A method for producing low temperature resistant cable
The low-temperature protective layer is formed by extrusion module and bubble module, and combined with the curing cooling and quality evaluation module, the parameters are dynamically adjusted to form an outer protective layer, which solves the problems of brittleness and hardness in extremely low-temperature environments of traditional cables and is difficult to monitor quality, improving the problem of brittleness and hardness in the environment of extreme low-temperature, The low temperature resistance and toughness of the cable are achieved, and efficient quality control is achieved.
Patent Information
- Application Number
- CN202410761410.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-13
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-06-13
AI Technical Summary
Traditional cables are brittle and hard in extremely low temperature environments, which affects mechanical performance and electrical safety, and the quality of the insulation layer is difficult to monitor in real time, resulting in reduced cable toughness and shortened service life.
A low-temperature resistant cable production method is adopted to form a low-temperature protective layer by combining the extrusion module and the bubble module, and curing and cross-linking is used to cure and cool the module. The sampling module and the quality evaluation module monitor and dynamically adjust the extrusion parameters to form an outer protective layer. , improve the low temperature resistance and toughness of the cable.
It improves the low temperature resistance of the cable, ensures the accuracy and protection of the manufacturing process, improves the toughness and service life of the cable, and realizes reliable quality control and intelligent management.
Smart Images

Figure CN118538485B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of cable manufacturing, and in particular to a production method of a low-temperature resistant cable. Background Art
[0002] In extremely low temperature environments, traditional cable insulation materials (such as ordinary polyethylene or PVC) may become brittle and hard, affecting their mechanical properties and electrical safety.
[0003] For example, Chinese patent CN114927274B discloses a low-temperature resistant three-core ultra-flexible cable. Although the wear resistance of the cable is improved by arranging a rubber wear-resistant outer skin, a filling cotton net, a support plate, a low-temperature resistant layer and a tension mechanism on the outer periphery of the cable, the weight of the cable has a significant impact on the operating performance and energy efficiency. At the same time, the traditional solid insulation material increases the weight of the cable, limiting the performance optimization of these applications.
[0004] At the same time, in traditional cable production, the quality and consistency of the insulation layer are often difficult to monitor in real time on the production line, resulting in cable quality problems being discovered only in later tests, affecting production efficiency and cost control.
[0005] In addition, low temperature environment may accelerate the aging process of certain insulating materials, such as causing the polymer network to break or the cross-linking density to change, thereby reducing the service life and safety of the cable. Under low temperature conditions, the toughness of the material decreases and it is more prone to mechanical damage.
[0006] The present invention is made to solve the common problems in the field, such as poor protection effect, easy aging, difficult quality control, lack of online evaluation, difficult to ensure cable toughness and intelligence level, etc. Summary of the invention
[0007] The purpose of the present invention is to propose a production method of a low-temperature resistant cable in view of the existing deficiencies.
[0008] In order to overcome the shortcomings of the prior art, the present invention adopts the following technical solutions:
[0009] A method for producing a low-temperature resistant cable, the method comprising the following steps:
[0010] S1, the raw material processing module processes the raw material and supplies the processed raw material to the extrusion module;
[0011] S2, extruding the raw material through the extrusion module and wrapping it around the outer periphery of the conductor to form a low-temperature protection layer;
[0012] S3, injecting a chemical or physical foaming agent into the raw material in the extrusion process of the extrusion module through a bubble module, so that tiny bubbles are formed in the low-temperature protection layer;
[0013] S4, curing and cooling the low-temperature protective layer through a curing and cooling module, and collecting state data of the low-temperature protective layer through a sampling module;
[0014] S5, obtaining the state data sampled by the sampling module through a quality assessment module, and evaluating the formed low-temperature protective layer to form an assessment result;
[0015] S6. Obtaining the evaluation result and the set qualified threshold range through the control module, and dynamically adjusting the extrusion parameters of the extrusion module if the trigger condition is met;
[0016] S7. Extruding the insulating material through the insulating protection module and wrapping it outside the low-temperature protection layer to form an outer protective layer.
[0017] Optionally, the method for producing the low-temperature resistant cable further comprises: the sampling module collects the status data of at least two angles of the circumference of the low-temperature protection layer during the process of sampling the low-temperature protection layer.
[0018] Optionally, in step S2, during the extrusion process of the extrusion module, the conductor is pulled by a pulling module so that the low-temperature protection layer is wrapped around the conductor;
[0019] Wherein, the pulling speed of the pulling module is adapted to the extrusion speed of the extrusion module.
[0020] Optionally, the method for producing the low-temperature resistant cable further comprises: adding a low-temperature plasticizer DOA or a flexible epoxy compound during the processing of the raw materials.
[0021] Optionally, in step S7, the insulating material used in the insulating protection module includes at least one of polyethylene, cross-linked polyethylene, polyvinyl chloride, polyvinylidene fluoride, polyetheretherketone or polyimide.
[0022] Optionally, the method for producing the low-temperature resistant cable further includes: in step S5, the state data includes: temperature T, attenuation coefficient A of the sound wave in the low-temperature protective layer, density D and elastic modulus E of the low-temperature protective layer.
[0023] Optionally, the method for producing the low-temperature resistant cable further includes: in step S5, the quality assessment module obtains the state data collected by the sampling module, and calculates the state index State of the low-temperature protection layer according to the following formula:
[0024]
[0025] In the formula, T is the temperature of the low-temperature protective layer, A is the attenuation coefficient of the sound wave in the low-temperature protective layer, D is the density of the low-temperature protective layer, and E is the elastic modulus of the low-temperature protective layer.
[0026] Optionally, the method for producing the low-temperature resistant cable further includes: in step 6, the trigger condition is set as:
[0027] The state index State exceeds a set qualified threshold range.
[0028] Optionally, the method for producing the low-temperature resistant cable further comprises: after obtaining the outer protective layer, performing a cooling treatment on the outer protective layer by a cooling module.
[0029] The beneficial effects achieved by the present invention are:
[0030] 1. Through the cooperation between the extrusion module and the bubble module, the low-temperature protective layer forms a bubble structure, which improves the low-temperature resistance of the cable and ensures that the entire cable production process has the advantages of strong low-temperature resistance, high manufacturing process precision, good cable protection effect and strong cable toughness; the curing and cooling module is arranged after the extrusion process of the extrusion module, and is used for the extruded low-temperature protective layer;
[0031] 2. Through the cooperation between the curing unit and the cooling unit, the low-temperature protective layer can be cured and cross-linked, the strength of the low-temperature protective layer is improved, and the stability and reliability of the foam structure of the low-temperature protective layer are maintained;
[0032] 3. Through the cooperation of the sampling module and the quality assessment module, the quality of the cable production process can be monitored and evaluated, which improves the reliability and accuracy of the entire cable preparation process and ensures that the entire system has the advantages of precise quality control, high intelligence, and good low-temperature antifreeze effect;
[0033] 4. Through the cooperation between the pulling module and the extrusion module, the cable production process is made more efficient, ensuring that the entire system has the advantages of high intelligence, strong low temperature resistance of the cable, high pulling stability, and good synchronous pulling reliability;
[0034] 5. Through the cooperation between the insulation protection module and the cooling module, the manufacturing precision of the outermost protective layer is higher, ensuring that the entire system has the advantages of good protection effect, precise quality control, good cable toughness and high intelligence. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] The present invention can be further understood from the following description in conjunction with the accompanying drawings. The components in the figures are not necessarily drawn to scale, but the emphasis is placed on illustrating the principles of the embodiments. In different views, the same reference numerals designate the same parts.
[0036] Figure 1The present invention is a schematic flow chart of the steps of the production method.
[0037] Figure 2 It is a block diagram of the production system of the present invention.
[0038] Figure 3 It is a schematic diagram of the evaluation process of the sampling module and the quality evaluation module of the present invention.
[0039] Figure 4 It is a top view schematic diagram of the production system of the present invention.
[0040] Figure 5 It is a schematic cross-sectional structure diagram of the pulling module of the present invention.
[0041] Figure 6 for Figure 4 Schematic cross-sectional view at AA in the middle.
[0042] Figure 7 for Figure 6 Enlarged schematic diagram of point C in the middle.
[0043] Figure 8 for Figure 7 Enlarged schematic diagram of point E in the middle.
[0044] Fig. 9 for Figure 6 A magnified schematic diagram of point B in the middle.
[0045] Fig.10 This is a schematic diagram of an application scenario in which the curing unit of the present invention performs a curing operation on a low-temperature protective layer.
[0046] Fig.11 This is a schematic diagram of an application scenario in which the cooling unit of the present invention performs cooling operation on the low-temperature protective layer.
[0047] Fig.12 It is a structural schematic diagram of the sampling module of the present invention.
[0048] Fig.13 It is a partial top view schematic diagram of the detection seat, steering gear and positioning marking member of the present invention.
[0049] Fig.14 It is a schematic side view of the insulation protection module of the present invention.
[0050] Fig.15 for Fig.14 Enlarged schematic diagram of point D in the middle.
[0051] Fig.16 This is a schematic diagram of an application scenario in which the cooling module of the present invention performs a cooling operation on an outer protective layer.
[0052] Explanation of reference numerals: 1. conductor; 2. pulling track; 3. connecting seat; 4. electronic pressure relief valve; 5. clamping airbag; 6. extrusion module; 7. curing chamber; 8. water storage tank; 9. sampling module; 10. insulation protection module; 11. cooling module; 12. cooling water tank; 13. positioning marker; 14. low temperature protection layer; 15. curing lamp; 16. atomizing nozzle; 17. cooling pipe; 18. steering drive mechanism; 19. identification probe; 20. detection base; 21. limit rod; 22. sliding track; 23. steering gear; 24. detection seat; 25. ultrasonic transmitter; 26. ultrasonic collector; 27. extrusion chamber; 28. Extrusion drive mechanism; 29, extrusion die; 30, extrusion screw; 31, bubble module; 32, supply chamber; 33, stirring rod; 34, stirring drive mechanism; 35, heating element; 36, supply screw; 37, supply drive mechanism; 38, extrusion chamber; 39, extrusion drive mechanism; 40, extrusion die; 41, heating element; 42, heating chamber; 43A, β temperature sensor; 43B, γ temperature sensor; 44, transmission drive mechanism; 45, transmission screw; 46, transmission chamber; 47, cooling chamber; 48, cooling nozzle; 49, outer protective layer; 50, cooling pipe; 51, liquid supply tank; 52, electronic on-off valve; 53, booster pump. DETAILED DESCRIPTION
[0053] The following is an explanation of the embodiments of the present invention through specific embodiments. Those skilled in the art can understand the advantages and effects of the present invention from the contents disclosed in this specification. The present invention can be implemented or applied through other different specific embodiments, and the details in this specification can also be modified and changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. In addition, the drawings of the present invention are only simple schematic illustrations and are not depicted according to actual sizes. It is stated in advance. The following embodiments will further explain the relevant technical contents of the present invention in detail, but the disclosed contents are not intended to limit the scope of protection of the present invention.
[0054] Embodiment 1: According to Figure 1 , Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 , Fig.14 , Fig.15 and Fig.16 As shown, this embodiment provides a method for producing a low-temperature resistant cable, and the method for producing a low-temperature resistant cable comprises the following steps:
[0055] S1, the raw material processing module processes the raw material and supplies the processed raw material to the extrusion module 6;
[0056] S2, extruding the raw material through the extrusion module 6 and wrapping it around the outer periphery of the conductor 1 to form a low-temperature protection layer 14;
[0057] In this embodiment, the extrusion module 6 can also be used to extrude the raw material and wrap it around the outer periphery of the conductor 1 wrapped with a protective sleeve (inner protective layer);
[0058] S3, injecting a chemical or physical foaming agent into the raw material in the extrusion process of the extrusion module 6 through the bubble module 31, so that tiny bubbles are formed in the low-temperature protection layer 14;
[0059] S4, curing and cooling the low temperature protection layer 14 through a curing and cooling module, and collecting state data of the low temperature protection layer 14 through a sampling module 9;
[0060] S5, obtaining the state data sampled by the sampling module 9 through a quality evaluation module, and evaluating the formed low-temperature protective layer 14 to form an evaluation result;
[0061] S6, obtaining the evaluation result and the set qualified threshold range through the control module, and dynamically adjusting the extrusion parameters of the extrusion module 6 if the trigger condition is met;
[0062] S7, extruding the insulating material through the insulating protection module 10 and wrapping it outside the low-temperature protection layer 14 to form an outer protective layer 49;
[0063] In the present embodiment, a production system for low-temperature resistant cables is also provided, the production system comprising a server, a central processing unit, a raw material processing module, a pulling module, an extrusion module 6, a bubble module 31, a curing and cooling module, a sampling module 9, a quality assessment module, a control module, an insulation protection module 10 and a cooling module 11, the server is respectively connected to the raw material processing module, the pulling module, the extrusion module 6, the bubble module 31, the curing and cooling module, the sampling module 9, the quality assessment module, the control module, the insulation protection module 10 and the cooling module 11 and stores the intermediate data and process data of the raw material processing module, the pulling module, the extrusion module 6, the bubble module 31, the curing and cooling module, the sampling module 9, the quality assessment module, the control module, the insulation protection module 10 and the cooling module 11 in the database of the server for query or call;
[0064] The central processing unit is respectively connected to the raw material processing module, the pulling module, the extrusion module 6, the bubble module 31, the curing cooling module, the sampling module 9, the quality assessment module, the control module, the insulation protection module 10 and the cooling module 11, and based on the central processing unit, the raw material processing module, the pulling module, the extrusion module 6, the bubble module 31, the curing cooling module, the sampling module 9, the quality assessment module, the control module, the insulation protection module 10 and the cooling module 11 are centrally controlled, and the control data is transmitted to the database of the server for storage, so as to improve the efficiency and reliability of the entire system for cable generation;
[0065] The raw material processing module pre-processes the raw material and supplies it to the extrusion module 6. The extrusion module 6 extrude the raw material processed by the raw material processing module and wraps it around the conductor 1 to form a low-temperature protection layer 14.
[0066] The bubble module 31 is used to apply pressurized gas to the low-temperature protection layer 14 so that tiny bubbles are formed in the low-temperature protection layer 14. The solidification and cooling module solidifies and cools the low-temperature protection layer 14. The sampling module 9 samples the low-temperature protection layer 14 to obtain the status data of the low-temperature protection layer 14. The quality assessment module assesses the low-temperature protection layer 14 according to the status data to form an assessment result. The control module obtains the assessment result and the set qualified threshold range. If the trigger condition is met, the extrusion parameter of the extrusion module 6 is dynamically adjusted. The insulation protection module 10 extrude and wrap the insulation material outside the low-temperature protection layer 14 to form an outer protective layer 49. The cooling module 11 is used to cool the outer protective layer 49.
[0067] Optionally, the production method of the low-temperature resistant cable further comprises: adding a low-temperature plasticizer DOA or a flexible epoxy compound during the processing of the raw materials;
[0068] In this embodiment, the raw materials include but are not limited to the following: polyethylene (PE), polyvinyl chloride (PVC), cross-linked polyethylene (XLPE), high-density polyethylene (HDPE);
[0069] The feedstock is configured to be processed in the feedstock processing module;
[0070] The raw material processing module includes a stirring unit, a heating unit and a supply unit, wherein the heating unit heats the raw material, the stirring unit stirs the heated raw material to make the raw material in a molten state more uniform, and the supply unit supplies the stirred molten raw material to the extrusion module 6;
[0071] The stirring unit comprises a stirring chamber, a stirring rod 33, a support seat and a stirring drive mechanism 34. The stirring chamber is used to place the raw materials. The stirring chamber is provided with an inlet. One end of the stirring rod 33 is drivingly connected to the stirring drive mechanism 34 to form a stirring portion. The other end of the stirring rod 33 extends toward the stirring chamber. The support seat is arranged on the inner wall of the inlet of the stirring chamber. The stirring portion is arranged on the support seat to stir the raw materials introduced through the inlet.
[0072] Among them, Fig. 9 As shown, the delivery ports are arranged on both sides of the support seat, so that the raw materials can easily enter the stirring chamber;
[0073] The supply unit includes a supply chamber 32, a supply screw 36 and a supply drive mechanism 37. The supply screw 36 is disposed in the supply chamber 32 and supplies the raw material entering the supply chamber 32. One end of the supply screw 36 is drivingly connected to the supply drive mechanism 37 to form a supply portion. The other end of the supply screw 36 extends into the supply chamber 32 and supplies the raw material in a molten state in the supply chamber 32, so that the raw material can be supplied from the stirring chamber to the extrusion module 6.
[0074] Among them, Fig. 9 As shown, the supply portion is arranged outside the supply cavity 32;
[0075] The heating unit is disposed in the inner wall of the stirring chamber and the supply chamber 32, and heats the raw material put into the stirring chamber and the raw material supplied in the supply chamber 32;
[0076] The heating unit includes a heating element 35 and a current controller, wherein the heating element 35 is spirally arranged along the inner walls of the stirring chamber and the supply chamber 32, respectively, wherein the heating element 35 is electrically connected to the current controller, and the current controller controls the heating temperature of the heating element 35 so that the heating element 35 can heat and cause the raw material to become a molten state;
[0077] The raw materials are processed by the raw material processing module, so that the preparation process of the low temperature protection layer 14 of the cable is more efficient, ensuring that the entire cable production has the advantages of high reliability and strong stability in the preparation process;
[0078] The extrusion module 6 includes an extrusion screw 30, an extrusion cavity 27, an extrusion die 29, and an extrusion drive mechanism 28. One end of the extrusion screw 30 is drivingly connected to the extrusion drive mechanism 28 to form an extrusion portion. The other end of the extrusion screw 30 extends into the extrusion cavity 27 to extrude the raw material in the extrusion cavity 27. The extrusion die 29 is arranged at the extrusion port of the extrusion cavity 27 to shape the extruded low-temperature protective layer 14.
[0079] The extrusion module 6 further includes a mold placement cavity, which is arranged at the extrusion port of the extrusion cavity 27 and is used to place the extrusion mold 29;
[0080] In addition, the extrusion die 29 is detachably connected to the die placement cavity;
[0081] The bubble module 31 includes a liquid supply channel, a liquid supply tank 51, a booster pump 53 and an electronic on-off valve 52, wherein the liquid supply tank 51 stores the chemical or physical foaming agent, one end of the liquid supply channel is connected to the booster pump 53 to form a supply part, and the supply part is arranged in the liquid supply tank 51, and the other end of the liquid supply channel extends out of the extrusion cavity 27, so that bubbles can be generated in the raw material and extruded and wrapped around the outer periphery of the conductor 1;
[0082] The electronic on-off valve 52 is used to control the on-off of the liquid supply channel, and further control the liquid supply timing of the liquid supply channel;
[0083] The bubble module 31 injects a chemical or physical foaming agent into the raw material during the extrusion process of the extrusion module 6, including: a chemical or physical foaming agent;
[0084] Among them, chemical foaming agents decompose to produce gas during heating, such as azodicarbonamide (ADCA);
[0085] Physical foaming agents are gases such as carbon dioxide or nitrogen injected under high pressure;
[0086] In this embodiment, a chemical foaming agent is preferably used;
[0087] Through the cooperation between the extrusion module 6 and the bubble module 31, the low-temperature protection layer 14 forms a bubble structure, which improves the low-temperature resistance of the cable and ensures that the entire cable production process has the advantages of strong low-temperature resistance, high manufacturing process accuracy, good cable protection effect and strong cable toughness;
[0088] The curing and cooling module is arranged after the extrusion process of the extrusion module 6, and is used to cool the extruded low-temperature protective layer 14;
[0089] The curing and cooling module includes a curing unit and a cooling unit. The curing unit cures and cross-links the low-temperature protection layer 14, and the cooling unit cools the low-temperature protection layer 14 to maintain the stability and uniformity of the foam structure.
[0090] The curing unit comprises a curing chamber 7, a curing lamp 15 and an intensity adjuster, wherein the curing chamber 7 is used for allowing the conductor 1 wrapped with the low-temperature protective layer 14 to pass through, the curing lamp 15 cures the low-temperature protective layer 14, and the intensity adjuster is used for adjusting the intensity of the curing lamp 15;
[0091] The curing chamber 7 is configured as a hollow passage chamber, and the passage chamber is used for the conductor 1 wrapped with the low-temperature protection layer 14 to pass through. Meanwhile, the curing lamp 15 is arranged on the inner wall of the passage chamber;
[0092] In addition, the curing lamp 15 is electrically connected to the strength adjuster so that the conductor 1 wrapped with the low-temperature protection layer 14 can be cross-linked and cured to form a stable structure;
[0093] At the same time, the curing temperature of the curing lamp 15 needs to be adjusted in combination with historical data and set and adjusted through the intensity adjuster, so as to improve the stability and reliability of the low-temperature protection layer 14;
[0094] In this embodiment, after the curing or cross-linking operation, the conductor 1 wrapped with the low-temperature protection layer 14 is cooled by the cooling unit;
[0095] The cooling unit includes a cooling pipe 17, a cooling pump, a water storage tank 8, and at least two atomizing nozzles 16. The water storage tank 8 is used to store cooling water. One end of the cooling pipe 17 is connected to the at least two atomizing nozzles 16. The other end of the cooling pipe 17 is connected to the cooling pump to form a cooling part. The cooling part is arranged in the water storage tank 8, and the water in the water storage tank 8 is sprayed onto the low-temperature protection layer 14 through the cooling pipe 17 and the at least two atomizing nozzles 16 to achieve cooling.
[0096] At the same time, at least two atomizing nozzles 16 are symmetrically arranged on the inner wall of the passage cavity, and generate an atomized cooling mist curtain, so that the temperature of the low-temperature protection layer 14 can be quickly reduced;
[0097] Through the cooperation between the curing unit and the cooling unit, the low-temperature protection layer 14 can be cured and cross-linked, thereby improving the strength of the low-temperature protection layer 14 and maintaining the stability and reliability of the foam structure of the low-temperature protection layer 14;
[0098] Optionally, in step S2, while the extrusion module 6 extrude the raw material, gas is injected into the formed low-temperature protection layer 14 through the bubble module 31, so that tiny bubbles are formed in the low-temperature protection layer 14;
[0099] Optionally, the method for producing the low-temperature resistant cable further comprises: the sampling module collects the state data of at least two angles of the circumference of the low-temperature protection layer 14 during the process of sampling the low-temperature protection layer 14;
[0100] Optionally, in step S2, during the extrusion process of the extrusion module 6, the conductor 1 is pulled by a pulling module so that the conductor 1 is wrapped with the low-temperature protection layer 14;
[0101] Wherein, the pulling speed of the pulling module is adapted to the extrusion speed of the extrusion module 6;
[0102] In this embodiment, if Figure 4 As shown, the pulling module is arranged on one side of the extrusion module 6 and the cooling module 11, that is, the conductor 1 is pulled, and the conductor 1 wrapped with the outer protective layer 49 after being cooled by the cooling module 11 is pulled;
[0103] The pulling module includes a pulling unit and a pulling evaluation unit, wherein the pulling unit is used to pull the conductor 1 and the conductor 1 wrapped with the outer protective layer 49 synchronously, and the pulling evaluation unit evaluates the pulling speed of the pulling airbag so that the pulling airbag conductor 1 and the conductor 1 wrapped with the outer protective layer 49 are pulled synchronously;
[0104] The pulling unit includes a clamping airbag 5, an air pump, an electronic pressure relief valve 4, a connecting seat 3, a pulling track 2, a pulling drive mechanism and a supporting seat, wherein the supporting seat supports the pulling track 2, and the connecting seat 3 is slidably connected with the pulling track 2, wherein the pulling drive mechanism is arranged on the connecting seat 3, and drives the connecting seat 3 to slide along the direction of the pulling track 2, and the air pump inflates the clamping airbag 5 so that the clamping airbag 5 is inflated and expanded, so as to clamp the conductor 1 and the conductor 1 wrapped with the outer protective layer 49, wherein the clamping airbag 5 is provided with an electronic pressure relief valve 4, and the gas in the clamping airbag 5 is discharged, and the clamping airbag 5 is arranged on the connecting seat 3, and moves with the movement of the connecting seat 3;
[0105] The clamping airbag 5 is set to be annular, and after being inflated, it can clamp the conductor 1 and the conductor 1 wrapped with the outer protective layer 49;
[0106] The pulling process of the pulling module includes:
[0107] The connecting seat 3 is at the initial end of the pulling track 2, and the central processing unit controls the air pump to inflate the clamping airbag 5, so that the clamping airbag 5 is inflated and expanded to clamp the conductor 1 and the conductor 1 wrapped with the outer protective layer 49. At this time, the central processing unit controls the connecting seat 3 to slide along the length direction of the pulling track 2, so that the connecting seat 3 and the clamping airbag 5 on the connecting seat 3 move forward synchronously, so that the clamping airbag and the connecting seat 3 move to the end of the pulling track 2 (the pulling length is equivalent to the length of the pulling track 2);
[0108] When the connection seat 3 reaches the end of the pulling track 2, the central processor controls the electronic pressure relief valve 4 to discharge the gas in the clamping airbag 5, thereby releasing the clamping state of the clamping airbag 5 on the conductor 1 and the conductor 1 wrapped with the outer protective layer 49, and the central processor controls the pulling drive mechanism to drive the connection seat 3 from the end of the pulling track 2 back to the initial end, and repeats the above process, thereby realizing the reciprocating pulling of the conductor 1 and the conductor 1 wrapped with the outer protective layer 49;
[0109] The pulling evaluation unit obtains the extrusion speed of the extrusion molding module and determines the pulling speed V of the pulling unit according to the following formula: PULL :
[0110] V PULL =V extrusion (1+μ);
[0111] Where μ is the adjustment coefficient, and its value is determined based on historical operating data. extrusion is the actual extrusion speed parameter (m / s, meters per second) of the extrusion molding module on the outer protective layer, and its value is determined according to the following formula:
[0112] V extrusion =n·τ·(1-k F F);
[0113] Wherein, n is the target speed of the extrusion screw for the outer protective layer, the unit is: revolutions per second (1 / s), the speed is the known speed pre-set by the staff according to the extruded material, τ is the conversion coefficient, that is, through experimental determination, the screw speed is measured when there is no resistance (that is, the screw idling speed), the actual extrusion speed is measured under an ideal working environment, and the linear speed generated by each screw rotation is determined, the unit is: meter per revolution (m / revolution), F is the resistance of the screw (that is, the resistance F of the screw is related to the properties of the extruded material itself, which can be obtained by the pressure sensor on the screw. Unit: (1 / N, 1 / Newton)), k FTo adjust the factor, the actual extrusion speed of the screw was measured under different resistances through experimental determination and determined by fitting the data;
[0114] In this embodiment, the conversion coefficient τ and the adjustment factor k are determined according to the following steps: F , specifically:
[0115] 1) Conversion coefficient τ:
[0116] Experimental determination: Measure the screw speed n' without resistance, and measure the actual extrusion speed V in an ideal working environment using the same material as the outer protective layer. extrusion (i.e. the actual extrusion speed when the same material as the outer protective layer is extruded with the speed n' as the instruction under the ideal working environment), determine τ:
[0117]
[0118] 2) Adjustment factor k F :
[0119] Experimental determination: Based on the resistance generated by different materials, measure the actual extrusion speed V extrusion (i.e. the actual extrusion speed generated when different materials are extruded with the speed n' as the instruction under the ideal working environment), k is determined by linear regression fitting of the data F :
[0120]
[0121] In this embodiment, the pulling module and the extrusion module 6 cooperate with each other to make the production process of the cable more efficient, ensuring that the entire system has the advantages of high intelligence, strong low temperature resistance of the cable, high pulling stability, and good synchronous pulling reliability;
[0122] The sampling module 9 includes a steering unit and a sampling unit, wherein the sampling unit collects the status data of the low temperature protection layer 14, and the steering unit adjusts the collection angle of the sampling unit so that the sampling unit can collect the performance data of multiple angles of the low temperature protection layer 14;
[0123] The sampling unit includes an ultrasonic transmitter 25, an ultrasonic collector 26, a β temperature sensor 43A and a data storage device. The ultrasonic transmitter 25 transmits ultrasonic waves to the low-temperature protection layer 14. The ultrasonic collector 26 collects ultrasonic wave data reflected by the low-temperature protection layer 14. The β temperature sensor 43A collects temperature data of the low-temperature protection layer 14. The data storage device stores the ultrasonic wave emission intensity of the ultrasonic transmitter 25, the ultrasonic wave intensity obtained by the ultrasonic wave collection, and the temperature data collected by the β temperature sensor 43A.
[0124] The steering unit includes a detection base 20, a detection seat 24, a steering gear 23, a steering drive mechanism 18, an identification probe 19, and at least two positioning markers 13. The detection base 20 is provided with a detection hole, and the detection hole is for the conductor 1 to pass through. The sampling unit is arranged on the detection seat 24, and the steering gear 23 is nested on the detection seat 24. The steering gear 23 is arranged on the inner wall of the detection cavity and meshes with the steering gear 23. At least two positioning markers 13 are arranged on the detection seat 24 and are distributed at equal intervals along the circumferential direction of the outer wall of the detection seat 24. The identification probe 19 is arranged on the inner wall of the detection hole and is arranged relative to the positioning marker 13.
[0125] A sliding track 22 is provided on the cavity wall of the detection base 20, and the sliding track 22 is coaxially arranged with the detection hole;
[0126] The steering unit further includes at least two limiting rods 21, each limiting rod 21 being U-shaped, and one end of each limiting rod 21 being connected to the connecting seat 3, and the other end of each limiting rod 21 being slidably connected to the sliding track 22, and when the steering drive mechanism 18 drives the detection seat 24, the detection seat 24 can be limited, so that the sampling unit can collect the performance data of the low temperature protection layer 14;
[0127] Optionally, the method for producing the low-temperature resistant cable further comprises: in step S5, the state data comprises: temperature T, attenuation coefficient A of the sound wave in the low-temperature protective layer 14, density D and elastic modulus E of the low-temperature protective layer 14;
[0128] In this embodiment, the temperature T is directly measured by the β temperature sensor 43A, and the attenuation coefficient A in the low temperature protection layer 14 is calculated by the following formula:
[0129]
[0130] Wherein, P0 is the power before material attenuation, and its value is determined by the ultrasonic transmitter; P is the power after material attenuation, and its value is collected by the ultrasonic collector; d is the distance that the sound wave propagates in the material, and the distance unit is preferably centimeters (CM), that is, the fixed distance of the extruded low-temperature protective layer (such as Fig.12 shown);
[0131] The density D of the low temperature protection layer (unit: kg / m 3 ) is calculated according to the following formula:
[0132]
[0133] Where Z is the acoustic impedance of the cryogenic protection layer, unit: Pa·s / m or kg / (m 2 ·s), whose value is directly measured by experimental means (equivalent to a known value), v is the propagation speed of the ultrasonic wave in the low-temperature protective layer, in meters per second (m / s), and its value is based on:
[0134]
[0135] Wherein, d is the distance that the sound wave propagates in the material, in meters, and t is the propagation time of the sound wave, in seconds, that is, the time from when the ultrasonic generator emits the sound wave to when the ultrasonic collector receives the ultrasonic wave;
[0136] The elastic modulus E is calculated according to the following formula:
[0137] E=D·v 2 ;
[0138] Wherein, D is the density of the low temperature protection layer, unit: (kg / m 3 ), v is the propagation speed of the ultrasonic wave in the low-temperature protective layer, unit: meter per second (m / s);
[0139] Optionally, the method for producing the low-temperature resistant cable further includes: in step S5, the quality assessment module obtains the state data collected by the sampling module, and calculates the state index State of the low-temperature protection layer according to the following formula:
[0140]
[0141] Wherein, T is the temperature of the cryogenic protective layer, unit: Celsius (℃), A is the attenuation coefficient of the sound wave in the cryogenic protective layer, decibel per centimeter (dB / cm), and D is the density of the cryogenic protective layer, unit: kg / m 3 , E is the elastic modulus of the low-temperature protective layer, unit: Pascal (Pa);
[0142] Optionally, the method for producing the low-temperature resistant cable further includes: in step 6, the trigger condition is set as:
[0143] The state index State exceeds the set qualified threshold range;
[0144] The qualified threshold range (Range 1 and Range 2 are used as examples) is set by the administrator or the system according to the actual situation of the low-temperature protection layer. This is a technical means well known to those skilled in the art. Those skilled in the art can refer to relevant technical manuals to learn about the technology, so it will not be described in detail in this embodiment.
[0145] Specifically, if the state index State of the low-temperature protection layer is not in the range of [Range1, Range2], it means that the state of the low-temperature protection layer does not meet the system requirements, and the adjustment module is triggered to adjust the extrusion parameters of the extrusion module;
[0146] If the state index State of the low-temperature protection layer is in the range of [Range1, Range2], it means that the state of the low-temperature protection layer meets the system requirements, and the current extrusion parameters of the extrusion module and the foaming parameters of the bubble module are maintained;
[0147] The control module includes an extrusion parameter adjustment unit and an extrusion analysis unit, wherein the extrusion analysis unit is used to analyze the extrusion parameters of the extrusion module to form an extrusion analysis result, and the extrusion parameter adjustment unit triggers the adjustment of the extrusion parameters of the extrusion module according to the extrusion analysis result of the extrusion analysis unit;
[0148] The extrusion analysis unit obtains the state index State and the set qualified threshold range, and calculates the extrusion parameter according to the following formula:
[0149]
[0150] Where, T new is the newly adjusted temperature adjustment value, P new is the newly adjusted pressure adjustment value, T is the original temperature value, P is the original pressure value, α T is the temperature adjustment proportional factor, and its value is set according to the actual situation. P is the pressure adjustment proportional factor, and its value is set according to the specific actual situation. If State < Range1, it takes a "+" sign, if State > Range2, it takes a "-" sign, State is the state index of the low-temperature protection layer, and Target is the center point of the set qualified threshold: its value is determined according to the following formula (the set qualified threshold range [Range1, Range2], that is, taking Range1, Range2 as an example):
[0151]
[0152] In the formula, Range1 is the lower limit of the set qualified threshold range, Range2 is the upper limit of the set qualified threshold range, and Range2>Range1;
[0153] The temperature adjustment proportional factor α T and the pressure adjustment proportional factor α P The value ranges are:
[0154] αT ∈[0.1, 1.0];
[0155] α P ∈[0.1, 5.0];
[0156] In this embodiment, a method for determining the temperature adjustment proportional factor α is provided. T and pressure adjustment factor α P An example, specifically:
[0157] (1) When the raw material is cross-linked polyethylene (XLPE), then:
[0158] Temperature adjustment factor α T =0.8;
[0159] Pressure adjustment proportional factor α P =2.0;
[0160] (2) When the raw material is PVC, then:
[0161] Temperature adjustment factor α T =0.5;
[0162] Pressure adjustment proportional factor α P =1.0;
[0163] (3) When the raw material is high-density polyethylene (HDPE), then:
[0164] Temperature adjustment factor α T =0.6;
[0165] Pressure adjustment proportional factor α P =1.5;
[0166] For any of the above scenarios, the tuning steps include:
[0167] S11. Experiment and data collection: Conduct controlled experiments in actual production environments and collect data on the effects of temperature and pressure on state indexes;
[0168] S12, optimization and adjustment: based on the collected data, using statistical methods to optimize the temperature adjustment proportional factor and the pressure adjustment proportional factor;
[0169] S13, implementation and monitoring: apply the optimized temperature adjustment proportional factor and pressure adjustment proportional factor to production, continuously monitor their effects, and make fine adjustments as needed;
[0170] In summary, the process of setting and optimizing the temperature adjustment proportional factor and the pressure adjustment proportional factor will ensure the quality and consistency of cable production to meet the needs of specific applications;
[0171] The extrusion parameter adjustment unit obtains the new extrusion parameter (extrusion analysis result) calculated by the extrusion analysis unit, transmits the extrusion parameter to the central controller, and triggers the central controller to control the extrusion module 6 to improve the control accuracy and reliability of the low-temperature protection layer 14;
[0172] Optionally, in step S6, the insulating material used by the insulating protection module 10 includes at least one of polyethylene (PE), cross-linked polyethylene (XLPE), polyvinyl chloride (PVC), polyvinylidene fluoride (PVDF), polyetheretherketone (PEEK) or polyimide (PI);
[0173] The insulation protection module 10 includes a heating unit, an extrusion unit and a transmission unit. The heating unit heats the insulation material. The transmission unit transmits the insulation material heated by the heating unit to the extrusion unit. The extrusion unit extrude the molten insulation material and wraps it around the low-temperature protection layer 14 to form an outer protective layer.
[0174] The temperature rising unit comprises a heating chamber 42, a temperature rising component 41, a temperature rising controller and a γ temperature sensor 43B. The heating chamber 42 is used to place the insulating material. The γ temperature sensor 43B collects the temperature in the heating chamber 42. The temperature rising component 41 heats the insulating material in the heating chamber 42 so that the insulating material can become a molten state. The temperature rising controller controls the temperature of the temperature rising component 41 based on the γ temperature sensor 43B.
[0175] The transmission unit includes a transmission chamber 46, a transmission screw 45, and a transmission drive mechanism 44. The transmission chamber 46 connects the heating chamber 42 and the extrusion unit so that the molten insulating material can be processed and transmitted smoothly. One end of the transmission screw 45 is drivingly connected to the transmission drive mechanism 44 to form a transmission part, and the other end of the transmission screw 45 passes through the transmission chamber 46 and extends out of the transmission chamber 46.
[0176] In addition, the transmission chamber 46 is set as a sealed chamber structure;
[0177] The temperature raising member 41 is disposed around the inner wall of the heating chamber 42 and the transmission chamber 46, so that the molten insulating material processed and transmitted through the heating chamber 42 and the transmission chamber 46 can be processed and supplied smoothly;
[0178] The extrusion unit includes an extrusion cavity 38, an extrusion screw, and an extrusion drive mechanism 39. The extrusion cavity 38 is used to place the extrusion screw. The extrusion cavity 38 is used to place the insulating material in a molten state, and the extrusion cavity 38 is provided with an extrusion port. The extrusion screw 30 is arranged in the extrusion cavity 38, and extrude the insulating material in a molten state from the extrusion port of the extrusion cavity 38. One end of the extrusion screw is connected to an extrusion portion driven by the extrusion drive mechanism 39. The extrusion portion is arranged outside the extrusion cavity 38, so that the other end of the extrusion screw passes through the extrusion cavity 38 and extends into the interior of the extrusion cavity 38, and extrude the insulating material in a molten state from the extrusion port of the extrusion cavity 38.
[0179] The extrusion unit further includes a mold placement groove and an extrusion mold 40, wherein the mold placement groove is for placing the extrusion mold 40, and the extrusion placement groove is arranged at the extrusion port, and the extrusion mold 40 performs shaping on the extruded outer protective layer 49 so that the insulating material in a molten state is evenly wrapped around the outer periphery of the low-temperature protective layer 14;
[0180] Wherein, the extrusion mold 40 is detachably connected to the mold placement groove;
[0181] Meanwhile, for the manufacture of cables with different circumferences, an appropriate extrusion die 40 is selected, which is a technical means well known to those skilled in the art. Those skilled in the art can refer to relevant technical manuals to learn about the technology, so it will not be described in detail in this embodiment.
[0182] Optionally, the method for producing the low-temperature resistant cable further comprises: after obtaining the outer protective layer, cooling the outer protective layer 49 by means of a cooling module 11;
[0183] The cooling module 11 includes a cooling chamber 47, a cooling pipe 50, a cooling water tank 12, and at least two cooling nozzles 48. The cooling chamber 47 is provided with a hollow sliding channel. The cooling water tank 12 stores cooling water. The cooling nozzle 48 sprays cooling water to cool the extruded outer protective layer 49. The cooling pipe 50 connects the cooling water tank 12 and the cooling nozzle 48.
[0184] The cooling nozzle 48 is disposed on the inner wall of the cooling chamber 47 and is disposed toward the outer protective layer 49;
[0185] At the same time, the cooling module 11 uses water cooling to quickly cool the extruded outer protective layer 49;
[0186] The units involved in this example are all examples, and those skilled in the art can set different appropriate units according to their own needs when implementing this solution.
[0187] In this embodiment, through the cooperation between the insulation protection module 10 and the cooling module 11, the manufacturing accuracy of the outermost protective layer 49 is higher, ensuring that the entire system has the advantages of good protection effect, precise quality control, good cable toughness and high intelligence.
[0188] Embodiment 2: This embodiment should be understood to include all the features of any of the above embodiments, and further improve upon them. Figure 1 , Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 , Fig.14 , Fig.15 and Fig.16 As shown, the control module further includes a foaming analysis unit and a foaming parameter adjustment unit, wherein the foaming analysis unit is used to analyze the foaming parameters of the foaming module to form a foaming analysis result, and the foaming parameter adjustment unit triggers the adjustment of the foaming parameters of the foaming module according to the foaming analysis result of the foaming analysis unit;
[0189] The qualified threshold range (Range 1 and Range 2 are used as examples) is set by the administrator or the system according to the actual situation of the low-temperature protection layer. This is a technical means well known to those skilled in the art. Those skilled in the art can refer to relevant technical manuals to learn about the technology, so it will not be described in detail in this embodiment.
[0190] Specifically, if the state index State of the low-temperature protection layer is not in the range of [Range1, Range2], it means that the state of the low-temperature protection layer does not meet the system requirements, and the adjustment module is triggered to adjust the foaming parameters of the bubble module;
[0191] If the state index State of the low-temperature protection layer is in the range of [Range1, Range2], it means that the state of the low-temperature protection layer meets the system requirements, and the current foaming parameters of the bubble module are maintained;
[0192] The foaming analysis unit obtains the state index State and the set qualified threshold range, and calculates the foaming parameter according to the following formula:
[0193]
[0194] In the formula, R f,new is the newly adjusted foaming ratio value, that is, the volume ratio of the foaming agent to the low-temperature protective layer, R f is the original foaming agent ratio, α R It is the proportional factor for adjusting the proportion of the foaming agent. Its value is set according to the actual situation. Range1 is the lower limit of the qualified threshold range, Range2 is the upper limit of the qualified threshold range, and Range2>Range1 (Range2 and Range1 are not 0). If State<Range1, then take the "+" sign, if State>Range2, then take the "-" sign;
[0195] In this example, the proportional factor α of the foaming agent ratio adjustment is R The value range of is: 0.01% to 0.1% per unit state index difference;
[0196] In this embodiment, a proportional factor α is provided to determine the proportion of the foaming agent. R An example, specifically:
[0197] (1) When the raw material is cross-linked polyethylene (XLPE), then:
[0198] Proportional factor α for adjusting the proportion of foaming agent R =0.04%;
[0199] (2) When the raw material is PVC, then:
[0200] Proportional factor α for adjusting the proportion of foaming agent R =0.02%;
[0201] (3) When the raw material is high-density polyethylene (HDPE), then:
[0202] Proportional factor α for adjusting the proportion of foaming agent R =0.03%;
[0203] In summary, for any of the above scenarios, the tuning steps include:
[0204] S21. Experiment and data collection: Conduct controlled experiments in actual production environments to collect data on the effect of the foaming agent ratio on the state index;
[0205] S22, optimization and adjustment: based on the collected data, using statistical methods to optimize the blowing agent ratio factor;
[0206] S23, implementation and monitoring: applying the optimized foaming agent ratio factor to production, continuously monitoring its effect, and making fine adjustments as needed;
[0207] In summary, the setting and optimization process of the foaming agent ratio factor will ensure the quality and consistency of cable production to meet the needs of specific applications;
[0208] The foaming parameter adjustment unit obtains the new foaming parameter (foaming analysis result) calculated by the foaming analysis unit, transmits the foaming parameter to the central controller, and triggers the central controller to control the foaming module to improve the control accuracy and reliability of the low-temperature protection layer;
[0209] Through the cooperation of the foaming analysis unit and the foaming parameter adjustment unit, the low-temperature protection layer can form pores, thereby improving the low-temperature protection level of the cable and ensuring that the entire cable has the advantages of strong low-temperature resistance, good protection effect and good reliability.
[0210] The contents disclosed above are only preferred feasible embodiments of the present invention, and do not limit the protection scope of the present invention. Therefore, all equivalent technical changes made using the contents of the present invention specification and drawings are included in the protection scope of the present invention. In addition, the elements therein can be updated as technology develops.
Claims
1. A method for producing a low-temperature resistant cable, characterized in that: The production method of the low temperature resistant cable comprises the following steps: S1, the raw material processing module processes the raw material and supplies the processed raw material to the extrusion module; S2, extruding the raw material through the extrusion module and wrapping it around the outer periphery of the conductor to form a low-temperature protection layer; S3, injecting a chemical or physical foaming agent into the raw material in the extrusion process of the extrusion module through a bubble module, so that tiny bubbles are formed in the low-temperature protective layer; S4, curing and cooling the low-temperature protective layer through a curing and cooling module, and collecting state data of the low-temperature protective layer through a sampling module; S5, obtaining the state data sampled by the sampling module through a quality assessment module, and evaluating the formed low-temperature protective layer to form an assessment result; S6. Obtaining the evaluation result and the set qualified threshold range through the control module, and dynamically adjusting the extrusion parameters of the extrusion module if the trigger condition is met; S7, extruding the insulating material through the insulating protection module and wrapping it outside the low-temperature protection layer to form an outer protective layer; The method for producing a low-temperature resistant cable further comprises: the sampling module collecting the state data of at least two angles of the circumference of the low-temperature protective layer during sampling of the low-temperature protective layer; During the extrusion process of the extrusion module, the conductor is pulled by the pulling module so that the low-temperature protection layer is wrapped around the conductor; wherein the pulling speed of the pulling module is adapted to the extrusion speed of the extrusion module; The method for producing a low-temperature resistant cable further comprises: in step S5, the state data comprises: temperature T, attenuation coefficient A of the sound wave in the low-temperature protective layer, density D and elastic modulus E of the low-temperature protective layer; The method for producing low-temperature resistant cables further comprises: in step S5, the quality assessment module obtains the state data collected by the sampling module, and calculates the state index State of the low-temperature protection layer according to the following formula: ; Wherein, T is the temperature of the low-temperature protective layer, A is the attenuation coefficient of the sound wave in the low-temperature protective layer, D is the density of the low-temperature protective layer, and E is the elastic modulus of the low-temperature protective layer; The temperature T is directly measured by the β temperature sensor, and the attenuation coefficient A in the low temperature protection layer is calculated by the following formula: ; Wherein, P0 is the power before material attenuation, and its value is determined by the ultrasonic transmitter; P is the power after material attenuation, and its value is collected by the ultrasonic collector; d is the distance that the sound wave propagates in the material, and the distance unit is centimeters, that is, the fixed distance of the extruded low-temperature protective layer; The density D of the low temperature protection layer, unit: kg / m 3, Calculate according to the following formula: ; Where Z is the acoustic impedance of the cryogenic protection layer, unit: Pa·s / m, or kg / (m 2 ⋅s), its value is directly measured by experimental means, v is the propagation speed of the ultrasonic wave in the low temperature protection layer, unit: meter per second, its value is calculated according to the following formula: ; Wherein, d is the distance that the sound wave propagates in the material, in meters, and t is the propagation time of the sound wave, in seconds, that is, the time from when the ultrasonic generator emits the sound wave to when the ultrasonic collector receives the ultrasonic wave; The elastic modulus E is calculated according to the following formula: ; Wherein, D is the density of the low temperature protection layer, unit: kg / m 3 , v is the propagation speed of the ultrasonic wave in the low-temperature protection layer, unit: meter per second.
2. The method for producing a low-temperature resistant cable according to claim 1, characterized in that: The method for producing a low-temperature resistant cable further comprises: in step 6, the trigger condition is set as: The state index State exceeds a set qualified threshold range.
3. The method for producing a low-temperature resistant cable according to claim 2, characterized in that: The production method of the low-temperature resistant cable further comprises: adding a low-temperature plasticizer DOA or a flexible epoxy compound during the processing of the raw materials.
4. The method for producing a low-temperature resistant cable according to claim 3, characterized in that: In step S7, the insulating material used in the insulating protection module includes at least one of polyethylene, cross-linked polyethylene, polyvinyl chloride, polyvinylidene fluoride, polyetheretherketone or polyimide.
5. The method for producing a low-temperature resistant cable according to claim 4, characterized in that: The method for producing the low-temperature resistant cable further comprises: after obtaining the outer protective layer, cooling the outer protective layer by a cooling module.