precipitate with petroleum ether 3-4 times, wash the precipitate with anhydrous ethanol 3-4 times, and then completely immerse in a hydrochloric acid aqueous solution at room temperature for 10-20 min, centrifuge at a speed of 8000-9000 rpm for 5-6 min, take the precipitate, wash the precipitate with distilled water 3-4 times, and place it at 70-80 ° C. Vacuum drying for 8-9 h to obtain chitosan microspheres;
[0017] In the preparation of chitosan microspheres, the mass volume ratio of chitosan acetic acid solution, liquid paraffin, polysorbate 80, glutaraldehyde aqueous solution, calcium carbonate, and hydrochloric acid aqueous solution is 100-110 mL: 450-500 mL: 3-4 mL: 10-12 mL: 0.3-0.4 g: 40-50 mL;
[0018] The volume concentration of the glutaraldehyde aqueous solution is 5%;
[0019] The mass concentration of the hydrochloric acid aqueous solution is 10%;
[0020] The particle size of the calcium carbonate is 100 nm;
[0021] The chitosan acetic acid solution is added at a rate of 4-5 mL / min;
[0022] The dropping speed of the polysorbate 80 is 1-1.5 mL / min;
[0023] The mass concentration of the sodium hydroxide aqueous solution is 1%;
[0024] The grafting comprises mixing chitosan microspheres and distilled water, stirring at a stirring speed of 400-500 rpm for 20-30 min at room temperature, adding block copolymer, stirring at a stirring speed of 400-500 rpm for 20-30 min at room temperature, adding glutaraldehyde aqueous solution, stirring at a stirring speed of 400-500 rpm for 50-60 min at 40-50° C., adding sodium hydroxide aqueous solution to adjust the pH to 9-9.5, stirring at a stirring speed of 400-500 rpm for 2-2.5 h at 60-65° C., centrifuging at a speed of 8000-9000 rpm for 5-6 min, taking a precipitate, washing the precipitate with distilled water for 3-4 times, and freeze-drying at -40° C. to -35° C. for 25-30 h to obtain a carrier;
[0025] In the grafting, the mass volume ratio of chitosan microspheres, distilled water, block copolymer, and glutaraldehyde aqueous solution is 5-6 g: 140-160 mL: 15-18 g: 50-55 mL;
[0026] The volume concentration of glutaraldehyde aqueous solution is 5%;
[0027] The mass concentration of the sodium hydroxide aqueous solution is 1%;
[0028] The preparation of the composite nanowires comprises the following steps: preparing hybrid nanowires, composite;
[0029] The hybrid nanowires are prepared by adding zinc nitrate and L-cysteine into distilled water, stirring at a stirring speed of 100-200 rpm for 20-30 min at room temperature, adding sodium hydroxide aqueous solution to adjust the pH to 9-9.5, stirring at a stirring speed of 100-200 rpm for 25-30 h at room temperature, centrifuging at a speed of 7000-8000 rpm for 8-10 min, taking a precipitate, washing the precipitate with distilled water for 3-4 times, and freeze-drying at -40°C to -35°C for 25-30 h to obtain the hybrid nanowires;
[0030] In the preparation of the hybrid nanowires, the mass volume ratio of zinc nitrate, L-cysteine, and distilled water is 20-22 g: 22-25 g: 950-1050 mL;
[0031] The mass concentration of the sodium hydroxide aqueous solution is 1%;
[0032] The composite comprises mixing γ-polyglutamic acid and PBS buffer solution, stirring at a stirring speed of 200-400 rpm for 10-15 min at room temperature, sequentially adding 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution and N-hydroxysuccinimide aqueous solution, stirring at a stirring speed of 200-400 rpm for 10-15 min at room temperature, then adding hybrid nanowires in an ice water bath, stirring in an ice water bath for 10-12 h, centrifuging at a speed of 7000-8000 rpm for 8-10 min, taking a precipitate, washing the precipitate with distilled water for 3-4 times, and freeze-drying at -40°C to -35°C for 25-30 h to obtain composite nanowires;
[0033] In the composite, the mass volume ratio of γ-polyglutamic acid, PBS buffer solution, 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution, N-hydroxysuccinimide, and hybrid nanowires is 2-2.1 g: 5000-5500 mL: 1000-1100 mL; 1300-1500 mL: 3-3.5 g;
[0034] The mass concentration of the 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution is 0.5%;
[0035] The mass concentration of the N-hydroxysuccinimide aqueous solution is 0.3%;
[0036] The weight average molecular weight of the γ-polyglutamic acid is 1×10 5 ;
[0037] The molar concentration of the PBS buffer solution is 0.01 mol / L, and the pH is 5.5;
[0038] The preparation of the antimicrobial peptide solution comprises the following steps: fermentation and treatment;
[0039] The fermentation comprises picking two loops of Bacillus subtilis from the slant with an inoculation loop, inoculating them into 120-150 mL of LB liquid culture medium, and culturing them at 36.5-37.5° C. and 120-150 rpm for 18-24 hours to obtain a seed solution; inoculating the seed solution into 4500-5000 mL of fermentation culture medium at an inoculation amount of 2-2.5% (volume percentage), and culturing them at 36.5-37.5° C. and 300-350 rpm for 24-30 hours to obtain a fermentation solution;
[0040] The ingredients of the LB liquid culture medium are: 10 g / L tryptone, 5 g / L yeast powder, 10 g / L sodium chloride, pH 7.0;
[0041] The fermentation medium comprises: 5% soybean meal, 4% corn starch, 2% glucose, 0.5% yeast extract powder, 0.15% sodium chloride, 0.1% magnesium sulfate, 0.05% potassium dihydrogen phosphate, 0.02% manganese sulfate, pH 7.0;
[0042] The Bacillus subtilis was purchased from the General Microbiological Center of China Microorganism Culture Collection Administration, and its classification name is Bacillus subtilis, and its collection number is CGMCC No.1.15792.
[0043] The treatment comprises centrifuging the fermentation broth at a speed of 15000-16000 rpm for 9-10 minutes, taking the supernatant, adding a hydrochloric acid aqueous solution with a molar concentration of 0.1 mol / L to the supernatant until no precipitation is generated, collecting the generated precipitate, adding a phosphate buffer to the precipitate until it is completely dissolved, filtering with an ultrafiltration membrane with a molecular weight cutoff of 20 kDa, collecting the filtrate, and then filtering with an ultrafiltration membrane with a molecular weight cutoff of 1 kDa, collecting the retentate, and concentrating the retentate at a vacuum degree of 0.095-0.097 MPa to one third of the original volume, and then placing it at -40°C to -35°C for freeze drying for 40-45 hours to obtain the antimicrobial peptide;
[0044] The molar concentration of the phosphate buffer is 0.02 mol / L, and the pH is 6.8;
[0045] The load comprises mixing the carrier, the antimicrobial peptide and distilled water, stirring at a stirring speed of 40-60 rpm for 2-2.5 hours at room temperature, centrifuging at a speed of 8000-9000 rpm for 5-6 minutes, taking the precipitate, washing the precipitate with distilled water for 3-4 times, and freeze-drying at -40°C to -35°C for 25-30 hours to obtain the load;
[0046] In the load, the mass volume ratio of the carrier, the antimicrobial peptide, and the distilled water is 30-32 g: 3-3.5 g: 600-650 mL;
[0047] The mixing, after mixing the load with the composite nanowires, is stirred at room temperature at a stirring speed of 40-60 rpm for 10-15 minutes to obtain a plant antibacterial agent containing antibacterial peptides;
[0048] In the mixing, the mass ratio of the support to the composite nanowires is 50-55:13-15.
[0049] A plant antibacterial agent containing antibacterial peptides prepared by the above-mentioned preparation method.
[0050] Compared with the prior art, the present invention has the following beneficial effects:
[0051] (1) In the preparation of the plant disease resistance agent containing antimicrobial peptides, a carrier is used to load the antimicrobial peptides. The antimicrobial peptides are produced by fermentation of Bacillus subtilis. In the preparation of the carrier, methoxy polyethylene glycol amino groups are first mixed with N6-benzyloxycarbonyl-L-lysine anhydride, and the amino groups in the methoxy polyethylene glycol amino groups react with the carboxyl groups after the ring opening of N6-benzyloxycarbonyl-L-lysine anhydride to generate a block copolymer with methoxy polyethylene glycol on one side and polylysine protected by a side chain containing a benzene ring on the other side, wherein the two end groups of the block copolymer are methoxy and amino groups, respectively; then chitosan microspheres are prepared, specifically, chitosan acetic acid solution is added to liquid paraffin, emulsified with polysorbate 80, and then glutaraldehyde is added to cross-link the chitosan, and calcium carbonate is added at the same time. The calcium carbonate is present in the cross-linked chitosan, and finally the calcium carbonate is removed by a hydrochloric acid aqueous solution to obtain chitosan microspheres with high porosity; finally, the block copolymer is mixed with the chitosan microspheres. Glutaraldehyde is added, and under the action of glutaraldehyde, the amino groups on the block copolymer are cross-linked with the amino groups remaining on the chitosan microspheres, and the amino groups on the block copolymer are also cross-linked with each other. Finally, the cross-linked products of the block copolymer and the chitosan microspheres are collected by centrifugation to obtain a carrier with chitosan microspheres as cores and the block copolymer grafted on the surface. When the carrier is used to load the antimicrobial peptide, most of the antimicrobial peptide is adsorbed in the chitosan microspheres, and the chitosan microspheres can play a role in sustained release and protection of the antimicrobial peptide. The polyethylene glycol of the block copolymer can promote dispersion and avoid agglomeration. The benzene ring in the polyethylene glycol and the polylysine with a side chain protection containing a benzene ring can play a stabilizing and protective role, and can prevent the temperature and the salt content in the soil from entering the chitosan microspheres to affect the antimicrobial peptide. At the same time, the polyethylene glycol can also improve the adsorption of the carrier to plants. The polylysine with a side chain protection containing a benzene ring can be adsorbed on the plant surface after use to promote the absorption of the antimicrobial peptide by the plant.In addition, in the preparation of the plant disease resistance agent containing antimicrobial peptides, the present invention also adds composite nanowires. In the preparation of the composite nanowires, zinc salt and L-cysteine are first mixed, and L-cysteine is dehydrated and polymerized under alkaline conditions, and zinc ions are bonded to the surface of the dehydrated polymer to obtain a nanoscale mixture containing zinc ions. The mixture contains not only zinc ions and polycysteine, but also unpolymerized L-cysteine. The zinc ions and peptide bonds can play a synergistic role to promote the adsorption of antimicrobial peptides by plants. However, considering that the mixture has poor dispersibility and is easy to precipitate, γ-polyglutamic acid is mixed with the mixture, and 1-ethyl-(3-dimethylamino)-1-nitropropene is added. The carboxyl groups in γ-polyglutamic acid are activated by using 1,2-diaminopropyl)carbodiimide, and the carboxyl groups in γ-polyglutamic acid react with the amino groups in the mixture, specifically react with the terminal amino groups in polycysteine and the amino groups in the adsorbed L-cysteine, thereby obtaining nanowires with γ-polyglutamic acid composited on the surface. The presence of γ-polyglutamic acid can improve the dispersibility of the nanowires. γ-polyglutamic acid also introduces new peptide bonds, thereby further improving the adsorption of antimicrobial peptides by plants. Zinc ions, polycysteine and γ-polyglutamic acid can also work synergistically to improve the disease resistance and stress resistance of plants, thereby avoiding the influence of temperature and salt content in the soil on plant growth.
[0052] (2) The anti-disease effect of the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention is less affected by temperature. In an environment of 10°C, wheat seeds were soaked in the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention and then sown. The average germination rate after 7 days was 97.3-97.5%, and the average seedling emergence rate after 14 days was 97.0-97.5%. In an environment of 25°C, wheat seeds were soaked in the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention and then sown. The average germination rate after 7 days was 98.0-98.3%, and the average seedling emergence rate after 14 days was 97.5-98.0%.
[0053] (3) The anti-disease effect of the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention is less affected by the salt content in the soil. After wheat seeds were sown in soil with a salt content of 0.2% for 14 days, the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention was sprayed twice, each time with an interval of 10 days. After the second spraying treatment for 20 days, the survival rate was 97.6-98.2%; after wheat seeds were sown in soil with a salt content of 0.05% for 14 days, the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention was sprayed twice, each time with an interval of 10 days. After the second spraying treatment for 20 days, the survival rate was 98.0-98.4%;
[0054] (4) The plant disease-resistant agent containing antimicrobial peptides prepared by the present invention is not easy to agglomerate during use. After the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention was sprayed on wheat twice, there was no powder agglomeration on the surface of the wheat plants;
[0055] (5) The plant disease-resistant agent containing antimicrobial peptides prepared by the present invention has good dispersibility in water. After 10 g of the plant disease-resistant agent containing antimicrobial peptides prepared by the present invention was mixed with 500 mL of distilled water, the mixture was stirred at room temperature at a stirring speed of 100 rpm for 30 min and then allowed to stand for 2 h. No precipitation was generated at the bottom. DETAILED DESCRIPTION
[0056] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific implementation methods of the present invention are now described.
[0057] Example 1
[0058] A method for preparing a plant disease-resistant agent containing antimicrobial peptides, specifically comprising:
[0059] 1. Preparation of carrier:
[0060] (1) Preparation of block copolymer: Under the protection of nitrogen, 5 g of methoxy polyethylene glycol amino and 1000 mL of N,N-dimethylformamide were mixed, and the mixture was stirred at 40°C at a stirring speed of 50 rpm for 10 min, 7 g of N6-benzyloxycarbonyl-L-lysine cyclic anhydride was added, and the mixture was stirred at 40°C at a stirring speed of 50 rpm for 45 h. After adding 6000 mL of ether for precipitation, the mixture was filtered, and the residue was washed with ether for 3 times, and freeze-dried at -40°C for 25 h to obtain a block copolymer;
[0061] The weight average molecular weight of the methoxy polyethylene glycol amino group is 2×10 3 ;
[0062] (2) Preparation of chitosan acetic acid solution: 2 g of chitosan and 200 mL of 1.5% acetic acid aqueous solution were mixed, and the mixture was stirred at room temperature at a stirring speed of 50 rpm for 20 min to obtain a chitosan acetic acid solution;
[0063] The weight average molecular weight of the chitosan is 1×10 4 , the degree of deacetylation is 90%;
[0064] (3) Preparation of chitosan microspheres: 100 mL of chitosan acetic acid solution was added dropwise to 450 mL of liquid paraffin at room temperature. The liquid paraffin was stirred at a stirring speed of 300 rpm. The chitosan acetic acid solution was added at a dropping speed of 4 mL / min. After the addition, the mixture was stirred at a stirring speed of 300 rpm for 30 min at room temperature. After the addition, the mixture was stirred at a stirring speed of 300 rpm for 20 min at 40 °C. While maintaining the temperature and stirring speed, 3 mL of polysorbate 80 was added dropwise. The dropping speed was controlled to be 1 mL / min. After the addition, the mixture was stirred at a stirring speed of 300 rpm for 20 min at 40 °C. Then, 10 mL of 5% by volume concentration of polysorbate 80 was added in sequence. Glutaraldehyde aqueous solution and 0.3g calcium carbonate were stirred at 40°C at a stirring speed of 300rpm for 50min, a sodium hydroxide aqueous solution with a mass concentration of 1% was added to adjust the pH to 9, and the mixture was stirred at a stirring speed of 300rpm for 3h at 60°C, centrifuged at a speed of 8000rpm for 8min, the precipitate was taken, and the precipitate was washed 3 times with petroleum ether, and the precipitate was washed 3 times with anhydrous ethanol, and then completely immersed in 40mL of a 10% hydrochloric acid aqueous solution at room temperature for 10min, centrifuged at a speed of 8000rpm for 5min, the precipitate was taken, and the precipitate was washed 3 times with distilled water, and vacuum dried at 70°C for 8h to obtain chitosan microspheres;
[0065] The particle size of the calcium carbonate is 100 nm;
[0066] (4) Grafting: 5 g of chitosan microspheres and 140 mL of distilled water were mixed, and the mixture was stirred at 400 rpm for 20 min at room temperature. 15 g of block copolymer was added, and the mixture was stirred at 400 rpm for 20 min at room temperature. 50 mL of 5% glutaraldehyde aqueous solution was added, and the mixture was stirred at 400 rpm for 50 min at 40°C. A 1% sodium hydroxide aqueous solution was added to adjust the pH to 9, and the mixture was stirred at 400 rpm for 2 h at 60°C. The mixture was centrifuged at 8000 rpm for 5 min, and the precipitate was taken. The precipitate was washed three times with distilled water, and freeze-dried at -40°C for 25 h to obtain a carrier.
[0067] 2. Preparation of composite nanowires:
[0068] (1) Preparation of hybrid nanowires: 20 g zinc nitrate and 22 g L-cysteine were added to 950 mL distilled water, stirred at 100 rpm for 20 min at room temperature, 1% sodium hydroxide aqueous solution was added to adjust the pH to 9, stirred at 100 rpm for 25 h at room temperature, centrifuged at 7000 rpm for 8 min, the precipitate was taken, washed with distilled water for 3 times, and freeze-dried at -40 °C for 25 h to obtain hybrid nanowires;
[0069] (2) Composite: 2 g of γ-polyglutamic acid and 5000 mL of PBS buffer solution (0.01 mol / L, pH 5.5) were mixed, stirred at 200 rpm for 10 min at room temperature, 1000 mL of 0.5% 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution and 1300 mL of 0.3% N-hydroxysuccinimide aqueous solution were added in sequence, stirred at 200 rpm for 10 min at room temperature, and then 3 g of hybrid nanowires were added in an ice-water bath, stirred in an ice-water bath for 10 h, centrifuged at 7000 rpm for 8 min, and the precipitate was taken. The precipitate was washed with distilled water for 3 times and freeze-dried at -40 °C for 25 h to obtain composite nanowires.
[0070] The weight average molecular weight of the γ-polyglutamic acid is 1×10 5 ;
[0071] 3. Preparation of antimicrobial peptide solution:
[0072] (1) Fermentation: Use an inoculation loop to pick two loops of Bacillus subtilis from the slant, inoculate them into 120 mL of LB liquid medium, and culture them at 36.5°C and 120 rpm for 18 h to obtain seed liquid; inoculate the seed liquid into 4500 mL of fermentation medium at an inoculation rate of 2% (volume percentage), and culture them at 36.5°C and 300 rpm for 24 h to obtain fermentation liquid;
[0073] The ingredients of the LB liquid culture medium are: 10 g / L tryptone, 5 g / L yeast powder, 10 g / L sodium chloride, pH 7.0;
[0074] The fermentation medium comprises: 5% soybean meal, 4% corn starch, 2% glucose, 0.5% yeast extract powder, 0.15% sodium chloride, 0.1% magnesium sulfate, 0.05% potassium dihydrogen phosphate, 0.02% manganese sulfate, pH 7.0;
[0075] The Bacillus subtilis was purchased from the General Microbiological Center of China Microorganism Culture Collection Administration, and its classification name is Bacillus subtilis, and its collection number is CGMCC No.1.15792.
[0076] (2) Treatment: centrifuge the fermentation broth at a speed of 15000 rpm for 9 minutes, take the supernatant, add a hydrochloric acid aqueous solution with a molar concentration of 0.1 mol / L to the supernatant until no precipitation is generated, collect the generated precipitate, add phosphate buffer (0.02 mol / L, pH 6.8) to the precipitate until it is completely dissolved, filter using an ultrafiltration membrane with a molecular weight cutoff of 20 kDa, collect the filtrate, and then filter using an ultrafiltration membrane with a molecular weight cutoff of 1 kDa, collect the retentate, and low-pressure concentrate the retentate to one-third of the original volume at a vacuum degree of 0.095 MPa, and then freeze-dry it at -40°C for 40 hours to obtain the antimicrobial peptide;
[0077] 4. Loading: Mix 30 g of carrier, 3 g of antimicrobial peptide, and 600 mL of distilled water, stir at room temperature at a stirring speed of 40 rpm for 2 h, centrifuge at a speed of 8000 rpm for 5 min, take the precipitate, wash the precipitate with distilled water 3 times, and freeze-dry at -40 ° C for 25 h to obtain the loading material;
[0078] 5. Mixing: After mixing 50 g of the load with 13 g of the composite nanowires, stir at room temperature at a stirring speed of 40 rpm for 10 min to obtain a plant antibacterial agent containing antibacterial peptides.
[0079] This embodiment also provides a plant antibacterial agent containing antibacterial peptides prepared by the aforementioned preparation method.
[0080] Example 2
[0081] A method for preparing a plant disease-resistant agent containing antimicrobial peptides, specifically comprising:
[0082] 1. Preparation of carrier:
[0083] (1) Preparation of block copolymer: Under the protection of nitrogen, 5.2 g of methoxy polyethylene glycol amino and 1100 mL of N,N-dimethylformamide were mixed, and the mixture was stirred at 45°C at a stirring speed of 50 rpm for 15 min, 7.5 g of N6-benzyloxycarbonyl-L-lysine cyclic anhydride was added, and the mixture was stirred at 45°C at a stirring speed of 50 rpm for 48 h. After adding 6500 mL of ether for precipitation, the mixture was filtered, and the residue was washed with ether for 3 times, and freeze-dried at -40°C for 28 h to obtain a block copolymer;
[0084] The weight average molecular weight of the methoxy polyethylene glycol amino group is 2×10 3 ;
[0085] (2) Preparation of chitosan acetic acid solution: 2.2 g of chitosan and 250 mL of 1.5% acetic acid aqueous solution were mixed, and the mixture was stirred at room temperature at a stirring speed of 50 rpm for 25 min to obtain a chitosan acetic acid solution;
[0086] The weight average molecular weight of the chitosan is 1×10 4 , the degree of deacetylation is 90%;
[0087] (3) Preparation of chitosan microspheres: 105 mL of chitosan acetic acid solution was added dropwise to 470 mL of liquid paraffin at room temperature. The liquid paraffin was stirred at a stirring speed of 350 rpm. The chitosan acetic acid solution was added dropwise at a speed of 4 mL / min. After the addition was completed, the mixture was stirred at a stirring speed of 350 rpm for 35 min at room temperature. After the addition was completed, the mixture was stirred at a stirring speed of 350 rpm for 25 min at 45 °C. While maintaining the temperature and stirring speed, 3 mL of polysorbate 80 was added dropwise at a speed of 1 mL / min. After the addition was completed, the mixture was stirred at a stirring speed of 350 rpm for 25 min at 45 °C. Then, 11 mL of 5% by volume Glutaraldehyde aqueous solution and 0.3g calcium carbonate were stirred at 45°C at a stirring speed of 350rpm for 55min, a sodium hydroxide aqueous solution with a mass concentration of 1% was added to adjust the pH to 9, and the mixture was stirred at a stirring speed of 350rpm for 3h at 60°C, centrifuged at a speed of 8500rpm for 9min, the precipitate was taken, and the precipitate was washed 3 times with petroleum ether, and washed 3 times with anhydrous ethanol, and then completely immersed in 45mL of a 10% hydrochloric acid aqueous solution at room temperature for 15min, centrifuged at a speed of 8500rpm for 5min, the precipitate was taken, and the precipitate was washed 3 times with distilled water, and vacuum dried at 75°C for 8h to obtain chitosan microspheres;
[0088] The particle size of the calcium carbonate is 100 nm;
[0089] (4) Grafting: 5.5 g of chitosan microspheres and 150 mL of distilled water were mixed, stirred at 450 rpm for 25 min at room temperature, 17 g of block copolymer was added, stirred at 450 rpm for 25 min at room temperature, 52 mL of 5% glutaraldehyde aqueous solution was added, stirred at 45°C for 55 min at 450 rpm, 1% sodium hydroxide aqueous solution was added to adjust the pH to 9, stirred at 450 rpm for 2 h at 62°C, centrifuged at 8500 rpm for 5 min, the precipitate was taken, washed with distilled water 3 times, and freeze-dried at -40°C for 27 h to obtain a carrier;
[0090] 2. Preparation of composite nanowires:
[0091] (1) Preparation of hybrid nanowires: 21 g zinc nitrate and 24 g L-cysteine were added to 1000 mL distilled water, stirred at 150 rpm for 25 min at room temperature, 1% sodium hydroxide aqueous solution was added to adjust the pH to 9, stirred at 150 rpm for 27 h at room temperature, centrifuged at 7500 rpm for 9 min, the precipitate was taken, washed with distilled water for 3 times, and freeze-dried at -40°C to -35°C for 27 h to obtain hybrid nanowires;
[0092] (2) Composite: 2 g of γ-polyglutamic acid and 5200 mL of PBS buffer solution (0.01 mol / L, pH 5.5) were mixed, stirred at 300 rpm for 12 min at room temperature, and 1050 mL of 0.5% 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution and 1400 mL of 0.3% N-hydroxysuccinimide aqueous solution were added in sequence, stirred at 300 rpm for 12 min at room temperature, and then 3.2 g of hybrid nanowires were added in an ice-water bath, stirred in an ice-water bath for 11 h, centrifuged at 7500 rpm for 9 min, and the precipitate was taken. The precipitate was washed with distilled water for 3 times and freeze-dried at -40 °C for 27 h to obtain composite nanowires.
[0093] The weight average molecular weight of the γ-polyglutamic acid is 1×10 5 ;
[0094] 3. Preparation of antimicrobial peptide solution:
[0095] (1) Fermentation: Use an inoculation loop to pick two loops of Bacillus subtilis from the slant, inoculate them into 140 mL of LB liquid medium, and culture them at 37°C and 140 rpm for 21 h to obtain seed liquid; inoculate the seed liquid into 4800 mL of fermentation medium at an inoculation rate of 2.2% (volume percentage), and culture them at 37°C and 320 rpm for 27 h to obtain fermentation liquid;
[0096] The ingredients of the LB liquid culture medium are: 10 g / L tryptone, 5 g / L yeast powder, 10 g / L sodium chloride, pH 7.0;
[0097] The fermentation medium comprises: 5% soybean meal, 4% corn starch, 2% glucose, 0.5% yeast extract powder, 0.15% sodium chloride, 0.1% magnesium sulfate, 0.05% potassium dihydrogen phosphate, 0.02% manganese sulfate, pH 7.0;
[0098] The Bacillus subtilis was purchased from the General Microbiological Center of China Microorganism Culture Collection Administration, and its classification name is Bacillus subtilis, and its collection number is CGMCC No.1.15792.
[0099] (2) Treatment: centrifuge the fermentation broth at a speed of 15000 rpm for 10 min, take the supernatant, add a hydrochloric acid aqueous solution with a molar concentration of 0.1 mol / L to the supernatant until no more precipitation is produced, collect the produced precipitate, add phosphate buffer (0.02 mol / L, pH 6.8) to the precipitate until it is completely dissolved, filter using an ultrafiltration membrane with a molecular weight cutoff of 20 kDa, collect the filtrate, and then filter using an ultrafiltration membrane with a molecular weight cutoff of 1 kDa, collect the retentate, and low-pressure concentrate the retentate to one-third of the original volume at a vacuum degree of 0.096 MPa, and then freeze-dry it at -40°C for 42 hours to obtain the antimicrobial peptide;
[0100] 4. Loading: 31 g of carrier, 3.2 g of antimicrobial peptide, and 620 mL of distilled water were mixed, stirred at 50 rpm for 2 h at room temperature, centrifuged at 8500 rpm for 5 min, the precipitate was taken, washed with distilled water for 3 times, and freeze-dried at -40 ° C for 27 h to obtain the loading material;
[0101] 5. Mixing: After mixing 52 g of the load with 14 g of the composite nanowires, stir at room temperature at a stirring speed of 50 rpm for 12 min to obtain a plant antibacterial agent containing antibacterial peptides.
[0102] This embodiment also provides a plant antibacterial agent containing antibacterial peptides prepared by the aforementioned preparation method.
[0103] Example 3
[0104] A method for preparing a plant disease-resistant agent containing antimicrobial peptides, specifically comprising:
[0105] 1. Preparation of carrier:
[0106] (1) Preparation of block copolymer: Under the protection of nitrogen, 5.5 g of methoxy polyethylene glycol amino and 1200 mL of N,N-dimethylformamide were mixed, and the mixture was stirred at 50°C at a stirring speed of 100 rpm for 20 min, 8 g of N6-benzyloxycarbonyl-L-lysine cyclic anhydride was added, and the mixture was stirred at 50°C at a stirring speed of 100 rpm for 50 h. After adding 7000 mL of ether for precipitation, the mixture was filtered, and the residue was washed with ether for 4 times, and freeze-dried at -35°C for 30 h to obtain a block copolymer;
[0107] The weight average molecular weight of the methoxy polyethylene glycol amino group is 2×10 3 ;
[0108] (2) Preparation of chitosan acetic acid solution: 2.5 g of chitosan and 300 mL of 2% acetic acid aqueous solution were mixed, and the mixture was stirred at room temperature at a stirring speed of 100 rpm for 30 min to obtain a chitosan acetic acid solution;
[0109] The weight average molecular weight of the chitosan is 1×10 4 , the degree of deacetylation is 90%;
[0110] (3) Preparation of chitosan microspheres: 110 mL of chitosan acetic acid solution was added dropwise to 500 mL of liquid paraffin at room temperature, while stirring the liquid paraffin at a stirring speed of 400 rpm. The chitosan acetic acid solution was added dropwise at a speed of 5 mL / min. After the addition was completed, the mixture was stirred at a stirring speed of 400 rpm for 40 min at room temperature, and at a stirring speed of 400 rpm for 30 min at 50°C. While maintaining the temperature and stirring speed, 4 mL of polysorbate 80 was added dropwise at a speed of 1.5 mL / min. After the addition was completed, the mixture was stirred at a stirring speed of 400 rpm for 30 min at 50°C. Then, 12 mL of 5% pentanediol was added in sequence. The aldehyde aqueous solution and 0.4g calcium carbonate were stirred at 50°C at a stirring speed of 400rpm for 60min, a sodium hydroxide aqueous solution with a mass concentration of 1% was added to adjust the pH to 9.5, and the mixture was stirred at a stirring speed of 400rpm at 65°C for 3.5h, centrifuged at a speed of 9000rpm for 10min, the precipitate was taken, and the precipitate was washed 4 times with petroleum ether, and the precipitate was washed 4 times with anhydrous ethanol, and then completely immersed in 50mL of a 10% hydrochloric acid aqueous solution at room temperature for 20min, centrifuged at a speed of 9000rpm for 6min, the precipitate was taken, and the precipitate was washed 4 times with distilled water, and vacuum dried at 80°C for 9h to obtain chitosan microspheres;
[0111] The particle size of the calcium carbonate is 100 nm;
[0112] (4) Grafting: 6 g of chitosan microspheres and 160 mL of distilled water were mixed, and stirred at 500 rpm for 30 min at room temperature. 18 g of block copolymer was added, and stirred at 500 rpm for 30 min at room temperature. 55 mL of 5% glutaraldehyde aqueous solution was added, and stirred at 500 rpm for 60 min at 50°C. 1% sodium hydroxide aqueous solution was added to adjust the pH to 9.5, and stirred at 500 rpm for 2.5 h at 65°C. The mixture was centrifuged at 9000 rpm for 6 min, and the precipitate was taken. The precipitate was washed with distilled water for 4 times, and freeze-dried at -35°C for 30 h to obtain a carrier.
[0113] 2. Preparation of composite nanowires:
[0114] (1) Preparation of hybrid nanowires: 22 g zinc nitrate and 25 g L-cysteine were added to 1050 mL distilled water, stirred at 200 rpm for 30 min at room temperature, 1% sodium hydroxide aqueous solution was added to adjust the pH to 9.5, stirred at 200 rpm for 30 h at room temperature, centrifuged at 8000 rpm for 10 min, the precipitate was taken, washed with distilled water 4 times, and freeze-dried at -35 °C for 30 h to obtain hybrid nanowires;
[0115] (2) Composite: 2.1 g of γ-polyglutamic acid and 5500 mL of PBS buffer solution (0.01 mol / L, pH 5.5) were mixed, stirred at 400 rpm for 15 min at room temperature, 1100 mL of 0.5% 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution and 1500 mL of 0.3% N-hydroxysuccinimide aqueous solution were added in sequence, stirred at 400 rpm for 15 min at room temperature, and then 3.5 g of hybrid nanowires were added in an ice-water bath, stirred in an ice-water bath for 12 h, centrifuged at 8000 rpm for 10 min, and the precipitate was taken. The precipitate was washed with distilled water 4 times and freeze-dried at -35 °C for 30 h to obtain composite nanowires.
[0116] The weight average molecular weight of the γ-polyglutamic acid is 1×10 5 ;
[0117] 3. Preparation of antimicrobial peptide solution:
[0118] (1) Fermentation: Use an inoculation loop to pick two loops of Bacillus subtilis from the slant, inoculate them into 150 mL of LB liquid culture medium, and culture them at 37.5°C and 150 rpm for 24 h to obtain seed liquid; inoculate the seed liquid into 5000 mL of fermentation medium at an inoculation rate of 2.5% (volume percentage), and culture them at 37.5°C and 350 rpm for 30 h to obtain fermentation liquid;
[0119] The ingredients of the LB liquid culture medium are: 10 g / L tryptone, 5 g / L yeast powder, 10 g / L sodium chloride, pH 7.0;
[0120] The fermentation medium comprises: 5% soybean meal, 4% corn starch, 2% glucose, 0.5% yeast extract powder, 0.15% sodium chloride, 0.1% magnesium sulfate, 0.05% potassium dihydrogen phosphate, 0.02% manganese sulfate, pH 7.0;
[0121] The Bacillus subtilis was purchased from the General Microbiological Center of China Microorganism Culture Collection Administration, and its classification name is Bacillus subtilis, and its collection number is CGMCC No.1.15792.
[0122] (2) Treatment: centrifuge the fermentation broth at a speed of 16000 rpm for 10 min, take the supernatant, add a hydrochloric acid aqueous solution with a molar concentration of 0.1 mol / L to the supernatant until no precipitation is generated, collect the generated precipitate, add phosphate buffer (0.02 mol / L, pH 6.8) to the precipitate until it is completely dissolved, filter using an ultrafiltration membrane with a molecular weight cutoff of 20 kDa, collect the filtrate, and then filter using an ultrafiltration membrane with a molecular weight cutoff of 1 kDa, collect the retentate, and low-pressure concentrate the retentate to one-third of the original volume at a vacuum degree of 0.097 MPa, and then freeze-dry it at -35°C for 45 hours to obtain the antimicrobial peptide;
[0123] 4. Loading: 32 g of carrier, 3.5 g of antimicrobial peptide and 650 mL of distilled water were mixed, stirred at 60 rpm for 2.5 h at room temperature, centrifuged at 9000 rpm for 6 min, the precipitate was taken, washed with distilled water 4 times, and freeze-dried at -35 ° C for 30 h to obtain the loading material;
[0124] 5. Mixing: After mixing 55 g of the load with 15 g of the composite nanowires, stir at room temperature at a stirring speed of 60 rpm for 15 min to obtain a plant antibacterial agent containing antibacterial peptides.
[0125] This embodiment also provides a plant antibacterial agent containing antibacterial peptides prepared by the aforementioned preparation method.
[0126] Comparative Example 1
[0127] The difference between this comparative example and Example 2 is that: in the first step of preparing the carrier, the step (1) of preparing the block copolymer and the step (4) of grafting are omitted, that is, the chitosan microspheres obtained in the step (3) of preparing the chitosan microspheres are used as the carrier in the loading step 4.
[0128] The remaining operations are the same as those in Example 2.
[0129] Comparative Example 2
[0130] The difference between this comparative example and Example 2 is that the second step of preparing the composite nanowires and the fifth step of mixing are omitted, that is, the loaded material obtained in the fourth step is directly used as the plant antibacterial agent containing antibacterial peptides.
[0131] The remaining operations are the same as those in Example 2.
[0132] Test Example 1
[0133] 1200 wheat seeds of Jimai 22 with full grains were selected and divided into 6 groups, each with 200 seeds, and marked as groups 1-6;
[0134] At 10°C, groups 1-6 of wheat seeds were completely soaked in distilled water, and after 30 hours, the wheat seeds were taken out, and then the plant antibacterial agents containing antimicrobial peptides prepared in Examples 1-3 and Comparative Examples 1-2 were mixed with distilled water to prepare treatment solutions with a concentration of 200 mg / L; then, at 10°C, groups 1-5 of wheat seeds were soaked in 500 mL of the treatment solution, and group 6 was used as a blank control, and 6 groups were soaked in 500 mL of distilled water, and the corresponding relationship is as follows:
[0135]
[0136] After 30 minutes, take out the seeds and sow them in germination boxes covered with 3 cm thick nutrient soil. The sowing method and sowing density are controlled to be the same. Then cover with 0.5 cm nutrient soil and spray water to keep the nutrient water moist. Then place the germination box in an environment with a temperature of 10°C and spray water once in the morning and evening to keep the nutrient water moist. After 7 days, the germination rate is counted, and after 14 days, the seedling rate is counted.
[0137] The above test was repeated 3 times, and the average germination rate and average seedling rate were calculated. The results are as follows:
[0138]
[0139] Test Example 2
[0140] 1200 wheat seeds of Jimai 22 with full grains were selected and divided into 6 groups, each with 200 seeds, and marked as groups 1-6;
[0141] At 25°C, groups 1-6 of wheat seeds were completely soaked in distilled water. After 30 hours, the wheat seeds were taken out, and then the plant antibacterial agents containing antimicrobial peptides prepared in Examples 1-3 and Comparative Examples 1-2 were mixed with distilled water to prepare treatment solutions with a concentration of 200 mg / L; then, at 25°C, groups 1-5 of wheat seeds were soaked in 500 mL of the treatment solution, and group 6 was used as a blank control. The corresponding relationships are as follows:
[0142]
[0143] After 30 minutes, the seeds were taken out and sown in germination boxes covered with 3 cm thick nutrient soil, and the sowing method and sowing density were controlled to be the same. Then, 0.5 cm of nutrient soil was covered and water was sprayed to keep the nutrient water moist. Then, the germination box was placed in an environment with a temperature of 25°C and water was sprayed once in the morning and evening to keep the nutrient water moist. After 7 days, the germination rate was counted, and after 14 days, the seedling rate was counted.
[0144] The above test was repeated 3 times, and the average germination rate and average seedling rate were calculated. The results are as follows:
[0145]
[0146] Test Example 3
[0147] 3,000 wheat seeds of Jimai 22 with full grains were selected and divided into 6 groups, each with 500 seeds, and marked as groups 1-6;
[0148] At 25°C, the wheat seeds of groups 1-6 were completely soaked in distilled water. After 30 hours, the wheat seeds were taken out and then sown in soil with a salt content of 0.2%. The sowing method and sowing density were controlled to be the same. After 14 days, the plant antibacterial agent containing antimicrobial peptides prepared in Examples 1-3 and Comparative Examples 1-2 were mixed with distilled water to prepare a treatment solution with a concentration of 50 mg / L. Then, 1200 mL of the treatment solution was used to spray groups 1-5 for the first time, and group 6 was used as a blank control. 1200 mL of distilled water was used to spray the 6 groups. The corresponding relationship is as follows:
[0149]
[0150] 10 days after the first spraying treatment, the second spraying treatment was carried out on groups 1-6. The first spraying treatment was carried out in the same way as the second spraying treatment. 20 days after the second spraying treatment, the survival rate was calculated. The statistical results are as follows:
[0151]
[0152] Test Example 4
[0153] 3,000 wheat seeds of Jimai 22 with full grains were selected and divided into 6 groups, each with 500 seeds, and marked as groups 1-6;
[0154] At 25°C, the wheat seeds of groups 1-6 were completely soaked in distilled water. After 30 hours, the wheat seeds were taken out and then sown in soil with a salt content of 0.05%. The sowing method and sowing density were controlled to be the same. After 14 days, the plant antibacterial agent containing antimicrobial peptides prepared in Examples 1-3 and Comparative Examples 1-2 were mixed with distilled water to prepare a treatment solution with a concentration of 50 mg / L. Then, 1200 mL of the treatment solution was used to spray groups 1-5 for the first time, and group 6 was used as a blank control. 1200 mL of distilled water was used to spray the 6 groups. The corresponding relationship is as follows:
[0155]
[0156] 10 days after the first spraying treatment, the second spraying treatment was carried out on groups 1-6. The first spraying treatment was carried out in the same way as the second spraying treatment. 20 days after the second spraying treatment, the survival rate was calculated. The statistical results are as follows:
[0157]
[0158] Ten days after the second spraying, the presence of powder agglomeration on wheat plants in groups 1-5 was observed. The results are as follows:
[0159]
[0160] Test Example 5
[0161] 10 g of the plant antibacterial agent containing antimicrobial peptides prepared in Example 1-3 and Comparative Example 1-2 were mixed with 500 mL of distilled water, stirred at room temperature at a stirring speed of 100 rpm for 30 min, and then allowed to stand for 2 h to observe whether there was precipitation at the bottom. The observation results were as follows:
[0162]
[0163] From the results of Experimental Examples 1-5, it can be seen that by using block copolymers to graft chitosan microspheres as carriers, the effects of temperature and soil salt content on the anti-disease effect of the antimicrobial peptide-containing plant disease-resistant agent can be reduced, and the antimicrobial peptide-containing plant disease-resistant agent can be ensured to be less likely to agglomerate during use and have good dispersibility in water;
[0164] By adding composite nanowires to the plant disease-resistant agent containing antimicrobial peptides, the effects of temperature and salt content in the soil on the disease-resistant effect of the plant disease-resistant agent containing antimicrobial peptides can be reduced.
[0165] Unless otherwise specified, all percentages used in the present invention are by mass.
[0166] Finally, it should be noted that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing a plant disease resistance agent containing antimicrobial peptides, characterized in that: The method comprises the following steps: preparing a carrier, preparing a composite nanowire, preparing an antimicrobial peptide solution, loading, and mixing; The preparation of the carrier comprises the following steps: preparing a block copolymer, preparing a chitosan acetic acid solution, preparing chitosan microspheres, and grafting; The block copolymer is prepared by mixing methoxy polyethylene glycol amino and N,N-dimethylformamide under the protection of nitrogen, stirring at 40-50° C., adding N6-benzyloxycarbonyl-L-lysine cyclic anhydride, stirring at 40-50° C., adding ether for precipitation, filtering, taking the filter residue, washing, and freeze-drying the filter residue to obtain the block copolymer; The preparation of chitosan microspheres comprises the following steps: adding chitosan acetic acid solution dropwise to liquid paraffin at room temperature, stirring the liquid paraffin at the same time, stirring at room temperature after the addition is completed, stirring at 40-50° C., adding polysorbate 80 dropwise while maintaining the temperature and stirring speed unchanged, stirring at 40-50° C. after the addition is completed, adding glutaraldehyde aqueous solution and calcium carbonate in sequence, stirring at 40-50° C., adjusting the pH to 9-9.5, stirring at 60-65° C., centrifuging, taking a precipitate, washing the precipitate, and then completely immersing the mixture in a hydrochloric acid aqueous solution at room temperature, centrifuging, taking a precipitate, washing, and vacuum drying the precipitate to obtain chitosan microspheres; The grafting comprises mixing chitosan microspheres and distilled water, stirring at room temperature, adding block copolymer, stirring at room temperature, adding glutaraldehyde aqueous solution, stirring at 40-50° C., adjusting the pH to 9-9.5, stirring at 60-65° C., centrifuging, taking a precipitate, washing, and freeze-drying the precipitate to obtain a carrier; The preparation of the composite nanowires comprises the following steps: preparing hybrid nanowires, composite; The hybrid nanowires are prepared by adding zinc nitrate and L-cysteine to distilled water, stirring at room temperature, adding sodium hydroxide aqueous solution to adjust the pH to 9-9.5, stirring at room temperature, centrifuging, taking a precipitate, washing, and freeze-drying the precipitate to obtain a hybrid nanowire; The composite comprises mixing γ-polyglutamic acid and PBS buffer solution, stirring at room temperature, sequentially adding 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution and N-hydroxysuccinimide aqueous solution, stirring at room temperature, then adding hybrid nanowires in an ice-water bath, stirring in an ice-water bath, centrifuging, taking a precipitate, washing, and freeze-drying the precipitate to obtain composite nanowires; The loading comprises mixing the carrier, the antimicrobial peptide and distilled water, stirring at room temperature, centrifuging, taking a precipitate, washing and freeze-drying the precipitate to obtain a loading substance; The loading material and the composite nanowires are mixed and then stirred at room temperature to obtain a plant antibacterial agent containing antibacterial peptides.
2. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: In the preparation of the block copolymer, the mass volume ratio of methoxy polyethylene glycol amino, N,N-dimethylformamide, N6-benzyloxycarbonyl-L-lysine cyclic anhydride and ether is 5-5.5g:1000-1200mL:7-8g:6000-7000mL.
3. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: The preparation of chitosan acetic acid solution comprises mixing chitosan and acetic acid aqueous solution, and stirring at room temperature to obtain chitosan acetic acid solution; In the preparation of the chitosan acetic acid solution, the mass volume ratio of chitosan to acetic acid aqueous solution is 2-2.5 g: 200-300 mL; The mass concentration of the acetic acid aqueous solution is 1.5-2%.
4. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: In the preparation of chitosan microspheres, the mass volume ratio of chitosan acetic acid solution, liquid paraffin, polysorbate 80, glutaraldehyde aqueous solution, calcium carbonate, and hydrochloric acid aqueous solution is 100-110 mL: 450-500 mL: 3-4 mL: 10-12 mL: 0.3-0.4 g: 40-50 mL; The volume concentration of the glutaraldehyde aqueous solution is 5%; The mass concentration of the hydrochloric acid aqueous solution is 10%; The chitosan acetic acid solution is added at a rate of 4-5 mL / min; The dropping speed of the polysorbate 80 is 1-1.5 mL / min.
5. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: In the grafting, the mass volume ratio of chitosan microspheres, distilled water, block copolymer, and glutaraldehyde aqueous solution is 5-6 g: 140-160 mL: 15-18 g: 50-55 mL; The volume concentration of the glutaraldehyde aqueous solution is 5%.
6. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: In the preparation of the hybrid nanowires, the mass volume ratio of zinc nitrate, L-cysteine and distilled water is 20-22g:22-25g:950-1050mL.
7. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: In the composite, the mass volume ratio of γ-polyglutamic acid, PBS buffer solution, 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution, N-hydroxysuccinimide, and hybrid nanowires is 2-2.1 g: 5000-5500 mL: 1000-1100 mL: 1300-1500 mL: 3-3.5 g; The mass concentration of the 1-ethyl-(3-dimethylaminopropyl)carbodiimide aqueous solution is 0.5%; The mass concentration of the N-hydroxysuccinimide aqueous solution is 0.3%; The concentration of the PBS buffer solution is 0.01 mol / L, and the pH is 5.
5.
8. The method for preparing the plant disease resistance agent containing antimicrobial peptides according to claim 1, characterized in that: The preparation of the antimicrobial peptide solution comprises the following steps: fermentation and treatment; The fermentation comprises picking two loops of Bacillus subtilis from the slant with an inoculation loop, inoculating them into 120-150 mL of LB liquid culture medium, and culturing them at 36.5-37.5° C. and 120-150 rpm for 18-24 hours to obtain a seed solution; inoculating the seed solution into 4500-5000 mL of fermentation culture medium at an inoculation rate of 2-2.5%, and culturing them at 36.5-37.5° C. and 300-350 rpm for 24-30 hours to obtain a fermentation solution; The ingredients of the LB liquid culture medium are: 10 g / L tryptone, 5 g / L yeast powder, 10 g / L sodium chloride, pH 7.0; The fermentation medium comprises: 5% soybean meal, 4% corn starch, 2% glucose, 0.5% yeast extract powder, 0.15% sodium chloride, 0.1% magnesium sulfate, 0.05% potassium dihydrogen phosphate, 0.02% manganese sulfate, pH 7.0; The Bacillus subtilis was purchased from the General Microbiological Center of China Microorganism Culture Collection Administration, and its classification name is Bacillus subtilis, and its collection number is CGMCC No.1.15792; The treatment comprises centrifuging the fermentation broth, taking the supernatant, adding a hydrochloric acid aqueous solution with a molar concentration of 0.1 mol / L to the supernatant until no precipitation is generated, collecting the generated precipitate, adding a phosphate buffer to the precipitate until it is completely dissolved, filtering with an ultrafiltration membrane with a molecular weight cutoff of 20 kDa, collecting the filtrate, and then filtering with an ultrafiltration membrane with a molecular weight cutoff of 1 kDa, collecting the retentate, concentrating under reduced pressure, and freeze-drying to obtain the antimicrobial peptide; The molar concentration of the phosphate buffer is 0.02 mol / L, and the pH is 6.
8.
9. The method for preparing a plant disease resistance agent containing an antimicrobial peptide according to claim 1, characterized in that: In the load, the mass volume ratio of the carrier, the antimicrobial peptide, and the distilled water is 30-32 g: 3-3.5 g: 600-650 mL; In the mixing, the mass ratio of the support to the composite nanowires is 50-55:13-15.
10. A plant antibacterial agent containing antibacterial peptides prepared by the preparation method according to any one of claims 1 to 9.